Precast asphalt pavement

Precast asphalt slabs using metal frames and steel paper with thermoplastic resin, combined with steel fibers, address the challenges of temperature-induced deformation and adhesive requirements, enabling efficient and low-emission construction.

JP7596143B2Active Publication Date: 2024-12-09OBAYASHI ROAD CORPORATION
View PDF 11 Cites 0 Cited by

Patent Information

Application Number
JP2020218435
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2020-12-28
Publication Date
2024-12-09
Estimated Expiration
2040-12-28

AI Technical Summary

Technical Problem

The construction of asphalt pavement is challenging due to its thermoplastic nature, which softens and deforms with temperature changes, and requires adhesives for bonding precast plates, leading to inefficiencies and environmental impacts.

Method used

The use of metal frames or steel paper coated with thermoplastic resin, combined with steel fibers in the asphalt mixture, allows for precast asphalt slabs that can be stacked and joined using electrical resistance or induction heating to bond the slabs, reducing deformation and emissions.

Benefits of technology

This method enables efficient transportation and installation with reduced noise and vibration, facilitates easy joining and peeling of slabs, and significantly reduces greenhouse gas emissions by using electric power for construction processes.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007596143000001
    Figure 0007596143000001
  • Figure 0007596143000002
    Figure 0007596143000002
  • Figure 0007596143000003
    Figure 0007596143000003
Patent Text Reader

Abstract

To provide a precast asphalt pavement slab that overcomes a technical problem of asphalt pavement which is difficult to precast.SOLUTION: A precast asphalt pavement slab PA is provided with a left-in-place formwork 1 made of a rectangular parallelepiped thin metal plate or a wire net with an upper surface opened, a thermoplastic-resin layer 3 placed on the outer surface of the left-in-place formwork 1, and an asphalt mixture 2 loaded in the left-in-place formwork 1.SELECTED DRAWING: Figure 2
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a precast asphalt pavement slab. [Background technology]

[0002] A typical asphalt pavement is constructed by spreading a hot asphalt mixture or a cold asphalt mixture on-site evenly using an asphalt finisher or the like, and then compacting it with a roller or the like.

[0003] Generally, larger machines are used for asphalt paving as the scale of the paving increases, and it is known that the quality of the paving is directly affected by the skill of the operators and manual finishing workers, as well as the weather conditions during construction.

[0004] The basic construction methods for conventional asphalt pavement have not changed significantly since the early days of pavement after the war, and even today there are issues with noise, vibration, greenhouse gas emissions, restrictions due to weather conditions, and waste of materials after use.

[0005] On the other hand, precasting asphalt pavement to solve these problems is considered difficult compared to concrete pavement due to the following reasons: In the field of precast pavement slabs, there are proposals for precast concrete pavement slabs, as exemplified in the following patent documents, but no proposals for precast asphalt pavement slabs have been found.

[0006] In other words, thermoplastic asphalt pavement softens and deforms due to rising temperatures and solar radiation even in natural environments; even if the pavement is precast, adhesives are required to join the precast slabs top to bottom, left to right, and front to back, which significantly reduces construction efficiency; and even if precast, the paving efficiency is low and special construction machinery is required. For these reasons, it is considered difficult to precast asphalt pavement. [Prior art documents] [Patent documents]

[0007] [Patent Document 1] Patent No. 6572419 [Patent Document 2] Patent No. 5835788 [Patent Document 3] Utility Model Registration No. 3150582 Summary of the Invention [Problem to be solved by the invention]

[0008] An object of the present invention is to provide a precast asphalt pavement slab that can overcome the technical problem that asphalt pavement is difficult to precast. [Means for solving the problem]

[0009] In the present invention, which has been made with the aim of solving the above problems, an asphalt pavement slab is precast by the following method.

[0010] Metal frame method A five-sided rectangular solid formwork (hereinafter simply referred to as formwork) except for the top surface is made of a metal plate or wire mesh with a thickness of 5 mm or less, such as thin iron sheet, or galvanized iron or tinplate, which is a conductor that has high electrical resistance and is relatively inexpensive, and has minimal rust prevention measures in place.Asphalt mixture is poured into the formwork to create a precast asphalt pavement slab (hereinafter referred to as precast pavement slab).The sides of the formwork are made about 10 mm lower than the finished precast pavement slab, and the outer surface is coated with thermoplastic resin.

[0011] Steel Paper Method During factory production, steel paper coated with thermoplastic resin on both sides is laid on the bottom of the molded formwork with four sides about 10 mm shorter than the side wall height, and composite material is filled into it to make a rectangular precast pavement slab, after which the excess is folded up and wrapped around the side walls. There is also a method in which the excess is not removed for this precast pavement slab, and steel paper coated with thermoplastic resin on both sides is placed on only the bottom wall.

[0012] How to incorporate steel fibers into asphalt mixtures Steel fibers are mixed into the asphalt mixture and then formed into a skeleton to form a precast pavement slab, in which thermoplastic resin or asphalt emulsion is placed on the side walls and bottom walls to bond the precast pavement slabs together. Effect of the Invention

[0013] The precast pavement slab of the present invention can be stored and transported in layers because deformation due to temperature changes is suppressed by the use of metal or steel-paper forms.

[0014] Because it is a precast pavement slab, it can be laid using electric forklifts and Unic cranes, so construction noise and vibration are minimal.

[0015] Precast pavement slabs are joined together by either directly connecting them to the metal formwork, or by using induction heating, which uses the electrical resistance of the metal formwork to generate heat and fuse the slabs together with the thermoplastic resin on the outer surface.

[0016] Conversely, precast pavement slabs can also be easily removed by applying the same heat generation principle as described above.

[0017] Most of the power used for work on paving sites can be generated electrically, which helps reduce greenhouse gas emissions. [Brief description of the drawings]

[0018] [Figure 1] FIG. 2 is a plan view of an example of a precast pavement slab of the present invention. [Diagram 2] Cross-sectional view of the precast pavement slab along the line AA in Figure 1. [Diagram 3] FIG. 4 is a cross-sectional view of another example of the precast pavement slab of the present invention. [Figure 4] FIG. 4 is a cross-sectional view of the left half of another example of the precast pavement slab of the present invention. [Diagram 5] 1 is a cross-sectional view showing a schematic diagram of a method for constructing the precast pavement slab of the present invention on an earthwork section (subgrade, roadbed). [Figure 6] FIG. 2 is a cross-sectional view showing a schematic example of a method for constructing the precast pavement slab of the present invention on a concrete slab. [Figure 7] FIG. 7 is a cross-sectional view showing a schematic example of another current supply mode in the construction shown in FIG. 6. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0019] Next, an embodiment of the present invention will be described with reference to the drawings. Figures 1 and 2 show an example of the precast pavement slab PA of the present invention. As shown in Figures 1 and 2, a rectangular solid filled-in formwork 1 (hereinafter simply referred to as formwork) with five sides excluding the top surface is formed from a thin steel plate, or a metal plate with a thickness of about 5 mm or less that has been treated for rust prevention such as galvanized iron or tinplate, or a wire mesh. Next, this formwork 1 is set in a molding formwork 1M, and heated asphalt mixture 2 (hereinafter also simply referred to as "mixture 2") is loaded into the formwork 1M to produce the precast asphalt pavement slab PA of the present invention (hereinafter simply referred to as precast slab PA).

[0020] In addition, in order to make the height h1 of the side surface 1a of the formwork 1 about 10 mm lower than the height h2 of the finished precast panel PA, a collar 1c is placed at the opening of the forming formwork 1M for forming. A thermoplastic resin is formed on the outer surface of the formwork 1 as a thermoplastic synthetic resin layer 3 by coating or the like. The thermoplastic synthetic resin layer 3 may be formed either before or after the molding of the precast panel PA, and the resin layer 3 may also be formed by attaching or wrapping a resin sheet other than coating. In the figure, 1b is the bottom plate of the forming formwork 1M.

[0021] As an example, Fig. 3 shows a rectangular precast slab PA in which steel paper 4 with asphalt emulsion 5 applied to the underside is laid on a backing plate 1B placed on the bottom slab 1b of a forming formwork 1M, and a composite material 2 is loaded into the forming formwork 1M to make the precast slab PA. Only the bottom surface of the precast slab PA is covered with a metal film (steel paper 4). In Fig. 2, a collar 1c with the same height as the total height 2h of the formwork side wall is used.

[0022] FIG. 4 is a cross-sectional view of a main part for explaining a precast panel PA of the present invention in which steel fibers 6 are mixed into an asphalt mixture 2 to form a skeleton of the steel fibers 6. As shown in FIG.

[0023] Next, the case of laying or dismantling (peeling off) the precast slab PA of the present invention explained with reference to Figs. 1 to 4 will be explained with reference to Figs. 5 and 6.

[0024] FIG. 5 is a cross-sectional view showing a schematic state in which asphalt pavement is laid on a roadbed or subgrade G of an earthwork portion using any of the precast panels PA of the present invention shown in FIGS.

[0025] In Figure 5, the precast panels of the present invention PA are arranged face down (with the mix material 2 exposed on the bottom) on the roadbed or subgrade G to form a lower panel L-PA, and the same precast panels of the present invention PA are arranged on top of this lower panel L-PA with the mix material 2 facing upwards to form an upper panel U-PA.

[0026] In Fig. 5, when each precast panel PA stacked on the lower panel L-PA and the upper panel U-PA is electrically joined by its respective metal formwork 1, if both ends of the upper panel U-PA are connected to an AC 200V power source EP shown in Fig. 5 via an electrical cord EC and electricity is applied, each formwork 1 will generate heat through electrical current. The formwork 1 can be heated by connecting an electrical cord EC to each of the formwork 1 of each layer panel U-PA and L-PA, and each formwork 1 can generate heat separately. Passing electricity through each formwork 1 is useful in cases where the formworks 1 are not electrically joined together.

[0027] When each formwork 1 generates heat, the thermoplastic resin 3 applied to the outer surface of each formwork 1 melts, and the outer surfaces of each formwork 1 that are in contact are welded and joined by the molten resin, so that the lower layer L-PA and upper layer U-PA are integrated to form an asphalt pavement made of precast plate PA.

[0028] The formwork 1 of the stacked lower plate L-PA and upper plate U-PA can also be heated by placing an induction coil IH, shown by phantom lines in Figure 5, above the upper plate U-PA and passing alternating current from the power source EP to pass current through the form 1 by electromagnetic induction, thereby generating heat.

[0029] In FIG. 6, the precast plate PA of the present invention is placed on the concrete floor GC as a surface pavement plate (upper plate U-PA), and the formwork 1 is heated by electrical heating from an AC200V power source EP or induction heating from an induction coil IH as in the case of FIG. 5, thereby melting the thermoplastic resin on the outer surface of the formwork, welding and joining the precast plates PA together, and bonding the bottom surface of the precast plate PA to the concrete floor GC, thereby constructing a precast asphalt pavement using the precast plate PA of the present invention. FIG. 7 is a schematic diagram showing an example of applying electrical heating to each formwork 1 as shown in FIG. 6. The above explanation can be applied to a precast plate PA formed by laying steel paper 4 in a forming formwork 1M (not shown) and raising the four periphery of the steel paper 4 along the side walls of the forming formwork 1M to form the formwork 1, filling the formwork-shaped steel paper 4 with a mixture material 2. Some precast plates PA have asphalt emulsion placed on the bottom and side walls. The formwork-shaped steel paper 4 is integrated into the precast plate PA in a manner that encases the composite material 2 to be loaded.

[0030] The explanation in paragraphs 0025 to 0029 above was an example of the construction form of an asphalt pavement using the precast plate PA of the present invention, but the above-mentioned heating mode of the present invention can be applied to melt the thermoplastic resin 3 or asphalt emulsion (not shown) that welds and bonds the formwork 1 between each precast plate PA when peeling off the precast plate PA that has been used in the asphalt pavement using the precast plate PA of the present invention.

[0031] In the present invention, the formwork 1 used when placing the precast plate PA of the present invention on the concrete slab GC and paving it with asphalt is a rectangular parallelepiped made of thin steel plate or wire mesh with an open top, and in order to ensure that the bottom of the precast plate PA can be tightly bonded to the concrete slab GC, steel paper 4 coated with asphalt emulsion is placed on the bottom of the formwork 1. This allows for a stronger bond with the concrete slab GC.

[0032] In the present invention, the precast panel PA of the present invention, in which steel fibers 6 are mixed with the asphalt mixture 2 loaded into the formwork 1, generates heat in the asphalt mixture 2 when heated by induction coil IH, softening the mixture 2, so that when paving, the stacked precast panels PA are joined together without any gaps, and when peeling them off, the mixture 2 of the stacked precast panels PA is softened, making them easy to peel off.

[0033] The present invention is as described above. Since deformation of the precast panel PA of the present invention due to temperature changes is suppressed by the formwork 1 and the synthetic resin layer 3 formed on the formwork 1 by coating or the like, it becomes possible to store and transport the panel.

[0034] In addition, precast PA panels can be transported to the paving site using an electric forklift and then installed, so construction noise is minimal.

[0035] Furthermore, the precast panels PA are joined together by either connecting an electric cord EC directly to the formwork 1 and heating it through electrical current, or by dielectric heating using an induction coil IH to weld the thermoplastic resin layer 3 on the outer surface of the formwork 1, so the joining method is simple and easy, and this heating method can also be applied to peeling off the precast panels PA, making it quite rational.

[0036] As described above, in asphalt pavement using the precast panels of the present invention, most of the power required for both paving and removal can be provided by electricity, making it possible to reduce greenhouse gas emissions associated with paving work. [Explanation of symbols]

[0037] PA Precast asphalt pavement slab (precast slab) 1M Formwork 1. Buried formwork (formwork 1) 2. Asphalt mixture (mixture 2) 3 Thermoplastic resin coating 4. Steel Paper 5. Asphalt emulsion 6 Steel Fiber EP AC power supply EC Power Cord IH Induction Coil

Claims

1. This precast asphalt pavement slab is formed by comprising a rectangular parallelepiped embedded formwork made of thin metal plate or wire mesh with an open top, a thermoplastic resin layer placed on the outer surface of the embedded formwork, and an asphalt mixture loaded into the embedded formwork.

2. A precast asphalt pavement slab is formed comprising: formwork-shaped steel paper that is set in a formwork shape within a molding form so as to encase the asphalt mixture to be loaded; a thermoplastic resin layer or an asphalt emulsion layer disposed on the outer surface of the formwork-shaped steel paper; and an asphalt mixture loaded into the formwork-shaped steel paper.

3. 3. A precast asphalt pavement slab according to claim 1 or 2, wherein steel fibers are mixed into the asphalt mixture.

4. A method for manufacturing a precast asphalt pavement slab, comprising: setting formwork-shaped steel paper within a molding formwork so that it fits snugly within the molding formwork; and loading heated asphalt mixture into the molding formwork with the formwork-shaped steel paper set, thereby forming a precast asphalt pavement slab equipped with the formwork-shaped steel paper.

5. 5. The method for manufacturing a precast asphalt pavement slab according to claim 4, wherein a layer of thermoplastic synthetic resin is previously placed on the outer surface of said formwork-shaped steel paper.

6. An asphalt paving method in which, when a precast asphalt paving slab according to any one of claims 1 to 3 is laid on a roadbed, subgrade, or concrete slab to perform asphalt paving, the precast asphalt paving slab is heated by passing electricity through it or by an induction coil to bond the laid precast asphalt paving slabs together and to bond the precast asphalt paving slab to the roadbed, subgrade, or concrete slab.

Citation Information

Patent Citations

  • Takoseiheiban

    JP1976074441A

  • JP1976141928U

  • Magnetic bubble storage device

    JP1983035788A

  • Prefabricated pavement construction method applying high frequency

    JP1985208501A

  • Deformation of lumpy body

    JP1986165404A