Semiconductor layer sequence
The semiconductor layer sequence addresses inefficiencies in radiative recombination by using an electron barrier layer with a band gap peak and piezoelectric effect to restrict electron flow, improving the efficiency of light-emitting diodes and lasers.
Patent Information
- Application Number
- PCT/EP2024/053789
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-03-30
- Filing Date
- 2024-02-15
- Publication Date
- 2024-10-03
AI Technical Summary
Existing semiconductor layer sequences face inefficiencies in radiative recombination due to electron outflow from the active region, particularly at high electrical current densities, as electrons flow away without radiatively recombining, reducing the efficiency of light-emitting diodes and lasers.
Incorporating an electron barrier layer with a band gap peak on the side facing away from the active region, utilizing the piezoelectric effect to enhance the barrier effect for electrons while minimizing the impact on hole injection, by adjusting the band gap and valence band energies to restrict electron flow while allowing hole flow.
The electron barrier layer significantly improves the radiative recombination efficiency by effectively blocking electron outflow while maintaining hole injection, enhancing the performance of light-emitting diodes and lasers.
Smart Images

Figure EP2024053789_03102024_PF_FP_ABST
Abstract
Description
[0001] Description
[0002] SEMICONDUCTOR LAYER SEQUENCE
[0003] A semiconductor layer sequence is specified.
[0004] The aim is to provide a semiconductor layer sequence with an improved electron barrier layer. This object is achieved by a subject matter having the features of independent patent claim 1.
[0005] Advantageous embodiments and further developments of the semiconductor layer sequence are specified in the dependent claims.
[0006] According to one embodiment, the semiconductor layer sequence has a p-doped region and an n-doped region. The semiconductor layer sequence is preferably an epitaxial semiconductor layer sequence. In particular, the semiconductor layer sequence comprises a plurality of semiconductor layers which have been grown epitaxially, for example, on a growth substrate. For example, the p-doped region follows the n-doped region in a growth direction of the semiconductor layer sequence. The growth substrate can be detached from the semiconductor layer sequence. For example, the semiconductor layer sequence is arranged on a carrier, wherein the p-doped region or the n-doped region can face the carrier.
[0007] The semiconductor layer sequence comprises, for example, a II / IV compound semiconductor material or is formed from one or more II / IV compound semiconductor materials. III / V compound semiconductor materials comprise at least one element from the third main group, such as, for example, B, Al, Ga, In, and one element from the fifth main group, such as, for example, N, P, As. In particular, the term "III / V compound semiconductor material" encompasses the group of binary, ternary, or quaternary compounds which contain at least one element from the third main group and at least one element from the fifth main group.
[0008] Examples of III / V compound semiconductor materials are arsenide compound semiconductor materials from the material system aluminum indium gallium arsenide Al x In y Gai- x-y As , phosphide compound semiconductor materials from the material system aluminum indium gallium phosphide Al x Iny Gai- x-y P, as well as nitride compound semiconductor materials from the material system aluminum indium gallium nitride Al x In y Gai- x-y N, where 0 < x < 1, 0 < y < 1, and x+y < 1. The semiconductor layer sequence preferably comprises a nitride compound semiconductor material or consists of a nitride compound semiconductor material. For example, the semiconductor layer sequence comprises aluminum indium gallium nitride or consists of aluminum indium gallium nitride.
[0009] Such binary, ternary or quaternary compounds may also contain, for example, one or more dopants and additional components.
[0010] The p-doped region in particular comprises at least one p-dopant. The p-dopant is, for example, acceptor atoms which at least partially replace atoms of the II IV compound semiconductor material in the crystal lattice of the semiconductor layer sequence. An acceptor atom in particular has a lower valence than an atom of the II IV compound semiconductor material which is replaced by the acceptor atom. For example, the semiconductor layer sequence comprises aluminum indium gallium nitride, and the p-dopant comprises magnesium atoms or consists of magnesium atoms as acceptor atoms.
[0011] The n-doped region has at least one n-dopant. The n-dopant is, for example, donor atoms that at least partially replace atoms of the II IV compound semiconductor material in the crystal lattice of the semiconductor layer sequence. A donor atom has, in particular, a higher valence than an atom of the II IV compound semiconductor material that is replaced by the donor atom. For example, the semiconductor layer sequence has aluminum indium gallium nitride, and the n-dopant has silicon atoms or consists of silicon atoms as donor atoms.
[0012] According to a further embodiment, the semiconductor layer sequence has an active region which is designed to generate electromagnetic radiation and is arranged between the p-doped region and the n-doped region. In the active region, the electromagnetic radiation is generated in particular by radiative recombination of free charge carriers, for example by radiative recombination of electrons and holes. The free charge carriers are introduced into the active region, for example by applying an electrical voltage to the semiconductor layer sequence and the electrical current generated thereby. The active region emits, for example, electromagnetic radiation in a spectral range between infrared and ultraviolet radiation. The active region comprises in particular a pn junction which is designed, for example, as a quantum well structure or as a multiple quantum well structure.Here and in the following, any structure in which charge carriers experience a quantization of their energy states through spatial confinement is referred to as a "quantum well structure". The confinement of the charge carriers can occur in one, two, or three dimensions. For example, the active region comprises a plurality of quantum well layers with barrier layers arranged between them.
[0013] For example, the semiconductor layer sequence described here is part of an optoelectronic semiconductor chip. During operation of the semiconductor chip, an electrical operating current is converted into electromagnetic radiation in the active region of the semiconductor layer sequence. For example, the semiconductor chip is a light-emitting diode (LED for short), an edge-emitting laser diode, a VCSEL (vertical cavity surface emitting laser), or a PCSEL (photonic crystal surface emitting laser).
[0014] According to a further embodiment, the semiconductor layer sequence has an electron barrier layer on a side of the active region facing the p-doped region. The electron barrier layer is, for example, arranged completely or partially in the p-doped region. The electron barrier layer can also be arranged outside the p-doped region. For example, the electron barrier layer has a larger band gap than all other semiconductor layers in the active region and / or in the p-doped region of the semiconductor layer sequence. The electron barrier layer is designed, for example, to increase the efficiency or yield of radiative recombination in the active region. At high electrical current densities, free charge carriers can cross the active region and flow away unused without radiative recombination.In particular, the electron barrier layer reduces or hinders the outflow of electrons from the active region into the p-doped region, thereby improving the efficiency of radiative recombination.
[0015] According to a further embodiment of the semiconductor layer sequence, the band gap of the electron barrier layer is larger on a side facing away from the active region than on a side facing the active region. Here and below, the band gap refers in particular to a minimum energy separation between a valence band and a conduction band in a band structure of the semiconductor layer or a region of the semiconductor layer.
[0016] The features of the semiconductor layer sequence described here and below, for example the band gap, the valence band, the conduction band, as well as an energy of the valence band and an energy of the conduction band, are intrinsic features of the semiconductor layer sequence in thermodynamic equilibrium, for example at room temperature or at a designated operating temperature of the semiconductor layer sequence. Intrinsic features are in particular features that are not influenced and / or changed by an external factor. External factors are, for example, the application of an electric field to the semiconductor layer sequence, the application of a magnetic field to the semiconductor layer sequence, the application of a temperature gradient to the semiconductor layer sequence, and / or the action of pressure or other external forces on the semiconductor layer sequence.The features of the semiconductor layer sequence described here and below, in particular the band gap, the valence band, the conduction band, the energy of the valence band and / or the energy of the conduction band, apply in particular to the case that no external electric field and / or no external magnetic field is applied to the semiconductor layer sequence from the outside.
[0017] Here and in the following, the valence band refers to the energetically highest band completely occupied with electrons in the band structure of the semiconductor layer or of a region of the semiconductor layer in thermodynamic equilibrium at absolute zero temperature. In other words, a chemical potential in an electron distribution function is greater than a maximum energy of the valence band. The conduction band refers here and in the following to an energy band which lies energetically immediately above the valence band and is not occupied by electrons at absolute zero temperature. In other words, the chemical potential is smaller than the minimum energy of the conduction band. Here and in the following, free charge carriers are, for example, excited electrons in the conduction band and / or holes in the valence band, which contribute in particular to the electric current through the semiconductor layer sequence.Holes are, in particular, levels in the valence band that are unoccupied by electrons.
[0018] The band gap can change, for example, as a function of the growth direction of the semiconductor layer sequence if, for example, a material composition within a semiconductor layer and / or a material composition of the semiconductor layer sequence changes. For example, the band gap of the electron barrier layer has a band gap peak or spike on the side facing the p-doped region, which particularly effectively impedes the flow of electrons from the active region into the p-doped region.
[0019] According to a further embodiment of the semiconductor layer sequence, the energy of the valence band of the electron barrier layer on the side facing away from the active region is the same or higher than on the side facing the active region. Thus, for example, a hole flow from the p-doped region into the active region is advantageously not impeded, or impeded as little as possible, by the tip or spike in the band gap of the electron barrier layer.
[0020] The energy of the valence band of the electron barrier layer may also be slightly lower on the side facing away from the active region than on the side facing the active region. For example, the energy of the valence band of the electron barrier layer on the side facing away from the active region is at most 0.03 eV lower, preferably at most 0.01 eV lower than the energy of the valence band of the electron barrier layer on the side facing the active region. According to a preferred embodiment, the
[0021] Haiblei ter layer sequence:
[0022] - the p-doped region and the n-doped region,
[0023] - the active region, which is arranged to generate electromagnetic radiation and is arranged between the p-doped region and the n-doped region, and
[0024] - the electron barrier layer on the side of the active region facing the p-doped region, where
[0025] - the band gap of the electron barrier layer is larger on the side facing away from the active region than on the side facing the active region, and
[0026] - the energy of the valence band of the electron barrier layer on the side facing away from the active region is the same or higher than on the side facing the active region.
[0027] The semiconductor layer sequence described here is based, in particular, on the idea of providing a particularly efficient semiconductor layer sequence for generating electromagnetic radiation. This is achieved, for example, by the electron barrier layer, which particularly effectively restricts the flow of electrons from the active region into the p-doped region, while impeding the flow of holes from the p-doped region into the active region as little as possible.
[0028] For example, the larger the band gap of the electron barrier layer is compared to the band gap of an adjacent semiconductor layer of the active region, the more the outflow of electrons from the active region is hindered by the electron barrier layer. However, a large band gap of the electron barrier layer can also hinder the flow of holes from the p-doped region into the active region, which can, for example, reduce the efficiency of the light-emitting diode, edge-emitting laser diode, VCSEL or PCSEL and / or increase the voltage drop between the p-doped region and the n-doped region. It may therefore be necessary to find a compromise between the largest possible band gap for good electron blocking and, at the same time, the smallest possible band gap for minimal influence on hole injection into the active region.
[0029] In the present semiconductor layer sequence, in particular a band bending by a piezoelectric effect in conjunction with a band gap peak on the side of the electron barrier layer facing away from the active region is utilized in order to improve a barrier effect of the electron barrier layer for the electrons and to create as few disadvantages as possible for the hole flow.
[0030] II IV compound semiconductor materials often exhibit strains in the crystal lattice at boundaries between different semiconductor layers. Due to the piezoelectric effect, these strains can generate electric polarization charges and thus internal electric fields in the semiconductor layer sequence, which can result in, for example, bending or tilting of the energy bands, in particular the valence band and the conduction band. This piezoelectric effect is particularly pronounced in nitride compound semiconductor materials such as aluminum indium gallium nitride. For example, the piezoelectric effect increases the energies of the conduction band and the valence band of the electron barrier layer on the side facing the p-doped region and / or decreases them on the side facing the active region.
[0031] By forming an electron barrier layer with a band gap peak on the side facing away from the active region, the barrier effect for the electrons is increased in particular. Furthermore, by forming the band gap peak in such a way that the energy of the valence band in the region of the band gap peak is the same as or higher than on the side facing the active region, hole injection into the active region is in particular not hindered or is hindered as little as possible. In other words, the energy of the valence band in the region of the band gap peak is in particular the same as or higher than the energy of the valence band on the side of the electron barrier layer facing the active region, which energy is reduced by the piezoelectric effect.
[0032] According to a further embodiment of the semiconductor layer sequence, the band gap of the electron barrier layer on the side facing away from the active region is at least 0.02 electron volts larger, preferably at least 0.04 electron volts larger, or particularly preferably at least 0.06 electron volts larger, than on the side facing the active region.
[0033] For example, the electron barrier layer comprises aluminum indium gallium nitride and its aluminum content on the side facing away from the active region is at least one percentage point, preferably at least two percentage points, or particularly preferably at least three percentage points higher, than on the side facing the active region.
[0034] According to a further embodiment of the semiconductor layer sequence, the band gap of the electron barrier layer on the side facing away from the active region is at most 0.3 electron volts larger, preferably by at most 0.25 electron volts, or particularly preferably by at most 0.2 electron volts, than on the side facing the active region. For example, the electron barrier layer comprises aluminum indium gallium nitride, and its aluminum content on the side facing away from the active region is at most fifteen percentage points, preferably by at most twelve percentage points, or particularly preferably by at most nine percentage points higher, than on the side facing the active region.
[0035] According to a further embodiment of the semiconductor layer sequence, the band gap of the electron barrier layer decreases continuously toward the active region. For example, the aluminum content in the electron barrier layer decreases continuously toward the active region.
[0036] According to a further embodiment of the semiconductor layer sequence, the band gap of the electron barrier layer has a maximum between the side facing the active region and the side facing away from the active region. For example, the aluminum content of the electron barrier layer has a maximum between the side facing the active region and the side facing away from the active region. According to a further embodiment of the semiconductor layer sequence, the electron barrier layer comprises a first barrier layer and a second barrier layer, wherein the first barrier layer is arranged between the second barrier layer and the active region. For example, the first barrier layer and the second barrier layer directly adjoin one another. For example, the electron barrier layer is formed from the first barrier layer and the second barrier layer.
[0037] According to a further embodiment of the semiconductor layer sequence, the second barrier layer has a larger band gap than the first barrier layer. For example, the band gap peak is formed in the region of the second barrier layer, or the second barrier layer forms the band gap peak of the electron barrier layer.
[0038] According to a further embodiment, the semiconductor layer sequence comprises aluminum indium gallium nitride or consists of aluminum indium gallium nitride.
[0039] According to a further embodiment of the semiconductor layer sequence, the second barrier layer has a higher aluminum content than the first barrier layer.
[0040] According to a further embodiment of the semiconductor layer sequence, the aluminum content of the second barrier layer is between 1 percentage point and 15 percentage points higher, preferably between 2 percentage points and 12 percentage points higher, or particularly preferably between 3 percentage points and 9 percentage points higher, than the aluminum content of the first barrier layer. The aluminum content here and below is in particular an absolute aluminum content of the respective semiconductor layer. For example, for aluminum indium gallium nitride, an aluminum content of p percentage points corresponds to the material composition Al x In y Gai- x-y N with x = p / 100 and 0 < y < 1 - p / 100 .
[0041] According to a further embodiment of the semiconductor layer sequence, the aluminum content of the first barrier layer is at least 12 percentage points higher, preferably at least 15 percentage points higher, or particularly preferably at least 20 percentage points higher, than an aluminum content of a semiconductor layer which directly adjoins the electron barrier layer on the side facing the active region.
[0042] If the semiconductor layer immediately preceding the electron barrier layer in the growth direction comprises indium, an aluminum content of the electron barrier layer can be reduced according to the indium content. In other words, the increased aluminum content of the electron barrier layer can be adjusted based on the indium content. For example, the aluminum content of the electron barrier layer is reduced by the same value as the indium content of the preceding layer. In particular, the aluminum content of the electron barrier can be increased by 0.55 times the indium content of the preceding
[0043] layer. Furthermore, the electron barrier layer can also be made of aluminum indium nitride Al x Ini x N with 0 < x < 1, for example to reduce strain to gallium nitride GaN.
[0044] According to a further embodiment of the semiconductor layer sequence, the thickness of the second barrier layer is at most 5 nanometers, preferably at most 3 nanometers, or particularly preferably at most 1.5 nanometers. The thickness denotes a spatial extent of the respective semiconductor layer in the growth direction. The entire electron barrier layer has, for example, a thickness of between 3 nanometers and 50 nanometers, preferably between 4 nanometers and 30 nanometers, and particularly preferably between 5 nanometers and 15 nanometers.
[0045] According to a further embodiment of the semiconductor layer sequence, the band gap of the second barrier layer increases or decreases toward the active region. For example, the aluminum content of the second barrier layer increases or decreases toward the active region.
[0046] According to a further embodiment of the semiconductor layer sequence, the band gap in the first barrier layer and / or in the second barrier layer is constant or approximately constant. For example, the aluminum content in the first barrier layer and / or in the second barrier layer is constant or approximately constant.
[0047] According to a further embodiment, the
[0048] The semiconductor layer sequence additionally comprises a transition region on the side of the electron barrier layer facing away from the active region. For example, the transition region improves the barrier effect of the electron barrier layer. The transition region can comprise one or more semiconductor layers. For example, the transition region has a thickness of between 3 nanometers and 200 nanometers, preferably between 4 nanometers and 60 nanometers, and particularly preferably between 6 nanometers and 25 nanometers.
[0049] According to a further embodiment of the semiconductor layer sequence, a band gap in the transition region is larger than a band gap of a semiconductor layer which directly borders the transition region on the side of the transition region facing away from the active region.
[0050] According to a further embodiment of the semiconductor layer sequence, the band gap in the transition region is smaller than the band gap in the electron barrier layer. For example, the transition region is designed as a band gap ramp, wherein the band gap in the transition region increases continuously towards the electron barrier layer. In other words, the continuously increasing band gap in the transition region does not have any steps or abrupt changes, but rather increases steadily. In particular, the band bending in the electron barrier layer due to the piezoelectric effect can be adjusted by designing the band gap in the transition region, for example by selecting the aluminum content, in such a way that the effect of the band gap peak is improved. According to a further embodiment of the semiconductor layer sequence, the band gap in the transition region increases continuously towards the electron barrier layer.In other words, the band gap in the transition region exhibits no steps or abrupt changes. For example, the transition region comprises aluminum indium gallium nitride or consists of aluminum indium gallium nitride, with the aluminum content in the transition region continuously and / or steadily increasing toward the electron barrier layer.
[0051] According to a further embodiment of the semiconductor layer sequence, the transition region directly adjoins the electron barrier layer on the side of the electron barrier layer facing away from the active region.
[0052] According to a further embodiment of the semiconductor layer sequence, the transition region and the electron barrier layer comprise or consist of aluminum indium gallium nitride.
[0053] According to a further embodiment of the semiconductor layer sequence, the aluminum content of the transition region at the boundary to the electron barrier layer is between 30% and 100% inclusive, preferably between 50% and 90% inclusive, or particularly preferably between 60% and 80% inclusive of a maximum aluminum content in the electron barrier layer.
[0054] According to a further embodiment of the
[0055] In a semiconductor layer sequence, the transition region comprises a first transition layer and a second transition layer, the first transition layer being arranged between the second transition layer and the electron barrier layer. For example, the first transition layer and the second transition layer directly adjoin one another. The transition region may also have more than two semiconductor layers. For example, the transition region has three, four, or ten semiconductor layers.
[0056] According to a further embodiment of the semiconductor layer sequence, a band gap of the first transition layer is larger than a band gap of the second transition layer. For example, the aluminum content in the first transition layer is larger than in the second transition layer.
[0057] According to a further embodiment of the semiconductor layer sequence, the band gap of the first transition layer and / or the band gap of the second transition layer increases continuously toward the electron barrier layer. For example, the aluminum content in the first transition layer and / or the aluminum content of the second transition layer increases continuously toward the electron barrier layer. The band gap or the aluminum content of the first transition layer and / or the second transition layer can also be constant or approximately constant.
[0058] According to a further embodiment of the semiconductor layer sequence, a band gap of a semiconductor layer which directly borders the electron barrier layer on a side facing the active region is larger or smaller than a band gap of a semiconductor layer which directly borders the transition region on a side facing away from the active region. The band gap of the semiconductor layer which directly borders the electron barrier layer on the side facing the active region can, for example, also be the same size as the band gap of the semiconductor layer which directly borders the transition region on the side facing away from the active region.
[0059] According to a further embodiment of the semiconductor layer sequence, the electron barrier layer is arranged in the p-doped region. For example, the electron barrier layer is arranged entirely in the p-doped region. The electron barrier layer can also be arranged at a boundary of the p-doped region. For example, a concentration of the p-dopant within the electron barrier layer or at the edge of the electron barrier layer decreases by at least three orders of magnitude toward the active region.
[0060] According to a further embodiment of the semiconductor layer sequence, the concentration of the p-dopant in the electron barrier layer is constant or approximately constant.
[0061] According to a further embodiment of the semiconductor layer sequence, the concentration of the p-dopant in the electron barrier layer has a maximum. In other words, the concentration of the p-dopant in the electron barrier layer is, in particular, higher than in all other semiconductor layers of the semiconductor layer sequence that directly border the electron barrier layer. The concentration of the p-dopant can also be constant or approximately constant throughout the entire p-doped region, which includes, for example, the electron barrier layer.
[0062] According to a further embodiment of the semiconductor layer sequence, the concentration of the p-dopant on the side of the electron barrier layer facing away from the active region is at least 10%, preferably at least 25%, or particularly preferably at least 50% lower than the maximum concentration of the p-dopant in the electron barrier layer. This can, for example, reduce absorption losses of electromagnetic radiation generated in the active region. For example, the concentration of the p-dopant in the transition region continuously decreases in a direction away from the electron barrier layer until the concentration of the p-dopant on the side of the transition region facing away from the electron barrier layer is at least 10%, preferably at least 25%, or particularly preferably at least 50% lower than the maximum concentration of the p-dopant in the electron barrier layer.
[0063] According to a further embodiment of the semiconductor layer sequence, the concentration of the p-dopant decreases continuously from the electron barrier layer towards the active region.
[0064] According to a further embodiment of the semiconductor layer sequence, the concentration of the p-dopant at a distance of at most 30 nanometers, preferably of at most 10 nanometers, or particularly preferably of at most 5 nanometers from the electron barrier layer on the side of the active region is at most 10 17 / cm 3 , preferably no more than 10 16 / cm 3 In other words, the concentration of the p-dopant increases in a direction from the active region to the p-doped region before the band gap in the electron barrier layer increases. This can, for example, improve the injection efficiency of holes into the active region.
[0065] According to a further embodiment of the semiconductor layer sequence, the concentration of the p-dopant in the p-doped region and / or in the electron barrier layer is between 10 and 15 18 / cm 3 and including 10 20 / cm 3 , preferably between 6* 10 18 / cm 3 and including 6* 10 19 / cm 3 , or particularly preferably between 10 and 15 19 / cm 3 and including 3* 10 19 / cm 3 .
[0066] The concentration of the p-dopant or a doping profile in the p-doped region can also have further ramps and / or peaks in order, for example, to improve the in ection efficiency of holes and / or to reduce absorption losses.
[0067] Further advantageous embodiments and developments of the semiconductor layer sequence emerge from the exemplary embodiments described below in conjunction with the figures.
[0068] Figure 1 shows a schematic sectional view of a semiconductor layer sequence according to an embodiment. Figure 2 shows a schematic band diagram of a semiconductor layer sequence according to an embodiment.
[0069] Figure 3 shows a schematic representation of an output power of electromagnetic radiation which is generated by a semiconductor layer sequence according to an embodiment during operation.
[0070] Figures 4 to 13 show schematic representations of a band gap in semiconductor layer sequences according to various embodiments.
[0071] Figures 14 to 17 show schematic representations of a dopant concentration of a p-dopant in connection with a band gap in semiconductor layer sequences according to various embodiments.
[0072] Identical, similar, or functionally equivalent elements are provided with the same reference symbols in the figures. The figures and the relative sizes of the elements depicted in the figures are not to be considered to scale. Rather, individual elements, particularly layer thicknesses, may be exaggerated for clarity and / or clarity.
[0073] The semiconductor layer sequence according to the exemplary embodiment in Figure 1 has an n-doped region N, an active region A and a p-doped region P, which are arranged successively in the growth direction R. The growth direction R is a direction perpendicular to a main extension plane of semiconductor layers of the semiconductor layer sequence. The active region A is designed to convert an electric current I into electromagnetic radiation. The p-doped region P, the active region A and / or the n-doped region N can also overlap at least in places.
[0074] An electron barrier layer 1 is arranged on the side of the active region A facing the p-doped region P. Further semiconductor layers, for example cladding layers and / or spacer layers, can be arranged between the active region A and the electron barrier layer 1 and can have a thickness of between 50 nanometers and 500 nanometers, for example. The electron barrier layer 1 is arranged within the p-doped region P. However, the electron barrier layer 1 can also be arranged only partially within the p-doped region P or outside the p-doped region P. A band gap A of the electron barrier layer 1 is larger than the band gaps A of all the other semiconductor layers in the semiconductor layer sequence.
[0075] The electron barrier layer A has a region with a band gap peak As (see, for example, Figure 2), which is formed on a side of the electron barrier layer 1 facing away from the active region A. In the region of the band gap peak As, the band gap A of the electron barrier layer 1 is in particular larger than in other regions of the electron barrier layer 1. The band gap peak As is formed such that the energy E of the valence band VB in the region of the band gap peak As is at least as high as or higher than the energy E of the valence band VB on the side of the electron barrier layer 1 facing the active region A (see, for example, Figure 2). This can be achieved by exploiting a piezoelectric effect, which in particular reduces energies E of the conduction band LB and the valence band VB on the side facing the active region A and / or increases them on the side facing away from the active region A.By such a design of the electron barrier layer 1, the barrier effect for the electrons e- is advantageously increased by the band gap peak As, while the injection of holes h+ into the active region A is advantageously not or only slightly hindered by the band gap peak As.
[0076] A transition region 2 is arranged on the side of the electron barrier layer 1 facing away from the active region A. The transition region 2 is designed as a band gap ramp Ar, in which the band gap A increases toward the electron barrier layer 1. The transition region 2 allows the band bending in the electron barrier layer 1 to be adjusted such that the effect of the electron barrier layer 1 is improved.
[0077] Figure 2 shows a schematic representation of the energies E of a valence band VB and a conduction band LB of the semiconductor layer sequence 1 as a function of the growth direction R according to an exemplary embodiment of the semiconductor layer sequence. Figure 2 shows a section of the valence band VB and the conduction band LB in the electron barrier layer 1 and their immediate surroundings. In particular, the bands LB, VB in the active region A can have a more complex structure, for example due to a multi-quantum well structure with a series of well layers and barrier layers arranged therebetween, which have band gaps A of different sizes. The electron barrier layer 1 comprises a first barrier layer 11 and a second barrier layer 12, the band gap peak As being formed in the second barrier layer 12.In other words, the second barrier layer 12 has a larger band gap A than the first barrier layer 11 and is arranged on the side of the electron barrier layer 1 facing away from the active region A. Both the valence band VB and the conduction band LB are bent or tilted in the electron barrier layer 1 due to the piezoelectric effect such that the energies E of the bands LB, VB are reduced on the side facing the active region A and / or increased on the side facing away from the active region A. As a result, in particular the band gap peak As is energetically pulled upwards, whereby the barrier effect for the electrons e- is increased. Furthermore, a minimum energy of the valence band VB is not reduced by the band gap peak As compared to an electron barrier layer 1 without a band gap peak As.In other words, the energy E of the valence band VB in the region of the second barrier layer 12 is equal to or higher than the energy E of the valence band VB on the side of the electron barrier layer 1 facing the active region A, as indicated by the horizontal dashed line in Figure 2. Thus, the injection of holes h+ into the active region A is not hindered or is hindered as little as possible by the band gap peak As in the second barrier layer 12.
[0078] Figure 3 shows simulation results of an output power Pout of the electromagnetic radiation generated in the active region A of the semiconductor layer sequence during operation as a function of an electric current I. The first curve 31 shows the output power Pout of a semiconductor layer sequence with an electron barrier layer 1 without a band gap peak As according to one example. The second curve 32 shows the output power Pout of a semiconductor layer sequence with an electron barrier layer 1 with a band gap peak As according to one exemplary embodiment. The band gap peak As increases the output power Pout for a given electric current I. The efficiency of the semiconductor layer sequence is therefore also advantageously increased. The third curve 33 shows the output power Pout of a semiconductor layer sequence with an electron barrier layer 1 with a band gap peak As and a transition region 2 according to a further exemplary embodiment.Through the transition region 2, the output power Pout and thus the efficiency of the semiconductor layer sequence can be advantageously further increased.
[0079] Figure 4 shows a band gap A of a semiconductor layer sequence according to an exemplary embodiment as a function of the growth direction R. A section of the semiconductor layer sequence is shown, which includes the electron barrier layer 1 and its immediate surroundings. In particular, details of the configuration of the band gap A in the active region are not shown.
[0080] The electron barrier layer 1 comprises aluminum indium gallium nitride and includes a first barrier layer 11 and a second barrier layer 12 immediately following in the growth direction R. The band gap A in the first barrier layer 11 and in the second barrier layer 12 is in each case constant or approximately constant in the growth direction R. The second barrier layer 12 has a larger band gap A than the first barrier layer 11. The thickness d of the second barrier layer 12 in the growth direction R is at most 5 nanometers, preferably at most 3 nanometers and particularly preferably at most 1.5 nanometers.
[0081] The aluminum content of the first barrier layer 11 is at least 12 percentage points, preferably at least 15 percentage points, and particularly preferably at least 20 percentage points greater than the aluminum content of the semiconductor layer arranged immediately before in the growth direction R. The aluminum content of the second barrier layer 12 is between 1 percentage point and 15 percentage points, preferably between 2 percentage points and 12 percentage points, and particularly preferably between 3 percentage points and 9 percentage points higher than the aluminum content of the first barrier layer 11. Here, the aluminum content refers to an absolute aluminum content, i.e. an aluminum content of p percentage points in aluminum indium gallium arsenide corresponds to the material composition Al x In y Gai- x-yN with x = p / 100 , where the indium content y can, for example, take values between 0 and 1- p / 100 .
[0082] Figure 5 shows a band gap A of a semiconductor layer sequence according to another exemplary embodiment. In contrast to the exemplary embodiment described in connection with Figure 4, the band gap A within the second barrier layer 12 is not constant, but rather increases continuously, in particular linearly, toward the active region A.
[0083] Figure 6 shows a band gap A of a semiconductor layer sequence according to another exemplary embodiment. In contrast to the exemplary embodiment described in connection with Figure 4, the band gap A within the second barrier layer 12 is not constant, but decreases continuously, in particular linearly, toward the active region A.
[0084] Figure 7 shows a band gap A of a semiconductor layer sequence according to a further exemplary embodiment. In contrast to the exemplary embodiment described in connection with Figure 4, the electron barrier layer 1 comprises only a single semiconductor layer, the band gap A of which decreases linearly toward the active region A. The band gap A can also decrease nonlinearly within the electron barrier layer 1.
[0085] Figure 8 shows a band gap A of a semiconductor layer sequence according to a further exemplary embodiment. In comparison to the exemplary embodiment described in connection with Figure 4, the semiconductor layer sequence additionally comprises a transition region 2 which directly adjoins the electron barrier layer 1 in the growth direction R. The transition region 2 is designed as a band gap ramp Ar, wherein the band gap A increases linearly in the direction of the electron barrier layer 1. The band gap can also increase non-linearly in the transition region 2.
[0086] The electron barrier layer 1 and the transition region 2 comprise aluminum indium gallium nitride. At the boundary to the electron barrier layer 1, the aluminum content of the transition region 2 is between 30% and 100% inclusive, preferably between 50% and 90% inclusive, and particularly preferably between 60% and 80% inclusive of the aluminum content of the second barrier layer 12. The electron barrier layer 1 can also be produced according to the method described in connection with Figures 5 to 7.
[0087] Be designed from examples.
[0088] Figure 9 shows a band gap A of a semiconductor layer sequence according to a further exemplary embodiment. In contrast to the exemplary embodiment described in connection with Figure 8, the band gap A does not increase continuously within the transition region 2, but has two steps. The band gap A can also have more than two steps in the transition region 2. In other words, the transition region 2 comprises a first transition layer 21 and a second transition layer 22, each of which has a constant, different band gap A. The first transition layer 21 borders directly on the electron barrier layer 1 and has a larger band gap A than the second transition layer 22.
[0089] Figure 10 shows a band gap A of a semiconductor layer sequence according to a further exemplary embodiment. In contrast to the exemplary embodiment described in connection with Figure 8, the band gap A within the transition region 2 does not increase continuously, but is constant or approximately constant. The band gap A in the transition region 2 is smaller than the band gap A in the electron barrier layer 1 and larger than the band gap A of a semiconductor layer immediately following the transition region 2 in the growth direction R.
[0090] Figure 11 shows a band gap A of a semiconductor layer sequence according to another exemplary embodiment. In contrast to the exemplary embodiment described in connection with Figure 8, the band gap A does not increase continuously within the transition region, but rather has a region with a constant band gap A in the center of the transition layer.
[0091] Figure 12 shows a band gap A of a semiconductor layer sequence according to a further exemplary embodiment. In contrast to the exemplary embodiment described in connection with Figure 9, the band gap A within the first transition layer 21 is not constant, but increases continuously in the direction of the electron barrier layer 1. Furthermore, a band gap A of a semiconductor layer immediately following the transition region 2 in the growth direction R is larger than the band gap A of a semiconductor layer arranged immediately in front of the electron barrier layer 1 in the growth direction R.
[0092] Figure 13 shows a band gap A of a semiconductor layer sequence according to a further exemplary embodiment. In contrast to the exemplary embodiment described in connection with Figure 8, the band gap A of a semiconductor layer immediately following the transition region 2 in the growth direction R is smaller than the band gap A of a semiconductor layer arranged immediately before the electron barrier layer 1 in the growth direction R.
[0093] Figure 14 shows a band gap A of a semiconductor layer sequence according to an exemplary embodiment, together with a concentration C of a p-dopant as a function of the growth direction R. A section of the semiconductor layer sequence is shown, which includes the electron barrier layer 1 and its immediate surroundings. In particular, details of the configuration of the band gap A in the active region A are not shown.
[0094] The design of the band gap A of the embodiment shown in Figure 14 corresponds to the embodiment described in connection with Figure 8. The band gap A can, for example, also be designed according to one of the embodiments shown in connection with Figures 4 to 7 or 9 to 13.
[0095] The semiconductor layer sequence comprises aluminum indium gallium nitride and p-dopant comprises magnesium. The concentration C of the p-dopant is constant or approximately constant within the p-doped region P. Within the p-doped region P, the concentration C of the p-dopant is between 10 and 15 inclusive. 18 / cm 3 and including 10 20 / cm 3 , preferably between 6* 10 18 / cm 3 and including 6* 10 19 / cm 3 , or particularly preferably between 10 and 15 19 / cm 3and including 3* 10 19 / cm 3 . The electron barrier layer 1 is arranged within the p-doped region P at the edge of the p-doped region P in such a way that the concentration C of the p-dopant decreases together with the band gap A of the electron barrier layer 1 on the side facing the active region A. For example, the concentration C of the p-dopant in the active region A is at least three orders of magnitude smaller than in the p-doped region P.
[0096] Figure 15 shows a band gap A of a semiconductor layer sequence together with a concentration C of a p-dopant according to another exemplary embodiment. In contrast to the exemplary embodiment described in connection with Figure 14, the electron barrier layer 1 is only partially arranged in the p-doped region P. In other words, the concentration C of the p-dopant already drops sharply within the electron barrier layer 1, for example, by at least three orders of magnitude.
[0097] Figure 16 shows a band gap A of a semiconductor layer sequence together with a concentration C of a p-dopant according to a further exemplary embodiment. In contrast to the exemplary embodiment described in connection with Figure 14, the concentration C of the p-dopant decreases continuously, for example linearly or non-linearly, on the side facing the active region A. The dopant concentration C is at least three orders of magnitude smaller at a distance of at most 30 nanometers, preferably of at most 10 nanometers and particularly preferably of at most 5 nanometers from the electron barrier layer 1 than a maximum concentration C of the p-dopant in the p-doped region P.
[0098] Figure 17 shows a band gap A of a semiconductor layer sequence together with a concentration C of a p-dopant according to a further exemplary embodiment. In contrast to the exemplary embodiment described in connection with Figure 16, the concentration C of the p-dopant in the p-doped region P is not constant, but has a maximum in the region of the electron barrier layer 1. The concentration C of the p-dopant decreases continuously in the transition region 2 in the growth direction R, for example by a total of at least 10%, preferably at least 25% and particularly preferably at least 50%. In a region following the transition region 2 in the growth direction R, the concentration C of the p-dopant is, for example, constant or approximately constant. This patent application claims priority from German patent application DE 102023108165.9, the disclosure content of which is hereby incorporated by reference.
[0099] The invention is not limited to the embodiments described herein. Rather, the invention encompasses any novel feature and any combination of features, including, in particular, any combination of features in the claims, even if this feature or combination itself is not explicitly stated in the claims or embodiments.
[0100] Reference symbol list
[0101] N n-doped region
[0102] A active area
[0103] P p-doped region
[0104] 1 electron barrier layer
[0105] 11 first barrier layer
[0106] 12 second barrier layer
[0107] 2 Transition area
[0108] 21 first transition layer
[0109] 22 second transition layer
[0110] 31 first curve
[0111] 32 second curve
[0112] 33 third curve
[0113] A band gap
[0114] As band gap peak
[0115] Ar bandgap ramp
[0116] C Concentration of the p-dopant d Thickness
[0117] E Energy
[0118] LB conduction band
[0119] VB valence band
[0120] R Growth direction
[0121] I electric current
[0122] Pout output power e- electron h+ hole
Claims
Patent claims 1. Semiconductor layer sequence, comprising: - a p-doped region (P) and an n-doped region (N), - an active region (A) arranged to generate electromagnetic radiation and arranged between the p-doped region (P) and the n-doped region (N), and - an electron barrier layer (1) on a side of the active region (A) facing the p-doped region (P), wherein - a band gap (A) of the electron barrier layer (1) is larger on a side facing away from the active region (A) than on a side facing the active region (A), and - an energy (E) of a valence band (VB) of the electron barrier layer (1) on the side facing away from the active region (A) is the same or higher than on the side facing the active region (A).
2. Semiconductor layer sequence according to the preceding claim, wherein the band gap (A) of the electron barrier layer (1) on the side facing away from the active region (A) is at least 0.02 electron volts larger than on the side facing the active region (A).
3. Semiconductor layer sequence according to one of the preceding claims, wherein the band gap (A) of the electron barrier layer (1) on the side facing away from the active region (A) is at most 0.3 electron volts larger than on the side facing the active region (A).
4. Semiconductor layer sequence according to one of the preceding claims, wherein the band gap (A) of the electron barrier layer (1) decreases continuously towards the active region (A).
5. Semiconductor layer sequence according to one of claims 1 to 3, wherein the band gap (A) of the electron barrier layer (1) has a maximum between the side facing the active region (A) and the side facing away from the active region (A).
6. Semiconductor layer sequence according to one of the preceding claims, wherein - the electron barrier layer (1) comprises a first barrier layer (11) and a second barrier layer (12), wherein - the first barrier layer (11) is arranged between the second barrier layer (12) and the active region (A), and - the second barrier layer (12) has a larger band gap (A) than the first barrier layer (11).
7. Semiconductor layer sequence according to one of the preceding claims, wherein - the electron barrier layer (1) comprises a first barrier layer (11) and a second barrier layer (12), - the semiconductor layer sequence comprises aluminium indium gallium nitride, and - the second barrier layer (12) has a higher aluminum content than the first barrier layer (11).
8. Semiconductor layer sequence according to the preceding claim, wherein the aluminum content of the second barrier layer (12) is between 1 percentage point and 15 percentage points higher than the aluminum content of the first barrier layer (11).
9. Semiconductor layer sequence according to one of claims 7 or 8, wherein the aluminum content of the first barrier layer (11) is at least 12 percentage points higher than an aluminum content of a semiconductor layer which directly adjoins the electron barrier layer (1) on the side facing the active region (A).
10. Semiconductor layer sequence according to one of claims 6 to 9, wherein a thickness (d) of the second barrier layer (12) is at most 5 nanometers.
11. Semiconductor layer sequence according to one of claims 6 to 10, wherein the band gap (A) of the second barrier layer (12) increases or decreases towards the active region (A).
12. Semiconductor layer sequence according to one of the preceding claims, additionally comprising: - a transition region (2) on the side of the electron barrier layer (1) facing away from the active region (A), wherein - a band gap (A) in the transition region (2) is larger than a band gap (A) of a semiconductor layer which directly borders the transition region (2) on a side of the transition region (2) facing away from the electron barrier layer (1), and - the band gap (A) in the transition region (2) is smaller than the band gap (A) in the electron barrier layer (1).
13. Semiconductor layer sequence according to one of the preceding claims, additionally comprising: - a transition region (2) on the side of the electron barrier layer (1) facing away from the active region (A), wherein - a band gap (A) in the transition region (2) to the electron barrier layer (1) increases continuously.
14. Semiconductor layer sequence according to one of the preceding claims, wherein - a transition region (2) on the side of the electron barrier layer (1) facing away from the active region (A) directly adjoins the electron barrier layer (1), - the transition region (2) and the electron barrier layer (1) comprise aluminium indium gallium nitride, and - an aluminum content of the transition region (2) at a boundary to the electron barrier layer (1) is between 30% and 100% inclusive of a maximum aluminum content in the electron barrier layer (1).
15. Semiconductor layer sequence according to one of claims 12 to 14, wherein - the transition region (2) comprises a first transition layer (21) and a second transition layer (22), - the first transition layer (21) is arranged between the second transition layer (22) and the electron barrier layer (1), and - a band gap (A) of the first transition layer (21) is larger than a band gap (A) of the second transition layer (22).
16. Semiconductor layer sequence according to the preceding claim, wherein the band gap (A) of the first transition layer (21) and / or the band gap (A) of the second transition layer (22) increases continuously towards the electron barrier layer (1).
17. Semiconductor layer sequence according to one of the preceding claims, wherein the electron barrier layer (1) is arranged in the p-doped region (P).
18. Semiconductor layer sequence according to one of the preceding claims, wherein a concentration (C) of a p-dopant in the electron barrier layer (1) has a maximum.
19. Semiconductor layer sequence according to one of the preceding claims, wherein a concentration (C) of a p-dopant on the side of the electron barrier layer (1) facing away from the active region (A) is at least 10% lower than a maximum concentration (C) of the p-dopant in the electron barrier layer (1).
20. Semiconductor layer sequence according to one of the preceding claims, wherein the concentration of the p-dopant decreases continuously from the electron barrier layer towards the active region.
Citation Information
Patent Citations
Semiconductor layer sequence
DE102023108165A1
Semiconductor device and semiconductor device package including same
EP3514840A1
Light emitting device
KR1020130067821A
Semiconductor light emitting device
US20140029636A1