An acoustic device comprising a dense polyethylene membrane, an electronic devicecomprising the acoustic device, a method of making the acoustic device, and use ofa dense polyethylene membrane in an acoustic device

WO2024129627A8PCT designated stage expired Publication Date: 2024-10-31WL GORE & ASSOC INC
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
PCT/US2023/083466
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2022-12-12
Filing Date
2023-12-12
Publication Date
2024-10-31

AI Technical Summary

Technical Problem

Existing acoustic devices face challenges with sound transmission loss and mechanical strength due to the need for thick, non-porous membranes to prevent water, dust, and contaminants, which compromise sound quality and durability under external pressure.

Method used

A dense polyethylene membrane with a thickness of 0.5 to 3.0 pm, a mean mass per area of 0.4 to 3 g/m², and a geometric mean 5-point modulus of at least 1500 MPa, formed from ultrahigh molecular weight polyethylene, is used to cover openings in acoustic devices, providing a balance between sound transmission and mechanical strength.

Benefits of technology

The dense polyethylene membrane effectively prevents contaminant ingress, withstands external pressure without damage, and maintains minimal sound transmission loss, outperforming current PTFE membranes in terms of mechanical strength and acoustic performance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure US2023083466_31102024_PF_FP_ABST
    Figure US2023083466_31102024_PF_FP_ABST
Patent Text Reader

Abstract

The present disclosure relates to an acoustic device comprising a dense polyethylene membrane. The present disclosure also relates to an electronic device comprising the acoustic device, a method of making the acoustic device and the use of a dense polyethylene membrane in an acoustic device.
Need to check novelty before this filing date? Find Prior Art

Description

AN ACOUSTIC DEVICE COMPRISING A DENSE POLYETHYLENE MEMBRANE, AN ELECTRONIC DEVICE COMPRISING THE ACOUSTIC DEVICE, A METHOD OF MAKING THE ACOUSTIC DEVICE, AND USE OF A DENSE POLYETHYLENE MEMBRANE IN AN ACOUSTIC DEVICEFIELD OF THE INVENTION

[0001] The present disclosure relates to an acoustic device comprising a dense polyethylene membrane. The present disclosure also relates to an electronic device comprising the acoustic device, a method of making the acoustic device and the use of a dense polyethylene membrane in an acoustic device.BACKGROUND

[0002] An electronic product such as a smartwatch includes an acoustic device such as a microphone. In the acoustic device, a sound transducer is held in a housing having an opening through which an acoustic wave passes. When water (including water vapour), dust (including fine dust) or other contaminants enter the housing through the opening during use of the electronic product, this may lead to malfunction of the acoustic device and undesirable noise.

[0003] Accordingly, the opening of the housing is usually covered by a membrane which can allow sound to propagate through and prevent ingress of water, dust, and / or other contaminants from the exterior to the interior of the housing. For a membrane to be functional during certain uses which apply external pressure to the membrane, the membrane needs to be able to allow sound to propagate through without significant sound transmission loss, but be strong enough to prevent the external pressure from rupturing or damaging the membrane. The membrane should also be elastic, so that it can return to (or close to) its original position once an external pressure is released. An external pressure may be applied to the acoustic device when it is in use, for example when it is submerged in water.

[0004] For a membrane to prevent ingress of water vapour and / or fine dust, the membrane is typically porous. However, when a non-porous membrane is used in an acoustic device, the thickness of the membrane becomes a more important factor for sound transmission because there are no interconnected pores for the sound to travel through. Typically, a thicker membrane will suffer more from sound transmission loss relative to a thinner membrane. This is particularly the case for dense (or non-porous) membranes.

[0005] PTFE membranes are currently used in acoustic devices to prevent the ingress of water, dust, and / or other contaminants. Typically, for non-porous PTFE membranes to be strong enough for practical use involving external pressure, a relatively thick membrane is required. However,the required thickness of the non-porous PTFE membranes adversely affects sound transmission and may result in significant sound transmission loss.

[0006] Thus, there is a need for improved membranes for acoustic devices which prevent ingress of water (including water vapour), dust (including fine dust) and other contaminants, wherein the membranes are strong to withstand external pressure, and do not result in significant sound transmission loss.

[0007] The present disclosure addresses the problems mentioned above.SUMMARY

[0008] In a first aspect, there is provided an acoustic device comprising: a housing comprising at least one opening in communication with the exterior of the acoustic device; a sound transducer, wherein the sound transducer is positioned within the housing; and a dense polyethylene membrane covering the at least one opening in communication with the exterior of the acoustic device, the dense polyethylene membrane having a first direction and a second direction, the second direction being orthogonal to the first direction, wherein: the dense polyethylene membrane has a thickness of from about 0.5 pm to about 3.0 pm, wherein the first and second directions are each orthogonal to the thickness direction; the dense polyethylene membrane has a mean mass per area of from about 0.4 g / m2to about 3 g / m2; the dense polyethylene membrane has a geometric mean 5-point modulus of at least about 1500 MPa; and the dense polyethylene membrane is formed from a polyethylene polymer comprising ultrahigh molecular weight polyethylene (UHMWPE).

[0009] It has been surprisingly discovered that a dense polyethylene membrane having (i) a thickness of from about 0.5 pm to about 3.0 pm, (ii) a mean mass per area of from about 0.4 g / m2to about 3 g / m2, and (iii) a geometric mean 5-point modulus of at least about 1500 MPa, which is formed from a polyethylene polymer comprising ultrahigh molecular weight polyethylene, has an ideal balance of properties for use in an acoustic device. Specifically, the use of the dense polyethylene membrane for covering an opening in an acoustic device successfully prevents ingress of water (including water vapour), dust (including fine dust) and other contaminants (herein collectively referred to as "contaminants") into the acoustic device. Moreover, the dense polyethylene membrane is strong and therefore withstands external pressure without damage and / or rupture. Also, the dense polyethylene membrane does not result in significant sound transmission loss.

[0010] Specifically, the dense polyethylene membrane having a thickness of from about 0.5 pm to about 3.0 pm and a mean mass per area of from about 0.4 g / m2to about 3 g / m2ensures that the membrane does not result in significant sound transmission loss. Typically, the thicker amembrane, the more sound transmission loss occurs relative to a thinner membrane. This is particularly the case for dense (or non-porous) membranes. The membrane having a thickness of from about 0.5 pm to about 3.0 pm is therefore beneficial for sound transmission. Likewise, the higher the mean mass per area of the membrane, typically the more sound transmission loss occurs relative to a lower mean mass per area of the membrane. Again, this is particularly the case for dense (or non-porous) membranes. The membrane having a mean mass per area of from about 0.4 g / m2to about 3 g / m2is therefore beneficial for sound transmission.

[0011] It has been found that the dense polyethylene membrane having a geometric mean 5-point modulus of at least about 1500 MPa results in good strength properties, and can be achieved for dense polyethylene membranes having a thickness of less than 3.0 pm and a mean mass per area of less than 3 g / m2. This geometric mean 5-point modulus ensures that the membrane can withstand external pressure.

[0012] Compared to the current state of the art membranes for acoustic devices, such as a PTFE membrane, the dense polyethylene membrane having the above-described properties has an improved balance of properties for use as an acoustic cover. Specifically, when the dense polyethylene membrane and a dense PTFE membrane, both having the same thickness, are compared, it is generally the case that the dense polyethylene membrane has improved properties as exhibited by the geometric mean 5-point modulus. The dense PTFE membrane would need to be thicker than the dense polyethylene membrane in order to obtain the same or comparable mechanical strength properties, which would adversely affect the sound transmission loss. Moreover, PTFE has a skeletal density that is roughly double that of polyethylene, and this further adversely affects the sound transmission loss in a dense membrane.

[0013] In one embodiment, the dense polyethylene membrane may have a mean 5-point modulus in the first in-plane direction of at least about 1500 MPa. In another embodiment, the dense polyethylene membrane may have a mean 5-point modulus in the second orthogonal in-plane direction of at least about 1000 MPa. The geometric mean 5-point modulus is the square root of the product of the mean 5-point modulus in the first direction and the mean 5-point modulus in the second direction. Thus, the mean 5-point modulus in the first direction and the mean 5-point modulus in the second direction are related to the geometric mean 5-point modulus, and the values described above result in excellent mechanical properties of the dense polyethylene membrane.

[0014] In one embodiment, the dense polyethylene membrane may have a mean matrix tensile strength (MTS) in the first in-plane direction of at least about 200 MPa. In another embodiment, the dense polyethylene membrane may have a mean matrix tensile strength (MTS) in the second orthogonal in-plane direction of at least about 150 MPa. In another embodiment, the dense polyethylene membrane may have a geometric mean matrix tensile strength (MTS) of at least about 175 MPa. The geometric mean matrix tensile strength is the square root of the product of the mean matrix tensile strength (MTS) in the first direction and the mean matrix tensile strength (MTS) in the second direction. Thus, the mean matrix tensile strength (MTS) in the first direction and the mean matrix tensile strength (MTS) in the second direction are related to the geometric mean matrix tensile strength (MTS), and the values described above result in excellent mechanical properties of the dense polyethylene membrane.

[0015] In one embodiment, the dense polyethylene membrane may have a moisture vapour permeability coefficient of from about 0.0001 g-mm / m2 / day to about 0.3 g-mm / m2 / day. In this case, the dense polyethylene membrane allows very little water vapour through, thereby protecting the acoustic device from water damage.

[0016] In one embodiment, the dense polyethylene membrane may have a density of at least about 0.88 g / cm3.

[0017] In one embodiment, the dense polyethylene membrane may have substantially no measurable airflow. This helps prevent contaminants entering the acoustic device.

[0018] In one embodiment, the acoustic device has an average delta transmission loss (dB) of less than about 3 dB , wherein the average delta transmission loss is calculated by subtracting the measured transmission loss before a pressure test from the measured transmission loss 24 hours after the pressure test, wherein the pressure test is a 1 bar open hole challenge and the sound frequency is 3 KHz.

[0019] In one embodiment, the dense polyethylene membrane may have a thickness of from about 0.7 pm to about 2.8 pm, optionally from about 0.8 pm to 2.4 pm. An excessively thin membrane may lack mechanical strength.

[0020] In one embodiment, the dense polyethylene membrane may have a mean mass per area of from about 0.6 g / m2to about 2.8 g / m2, or optionally from about 0.7 g / m2to about 2.4 g / m2.

[0021] In one embodiment, the acoustic device may further comprise a stiffener plate to provide support for the dense polyethylene membrane. The stiffener plate may be selected from a perforated metal plate, a woven fabric, a nonwoven fabric, a mesh, a net, a sponge, a foam and a porous body made of a metal or a resin. The function of the stiffener plate is to providemechanical support to the membrane when an external pressure is applied to the acoustic device. The stiffener plate may cover the at least one opening of the housing. The stiffener plate may be located between the dense polyethylene membrane and the sound transducer. The acoustic device may have an average delta transmission loss (dB) of less than about 3 dB, wherein average delta transmission loss is calculated by subtracting the measured transmission loss before a pressure test from the measured transmission loss 24 hours after the pressure test, wherein the pressure test is a 10 bar challenge (with stiffener plate) and the sound frequency is 3 KHz.

[0022] In one embodiment, the the acoustic device may further comprise a coating layer on a surface of the dense polyethylene membrane. The dense polyethylene membrane may be located between the coating layer and the sound transducer. Alternatively, the coating layer may be located between the dense polyethylene film and the sound transducer, or be co-located on both surfaces of the dense polyethylene film. The coating layer may comprise one or more of the group consisting of metal, carbon and an electronically conductive polymer. The coating layer may be an anti-static layer. The anti-static layer may comprise an anti-static component. The anti-static component may be selected from one or more of the group consisting of metal, carbon and an electronically conductive polymer.

[0023] In one embodiment, the dense polyethylene membrane may further comprise an additive. The additive may be selected from one or more of the group consisting of metal, carbon and an electronically conductive polymer. The additive may be within the dense polyethylene membrane. The additive may be an anti-static component. The anti-static component may be selected from one or more of the group consisting of metal, carbon and an electronically conductive polymer. In one embodiment, the sound transducer may be positioned within the housing such that the opening guides sound to the sound transducer.

[0024] In one embodiment, the ultrahigh molecular weight polyethylene polymer has an average molecular weight of 1,000,000 g / mol to 10,000,000 g / mol. Optionally, the ultrahigh molecular weight polyethylene polymer has an average molecular weight of 2,000,000 g / mol to 10,000,000 g / mol.

[0025] The process for preparing the dense polyethylene membrane is not particularly limited. In one embodiment, the dense polyethylene membrane may be prepared by the following process: dissolving a polyethylene polymer in a solvent to form a solution; shaping the solution into a tape at a temperature above the solution temperature of the polyethylene polymer; cooling the tape to a temperature below the solution temperature to achieve gelation of thetape; removing the solvent from the gelled tape; and biaxially stretching the gelled tape above the melt temperature to form the dense polyethylene membrane.

[0026] In one embodiment, the dense polyethylene membrane may be prepared by the following process: providing a paste comprising polyethylene polymer and a lubricant; shaping the paste into a tape; removing the lubricant from the tape to form a dry polyethylene tape; compressing the dry polyethylene tape below the melting temperature of the polyethylene polymer; and stretching the polyethylene tape in at least two directions at a temperature above the melt temperature of the polyethylene polymer to form a dense polyethylene membrane.

[0027] In one embodiment, the acoustic device may be a microphone or a speaker.

[0028] In a second aspect, an electronic device comprises the acoustic device of the present disclosure. The electronic device may be a smartwatch, a mobile phone, a buzzer, a voice recorder, or any other device in which the acoustic device may find utility. In one embodiment, a smartwatch comprises the acoustic device of the present disclosure.

[0029] In a third aspect, there is provided a method of making the acoustic device of the present disclosure, the method comprising the steps of:(i) providing a housing, a sound transducer and a dense polyethylene membrane, wherein the housing comprises at least one opening in communication with the exterior of the acoustic device;(ii) positioning the sound transducer within the housing; and(iii) covering the at least one opening of the housing in communication with the exterior of the acoustic device with the dense polyethylene membrane.

[0030] In one embodiment, the method of making the acoustic device may further comprise the steps of forming the dense polyethylene membrane by the processes described above.

[0031] In one embodiment, the method of making the acoustic device may further comprise the step of fixing the dense polyethylene membrane to the housing with, for example, an adhesive. Optionally, the method of making the acoustic device may further comprise the step of hermetically sealing the dense polyethylene membrane to the housing. This forms a watertight seal and therefore prevents contaminants from entering the acoustic device through the interface between the dense polyethylene membrane and the housing.

[0032] In one embodiment, the method of making the acoustic device may further comprise the step of providing a stiffener plate and positioning the stiffener plate to cover the at least one opening of the housing in communication with the exterior of the acoustic device, thereby providing support to the dense polyethylene membrane. In one embodiment, the densepolyethylene membrane is positioned between the opening of the housing and the stiffener plate.

[0033] In one embodiment of the method of making the acoustic device, the step of providing a dense polyethylene membrane may include providing a dense polyethylene membrane having a coating layer on a surface of the dense polyethylene membrane. In one embodiment, the dense polyethylene membrane is located between the coating layer and the sound transducer. In other embodiments, the coating layer may be located between the dense polyethylene film and the sound transducer, or may be co-located on both surfaces of the dense polyethylene film. The coating layer may be as described above. For instance the coating layer may an antistatic-layer, e.g. the anti-static layer may comprise an anti-static component. In embodiments, the anti-static layer may be located between the coating layer and the sound transducer, between the dense polyethylene film and the sound transducer, or may be colocated on both surfaces of the dense polyethylene film.

[0034] In one embodiment of the method of making the acoustic device, the step of providing a dense polyethylene membrane may include providing a dense polyethylene membrane comprising an additive. The additive may be as described above. The additive may be within the dense polyethylene membrane. For instance the additive may be an anti-static component.

[0035] In a fourth aspect, there is provided a use of the dense polyethylene membrane of the present disclosure in an acoustic device. The use of the dense polyethylene membrane may be directed to prevent ingress of water (including water vapour), dust (including fine dust) and other contaminants into the acoustic device by covering the opening in the housing.

[0036] The present disclosure also provides an acoustic device comprising: a housing comprising at least one opening in communication with the exterior of the acoustic device; a sound transducer, wherein the sound transducer is positioned within the housing; and a dense polyethylene membrane covering the at least one opening in communication with the exterior of the acoustic device, the dense polyethylene membrane having a first direction and a second direction, the second direction being orthogonal to the first direction, wherein: the dense polyethylene membrane has a thickness of from about 0.5 pm to about 7.0 pm, wherein the first and second directions are each orthogonal to the thickness direction; the dense polyethylene membrane has a mean mass per area of from about 0.4 g / m2to about 7 g / m2; the dense polyethylene membrane has a geometric mean 5-point modulus of at least about 1500 MPa; and the dense polyethylene membrane is formed from a polyethylene polymer comprising ultrahigh molecular weight polyethylene. The dense polyethylene membrane mayhave a thickness of from about 0.5 pm to about 6 pm, or from about 0.5 pm to about 5 pm, or from about 0.5 pm to about 4 pm.

[0037] The foregoing embodiments should not be read to limit or otherwise narrow the scope of any of the inventive concepts otherwise provided by the present disclosure. While multiple embodiments are disclosed, other embodiments will become apparent to those skilled in the art from the following description and drawings. Accordingly, the description and drawings are to be regarded as illustrative rather than restrictive.BRIEF DESCRIPTION OF THE FIGURES

[0038] Figure 1 (FIG. 1) shows a schematic representation of an acoustic device according to an embodiment of the present disclosure.

[0039] Figure 2 (FIG. 2) shows a schematic representation of the acoustic device of Figure 1, additionally comprising a perforated stiffener plate, according to an embodiment of the present disclosure.

[0040] Figure 3 (FIG. 3) shows a schematic representation of the acoustic device of Figure 1, additionally comprising an anti-static layer, according to an embodiment of the present disclosure.

[0041] Figure 4 (FIG. 4) shows a schematic representation of an example setup for a pressure test.

[0042] Figure 5 (FIG. 5) shows a scanning electron micrograph of a dense polyethylene membrane having a physical vapor deposited tantalum layer which can be used in an acoustic device of the present disclosure.

[0043] Figure 6 (FIG. 6) shows a plot of the acoustic transmission loss for ultrahigh molecular weight polyethylene having no tantalum layer (deposition time 0 s) and samples having tantalum layers deposited for 1, 2 and 5 s and an initial time point without a stiffener plate.

[0044] It should be noted that the accompanying figures referred to herein are not necessarily drawn to scale but may be exaggerated to illustrate various aspects of the present disclosure, and in that regard, the figures should not be construed as limiting.DETAILED DESCRIPTION

[0045] The present disclosure relates to an acoustic device comprising: a housing comprising at least one opening in communication with the exterior of the acoustic device; a sound transducer, wherein the sound transducer is positioned within the housing; and a dense polyethylene membrane covering the at least one opening in communication with the exterior of the acoustic device, the dense polyethylene membrane having a first direction and a second direction, the second direction being orthogonal to the first direction, wherein: the densepolyethylene membrane has a thickness of from about 0.5 pm to about 3.0 pm, wherein the first and second directions are each orthogonal to the thickness direction; the dense polyethylene membrane has a mean mass per area of from about 0.4 g / m2to about 3 g / m2; the dense polyethylene membrane has a geometric mean 5-point modulus of at least about 1500 MPa; and the dense polyethylene membrane is formed from a polyethylene polymer comprising ultrahigh molecular weight polyethylene.

[0046] As mentioned above, it been surprisingly discovered that such a dense polyethylene membrane has an ideal balance of properties for use in an acoustic device. Specifically, the use of the dense polyethylene membrane for covering an opening in an acoustic device successfully prevents ingress of water (including water vapour), dust (including fine dust) and other contaminants into the acoustic device. Moreover, the dense polyethylene membrane is strong and therefore withstands external pressure without damage and / or rupture. Also, the dense polyethylene membrane does not result in significant sound transmission loss.

[0047] [The components of the acoustic device]

[0048] The acoustic device comprises a housing, a sound transducer and a dense polyethylene membrane.

[0049] The housing is hollow and comprises an acoustic cavity, and the housing accommodates a sound transducer. The housing also has at least one opening in communication with the exterior of the acoustic device, through which sound passes and is received by the sound transducer. The sound passes through an acoustic cavity in the housing to reach the sound transducer.

[0050] The material the housing is made from is not particularly limited, and may be any suitable material known in the art such as a resin, a polymer, a metal or the like. The housing provides protection for the sound transducer from contaminants. Any suitable housing known in the art may be used in the present disclosure.

[0051] The sound transducer is not particularly limited, and its function may be to convert sound into electrical signals. Any suitable sound transducer known in the art may be used in the present disclosure.

[0052] The at least one opening of the housing in communication with the exterior of the acoustic device is covered by the dense polyethylene membrane. In one embodiment, the dense polyethylene membrane fully covers the at least one opening so as to prevent ingress of contaminants. The dense polyethylene membrane, in combination with the housing, therefore protects the sound transducer from contaminants. This helps to improve theperformance of the acoustic device, as contaminants affect the performance of the sound transducer.

[0053] The dense polyethylene membrane may be fixed to the housing so as to cover the at least one opening. The membrane may form a hermetic seal with the housing so as to cover the at least one opening. A hermetic seal ensures water and other contaminants cannot enter the acoustic device via the seal. The seal between the housing and the dense polyethylene membrane may be formed by a layer of adhesive. The adhesive is not particularly limited and any suitable adhesive known in the art may be used.

[0054] Figure 1 (FIG.l) depicts an example of an acoustic device (100) comprising a housing (110) having an opening (112) in communication with the exterior of the device (101), a sound transducer (120) and a dense polyethylene membrane (130) covering the opening. The dense polyethylene membrane fully covers the opening and is fixed by an adhesive (140) to the housing. The sound transducer (120) is positioned within the housing (114). In the embodiment depicted, the sound transducer (120) is supported on a device body (116) which is positioned within the housing.

[0055] The acoustic device may further comprise a stiffener plate to provide support for the polyethylene membrane. The stiffener plate may be selected from a perforated metal plate, a woven fabric, a nonwoven fabric, a mesh, a net, a sponge, a foam and a porous body made of a metal or a resin. The stiffener plate may be a perforated metal plate.

[0056] The function of the stiffener plate is to act as a support for the dense polyethylene membrane when an external pressure is applied to the acoustic device, which pushes the membrane towards the inside of the acoustic device or housing. Typically, the dense polyethylene membrane is positioned between the opening of the housing and the stiffener plate, such that when an external pressure is applied to the acoustic device, the dense polyethylene membrane deforms towards the inside of the housing and pushes against the stiffener plate. The stiffener plate therefore provides mechanical support for the membrane and prevents further deformation. The stiffener plate is not in contact with the dense polyethylene membrane in the absence of external pressure on the acoustic device. The stiffener plate may be separated from the dense polyethylene membrane by a distance being at least about 30 pm. For example, the distance may be from about 30 pm to about 100 pm, or about 30 pm to 70 pm, or about 50 pm.

[0057] The stiffener plate may be porous, or may contain holes or openings running through the thickness of the plate, such that the stiffener plate does not significantly affect soundtransmission. In one embodiment, there is little to no sound transmission loss caused by the stiffener plate.

[0058] An example of a stiffener plate in an acoustic device is provided in Figure 2 (FIG. 2). In Figure 2, the stiffener plate (210) is a perforated metal plate. As an external pressure is applied, the dense polyethylene membrane deforms towards the inside of the acoustic device and pushes against the stiffener plate. The stiffener plate therefore provides mechanical support to the dense polyethylene membrane.

[0059] A coating layer may be provided on a surface of the dense polyethylene membrane. The coating layer may comprise one or more of the group consisting of metal, carbon and electronically conductive polymer. Preferred metals may be aluminum or tantalum. Preferred carbon may be graphite, carbon nanotubes, graphene or carbon-black. Preferred electronically conductive polymer may be poly(3,4-ethylenedioxythiophene) polystyrene sulfonate (PEDOT:PSS).

[0060] The coating layer may improve one or both of the gas and moisture permeability of the dense polyethylene membrane e.g. by reducing the gas and / or moisture permeability of the membrane. Such coating layers may comprise metal, for instance be a layer of physical vapor deposited (PVD) metal, such as aluminum or tantalum. Such layers may have a thickness in the range of from 10 to 150 nanometers, preferably in the range of from 20 to 100 nanometers, such as a thickness of 20 nanometers or 35 nanometers. PVD layers may be deposited by known methods, such as those disclosed in "Metallization of polymers and composites: State- of-the-art approaches," Materials & Design, 221, (2022) 110958.

[0061] The dense polyethylene membrane may be located between the coating layer and the sound transducer. This orientation situates the coating layer facing the exterior of the device, with the dense polyethylene membrane facing the interior of the device. The coating layer may promote adhesion of the dense polyethylene membrane to the housing by the adhesive.

[0062] The coating layer may also improve the durability of the dense polyethylene membrane, for instance by reducing degradation by ultraviolet light. Such coating layers may comprise one or both of metal and carbon. Preferred metal and carbon may be of the types discussed above for the coating layer.

[0063] The coating layer may also improve the handling of the dense polyethylene membrane, for instance if the coating layer comprises an anti-static component. Thus, the dense polyethylene membrane may be a static dissipative membrane. The coating layer may therefore be an anti-static layer. Thus, the static dissipative membrane may comprise dense polyethylene membrane and anti-static layer. The anti-static layer may comprise an anti-static component. The anti-static component may be an electronically conductive component. The anti-static component may be selected from one or more of the group consisting of metal, carbon and electronically conductive polymer. Preferred metal, carbon and electronically conductive polymer may be of the types discussed above for the coating layer. The anti-static layer may have a thickness in the range of from 10 to 150 nanometers, preferably in the range of from 20 to 100 nanometers, such as 20 nanometers or 35 nanometers. The anti-static layer may form less than or equal to 35 wt.%, preferably less than or equal 25 wt.% by total weight of the static dissipative membrane i.e. the combined weight of the anti-static layer and dense polyethylene membrane. Maintaining the anti-static layer at less than or equal to 35 wt.% of the total weight of the static dissipative membrane ensures that the acoustic properties of the membrane are not substantially affected. The anti-static layer may be present in a range of from 1 to 35 wt.% by total weight of the static dissipative membrane or in a range of from 5 to 25 wt.% by total weight of the static dissipative membrane.

[0064] An additive may be incorporated into the dense polyethylene membrane e.g. into the bulk of the dense polyethylene membrane. The additive may be one or more of the group consisting of metal, carbon and electronically conductive polymer. The additive may be an anti-static component, such as an electrically conductive component. Thus, the dense polyethylene membrane may comprise polyethylene and an anti-static component. Thus, the dense polyethylene membrane may be a static dissipative membrane. The anti-static component may be selected from one or more of the group consisting of a metal, carbon and an electronically conductive polymer. Preferred metal, carbon and electronically conductive polymer may be of the types discussed above for the coating layer. The anti-static component may be present in an amount of less than or equal to 35 wt.%, by total weight of the dense polyethylene membrane e.g. anti-static component and polyethylene, such as in a range of from 1 to 35 wt.% by total weight of the dense polyethylene membrane or in a range of from 5 to 25 wt.% by total weight of the dense polyethylene membrane.

[0065] A static dissipative membrane has a lower surface resistivity compared to a dense polyethylene membrane which does not contain an anti-static component and / or have an anti-static layer on a surface thereof. The presence of the anti-static component and / or antistatic layer reduces electrostatic charging on the membrane.

[0066] Figure 3 (FIG. 3) illustrates an acoustic device (100) comprising a coating layer (150) on a surface of the dense polyethylene membrane (130). The dense polyethylene membrane (130) may be located between the coating layer (150) and the sound transducer (120). The dense polyethylene membrane may have opposing first and second surfaces. The coating layer maybe disposed on the first surface of the dense polyethylene membrane, which may face towards the exterior of the housing (114). The second surface of the dense polyethylene membrane may be disposed on the stiffener plate (210), if present, and may face the sound transducer (120). The coating layer (150) may be fixed to the housing (114) by adhesive (140) as discussed in the embodiment of Figure 1.

[0067] In some embodiments, the acoustic device is a microphone or a speaker. In one embodiment, the acoustic device is a microphone.

[0068] [Dense polyethylene membrane]

[0069] The dense polyethylene membrane covers the at least one opening in the housing. To function most effectively as a barrier for contaminants, the membrane should be non-porous. In the context of the present disclosure, the term "dense" refers to a polyethylene membrane that is non-porous or substantially non-porous, meaning that substantially no pore(s) is present that allows a first main surface of the membrane to be in fluid communication with a second main surface opposite the first surface. For example, a membrane in which the air permeability, when measured using the ATEQ. test described herein, between one main surface and the other main surface is below detectable levels is said to be a dense or non- porous membrane. A "dense" membrane in the context of the present invention may also mean that that membrane density is at least about 0.88 g / cm3.

[0070] The dense polyethylene membrane has a first direction and a second direction, the second direction being orthogonal to the first direction. The dense polyethylene membrane has a thickness of from about 0.5 pm to about 3.0 pm, wherein the first and second directions are each orthogonal to the thickness direction. A membrane thickness of from about 0.5 pm to about 3.0 pm is beneficial for sound transmission, because generally the thinner the membrane, the better the sound transmission through the membrane. For example, a given membrane having a thickness of 5 pm would generally have more sound transmission loss relative to an identical membrane differing only in that it has a thickness of less than about 3.0 pm.

[0071] The dense polyethylene membrane has a thickness of at least 0.5 pm. An excessively thin membrane has poor mechanical and strength properties.

[0072] In some embodiments, the dense polyethylene membrane may have a thickness of from about 0.6 pm to about 3.0 pm, or from about 0.7 pm to about 2.9 pm, or from about 0.7 pm to about 2.8 pm, or from about 0.7 pm to about 2.7 pm, or from about 0.7 pm to about 2.6 pm, or from about 0.7 pm to about 2.5 pm, or from about 0.8 pm to about 2.4 pm, or from about 0.8 pm to about 2.3 pm, or from about 0.8 pm to about 2.2 pm, or from about 0.8 pmto about 2.1 pm, or from about 0.8 pm to about 2.0 pm, or from about 0.8 pm to about 1.9 pm, or from about 0.8 pm to about 1.8 pm, or from about 0.8 pm to about 1.7 pm, or from about 0.9 pm to about 1.6 pm, or from about 0.9 pm to about 1.6 pm, or from about 1.0 pm to about 1.5 pm. Such a membrane thickness results in excellent sound transmission properties.

[0073] The membrane thickness is measured as indicated in the test methods described herein.

[0074] Also significant to sound transmission loss is the mean mass per area of the membrane. The dense polyethylene membrane has a mean mass per area of from about 0.4 g / m2to about 3 g / m2. A membrane mean mass per area of from about 0.4 g / m2to about 3 g / m2is beneficial for sound transmission, because generally the lower the mean mass per area of a membrane, the lower the sound transmission loss. For example, a membrane having a mean mass per area of 5 g / m2would generally have more sound transmission loss relative to an identical membrane differing only in that it has a mean mass per area of less than 3 g / m2.

[0075] In some embodiments, the dense polyethylene membrane may have a mean mass per area of from about 0.5 g / m2to about 3 g / m2, or from about 0.6 g / m2to about 2.9 g / m2, or from about 0.7 g / m2to about 2.8 g / m2, or from about 0.6 g / m2to about 2.7 g / m2, or from about 0.6 g / m2to about 2.6 g / m2, or from about 0.6 g / m2to about 2.5 g / m2, or from about 0.7 g / m2to about 2.4 g / m2, or from about 0.7 g / m2to about 2.3 g / m2, or from about 0.7 g / m2to about 2.2 g / m2, or from about 0.7 g / m2to about 2.1 g / m2, or from about 0.7 g / m2to about 2 g / m2, or from about 0.7 g / m2to about 1.9 g / m2, or from about 0.7 g / m2to about 1.8 g / m2, or from about 0.7 g / m2to about 1.7 g / m2, or from about 0.8 g / m2to about 1.6 g / m2, or from about 0.9 g / m2to about 1.5 g / m2. Such a membrane mean mass per area results in excellent sound transmission properties.

[0076] The mean mass per area of a membrane is measured as indicated in the test methods described herein. For a given polyethylene density, the mean mass per area is related to the thickness of the membrane.

[0077] The dense polyethylene membrane has a geometric mean 5-point modulus of at least about 1500 MPa. This ensures that the membrane has suitable strength properties to function effectively as an acoustic cover. A geometric mean 5-point modulus of at least about 1500 MPa ensures that the membrane does not deform excessively under external pressure. Specifically, the membrane is strong enough to withstand external pressure, such as the pressure experienced when submerged in water. A membrane having an excessively low geometric mean 5-point modulus would have poor mechanical and strength properties.

[0078] Moreover, the membrane should be elastic so that when the external pressure is released, the membrane may deform back to its original position or close to its original position, without being permanently stretched.

[0079] In some embodiments, the dense polyethylene membrane may have a geometric mean 5- point modulus of at least about 1550 MPa, or at least about 1600 MPa, or at least about 1700 MPa, or at least about 1800 MPa, or at least about 1900 MPa, or at least about 2000 MPa, or at least about 2100 MPa, or a least about 2200 MPa, or at least about 2300 MPa, or at least about 2400 MPa, or at least about 2500 MPa. The dense polyethylene membrane may have a geometric mean 5 point-modulus of from about 1500 MPa to about 5000 MPa, or from about 1550 MPa to about 5000 MPa, or from about 1600 MPa to about 4500 MPa, or from about 1700 MPa to about 4500 MPa, or from about 1800 MPa to about 4500 MPa, or from about 1900 MPa to about 4500 MPa, or from about 2000 MPa to about 4500 MPa, or from about 2100 MPa to about 4000 MPa, or from about 2200 MPa to about 4000 MPa, or from about 2300 MPa to about 4000 MPa.

[0080] The geometric mean 5-point modulus is defined as the square root of the product of the mean 5-point modulus in the first direction and the mean 5-point modulus in the second direction.5-point modulusfleo-ean 5- point modulus / irs.t directionx mean 5- point modulussecond directiOn

[0081] Thus, the mean 5-point modulus in the first direction and the mean 5-point modulus in the second direction are related to the geometric mean 5-point modulus.

[0082] In some embodiments, the dense polyethylene membrane may have a mean 5-point modulus in the first direction of at least about 1500 MPa, or at least about 1750 MPa, or at least about 2000 MPa, or at least about 2250 MPa, or at least about 2500 MPa, or at least about 2750 MPa, or at least about 3000 MPa, or from about 1500 MPa to about 4500 MPa, or from about 1750 MPa to about 4500 MPa, or from about 2000 MPa to about 4500 MPa, or from about 2250 MPa to about 4500 MPa , or from about 2500 MPa to about 4500 MPa.

[0083] In some embodiments, the dense polyethylene membrane may have a mean 5-point modulus in the second direction of at least about 1000 MPa, or at least about 1250 MPa, or at least about 1500 MPa, or at least about 2000 MPa, or from about 1000 MPa to about 3500 MPa, or from about 1250 MPa to about 3500 MPa, or from about 1500 MPa to about 3500 MPa, or from about 1750 MPa to about 3500 MPa , or from about 2000 MPa to about 3500 MPa.

[0084] The mean 5-point modulus for each direction is calculated as indicated in the test methods described herein.

[0085] The dense polyethylene membrane is formed from a polyethylene polymer comprising ultrahigh molecular weight polyethylene. In the context of the present disclosure, ultrahigh molecular weight polyethylene refers to polyethylene having an average molecular weight of about 1,000,000 g / mol to about 10,000,000 g / mol. The average molecular weight may refer to the viscosity-average molecular weight, calculated from the intrinsic viscosity, as discussed in for example Pure Appl. Chem. 2020; 92(9):1469-1483. In some embodiments, the ultrahigh molecular weight polyethylene polymer has an average molecular weight of about 1,500,000 to about 10,000,000 g / mol, or about 2,000,000 g / mol to about 10,000,000 g / mol, or about 4,000,000 g / mol to about 8,000,000 g / mol.

[0086] In some embodiments, the dense polyethylene membrane may have a mean matrix tensile strength (MTS) in the first direction of at least about 200 MPa, or from about 200 MPa to about 700 MPa, or from about 225 MPa to about 600 MPa, or from about 250 MPa to about 550 MPa.

[0087] In some embodiments, the dense polyethylene membrane may have a mean matrix tensile strength (MTS) in the second direction of at least about 150 MPa, or from about 150 MPa to about 600 MP, or from about 175 MPa to about 550 MPa, or from about 200 MPa to about 500 MPa.

[0088] In some embodiments, the dense polyethylene membrane may have a geometric mean matrix tensile strength (MTS) of at least about 175 MPa, or from about 175 MPa to about 600 MPa, or from about 200 MPa to about 550 MPa, or from about 200 MPa to about 500 MPa.

[0089] The geometric mean matrix tensile strength (MTS) = square root of the product of the mean MTS in the first direction and the mean MTS in the second direction.

[0090] The mean matrix tensile strength for each direction is calculated as indicated in the test methods described herein.

[0091] In some embodiments, the dense polyethylene membrane may have a moisture vapour permeability coefficient of from about 0.0001 g-mm / m2 / day to about 0.3 g-mm / m2 / day, or from about 0.0001 g-mm / m2 / day to about 0.2 g-mm / m2 / day, or from about 0.0001 g- mm / m2 / day to about 0.1 g-mm / m2 / day. In some embodiments, the dense polyethylene membrane is substantially water impermeable.

[0092] The moisture vapour permeability coefficient is measured as indicated in the test methods described herein.

[0093] In some embodiments, the dense polyethylene membrane may have a density of at least about 0.88 g / cm3, or at least about 0.89 g / cm3, or at least about 0.90 g / cm3, or at least about0.91 g / cm3, or at least about 0.92 g / cm3, or at least about 0.93 g / cm3, or at least about 0.94 g / cm3. In some embodiments, the dense polyethylene membrane may have a density of from about 0.88 g / cm3to about 1.0 g / cm3, or from about 0.88 g / cm3to about 0.98 g / cm3, or from about 0.88 g / cm3to about 0.96 g / cm3, or from about 0.89 g / cm3to about 0.95 g / cm3. In the context of the present disclosure, density refers to bulk density (as opposed to skeletal density).

[0094] In one embodiment, the dense polyethylene membrane may have substantially no measurable airflow. In one embodiment, the air permeability of the dense polyethylene membrane is substantially zero (or not detectable) when evaluated based on the ATEQ. test described herein, indicating that there is substantially no airflow through the membrane. This helps prevent contaminants entering the acoustic device, especially water vapour, thereby protecting the acoustic device from water damage. It is important to prevent water vapour entering the acoustic device because it may condense and cause the device to malfunction.

[0095] In some embodiments, the acoustic device may have an average delta transmission loss of less than about 3 dB, wherein the average delta transmission loss is calculated by subtracting the measured transmission loss before a pressure test from the measured transmission loss 24 hours after the pressure test, wherein the pressure test is a 1 bar open hole challenge for 30 minutes and the sound frequency is 3 KHz. The acoustic device may have an average delta transmission loss of less than about 2.1 dB, or less than about 2.0 dB, or less than about 1.9 dB, or less than about 1.5 dB, or less than about 1.0 dB .

[0096] The acoustic device may have an average delta transmission loss of less than about 3 dB when a stiffener plate is used in the acoustic device, wherein the average delta transmission loss is calculated by subtracting the measured transmission loss before a pressure test from the measured transmission loss 24 hours after the pressure test, wherein the pressure test is a 10 bar challenge for 15 minutes and the sound frequency is 3 KHz.

[0097] FIG. 4 illustrates an example setup for a pressure test. A pressure test can be performed by placing a sample membrane (300) between two rigid supports (302, 304). A pressure, either air or water, at a selected level can then be applied to the membrane, causing the membrane to deform into a dome shape (306). A stiffener plate may also be employed for the pressure test, located between the membrane (300) and the rigid support (302), but not in direct contact with the membrane when no pressure is applied. For example, there may be a separation distance of about 50 pm between the dense polyethylene membrane and the stiffener plate. The arrow indicates the direction of the pressure.

[0098] The average delta transmission loss (dB) is measured as indicated in the test methods described herein.

[0099] In one embodiment, the dense polyethylene membrane has a thickness of from about 0.7 pm to about 2.8 pm, a mean mass per area of from about 0.6 g / m2to about 2.8 g / m2, and a geometric 5-point modulus of at least about 1500 MPa.[000100] In another embodiment, the dense polyethylene membrane has a thickness of from about 0.8 pm to about 2.4 pm, a mean mass per area of from about 0.7 g / m2to about 2.4 g / m2, and a geometric 5-point modulus of at least 1500 MPa.[000101] In another embodiment, the dense polyethylene membrane has a thickness of from about 0.9 pm to about 1.6 pm, a mean mass per area of 0.8 g / m2to 1.6 g / m2, and a geometric 5-point modulus of at least about 1500 MPa.[000102] [Method of making the dense polyethylene membrane][000103] The method of making the dense polyethylene membrane is not particularly limited and any method known in the art may be used, as long as the membrane has the required properties. [000104] One method known in the art to produce porous polyethylene membranes is through a wet or gel process. In this process, polyethylene is mixed with a hydrocarbon liquid and other additives. This mixture is heated over the polymer melt and extruded into a sheet. This sheet can then be orientated biaxially before and / or after the hydrocarbon liquid is extracted, producing a microporous membrane. Various process details are known, such as those disclosed in US 5,248,461; US 4,873,034; US 5,051,183; and US 6,566,012; each of which are hereby incorporated-by-reference in their entirety. Additional discussion includes Casting and stretching of filled and unfilled UHMW-polyethylene films, Ir.F.H. Assinck, Centre for polymers and composites, Eindhoven University of Technology, Nov 1995 and Porous Biaxially, drawn UHMWPE Films, H.M. Fortuin, DSM Research BV, Department of Materials Technology - Fifth Int. Conf, of Environmental Ergonomics.[000105] The dense polyethylene membrane of the present disclosure may be made by a "gel process" for producing a dense polyethylene film, which is described in numerous documents such as US 4,948,544. For example, the dense polyethylene membrane may be formed by dissolving a polyethylene polymer in a solvent to form a solution, shaping the solution into a tape or sheet at a temperature above the solution temperature of the polyethylene polymer, cooling the tape or sheet to a temperature below the solution temperature to achieve gelation of the tape or sheet, removing the solvent from the gelled tape or sheet and biaxially stretching the gelled tape or sheet above the melt temperature to form the dense polyethylene membrane.[000106] Alternatively, the dense polyethylene membrane may be formed via a "paste-process", which involves processing of polyethylene polymers to make tapes or membranes that are subsequently subjected to processing conditions suitable for the formation of a dense membrane. Such processing conditions may include heated compression and / or biaxial stretching of the tape or membrane.[000107] The dense polyethylene membrane may be formed by (i) forming a polyethylene tape from a polyethylene polymer; (ii) compressing the polyethylene tape below the melting temperature of the polyethylene polymer; and (iii) stretching the polyethylene tape in at least two directions at a temperature above the melt temperature of the polyethylene polymer to form a dense polyethylene membrane. The polyethylene polymer may have an average molecular weight of about 1,000,000 g / mol to about 10,000,000 g / mol, the compression temperature may be from 120°C to 135°C, the compression pressure may be at least 1 MPa, and the stretching temperature may be from 140°C to 170°C. The polyethylene tape is formed by providing a paste comprising polyethylene polymer and a lubricant, shaping the paste into a tape, and removing the lubricant to form a dry polyethylene tape. For instance, polyethylene polymer particles may be initially mixed with a suitable lubricant (such as an isoparaffinic hydrocarbon) following the general process described in US 9,926,416 B2. The lubricated polymer particles may then be formed into a tape, which is then dried (to remove lubricant) prior to forming the dense polyethylene membrane using heated compression, biaxial stretching, or a combination thereof. The tape may be referred to as a sheet.[000108] The skilled person will appreciate that the exact conditions, process steps and amounts of each component will depend on the nature of the polyethylene polymer and the desired properties of the resulting dense polyethylene membrane.[000109] The dense polyethylene membrane is formed from a polyethylene polymer comprising ultrahigh molecular weight polyethylene. As discussed above, in the context of the present disclosure, ultrahigh molecular weight polyethylene refers to polyethylene having an average molecular weight of about 1,000,000 g / mol to about 10,000,000 g / mol. In some embodiments, the ultrahigh molecular weight polyethylene polymer has an average molecular weight of about 1,500,000 to about 10,000,000 g / mol, or about 2,000,000 g / mol to about 10,000,000 g / mol, or about 4,000,000 g / mol to about 8,000,000 g / mol.[000110] The ultrahigh molecular weight polyethylene polymer may be a homopolymer of ethylene or a copolymer of ethylene and at least one comonomer. Suitable copolymers include an alphaolefin or a cyclic olefin having 3 to 20 carbon atoms, such as 1-butene, 1-pentene, 1-hexene, 1-heptene, 1-octene, cyclohexene, and dienes with up to 20 carbon atoms. The comonomermay be present in the polyethylene copolymer in an amount of from 0.001 mol% to 10 mol%, or from 0.01 mol% to 5 mol%, or from 0.1 mol% to 1 mol%.[000111] The polyethylene polymer may also comprise a blend of ultrahigh molecular weight polyethylene and polyethylene having a relatively lower molecular weight, such as polyethylene having an average molecular weight of below about 1,000,000 g / mol.[000112] The dense polyethylene membrane may also be treated, for example to provide a coating thereon. For the avoidance of doubt, the membrane thickness, mean mass per area and geometric moduli, and the other properties described herein, refer to properties of the dense polyethylene membrane without the treatment or coating.[000113] [Method of making the acoustic device][000114] The present disclosure provides a method of making the acoustic device described herein, the method comprising the steps of: providing the housing, the sound transducer and the dense polyethylene membrane, wherein the housing comprises at least one opening in communication with the exterior of the acoustic device; positioning the sound transducer within the housing; and covering the at least one opening of the housing in communication with the exterior of the acoustic device with the polyethylene membrane.[000115] The method may further comprise the steps of forming the dense polyethylene membrane by the above described "gel process" or "paste process".[000116] In some embodiments, the method may further comprise the step of fixing the dense polyethylene membrane to the housing, for example by using an adhesive. In some embodiments, the method may further comprise the step of hermetically sealing the dense polyethylene membrane to the housing to provide a waterproof seal between the housing and the dense polyethylene membrane. In this way, the perimeter of the dense polyethylene membrane is sealed to the housing and covers the opening.[000117] In some embodiments, the method may further comprise the step of providing a stiffener plate and positioning the stiffener plate to cover the opening of the housing, such that the stiffener plate provides support to the dense polyethylene membrane when an external pressure is applied to the acoustic device. The stiffener plate may be the same as those described above. In one embodiment, the dense polyethylene membrane is positioned between the opening of the housing and the stiffener plate.[000118] [Use of the dense polyethylene membrane in an acoustic device][000119] The present disclosure provides a use of the dense polyethylene membrane described herein in an acoustic device. The dense polyethylene membrane is used to prevent ingress of water (including water vapour), dust (including fine dust) and other contaminants into the acousticdevice by covering the opening of the housing, thereby providing a barrier to said contaminants. This protects the sound transducer and, in combination with the strength and acoustic properties of the dense polyethylene membrane, therefore ensures excellent performance of the acoustic device.[000120] In one embodiment, the dense polyethylene membrane may be used as a cover for a microphone or speaker. In another embodiment, the dense polyethylene membrane may be used as a cover for a microphone.[000121] [Electronic devices containing the acoustic device][000122] An electronic device may contain the acoustic device of the present disclosure. The electronic device is not particularly limited and may include a smartwatch, mobile phone, digital camera, headphones, earphones, a voice recorder and the like. In one embodiment, the electronic device is a smartwatch.[000123] [Test methods][000124] These tests methods relate to the above description and the examples section below.[000125] Mass per area: samples were die cut to form circular sections of 5.64 cm radius (area = 100 cm2). Each sample was weighed using a Mettler Toledo ME104TE Analytical balance and the average of six samples was divided by the test area of 100 cm2and multiplied by 100 to calculate the mass per area in units of g / m2.[000126] Bulk density: using the thickness measured using the Mitutoyo Litematic thickness gage (see explanation below), the bulk density of the samples was calculated using the following formula:where: m = mass (g) r = circle cut radius (5.64 cm) t = thickness (cm).[000127] The bulk density therefore includes the pore spaces within the sample in the volume measurement.[000128] Skeletal density: is the ratio of the mass of solid material to the sum of the volumes of the solid material and closed (or blind) pores within the material as per the definition in ASTM D3766. Thus, the skeletal density of a solid is calculated by excluding all open pores but including internal (or blind) pore volume. The skeletal density can never be lower than the true bulk density calculated by the measurement of mass and volume directly if the thickness and mass of the polyethylene film are accurately known. The skeletal density of polyethylenewas assumed to be p (polymer) = 0.94 g / cc. The skeletal density of polyethylene may change with the ratio of amorphous to crystalline regions in the polyethylene, which can be a result of the process of preparing such polymers. The skeletal density of polyethylene films, including dense polyethylene membranes, may be measured by gas pycnometry. A gas pycnometry instrument such as Micrometrics AccuPyc II 1340 can measure the skeletal volume of a material by He gas displacement using the volume-pressure relationship of Boyle's Law.[000129] Airflow: the ATEQ airflow test typically measures laminar volumetric flow rates of air through membrane and film samples. We used this measurement to indicate that the polyethylene films were non-porous with respect to measurable airflow. Each film sample was clamped between two plates in a manner that seals an area of 2.99 cm2across the flow pathway. An ATEQ® (ATEQ Corp., Livonia, Ml) Premier D Compact Flow Tester was used to determine whether the airflow rate was below the lower detection of 0.5 L / hr of the instrument by challenging it with a differential air pressure of 1.2 kPa (12 mbar) across the film. The instrument was operated with a calibrated 30 L flow tube to confirm the airflow was non- detectable below the instrument detection limit of 0.5 L / hr. If no airflow was detected, the membrane was said to be non-porous.[000130] Thickness: the contact thickness of the membranes was measured using a Mitutoyo Litematic VL-50S motorized height gage (commercially available from Mitutoyo Corporation, Kawasaki, Japan). The optical measurement is made by gently placing the sample membrane on a polished flat granite block and lower the contact probe to apply a 1 gram force. The average of the twelve measurements was utilized.[000131] Transmission loss: transmission loss and phase angle testing were performed by the Impedance Tube Transfer Matrix Test ("ITTMT"), which is a modified version of ASTM-E2611- 09 - the standard test method for measuring normal incidence sound transmission loss and phase based on the 4 microphone transfer matrix method. All modifications to ASTM-E2611- 09 are set forth herein. The transfer matrix of the assembly was measured, and we use T12 element of the transfer matrix as the acoustic impedance value for all the assemblies described in the examples.[000132] An impedance tube was used to make measurements across a frequency range of 500 Hz to 20,000 Hz. The inner diameter of the tube was 8 mm. The impedance tube was designed in accordance with ASTM E1050-12 and ASTM E2611-09. A JBL 2426H compression driver was mounted at one end of the tube and powered by a Bruel and Kjaer Type 2735 amplifier connected to a 31-band ART 351 graphic equalizer. The measurement system used 4 Brueland Kjaer Type 4138 microphones connected to a 4 channel Bruel and Kjaer Type 3160-A-042 LAN-XI Frontend with a generator output. Data was acquired and processed using Bruel and Kjaer PULSE Labshop with Type 7758 Acoustic Material Testing Software, version 21.[000133] The sample assemblies that were tested had an inner diameter of 1.5 mm, which was smaller than the inner diameter of the impedance tube. A pair of conical adapters was therefore required in order to mount the sample assemblies. The convergent cone had an inlet diameter of 8 mm and an outlet diameter of 1.5 mm. The divergent cone had an inlet diameter of 1.5 mm and an outlet diameter of 8 mm.[000134] When using conical adapters, additional processing of the data was required to account for the converging geometry of the cones. Theoretical equations were derived to calculate the transfer matrices of the conical adapters and can be found in the literature (Hua, X. and Herrin, D., "Practical Considerations when using the Two-Load Method to Determine the Transmission Loss of Mufflers and Silencers," SAE Int. J. Passeng. Cars - Meeh. Syst. 6(2):1094- 1101, 2013 & Mechel, F. P. (2008). Formulas of Acoustics. New York, NY: Springer).[000135] Mean 5-point modulus: to determine the mean 5-point modulus, a sample polyethylene membrane was cut in the longitudinal and transverse directions using either an ASTM D638 Type V Die (D638) (e.g. for dog bone samples 3.5 inches in length) or an ASTM D412 Type F Die (D412F) (e.g. for dog bone samples 5 inches in length). Tensile load as a function of displacement was measured at a frequency of 50 Hz using an INSTRON® 5565 (Illinois Tool Works Inc., Norwood, MA) tensile test machine equipped with flat-faced grips and a 100 N load cell. The grip separation distance for ASTM D638V tests was set to 3.18 cm and using an ASTM defined gage length of 0.76 cm, a strain rate of 0.127 cm / s or 16.7 % / s was used. The grip separation distance for ASTM D412F tests was set to 8.26 cm and using an ASTM defined gage length of 5.89 cm, a strain rate of 0.847 cm / s or 14.4 % / s was used. After placing the sample in the grips, the sample was retracted 1.27 cm to obtain a baseline followed by a tensile test at the aforementioned strain rate. Three samples for each condition were tested individually in each orthogonal (e.g., longitudinal and transverse) direction. In each test, the maximum tensile modulus was determined using a maximum linear fit as further described below and their respective averages were reported.[000136] The maximum linear fit was determined by importing the raw data from the tensile test machine into a data analysis program. The tensile modulus was calculated by making a series of linear fits of stress versus strain for sequential groups of every five data points collected by the tensile test machine. The highest slope of any group of five data points is the 5-point modulus for that sample. Three samples in each orthogonal (e.g. longitudinal and transverse)direction were tested and their respective averages were reported as the mean 5 point modulus. The larger of the two mean 5-point moduli determined for the two orthogonal directions was assigned that of the first direction. The smaller of the two mean 5-point moduli determined for the two orthogonal directions was assigned that of the second direction. Different data acquisition rates, and different numbers of data points for calculation of the modulus may be used, so long as the regions of data for fitting slopes are substantially linear and substantially unaffected by noise in the measurement of both stress and strain.[000137] Matrix tensile strength: to determine the matrix tensile strength (MTS), a sample polyethylene membrane was cut in the longitudinal and transverse directions using either an ASTM D638 Type V Die (D638) or an ASTM D412 Type F Die (D412F). Tensile load as a function of displacement was measured using an INSTRON® 5565 (Illinois Tool Works Inc., Norwood, MA) tensile test machine equipped with flat-faced grips and a 100 N load cell. The grip separation distance for ASTM D638V tests was set to 3.18 cm and using an ASTM defined gage length of 0.76 cm, a strain rate of 0.127 cm / s or 16.7 % / s was used. The grip separation distance for ASTM D412F tests was set to 8.26 cm and using an ASTM defined gage length of 5.89 cm, a strain rate of 0.847 cm / s or 14.4 % / s was used. After placing the sample in the grips, the sample was retracted 1.27 cm to obtain a baseline followed by a tensile test at the aforementioned strain rate. Three samples for each condition were tested individually samples in each orthogonal (e.g., longitudinal and transverse) direction and their respective averages were reported.[000138] The ultimate tensile strength was measured by the Instron load cell and is defined as the maximum load reached during each test run divided by the cross-section area at the center of the die cut dogbone. Data was exported into a data analysis program. Three samples in each orthogonal (e.g. longitudinal and transverse) direction were tested and their respective averages were reported. The larger of the two average maximum tensile moduli determined for the two orthogonal directions was assigned that of the first direction. The smaller of the two average maximum tensile moduli determined for the two orthogonal directions was assigned that of the second direction.[000139] The matrix tensile strength (MTS) is used to communicate the tensile strength of a polymer making up a porous or non-porous article, and is calculated using the following formula:MTS — TS * p polymer / P bulk-Where TS = ultimate tensile strength from the uniaxial tensile testing;Pbuik = sample bulk density;Ppoiymer = theoretical skeletal density of PE, taken as 0.94 g / cm3Ppoiymer = theoretical skeletal density of PTFE, taken as 2.186 g / cm3[000140] Transmission loss testing before and after pressure testing: sample assemblies were subjected to the following Pressure Test procedure. The purpose of this test was to replicate the pressure exerted on a membrane assembly in a device that was submerged in a given depth of water for a given duration of time. A transmission loss was measured before the pressure test and then remeasured 24 hours after the pressure test. The change in transmission loss, due to the pressure test, was calculated by subtracting the pre-test transmission loss from the post-test transmission loss.[000141] Biaxial Pressure Test: To apply challenge pressure to samples of membranes, flat sheets of membrane were sandwiched between two aligned sheets of FR4 epoxy laminate, each having a 1.6 mm diameter orifice, and were adhered using a pressure sensitive adhesive (tesa® 4983). The entire assembly was held in place in a metal fixture with a metal top plate having a 1.6 mm orifice aligned with the orifices in the FR4 sheets, where the top plate was clamped down with screws. The metal fixture was connected to a pressure vessel containing air. The pressure vessel was connected to a control box with programmable features that enable pressure ramp and pressure control of air. The control box was programmed to ramp the incoming pressure at 0.5 psi per second ramp rate until a maximum gage pressure of 14.5 psi (1 bar) was reached. This target pressure (e.g., 14.5 psi) represents a 10-meter water immersion depth rating that is an industry standard. When testing at 14.5 psi, the samples were held at the target pressure for a 30-minute duration. Alternatively, a gage pressure of 145 psi (10 bar) was used, representing a 100-meter water immersion depth rating. When testing at 145 psi, the samples were tested for a duration of 15 minutes and were tested in conjunction with a stiffener plate.[000142] FIG. 4 illustrates an example setup for a pressure test. A "Pressure Test" can be performed by placing a sample membrane 100 between two rigid supports 102, 104. Pressurized air at a selected level can then be applied to the membrane. For example, the pressure test can include a 1 bar air pressure applied to the membrane 100 for a period of 30 minutes, or 10 bar air pressure applied to the membrane 100 for a period of 30 minutes in conjunction with the use of a stiffener plate. After the testing period is complete, the pressure is no longer applied and the membrane 100 is allowed to return to its original state.[000143] Moisture vapor permeability coefficient: Determination of the moisture vapor permeability coefficient of the materials was carried out following the ASTM method F-1249. The instrument used to test the moisture vapor permeation of the materials was a MOCON Permatran-W Model 3 / 34 G (Ametek MOCON Inc., Minneapolis, Minn.). The permeant used was 90% RH water vapor (55.3 mmHg), the carrier gas was 100% nitrogen, dry, at ambientpressure and the temperature at which the test was carried out was 40.0° C. Samples were cut and masked such that the testing area was approximately either 5.0 or 50 cm2, affixed in the instrument diffusion cell. Moisture vapor transmission rate, or MVTR, was reported by the instrument in g / m2 / day. The moisture vapor permeability coefficient of each sample was calculated by multiplying the moisture vapor transmission rate by the thickness of the test sample. Mean results of two or more samples are reported as g-mm / m2 / day.[000144] Sample assemblies and comparative sample assemblies described herein were prepared as follows:[000145] All example sample assemblies and comparative sample assemblies are composed of two adhesive-backed fiberglass sample carriers that are used to construct a sandwich containing the flat sheet membrane, referred to simply as fiberglass sample carriers from this point forward. The fiberglass sample carriers were prepared by applying a double-sided pressure sensitive adhesive (tesa® 4983) to one side of a fiberglass sheet (purchased commercially from McMaster-Carr, product # 1331T37). The fiberglass / adhesive sheets were then laser cut into coupons. An approximately 1.6mm diameter center aperture is fabricated and aligned with the inner bore of the impedance tube and corresponds to the active area of the sample to be measured.[000146] All example sample assemblies and comparative sample assemblies built for acoustic testing in a configuration including a stiffener plate are composed of one adhesive-backed fiberglass sample carrier and a 300 micron thick brass plate with an array of holes having a diameter between 150 to 200 microns with a percent open area of approximately 25% located within an approximate 1.5 mm aperture that are used to construct a sandwich containing the flat sheet membrane. The fiberglass sample carrier on one side was prepared identically to the paragraph above. A double-sided pressure sensitive adhesive (Nitto Denko® 5605BN) with an array of pre-cut holes including a 1.6 mm aperture aligned with the active area of the sample to be measured was applied to one side of the brass stiffener plate. The total thickness of the adhesive layer is roughly 50 microns and, hence, the membrane is separated from the stiffener plate by approximately 50 microns when it is under acoustic test. The roughly 1.6 mm diameter center aperture is aligned with the inner bore of the impedance tube and corresponds to the active area of the sample to be measured.[000147] A piece of membrane positioned and adhered in a four-sided rectangular cardboard frame is partially cut free from two adjacent sides of the frame to relieve residual tension and placed on a smooth and level surface so that the membrane is flat and free of any wrinkles. The adhesive release liner was removed from a pre-cut fiberglass sample carrier to expose theadhesive. With adhesive layer exposed, the sample carrier was gently placed onto the membrane and any excess membrane was cut away from the perimeter of the sample carrier. The sample carrier was then placed onto an alignment jig with membrane side facing up. The release liner was removed from a second fiberglass sample carrier and placed onto the alignment jig with adhesive side facing down, towards the membrane. Light (i.e., manual) pressure was applied to bring the bottom and top sample carriers together to form an assembly having one of the following stack ups: (1) fiberglass sample carrier / adhesive / membrane / adhesive / fiberglass sample carrier, or (2) fiberglass sample carrier / adhesive / membrane / adhesive / perforated brass stiffener plate.[000148] [Examples][000149] The present disclosure will be described in more detail with reference to Examples. The present disclosure is not limited to the following Examples.[000150] Example 1[000151] Powder preparation:[000152] 300 g of ultrahigh molecular weight polyethylene (UHMWPE) powder having a molecular weight of approximately 7,000,000 g / mol (Mitsui Chemicals Inc., made as described in WO2012053261) was placed in a 2-liter screw cap jar. 180 mL of an isoparaffinic hydrocarbon lubricant (ISOPAR™ V; ExxonMobil Chemical Company, Spring, Texas) was added and mixed at room temperature for 15 minutes at 30 rpm using a tumbler. The mixture was preheated to 60°C prior to calendering.[000153] Tape calender process:[000154] Calender rolls with a diameter of 20.3 cm were preheated to 121°C with the gap between the rolls set at 0.2 mm. The lubricated polymer was introduced into the gap with a feeder to produce a 15.2 cm wide continuous tape at a line speed of 2.0 m / min. The tape was opaque, flexible, and approximately 0.21 mm thick.[000155] Lubricant removal:[000156] The tape was run roll-to-roll through a large bath containing a low aromatic hydrocarbon solvent (ISOPAR™ G; ExxonMobil Chemical Company, Spring, Texas) to displace the Isopar V™ with Isopar™ G and subsequently dried at 50°C.[000157] Heated compression:[000158] After lubricant removal, the dried tape was re-calendered between 30.5 cm diameter rolls preheated to 130°C at a line speed of 0.3 mm / min with the gap between the rolls set at 0.09 mm. The resulting compressed tape was translucent and flexible.[000159] Biaxial stretching: 1[000160] Samples were cut from the tape and placed in a Karo IV biaxial expansion machine (commercially available from Bruckner Group GmbH, Siegsdorf, Germany) and simultaneously stretched according to the steps below:1. Preheat the sample at 145°C for 120 seconds2. At 145°C: 6. OX at 37.5 % / s in the calendered direction and 9. OX at 37.5 % / s in the transverse (perpendicular to the calender) direction.[000161] The properties of the resultant membrane are detailed in Table 1. The resultant membrane is non-porous and has an airflow of <0.5 L / hr at 12 mbar and 2.99 cm2. The matrix tensile strengths and mean 5-point moduli were calculated using an ASTM type D638V dog bone.[000162] Example 2[000163] A paste-processed ultra-high-molecular-weight polyethylene (UHMWPE) tape after heated compression identical to that described in Example 1 was treated as follows:[000164] Biaxial Stretching:[000165] Samples were cut from the tape and placed in a Karo IV biaxial expansion machine (commercially available from Bruckner Group GmbH, Siegsdorf, Germany) and simultaneously stretched according to the steps below:1. Preheat the sample at 145°C for 120 seconds2. At 145°C: 9.5X at 37.5 % / s in the calendered direction and 9.5X at 37.5 % / s in the transverse (perpendicular to the calender) direction.[000166] The properties of the resultant membrane are detailed in Table 1. The resultant membrane is non-porous and has an airflow of <0.5 L / hr at 12 mbar and 2.99 cm2. The matrix tensile strengths and mean 5-point moduli were calculated using an ASTM type D638V dog bone.[000167] Example 3[000168] A gel-processed ultra-high-molecular-weight polyethylene (UHMWPE) membrane with a mass per area of 2.44 g / m2, an airflow of 4.9 L / hr at 12 mbar and 2.99 cm2, a thickness of 9.6 pm, an ultimate tensile strength in a first direction of 76 MPa, an ultimate tensile strength in a second direction (orthogonal to the first direction) of 65 MPa was used as a precursor in this example. The starting resin used to make the membrane had a molecular weight of 4,300,000 g / mol, according to the supplier.[000169] The above described membrane was drawn in the longitudinal / machine direction between banks of rolls at a gap distance of 19 cm over a heated plate set to a temperature of 130°C at a run speed of 3.0 m / min. The speed ratio between the second bank of rolls and the first bank of rolls, and hence the expansion ratio was 2:1.[000170] The longitudinally drawn membrane was then drawn transversely at a temperature of approximately 145°C to a ratio of 3.2:1 at a strain rate of 3.7 % / s for a residence time of 3.5 min.[000171] The properties of the resultant membrane are detailed in Table 1. The resultant membrane is non-porous and has an airflow of <0.5 L / hr at 12 mbar and 2.99 cm2. The matrix tensile strengths and mean 5-point moduli were calculated using an ASTM type D412F dog bone.[000172] Example 4[000173] A gel-processed ultra-high-molecular-weight polyethylene (UHMWPE) membrane with a mass per area of 3.92 g / m2, an airflow of 3.3 L / hr at 12 mbar and 2.99 cm2, a thickness of 10.8 pm, an ultimate tensile strength in a first direction of 107 MPa, an ultimate tensile strength in a second direction (orthogonal to the first direction) of 85 MPa was used as a precursor in this example. The starting resin used to make the membrane had a molecular weight of 4,300,000 g / mol, according to the supplier.[000174] The above described membrane was drawn in the longitudinal / machine direction between banks of rolls at a gap distance of 36 cm over a heated plate set to a temperature of 130°C at a run speed of 4.6 m / min. The speed ratio between the second bank of rolls and the first bank of rolls, and hence the expansion ratio was 2:1.[000175] The longitudinally drawn membrane was then drawn transversely at a temperature of approximately 145°C to a ratio of 3.0:1 at a run speed of 2 m / min at a strain rate of 3.5 % / s for a residence time of 2.5 min. This was followed by a temperature treatment at 150°C for a residence time of 1.0 min while restrained.[000176] The properties of the resultant membrane are detailed in Table 1. The resultant membrane is non-porous and has an airflow of <0.5 L / hr at 12 mbar and 2.99 cm2. The matrix tensile strengths and mean 5-point moduli were calculated using an ASTM type D412F dog bone.[000177] Example 5[000178] A gel-processed ultra-high-molecular-weight polyethylene (UHMWPE) membrane identical to that described in Example 4 was treated as follows:[000179] The above described membrane was drawn in the longitudinal / machine direction between banks of rolls at a gap distance of 36 cm over a heated plate set to a temperature of 130°C at a run speed of 4.6 m / min. The speed ratio between the second bank of rolls and the first bank of rolls, and hence the expansion ratio was 2:1.[000180] The longitudinally drawn membrane was then drawn transversely at a temperature of approximately 145°C to a ratio of 3.35:1 at a run speed of 2 m / min at a strain rate of 3.9 % / sfor a residence time of 2.5 min. This was followed by a temperature treatment at 150°C for a residence time of 1.0 min while restrained.[000181] The properties of the resultant membrane are detailed in Table 1. The resultant membrane is non-porous and has an airflow of <0.5 L / hr at 12 mbar and 2.99 cm2. The matrix tensile strengths and mean 5-point moduli were calculated using an ASTM type D412F dog bone.[000182] Example 6[000183] Using a biaxial pantograph machine, the Karo IV (commercially available from Bruckner Group GmbH, Siegsdorf, Germany), the initial gel-processed membrane identical to the membrane used in Example 3 was heated to 150 °C for 60 seconds while restrained in both longitudinal and transverse directions. The sample was then drawn simultaneously in both directions at a rate of 0.7 % / sec at constant speed to a ratio of 1.7 by 1.7.[000184] The properties of the resultant membrane are detailed in Table 1. The resultant membrane is non-porous and has an airflow of <0.5 L / hr at 12 mbar and 2.99 cm2. The matrix tensile strengths and mean 5-point moduli were calculated using an ASTM type D638V dog bone.[000185] Example 7[000186] A gel-processed ultra-high-molecular-weight polyethylene (UHMWPE) membrane identical to that described in Example 3 was treated as follows.[000187] The above described membrane was drawn in the longitudinal / machine direction between banks of rolls at a gap distance of 19 cm over a heated plate set to a temperature of 130°C at a run speed of 3.0 m / min. The speed ratio between the second bank of rolls and the first bank of rolls, and hence the expansion ratio was 2.5:1.[000188] The longitudinally drawn membrane was then drawn transversely at a temperature of approximately 147°C to a ratio of 3.2:1 at a strain rate of 3.7 % / s for a residence time of 3.5 min.[000189] The properties of the resultant membrane are detailed in Table 1. The resultant membrane is non-porous and has an airflow of <0.5 L / hr at 12 mbar and 2.99 cm2. The matrix tensile strengths and mean 5-point moduli were calculated using an ASTM type D412F dog bone.[000190] Comparative Example 1[000191] Using the Karo IV biaxial pantograph machine, a 13 micron LDPE film (commercially available from Ace Hardware as Item # 11165, Mfr #626206) was heated to 85 °C for 60 seconds while restrained in both longitudinal and transverse directions with the diffuser plate in the off position. The sample was then drawn simultaneously in both directions at a rate of 0.7 % / sec at constant speed to a ratio of 1.4 by 1.4.[000192] The properties of the resultant membrane are detailed in Table 1. The resultant membrane is non-porous and has an airflow of <0.5 L / hr at 12 mbar and 2.99 cm2. The matrix tensile strengths and mean 5-point moduli were calculated using an ASTM type D412F dog bone.[000193] Comparative Example 2[000194] Using the Karo IV biaxial pantograph machine, the 13 micron commercial LDPE micron film identical to that used in Comparative Example 1 was heated to 115 °C for 60 seconds while restrained in both longitudinal and transverse directions with the diffuser plate in the off position. The sample was then drawn simultaneously in both directions at a rate of 0.7 % / sec at constant speed to a ratio of 1.8 by 1.8.[000195] The resultant membrane bifurcated into thin and thick striations. Following the removal of the sample, thickness and acoustic transmission loss measurements were made using samples selected exclusively from the thicker region of the membrane.[000196] The properties of the thicker region of the membrane are detailed in Table 1. The resultant membrane is non-porous and has an airflow of <0.5 L / hr at 12 mbar and 2.99 cm2. The matrix tensile strengths and mean 5-point moduli were calculated using an ASTM type D412F dog bone.[000197] Comparative Example 3[000198] A PTFE dense film was made in accordance with US7,521,010 B2. The properties of the resultant membrane are detailed in Table 1. The resultant membrane is non-porous and has an airflow of <0.5 L / hr at 12 mbar and 2.99 cm2. The matrix tensile strengths and mean 5- point moduli were calculated using an ASTM type D412F dog bone.* refers to calculated membrane thickness. The calculated film thickness (microns) is the mass per area of the sample (g / cm2) divided by the skeletal density of the sample (g / cc).[000199] Examples 1-7 represent membranes in accordance with the present disclosure. ComparativeExamples 1-3 represent membranes not in accordance with the present disclosure.[000200] Examples 1-7 each have higher geometric mean 5-point modulus than ComparativeExamples 1-3, and thus have a superior strength property, despite having a smaller membrane thickness and mean mass per area.[000201] Transmission loss tests:[000202] Samples assemblies containing the membranes of Examples 1-7 and comparative sample assemblies containing the membranes of comparative examples 1-3 were built in accordance with the above described method. The transmission loss and delta transmission loss for the membranes of Examples 1-7 and Comparative Examples 1-3 were tested in accordance with the above described test methods. The delta transmission loss @ 3kHz (dB), for a pressure test using 1 bar for 30 minutes, in an open hole challenge with no stiffener plate (as shown in FIG. 4), are reported in Table 2. The delta transmission loss @ 3kHz (dB), for a pressure test using 10 bar for 15 minutes, and a stiffener plate located between the membrane (300) and rigid support (102) but not in contact with the membrane when no pressure is applied, are also reported in Table 2. The separation gap between the stiffener plate and the dense polyethylene membrane is approximately 50 pm.[000203] The membranes of Examples 1-7 have a significantly lower initial transmission loss and delta transmission loss for both the 1 bar test and 10 bar test (with stiffener plate) than themembranes of Comparative Examples 1 and 3, and the membrane of comparative example 2 broke during testing at 10 bar. Thus, membranes of Examples 1-7 are more suited to an acoustic device.[000204] Thus, it is clear in view of the Examples that the dense polyethylene membranes prevent ingress of water (including water vapour), dust (including fine dust) and other contaminants into the acoustic device, that the dense polyethylene membranes are strong enough to withstand external pressure, and that the dense polyethylene membranes do not result in significant sound transmission loss.[000205] Example 8[000206] A gel-processed ultra-high-molecular-weight polyethylene (UHMWPE) membrane with a mass per area of 3.65 g / m2, an airflow of 2.5 L / hr at 12 mbar and 2.99 cm2, a thickness of 11.8 pm, an ultimate tensile strength in a first direction of 78.4 MPa, an ultimate tensile strength in a second direction (orthogonal to the first direction) of 63.3 MPa was used as a precursor in this example. The starting resin used to make the membrane had a molecular weight of 4,300,000 g / mol, according to the supplier.[000207] The above described membrane was drawn transversely at a temperature of approximately 135°C to a ratio of 1.9:1 at a run speed of 2 m / min at a strain rate of 1.6 % / s for a residence time of 2.5 min. This was followed by an additional transverse draw at a temperature of approximately 150°C to an additional ratio of 1.2:1 a run speed of 2 m / min at a strain rate of 0.8 % / s for a residence time of 0.5 min. This was followed by a temperature treatment at 150°C for a residence time of 0.5 min while restrained.[000208] The properties of the resultant membrane are detailed in Table 3. The resultant membrane is non-porous and has an airflow of <0.5 L / hr at 12 mbar and 2.99 cm2. The matrix tensile strengths and mean 5-point moduli were calculated using an ASTM type D412F dog bone.[000209] A Denton Vacuum Explore™-14 sputtering machine equipped with a Tantalum target, 99.95% pure, 3.00" diameter x 0.250" thick from Kurt J Lesker, krypton (99.9%) (Airgas) process gas and argon / oxygen mixture (with 2% O2) (Airgas) venting gas was used to form a physical vapor deposited layer of tantalum on the ultrahigh molecular weight polyethylene membrane by the following process. A sample of UHMWPE membrane with a Kapton backer was taped down on the sample stage of the sputtering machine by Kapton tape. Cathode 1 was used during the deposition, and was positioned at confocal setting, with the center of the target at about 9 cm above the sample stage. The following conditions were used: a chamber pressure of 60 mTorr, a Kr process gas flow rate of 40 standard cubic cm per minute, a power (DC) of 300 W and deposition times of Is, 2s, and 5 sec, respectively, to achieve the deposited Ta coating thickness on the film in the nanometer range.[000210] Figure 5 (FIG. 5) shows a scanning electron micrograph (SEM) of a cross-section of the UHMWPE having a tantalum coating appl by a 5 sec deposition time. The SEM was prepared by mounting surface samples directly on a double-sided carbon tape (Ted Pella, CA) applied to an SEM mount. Cross-sections were prepared with Gatan® I Ilion2 broad beam ion mill (Gatan, CA). The sample was coated with a thin layer of platinum with a Cressington® 208HR sputter coater (Cressington, UK) and SEM analysis was performed on a Hitachi® SU8230 field emission electron microscope (FESEM) (Hitachi, JP).[000211] The mean deposited tantalum layer thickness was 18 nm determined as the average of fourteen measurements. Assuming a density of tantalum of 16.65 g / cm3and a mass per area of UHMWPE of 1.4 g / m2, this corresponds to a mass per area of tantalum metal of 0.3 g / m2The presence of the tantalum layer results in a 21% increase in mass density over UHMWPE without the deposited tantalum layer.[000212] Figure 6 (FIG. 6) shows the acoustic transmission loss for UHMWPE having no tantalum layer (deposition time 0 s) and samples having tantalum layers deposited for 1, 2 and 5 s and an initial time point without a stiffener plate.[000213] An error band was constructed using the minimum and maximum of three replicate test coupons and measurements per condition. The range of each data curves for the four individual deposition conditions show that the initial acoustic transmission loss is essentially unaffected by the presence of up to approximately twenty nanometer thick tantalum layers.[000214] All ranges described herein are exemplary in nature and include any and all values in between. The terms "substantially," "approximately" and "about" used herein are interchangeable and refer to a measurement that includes the stated measurement and any measurements reasonably close to the stated measurement. Measurements that are reasonably close to thestated measurement deviate from the stated measurement by a reasonably small amount as understood and readily ascertained by individuals having ordinary skill in the relevant arts. Such deviations may be attributable to measurement error, differences in measurement and / or manufacturing equipment calibration, human error in reading and / or setting measurements, minor adjustments made to optimize performance and / or structural parameters in view of differences in measurements associated with other components, particular implementation scenarios, imprecise adjustment and / or manipulation of objects by a person or machine. In the event it is determined that individuals having ordinary skill in the relevant arts would not readily ascertain values for such reasonably small differences, the terms "about" and "approximately" can be understood to mean plus or minus 10% of the stated value.[000215] Throughout the description and claims, the terms take the meanings explicitly defined herein, unless the context clearly dictates otherwise.[000216] The phrases "in one embodiment", "in an embodiment" and "in some embodiments" etc. as used herein do not necessarily refer to the same embodiment(s), though they may. Furthermore, the phrases "in another embodiment" and "in some other embodiments" as used herein do not necessarily refer to a different embodiment, though they may. All embodiments of the disclosure are intended to be combinable.[000217] The terms "comprises" and "comprising" mean to include but not limited to, such that further features may be present. The terms may also mean to consist of.[000218] All references and test methods cited herein are incorporated by reference in their entireties.- END -

Claims

CLAIMS An acoustic device (100) comprising: a housing (110) comprising at least one opening (112) in communication with the exterior of the acoustic device; a sound transducer (120), wherein the sound transducer is positioned within the housing (114); and a dense polyethylene membrane (130) covering the at least one opening in communication with the exterior of the acoustic device, the dense polyethylene membrane having a first direction and a second direction, the second direction being orthogonal to the first direction, wherein: the dense polyethylene membrane has a thickness of from about 0.5 pm to about3.0 pm, wherein the first and second directions are each orthogonal to the thickness direction; the dense polyethylene membrane has a mean mass per area of from about 0.4 g / m2to about 3 g / m2; the dense polyethylene membrane has a geometric mean 5-point modulus of at least about 1500 MPa; and the dense polyethylene membrane is formed from a polyethylene polymer comprising ultrahigh molecular weight polyethylene. An acoustic device according to Claim 1, wherein the dense polyethylene membrane has a mean 5-point modulus in the first direction of at least about 1500 MPa. An acoustic device according to Claim 1 or Claim 2, wherein the dense polyethylene membrane has a mean 5-point modulus in the second direction of at least about 1000 MPa. An acoustic device according to any preceding claim, wherein the dense polyethylene membrane has a mean matrix tensile strength (MTS) in the first direction of at least about 200 MPa. An acoustic device according to any preceding claim, wherein the dense polyethylene membrane has a mean matrix tensile strength (MTS) in the second direction of at least about 150 MPa.An acoustic device according to any preceding claim, wherein the dense polyethylene membrane has a geometric mean matrix tensile strength (MTS) of at least about 175 MPa. An acoustic device according to any preceding claim, wherein the dense polyethylene membrane has a moisture vapour permeability coefficient of from about 0.0001 g- mm / m2 / day to about 0.3 g-mm / m2 / day. An acoustic device according to any preceding claim, wherein the dense polyethylene membrane has a density of at least about 0.88 g / cm3. An acoustic device according to any preceding claim, wherein the dense polyethylene membrane has substantially no measurable airflow. An acoustic device according to any preceding claim, wherein the acoustic device has an average delta transmission loss (dB) of less than about 3 dB , wherein the average delta transmission loss is calculated by subtracting the measured transmission loss before a pressure test from the measured transmission loss 24 hours after the pressure test, wherein the pressure test is a 1 bar open hole challenge and the sound frequency is 3 KHz. An acoustic device according to any preceding claim, wherein the dense polyethylene membrane has a thickness of from about 0.7 pm to about 2.8 pm, or optionally from about 0.8 pm to about 2.4 pm. An acoustic device according to any preceding claim, wherein the dense polyethylene membrane has a mean mass per area of from about 0.6 g / m2to about 2.8 g / m2, or optionally from about 0.7 g / m2to about 2.4 g / m2. An acoustic device according to any preceding claim, wherein the acoustic device further comprises a stiffener plate (210) to provide support for the polyethylene membrane. An acoustic device according to Claim 13, wherein the stiffener plate is selected from a perforated metal plate, a woven fabric, a nonwoven fabric, a mesh, a net, a sponge, a foam and a porous body made of a metal or a resin.An acoustic device according to Claim 13 or Claim 14, wherein the acoustic device has an average delta transmission loss (dB) of less than about 3 dB, wherein the delta transmission loss is calculated by subtracting the measured transmission loss before a pressure test from the measured transmission loss 24 hours after the pressure test, wherein the pressure test is a 10 bar challenge and the sound frequency is 3 KHz. An acoustic device according to any preceding claim, wherein the acoustic device further comprises a coating layer on a surface of the dense polyethylene membrane. An acoustic device according to Claim 16, wherein the dense polyethylene membrane is located between the coating layer and the sound transducer. An acoustic device according to Claim 16 or Claim 17, wherein the coating layer comprises an anti-static component. An acoustic device according to any preceding claim, wherein the dense polyethylene membrane further comprises an anti-static component within the dense polyethylene membrane. An acoustic device according to Claim 18 or Claim 19, wherein the anti-static component is selected from one or more of the group consisting of metal, carbon and an electronically conductive polymer. An acoustic device according to any preceding claim, wherein the sound transducer is positioned within the housing such that the opening guides sound to the sound transducer. An acoustic device according to any preceding claim, wherein the ultrahigh molecular weight polyethylene has an average molecular weight of from about 1,000,000 g / mol to about 10,000,000 g / mol, optionally from about 2,000,000 g / mol to about 10,000,000 g / mol. An acoustic device according to any preceding claim, wherein the dense polyethylene membrane is prepared by the following process: dissolving a polyethylene polymer in a solvent to form a solution; shaping the solution into a tape at a temperature above the solution temperature of the polyethylene polymer;cooling the tape to a temperature below the solution temperature to achieve gelation of the tape; removing the solvent from the gelled tape; and biaxially stretching the gelled tape above the melt temperature to form the dense polyethylene membrane. An acoustic device according to any of Claims 1-22, wherein the dense polyethylene membrane is prepared by the following process: providing a paste comprising polyethylene polymer and a lubricant; shaping the paste into a tape; removing the lubricant from the tape to form a dry polyethylene tape; compressing the dry polyethylene tape below the melting temperature of the polyethylene polymer; and stretching the polyethylene tape in at least two directions at a temperature above the melt temperature of the polyethylene polymer to form a dense polyethylene membrane. An acoustic device according to any preceding claim, wherein the acoustic device is a microphone or a speaker. An electronic device comprising an acoustic device as defined in any of Claims 1 to 25, optionally wherein the electronic device is a smartwatch. A method of making an acoustic device (100) as defined in any one of Claims 1-25, the method comprising the steps of:(i) providing a housing (110), a sound transducer (120) and a dense polyethylene membrane (130), wherein the housing comprises at least one opening (112) in communication with the exterior of the acoustic device;(ii) positioning the sound transducer within the housing (114); and(iii) covering the at least one opening of the housing in communication with the exterior of the acoustic device with the dense polyethylene membrane. A method according to Claim 27, further comprising the step of fixing the dense polyethylene membrane to the housing with an adhesive (140).A method according to Claim 27 or Claim 28, further comprising the step of hermetically sealing the dense polyethylene membrane to the housing. A method according to any one of Claims 27-29, further comprising the step of providing a stiffener plate (210) and positioning the stiffener plate to cover the at least one opening of the housing, thereby providing support to the dense polyethylene membrane. Use of a dense polyethylene membrane (130) in an acoustic device (100), wherein: the dense polyethylene membrane has a first direction and a second direction, the second direction being orthogonal to the first direction; the dense polyethylene membrane has a thickness of from about 0.5 pm to about 3.0 pm, wherein the first and second directions are each orthogonal to the thickness direction; the dense polyethylene membrane has a mean mass per area of from about 0.4 g / m2to about 3 g / m2; the dense polyethylene membrane has a geometric mean 5-point modulus of at least about 1500 MPa; and the dense polyethylene membrane is formed from a polyethylene polymer comprising ultrahigh molecular weight polyethylene. Use according to Claim 31, wherein the acoustic device comprises a housing (110) comprising at least one opening (112) in communication with the exterior of the acoustic device and a sound transducer (120), the sound transducer being positioned within the housing (114), and wherein the dense polyethylene membrane is used to cover the at least one opening of the housing to prevent ingress of water, dust and / or other contaminants.