Composite film, and preparation method therefor and use thereof
By designing the multi-layer structure of the composite film and using a combination of non-Newtonian fluid materials and adhesives to absorb and dissipate impact energy, the problem that the existing car front window glass protective film cannot prevent damage caused by the impact of small stones during high-speed driving is solved. Achieving high impact resistance and multiple protection effects of glass.
Patent Information
- Application Number
- PCT/CN2024/095810
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-04-12
- Filing Date
- 2024-05-28
- Publication Date
- 2024-10-17
AI Technical Summary
Existing car front window glass protective films cannot effectively prevent the glass from being damaged by small stones brought up by high-speed driving, causing the glass to be easily scratched or broken.
A composite membrane is designed, including a first protective layer from top to bottom, a buffer elastic layer and an impact hardening layer. Through the combination of non-Newtonian fluid materials and adhesives, a high damping and high viscosity state is formed to absorb and Dissipates impact energy and improves the impact resistance of the glass through the synergistic effect of the multi-layer structure.
The composite film can effectively slow down external impact, protect the glass from damage, and recover after multiple impacts without losing its own impact resistance, making it suitable for mass production.
Smart Images

Figure CN2024095810_17102024_PF_FP_ABST
Abstract
Description
Composite membrane and its preparation method and application Technical Field
[0001] The present invention relates to the field of membrane technology, in particular to a composite membrane and a preparation method and application thereof. Background Art
[0002] Glass is a commonly used material and is widely used in our daily life. However, in order to prevent the glass from being scratched or worn, a protective film is often applied to protect the glass from damage.
[0003] The exterior of a car's windshield is generally unprotected, making it susceptible to external impact and friction during driving, leading to scratches and cracks on the glass surface. Current windshield designs primarily incorporate a protective film on the inside of the windshield to prevent injuries to occupants when the glass breaks. However, this measure only protects occupants and does not protect the windshield from damage.
[0004] Patent publication number CN218321205U discloses an anti-glare automotive glass protective film, relating to the field of automotive product technology. The protective film includes an anti-glare layer for blocking light to achieve an anti-glare function, an anti-scratch layer for preventing scratches from stones attached to the upper side of the anti-glare layer, a second release protective layer for protecting the anti-scratch layer attached to the upper surface of the anti-scratch layer, a reinforcing layer provided on the lower side of the anti-glare layer, a buffer layer provided on the lower side of the reinforcing layer, an adhesive layer for adhering to the automotive glass provided on the lower side of the buffer layer, and a first release protective layer provided on the lower side of the adhesive layer for protecting the glass. However, the protective film of this technical solution can only prevent scratches caused by sand and stones. If a vehicle traveling at high speed on the highway picks up small stones on the ground and impacts the glass, the strong impact force can easily break through the protective film and hit the front windshield, causing cracks or even breakage. Therefore, the development of an impact-resistant protective film for glass protection has become an urgent need.
[0005] Summary of the Invention
[0006] Based on the technical problems existing in the background technology, the purpose of the present invention is to provide a composite film that can improve the impact resistance of glass.
[0007] The present invention provides a composite film, which is provided with a first protective layer, a buffering elastic layer and an impact hardening layer from top to bottom. A first adhesive layer is provided between the first protective layer and the buffering elastic layer. The impact hardening layer contains a non-Newtonian fluid material and an adhesive. The weight ratio of the non-Newtonian fluid material to the adhesive is 1:0.6-1.2.
[0008] A preferred technical solution of the present invention is that the buffer elastic layer is provided with a liquid-containing through-hole array, and the diameter of the through-holes of the liquid-containing through-hole array is 0.05-0.1 mm.
[0009] A preferred technical solution of the present invention is that the material of the first adhesive layer is OCA glue or PU glue.
[0010] The preferred technical solution of the present invention is that the thickness of the first protective layer is 70-200um, the thickness of the buffer elastic layer is 50-100um, the thickness of the first adhesive layer is 20-30um, and the thickness of the impact hardening layer is 80-120um.
[0011] A preferred technical solution of the present invention is that a second adhesive layer and an attachment layer are sequentially provided between the buffer elastic layer and the impact hardening layer from top to bottom.
[0012] A preferred technical solution of the present invention is that the second adhesive layer is OCA glue; and the attachment layer is PET film or PC film.
[0013] A preferred technical solution of the present invention is that the thickness of the second adhesive layer is 15-35 um; and the thickness of the attachment layer is 30-70 um.
[0014] Another object of the present invention is to provide a method for preparing the composite film, comprising the following steps:
[0015] S0: coating a first adhesive layer on the first protective layer so that the first protective layer and the buffer elastic layer are bonded together;
[0016] S1: Coating an impact hardening layer on the other side of the buffer elastic layer;
[0017] Among them, in S1, the impact hardening layer is coated by first coating the non-Newtonian fluid material and then coating the adhesive, or by first mixing and stirring the non-Newtonian fluid material and the adhesive and then coating them on the buffer elastic layer.
[0018] The preferred technical solution of the present invention is that in S3, the impact hardening layer is coated by first coating the non-Newtonian fluid material and then coating the adhesive, wherein the ambient temperature for coating the non-Newtonian fluid material is 15-25°C and the coating speed is 150-200 mm / s.
[0019] Another object of the present invention is to provide application of the composite film in automobile protective films.
[0020] Compared with the prior art, the present invention has the following beneficial effects:
[0021] (1) The composite film provided by the present invention is an orderly combination of a first protective layer, a buffer elastic layer, and an impact hardening layer. Through the functions of the three different structures, the interaction forms a synergistic effect, thereby improving the impact resistance of the composite film formed by the combination, thereby obtaining a new composite film with impact resistance. The first protective layer first bears the impact force, and absorbs the force through the deformable buffer elastic layer. Under the action of the impact force transmitted by the first protective layer, the buffer elastic layer absorbs and disperses the impact energy, thereby reducing the destructive effect of the external impact force on the first protective layer. At the same time, the impact force can be further transmitted to the impact hardening layer. After the impact hardening layer is subjected to the impact force, the impact hardening layer forms a state with high damping and high viscosity in a short time due to the special properties of shear hardening of non-Newtonian fluid materials, so that the shock wave is better dissipated and absorbed, thereby protecting the glass from damage.
[0022] (2) Impact hardening layer: When the impact is removed, the impact hardening layer will return to its original state without causing damage to the impact hardening layer itself. In this regard, the composite film can effectively protect the glass many times, and the impact resistance of the composite film itself will not be significantly reduced;
[0023] (3) The preparation method of the composite membrane provided by the present invention is simple and easy, and the production process is simple and suitable for mass production. BRIEF DESCRIPTION OF THE DRAWINGS
[0024] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the following briefly introduces the drawings required for use in the embodiments or the description of the prior art. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying any creative work.
[0025] FIG1 is a longitudinal cross-sectional view of a composite membrane of Example 1.
[0026] In the picture:
[0027] 1-first protective layer; 2-buffering elastic layer; 31-first adhesive layer; 32-second adhesive layer; 4-adhesion layer; 5-impact hardening layer; 51-non-Newtonian fluid material layer; 52-adhesive layer; 6-release film layer. DETAILED DESCRIPTION
[0028] The present invention is further described below with reference to the examples. These examples are intended to illustrate the present invention only and are not intended to limit the scope of the present invention. The experimental methods in the following examples, for which specific conditions are not specified, are generally based on conventional conditions in the art or the conditions recommended by the manufacturer; the raw materials and reagents used, unless otherwise specified, are all commercially available from conventional markets. Any non-substantial changes and substitutions made by those skilled in the art based on the present invention fall within the scope of protection claimed in the present invention.
[0029] The following Table 1 shows the sources of raw materials in the examples and comparative examples of the present application:
[0030] Table 1 - Sources and types of raw materials in the examples and comparative examples of this application
[0031] Examples 1-6
[0032] Example 1
[0033] A method for preparing a composite film comprises the following steps:
[0034] Step 1: Prepare materials, wherein the first protective layer 1 is made of 188 μm thick PET film, the buffer elastic layer 2 is made of TPU film, the first adhesive layer 31 and the second adhesive layer 32 are made of OCA glue, and the attachment layer 4 is made of 50 μm thick PET film;
[0035] Step 2: Place the material in a coating machine in a dust-free coating environment (the same below), first bond the first protective layer and the buffer elastic layer at a coating speed of 500 mm / s to obtain a first composite film, wherein the thickness of the first adhesive layer is about 25 μm;
[0036] Step 3: bonding the buffer elastic layer and the adhesion layer of the first composite film at a coating speed of 500 mm / s to obtain a second composite film, wherein the thickness of the second adhesive layer is about 25 μm;
[0037] Step 4: The impact hardening layer 5 is composed of a non-Newtonian fluid material layer 51 and an adhesive layer 52 stacked together. The non-Newtonian fluid material layer is first coated on the attachment layer side of the second composite film, and then the adhesive layer is coated. The ambient temperature for coating the non-Newtonian fluid material layer is 20°C, the coating speed is 200 mm / s, the heating temperature of the adhesive layer is 80°C, and the coating speed is 200 mm / s. The thickness of the non-Newtonian fluid material layer is about 40 μm, the thickness of the adhesive layer is about 40 μm, and the weight ratio of the non-Newtonian fluid material layer to the adhesive layer is 1:0.6.
[0038] Step 5: Attach a release film layer to the other side of the adhesive layer.
[0039] Step 6: Dry the formed film, dry it naturally, and the drying time is 6 hours to obtain a composite film.
[0040] Example 2
[0041] A method for preparing a composite membrane, wherein each step and the reagents and process parameters used in each step are the same as those in Example 1, except that the thickness of the non-Newtonian fluid material layer is about 40 μm, the thickness of the adhesive layer is about 80 μm, and the weight ratio of the non-Newtonian fluid material layer to the adhesive layer is 1:1.2.
[0042] Example 3
[0043] A method for preparing a composite membrane, wherein each step and the reagents and process parameters used in each step are the same as those in Example 1, except that a non-Newtonian fluid material and an adhesive are mixed in a weight ratio of 1:1 and then coated on a buffer elastic layer as an impact hardening layer with a thickness of approximately 100 μm.
[0044] Example 4
[0045] A method for preparing a composite membrane, wherein each step and the reagents and process parameters used in each step are the same as those in Example 1, except that the TPU membrane is provided with a liquid-containing through-hole array, the through-hole diameter of the liquid-containing through-hole array is 0.1 mm, and the through-holes are spaced 0.5 mm apart.
[0046] Example 5
[0047] A method for preparing a composite membrane, wherein each step and the reagents and process parameters used in each step are the same as those in Example 1, except that the first protective layer uses a PC film with a thickness of 70 μm.
[0048] Example 6
[0049] A method for preparing a composite film, wherein each step and the reagents and process parameters used in each step are the same as those in Example 5, except that the first adhesive layer and the second adhesive layer use PU glue, wherein the thickness of the first adhesive layer is about 20 μm, and the thickness of the second adhesive layer is about 15 μm.
[0050] Comparative Example 1
[0051] A method for preparing a composite membrane, wherein each step and the reagents and process parameters used in each step are the same as those in Example 1, except that no non-Newtonian fluid material is coated.
[0052] Performance testing
[0053] 1. Impact resistance test: Cut the composite film into 20cm*20cm pieces and glue them to the car glass. Keep the surface clean and flat, with no visible bubbles remaining. Use a fixture to fix the car glass. Use a 100g steel ball to drop from a height of 1.5 meters above the composite film. Observe the damage to the composite film and the glass.
[0054] 2. Durability test: Repeat the impact resistance test 10 times and observe the damage of the composite film and glass;
[0055] 3. Light transmittance: Use a light transmittance tester to test.
[0056] The results of the above performance test are shown in Table 2.
[0057] Table 2 - Performance test results of impact resistance and light transmittance of composite films of Examples 1-6 and Comparative Example 1
[0058] In specific embodiments of the present invention, impact resistance testing was used to simulate the impact of small pebbles on glass caused by a high-speed vehicle on a highway. As demonstrated in Examples 1-6, the composite films produced by the present invention exhibited excellent impact resistance. Neither the composite film nor the glass surface showed visible cracks, and the light transmittance exceeded 85%, meeting the requirements for windshield protection. Multiple tests revealed that even if white spots or cracks appeared on the composite film, the glass itself remained intact, demonstrating the composite film's ability to provide repeated protection.
[0059] Comparing the data of Example 2, it can be clearly found that increasing the thickness of the adhesive will reduce the transmittance, but has little effect on durability.
[0060] Comparing the data from Example 3, it is clear that the hybrid-recoating process significantly improves the durability of the composite film. This is because hybrid-recoating reduces the unevenness caused by delamination between the non-Newtonian fluid material and the adhesive, thereby making the composite film more uniformly stressed and improving its durability. However, mixing the non-Newtonian fluid material and the adhesive fills the structural gaps between them, resulting in a significant decrease in light transmittance. Furthermore, the hybrid-recoating process eliminates a time-consuming coating step, improving the production efficiency of the composite film.
[0061] Comparing the data of Example 4, it can be clearly found that the provision of a liquid-containing through-hole array is beneficial in the coating and lamination process, so that the adhesive of the uneven part of the bonding layer will flow toward and fill the through-holes in the liquid-containing through-hole array, thereby making the bonding of the composite film smooth, improving the uniformity of the force applied to the composite film, and further improving the durability of the composite film.
[0062] Comparing the data of Example 5, it can be found that even though the PC film is thinner, the performance of the PC film itself is better than that of the PET film, and the durability of the composite film prepared therefrom is also better. However, the cost of the PC film is relatively more expensive.
[0063] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention and are not intended to limit the scope of protection of the present invention. Although the present invention has been described in detail with reference to preferred embodiments, those skilled in the art should understand that the technical solutions of the present invention may be modified or replaced by equivalents without departing from the essence and scope of the technical solutions of the present invention.
Claims
1. A composite film, characterized in that: A first protective layer, a buffer elastic layer and an impact hardening layer are provided in sequence from top to bottom, and a first adhesive layer is provided between the first protective layer and the buffer elastic layer; The impact hardening layer comprises a non-Newtonian fluid material and an adhesive, wherein the weight ratio of the non-Newtonian fluid material to the adhesive is 1:0.6-1.2, and the non-Newtonian fluid material and the adhesive are mixed according to the weight ratio and then coated as the impact hardening layer; The brand of the non-Newtonian fluid material is FX-480 produced by Dongguan Qinghe Research and Development Technology Co., Ltd.
2. The composite membrane according to claim 1, characterized in that: The buffer elastic layer is provided with a liquid-containing through hole array, and the through hole diameter of the liquid-containing through hole array is 0.05-0.1 mm.
3. The composite membrane according to claim 1, characterized in that: The material of the first adhesive layer is OCA glue or PU glue.
4. The composite membrane according to claim 1, characterized in that: The thickness of the first protective layer is 70-200 um, the thickness of the buffer elastic layer is 50-100 um, the thickness of the first adhesive layer is 20-30 um, and the thickness of the impact hardening layer is 80-120 um.
5. The composite membrane according to claim 1, characterized in that: A second adhesive layer and an attachment layer are arranged in sequence from top to bottom between the buffer elastic layer and the impact hardening layer.
6. The composite membrane according to claim 5, characterized in that: The second adhesive layer is OCA glue; the attachment layer is PET film or PC film.
7. The composite membrane according to claim 6, characterized in that: The thickness of the second adhesive layer is 15-35 um; the thickness of the attachment layer is 30-70 um.
8. A method for preparing a composite membrane according to any one of claims 1 to 7, characterized in that: The following steps are involved: S0: coating the first adhesive layer on the first protective layer so that the first protective layer and the buffer elastic layer are bonded to each other; S1: coating the impact hardening layer on the other side of the buffer elastic layer; Among them, in S1, the impact hardening layer is coated by first mixing and stirring the non-Newtonian fluid material and the adhesive and then coating the mixture on the buffer elastic layer.
9. Use of the composite film according to any one of claims 1 to 7 in an automobile protective film.
Citation Information
Patent Citations
Process for treating and / or forming a non-newtonian fluid using microchannel process technology
CN101472676A
Method for producing a non-newtonian fluid in particular for impact protection, method for producing an impact protection by means of a non-newtonian fluid, impact protection by means of a non-newtonian fluid, and object with such impact protection
CN104540878A
Non-Newtonian fluid material and intelligent anti-collision textile
CN108546324A
Sound insulation and vibration attenuation structure
CN108878119A
Composite membrane as well as preparation method and application thereof
CN116355546A