Magnetic tunneling junction device, memory device including the smae, and method of manufacturing the same
By using an oxygen-deficient oxide layer and metal-doped magnetic layer to trap oxygen/nitrogen, the device addresses RA and speed issues, resulting in improved operating speed and stability of magnetic tunnel junctions.
Patent Information
- Application Number
- KR1020210028968
- Authority / Receiving Office
- KR · KR
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2021-03-04
- Publication Date
- 2026-11-06
- Estimated Expiration
- 2041-03-04
AI Technical Summary
Existing magnetic tunnel junction devices face challenges in maintaining resistance area product (RA) and operating speed due to oxygen or nitrogen trapping in the magnetic layer during the manufacturing process, which affects the switching efficiency of the free layer.
The magnetic tunnel junction device incorporates a first oxide layer with a stoichiometrically oxygen-deficient composition and a second magnetic layer doped with metal elements, along with a metal layer to trap oxygen or nitrogen, preventing their diffusion into the free layer, thereby maintaining RA and improving operating speed.
This approach allows for the formation of a free layer with low saturation magnetization, enhancing the operating speed of the magnetic tunnel junction device while maintaining resistance area product, and improving stability and anisotropy.
Smart Images

Figure 112021025873103-PAT00001_ABST
Abstract
Description
Technology Field
[0001] The disclosed embodiments relate to a magnetic tunnel junction device, a memory device including a magnetic tunnel junction device, and a method for manufacturing a magnetic tunnel junction device. Background Technology
[0002] The resistance of a magnetic tunnel junction device depends on the magnetization direction of the free layer. For example, when the magnetization direction of the free layer is the same as that of the pinned layer, the magnetic tunnel junction device has a low resistance value, and when they are opposite, it can have a high resistance value. When utilizing this characteristic in a memory device, for instance, the magnetic tunnel junction device can correspond to data '0' when it has a low resistance value and to data '1' when it has a high resistance value.
[0003] Magnetic memory devices, such as MRAM (Magnetic Random Access Memory), are memory devices that store data by utilizing changes in resistance of magnetic tunnel junctions. These magnetic memory devices have advantages such as non-volatility, high-speed operation, and high durability. For example, STT-MRAM (Spin Transfer Torque-Magnetic RAM), currently in mass production, has an operating speed of approximately 50 to 100 nsec and can provide excellent data retention for more than 10 years. Furthermore, research is underway to achieve even faster operating speeds of less than 10 nsec. The problem to be solved
[0004] The present invention provides a magnetic tunnel junction device, a memory device including a magnetic tunnel junction device, and a method for manufacturing a magnetic tunnel junction device. means of solving the problem
[0005] A magnetic tunnel junction device according to one embodiment comprises: a first magnetic layer; a second magnetic layer disposed facing the first magnetic layer; and a first oxide layer disposed between the first magnetic layer and the second magnetic layer and comprising a metal oxide, wherein the metal oxide of the first oxide layer has a stoichiometrically oxygen-deficient composition, and the second magnetic layer may comprise a magnetic material doped with a metal element.
[0006] The first oxide layer comprises a first region adjacent to the first magnetic layer and a second region adjacent to the second magnetic layer, and the ratio of oxygen or nitrogen in the second region may be higher than the ratio of oxygen or nitrogen in the first region.
[0007] The first oxide layer may further include a metal layer disposed between the first region and the second region.
[0008] The thickness of the second region may be smaller than the thickness of the first region.
[0009] For example, the thickness of the metal layer may be 2 Å to 3 Å.
[0010] The metal material of the metal layer above may be the same as the metal material of the metal oxide of the first oxide layer above.
[0011] The magnetic tunnel junction element may further include a second oxide layer comprising a metal oxide, which is positioned facing the first oxide layer with the second magnetic layer in between.
[0012] The metal oxide of the second oxide layer above may have a stoichiometrically oxygen-deficient composition.
[0013] The second oxide layer comprises a first region disposed further from the second magnetic layer and a second region adjacent to the second magnetic layer, wherein the ratio of oxygen or nitrogen in the second region may be higher than the ratio of oxygen or nitrogen in the first region.
[0014] The second oxide layer may further include a metal layer disposed between the first region and the second region.
[0015] The first oxide layer contains MgO, and the proportion of Mg in the first oxide layer may be greater than 50 at% and the proportion of O may be less than 50 at%.
[0016] The oxygen affinity of the metal element of the second magnetic layer may be greater than the oxygen affinity of the magnetic material of the second magnetic layer.
[0017] For example, the magnetic material of the second magnetic layer comprises at least one of Fe, Co, Ni, Mn, Fe-containing alloy, Co-containing alloy, Ni-containing alloy, Mn-containing alloy, and Heusler alloy, and the metal element of the second magnetic layer may comprise at least one of Ca, Sc, Y, Mg, Sr, Ba, Zr, Be, Ti, Hf, V, Zn, Nb, Mn, Al, Cr, Li, Cd, Pb, In, Ga, and Ta.
[0018] A memory device according to another embodiment comprises a plurality of memory cells, each comprising a magnetic tunnel junction element and a switching element connected to the magnetic tunnel junction element, wherein the magnetic tunnel junction element comprises: a first magnetic layer; a second magnetic layer disposed facing the first magnetic layer; and an oxide layer disposed between the first magnetic layer and the second magnetic layer and comprising a metal oxide; wherein the metal oxide of the oxide layer has a stoichiometrically oxygen-deficient composition, and the second magnetic layer may comprise a magnetic material doped with a metal element.
[0019] A method for manufacturing a magnetic tunnel junction device according to another embodiment comprises the steps of: providing an oxide layer containing a metal oxide; cooling the oxide layer to a temperature range of 250 K or lower; depositing a wet layer containing a magnetic material on the oxide layer; oxidizing or nitriding the wet layer; depositing a magnetic layer containing a magnetic material doped with a metal element on the wet layer; and annealing the magnetic layer at a temperature of 300 K or higher; wherein the metal oxide may have a stoichiometrically oxygen-deficient composition.
[0020] The method for manufacturing the magnetic tunnel junction device may further include a step of increasing the ratio of oxygen or nitrogen in the region adjacent to the magnetic layer within the oxide layer by diffusing oxygen or nitrogen in the wet layer into the oxide layer while annealing the magnetic layer.
[0021] For example, the above temperature range may be 50K or higher and 150K or lower.
[0022] The above wet layer may include a single layer thickness.
[0023] For example, the wet layer may include at least one of Fe, Co, Ni, Mn, Fe-containing alloy, Co-containing alloy, Ni-containing alloy, and Mn-containing alloy.
[0024] The method for manufacturing the above magnetic tunnel junction device may further include the step of depositing an additional oxide layer comprising a metal oxide on the magnetic layer; and the step of depositing an additional magnetic layer comprising a magnetic material doped with a metal element on the additional oxide layer. Effects of the invention
[0025] According to the disclosed embodiment, a magnetic layer having low saturation magnetization characteristics can be formed on an oxide layer. Accordingly, the operating speed of the magnetic tunnel junction device can be improved. In addition, by preventing oxygen or nitrogen from being trapped in the magnetic layer during the process of forming the magnetic layer having low saturation magnetization characteristics on the oxide layer, the resistance area product (RA) of the magnetic tunnel junction device can be appropriately maintained. Brief explanation of the drawing
[0026] FIG. 1 is a cross-sectional view showing the schematic structure of a magnetic tunnel junction element according to one embodiment. FIGS. 2a to 2e are cross-sectional views schematically showing the process of manufacturing a magnetic tunnel junction device illustrated in FIG. 1. Figure 3 is a cross-sectional view conceptually showing the state in which oxygen or nitrogen is trapped in the magnetic layer of a magnetic tunnel junction device according to a comparative example. FIG. 4 is a cross-sectional view showing the schematic structure of a magnetic tunnel junction element according to another embodiment. FIG. 5 is a cross-sectional view showing the schematic structure of a magnetic tunnel junction element according to another embodiment. FIG. 6 is a cross-sectional view showing the schematic structure of a magnetic tunnel junction element according to another embodiment. FIG. 7 is a cross-sectional view showing the schematic structure of a magnetic tunnel junction element according to another embodiment. FIG. 8 is a cross-sectional view showing the schematic structure of a magnetic tunnel junction element according to another embodiment. FIG. 9 schematically shows a memory cell including a magnetic tunnel junction element according to one embodiment. FIG. 10 is a circuit diagram schematically showing the configuration of a memory device including a plurality of memory cells as illustrated in FIG. 9. Specific details for implementing the invention
[0027] Hereinafter, with reference to the attached drawings, a magnetic tunnel junction device, a memory device including a magnetic tunnel junction device, and a method for manufacturing a magnetic tunnel junction device will be described in detail. In the drawings below, the same reference numerals refer to the same components, and the size of each component in the drawings may be exaggerated for clarity and convenience of explanation. Furthermore, the embodiments described below are merely illustrative, and various modifications are possible from these embodiments.
[0028] In the following, terms designated as "upper" or "upper" may include not only those directly above in contact but also those above non-contact. Singular expressions include plural expressions unless the context clearly indicates otherwise. Furthermore, when a part is described as "comprising" a certain component, this means that, unless specifically stated otherwise, it does not exclude other components but may include additional components.
[0029] The use of the term "for example" and similar descriptive terms may apply to both the singular and the plural. Unless there is an explicit description of the order of the steps constituting the method, these steps may be performed in a suitable order and are not necessarily limited to the described order.
[0030] Additionally, terms such as "...part," "module," etc., as described in the specification refer to a unit that processes at least one function or operation, and this may be implemented in hardware or software, or as a combination of hardware and software.
[0031] The connections of lines or connecting members between the components shown in the drawings are exemplary representations of functional connections and / or physical or circuit connections, and may be replaced or additionally represented as various functional connections, physical connections, or circuit connections in the actual device.
[0032] All examples or the use of exemplary terms are merely for the purpose of describing technical ideas in detail, and unless limited by the claims, the scope is not limited by such examples or exemplary terms.
[0033] FIG. 1 is a cross-sectional view showing the schematic structure of a magnetic tunnel junction device according to one embodiment. Referring to FIG. 1, the magnetic tunnel junction device (100) according to the embodiment may include a first magnetic layer (101), a first oxide layer (102) disposed on the first magnetic layer (101), a second magnetic layer (105) disposed on the first oxide layer (102), and a second oxide layer (106) disposed on the second magnetic layer (105). Here, the expression "disposed on" is for convenience of explanation and does not necessarily imply a vertical relationship. In other words, the first oxide layer (102) may be disposed between the first magnetic layer (101) and the second magnetic layer (105), and the second magnetic layer (105) may be disposed between the first oxide layer (102) and the second oxide layer (106).
[0034] The first magnetic layer (101) and the second magnetic layer (105) may be made of a ferromagnetic metal material having magnetism. For example, the first magnetic layer (101) and the second magnetic layer (105) may include at least one of iron (Fe), cobalt (Co), nickel (Ni), manganese (Mn), Fe-containing alloy, Co-containing alloy, Ni-containing alloy, Mn-containing alloy, and Heusler alloy. One of the first magnetic layer (101) and the second magnetic layer (105) may be a pinned layer having a fixed magnetization direction, and the other may be a free layer having a variable magnetization direction. The magnetic tunnel junction element (100) has low resistance when the magnetization directions of the first magnetic layer (101) and the second magnetic layer (105) are the same, and high resistance when the magnetization directions are opposite. This phenomenon is called tunneling magnetoresistance (TMR). By applying this TMR phenomenon, a magnetic tunnel junction device (100) can be used in a memory device.
[0035] The first magnetic layer (101) and the second magnetic layer (105) may be made of the same magnetic material, but are not necessarily limited thereto. In order to improve the operating speed of a memory device using a magnetic tunnel junction device (100), the magnetic layer acting as a free layer among the first magnetic layer (101) and the second magnetic layer (105) may have a low saturation magnetization (Ms). For example, the magnetic layer acting as a free layer among the first magnetic layer (101) and the second magnetic layer (105) may be formed so as not to contain boron (B). The presence of boron in the free layer may increase the saturation magnetization and reduce the switching efficiency of the magnetic tunnel junction device (100). To further lower the saturation magnetization of the free layer, the magnetic layer acting as a free layer among the first magnetic layer (101) and the second magnetic layer (105) may further include a magnetic material doped with a metal element other than boron. The magnetic layer acting as a fixed layer as well as the free layer may include boron-free magnetic material or magnetic material doped with other metal elements.
[0036] The first magnetic layer (101) and the second magnetic layer (105) may have high perpendicular magnetic anisotropy (PMA). In other words, the perpendicular magnetic anisotropy energy of the first magnetic layer (101) and the second magnetic layer (105) may exceed the out-of-plane demagnetization energy. In this case, the magnetic moments of the first magnetic layer (101) and the second magnetic layer (105) may be stabilized in a direction perpendicular to the layer direction. Such a magnetic tunnel junction device (100) may be applied to an STT-MRAM. However, the magnetization direction of the first magnetic layer (101) and the second magnetic layer (105) is not limited to a direction perpendicular to the layer direction, and the first magnetic layer (101) and the second magnetic layer (105) may have a magnetization direction parallel to the layer direction. In addition, the magnetic tunnel junction device (100) can be applied not only to STT-MRAM but also to SOT (spin-orbit coupling torque) MRAM.
[0037] A first oxide layer (102) disposed between the first magnetic layer (101) and the second magnetic layer (105) can serve as a tunnel barrier layer for magnetic tunneling junctions. The first oxide layer (102) may include crystalline Mg oxide. For example, the first oxide layer (102) may be MgO, MgAl2O4, or MgTiO2 x It may include. Additionally, the second oxide layer (106) may serve as a capping layer. The second oxide layer (106) may be made of any oxide material, but is typically made of the same material as the first oxide layer (102).
[0038] FIGS. 2a to 2e are cross-sectional views schematically showing the process of manufacturing the magnetic tunnel junction element illustrated in FIG. 1. Hereinafter, a method for manufacturing the magnetic tunnel junction element (100) illustrated in FIG. 1 will be described with reference to FIGS. 2a to 2e.
[0039] First, referring to FIG. 2a, a first oxide layer (102) is formed on a first magnetic layer (101). The first oxide layer (102) may be made of a metal oxide having a stoichiometrically oxygen-deficient composition so as to be able to trap oxygen or nitrogen generated during the annealing process described later. For example, if the first oxide layer (102) is made of MgO, the proportion of magnesium (Mg) in the first oxide layer (102) may be greater than 50 at% and the proportion of oxygen (O) may be less than 50 at%. Also, for example, the proportion of magnesium (Mg) in the first oxide layer (102) may be about 52 at% to about 65 at%, and the proportion of oxygen (O) may be about 40 at% to about 35 at%. When the first oxide layer (102) is composed of MgAl2O4, the proportion of oxygen (O) in the first oxide layer (102) may be less than about 57 at%. In other words, the first oxide layer (102) may be formed to have an oxygen composition that is less than the inherent oxygen composition of the oxide material forming the first oxide layer (102).
[0040] This first oxide layer (102) can be formed, for example, through RF (radio frequency) sputtering, and the oxygen composition within the first oxide layer (102) can be controlled by controlling the amount of material supplied onto the first magnetic layer (101) in the chamber. Alternatively, the first oxide layer (102) may be formed by first depositing an oxide metal material onto the first magnetic layer (101) and then oxidizing the metal material. In this case, the oxygen composition of the first oxide layer (102) can be controlled by the time of oxidation of the metal material. For example, Mg may be formed by first depositing Mg onto the first magnetic layer (101) and then oxidizing the Mg. At this time, if oxidation is performed for a shorter time than the time required to completely oxidize Mg, the MgO of the first oxide layer (102) may have an oxygen-deficient composition.
[0041] After forming the first oxide layer (102), the first magnetic layer (101) and the first oxide layer (102) are cooled to a low temperature. Generally, the oxide of the first oxide layer (102) has a relatively low surface energy, whereas the metal material of the second magnetic layer (105) has a relatively high surface energy. As a result, when forming the second magnetic layer (105) on the first oxide layer (102), the metal material may not be evenly distributed on the surface of the first oxide layer (102). This problem can be improved by lowering the temperature of the first oxide layer (102) to reduce the mobility of the metal material. For example, the first oxide layer (102) can be cooled to a temperature of about 250 K or less, or about 50 K to about 150 K, or about 70 K to about 100 K.
[0042] Referring to FIG. 2b, a wet layer (103) may be formed first on the first oxide layer (102) before forming the second magnetic layer (105). The wet layer (103) may increase the surface energy of the first oxide layer (102) to help deposit the second magnetic layer (105) on the first oxide layer (102). The wet layer (103) may be formed by methods such as sputtering or PVD (physical vapor deposition). The wet layer (103) may be used as a precursor for the second magnetic layer (105). To this end, the wet layer (103) may include a 3d transition metal and / or an alloy thereof. For example, the wet layer (103) may include at least one material among Fe, Co, Ni, Mn, Fe-containing alloys, Co-containing alloys, Ni-containing alloys, and Mn-containing alloys. Optionally, the wet layer (103) may include an alloy of other materials, such as non-transfer metals excluding boron (B).
[0043] The wet layer (103) can be formed with a very thin thickness. For example, the wet layer (103) can be formed with only two or three monolayers. This wet layer (103) can be distributed generally uniformly over the first oxide layer (102), but because it has a very thin thickness, it does not need to have a completely smooth and continuous distribution, and there may be partial voids within the wet layer (103).
[0044] Referring to FIG. 2c, the wet layer (103) can be oxidized or nitrided to bond oxygen or nitrogen atoms (104) to the wet layer (103). For example, the wet layer (103) can be naturally oxidized, or other oxidation methods such as reactive oxidation may be used. Alternatively, the wet layer (103) can be nitrided naturally or through an intentional reaction. This oxidation / nitriding reaction may be performed until a target resistance area product (RA) is achieved. Through the oxidation / nitriding reaction, the wet layer (103) may be completely oxidized or nitrided, but the oxidation / nitriding reaction may be terminated before the wet layer (103) is completely oxidized or nitrided. As a result, an oxidized / nitrided wet layer (103') is formed on the first oxide layer (102).
[0045] Referring to FIG. 2d, a second magnetic layer (105) can be deposited on an oxidized / nitrided wet layer (103'). The second magnetic layer (105) may be made of a boron-free magnetic material that does not contain boron (B). For example, to form the second magnetic layer (105) on an oxidized / nitrided wet layer (103'), at least one of 3d transition metals such as iron (Fe), cobalt (Co), nickel (Ni), and manganese (Mn), 3d transition metal alloys such as Fe-containing alloys, Co-containing alloys, Ni-containing alloys, and Mn-containing alloys, or Heusler alloys such as Co2Fe, Co2MnSi, Co2FeMnSi, Co2FeSi, MnGa, MnGe, etc. may be deposited. Boron can lower the surface energy of the second magnetic layer (105) to facilitate the formation of the second magnetic layer (105) on the first oxide layer (102), but as previously explained, it can cause a decrease in the switching efficiency of the magnetic tunnel junction device (100).
[0046] In addition, as previously explained, the second magnetic layer (105) may be doped with additional metal elements other than boron. For example, the additional metal elements doped into the second magnetic layer (105) may include at least one of calcium (Ca), scandium (Sc), yttrium (Y), magnesium (Mg), strontium (Sr), barium (Ba), zirconium (Zr), beryllium (Be), titanium (Ti), hafnium (Hf), vanadium (V), zinc (Zn), niobium (Nb), manganese (Mn), aluminum (Al), chromium (Cr), lithium (Li), cadmium (Cd), lead (Pb), indium (In), gallium (Ga), and tantalum (Ta). These additional metal elements may be non-magnetic metals, but are not necessarily limited to non-magnetic metals. In particular, the additional metal element doped into the second magnetic layer (105) may have a higher oxygen affinity than the oxygen affinity of the ferromagnetic material in the second magnetic layer (105) for reasons described later.
[0047] In the step of forming the second magnetic layer (105), the first oxide layer (102) may still be in a cryogenically cooled state. This is because the time from cooling the first oxide layer (102) until depositing the second magnetic layer (105) may be significantly shorter than the time it takes for the temperature of the first oxide layer (102) to naturally rise to room temperature. Even if the temperature of the first oxide layer (102) rises naturally, the temperature of the first oxide layer (102) in the step of forming the second magnetic layer (105) may be 300 K or less, for example, 250 K or less. Alternatively, the temperature of the first oxide layer (102) may be 200 K or less at the start of depositing the second magnetic layer (105). If necessary, additional cooling may be performed before forming the oxidized / nitrided wet layer (103') and depositing the second magnetic layer (105).
[0048] After forming the second magnetic layer (105), a second oxide layer (106) may be further formed on the second magnetic layer (105). The second oxide layer (106) may include the same oxide material as the first oxide layer (102), but may also include a different oxide material. However, the second oxide layer (106) is not an essential component, and in some cases, the step of forming the second oxide layer (106) may be omitted.
[0049] Finally, referring to FIG. 2e, the second magnetic layer (105) may be annealed at a temperature above room temperature (300 K) to improve the crystallinity of the second magnetic layer (105). For example, rapid thermal annealing may be performed. During the annealing process, oxygen or nitrogen atoms (104) bonded to the oxidized / nitrided wet layer (103') may diffuse into the first oxide layer (102). As oxygen or nitrogen atoms (104) within the oxidized / nitrided wet layer (103') diffuse into the first oxide layer (102), the proportion of oxygen or nitrogen in the region adjacent to the second magnetic layer (105) within the first oxide layer (102) may increase. The wet layer (103) from which the oxygen or nitrogen atoms (104) have escaped may be fused into the second magnetic layer (105) and may be virtually indistinguishable from the second magnetic layer (105).
[0050] As previously explained, the first oxide layer (102) has an oxygen-deficient composition. Therefore, the first oxide layer (102) can easily combine with oxygen or nitrogen atoms (104) that escape from the oxidized / nitrided wet layer (103'). Oxygen or nitrogen atoms (104) that escape from the oxidized / nitrided wet layer (103') can be mainly combined in the upper region of the first oxide layer (102) that is in contact with the wet layer (103). Thus, after the step illustrated in FIG. 2e, the first oxide layer (102) may include a first region (102a) adjacent to the first magnetic layer (101) and a second region (102b) adjacent to the second magnetic layer (105), and the ratio of oxygen or nitrogen in the second region (102b) may be higher than the ratio of oxygen or nitrogen in the first region (102a).
[0051] In the method for manufacturing a magnetic tunnel junction device (100) illustrated in FIGS. 2a to 2e, the first magnetic layer (101) may be a fixed layer and the second magnetic layer (105) may be a free layer. According to the method illustrated in FIGS. 2a to 2e, since the first oxide layer (102) has an oxygen-deficient composition, oxygen or nitrogen atoms (104) escaping from the oxidized / nitrided wet layer (103') do not diffuse into the second magnetic layer (105), which is mostly a free layer, but instead diffuse into the first oxide layer (102) and can be trapped within the first oxide layer (102). Therefore, it is possible to prevent an increase in the RA of the magnetic tunnel junction device (100) due to oxygen or nitrogen atoms within the free layer.
[0052] FIG. 3 is a conceptual cross-sectional view showing the state in which oxygen or nitrogen is trapped in the magnetic layer of a magnetic tunnel junction device according to a comparative example. Referring to FIG. 3, the magnetic tunnel junction device according to the comparative example includes a first magnetic layer (11), a first oxide layer (12), a second magnetic layer (15), and a second oxide layer (16). The first oxide layer (12) has a composition that is not stoichiometrically deficient in oxygen. In this case, as shown in FIG. 3, oxygen or nitrogen atoms (14) separated from the wet layer during the annealing process may diffuse into the second magnetic layer (15), which is a free layer. The oxygen or nitrogen atoms (14) diffused into the second magnetic layer (15) may cause an increase in the RA of the magnetic tunnel junction device according to the comparative example.
[0053] In particular, when a metal having high oxygen affinity is doped into the second magnetic layer (105), the likelihood of oxygen or nitrogen atoms (104) being captured by the metal having high oxygen affinity within the second magnetic layer (105) increases. According to the present embodiment, since the first oxide layer (102) having a stoichiometrically oxygen-deficient composition bonds with almost all oxygen or nitrogen atoms (104), it is possible to form the second magnetic layer (105) doped with a metal having high oxygen affinity on the first oxide layer (102) without degradation. For example, even if the second magnetic layer (105) is doped with a metal having a higher oxygen affinity than the oxygen affinity of the ferromagnetic material within the second magnetic layer (105), oxygen or nitrogen atoms (104) may not diffuse into the second magnetic layer (105) due to the first oxide layer (102) having an oxygen-deficient composition.
[0054] Accordingly, according to the present embodiment, a free layer having low saturation magnetization characteristics can be formed on an oxide layer, and as a result, the operating speed of the magnetic tunnel junction device (100) can be improved. In addition, the RA of the magnetic tunnel junction device (100) can be appropriately maintained by preventing oxygen or nitrogen from being trapped inside the free layer during the process of forming the free layer having low saturation magnetization characteristics on the oxide layer. In addition, a boron-free free layer can be uniformly formed with a relatively thin thickness on an oxide layer having relatively low surface energy. The free layer formed in this way can have improved stability and improved normal magnetic anisotropy. As a result, the operating speed of the magnetic tunnel junction device (100) can be further improved.
[0055] FIG. 4 is a cross-sectional view showing the schematic structure of a magnetic tunnel junction element according to another embodiment. Referring to FIG. 4, the magnetic tunnel junction element (200) may include a first magnetic layer (201), a first oxide layer (202) disposed on the first magnetic layer (201), a second magnetic layer (205) disposed on the first oxide layer (202), and a second oxide layer (206) disposed on the second magnetic layer (205). For example, the first magnetic layer (201) may be a fixed layer and the second magnetic layer (205) may be a free layer. Additionally, the first oxide layer (202) may be a tunnel barrier layer and the second oxide layer (206) may be a capping layer. If necessary, the second oxide layer (206) may be omitted.
[0056] The first oxide layer (202) may include a metal oxide having a stoichiometrically oxygen-deficient composition. Additionally, the first oxide layer (202) may include a first region (202a) adjacent to the first magnetic layer (201), a second region (202b) adjacent to the second magnetic layer (205), and a metal layer (202c) disposed between the first region (202a) and the second region (202b). The metal layer (202c) may include the same metal material as the metal material of the metal oxide forming the first oxide layer (202). For example, if the first oxide layer (202) includes MgO, the metal layer (202c) may be made of Mg. However, the material of the metal layer (202c) is not necessarily limited to this and may include other metal materials that are easy to deposit on the metal oxide of the first oxide layer (202) and easy to combine with oxygen or nitrogen.
[0057] The metal layer (202c) can serve to capture oxygen or nitrogen atoms (204) that escape from the wet layer (203) during the annealing process of the second magnetic layer (205). Due to the metal layer (202c), the first oxide layer (202) can capture more oxygen or nitrogen atoms (204) and further reduce the oxygen or nitrogen atoms that diffuse into the second magnetic layer (205). Because the metal layer (202c) combines with oxygen or nitrogen atoms (204) during the annealing process, the final metal layer (202c) may have a partially oxidized or nitrided state.
[0058] A metal layer (202c) within the first oxide layer (202) can be positioned as close as possible to the second magnetic layer (205). To this end, the thickness of the second region (102b) of the first oxide layer (202) may be smaller than the thickness of the first region (102a). Additionally, the metal layer (202c) may have a thin thickness so as not to affect the tunnel barrier layer function of the first oxide layer (202). For example, the thickness of the metal layer (202c) may be within the range of about 2 Å to about 3 Å. Meanwhile, as previously described, the ratio of oxygen or nitrogen in the second region (102b) of the first oxide layer (202) may be higher than the ratio of oxygen or nitrogen in the first region (102a). The remaining components of the magnetic tunnel junction element (200) may be identical to the components of the magnetic tunnel junction element (100) shown in FIG. 1.
[0059] FIG. 5 is a cross-sectional view showing the schematic structure of a magnetic tunnel junction element according to another embodiment. In the magnetic tunnel junction elements (100, 200) shown in FIG. 1 and FIG. 4, a fixed layer is positioned at the bottom and a free layer is positioned at the top. However, it is also possible for a free layer to be positioned at the bottom and a fixed layer to be positioned at the top. Referring to FIG. 5, the magnetic tunnel junction element (300) may include a second oxide layer (306), a second magnetic layer (305) positioned on the second oxide layer (306), a first oxide layer (302) positioned on the second magnetic layer (305), and a first magnetic layer (301) positioned on the first oxide layer (302). The first magnetic layer (301) may be a fixed layer and the second magnetic layer (305) may be a free layer, and the first oxide layer (302) may be a tunnel barrier layer and the second oxide layer (306) may be a capping layer.
[0060] In this embodiment, a second magnetic layer (305), which is a free layer, can be formed on a second oxide layer (306), which is a capping layer. To do this, a wet layer (303) can be formed on the second oxide layer (306) while the second oxide layer (306) is cooled to a cryogenic temperature, and the wet layer (303) can be oxidized or nitrided. Additionally, after forming the second magnetic layer (305) on the wet layer (303), the second oxide layer (306) may have an oxygen-deficient composition so that oxygen or nitrogen atoms (304) coming from the wet layer (303) during the annealing process of the second magnetic layer (305) can be captured within the second oxide layer (306). When the annealing process is completed, the second oxide layer (306) comprises a first region (306a) with a relatively low ratio of oxygen or nitrogen and a second region (306b) with a relatively high ratio of oxygen or nitrogen. The second region (306b) is a region positioned adjacent to the second magnetic layer (305).
[0061] The first oxide layer (302) may be made of a metal oxide material containing a fixed amount of oxygen. For example, if the first oxide layer (302) contains MgO, the ratio of Mg and the ratio of O within the first oxide layer (302) may each be about 50 at%.
[0062] FIG. 6 is a cross-sectional view showing the schematic structure of a magnetic tunnel junction device according to another embodiment. In the magnetic tunnel junction device (300) illustrated in FIG. 5, a first magnetic layer (301), which is a fixed layer, can be deposited in a conventional manner on a first oxide layer (302), which is a tunnel barrier layer. For example, in the embodiment illustrated in FIG. 5, the first magnetic layer (301) may include a ferromagnetic material containing boron, or it may not be doped with other metal elements. However, if high quality is required for the first magnetic layer (301), which is a fixed layer, the first magnetic layer (301) may also include a boron-free magnetic material and may be doped with other metal elements having a relatively high oxygen affinity.
[0063] To this end, referring to FIG. 6, the magnetic tunnel junction element (300') may include a first oxide layer (302) having an oxygen-deficient composition. Additionally, while the first oxide layer (302) is cooled to a cryogenic temperature, a wet layer (303) may be formed and an oxidation / nitriding process performed on the first oxide layer (302), and a first magnetic layer (301) may be deposited on the wet layer (303). Afterward, when the first magnetic layer (301) is annealed, oxygen or nitrogen atoms (304) may be trapped within the first oxide layer (302) without diffusing into the first magnetic layer (301). Accordingly, the first oxide layer (302) includes a first region (302a) in which the ratio of oxygen or nitrogen is relatively low and a second region (302b) in which the ratio of oxygen or nitrogen is relatively high. Here, the first region (302a) is positioned adjacent to the second magnetic layer (305), and the second region (306b) is positioned adjacent to the first magnetic layer (301).
[0064] FIG. 7 is a cross-sectional view showing the schematic structure of a magnetic tunnel junction element according to another embodiment. Referring to FIG. 7, the magnetic tunnel junction element (400) may include a second oxide layer (406), a second magnetic layer (405) disposed on the second oxide layer (406), a first oxide layer (402) disposed on the second magnetic layer (405), and a first magnetic layer (401) disposed on the first oxide layer (402).
[0065] The second oxide layer (406) may include a metal oxide having a stoichiometrically oxygen-deficient composition. Additionally, the second oxide layer (406) may include a first region (406a) with a relatively low ratio of oxygen or nitrogen, a second region (406b) with a relatively high ratio of oxygen or nitrogen, and a metal layer (406c) disposed between the first region (406a) and the second region (406b). The metal layer (406c) may be identical to the metal layer (202c) of the first oxide layer (202) described in FIG. 4. Other configurations of the magnetic tunnel junction element (400) not described may be identical to the configurations of the magnetic tunnel junction element (300) shown in FIG. 5. Additionally, the first oxide layer (402) of the magnetic tunnel junction element (400) may further have the configuration described in FIG. 6.
[0066] FIG. 8 is a cross-sectional view showing the schematic structure of a magnetic tunnel junction element according to another embodiment. Referring to FIG. 8, the magnetic tunnel junction element (500) may include a first magnetic layer (501), a first oxide layer (502) disposed on the first magnetic layer (501), a second magnetic layer (505) disposed on the first oxide layer (502), a second oxide layer (512) disposed on the second magnetic layer (505), a third magnetic layer (511) disposed on the second oxide layer (512), and a third oxide layer (506) disposed on the third magnetic layer (511).
[0067] The first magnetic layer (501) and the third magnetic layer (511) may be fixed layers, and the second magnetic layer (505) may be a free layer. Accordingly, the magnetic tunnel junction element (500) may include two fixed layers and one free layer disposed between them. Additionally, the first oxide layer (502) and the second oxide layer (512) may be tunnel barrier layers, and the third oxide layer (506) may be an optional capping layer. To capture oxygen or nitrogen atoms (504), the first oxide layer (502) disposed below the second magnetic layer (505), which is a free layer, may have an oxygen-deficient composition.
[0068] FIG. 8 illustrates that the second oxide layer (512), which is positioned below the third magnetic layer (511) which is the fixed layer, also has an oxygen-deficient composition and that oxygen or nitrogen atoms (504) are trapped within the second oxide layer (512). However, this is optional and is not necessarily limited thereto. For example, the second oxide layer (512) may be made of a metal oxide material containing a fixed amount of oxygen. The third magnetic layer (511), which is the fixed layer, may be deposited on the second oxide layer (512) by a conventional method.
[0069] FIG. 9 schematically shows a memory cell including a magnetic tunnel junction element according to one embodiment. Referring to FIG. 9, the memory cell (MC) may include a magnetic tunnel junction element (100) and a switching element (TR) connected thereto. The switching element (TR) may be a thin-film transistor. The memory cell (MC) may be connected between a bit line (BL) and a word line (WL). The bit line (BL) and the word line (WL) may be arranged to intersect each other, and the memory cell (MC) may be placed at the intersection of these lines. The bit line (BL) may be electrically connected to a second magnetic layer (105), which is a free layer of the magnetic tunnel junction element (100), and the word line (WL) may be connected to the gate of the switching element (TR). Additionally, the first source / drain electrode of the switching element (TR) may be electrically connected to the first magnetic layer (101), which is the fixed layer of the magnetic tunnel junction element (100), and the second source / drain electrode may be electrically connected to the select line (SL). In this structure, a write current, a read current, an erase current, etc., may be applied to the memory cell (MC) through the word line (WL) and the bit line (BL). Although FIG. 9 is illustrated as having a memory cell (MC) that includes the magnetic tunnel junction element (100) shown in FIG. 1, other memory cells (MC) in other embodiments may include magnetic tunnel junction elements (200, 300, 400, 500).
[0070] FIG. 10 is a circuit diagram schematically showing the configuration of a memory device including a plurality of memory cells illustrated in FIG. 9. Referring to FIG. 10, the memory device (600) may include a plurality of bit lines (BL), a plurality of word lines (WL), a plurality of select lines (SL), a plurality of memory cells (MC) respectively disposed at the intersections of the plurality of bit lines (BL) and the plurality of word lines (WL), a bit line driver (601) for applying current to the plurality of bit lines (BL), a word line driver (602) for applying current to the plurality of word lines (WL), and a select line driver (603) for applying current to the plurality of select lines (SL). Each memory cell (MC) may have the configuration illustrated in FIG. 9.
[0071] The memory device (600) illustrated in FIG. 10 may be a magnetic random access memory (MRAM) and may be used in electronic devices that use non-volatile memory. In particular, the memory device (600) illustrated in FIG. 10 may be an STT-MRAM in which the magnetization direction of the free layer is changed by a spin current directly applied to the free layer of a magnetic tunnel junction device. Since the STT-MRAM does not require a separate wire for generating an external magnetic field, it is advantageous for high integration and has a simple operation method. Although an STT-MRAM is illustrated as an example in FIG. 10, the disclosed magnetic tunnel junction device may also be applied to an SOT-MRAM.
[0072] The magnetic tunnel junction device, the memory device including the magnetic tunnel junction device, and the method for manufacturing the magnetic tunnel junction device described above have been described with reference to the embodiments illustrated in the drawings, but this is merely illustrative and those skilled in the art will understand that various modifications and equivalent alternative embodiments are possible therefrom. Therefore, the disclosed embodiments should be considered in an illustrative rather than a restrictive sense. The scope of rights is defined in the claims, not in the foregoing description, and all variations within the scope of equivalence should be interpreted as being included in the scope of rights. Explanation of the symbols
[0073] 100, 200, 300, 400, 500.....Magnetic tunnel junction device 101, 105, 201, 205, 301, 305, 401, 405, 501, 505.....magnetic layer 102, 106, 202, 206, 302, 306, 402, 406, 502, 506.....oxide layer 103, 203, 303, 403, 503.....wet layer 104.....Oxygen or nitrogen atom 600.....Memory device 601.....bit line driver 602.....Word line driver 603.....Select Line Driver BL.....Beat Line MC.....Memory cell SL.....Selection Line TR.....switching element WL.....Word Line
Claims
Claim 1 A magnetic tunnel junction device comprising: a first magnetic layer; a second magnetic layer disposed opposite the first magnetic layer; and a first oxide layer disposed between the first magnetic layer and the second magnetic layer and comprising a metal oxide; wherein the metal oxide of the first oxide layer has a stoichiometrically oxygen-deficient composition; wherein the second magnetic layer comprises a magnetic material doped with a metal element; wherein the magnetic material of the second magnetic layer comprises at least one of Fe, Co, Ni, Mn, Fe-containing alloy, Co-containing alloy, Ni-containing alloy, Mn-containing alloy, and Heusler alloy; and wherein the metal element doped into the second magnetic layer comprises at least one of Ca, Sc, Y, Mg, Sr, Ba, Be, Zn, Al, Li, Cd, Pb, In, and Ga. Claim 2 A magnetic tunnel junction device according to claim 1, wherein the first oxide layer comprises a first region adjacent to the first magnetic layer and a second region adjacent to the second magnetic layer, wherein the ratio of oxygen or nitrogen in the second region is higher than the ratio of oxygen or nitrogen in the first region. Claim 3 In claim 2, the magnetic tunnel junction device further comprises a metal layer disposed between the first region and the second region in the first oxide layer. Claim 4 In claim 3, the magnetic tunnel junction element, wherein the thickness of the second region is smaller than the thickness of the first region. Claim 5 A magnetic tunnel junction element according to claim 3, wherein the thickness of the metal layer is 2 Å to 3 Å. Claim 6 In claim 3, the metal material of the metal layer is the same as the metal material of the metal oxide of the first oxide layer, in a magnetic tunnel junction device. Claim 7 A magnetic tunnel junction device according to claim 1, further comprising a second oxide layer comprising a metal oxide and disposed facing the first oxide layer with the second magnetic layer in between. Claim 8 In claim 7, the metal oxide of the second oxide layer has a stoichiometrically oxygen-deficient composition, forming a magnetic tunnel junction device. Claim 9 In claim 8, the second oxide layer comprises a first region disposed further from the second magnetic layer and a second region adjacent to the second magnetic layer, wherein the ratio of oxygen or nitrogen in the second region is higher than the ratio of oxygen or nitrogen in the first region, a magnetic tunnel junction device. Claim 10 In claim 9, the magnetic tunnel junction device further comprises a metal layer disposed between the first region and the second region in the second oxide layer. Claim 11 A magnetic tunnel junction device according to claim 1, wherein the first oxide layer comprises MgO, and the ratio of Mg in the first oxide layer is greater than 50 at% and the ratio of O is less than 50 at%. Claim 12 A magnetic tunnel junction device according to claim 1, wherein the oxygen affinity of the metal element of the second magnetic layer is greater than the oxygen affinity of the magnetic material of the second magnetic layer. Claim 13 delete Claim 14 A memory device comprising a plurality of memory cells, each including a magnetic tunnel junction element and a switching element connected to the magnetic tunnel junction element, wherein the magnetic tunnel junction element comprises: a first magnetic layer; a second magnetic layer disposed facing the first magnetic layer; and an oxide layer disposed between the first magnetic layer and the second magnetic layer and comprising a metal oxide; wherein the metal oxide of the oxide layer has a stoichiometrically oxygen-deficient composition; wherein the second magnetic layer comprises a magnetic material doped with a metal element; wherein the magnetic material of the second magnetic layer comprises at least one of Fe, Co, Ni, Mn, Fe-containing alloy, Co-containing alloy, Ni-containing alloy, Mn-containing alloy, and Heusler alloy; and wherein the metal element doped into the second magnetic layer comprises at least one of Ca, Sc, Y, Mg, Sr, Ba, Be, Zn, Al, Li, Cd, Pb, In, and Ga. Claim 15 A method for manufacturing a magnetic tunnel junction device, comprising: a step of providing an oxide layer containing a metal oxide; a step of cooling the oxide layer to a temperature range of 250 K or less; a step of depositing a wet layer containing a magnetic material on the oxide layer; a step of oxidizing or nitriding the wet layer; a step of depositing a magnetic layer containing a magnetic material doped with a metal element on the wet layer; and a step of annealing the magnetic layer at a temperature of 300 K or more; wherein the metal oxide has a stoichiometrically oxygen-deficient composition. Claim 16 A method for manufacturing a magnetic tunnel junction device according to claim 15, further comprising the step of increasing the ratio of oxygen or nitrogen in the region adjacent to the magnetic layer within the oxide layer by diffusing oxygen or nitrogen in the wet layer into the oxide layer while annealing the magnetic layer. Claim 17 A method for manufacturing a magnetic tunnel junction device according to claim 15, wherein the oxide layer comprises a metal layer embedded therein. Claim 18 A method for manufacturing a magnetic tunnel junction device according to claim 17, wherein the thickness of the metal layer is 2 Å to 3 Å. Claim 19 A method for manufacturing a magnetic tunnel junction device according to claim 17, wherein the metal material of the metal layer is the same as the metal material of the metal oxide of the oxide layer. Claim 20 A method for manufacturing a magnetic tunnel junction device according to claim 15, wherein the oxide layer comprises MgO, and the ratio of Mg in the oxide layer is greater than 50 at% and the ratio of O is less than 50 at%. Claim 21 A method for manufacturing a magnetic tunnel junction device according to claim 15, wherein the oxygen affinity of the metal element of the magnetic layer is greater than the oxygen affinity of the magnetic material of the magnetic layer. Claim 22 A method for manufacturing a magnetic tunnel junction device according to claim 21, wherein the magnetic material of the magnetic layer comprises at least one of Fe, Co, Ni, Mn, Fe-containing alloy, Co-containing alloy, Ni-containing alloy, Mn-containing alloy, and Heusler alloy, and the metal element of the magnetic layer comprises at least one of Ca, Sc, Y, Mg, Sr, Ba, Zr, Be, Ti, Hf, V, Zn, Nb, Mn, Al, Cr, Li, Cd, Pb, In, Ga, and Ta. Claim 23 A method for manufacturing a magnetic tunnel junction device according to claim 15, wherein the temperature range is 50K or higher and 150K or lower. Claim 24 A method for manufacturing a magnetic tunnel junction device according to claim 15, wherein the wet layer comprises a single layer thickness. Claim 25 A method for manufacturing a magnetic tunnel junction device according to claim 15, wherein the wet layer comprises at least one of Fe, Co, Ni, Mn, Fe-containing alloy, Co-containing alloy, Ni-containing alloy and Mn-containing alloy. Claim 26 A method for manufacturing a magnetic tunnel junction device according to claim 15, further comprising: a step of depositing an additional oxide layer comprising a metal oxide on the magnetic layer; and a step of depositing an additional magnetic layer comprising a magnetic material doped with a metal element on the additional oxide layer.
Citation Information
Patent Citations
Magnetic element having perpendicular anisotropy with enhanced efficiency
KR1020140107143A
Magnetic memory device and method for manufacturing the same
KR1020180016678A
Multiple Magneto-Resistance Devices Based on Doped Magnesium Oxide
US20090067232A1
Magnetoresistive effect devices having enhanced magnetic anisotropy