Solar Cell Module
The solar cell module employs a high modulus second encapsulant and UV-resistant sealing material at the edges to address edge crushing and enhance structural integrity, reducing sealant peeling and cracking risks.
Patent Information
- Application Number
- JP2021000927
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2021-01-06
- Publication Date
- 2024-11-29
- Estimated Expiration
- 2041-01-06
AI Technical Summary
Solar cell modules experience peripheral edge thinning and potential sealant peeling or cracking due to glass curvature post-lamination, leading to structural integrity issues.
A solar cell module design with a higher modulus second encapsulant at the peripheral edges and a combination of first and second protection members, along with a UV-resistant, dark-colored second sealing material to resist pressure and absorb heat, preventing edge crushing and enhancing structural integrity.
The design effectively prevents peripheral edge crushing during lamination, reducing sealant peeling and cracking risks, ensuring long-term module reliability.
Smart Images

Figure 0007591930000001 
Figure 0007591930000002
Abstract
Description
[Technical field]
[0001] The present invention relates to a solar cell module formed by sealing a plurality of solar cell strings with two plate-shaped protective members using a resin material. [Background technology]
[0002] A highly reliable solar cell module can be obtained by sandwiching a solar cell string between two flat glass sheets as protective members and sealing them with a resin material. One example is described in Patent Document 1.
[0003] On the other hand, in a solar cell module with this configuration, there is a concern that the peripheral portion of the sealed body in which the solar cell string is sealed with two pieces of glass will be subjected to the pressing pressure in the lamination process (see, for example, FIG. 3 of Patent Document 1) and will be crushed more than the central portion in the plan view, resulting in a thinning. In this state, the two pieces of glass at the peripheral portion are curved so that they approach each other toward the outer edges. Note that when the sealed body is rectangular, this phenomenon is prominent at the four corners. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] JP 2010-177282 A Summary of the Invention [Problem to be solved by the invention]
[0005] In solar cell modules, areas that have become excessively thin due to the above-mentioned reasons are problematic because, after the solar cell module is installed on site, the curved glass will attempt to return to its original shape (flat), which can cause the sealing resin to peel off from the glass or cracks to form in the sealing resin.
[0006] Therefore, an object of the present invention is to provide a solar cell module that can prevent the peripheral portion from being crushed during the lamination process. [Means for solving the problem]
[0007] The present invention is a solar cell module comprising a plurality of solar cell strings composed of a plurality of solar cell cells each having a first and second main surface, a plate-shaped first protective member arranged on the first main surface side of the plurality of solar cell cells, a plate-shaped second protective member arranged on the second main surface side of the plurality of solar cell cells, a first sealing material sealing the plurality of solar cell strings between the first protective member and the second protective member, and a second sealing material arranged outside the first sealing material corresponding to the peripheral portions of the first protective member and the second protective member, wherein the second sealing material has a higher elastic modulus at the heating temperature during lamination construction than the first sealing material.
[0008] Moreover, the second sealing material can have a higher elastic modulus at 80 to 120° C. than the first sealing material.
[0009] According to these configurations, by disposing the second sealing material, which has a higher elastic modulus at the heating temperature during lamination than the first sealing material disposed in the center of the sealing material, on the peripheral portion of the sealing material, the second sealing material can withstand the pressing pressure during lamination.
[0010] Furthermore, a portion of the periphery of the first protective member and the second protective member may be free of the second sealing material.
[0011] In addition, the first protective member and the second protective member may have a rectangular or square shape in a planar view, and the second sealing material may be positioned only on two opposing sides of the peripheral portions of the first protective member and the second protective member in a planar view.
[0012] According to these configurations, the first sealing material is prevented from being completely surrounded by the second sealing material, so that degassing of the first sealing material is less likely to be hindered during lamination.
[0013] The second encapsulant may also include a UV absorber.
[0014] According to this configuration, by using a second sealing material with high UV resistance for the second sealing material placed on the peripheral portion of the sealing body, it is possible to effectively prevent the second sealing material from peeling off from the first protective member and the second protective member at the peripheral portion.
[0015] Moreover, the second sealing material can have a dark color.
[0016] According to this configuration, by using a dark colored second sealing material, the second sealing material absorbs heat when the solar cell generates heat, so that a temperature difference is less likely to occur between the peripheral and central parts of the solar cell module, and cracks are less likely to occur in the sealing body. Effect of the Invention
[0017] In the present invention, the second sealing material can withstand the pressing pressure during lamination, and therefore the peripheral portion can be prevented from being crushed during the lamination process. [Brief description of the drawings]
[0018] [Figure 1] FIG. 2 is an exploded perspective view showing the respective components constituting the sealing body of one embodiment of the present invention. [Diagram 2] FIG. 2 is a vertical cross-sectional view illustrating an internal configuration of the sealing body. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0019] The present invention will be described below with reference to one embodiment in conjunction with the drawings.
[0020] In the solar cell module (not shown) of this embodiment, the frame and electrical wiring are removed, and a lump of material sandwiched between two protective members (glass) is described as a sealing body 1. This sealing body 1 is configured, for example, as shown in Figures 1 and 2, and mainly includes a solar cell string 2, a first protective member 3, a second protective member 4, a first sealing material 5, and a second sealing material 6.
[0021] The solar cell string 2 is configured by electrically connecting a plurality of (two in this embodiment) solar cell cells 21, 21 each having a first and second main surface. The first main surface corresponds to a light receiving surface that is mainly hit by sunlight, and the second main surface corresponds to a back surface. In the sealed body 1 of this embodiment, a plurality of (three in this embodiment) solar cell strings 2 are arranged in an electrically connected state.
[0022] The first protective member 3 is disposed on the first main surface side of the plurality of solar cells 21. The second protective member 4 is disposed on the second main surface side of the plurality of solar cells 21. Each of the protective members 3, 4 in this embodiment is a plate-shaped (flat) tempered glass. The shape of each of the protective members 3, 4 in a plan view is rectangular or square. In this embodiment, it is square. The thickness of each of the protective members 3, 4 can be set, for example, in the range of 1.5 to 3.2 mm. In this embodiment, it is 2.5 mm. The dimension of one side of the first protective member and the second protective member can be set, for example, in the range of 200 to 1500 mm. In this embodiment, it is 300 mm.
[0023] The first sealing material 5 is made of a thermoplastic resin material, and is in a sheet-like state before lamination. The first sealing material 5 seals the solar cell strings 2 between the first protective member 3 and the second protective member 4. The first sealing material 5 is disposed on each of the first and second main surfaces of the solar cell strings 21. Therefore, the solar cell strings 2 are sandwiched between the two sheets of the first sealing material 5. The thickness of the first sealing material 5 is the total thickness of the two sheets in a stacked state, and can be set to, for example, 1 to 3 mm. In this embodiment, it is set to 1.5 mm.
[0024] The second sealing material 6 is made of a thermoplastic resin material and is in a sheet-like state before lamination. The second sealing material 6 is disposed outside (closer to the periphery) of the first sealing material 5 in correspondence with the periphery of the first protective member 3 and the second protective member 4. The thickness of the second sealing material 6 is the total thickness of the two laminated sheets, similar to the first sealing material 5, and can be set to, for example, 1 to 3 mm. In this embodiment, it is set to 1.5 mm.
[0025] The width dimension of the second sealing material 6 is set within a range that allows the thickness to be maintained even when pressure is applied in the thickness direction during the lamination process, and does not impair the effective power generation area for the power generation by the solar cell string 2 (solar cell 21). Specifically, the width can be set to 4 to 20 mm. In this embodiment, the width is set to 7 to 8 mm.
[0026] The second sealing material 6 has a higher elastic modulus at the heating temperature during lamination compared to the first sealing material 5. The second sealing material 6 has a higher elastic modulus at 80 to 120°C compared to the first sealing material 5. The elastic modulus can be evaluated, for example, by the storage elastic modulus specified in JIS K 6394. It can also be evaluated by various elastic moduli such as the shear elastic modulus.
[0027] Regarding the material of each sealing material, in this embodiment, polyolefin elastomer (POE) is used for the first sealing material 5. In addition, for example, ethylene-vinyl acetate copolymer (EVA) or olefin-based thermoplastic elastomer (TPO) can be used for the first sealing material 5. In this embodiment, ionomer is used for the second sealing material 6. In addition, for example, polyolefin elastomer (POE) or olefin-based thermoplastic elastomer (TPO) having a higher elastic modulus than the first sealing material 5 can be used for the second sealing material 6.
[0028] The second sealing material 6 can be provided on the entire peripheral portion of the first protective member 3 and the second protective member 4 (all four sides in the shape of this embodiment). However, a part of the peripheral portion of the first protective member 3 and the second protective member 4 may not have the second sealing material 6. In this embodiment, the second sealing material 6 is disposed only on two sides (upper and lower sides in FIG. 1, left and right sides in FIG. 2) that face each other in a plan view among the peripheral portions of the first protective member 3 and the second protective member 4. Here, since the second sealing material 6 has a higher melting point than the first sealing material 5, there is a possibility that the second sealing material 6 may hinder degassing when the first sealing material 5 is softened. Therefore, by providing the second sealing material 6 in the above positional relationship, the first sealing material 5 can be prevented from being completely surrounded by the second sealing material 6 (i.e., an escape route for gas is provided), and therefore degassing from the softened first sealing material 5 is less likely to be hindered during lamination, and air bubbles are less likely to remain after the first sealing material 5 is hardened. In the case where the second sealing material 6 is provided only on two sides as in this embodiment, and the shape of the sealed body 1 in a plan view is rectangular, it is preferable to provide the second sealing material 6 on the long side. In addition, the second sealing material 6 is not limited to being provided along the entire length of the side, and can also be provided intermittently.
[0029] Here, the formation of the sealing body 1 by lamination is performed, for example, by a method as shown in FIG. 3 of Patent Document 1. Briefly, in a closed space where the air pressure can be reduced (where a vacuum can be drawn), an assembly in which a solar cell string 2, a first protective member 3, a second protective member 4, a first sealing material 5, and a second sealing material 6 are stacked in the thickness direction is placed on the upper surface of a table whose surface generates heat. In this state, a press is applied from above the assembly so that the protective members 3 and 4 located on the upper side are in surface contact with each other. The sealing materials 5 and 6 are softened by heating, and an integrated sealing body 1 is formed by the press pressure in the stacking direction of the assembly. Note that gas is generated from the softened sealing materials 5 and 6, but this is degassed by drawing a vacuum.
[0030] In the sealed body 1 of this embodiment, the second sealing material 6, which has a higher elastic modulus at the heating temperature during lamination than the first sealing material 5 arranged at the center of the sealed body 1, is arranged at the peripheral portion of the sealed body 1, so that the second sealing material 6 can withstand the pressing pressure during lamination. Therefore, even if the peripheral portion of the sealed body 1 in a plan view (both left and right ends in FIG. 2) is subjected to the pressing pressure in the lamination process, it is not crushed and thinned more than the central portion in a plan view (the central portion on the left and right in FIG. 2). Therefore, it is possible to greatly reduce the possibility that the sealing material peels off from the glass or cracks occur in the sealing material after the solar cell module is installed at the site, as in the conventional case.
[0031] Although one embodiment of the present invention has been described above, the present invention is not limited to the above embodiment, and various modifications are possible without departing from the gist of the present invention.
[0032] For example, the second sealing material 6 may contain a UV absorber, which can increase the UV resistance of the second sealing material 6. By using a material with high UV resistance for the second sealing material 6 disposed on the periphery of the sealed body 1, it is possible to effectively prevent the second sealing material 6 from peeling off from the first protective member 3 and the second protective member 4 at the periphery.
[0033] The second sealing material 6 may have a dark color. For example, it may be black. By using a dark color for the second sealing material 6, the second sealing material 6 absorbs heat when the solar cell 21 generates heat, so that a temperature difference is unlikely to occur between the peripheral portion and the center portion of the solar cell module, and therefore cracks are unlikely to occur in the sealing body 1.
[0034] In the above embodiment, two types of sealing materials, the first sealing material 5 and the second sealing material 6, are used as sealing materials, but three or more types may be used. [Explanation of symbols]
[0035] 1 Encapsulation body 2 Solar Strings 21 Solar Cell 3. First protective member 4 Second protective member 5 First sealing material 6 Second sealing material
Claims
1. a plurality of solar cell strings each including a plurality of solar cell cells having first and second main surfaces; a first protective member having a plate shape having a rectangular or square shape in a plan view and disposed on the first main surface side of the plurality of solar cells; a second protective member having a plate shape having a rectangular or square shape in a plan view and arranged on the second main surface side of the plurality of solar cells; a first sealing material sealing the solar cell strings between the first protection member and the second protection member; a second sealing material disposed outside the first sealing material in correspondence with peripheral portions of the first protective member and the second protective member; The second sealing material has a higher elastic modulus at a heating temperature during lamination than the first sealing material, a portion of a peripheral portion of the first protective member and the second protective member does not have the second sealing material; A solar cell module, characterized in that the second sealing material is disposed only on two opposing sides of the peripheral portions of the first protective member and the second protective member in a plan view.
2. 2. The solar cell module according to claim 1, wherein the second sealing material has a higher elastic modulus at 80 to 120° C. than the first sealing material.
3. The solar cell module according to claim 1 , wherein the second encapsulant contains a UV absorber.
4. 4. The solar cell module according to claim 1, wherein the second sealing material has a dark color.
Citation Information
Patent Citations
Method of manufacturing solar cell module
JP2010177282A
Photovoltaic module and method for production thereof
JP2012099818A
Photoelectric conversion module
JP2012199450A
Solar battery module
JP2016119339A
Method for forming a seal, method for manufacturing a sealing unit, sealing unit, and apparatus for forming a seal