Fusion method and electric fusion joint

The method controls resin fusion in electric fusion joints by energizing the stopper heat generating part before the socket part, addressing uneven swelling and gaps, enhancing water quality in semiconductor manufacturing piping.

JP7596095B2Active Publication Date: 2024-12-09SEKISUI CHEMICAL CO LTD
View PDF 20 Cites 0 Cited by

Patent Information

Application Number
JP2020138817
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2020-08-19
Publication Date
2024-12-09
Estimated Expiration
2040-08-19

AI Technical Summary

Technical Problem

Existing electric fusion joints face challenges in controlling resin fusion, leading to uneven swelling and gaps, which can cause turbulent flow and water quality deterioration, particularly in semiconductor manufacturing piping.

Method used

A method involving a cylindrical part with a stopper and socket heat generating parts, where the stopper heat generating part is energized first to fuse the pipe end and stopper, followed by energizing the socket heat generating part to fuse the outer and inner surfaces, controlling the resin flow and preventing uneven swelling.

Benefits of technology

This method suppresses resin gaps and uneven swelling, ensuring uniform resin distribution and reducing pressure loss, suitable for ultrapure water systems used in semiconductor manufacturing.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007596095000001
    Figure 0007596095000001
  • Figure 0007596095000002
    Figure 0007596095000002
  • Figure 0007596095000003
    Figure 0007596095000003
Patent Text Reader

Abstract

To provide an electric fusion joint that can suppress formation of a gap and uneven resin swelling.SOLUTION: A fusion method for fusing an electric fusion joint 1 to resin pipes 11, 12 includes a step S1, a step S3 and a step S4. In the step S1, the resin pipes 11, 12 are inserted into joint sockets 23, 24 of the electric fusion joint 1. In the step S3, energization of a stopper heating unit 4 is started. In the step S4, energization of a socket heating unit 3 is started after the start of energization to the stopper heating unit 4.SELECTED DRAWING: Figure 2
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a fusion method and an electrofusion joint. [Background technology]

[0002] 2. Description of the Related Art Electric fusion joints are often used to connect pipes made of resin, such as resin pipes and metal-reinforced composite pipes having a resin layer and a metal reinforcing layer (see, for example, Patent Document 1).

[0003] For example, the electric fusion joint shown in Patent Document 1 has a joint body made of thermoplastic resin with pipe receptacles formed at both ends into which the pipe to be connected is inserted, and a stopper portion protruding inward from the inner peripheral surface of the joint body. The stopper portion regulates the position of the pipe inserted into the pipe receptacle. A heating element is provided in each of the pipe receptacle and the stopper portion, and by generating heat from the heating elements, the resin around the heating element and the resin of the pipe are fused together, connecting the electric fusion joint and the pipe. [Prior art documents] [Patent documents]

[0004] [Patent Document 1] Japanese Patent Application Publication No. 5-87286 Summary of the Invention [Problem to be solved by the invention]

[0005] However, because fusion is performed at two points, at the stopper portion and the pipe receiving port, it is difficult to control the fusion, and there are cases in which the height of the resin that fused and rose inward between the stopper portion and the end of the pipe was uneven in the circumferential direction, or a gap (crevice) formed between the stopper portion and the end of the pipe.

[0006] When uneven resin mounds or crevices are formed, turbulence occurs, which makes it easier for some water or chemicals to stagnate in the piping. This can lead to the proliferation of microorganisms, causing a deterioration in water quality, or the deterioration of chemicals, which can reduce purity, which can lead to a decrease in product yield in piping used in semiconductor manufacturing, etc.

[0007] An object of the present invention is to provide a fusion method and an electric fusion joint that are capable of suppressing the formation of gaps and uneven resin swelling. [Means for solving the problem]

[0008] In order to achieve the above object, a fusion method according to a first aspect is a fusion method for fusing an electric fusion joint having a cylindrical portion, a stopper portion, a socket heating portion, and a stopper heating portion to a tube, and includes an insertion step, a first current application step, and a second current application step. The cylindrical portion has a joint socket portion into which a tube containing a thermoplastic resin can be inserted. The stopper portion is provided on the inner surface of the cylindrical portion so as to protrude inward, and can regulate the insertion position of the tube end of the tube when the tube is inserted inside the joint socket portion. The socket heating portion includes a heating wire arranged in the joint socket portion. The stopper heating portion includes a heating wire arranged in the stopper portion. The insertion step inserts the tube into the inside of the joint socket portion of the electric fusion joint. The first current application step starts current application to the stopper heating portion. The second current application step starts current application to the socket heating portion after current application to the stopper heating portion starts.

[0009] When electricity is applied to the stopper heating part, the end of the tube and the stopper part are fused, and when electricity is applied to the socket heating part, the outer peripheral surface of the tube and the inner peripheral surface of the fitting socket part are fused. The clearance formed between the tube and the electric fusion joint (including the clearance between the end of the tube and the stopper part and the clearance between the outer peripheral surface of the tube and the inner peripheral surface of the fitting socket part) is non-uniform and wide, so the molten resin flows into places where it is easy to flow. For example, if the molten resin on the outer peripheral surface of the tube and the inner peripheral surface of the fitting socket part flows non-uniformly between the end of the tube and the stopper part, the fused resin between the stopper part and the end of the tube rises inward non-uniformly in the circumferential direction, and in some cases a gap may form without rising.

[0010] In contrast, in the first aspect, the stopper heating part is energized before the socket heating part, so that the resin melted between the inner peripheral surface of the fitting socket part and the outer peripheral surface of the pipe does not flow unevenly between the stopper part and the end of the pipe, and the gap between the stopper part and the end of the pipe can be filled with melted or solidified resin. Therefore, unevenness in the rise of the resin in the circumferential direction can be suppressed. In addition, since the portion where the stopper part and the end of the pipe face each other is a narrow area, the amount of melted resin is small, and the amount of the resin rising inward can be reduced, making it possible to suppress pressure loss. Note that it is preferable that the above-mentioned melted resin is solidified to an extent that the resin can be prevented from flowing in. In addition, since unevenness in the rise can be suppressed, a depression in the resin does not occur, and the end of the pipe can be prevented from contacting the fluid.

[0011] A fusion method according to a second aspect is a fusion method for fusing an electric fusion joint having a tubular portion, a stopper portion, a socket heating portion, and a stopper heating portion to a tube, and includes an insertion step, a first current application step, and a second current application step. The tubular portion is tubular and has a joint socket portion into which a tube containing a thermoplastic resin can be inserted. The stopper portion is provided on the inner surface of the tubular portion so as to protrude inward, and can regulate the insertion position of the tube end of the tube when the tube is inserted inside the joint socket portion. The socket heating portion includes a heating wire arranged in the joint socket portion. The stopper heating portion includes a heating wire arranged in the stopper portion. The insertion step inserts the tube into the inside of the joint socket portion of the electric fusion joint. The first current application step starts current application to the socket heating portion. The second current application step starts current application to the stopper heating portion after current application to the socket heating portion starts.

[0012] For example, if molten resin between the end of the pipe and the stopper portion flows into the clearance between the inner surface of the fitting socket portion and the outer peripheral surface of the pipe, the molten resin between the stopper portion and the end of the pipe will rise unevenly in the circumferential direction, and in some cases a gap may form instead of a rise.

[0013] In contrast, in the second aspect, a wide range of clearance between the inner peripheral surface of the fitting receptacle and the outer peripheral surface of the pipe is filled with molten or solidified resin, so that the molten resin between the stopper portion and the end of the pipe is prevented from flowing into the gap between the inner peripheral surface of the fitting receptacle and the outer peripheral surface of the pipe. This makes it possible to suppress unevenness in the rise of the resin in the circumferential direction. It is also possible to prevent the end of the pipe from coming into contact with the fluid. In addition, since unevenness in the rise can be suppressed, no depressions are formed in the resin, and it is possible to prevent the end of the pipe from coming into contact with the fluid. It is preferable that the above-mentioned molten resin is solidified to an extent that it can prevent the resin from flowing in.

[0014] The electric fusion joint according to the third aspect includes a tubular portion, a stopper portion, a socket heating portion, a stopper heating portion, a pair of first terminals, and a pair of second terminals. The tubular portion is tubular and has a joint socket portion into which a tube containing a thermoplastic resin can be inserted. The stopper portion is provided on the inner surface of the tubular portion so as to protrude inward, and can regulate the insertion position of the tube end of the tube when the tube is inserted into the inside of the joint socket portion. The socket heating portion includes a heating wire disposed in the joint socket portion. The stopper heating portion includes a heating wire disposed in the stopper portion. The pair of first terminals are connected to the heating wire of the socket heating portion to pass current through the socket heating portion. The pair of second terminals are connected to the heating wire of the stopper heating portion to pass current through the stopper heating portion.

[0015] In this way, the heating wire of the stopper heating part and the heating wire of the receptacle heating part are not connected, but have a separate pair of terminals for passing electricity, so the timing of passing electricity to the stopper heating part and the timing of passing electricity to the receptacle heating part can be shifted.

[0016] As a result, fusion by the stopper heating part and fusion by the socket heating part can be controlled separately, and by speeding up either the timing of current flow to the stopper heating part or the timing of current flow to the socket heating part, depending on the material and size of the electric fusion joint and pipe, it is possible to prevent the formation of gaps and uneven resin swelling. Effect of the Invention

[0017] According to the present disclosure, it is possible to provide an electric fusion joint and a fusion method that are capable of suppressing the formation of gaps and uneven resin swelling. [Brief description of the drawings]

[0018] [Figure 1] 1 is an external view showing an electric fusion joint, a resin tube connected to the electric fusion joint, and a resin tube in a first embodiment according to the present disclosure. FIG. [Diagram 2] FIG. 2 is a cross-sectional view showing the electric fusion joint of FIG. 1. [Diagram 3]FIG. 2 is a cross-sectional view showing a state in which a resin tube and a resin tube are inserted into the electric fusion joint of FIG. 1. [Figure 4] 4 is a schematic diagram of an electric fusion joint showing the connection relationship between the socket heating portion and the stopper heating portion of FIG. 3 and the first connector mounting portion and the second connector mounting portion. [Diagram 5] FIG. 4 is a schematic diagram showing a state in which electricity is being applied to an electric fusion joint by an electric fusion device. [Figure 6] FIG. 2 is a flow diagram for explaining a fusion method using the electric fusion joint of FIG. 1. [Figure 7] FIG. 7 is a perspective view showing a pressure jig used in the fusion method of FIG. 6. [Figure 8] 8 is a diagram showing the state in which a resin tube, an electric fusion joint, and a resin tube are attached to the pressurizing jig of FIG. 7. [Figure 9] (a) Schematic diagram showing a state in which the resin is unevenly raised, and (b) Schematic diagram showing a state in which the resin is uniformly raised. [Figure 10] 4 is a cross-sectional view showing a state in which the stopper portion of the electric fusion joint and the pipe end of the plastic pipe are fused together by heat generated by the stopper heating portion. FIG. [Figure 11] FIG. 11 is a flow diagram for explaining a fusion method according to a modified example of an embodiment of the present disclosure. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0019] Hereinafter, an embodiment of the present invention will be described with reference to the drawings.

[0020] <Configuration> (Overview of Electric Fusion Joint 1) Fig. 1 is a diagram showing an electric fusion joint 1 according to an embodiment of the present invention, a resin pipe 11 (an example of a pipe containing a thermoplastic resin) and a resin pipe 12 (an example of a pipe containing a thermoplastic resin) connected by the electric fusion joint 1. Fig. 1 can also be said to be an exploded view of a piping structure 100. The piping structure 100 has, for example, the electric fusion joint 1, the resin pipe 11, and the resin pipe 12.

[0021] As shown in the figure, the electric fusion joint 1 is fused to a resin pipe 11 and a resin pipe 12 to connect the resin pipe 11 and the resin pipe 12 .

[0022] The resin pipe 11 and the resin pipe 12 are each made of a thermoplastic resin.

[0023] Flow paths 11f, 12f having a circular cross section extend inside resin pipe 11 and resin pipe 12. Flow path 1f having a circular cross section extends inside electric fusion joint 1. When resin pipe 11 and resin pipe 12 are connected by electric fusion joint 1, the axes of the flow paths of resin pipe 11, resin pipe 12, and electric fusion joint 1 are aligned on the same straight line.

[0024] The direction in which the axis of each of the flow paths of the electric fusion joint 1, the plastic pipe 11, and the plastic pipe 12 extends is defined as the axial direction A. In the electric fusion joint 1, the plastic pipe 11, and the plastic pipe 12, the direction perpendicular to each axis and moving toward or away from each other is defined as the radial direction B, and the direction rotating around each axis is defined as the circumferential direction C.

[0025] The resin pipe 11 moves in the direction of arrow A1 relative to the electric fusion joint 1 in the axial direction A to be connected to the electric fusion joint 1. Moreover, the resin pipe 12 moves in the direction of arrow A2 relative to the electric fusion joint 1 in the axial direction A to be connected to the electric fusion joint 1. The state in which the resin pipe 11 and the resin pipe 12 are connected to the electric fusion joint 1 constitutes the piping structure 100.

[0026] FIG. 2 is a diagram showing a cross-sectional configuration of the electric fusion joint 1. As shown in FIG.

[0027] As shown in FIGS. 1 and 2, the electric fusion joint 1 has a main body portion 2, a socket heating portion 3, a stopper heating portion 4, a first connector attachment portion 5, and a second connector attachment portion 6.

[0028] (Main body 2) The main body 2 is formed of a thermoplastic resin, and as shown in Fig. 2, has a tubular portion 21 and a stopper portion 22. The tubular portion 21 is cylindrical and has a fitting receptacle portion 23, a fitting receptacle portion 24, and a connecting portion 25. The resin pipe 11 is inserted into the inside of the fitting receptacle portion 23. The resin pipe 12 is inserted into the inside of the fitting receptacle portion 24.

[0029] The thermoplastic resin used in the main body 2 is not particularly limited, but one having a melting point of less than 230° C. is preferable.

[0030] FIG. 3 is a cross-sectional view showing the state in which the resin pipe 11 is inserted into the inside of the joint socket portion 23 of the electric fusion joint 1, and the resin pipe 12 is inserted into the inside of the joint socket portion 24. As shown in FIG.

[0031] The inner diameter of the joint socket portion 23 is formed to be equal to or larger than the outer diameter of the resin pipe 11. The inner diameter of the joint socket portion 24 is formed to be equal to or larger than the outer diameter of the resin pipe 12.

[0032] 2, the connecting portion 25 is connected to the joint socket portion 23 and the joint socket portion 24, and connects the joint socket portion 23 and the joint socket portion 24. The connecting portion 25 is a portion that connects the joint socket portion 23 and the joint socket portion 24, and a stopper portion 22, which will be described later, is provided on the inside in the radial direction B.

[0033] (Stopper portion 22) The stopper portion 22 is an annular portion. The stopper portion 22 is a protrusion formed on the inner surface 21a of the cylindrical portion 21 along the circumferential direction C, and is formed around the entire circumference. The stopper portion 22 also contains a thermoplastic resin, and is preferably formed of the same resin as the thermoplastic resin used for the cylindrical portion 21.

[0034] 2, the stopper portion 22 is formed so as to protrude radially inward from the inner surface 21a of the cylindrical portion 21. The stopper portion 22 is disposed on the inner side of the connecting portion 25 of the cylindrical portion 21 in the radial direction B. The stopper portion 22 may be formed as one member together with the cylindrical portion 21, or may be formed as a separate member from the cylindrical portion 21.

[0035] The stopper portion 22 has a first side surface 22a, a second side surface 22b, and a peripheral surface 22c. The peripheral surface 22c is an end surface of the stopper portion 22 on the inner side in the radial direction.

[0036] The first side surface 22a is formed approximately perpendicular to the axial direction A from the inner surface 21a of the cylindrical portion 21 toward the inside in the radial direction B.

[0037] The second side surface 22b is formed approximately perpendicular to the axial direction A from the inner surface 21a of the cylindrical portion 21 toward the inside in the radial direction B.

[0038] The peripheral surface 22c connects the radially inner end of the first side surface 22a and the radially inner end of the second side surface 22b. The peripheral surface 22c is formed generally parallel to the inner surface 21a of the cylindrical portion 21.

[0039] When the plastic pipe 11 is inserted into the fitting receptacle 23, the stopper portion 22 regulates the insertion position of the pipe end 11a, as shown in Fig. 3. Regulating the insertion position of the pipe end 11a includes a case in which the stopper portion 22 directly regulates the insertion position by the pipe end 11a coming into contact with the first side surface 22a of the stopper portion 22 as shown in Fig. 3, and a case in which the stopper portion 22 indirectly regulates the insertion position by the pipe end 11a coming into contact with a heating wire 41 (described later) of the stopper heat generating portion 4.

[0040] When the plastic pipe 12 is inserted into the fitting receptacle portion 24, the stopper portion 22 regulates the insertion position of the pipe end 12a, as shown in Fig. 3. Regulating the insertion position of the pipe end 12a includes a case in which the stopper portion 22 directly regulates the insertion position by causing the pipe end 12a to come into contact with the second side surface 22b of the stopper portion 22 as shown in Fig. 3, and a case in which the stopper portion 22 indirectly regulates the insertion position by causing the pipe end 12a to come into contact with a heating wire 41 (described later) of the stopper heating portion 4.

[0041] In this embodiment, the occurrence of crevices between the pipe end 11a and the first side surface 22a and between the pipe end 12a and the second side surface 22b (see position P) is suppressed.

[0042] (Inlet heating part 3) Fig. 4 is a schematic diagram of the electric fusion joint 1 showing the connection relationship between the socket heating part 3 and the stopper heating part 4 and the first connector mounting part 5 and the second connector mounting part 6. In Fig. 4, for ease of understanding, the winding configuration of the heating wire 31 in the socket heating part 3 is simplified.

[0043] As shown in Figs. 2 and 4, the socket heating portion 3 is provided in the joint socket portion 23 and the joint socket portion 24.

[0044] The socket heating portion 3 has a heating wire 31 embedded in the inner surface 21 a at the joint socket portion 23 and the joint socket portion 24 .

[0045] The heating wire 31 is arranged so as to be wound circumferentially along the inner surface 21a in the joint socket portion 23 and the joint socket portion 24. The heating wire 31 is arranged in the vicinity of the inner surface 21a. The heating wire 31 may be embedded in the tubular portion 21 so that a portion of the heating wire 31 is exposed on the flow path 1f side, or may be completely embedded.

[0046] For ease of understanding, the portion of the heating wire 31 that is arranged at the joint receptacle portion 23 is referred to as heating wire portion 31a, and the portion of the heating wire 31 that is arranged at the joint receptacle portion 24 is referred to as heating wire portion 31b.

[0047] Of the heating wire 31, the heating wire portion 31c that connects the heating wire portion 31a and the heating wire portion 31b is embedded in the connecting portion 25.

[0048] The heating wire portion 31c is located on the outer circumferential side of the stopper heat generating portion 4. The heating wire portion 31c is arranged so as not to come into contact with the heating wire 41 provided in the stopper heat generating portion 4.

[0049] Although a single heating wire 31 is arranged across the joint receptacle portion 23, the joint receptacle portion 24, and the connecting portion 25, each of the heating wire portion 31a, the heating wire portion 31b, and the heating wire portion 31c may be composed of separate heating wires, and these heating wires may be connected.

[0050] The heating wire 31 may have, for example, a conductor wire and an insulating film. The conductor wire may be, for example, a nichrome wire, an iron-chrome type 2 wire, an iron-chrome type 1 wire, or a nickel-chrome wire. The insulating film is provided so as to cover the conductor wire. The insulating film has a melting point of 230°C or higher. In this embodiment, it is preferable that the insulating film is set to a temperature at which the thermoplastic resin does not melt (for example, in the case of polyethylene, the heating wire is heated to 220°C). The insulating film may be formed of, for example, a fluorine-based resin or an imide-based resin, but it is more preferable to form the insulating film of a polyimide-based resin. For example, the thickness of the conductor wire may be set to 0.1 mm or more and 10 mm or less. The heating wire 31 generates heat at about 180°C to 230°C.

[0051] The following describes the arrangement of the heating wire 31 in the socket heating part 3. Since the socket heating part 3 is provided symmetrically with respect to the stopper part 22, the following description will focus on the heating wire 31 arranged in the joint socket part 23.

[0052] Heating wire portion 31a is arranged so that the heating wire density in joint socket portion 23 is smaller than the heating wire density in stopper heating portion 4, which will be described later.

[0053] In the joint socket portion 23, the heating wire 31 is wound two times so as to contact the joint socket portion 23, and two turns are repeatedly wound so as to contact the joint socket portion 23 with a predetermined interval therebetween along the axial direction A. In this embodiment, the heating wire 31 is wound, for example, eight times as shown in FIG.

[0054] 2, if the length along the axial direction A of the area in which the heating wires 31 are arranged is L, then in this embodiment, eight heating wires 31 are arranged over the length L. Note that length L can also be said to be the length of the socket heating part 3 along the axial direction A, or the length of the heating wires 31 along the axial direction A.

[0055] Here, if the outer diameter of the heating wire 31 is 1 mm and the specified spacing is 5 mm, then there are 8 heating wires in L = 23 mm, and the heating wire density in the socket heating section 3 is 8 (wires) / 23 (mm) ≒ 0.35 (wires / mm).

[0056] In this way, the heating wire density is defined as the number of heating wires per unit length (e.g., 1 mm). The heating wire density can be calculated by dividing the number of heating wires 31 arranged in a length L along the axial direction A of the region in which the heating wires 31 are arranged by that length L.

[0057] In order to generate heat in the receiving port heating portion 3, the clearance W1 (see Figure 3) between the inner surface of the fitting receiving port portion 23 and the outer surface of the plastic pipe 11 and the clearance W1 between the inner surface of the fitting receiving port portion 24 and the outer surface of the plastic pipe 12 are filled with molten resin, and the fitting receiving port portion 23 and the plastic pipe 11, as well as the fitting receiving port portion 242 and the plastic pipe 12 are fused together.

[0058] (First connector mounting portion 5) As shown in Fig. 2, the first connector attachment portion 5 has two pins 51b, 51c (one example of a pair of first terminals). The two pins 51b, 51c are provided so as to protrude radially outward from the outer surface 21d of the cylindrical portion 21. As shown in Fig. 2, one of the two pins 51b, 51c, pin 51b, is disposed near end 21b of the cylindrical portion 21, and the other pin 51c is disposed near end 21c.

[0059] 4, one end of the heating wire 31 of the receptacle heating part 3 on the joint receptacle 23 side is connected to pin 51b. The other end of the heating wire 31 of the receptacle heating part 3 on the joint receptacle 24 side is connected to pin 51c. The receptacle heating part 3 can be made to generate heat by attaching the first connector 81 of the electric fusion apparatus 8 to pins 51b and 51c and passing electricity through them.

[0060] The time for which electricity is applied to the receiving port heating portion 3 may be set to 1 minute when the nominal diameter is 50 mm, and 10 minutes when the nominal diameter is 300 mm, for example.

[0061] (Stopper heating part 4) The stopper heating portion 4 is provided in the stopper portion 22. The stopper heating portion 4 has a heating wire 41. The heating wire 41 is provided in the stopper portion 22 so as to be wound in the circumferential direction C along the axial direction A. In this embodiment, the heating wire 41 is wound around the stopper portion 22, for example, three times. In the stopper heating portion 4 of this embodiment, all adjacent heating wires 41 are in contact with each other.

[0062] The heating wire 41 may be made of the same material and have the same structure as the heating wire 31. The heating wire 41 generates heat at about 180 degrees to 230 degrees.

[0063] In the stopper heating part 4, the heating wire 41 is wound three times so as to be in contact with the wire. Therefore, three heating wires 41 are arranged in the length L (which can also be said to be the length of the stopper heating part 4) along the axial direction A of the region in which the heating wire 41 is arranged.

[0064] The diameter of the wound heating wire 41 in the stopper heating portion 4 is set to be smaller than the diameter of the wound heating wire 31 in the socket heating portion 3.

[0065] Further, the diameter of the wound heating wire 41 in the stopper heating portion 4 is set so that the position of the heating wire 41 falls within the thickness of the pipe walls of the resin pipes 11, 12 into which the heating wire 41 is inserted.

[0066] As described above, if the diameter of the heating wire is 1 mm, the heating wire density in the stopper heat generating portion 4 is set to 3 (wires) / 3 (mm)=1 (wire / mm).

[0067] As described above, the heating line density in receptacle heating portion 3 is approximately 0.35, so in this embodiment the heating line density in receptacle heating portion 3 is set to be smaller than the heating line density in stopper heating portion 4.

[0068] The arrangement of the heating wires 41 in the stopper heat generating portion 4 is not limited to the configuration of this embodiment, and the heating wires 41 do not have to be in contact with each other. Also, the three heating wires 41 do not have to be arranged along the axial direction A, and the middle one may be omitted and that part may be filled with the resin that forms the stopper portion 22.

[0069] The heating wire density in the above-mentioned receiving port heating section 3 is not limited to the configuration shown in Fig. 2, and although in this embodiment the heating wire 31 is wound so that two turns are in contact, this is not limiting. For example, the heating wire 31 may be wound so that three turns are in contact, or the heating wire 31 may be wound with one turn spaced apart so that there is no contact.

[0070] In order to generate heat in the stopper heating portion 4, the clearance W2 (see Figure 3) between the first side surface 22a of the stopper portion 22 and the pipe end 11a of the resin pipe 11 and the clearance W2 between the second side surface 22b of the stopper portion 22 and the pipe end 12a of the resin pipe 12 are filled with molten resin, and the stopper portion 22 and the resin pipe 11, as well as the stopper portion 22 and the resin pipe 12, are fused together.

[0071] (Second connector mounting portion 6) 2, the second connector attachment portion 6 has two pins 61b, 61c (an example of a pair of second terminals). The two pins 61b, 61c are provided so as to protrude radially outward from the outer surface 21d of the cylindrical portion 21. The two pins 61b, 61c are arranged side by side along the axial direction A near the center of the cylindrical portion 21.

[0072] Of the two pins 61b and 61c, one pin 61b is disposed on the end 21b side, and the other pin 61c is disposed on the end 21c side.

[0073] 4, one end of the heating wire 41 is connected to pin 61b, and the other end of the heating wire 41 is connected to pin 61c. By attaching a connector of an electric fusion device to pins 61b and 61c and passing electricity through them, the socket heating part 3 can be made to generate heat.

[0074] The time for which electricity is applied to the stopper heating part 4 is approximately one-fifth of the time for which electricity is applied to the socket heating part 3; for example, it may be set to 20 seconds when the nominal diameter is 50 mm, and 2 minutes when the nominal diameter is 300 mm.

[0075] In this way, because the first connector attachment portion 5 for generating heat in the receptacle heating portion 3 and the second connector attachment portion 6 for generating heat in the stopper heating portion 4 are provided separately, it is possible to stagger the timing of energizing the receptacle heating portion 3 and the timing of energizing the stopper heating portion 4. In other words, energization can be started after energizing the stopper heating portion 4, or energization can be started after energizing the receptacle heating portion 3.

[0076] (Electric fusion device 8) Next, there will be described an electric fusion apparatus 8 that applies electricity to the electric fusion joint 1. Fig. 5 is a schematic diagram showing a state in which electricity is being applied to the electric fusion joint 1 by the electric fusion apparatus 8.

[0077] The electric fusion device 8 has, for example, a pair of first connectors 81 attached to the pins 51b and 51c, and a pair of second connectors 82 attached to the pins 61b and 61c.

[0078] The electric fusion device 8 may be provided with, for example, a first energization switch for energizing the pair of first connectors 81 and a second energization switch for energizing the pair of second connectors 82. In this case, after the second energization switch is operated to start energizing the stopper heating portion 4, the first energization switch can be operated to start energizing the receptacle heating portion 3. Also, after the first energization switch is operated to start energizing the receptacle heating portion 3, the second energization switch may be operated to start energizing the stopper heating portion 4.

[0079] The time from the start of energizing one of the stopper heating part 4 and the socket heating part 3 to the start of energizing the other heating part is preferably after the clearance on the side where one heating part is provided is filled with resin. Note that being filled with resin may mean being filled with molten resin, and is not limited to being filled with solidified resin. In addition, depending on the performance, coil, and nominal diameter of the electric fusion joint 1, energizing the other heating part may start about 10 to 20 seconds after energizing one heating part. In addition, energizing the other heating part may start after the resin on the one heating part side has solidified.

[0080] Alternatively, the electric fusion device 8 may automatically energize the first connector 81 and the second connector 82 based on a preset program. When control is started, energization begins to flow to one of the stopper heating part 4 and the socket heating part 3, and then, after a preset time, energization begins to flow to the other heating part. Then, the electric fusion device 8 stops energizing the heating parts when the preset energization time has elapsed for each heating part.

[0081] In this case, the electrofusion apparatus 8 includes a processor and a storage device. The processor is, for example, a CPU (Central Processing Unit). Alternatively, the processor may be a processor different from the CPU. The processor executes processing for controlling energization according to a program. The storage device includes a non-volatile memory such as a ROM (Read Only Memory) and a volatile memory such as a RAM (Random Access Memory). The storage device may include an auxiliary storage device such as a hard disk or an SSD (Solid State Drive). The storage device is an example of a non-transitory computer-readable recording medium. The storage device stores a program and data for controlling the electrofusion apparatus 8. The storage device stores, for example, data on a terminal range to be described later and a predetermined threshold value of an operation speed.

[0082] <Fusing method> Next, a fusion method according to an embodiment of the present invention will be described with reference to Fig. 6, which is a flow chart for explaining the fusion method according to the present embodiment.

[0083] In this embodiment, a case will be described in which energization to socket heating portion 3 starts after energization to stopper heating portion 4 starts.

[0084] First, in step S1, the plastic pipe 11 is inserted into the joint socket portion 23 of the electric fusion joint 1 until the relative movement of the pipe end 11a of the plastic pipe 11 is restricted by the stopper portion 22.

[0085] Furthermore, the plastic pipe 12 is inserted into the joint socket portion 24 of the electric fusion joint 1 until the relative movement of the pipe end 12a of the plastic pipe 12 is restricted by the stopper portion 22. Figure 3 shows the state in which the plastic pipes 11 and 12 are inserted into the electric fusion joint 1. Step S1 corresponds to an example of an insertion process.

[0086] Next, in step S2, the plastic pipe 11 is pressurized in the direction of the stopper portion 22 (the direction of the arrow A1 shown in FIG. 8) so as to press the pipe end 11a against the first side surface 22a of the stopper portion 22. Also, the plastic pipe 12 is pressurized in the direction of the stopper portion 22 (the direction of the arrow A2 shown in FIG. 8) so as to press the pipe end 12a against the second side surface 22b of the stopper portion 22.

[0087] Here, the pressurizing jig used for pressurization will be described. Fig. 7 is a diagram showing a pressurizing jig 200. Fig. 8 is a diagram showing a state in which the resin pipe 11, the electric fusion joint 1, and the resin pipe 12 are attached to the pressurizing jig 200.

[0088] The pressing jig 200 has a first clamp portion 210, a second clamp portion 220, three guide members 230, and a pressing screw member 240.

[0089] The first clamp portion 210 has a first semi-annular portion 211 , a second semi-annular portion 212 , a hinge portion 213 , a fastening portion 214 , and a position fixing portion 215 .

[0090] The first semi-annular portion 211 and the second semi-annular portion 212 are roughly shaped like halves of a circle and can sandwich the outer periphery of the resin pipe 11. The first semi-annular portion 211 has a guide support portion 211b and a threaded portion 211c in the circumferential direction. A through hole is formed in the guide support portion 211b, and a rod-shaped guide member 230 is inserted therethrough.

[0091] The second semi-annular portion 212 has two guide supports 212b, 212c in the circumferential direction. A through hole is formed in each of the guide support portion 212b and the guide support portion 212c, and a rod-shaped guide member 230 is inserted therethrough.

[0092] The hinge portion 213 rotatably connects the circumferential ends of the first semi-annular portion 211 and the second semi-annular portion 212. The resin pipe 11 is disposed between the first semi-annular portion 211 and the second semi-annular portion 212 with the first semi-annular portion 211 and the second semi-annular portion 212 being opened with the hinge portion 213 at the center.

[0093] The fastening portion 214 is, for example, a screw, and is provided at the circumferential ends of the first semi-annular portion 211 and the second semi-annular portion 212 opposite the hinge portion 213. The circumferential end of the first semi-annular portion 211 opposite the hinge portion 213 protrudes outward, and a through hole is formed in the protruding portion 211a. Moreover, the circumferential end of the second semi-annular portion 212 opposite the hinge portion 213 protrudes outward, and a through hole is formed in the protruding portion 212a.

[0094] When first semi-annular portion 211 and second semi-annular portion 212 are in a closed state, the two through holes face each other, and fastening portion 214, which is a screw, is inserted into them. A screw shape is formed on the inner circumferential surface of the through hole of protruding portion 212a, and a screw shape is not formed in the through hole of protruding portion 211a. Fastening portion 214 is inserted through the through hole of protruding portion 211a and is screwed into the through hole of protruding portion 212a.

[0095] As a result, by rotating the fastening portion 214, the head of the fastening portion 214 presses the protruding portion 211a against the protruding portion 212a, and the plastic pipe 11 can be clamped by the first clamp portion 210. Note that the fastening portion 214 is not limited to a screw, and may be, for example, a bolt and a nut, and the configuration is not limited as long as it can fasten the first semi-annular portion 211 and the second semi-annular portion 212 together.

[0096] The position fixing portion 215 is a screw member, and is provided on the guide support portion 211b. In detail, a screw hole is formed in the guide support portion 211b toward the through hole into which the guide member 230 is inserted, and the position fixing portion 215 is inserted into the screw hole.

[0097] When the position fixing portion 215 is tightened, the tip of the position fixing portion 215 comes into contact with the guide member 230, so that the position of the first clamp portion 210 relative to the guide member 230 is fixed.

[0098] The second clamp portion 220 has a first semi-annular portion 221 , a second semi-annular portion 222 , a hinge portion 223 , and a fastening portion 224 .

[0099] First semi-annular portion 221 has a similar shape to first semi-annular portion 211, and has protrusion 221a, guide support portion 221b, and threaded portion 221c. Unlike guide support portion 211b, guide member 230 is fixed to guide support portion 221b.

[0100] Further, second semi-annular portion 222 has a shape similar to that of second semi-annular portion 212, and has protruding portion 222a, guide support portion 222b, and guide support portion 222c. Unlike guide support portions 212b and 212c, guide member 230 is fixed to guide support portions 222b and 222c.

[0101] Hinge portion 223 is similar to hinge portion 213, and rotatably connects circumferential ends of first semi-annular portion 221 and second semi-annular portion 222. Fastening portion 224 is similar to fastening portion 214, and is provided on protruding portion 221a and protruding portion 222a.

[0102] The guide member 230 is inserted through the guide support portion 211b and fixed to the guide support portion 221b. The guide member 230 is inserted through the guide support portion 212b and fixed to the guide support portion 222b. The guide member 230 is inserted through the guide support portion 212c and fixed to the guide support portion 222c.

[0103] The pressure applying screw member 240 is a ball screw, and is inserted through the screw portions 211c and 221c. The screw portions 211c and 221c are formed with screw holes through which the pressure applying screw member 240 is inserted, and the screw holes are formed in the screw portions 211c and 221c in the opposite direction. In other words, when the pressure applying screw member 240 is rotated, the first clamp portion 210 and the second clamp portion 220 move toward or away from each other along the guide member 230.

[0104] As shown in FIG. 8, the resin pipe 11 is clamped and fixed by the first clamp portion 210, and the resin pipe 12 is clamped and fixed by the second clamp portion 220, and then the pressure screw member 240 is rotated to bring the first clamp portion 210 and the second clamp portion 220 closer to each other (see arrows A1 and A2).

[0105] This allows the resin pipe 11 and the resin pipe 12 to be pressurized so that the pipe end 11a of the resin pipe 11 is pressed against the first side surface 22a of the stopper portion 22, and the pipe end 12a of the resin pipe 12 is pressed against the second side surface 22b of the stopper portion 22.

[0106] Furthermore, by tightening the position fixing portion 215 in a pressurized state, the pressurized state by the first clamp portion 210 and the second clamp portion 220 can be maintained.

[0107] Next, in step S3, in a pressurized state, the second connector 82 of the electric fusion device 8 is attached to the two pins 61b, 61c of the second connector attachment portion 6, and electricity is started. The pressurizing screw member 240 may be rotated while electricity is being applied to push the resin tube 11 and the resin tube 12 into the electric fusion joint 1. The temperature of the heating wire during electricity application may be any temperature that can melt the main body portion 2, and in the case of polyolefin, 220 degrees or less is preferable. This electricity application causes the heating wire 41 to heat up. Step S3 corresponds to an example of a first electricity application step.

[0108] Next, in step S4, in a pressurized state, the first connector 81 of the electric fusion apparatus 8 is attached to the two pins 51b, 51c of the first connector attachment portion 5, and electricity is passed for a predetermined time. The time from the start of step S3 to the start of step S4 depends on the performance of the electric fusion joint 1, the coil of the heating wire, and the nominal diameter of the pipe, as described above, but is preferably about 10 to 20 seconds. Step S4 corresponds to an example of a second electricity passing step.

[0109] Next, after a predetermined time has elapsed since step S3, in step S5, the supply of electricity to the two pins 61b and 61c by the electric fusion device 8 is stopped.

[0110] Then, after a predetermined time has elapsed since step S4, in step S6, the supply of electricity to the two pins 51b and 51c by the electric fusion device 8 is stopped.

[0111] <Features> The fusion method in this embodiment is a fusion method for fusing an electric fusion joint 1 having a cylindrical portion 21, a stopper portion 22, a socket heating portion 3, and a stopper heating portion 4 to plastic pipes 11, 12 (an example of a pipe), and includes step S1 (an example of an insertion step), step S3 (an example of a first current application step), and step S4 (an example of a second current application step). The cylindrical portion 21 has joint socket portions 23, 24 into which the plastic pipes 11, 12 containing thermoplastic resin can be inserted. The stopper portion 22 is provided on the inner surface of the cylindrical portion 21 so as to protrude inward, and can regulate the insertion positions of the pipe ends 11a, 12a of the plastic pipes 11, 12 when the plastic pipes 11, 12 are inserted into the inside of the joint socket portions 23, 24. The socket heating portion 3 includes a heating wire 31 arranged in the joint socket portions 23, 24. The stopper heating part 4 includes a heating wire 41 disposed in the stopper part 22. In step S1, the resin tubes 11, 12 are inserted into the inside of the joint socket parts 23, 24 of the electric fusion joint 1. In step S3, current is started to be passed through the stopper heating part 4. In step S4, current is started to be passed through the socket heating part 3 after current is started to be passed through the stopper heating part 4.

[0112] Passing current through the stopper heating section 4 fuses the pipe ends 11a, 12a of the plastic pipes 11, 12 with the stopper section 22, and passing current through the socket heating section 3 fuses the outer circumferential surfaces of the plastic pipes 11, 12 with the inner circumferential surfaces of the fitting socket sections 23, 24. The clearances formed between the plastic pipes 11, 12 and the electric fusion joint 1 (including the clearance W2 between the pipe ends 11a, 12a of the plastic pipes 11, 12 and the stopper section 22, and the clearance W1 between the outer circumferential surfaces of the plastic pipes 11, 12 and the inner circumferential surfaces of the fitting socket sections 23, 24) are nonuniform and wide, so that the molten resin flows into places where it is easy to flow. For example, if the molten resin flows non-uniformly into the space between the pipe ends 11a, 12a of the plastic pipes 11, 12 and the stopper portion 22, the molten resin will rise non-uniformly in the circumferential direction between the stopper portion 22 and the pipe ends 11a, 12a of the plastic pipes 11, 12, and in some cases a gap (which may also be called a depression) may form instead of the rise. Figure 9(a) shows a state in which the resin rise R is non-uniform in the circumferential direction C. In Figure 9(a), the resin rising inward from the stopper portion 22 and the inner circumferential surface of the plastic pipe 11 is indicated by R, and the depression is indicated by Q.

[0113] On the other hand, in this embodiment, by energizing the stopper heating part 4 before the socket heating part 3, the space between the stopper part 22 and the tube ends 11a, 12a of the resin tubes 11, 12 can be filled with molten or solidified resin so that the resin melted between the inner circumferential surface of the joint socket part 23, 24 and the outer circumferential surface of the resin tubes 11, 12 does not flow unevenly between the stopper part 22 and the tube ends 11a, 12a of the resin tubes 11, 12. Therefore, unevenness in the swelling of the resin in the circumferential direction can be suppressed. Note that the above-mentioned molten resin is preferably solidified to such an extent that the resin can be prevented from flowing in. FIG. 9(b) shows a state in which the swelling R of the resin is uniform in the circumferential direction C. FIG. 10 is a cross-sectional view showing a state in which the stopper part 22 of the electric fusion joint 1 and the tube ends 11a, 12a of the resin tubes 11, 12 are fused by the heat generated by the stopper heating part 4. In order to make the fusion of the stopper portion 22 easier to understand, FIG. 10 does not show the fusion between the electric fusion joint 1 and the plastic pipes 11, 12 caused by the heat generated by the socket heating portion 3.

[0114] As in this embodiment, by making the resin rise all around in the circumferential direction C, it is possible to suppress depressions and prevent the occurrence of dead water, and therefore it is suitable for use in fields related to ultrapure water. In particular, it is suitable for the field of ultrapure water used for semiconductor cleaning water. Furthermore, since no depressions are formed in the resin, it is possible to prevent the ends of the resin pipes 11, 12 from coming into contact with the fluid. Furthermore, by making the rise uniform, it is possible to suppress partial removal of the resin and the occurrence of current change. Furthermore, as shown in FIG. 10, the butting portions between the stopper portion 22 and the pipe ends 11a, 12a of the resin pipes 11, 12 are covered with resin when viewed in a cross section along the axial direction A (see the resin mound R in the figure) due to the fusion, so that water does not stagnate.

[0115] In addition, since the opposing portions of the stopper portion 22 and the pipe ends 11a, 12a of the resin pipes 11, 12 are narrow in area, the amount of resin that melts is small and the amount of resin that bulges inward can be reduced, making it possible to suppress pressure loss.

[0116] The electric fusion joint 1 of this embodiment includes a cylindrical portion 21, a stopper portion 22, a socket heating portion 3, a stopper heating portion 4, a pair of pins 51b, 51c, and a pair of pins 61b, 61c. The cylindrical portion 21 is cylindrical and has joint socket portions 23, 24 into which the resin pipes 11, 12 containing thermoplastic resin can be inserted. The stopper portion 22 is provided on the inner surface 21a of the cylindrical portion 21 so as to protrude inward, and can regulate the insertion positions of the pipe ends 11a, 12a of the resin pipes 11, 12 when the resin pipes 11, 12 are inserted into the joint socket portions 23, 24. The socket heating portion 3 includes a heating wire 31 arranged in the joint socket portions 23, 24. The stopper heating portion 4 includes a heating wire 41 arranged in the stopper portion 22. The pair of pins 51b, 51c are connected to the heating wire 31 of the receptacle heating part 3 to supply electricity to the receptacle heating part 3. The pair of pins 61b, 61c are connected to the heating wire 41 of the stopper heating part 4 to supply electricity to the stopper heating part 4.

[0117] In this way, the heating wire 41 of the stopper heating portion 4 and the heating wire 31 of the receptacle heating portion 3 are not connected, but have separate pairs of terminals for passing electricity, namely pins 51b, 51c and pins 61b, 61c, so that the timing of passing electricity to the stopper heating portion 4 and the timing of passing electricity to the receptacle heating portion 3 can be shifted.

[0118] As a result, fusion by the stopper heating part 4 and fusion by the receiving port heating part 3 can be controlled separately, and by speeding up either the timing of energizing the stopper heating part 4 or the timing of energizing the receiving port heating part 3 depending on the material and size of the electric fusion joint 1 and the pipe, it is possible to suppress the formation of gaps and uneven swelling of the resin.

[0119] <Other embodiments> Although one embodiment of the present invention has been described above, the present invention is not limited to the above embodiment, and various modifications are possible without departing from the gist of the invention.

[0120] (A) In the above embodiment, energization of the receptacle heating part 3 is started after energization of the stopper heating part 4 is started, but the opposite is also possible. In other words, energization of the receptacle heating part 3 may be started before energization of the stopper heating part 4.

[0121] The fusion method in this case is shown in the flow diagram of Figure 11. As shown in Figure 11, following step S2, in step S30, current begins to flow to the receptacle heating part 3. Thereafter, current begins to flow to the stopper heating part 4. Also, although it depends on the current flow time for each of the receptacle heating part 3 and the stopper heating part 4, if the interval between steps S30 and S40 is 10 to 20 seconds as described above, current flow to the stopper heating part 4 is stopped in step S50, which is the step after step S40. Then, finally, current flow to the receptacle heating part 3 is stopped in step S60.

[0122] For example, when molten resin between the pipe ends 11a, 12a of the plastic pipes 11, 12 and the stopper portion 22 flows into the clearance between the inner surface of the fitting receiving portion 23, 24 and the outer peripheral surface of the plastic pipes 11, 12, the molten resin between the stopper portion 22 and the pipe ends 11a, 12a of the plastic pipes 11, 12 will rise unevenly in the circumferential direction, and in some cases a gap may be formed instead of a rise.

[0123] In contrast, as described above, after starting the current supply to the socket heating part 3 in step S30 (an example of a first current supply step), starting the current supply to the stopper heating part 4 in step S40 (an example of a second current supply step) fills a wide range of clearances between the inner peripheral surfaces of the fitting socket parts 23, 24 and the outer peripheral surfaces of the plastic pipes 11, 12 with molten or solidified resin, so that the molten resin between the stopper part 22 and the pipe ends 11a, 12a of the plastic pipes 11, 12 does not flow into between the inner peripheral surfaces of the fitting socket parts 23, 24 and the outer peripheral surfaces of the plastic pipes 11, 12. Therefore, unevenness in the rise of the resin in the circumferential direction can be suppressed. In addition, since unevenness in the rise can be suppressed, no depressions are generated in the resin, and the ends of the pipes do not come into contact with the fluid.

[0124] (B) In the above embodiment, when viewed along the axial direction A, the outer diameter of the stopper portion 22 is circular, but this is not limited to a circle and may be polygonal.

[0125] (C) In the above embodiment, the socket heating parts 3 are provided symmetrically on both sides of the stopper part 22, but this is not limited thereto. For example, the heating wire 31 may be provided so as to make three turns of contact at one joint socket part 23 across the stopper part 22, and the heating wire 31 may be provided so as to make two turns of contact at the other joint socket part 24.

[0126] (D) In the above embodiment, all of the flow paths of the electric fusion joint 1 are formed straight, but the flow paths may be curved, that is, an elbow joint.

[0127] (E) In the above embodiment, the same electric heating wire 31 of the socket heating part 3 and the electric heating wire 41 of the stopper heating part 4 are used, so all of the electric heating wires 31, 41 are provided with an insulating coating, but this is not limited to the above. However, it is preferable that at least the electric heating wire 41 is provided with an insulating coating. This is because the electric heating wires 41 may be pressurized by the resin pipes 11 and 12, and may easily come into contact with each other.

[0128] (F) In the above embodiment, the pipe end 11a of the resin pipe 11 and the pipe end 12a of the resin pipe 12 are pressed against the stopper portion 22, but they do not have to be pressed. However, pressing them is preferable in order to prevent the occurrence of crevices, and it also makes it possible to shorten the construction time.

[0129] (G) In the above embodiment, the same number of turns (two turns) are in contact at the receiving port heating portion 3, but this is not limited to this. For example, the number of turns may be different, such as two turns of contact followed by three turns with a predetermined gap between them.

[0130] (H) In the above embodiment, the resin pipes 11 and 12 are used, but the present invention is not limited to this, and may be a pipe using resin, such as a metal-reinforced composite pipe having a metal reinforcing layer. [Industrial Applicability]

[0131] The electric fusion joint of the present invention has the effect of being able to suppress the formation of gaps and uneven resin swelling, and is useful, for example, as a piping structure for ultrapure water. [Explanation of symbols]

[0132] 1: Electric fusion joint 3: Heat generating part 4: Stopper heating part 11: Plastic pipe 12: Plastic pipe

Claims

1. a tubular portion having a fitting socket into which a tube containing a thermoplastic resin can be inserted; a stopper portion provided on an inner surface of the cylindrical portion so as to protrude inward, the stopper portion being capable of regulating an insertion position of a pipe end of the pipe when the pipe is inserted into the fitting socket portion; a socket heating portion including a heating wire disposed in the joint socket portion; a stopper heating portion including an electric heating wire disposed in the stopper portion; and a fusion method for fusion of the tube, comprising: an insertion step of inserting the tube into the inside of the joint socket portion of the electric fusion joint; a first current application step of starting current application to the stopper heat generating portion; and a second current application process in which current is applied to the receiving port heating portion after a clearance between the stopper portion and the tube is filled with thermoplastic resin after current application to the stopper heating portion is started and before the first current application process is completed. Fusion method.

2. a tubular portion having a fitting socket into which a tube containing a thermoplastic resin can be inserted; a stopper portion provided on an inner surface of the cylindrical portion so as to protrude inward, the stopper portion being capable of regulating an insertion position of a pipe end of the pipe when the pipe is inserted into the fitting socket portion; a socket heating portion including a heating wire disposed in the joint socket portion; a stopper heating portion including an electric heating wire disposed in the stopper portion; and a fusion method for fusion of the tube, comprising: an insertion step of inserting the tube into the inside of the joint socket portion of the electric fusion joint; a first current application step of starting current application to the receiving port heating portion; and a second current application process in which, after current application to the receiving port heating part is started, current application to the stopper heating part is started after a clearance between the receiving port heating part and the pipe is filled with thermoplastic resin and before the first current application process is completed. Fusion method.

3. a pressurizing step of pressing the tube in the direction of the stopper portion so as to press the tube end against the stopper portion, the first current application step is performed in a state in which the stopper portion is pressurized by the tube, The second current application step is performed in a state in which the stopper portion is pressed by the tube. The fusion method according to claim 1 or 2.

Citation Information

Patent Citations

  • Steel wire mesh framework reinforced polyethylene composite structure plastic electric melting pipeline

    CN211550872U

  • plastic pipe fittings

    JP1993019789U

  • Electric fusion joint

    JP1993087286A

  • Manufacture of electric fusion joint

    JP1993157190A

  • Connecting method for thermoplastic resin tube to electric fusion-bonding joint

    JP1993318596A