Quartz crucible and method for improving roughness of inner surface of quartz crucible
The side wall of the quartz crucible is ground by a grinding mechanism to remove unmelted micro-particles, which solves the problems of uneven temperature and abnormal bud breakage caused by the inlay of unmelted particles, and improves the cleanliness of the inner wall of the crucible and production efficiency.
Patent Information
- Application Number
- PCT/CN2024/072104
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-03-30
- Filing Date
- 2024-01-12
- Publication Date
- 2024-10-03
AI Technical Summary
During the quartz crucible manufacturing process, unmelted quartz microparticles are embedded in the inner wall, causing temperature unevenness, affecting the melting effect and abnormal bud breakage during the drawing process of silicon single crystal.
The inner surface of the quartz crucible side wall is ground through a grinding mechanism to remove unmelted quartz micro-particles and increase the inner surface roughness. The grinding part is used to contact the crucible side wall and move slowly to remove micro-particles, and the grinding thickness is controlled within Within the range of 0.01mm to 1mm.
Effectively remove micro-particles from the inner wall of the quartz crucible, reduce the risk of abnormal bud breakage, improve the cleanliness of the inner wall of the crucible, reduce modification costs, and accelerate mass production progress.
Smart Images

Figure CN2024072104_03102024_PF_FP_ABST
Abstract
Description
Quartz crucible and method for improving inner surface roughness of quartz crucible
[0001] This application claims priority to the Chinese patent application filed with the China Patent Office on March 30, 2023, with application number 202310325820.7 and application name “A quartz crucible and a method for improving the inner surface roughness of a quartz crucible”, the entire contents of which are incorporated by reference into this application. Technical Field
[0002] The embodiments of the present application relate to, but are not limited to, the field of solar photovoltaic technology, and specifically relate to a quartz crucible and a method for improving the inner surface roughness of the quartz crucible. Background Art
[0003] During the manufacturing process of the quartz crucible used for crystal pulling, the quartz crucible is formed into a finished product in one step, leaving only a margin in height. After melting is completed, the reserved height above is cut to meet the required height requirements. Since the height of the quartz crucible mold must be higher than the height of the finished product, the quartz sand can be formed normally in the above-mentioned reserved space, but the position of the electrode column is relatively fixed. During the manufacturing process of the quartz crucible, the heat demand at the bottom is higher than that at the top, and the highest temperature area of the electrode column cannot rise to the upper edge of the crucible, otherwise it will result in a large amount of heat energy waste and affect the melting effect of the bottom of the crucible. Due to the above reasons, the temperature at the upper edge of the crucible is lower than that at the middle and lower parts during the melting process of the crucible, resulting in a large number of unmelted quartz microparticles. After the crucible is melted, there is a risk that these quartz microparticles will fall onto the inner surface of the crucible, causing the quartz microparticles to be embedded in the inner wall of the quartz crucible. During the single crystal pulling process, the microparticles embedded in the inner wall are at risk of falling off, increasing the risk of heterogeneous nucleation of silicon single crystals. Technical issues
[0004] The present application provides a quartz crucible and a method for improving the inner surface roughness of the quartz crucible. By using special equipment and a customized process, unmelted quartz microparticles on the inner wall of the quartz crucible are removed, thereby improving the use effect of the quartz crucible and reducing the abnormal breakage of the bud during the silicon single crystal pulling process. Technical Solutions
[0005] The following is a summary of the subject matter described in detail herein. This summary is not intended to limit the scope of the claims.
[0006] In a first aspect, a quartz crucible comprises: a crucible body, the crucible body comprising a crucible sidewall and a crucible bottom, the crucible bottom comprising a bottom and an arc transition portion, the arc transition portion being provided along a circumference of the bottom;
[0007] The side wall is arranged around the arc transition portion, and the outermost layer of the inner surface of the crucible side wall is provided with a ground layer, and the thickness of the ground layer ranges from 0.01 mm to 1 mm.
[0008] In a second aspect, the present application also discloses a method for improving the inner surface roughness of a quartz crucible, comprising the steps of grinding the inner surface of the crucible side wall by a grinding mechanism to obtain the quartz crucible.
[0009] Optionally, the step of grinding the inner surface of the crucible side wall by a grinding mechanism includes:
[0010] Placing a quartz crucible on the support seat of the grinding mechanism, and driving the quartz crucible to rotate via the support seat;
[0011] The grinding part on the grinding mechanism extends from an initial position into the quartz crucible, and the grinding part is adjusted to fit the side wall of the crucible;
[0012] After the grinding part is in contact with the side wall of the crucible, the support seat drives the quartz crucible to rotate, and the grinding part moves away from the quartz crucible at a preset speed until the grinding part is separated from the inner wall of the crucible, completing the grinding.
[0013] Optionally, the support seat includes: rollers and roller supports arranged in pairs, both ends of the rollers are sleeved on the roller supports, and the quartz crucible is driven to rotate by the pair of rollers;
[0014] The quartz crucible is arranged between a pair of rollers, and the rollers drive the quartz crucible to operate at a speed ranging from 10 rpm to 30 rpm.
[0015] Optionally, the front end of the grinding portion extends from an initial position into the junction of the arc transition portion in the quartz crucible and the side wall of the crucible.
[0016] Optionally, the hardness of the grinding portion is greater than the hardness of silicon dioxide.
[0017] Optionally, the grinding part is controlled to descend until it contacts the inner surface of the crucible side wall. After contact, the grinding part slowly moves away from the quartz crucible at a speed ranging from 0.5 mm / s to 5.0 mm / s, and the rotation speed of the grinding part is from 1000 rpm to 10000 rpm.
[0018] Optionally, the support seat is controlled to carry the quartz crucible upward until the grinding part contacts the inner surface of the crucible side wall. After contact, the grinding part slowly moves away from the quartz crucible at a speed ranging from 0.5 mm / s to 5.0 mm / s, and the rotation speed of the grinding part is from 1000 rpm to 10000 rpm.
[0019] In a third aspect, the present application further discloses a grinding mechanism, comprising:
[0020] A support seat is provided on one side of the base and is used to support and drive the quartz crucible to rotate;
[0021] a grinding portion, the grinding portion being disposed on the other side of the base and being used for grinding the inner surface of the crucible side wall of the quartz crucible;
[0022] A grinding part moving mechanism, wherein the grinding part is connected to the base through the grinding part moving mechanism and moves relative to the quartz crucible on the support seat through the grinding part moving mechanism.
[0023] Optionally, the support seat includes: rollers and roller supports arranged in pairs, both ends of the rollers are mounted on the roller supports, and the quartz crucible is driven to rotate by the pair of rollers.
[0024] Optionally, the grinding part includes: a grinding shaft and a grinding head sleeved on the grinding shaft.
[0025] Optionally, the grinding part moving mechanism includes: an X-direction moving module and a Z-direction moving module, wherein the movable end of the X-direction moving module is connected to the grinding part, and the side of the X-direction moving module facing away from the grinding part is connected to the Z-direction moving module;
[0026] The Z-direction moving module is connected to the X-direction moving module via a follower connection member and drives the X-direction moving module to move;
[0027] One end of the Z-direction moving module facing away from the X-direction moving module is arranged on the upper end surface of the base.
[0028] Optionally, the invention further comprises: a support base moving mechanism, wherein the support base is connected to the base via the support base moving mechanism;
[0029] The support seat moving mechanism includes: a jacking module, the jacking module is arranged on the lower end surface of the support seat, and the support seat is connected to the base through the jacking module. Beneficial effects
[0030] Compared to existing technologies, this treatment solution can be performed after the quartz crucible is finished. With just one additional step, microparticles on the inner crucible walls can be removed without modifying the melting equipment or changing the melting process, reducing modification costs and accelerating mass production. Without adjusting the traditional crucible manufacturing process, the innovative addition of an inner surface impurity removal process eliminates the risk of unmelted quartz microparticles falling off the crucible wall during use, improving crystal formation.
[0031] After using this process, the particles on the inner wall of the quartz crucible can be reduced by 85%-95%. The microparticles in the parts that have not been cleaned are tightly bonded to the inner wall, and the risk of falling off during operation is extremely small. This measure greatly improves the cleanliness of the inner wall of the quartz crucible, which is of great advantage in increasing output and reducing production costs. BRIEF DESCRIPTION OF THE DRAWINGS
[0032] FIG1 is a schematic diagram of the crucible structure according to an embodiment of the present invention;
[0033] FIG2 is a schematic structural diagram of a grinding mechanism according to an embodiment of the present invention;
[0034] FIG3 is a schematic structural diagram of a support base moving mechanism and a support base according to an embodiment of the present invention;
[0035] Figure numerals: 100, crucible body; 110, crucible side wall; 120, crucible bottom; 121, bottom; 122, arc transition part; 200, grinding structure; 210, support seat; 220, grinding part; 230, grinding part moving mechanism; 240, base; 250, support seat moving mechanism; 211, roller; 212, roller support; 221, grinding shaft; 222, grinding head; 231, X-axis moving module; 232, Z-axis moving module; 251, lifting module. Implementation Methods of the Application
[0036] The following will be combined with the drawings in the embodiments of the present application to clearly and completely describe the technical solutions in the embodiments of the present application. The described embodiments are only part of the embodiments of the present application, not all of the embodiments. Based on the embodiments in the present application, all other embodiments obtained by those skilled in the art without making creative efforts are within the scope of protection of this application.
[0037] The disclosure below provides many different embodiments or examples to realize the different structures of the present application. In order to simplify the disclosure of the present application, the components and settings of specific examples are described below. Of course, they are only examples, and the purpose is not to limit the present application.
[0038] In the first aspect, as shown in FIG1 , a quartz crucible is provided, comprising: a crucible body 100, wherein the crucible body 100 includes a crucible sidewall 110 and a crucible bottom 120, wherein the crucible bottom 120 includes a bottom 121 and an arcuate transition portion 122, wherein the arcuate transition portion 122 is provided circumferentially along the bottom 121; and a crucible sidewall 110 is provided around the arcuate transition portion 122, wherein the outermost layer of the inner surface of the crucible sidewall 110 is provided with a ground layer having a thickness ranging from 0.01 mm to 1 mm. Conventional quartz crucibles may contain a large number of unmelted quartz particles during the crystal pulling process. After the crucible is melted, these quartz particles may fall onto the inner surface of the crucible, resulting in the quartz particles being embedded in the inner wall of the quartz crucible. During single crystal pulling, microparticles embedded in the inner wall pose a risk of falling off, increasing the risk of heterogeneous nucleation of silicon single crystals. In this embodiment, the ground layer on the inner surface of the crucible sidewall 110 is polished to a thickness ranging from 0.01 mm to 1 mm, thereby controlling the surface roughness of the inner surface of the crucible sidewall 110 to 1 μm to 10 μm. This eliminates the fused quartz microparticles on the inner wall of the quartz crucible, improves the performance of the quartz crucible, reduces the occurrence of abnormal bud breakage during silicon single crystal pulling, and improves the quality of the pulled crystal.
[0039] In a second aspect, the present invention also discloses a method for increasing the roughness of the inner layer of a quartz crucible to produce the aforementioned quartz crucible. The inner surface of the crucible sidewall is ground by a grinding mechanism. This treatment scheme can be performed after the quartz crucible is finished. By adding only one processing step, the removal of microparticles from the inner wall of the crucible can be achieved. This method eliminates the need for modifying the melting equipment or changing the melting process, thereby reducing modification costs and accelerating mass production. Specifically, the method comprises the following steps:
[0040] S1: Place the quartz crucible on the support base of the grinding mechanism, and drive the quartz crucible to rotate through the support base. The support base includes: a pair of rollers and roller supports, both ends of the rollers are mounted on the roller supports. During operation, the quartz crucible is placed between the pair of rollers. Specifically, the side of the quartz crucible is placed between the pair of rollers, and the side walls of the quartz crucible are in contact with the rollers. The rollers are driven by a motor to rotate, thereby driving the quartz crucible to rotate. In this embodiment, the operating speed of the rollers driving the quartz crucible ranges from 10 rpm to 30 rpm, achieving linkage with the grinding unit.
[0041] S2: The grinding portion on the grinding mechanism extends from the initial position into the quartz crucible, and the grinding portion is adjusted to fit the side wall of the crucible; wherein, the front end of the grinding portion extends from the initial position into the junction of the arc transition portion and the side wall of the crucible in the quartz crucible, and the inner surface of the crucible side wall of the quartz crucible is ground to remove quartz microparticles on the surface; in this embodiment, the initial position of the grinding portion is any position outside the quartz crucible, and no further limitation is made here.
[0042] It can be imagined that in order to achieve grinding, the hardness of the grinding part is greater than the hardness of silicon dioxide. Specifically, the grinding part can be made of a material with a hardness greater than silicon dioxide or directly connected to a grinding head with a hardness greater than silicon dioxide to achieve the removal of microparticles on the inner surface of the crucible side wall; the material of the grinding part can be an alloy or non-alloy with a hardness greater than quartz; similarly, the shape of the grinding part is not limited to a cylindrical shape.
[0043] S3: When the grinding part contacts the side wall of the crucible, the support seat drives the quartz crucible to rotate, and the grinding part moves away from the quartz crucible at a preset speed until the grinding part is separated from the inner wall of the crucible, and the grinding is completed.
[0044] In step S3, the grinding part is controlled to descend until the grinding part contacts the inner surface of the crucible side wall. After contact, the grinding part slowly moves away from the quartz crucible at a speed ranging from 0.5 mm / s to 5.0 mm / s, and the rotation speed of the grinding part is 1000 rpm to 10000 rpm. During this process, the support seat drives the quartz crucible to rotate, and the grinding part moves away from the quartz crucible after the support seat drives the quartz crucible to rotate at least one circle. It can be imagined that in an optional embodiment, the grinding part rotates in the opposite direction to the quartz crucible. In this embodiment, the grinding part can be driven to move by the grinding part moving mechanism to achieve the purpose of lowering the grinding part until it contacts the inner surface of the crucible side wall.
[0045] In some alternative embodiments, the support seat can be controlled to carry the quartz crucible upward until the grinding part contacts the inner surface of the crucible side wall. After contact, the grinding part slowly moves away from the quartz crucible at a speed ranging from 0.5 mm / s to 5.0 mm / s, and the rotation speed of the grinding part is 1000 rpm to 10000 rpm, thereby achieving the removal of quartz microparticles on the inner surface of the crucible side wall.
[0046] On the third aspect, the embodiment of the present application also discloses a grinding mechanism, and the grinding structure 200 includes: a support seat 210, a grinding part 220 and a grinding part moving mechanism 230. The support seat 210 is arranged on one side of the base 240, and the grinding part 220 is arranged on the opposite side of the support seat 210 on the base 240. The grinding part 220 is connected to the base 240 through the grinding part moving mechanism 230. During the grinding process, the quartz crucible is placed on the support seat 210, and the quartz crucible is driven to rotate by the support seat 210. The grinding part moving mechanism 230 drives the grinding part 220 to move relative to the quartz crucible on the support seat 210, and combined with the rotation of the grinding part 220 itself, the inner surface of the crucible side wall of the quartz crucible is ground.
[0047] As shown in Figure 3, the support base 210 includes: rollers 211 and roller supports 212 arranged in pairs. Both ends of the rollers 211 are mounted on the roller supports 212. The quartz crucible is supported between the pair of rollers 211. Specifically, the side of the quartz crucible is placed between the pair of rollers, and the side walls of the quartz crucible are in contact with the rollers. The rollers are driven to rotate by a motor, thereby driving the quartz crucible to rotate. In this embodiment, the operating speed of the quartz crucible driven by the rollers is within the range of 10-30rpm, realizing linkage coordination with the grinding part.
[0048] As shown in Figure 2, the grinding part 220 includes: a grinding shaft 221 and a grinding head 222 mounted on the grinding shaft 221. The grinding shaft 221 is driven to rotate by an external motor and then drives the grinding head 222 to rotate. In this embodiment, in order to achieve grinding, the hardness of the grinding head 222 is greater than the hardness of silicon dioxide. Specifically, the grinding head 222 can be made of a material with a hardness greater than silicon dioxide or directly connected to a grinding head with a hardness greater than silicon dioxide to achieve the removal of microparticles on the inner surface of the crucible side wall. The material of the grinding head 222 can be an alloy or non-alloy with a hardness greater than quartz. Similarly, the shape of the grinding head 222 is not limited to a cylindrical shape.
[0049] As shown in Figure 2, the grinding section moving mechanism 230 includes: an X-direction moving module 231 and a Z-direction moving module 232. The movable end of the X-direction moving module 231 is connected to the external motor of the grinding section 220. The side of the X-direction moving module 231 facing away from the grinding section 220 is connected to the Z-direction moving module 232. The Z-direction moving module 232 is connected to the X-direction moving module 231 through a connecting piece and drives the X-direction moving module 231 to move. The end of the Z-direction moving module 232 facing away from the X-direction moving module 231 is arranged on the upper end surface of the base 240.
[0050] In this embodiment, the Z-direction moving module 232 adopts a Z-direction telescopic cylinder, and the movable end of the Z-direction moving module 232 is connected to the X-direction moving module 231 through a connecting piece. At the same time, the other end of the Z-direction moving module 232 is set on the upper end surface of the base 240 through a connecting frame, wherein the connecting frame is a frame structure that only plays a connecting role and is not further limited here.
[0051] In this embodiment, the X-moving module 231 utilizes an X-moving telescopic cylinder, with the grinding unit 220 connected to its movable end. The Z-moving module 232 drives the X-moving module 231 to perform linear motion in the height direction. Simultaneously, the X-moving module 231 drives the grinding unit 220 to perform linear motion toward or away from the quartz crucible. During this process, the position and height of the grinding unit can be adjusted, facilitating precise grinding operations. The connector serves only as a connection and is not specifically defined herein.
[0052] In some alternative embodiments, the grinding mechanism 200 further includes: a support seat moving mechanism 250, through which the support seat 210 is connected to the base 240; as shown in FIG3 , the support seat moving mechanism 250 includes: a lifting module 251, which is disposed on the lower end surface of the support seat 210 and through which the support seat 210 is connected to the base. The lifting module 251 may be, but is not limited to, a telescopic cylinder. The lifting module 251 includes a plurality of telescopic cylinders, the movable ends of which are connected to the lower end surface of the support seat 210. Specifically, the lower end surface of the connecting platform provided on the roller support 212 may be connected to the movable ends of the telescopic cylinders, and the other ends of the telescopic cylinders are connected to the upper end surface of the base 240. By providing the lifting module 251, the height of the quartz crucible can be adjusted, facilitating fine grinding operations.
[0053] The above is a detailed introduction to a quartz crucible and a method for improving the inner surface roughness of a quartz crucible provided by the present application. Specific examples are used herein to illustrate the principles and implementation methods of the present application. The description of the above embodiments is only used to help understand the method and core idea of the present application. At the same time, for those skilled in the art, according to the ideas of the present application, there may be changes in the specific implementation methods and application scopes. In summary, the content of this specification should not be understood as limiting the present application.
Claims
1. A quartz crucible, wherein: include: A crucible body, the crucible body comprising a crucible side wall and a crucible bottom, the crucible bottom comprising a bottom and an arc transition portion, the arc transition portion being arranged along the circumference of the bottom; The side wall is arranged around the arc transition portion, and the outermost layer of the inner surface of the crucible side wall is provided with a ground layer, and the thickness of the ground layer ranges from 0.01 mm to 1 mm.
2. A method for improving the inner surface roughness of a quartz crucible, wherein: The steps are: grinding the inner surface of the crucible side wall by a grinding mechanism to obtain the quartz crucible as claimed in claim 1.
3. A method for improving the inner surface roughness of a quartz crucible according to claim 2, wherein: The step of grinding the inner surface of the crucible side wall by a grinding mechanism comprises: Placing a quartz crucible on a support seat of the grinding mechanism, and driving the quartz crucible to rotate via the support seat; The grinding part on the grinding mechanism extends from an initial position into the quartz crucible, and the grinding part is adjusted to fit the side wall of the crucible; When the grinding part is in contact with the side wall of the crucible, the support seat drives the quartz crucible to rotate, and the grinding part moves away from the quartz crucible at a preset speed until the grinding part is separated from the inner wall of the crucible, thereby completing the grinding.
4. A method for improving the inner surface roughness of a quartz crucible according to claim 3, wherein: The support seat comprises: rollers and roller supports arranged in pairs, both ends of the rollers are mounted on the roller supports, and the quartz crucible is driven to rotate by the pair of rollers; the quartz crucible is arranged between the pair of rollers.
5. A method for improving the inner surface roughness of a quartz crucible according to claim 4, wherein: The roller drives the quartz crucible to run at a speed ranging from 10 rpm to 30 rpm.
6. A method for improving the inner surface roughness of a quartz crucible according to claim 3, wherein: The front end of the grinding part extends from an initial position into the junction of the arc transition part in the quartz crucible and the side wall of the crucible.
7. A method for improving the inner surface roughness of a quartz crucible according to claim 3, wherein: The hardness of the grinding portion is greater than the hardness of silicon dioxide.
8. A method for improving the inner surface roughness of a quartz crucible according to claim 3, wherein: The grinding part is controlled to descend until it contacts the inner surface of the crucible side wall. After the contact, the grinding part slowly moves away from the quartz crucible at a speed ranging from 0.5 mm / s to 5.0 mm / s, and the rotation speed of the grinding part is from 1000 rpm to 10000 rpm.
9. A method for improving the inner surface roughness of a quartz crucible according to claim 3, wherein: The support seat is controlled to carry the quartz crucible upward until the grinding part contacts the inner surface of the crucible side wall. After the contact, the grinding part slowly moves away from the quartz crucible at a speed ranging from 0.5 mm / s to 5.0 mm / s, and the rotation speed of the grinding part is from 1000 rpm to 10000 rpm.
10. A grinding mechanism, wherein: include: A support seat, which is arranged on one side of the base and is used to support and drive the quartz crucible to rotate; A grinding part, which is disposed on the other side of the base and is used to grind the inner surface of the crucible side wall of the quartz crucible; A grinding part moving mechanism, wherein the grinding part is connected to the base through the grinding part moving mechanism, and moves relative to the quartz crucible on the supporting seat through the grinding part moving mechanism.
11. A grinding mechanism according to claim 10, wherein: The support seat comprises: rollers and roller supports arranged in pairs, both ends of the rollers are mounted on the roller supports, and the quartz crucible is driven to rotate by the pair of rollers; The grinding part comprises: a grinding shaft and a grinding head sleeved on the grinding shaft; The grinding section moving mechanism comprises: an X-direction moving module and a Z-direction moving module, wherein the movable end of the X-direction moving module is connected to the grinding section, and the side of the X-direction moving module away from the grinding section is connected to the Z-direction moving module; the Z-direction moving module is connected to the X-direction moving module via a follower connecting member and drives the X-direction moving module to move; and one end of the Z-direction moving module away from the X-direction moving module is arranged on the upper end surface of the base.
12. A grinding mechanism according to claim 10, wherein: Also includes: A support seat moving mechanism, wherein the support seat is connected to the base via the support seat moving mechanism.
13. A grinding mechanism according to claim 12, wherein: The support seat moving mechanism comprises: a jacking module, the jacking module is arranged on the lower end surface of the support seat, and the support seat is connected to the base through the jacking module.
Citation Information
Patent Citations
Quartz crucible grinding machine tool
CN114161259A
Polishing device of quartz ceramic crucible for ingot casting of single crystal
CN115056092A
Crucible inner wall polishing equipment
CN115256193A
Quartz crucible grinding device
CN208681190U
Quartz crucible grinding device with long service life and low deformation rate
CN216967319U