Method for producing hardened product

The method of producing a cured product by mixing inorganic substance powders with ultra-fine bubble water and adhesives, and molding under pressure, enhances hardness and reduces material usage, addressing the strength and environmental concerns of existing methods.

WO2024204119A1PCT designated stage expired Publication Date: 2024-10-03OHKAWA STRUCTURE DESIGN CO LTD

Patent Information

Application Number
PCT/JP2024/011802
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-03-30
Filing Date
2024-03-26
Publication Date
2024-10-03

AI Technical Summary

Technical Problem

Existing methods for producing cured products using lignin and cellulose from plant waste materials lack sufficient hardness, necessitating a method to enhance the strength and reduce material usage while minimizing environmental impact.

Method used

A method involving the production of a powder from inorganic substances, mixing with ultra-fine bubble water and an adhesive, and molding under pressure to induce hydration reactions, which increases the hardness of the cured product, and optionally reinforcing with aramid or carbon fiber sheets.

Benefits of technology

The method produces a stronger cured product with reduced material usage and lower environmental impact, capable of withstanding external forces and potentially reducing CO2 emissions by eliminating the need for cement and aggregates.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure JP2024011802_03102024_PF_FP_ABST
    Figure JP2024011802_03102024_PF_FP_ABST
Patent Text Reader

Abstract

In order to provide a method for producing a hardened product having high hardness, the hardened product is formed by mixing and stirring a powder obtained by pulverizing inorganic matter, an adhesive agent, and ultrafine bubble water, and hardening the mixture. The inorganic matter includes industrial waste and natural materials, and the industrial waste includes concrete, mortar, tiles, and the like generated when a structure such as a building is crushed. The natural materials include shells, rocks, sand, laterite, animal bones, and the like. The inorganic matter also includes dehydrated cakes. The average particle size of ultrafine bubbles contained in the ultrafine bubble water is approximately 0.13 μm or smaller, and the number of ultrafine bubbles per 1 cc is approximately one hundred million or more. In addition, an aramid fiber sheet may be attached to the surface of the hardened product, and alumina may be added to the mixture materials.
Need to check novelty before this filing date? Find Prior Art

Description

Manufacturing method of cured product

[0001] The present invention relates to a method for producing a cured product.

[0002] Patent Document 1 below discloses a method for producing a hardened material containing at least one selected from lignin and cellulose and waste materials such as concrete. Lignin and cellulose can be obtained from plant-derived waste materials.

[0003] Patent Document 1 discloses that the material has sufficient strength, but further increasing the strength would enable reduction in the amount of material.

[0004] Patent No. 7157984

[0005] An object of the present invention is to provide a method for producing a cured product having high hardness.

[0006] The cured product of the present invention includes the steps of producing a powder made of an inorganic substance, mixing and stirring the powder, ultra-fine bubble water, and an adhesive to produce a mixed material, pouring the mixed material into a formwork, and curing the mixed material.

[0007] According to the present invention, by using ultra-fine bubble water, the ultra-fine bubble water penetrates deep into the powder, causing a hydration reaction deep into the powder, thereby making the cured product stronger.

[0008] FIG. 1 is a schematic diagram of grinding inorganic materials; FIG. 2 is a schematic diagram of stirring a mixed material; FIG. 3 is a schematic diagram of putting a mixed material into a mold and hardening it in a pressure cooker; FIG. 4 is a schematic diagram of a hardened product removed from the mold; FIG. 5 is a schematic diagram of an aramid fiber sheet being attached to the hardened product; and FIG. 6 is a schematic diagram of a top coat material being applied onto the aramid fiber sheet.

[0009] The method for producing a cured product of the present invention will be described with reference to the drawings, which are schematic illustrations for the purpose of explanation.

[0010] [Embodiment 1] The cured product is formed by mixing powdered inorganic material, adhesive, and ultra-fine bubble water, stirring the mixture, and curing the mixture.

[0011] Inorganic waste includes industrial waste and natural waste. Industrial waste includes concrete, mortar, roofing tiles, etc. generated when buildings and other structures are crushed. Natural waste includes shells, rocks, sand, laterite, animal bones, etc. Inorganic waste also includes dehydrated cake and sludge.

[0012] The inorganic material is pulverized into a powder. The powder contains calcium or a calcium compound. Calcium compounds include calcium carbonate, calcium oxide, tricalcium silicate, dicalcium silicate, tricalcium aluminate, tetracalcium aluminate ferroferrate, and gypsum dihydrate. The average particle size of the powder is, for example, about 300 μm, but this may be changed as appropriate depending on the hardness of the cured product.

[0013] Adhesives can be made from natural rubber, acrylic, epoxy, silicone, or vinyl acetate materials. For example, latex (natural rubber) made from rubber trees is used as the adhesive. The average particle size of the adhesive is approximately 0.02 to 10 μm. The adhesive is attached to the periphery of each powder particle, joining the powder particles together. Using a natural rubber adhesive makes it possible to produce a cured product with a small environmental impact.

[0014] Ultra-fine bubble water is a liquid containing ultra-fine bubbles. The average diameter of the ultra-fine bubbles contained in ultra-fine bubble water is approximately 0.13 μm or less. The number of ultra-fine bubbles contained per cc is approximately 100 million or more. The ratio of the average diameter of the ultra-fine bubbles to the average diameter of the powder and adhesive is approximately 1:15,000:77.

[0015] Ultra-fine bubble water can penetrate deep into materials. Ultra-fine bubble water can penetrate deep into microscopic holes and cracks formed on the surface of powder. Powder contains calcium or calcium compounds, which undergo a hydration reaction with water and harden. In this case, ultra-fine bubble water causes a hydration reaction deep into the powder, increasing the hardness of the hardened product.

[0016] Next, a method for producing a hardened product is described. (1) A powder made of inorganic materials is produced. The inorganic materials include at least one of industrial waste concrete and mortar, naturally occurring shells (including edible shells), sand, and rocks. If the concrete contains reinforcing bars, the reinforcing bars are removed. As shown in FIG. 1 , prepared industrial waste 12 and the like are crushed in a crushing device 14 to produce a powder made of inorganic materials 16. The crushing device 14 is equipped with multiple cutters 18, which crush the industrial waste 12 and the like. Alternatively, sludge and the like may be dehydrated to produce a dehydrated cake, which may then be sieved to remove debris and the like to produce a powder made of inorganic materials. Because inorganic materials are recycled or abundant in nature, they have a low environmental impact.

[0017] (2) The powder 16, adhesive, and ultra-fine bubble water are mixed in a single container 20 and further stirred to form a mixture 22 (Figure 2). The ratio of the powder 16, adhesive, and ultra-fine bubble water is approximately 70-80% powder 16, approximately 20-10% adhesive, and approximately 10% ultra-fine bubble water. The ratio of the materials may be changed to match the hardness of the cured product, so that the total amount becomes 100%. Note that the ratio of the materials is an example and may be changed depending on the hardness and shape of the cured product.

[0018] For mixing and stirring, a stirrer 26 that stirs the materials placed in the container 20 with a propeller 24 or the like, a vibrator that directly or indirectly vibrates the mixed material 22, a tilting device that changes the angle of the container 20 for the mixed material 22, a blower that blows air on the mixed material 22 to stir it, and the like are used.

[0019] The powder 16, adhesive, and ultra-fine bubble water may be placed in the container 20 one by one and mixed and stirred, or multiple of these may be placed in the container 20 simultaneously and mixed and stirred. Alternatively, ultra-fine bubble water may be mixed in through a shower head during or after mixing the powder 16 and adhesive. The ultra-fine bubble water is sprayed in multiple directions from the shower head, making it easier for the ultra-fine bubble water to mix with the powder 16 and adhesive. The powder 16 contains calcium or a calcium compound, and the ultra-fine bubble water causes a hydration reaction in the powder 16, causing it to harden.

[0020] (3) The mixed material 22 is poured into the mold. To prevent air bubbles from forming in the mixed material 22 inside the mold, a vibrating device may be placed inside the mixed material 22 to vibrate the mixed material 22 and allow the air bubbles to escape upward. A release sheet, resin film, or the like may be provided on the inner wall of the mold so that the mixed material 22 can be removed from the mold after it has hardened.

[0021] (4) The mixed material 22 poured into the mold is cured. Pressure is applied to the mixed material 22 during curing. The mold 30 and mixed material 22 may be placed inside a pressure cooker 28 that is airtight and capable of increasing the atmospheric pressure inside (Figure 3). A heater 32 inside the pressure cooker is activated to raise the temperature inside the pressure cooker. As the mixed material 22 is heated, the water evaporating from the mixed material 22 increases the pressure inside the pressure cooker. The top of the mold 30 is open, and steam 34 applies pressure to the mixed material 22. For example, the heater 32 is set so that the atmospheric temperature inside the pressure cooker 28 is the boiling point of water, e.g., 100°C. The ultra-fine bubble water contained in the mixed material 22 expands approximately 1,700 times as it boils and turns into steam, increasing the pressure inside the pressure cooker. The pressure is determined and adjusted appropriately depending on the thickness of the cured product. Although the ambient temperature inside the pressure cooker is increased by the heater 32 inside the pressure cooker 28, a heater may be placed outside the pressure cooker 28 so that the ambient temperature inside the pressure cooker can be increased from the heater. The pressure cooker 28 may be configured so that air can be sucked in and exhausted, and the pressure inside the pressure cooker 28 can be adjusted.

[0022] (5) After the mixed material 22 has hardened, the formwork 30 is removed from the pressure cooker 28. The hardened product 10 is removed from the formwork 30, and the hardened product 10 is completed (FIG. 4). The hardened product 10 is used for civil engineering structures, buildings, etc.

[0023] As described above, the present invention produces the hardened product 10 without using cement or aggregates (sand, gravel). As the amount of cement and aggregates available on Earth is decreasing, it is possible to achieve a cement-free and aggregate-free environment. Since wood and the like are not used as in the prior art, a strong hardened product 10 can be produced. Because the strength of the hardened product 10 is increased, it is possible to make the thickness of the hardened product 10 used in a structure thinner or finer, which allows for a reduction in the amount of material used and reduces CO2 emissions. 2 Emissions can also be reduced.

[0024] [Embodiment 2] An aramid fiber sheet may be attached to the periphery of the cured product 10 produced in Embodiment 1. The aramid fiber sheet is composed of wholly aromatic aramid fibers. The aramid fiber sheet is formed into a sheet by aligning the fibers in one or two directions. The aramid fiber sheet is wrapped around and attached to the surface of the cured product 10. By attaching the aramid fiber sheet to the cured product 10, it is possible to withstand large external forces (axial force, bending moment, shear force, etc.).

[0025] The method for attaching the aramid fiber sheet will now be described. (1) The surface of the cured product 10 produced in embodiment 1 is primed. For example, the primed surface is polished with a polishing device. Note that if primed surface treatment is not required, it may be omitted.

[0026] (2) A primer is applied to the surface of the cured product 10 (primer treatment). An example of the primer is an epoxy resin. This enhances the adhesive strength of the aramid fiber sheet.

[0027] (3) An intermediate coating material 36 is applied to the surface of the cured product 10, and an aramid fiber sheet 38 is attached to the surface of the cured product 10 (FIG. 5). An example of the intermediate coating material 36 is epoxy resin. The primer and intermediate coating material 36 may be made of different materials. The aramid fiber sheet 38 may be attached while removing air with a degassing roller. The aramid fiber sheet 38 is attached before the intermediate coating material 36 dries.

[0028] (4) A top coat material 40 is applied from above the aramid fiber sheet 38 (FIG. 6). By applying the top coat material 40 so that the aramid fiber sheet 38 is not visible, a stronger cured product 42 is produced. Examples of the top coat material include an epoxy-based coating material, and it may be a material that is water-resistant, chemical-resistant, or oil-resistant.

[0029] The initial cured product 10 can be reinforced by the aramid fiber sheet 38. The cured product 10 has increased resistance to axial force, bending moment, shear force, torsion, etc. This provides stronger reinforcement than adding reinforcing materials such as steel bars to the cured product 42. The aramid fiber sheet 38 has higher tensile strength, is lighter, and is less susceptible to deterioration than steel bars, etc.

[0030] Instead of the aramid fiber sheet 38, a carbon fiber sheet may be attached to the surface of the cured product 10. The carbon fiber sheet is a sheet made of carbon fiber, and is about one-quarter the weight of steel, but about ten times stronger than steel. This can increase the strength of the cured product 10.

[0031] [Embodiment 3] In embodiment 1, pressure is applied to the admixture 22 poured into the mold 30 by increasing the pressure inside the pressure cooker with steam 34, but pressure may also be applied by other methods. For example, pressure may be applied to the admixture 22 by applying a load from above the admixture 22 using heat and pressure using a hot press method.

[0032] [Embodiment 4] In Embodiment 1, the cured product 10 may be produced by including an admixture, if necessary. The admixture may be added when the powder, adhesive, and ultra-fine bubble water are mixed to produce the admixture. Examples of the admixture include a water-reducing agent, a quick-setting agent, a setting retarder, and a hydration heat inhibitor.

[0033] [Embodiment 5] In the above embodiment, the powder, adhesive, and ultra-fine bubble water are mixed and stirred. However, alumina (aluminum oxide) may be added to and mixed with the powder, adhesive, and ultra-fine bubble water. The alumina is in powder form. The inclusion of alumina in the mixture can increase the thermal conductivity of the cured product 10. The proportion of alumina in the mixture can be adjusted depending on the desired thermal conductivity. For example, the temperature of the outer surface and the interior of the mixture can be made uniform during production, making it easier to produce a homogeneous cured product 10. Furthermore, placing the cured product 10 on the ground or the like allows heat exchange between the cured product 10 and the area where it is placed.

[0034] In addition, the present invention can be implemented in various forms with various improvements, modifications, and changes based on the knowledge of those skilled in the art, without departing from the spirit of the present invention. Each embodiment is not independent, but can be implemented in an appropriate combination based on the knowledge of those skilled in the art.

[0035] 10, 42: Hardened material 12: Industrial waste 14: Crushing device 16: Powder 18: Cutter 20: Container 22: Mixing material 24: Propeller 26: Stirrer 28: Pressure cooker 30: Formwork 32: Heater 34: Steam pressure 36: Undercoat material 38: Aramid fiber sheet 40: Topcoat material

Claims

1. A method for producing a hardened product, comprising the steps of: producing a powder made of inorganic matter, including concrete, mortar, roofing tiles, shells, rocks, sand, laterite, animal bones, dehydrated cake, or sludge; mixing and stirring the powder, ultra-fine bubble water, and a material containing an adhesive made of a natural rubber, acrylic, epoxy, silicone, or vinyl acetate material in a ratio of 70-80% powder, 20-10% adhesive, and 10% ultra-fine bubble water, totaling 100%, and allowing the ultra-fine bubble water to permeate holes and cracks in the powder to produce a mixed material; pouring the mixed material into a form; and hardening the mixed material by causing the adhesive to adhere to the periphery of the powder and bond the powder together.

2. The method for producing a cured product according to claim 1, wherein the step of curing the mixed material includes a step of curing the mixed material while applying pressure to the mixed material.

3. A method for producing the cured product of claim 1, further comprising the step of attaching an aramid fiber sheet or a carbon fiber sheet to the surface of the cured product formed by curing the mixture.

Citation Information

Patent Citations

  • Low-alkalinity curing agent, vegetation base material for ecological restoration of side slope and preparation method of vegetation base material

    CN114477937A

  • Microbubble ceramic composite board

    CN207245058U

  • Manufacture of flexible plate composite

    JP1978112985A

  • Fine bubble-containing solidified body and method for producing fine bubble-containing solidified body

    JP2020105049A

  • Hardened calcium silicate having high strength

    WO2002066396A1

Cited By

  • Water shutoff and heat insulation grouting material suitable for high-ground-temperature fractured rock mass and preparation method of water shutoff and heat insulation grouting material

    CN119822744A