Method for manufacturing semiconductor device
The method of plasma etching the organic insulating film in semiconductor devices addresses the thermal expansion mismatch issue by adjusting the level difference with argon plasma, improving bonding reliability and reducing defects in hybrid bonding techniques.
Patent Information
- Application Number
- PCT/JP2023/014899
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-04-12
- Publication Date
- 2024-10-17
AI Technical Summary
In hybrid bonding techniques for semiconductor devices, differences in thermal expansion coefficients between metal terminal electrodes and organic insulating materials lead to poor bonding due to surface position shifts, making it challenging to achieve a desired level difference between the organic insulating film and the electrode tip surface.
A method involving plasma etching of the organic insulating film to adjust its surface level relative to the electrode tip surface, using argon plasma with specific flow rates and power settings to ensure precise alignment and minimize surface roughening, allowing for reliable bonding by adjusting the elastic modulus and thermal expansion mismatch.
This method enables the precise adjustment of the level difference between the organic insulating film and the electrode, reducing bonding defects and misalignment caused by thermal expansion, thereby enhancing the reliability of hybrid bonding in semiconductor devices.
Smart Images

Figure JP2023014899_17102024_PF_FP_ABST
Abstract
Description
Semiconductor device manufacturing method
[0001] The present disclosure relates to a method for manufacturing a semiconductor device.
[0002] Patent Documents 1 to 3 disclose examples of hybrid bonding techniques used in wafer-to-wafer (W2W) bonding processes or chip-on-wafer (CoW) bonding processes in three-dimensional packaging of semiconductor devices.
[0003] Japanese Patent Application Laid-Open No. 2021-197430 Japanese Patent Application Laid-Open No. 2021-197431 Special Publication No. 2018-528622
[0004] In the hybrid bonding technology described in Patent Document 1 and the like, an organic material (resin) may be used for the insulating portion, and in this case, a difference in the thermal expansion coefficient (coefficient of linear thermal expansion CTE) between the metal material constituting the terminal electrode and the organic material constituting the insulating portion may cause a misalignment in the surface position, which may result in poor bonding in the insulating portion or the terminal electrode. For this reason, a method is desired that can easily provide a desired step in advance between the surface of the organic insulating film of a semiconductor substrate used for hybrid bonding and the tip surface of the electrode.
[0005] The present disclosure aims to provide a method for manufacturing a semiconductor device that can easily provide a desired step between the surface of an organic insulating film on a semiconductor substrate and the tip surface of an electrode in a hybrid bonding method using an organic insulating film.
[0006] [1] A method for manufacturing a semiconductor device according to one aspect of the present disclosure includes the steps of: preparing a first semiconductor substrate having a first substrate body, a first organic insulating film and a first electrode provided on one surface of the first substrate body; and irradiating a surface of the first semiconductor substrate with plasma. In the plasma irradiation step, at least the first organic insulating film is etched by the plasma so that the surface of the first organic insulating film is closer to the first substrate body than the tip surface of the first electrode.
[0007] In this semiconductor device manufacturing method, at least the first organic insulating film is etched with plasma so that the surface of the first organic insulating film is closer to the first substrate body than the tip surface of the first electrode. In this case, although plasma is irradiated toward both the first organic insulating film and the first electrode, the amount of etching by the plasma varies depending on the difference in elastic modulus between the two. Therefore, according to this manufacturing method, by changing the plasma conditions depending on the materials of the organic insulating film and the electrode or the difference in elastic modulus between the two, it is possible to easily create a desired step between the surface of the organic insulating film of the semiconductor substrate and the tip surface of the electrode in a hybrid bonding method using an organic insulating film.
[0008] [2] In the method for manufacturing a semiconductor device according to [1] above, it is preferable that the plasma irradiation step irradiates the first semiconductor substrate with argon plasma, which makes it easier to adjust the step between the surface of the organic insulating film on the semiconductor substrate and the tip surface of the electrode to a desired value.
[0009] [3] In the method for manufacturing a semiconductor device according to the above [1] or [2], in the step of irradiating plasma, the flow rate of the plasma gas is 3.38×10 -2 P.A.M. 3 / sec (20sccm) to 1.69Pa m 3 / sec (1000 sccm). -2 P.A.M. 3 By setting the flow rate of the plasma gas to 1.69 Pa·m / sec (20 sccm) or more, etching by plasma can be promoted, and the step between the surface of the organic insulating film of the semiconductor substrate and the tip surface of the electrode can be quickly reduced to a desired value. 3 By setting the flow rate to 1000 sccm or less, it is possible to prevent the surfaces of the organic insulating film and the electrodes from being roughened by the plasma.
[0010] [4] In any of the semiconductor device manufacturing methods [1] to [3] above, the plasma output in the plasma irradiation step is preferably 10 W to 1000 W. By using a plasma output of 10 W or more, etching by the plasma can be promoted, and the step between the surface of the organic insulating film of the semiconductor substrate and the tip surface of the electrode can be quickly reduced to a desired value. On the other hand, by using a plasma output of 1000 W or less, roughening of the surfaces of the organic insulating film and the electrode by the plasma can be suppressed.
[0011] [5] In the method for manufacturing a semiconductor device according to any one of [1] to [4] above, the plasma treatment time in the plasma irradiation step is preferably 30 seconds or more. By using a plasma treatment time of 30 seconds or more, etching by the plasma can be promoted, and the step between the surface of the organic insulating film on the semiconductor substrate and the tip surface of the electrode can be quickly reduced to a desired value.
[0012] [6] In the method for manufacturing a semiconductor device according to any one of the above [1] to [5], the elastic modulus of the first organic insulating film is preferably 7.5 GPa or less, which makes it possible to easily provide a desired step between the surface of the organic insulating film on the semiconductor substrate and the tip surface of the electrode.
[0013] [7] In the method for manufacturing a semiconductor device according to any one of [1] to [6] above, in the step of irradiating plasma, the surface of the first semiconductor substrate may be irradiated with plasma so that the step distance between the surface of the first organic insulating film and the tip face of the first electrode is 40 nm to 100 nm. In this case, when the first semiconductor substrate is bonded to another substrate by hybrid bonding, the amount of misalignment between the surface of the first organic insulating film and the tip face of the first electrode is reduced due to thermal expansion, thereby enabling more reliable bonding between the first semiconductor substrate and the other substrate.
[0014] [8] In the method for manufacturing a semiconductor device according to any one of [1] to [6] above, in the step of irradiating plasma, the surface of the first semiconductor substrate may be irradiated with plasma so that the step distance between the surface of the first organic insulating film and the tip face of the first electrode is 60 nm to 80 nm. In this case, when the first semiconductor substrate is bonded to another substrate by hybrid bonding, the amount of misalignment between the surface of the first organic insulating film and the tip face of the first electrode due to thermal expansion is reduced, thereby enabling more reliable bonding between the first semiconductor substrate and the other substrate.
[0015] [9] The semiconductor device manufacturing method according to any one of [1] to [8] above further includes a step of polishing the first organic insulating film and the first electrode provided on one surface of the first semiconductor substrate, and the step of polishing the first semiconductor substrate is preferably performed before the step of irradiating with plasma. The polishing step can reduce the surface roughness of the surface of the first organic insulating film of the first semiconductor substrate and the tip surface of the first electrode while achieving a desired level of step height, but fine adjustment of the step height is difficult. Therefore, if the desired level of step height is not achieved in the polishing step, the level of step height can be further adjusted by performing a step of irradiating with plasma after the polishing step. Therefore, this manufacturing method can reduce bonding defects in hybrid bonding.
[0016]
[10] In the method for manufacturing a semiconductor device according to [9] above, in the step of polishing the first semiconductor substrate, it is preferable to polish the first organic insulating film and the first electrode so that their respective surfaces have a surface roughness Ra of 5 nm or less, preferably 1 nm or less. In this case, it is possible to more reliably reduce bonding defects in hybrid bonding.
[0017]
[11] The semiconductor device manufacturing method according to any one of [1] to
[10] above may further include the steps of: preparing a second semiconductor substrate having a second substrate body, a second organic insulating film, and a second electrode provided on one surface of the second substrate body; aligning the second electrode of the second semiconductor substrate with the first electrode of the first semiconductor substrate; and heating and pressurizing the first semiconductor substrate and the second semiconductor substrate to bond the first organic insulating film and the second organic insulating film to each other and to bond the first electrode and the second electrode to each other. In this case, the first semiconductor substrate and the second semiconductor substrate can be bonded by hybrid bonding. Note that the hybrid bonding referred to here may be hybrid bonding used in either a wafer-to-wafer (W2W) bonding process or a chip-on-wafer (CoW) bonding process.
[0018]
[12] The method for manufacturing a semiconductor device according to
[11] above may further include a step of irradiating a surface of the second semiconductor substrate with plasma, and in the step of irradiating the second semiconductor substrate with plasma, at least the second organic insulating film may be etched by the plasma so that the surface of the second organic insulating film is closer to the second substrate body than the tip surface of the second electrode. In this case, by changing the plasma conditions depending on the materials of the organic insulating film and the electrode or the difference in elastic modulus between them, it becomes possible to easily provide a desired step between the surface of the organic insulating film of the semiconductor substrate and the tip surface of the electrode in the second semiconductor substrate as well.
[0019]
[13] In any of the semiconductor device manufacturing methods [1] to
[12] above, the resin material contained in the first organic insulating film may include bismaleimide, polyimide, a polyimide precursor, polyamideimide, benzocyclobutene (BCB), polybenzoxazole (PBO), or a PBO precursor. These materials are liquid or soluble in a solvent, making it easy to prepare the first organic insulating film by, for example, spin coating, and to form a thin film. Furthermore, these materials have high heat resistance, so they can withstand the high temperatures encountered when bonding the first semiconductor substrate to the second semiconductor substrate, enabling more reliable bonding of the substrates. The second organic insulating film of the second semiconductor substrate may also be formed using the organic material described above. Similar effects can be achieved in this case as well.
[0020] According to the present disclosure, in a hybrid bonding method using an organic insulating film, a desired step can be easily formed between the surface of the organic insulating film of a semiconductor substrate and the tip surface of the electrode.
[0021] Fig. 1 is a cross-sectional view schematically showing an example of a semiconductor device (CoW) manufactured by a semiconductor device manufacturing method according to an embodiment of the present disclosure. Fig. 2 is a diagram sequentially showing a method for manufacturing the semiconductor device shown in Fig. 1. Fig. 3 is a diagram schematically showing a plasma process in the method for manufacturing the semiconductor device shown in Fig. 2. Fig. 4 is a diagram showing a bonding method in the method for manufacturing the semiconductor device shown in Fig. 2.
[0022] Hereinafter, several embodiments of the present disclosure will be described in detail, with reference to the drawings as necessary. In the following description, identical or equivalent parts will be designated by the same reference numerals, and duplicate explanations will be omitted. Furthermore, positional relationships such as up, down, left, and right will be based on the positional relationships shown in the drawings unless otherwise specified. When terms such as "left," "right," "front," "back," "top," "bottom," "upper," and "lower" are used in the description and claims of this specification, these are intended for explanatory purposes and do not necessarily mean that these relative positions will always be the same. Furthermore, the dimensional ratios of the drawings are not limited to those shown in the drawings.
[0023] In this specification, the term "layer" encompasses not only a structure with a shape formed over the entire surface when observed in a plan view, but also a structure with a shape formed on a portion of the surface. Furthermore, in this specification, the term "process" includes not only an independent process, but also a process that cannot be clearly distinguished from other processes, as long as the intended effect of the process is achieved. Furthermore, a numerical range indicated using "to" indicates a range that includes the numerical values before and after "to" as the minimum and maximum values, respectively.
[0024] (Configuration of Semiconductor Device) FIG. 1 is a cross-sectional view schematically illustrating an example of a semiconductor device manufactured by a manufacturing method according to this embodiment. As shown in FIG. 1, the semiconductor device 1 is, for example, an example of a semiconductor package. The semiconductor device 1 includes multiple semiconductor chips 10 and a semiconductor substrate 20, and has a chip-on-wafer (CoW) structure. The multiple semiconductor chips 10 are fabricated by dicing a semiconductor substrate 100 (described later) into individual chips. The multiple semiconductor chips 10 are mounted on the semiconductor substrate 20 to form a three-dimensional mounting structure. The semiconductor substrate 20 may be a substrate on which multiple semiconductor chips, such as LSI (Large Scale Integrated Circuit) chips or CMOS (Complementary Metal Oxide Semiconductor) sensors, are formed in locations corresponding to the respective semiconductor chips 10. Each semiconductor chip 10 may be a semiconductor chip such as an LSI or memory. The multiple semiconductor chips 10 and the semiconductor substrate 20 are finely bonded to each other by hybrid bonding (described later) to firmly and without misalignment, with their respective terminal electrodes and their surrounding insulating films. 1 , the semiconductor device 1 may be further singulated into individual semiconductor devices each including one semiconductor chip 10 and a substrate portion that is a part of the semiconductor substrate 20 corresponding to one semiconductor chip 10. The manufacturing method according to this embodiment may also be applied to a W2W bonding process, in which case semiconductor substrates are bonded to each other.
[0025] (Method for manufacturing semiconductor device) Next, a method for manufacturing the semiconductor device 1 will be described with reference to Fig. 2 to Fig. 4. Fig. 2 is a diagram sequentially showing a method for manufacturing the semiconductor device shown in Fig. 1. Fig. 3 is a diagram schematically showing a plasma process in the method for manufacturing the semiconductor device shown in Fig. 2. Fig. 4 is a diagram showing a bonding method in the method for manufacturing the semiconductor device shown in Fig. 2.
[0026] The semiconductor device 1 can be manufactured, for example, through the following steps (a) to (j): (a) preparing a semiconductor substrate 100 corresponding to a plurality of semiconductor chips 10, the semiconductor substrate 100 having a substrate body 101, an insulating film 102, and a plurality of electrodes 103; (b) preparing a semiconductor substrate 200 having a substrate body 201, an insulating film 202, and a plurality of electrodes 203; (c) polishing the insulating film 102 of the semiconductor substrate 100 together with the electrodes 103; (d) polishing the insulating film 202 of the semiconductor substrate 200 together with the electrodes 203; (e) irradiating the insulating film 102 and the electrodes 103 of the semiconductor substrate 100 with plasma; (f) irradiating the insulating film 202 and the electrodes 203 of the semiconductor substrate 200 with plasma; and (g) singulating the semiconductor substrate 100 to obtain a plurality of semiconductor chips 10, each of which has an insulating film portion 102b corresponding to the insulating film 102 and an electrode 103. (h) a step of aligning the electrodes 103 of each of the plurality of semiconductor chips 10 with the electrodes 203 of the semiconductor substrate 200. (i) a step of bonding the insulating film portions 102b of each of the plurality of semiconductor chips 10 to the insulating film 202 of the semiconductor substrate 200. (j) a step of bonding the electrodes 103 of each of the plurality of semiconductor chips 10 to the electrodes 203 of the semiconductor substrate 200.
[0027] [Steps (a) and (b)] Step (a) is a step of preparing a semiconductor substrate 100 (second semiconductor substrate), which is a silicon substrate on which integrated circuits composed of semiconductor elements and wiring connecting them are formed, corresponding to a plurality of semiconductor chips 10. In step (a), as shown in FIG. 2A, a plurality of electrodes 103 (second electrodes) made of copper, aluminum, or the like are provided at predetermined intervals on one surface 101a of a substrate body 101 (second substrate body) made of silicon or the like, and an insulating film 102 (second organic insulating film) made of an inorganic or organic material is provided. The electrodes 103 are terminal electrodes for exposing the integrated circuits formed on the semiconductor substrate 100 to the outside through the insulating film 102. The insulating film 102 may be provided on the one surface 101a of the substrate body 101 before the plurality of electrodes 103 are provided, or the insulating film 102 may be provided on the one surface 101a of the substrate body 101 before the plurality of electrodes 103 are provided.
[0028] Step (b) is a step of preparing a semiconductor substrate 200 (first semiconductor substrate), which is a silicon substrate on which integrated circuits consisting of semiconductor elements and wiring connecting them are formed. In step (b), as shown in FIG. 2A, a plurality of electrodes 203 (first electrodes) made of copper, aluminum, or the like are provided at predetermined intervals on one surface 201a of a substrate body 201 (first substrate body) made of silicon or the like, and an insulating film 202 (first organic insulating film) made of an inorganic or organic material is provided. The electrodes 203 are terminal electrodes for exposing the integrated circuits and the like formed on the semiconductor substrate 200 to the outside through the insulating film 202. The insulating film 202 may be provided on the one surface 201a of the substrate body 201 before the plurality of electrodes 203 are provided, or the insulating film 202 may be provided on the one surface 201a of the substrate body 201 before the plurality of electrodes 203 are provided.
[0029] The insulating film 102 and the insulating film 202 used in the steps (a) and (b) are configured to contain an organic material. Examples of the organic material used for the insulating film include polyimide, a polyimide precursor (e.g., polyimide ester or polyamic acid), polyamideimide, benzocyclobutene (BCB), polybenzoxazole (PBO), and a PBO precursor. These organic materials include, for example, silicon oxide (SiO 2The organic material has a lower elastic modulus than inorganic materials such as silicon dioxide, making it a soft material. By using such an organic material, when bonding insulating films together in step (i) described below, even if fine foreign matter (debris) is present on the insulating film, it is absorbed into the insulating film, preventing bonding defects due to the foreign matter, thereby enabling reliable bonding of the insulating films together. The elastic modulus of the organic material constituting the insulating film 102 and the insulating film 202 may be, for example, 7.0 GPa or less, 5.0 GPa or less, 3.5 GPa or less, 3.0 GPa or less, or 2.5 GPa or less. The elastic modulus here refers to Young's modulus. By forming the insulating film from an organic material having such an elastic modulus, the thickness of the insulating film can be easily reduced by plasma irradiation in steps (e) and (f) described below. Furthermore, the thermal expansion coefficient of the organic material constituting the insulating film 102 and the insulating film 202 is preferably 70 ppm / K or less, and more preferably 50 ppm / K or less.
[0030] Furthermore, since the organic materials used for the insulating films are liquid or soluble in a solvent, each insulating film can be easily formed as a thin film by spin coating or the like. Furthermore, since these organic materials are heat-resistant, they can withstand the temperatures (e.g., high temperatures of 300°C or higher) used when bonding the electrodes 103 and 203 in step (j) described below, preventing the bonding between the insulating films from deteriorating due to high temperatures. The organic material constituting the insulating films 102 and 202 may be a photosensitive resin, a thermosetting non-conductive film (NCF), or a thermosetting resin. This organic material may be an underfill material. The insulating films 102 and 202 may be insulating films containing both inorganic and organic materials, or one insulating film may be formed from an inorganic material and the other from an organic material. The inorganic material used for the insulating films may be, for example, silicon oxide (SiO 2 ) etc.
[0031] The thickness of the insulating film 102 may be 20 μm or less. By making the insulating film 102 sufficiently thin, the wiring formed from the electrodes 103 can be made finer. For example, the minimum size (electrode width) of the electrodes 103 formed in the insulating film 102 is determined by the thickness of the insulating film 102 and the aspect ratio of the photosensitive material used. When the aspect ratio of the photosensitive material is, for example, 1:1 (opening width:depth), the thickness of the insulating film 102 of 20 μm or less allows the electrode width of the electrodes 103 to be 20 μm or less. The thickness of the insulating film 102 may be greater than 20 μm. In this case, when the insulating films are bonded together in step (i) described below, more foreign matter can be embedded in the resin insulating film 102, thereby more reliably bonding the insulating films together. Furthermore, one of the resin insulating films can alleviate the stress generated when bonding the insulating films together, thereby improving the adhesion between the insulating films.
[0032] Furthermore, the thickness of the insulating film 102 may be 4 μm or more. In this case, by embedding minute foreign particles in the resin insulating film, it is possible to improve the connection between the insulating film 102 and the insulating film 202 even if minute foreign particles remain. For example, the size of foreign particles that can be embedded in the insulating film 102 is determined by the thickness of the resin insulating film 102. If the thickness of the insulating film 102 is, for example, 4 μm, foreign particles with a diameter or width of 4 μm can be embedded in the insulating film 102. That is, according to this manufacturing method, even if debris smaller than the thickness of the insulating film 102 is present, embedding the debris in the resin insulating film makes it possible to improve the connection between the insulating film 102 and the insulating film 202. Note that the thickness of the insulating film 202 may be 20 μm or less, greater than 20 μm, or 4 μm or more, similar to the insulating film 102. As described above, the insulating film 202 may embed debris.
[0033] [Steps (c) and (d)] Step (c) is a step of polishing the semiconductor substrate 100. In step (c), the surface of the insulating film 102 on which the electrode 103 is provided is polished using a chemical mechanical polishing (CMP) method. This polishing is preferably performed before step (e) of plasma irradiation. This is because the surface of the insulating film 102 may be roughened by plasma irradiation in step (e), and the average roughness of the surface of the insulating film 102 is reduced in advance before joining by hybrid bonding. This polishing reduces the average roughness of the surface of the insulating film 102 to 5 nm or less, preferably 1 nm or less, enabling hybrid bonding, as described below. This polishing may remove debris from the surface of the semiconductor substrate 100. Note that this polishing step may also form a part of a step between the surface 102a of the insulating film 102 and the tip surface 103a of the electrode 103.
[0034] Step (d) is a step of polishing the semiconductor substrate 200. In step (d), the surface of the insulating film 202 on which the electrode 203 is provided is polished using a CMP method. This polishing is preferably performed before step (f). This is because, as in step (c), the surface of the insulating film 202 may be roughened by plasma irradiation in step (f), and the average roughness of the surface of the insulating film 202 is reduced before hybrid bonding. This polishing reduces the average roughness of the surface of the insulating film 202 to 5 nm or less, preferably 1 nm or less, enabling hybrid bonding, as described below. This polishing may remove debris from the surface of the semiconductor substrate 200. Note that this polishing step may also form a portion of a step between the surface 202a of the insulating film 202 and the tip surface 203a of the electrode 203.
[0035] In steps (c) and (d), the insulating film 102 may be polished so that the thickness of the insulating film 202 is the same as that of the insulating film 202. Alternatively, the insulating film 102 may be polished so that the thickness of the insulating film 102 is greater than that of the insulating film 202. On the other hand, the insulating film 102 may be polished so that the thickness of the insulating film 102 is less than that of the insulating film 202. When the insulating film 102 is thicker than the insulating film 202 and is made of an organic material, the insulating film 102 can contain most of the debris that adheres to the bonding interface during singulation into semiconductor chips 10 or during chip mounting, thereby reducing bonding defects. On the other hand, when the insulating film 102 is thinner than the insulating film 202, the height of the mounted semiconductor chip 10, i.e., the semiconductor device 1, can be reduced.
[0036] [Steps (e) and (f)] Step (e) is a step of irradiating plasma onto the insulating film 102 and the electrode 103 of the semiconductor substrate 100. In step (e), as shown in FIGS. 3A and 3B, the insulating film 102 is etched by the plasma so that the surface 102a of the insulating film 102 is closer to the substrate body 101 (toward the back) than the tip surface 103a of the electrode 103. The plasma used in step (e) is, for example, argon (Ar) plasma. The semiconductor substrate 100 is placed in a reduced pressure chamber, and the surface of the semiconductor substrate 100 is irradiated with argon plasma to perform etching. The argon plasma conditions are a flow rate of plasma gas (argon gas) of 3.38×10 -2 P.A.M. 3 / sec (20sccm) to 1.69Pa m 3 / sec (1000 sccm) (both refer to flow rates at 1 atmosphere and 0°C), the plasma output may be 10 W to 1000 W, and the plasma treatment time may be 30 seconds or more. The plasma treatment time may be 500 seconds or less. By irradiating with such plasma, as shown in FIG. 3B, the step D between the surface 102a of the insulating film 102 and the tip surface 103a of the electrode 103 becomes 40 nm or more and 100 nm or less. The formation of such a step D is due to the difference in elastic modulus between the insulating film 102 and the electrode 103. Plasma irradiation may be performed so that the step D between the surface 102a of the insulating film 102 and the tip surface 103a of the electrode 103 becomes 60 nm or more and 80 nm or less. From the viewpoint of an oxide film, argon plasma is preferable as the plasma to be used, but this is not limited thereto, and oxygen plasma or the like may also be used.
[0037] Step (f) is a step of irradiating plasma onto the insulating film 202 and the electrode 203 of the semiconductor substrate 200. In step (f), similar to step (e), the insulating film 202 is etched by the plasma so that the surface 202a of the insulating film 202 is closer to the substrate body 201 (toward the back) than the tip surface 203a of the electrode 203. The plasma used in step (f) is, for example, argon (Ar) plasma. The semiconductor substrate 200 is placed in a reduced pressure chamber, and the surface of the semiconductor substrate 200 is irradiated with argon plasma to perform etching. The argon plasma conditions are as follows: a flow rate of plasma gas (argon gas) of 3.38×10 -2 P.A.M. 3 / sec (20sccm) to 1.69Pa m 3 / sec (1000 sccm) (all meaning flow rates at 1 atmosphere and 0°C), the plasma output may be 10 W to 1000 W, and the plasma treatment time may be 30 seconds or more. The plasma treatment time may be 500 seconds or less. By irradiating with such plasma, as shown in FIG. 3B, the step D between the surface 202b of the insulating film 202 and the tip surface 203a of the electrode 203 becomes 40 nm or more and 100 nm or less. The formation of such a step D is due to the difference in elastic modulus between the insulating film 202 and the electrode 203. Plasma irradiation may be performed so that the step D between the surface 202b of the insulating film 202 and the tip surface 203a of the electrode 203 becomes 60 nm or more and 80 nm or less. Similar to step (e), a plasma other than argon may be used.
[0038] [Step (g)] Step (g) is a step of singulating the semiconductor substrate 100 to obtain multiple semiconductor chips 10. After polishing the semiconductor substrate 200, step (g) singulates the polished semiconductor substrate 100 to obtain multiple semiconductor chips 10 (semiconductor substrates), each of which has an insulating film portion 102b corresponding to the insulating film 102 and at least one electrode 103. In step (g), the semiconductor substrate 100 is placed on a dicing tape and singulated into multiple semiconductor chips 10 by cutting means such as dicing from the insulating film 102 toward the substrate body 101. When dicing the semiconductor substrate 100, the insulating film 102 may be covered with a protective material or the like before being singulated. In step (g), the insulating film 102 of the semiconductor substrate 100 is divided into insulating film portions 102b corresponding to each semiconductor chip 10, as shown in FIG. 2B. Similarly, the substrate body 101 is divided into corresponding substrate portions 101b. For example, plasma dicing, stealth dicing, or laser dicing can be used as a dicing method for dividing the semiconductor substrate 100. After the division by dicing is completed in step (g), the divided semiconductor chips 10 may be washed.
[0039] [Step (h)] Step (h) is a step of aligning the electrodes 103 of each of the multiple semiconductor chips 10 with the electrodes 203 of the semiconductor substrate 200, as shown in FIG. 2C (left side) and FIG. 4A. In step (h), each semiconductor chip 10 is aligned so that each electrode 103 of each semiconductor chip 10 faces the corresponding electrode 203 of the semiconductor substrate 200. FIG. 4A is a schematic diagram of an enlarged portion of FIG. 2C. As shown in FIG. 4A, before heating for bonding, steps remain between the insulating film portion 102b and the electrode 103, and between the insulating film 202 and the electrode 203. That is, the electrodes 103 and 203 protrude from the surfaces of the insulating film portion 102b and the insulating film 202.
[0040] [Step (i)] Step (i) is a step of bonding each insulating film portion 102b of the multiple semiconductor chips 10 to the insulating film 202 of the semiconductor substrate 200. In step (i), organic matter or metal oxide adhering to the surfaces of each semiconductor chip 10 and the semiconductor substrate 200 is removed, and then the semiconductor chip 10 is aligned with the semiconductor substrate 200. Once this is complete, as shown in (c) (right side) of FIG. 2 and (b) of FIG. 4, the insulating film portion 102b of each of the multiple semiconductor chips 10 is bonded to the insulating film 202 of the semiconductor substrate 200 by hybrid bonding. At this time, the insulating film portions 102b of the multiple semiconductor chips 10 and the insulating film 202 of the semiconductor substrate 200 may be uniformly heated before bonding. Heating for bonding causes the insulating film made of an organic material to expand more than the electrode, eliminating the step between the insulating film portion 102b and the electrode 103 and the step between the insulating film 202 and the electrode 203. This step may be completely eliminated, so that the surfaces of the insulating film portion 102b and the electrode 103 are flush, and the surfaces of the insulating film 202 and the electrode 203 are flush, or a slight step may remain. The temperature difference between the semiconductor chip 10 and the semiconductor substrate 200 during bonding is preferably, for example, 10°C or less. By performing heat bonding at such a uniform temperature, the insulating film portion 102b and the insulating film 202 are bonded to form an insulating bonded portion, and multiple semiconductor chips 10 are mechanically and firmly attached to the semiconductor substrate 200. Furthermore, since heat bonding is performed at a uniform temperature, misalignment at the bonding points is less likely to occur, allowing for high-precision bonding. At this attachment stage, the electrodes 103 of the semiconductor chip 10 and the electrodes 203 of the semiconductor substrate 200 are spaced apart and not connected (although they are aligned). The semiconductor chip 10 may be bonded to the semiconductor substrate 200 by other bonding methods, such as room-temperature bonding.
[0041] [Step (j)] Step (j) is a step of bonding the electrodes 103 of each of the multiple semiconductor chips 10 to the electrodes 203 of the semiconductor substrate 200. In step (j), as shown in FIG. 2D, after the bonding in step (i) is completed, a predetermined amount of heat H and / or pressure is applied to bond the electrodes 103 of the multiple semiconductor chips 10 to the electrodes 203 of the semiconductor substrate 200 by hybrid bonding. When the electrodes 103 and 203 are made of copper, the annealing temperature in step (j) is preferably 150°C or higher and 400°C or lower, and more preferably 200°C or higher and 300°C or lower. This bonding process forms an electrode bonded portion where the electrode 103 and the corresponding electrode 203 are bonded, and the electrodes 103 and 203 are firmly bonded mechanically and electrically. The electrode bonding in step (j) is performed after the bonding in step (i), but may also be performed simultaneously with the bonding in step (i). Thereafter, all the semiconductor chips 10 are bonded to the semiconductor substrate 200 to obtain the semiconductor device 1 shown in FIG.
[0042] As a result, it is possible to obtain a semiconductor device 1 in which a plurality of semiconductor chips 10 are electrically and mechanically installed with high precision at predetermined positions on the semiconductor substrate 200. After this, the semiconductor device (CoW) having the configuration shown in Fig. 1 may be further diced into individual pieces to form individual semiconductor devices each composed of one semiconductor chip 10 and a portion of the semiconductor substrate 200 corresponding to that semiconductor chip 10.
[0043] As described above, in the semiconductor device manufacturing method according to this embodiment, in steps (e) and (f), the insulating films 102 and 202 are etched with plasma so that the surfaces of the insulating films 102 and 202 are closer to the substrate body 101 and 201 than the leading edges of the electrodes 103 and 203. In this case, although plasma is irradiated toward both the insulating films 102 and 202 and the electrodes 103 and 203, the amount of etching by the plasma varies depending on factors such as the difference in elastic modulus between the insulating films 102 and 202 and the electrodes 103 and 203. Therefore, according to this manufacturing method, by changing the plasma conditions depending on the materials of the organic insulating film and the electrodes or the difference in elastic modulus between the insulating films 102 and 202, it is possible to easily form a desired step D between the surface of the insulating film 202 of the semiconductor substrate 100 and the leading edges of the electrodes 103 and 203 in a hybrid bonding method using the insulating films 102 and 202.
[0044] In the method for manufacturing a semiconductor device according to this embodiment, in steps (e) and (f), it is preferable to irradiate argon plasma onto the semiconductor substrates 100 and 200. In this case, it becomes easier to adjust the step between the surface of the insulating film 102 or 202 of the semiconductor substrate 100 or 200 and the tip end face of the electrode 103 or 203 to a desired value.
[0045] In the manufacturing method of the semiconductor device according to this embodiment, in steps (e) and (f), the flow rate of the plasma gas is 3.38×10 -2 P.A.M. 3 / sec (20sccm) to 1.69Pa m 3 / sec (1000 sccm). -2 P.A.M. 3 By setting the flow rate of the plasma gas to 1.69 Pa·m / sec (20 sccm) or more, etching by plasma is promoted, and the step between the surface of the insulating film 102, 202 of the semiconductor substrate 100, 200 and the tip surface of the electrode 103, 203 can be quickly set to a desired value. 3 By setting the flow rate to 1000 sccm or less, roughening of the surfaces of the insulating films 102 and 202 and the electrodes 103 and 203 due to the plasma can be suppressed.
[0046] In the semiconductor device manufacturing method according to this embodiment, the plasma output in steps (e) and (f) is preferably 10 W to 1000 W. A plasma output of 10 W or more promotes plasma etching, allowing the step height between the surface of the insulating film 102, 202 of the semiconductor substrate 100, 200 and the tip surface of the electrode 103, 203 to be quickly reduced to a desired value. On the other hand, a plasma output of 1000 W or less can prevent the surfaces of the insulating film 102, 202 and the electrode 103, 203 from being roughened by the plasma.
[0047] In the method for manufacturing a semiconductor device according to this embodiment, the plasma treatment time is preferably 30 seconds or more in steps (e) and (f). By setting the plasma treatment time to 30 seconds or more, etching by plasma can be promoted, and the step between the surface of the insulating film 102, 202 of the semiconductor substrate 100, 200 and the tip surface of the electrode 103, 203 can be quickly set to a desired value.
[0048] In the method for manufacturing a semiconductor device according to this embodiment, the elastic modulus of the insulating films 102 and 202 is preferably 7.5 GPa or less, which makes it possible to easily provide a desired step between the surface of the insulating films 102 and 202 of the semiconductor substrates 100 and 200 and the tip surfaces of the electrodes 103 and 203.
[0049] In the manufacturing method of the semiconductor device according to this embodiment, in steps (e) and (f), plasma may be irradiated onto the surfaces of the semiconductor substrates 100 and 200 so that the step distance between the surfaces of the insulating films 102 and 202 and the tip surfaces of the electrodes 103 and 203 is 40 nm or more and 100 nm or less. In this case, when the semiconductor substrates 100 and 200 are bonded to each other, the amount of misalignment between the surfaces of the insulating films 102 and 202 and the tip surfaces of the electrodes 103 and 203 is reduced due to thermal expansion, making it possible to more reliably bond the semiconductor substrates 100 and 200 to each other.
[0050] In the manufacturing method of the semiconductor device according to this embodiment, in steps (e) and (f), plasma may be irradiated onto the surfaces of the semiconductor substrates 100 and 200 so that the step distance between the surfaces of the insulating films 102 and 202 and the tip surfaces of the electrodes 103 and 203 is 60 nm or more and 80 nm or less. In this case, when the semiconductor substrates 100 and 200 are bonded to each other by hybrid bonding, the amount of misalignment between the surfaces of the insulating films 102 and 202 and the tip surfaces of the electrodes 103 and 203 is reduced due to thermal expansion, making it possible to more reliably bond the semiconductor substrates 100 and 200 to each other.
[0051] The semiconductor device manufacturing method according to this embodiment further includes a step of polishing the insulating films 102, 202 and the electrodes 103, 203 formed on one surface of the semiconductor substrate 100, 200. The step of polishing the semiconductor substrate 100, 200 is preferably performed before the plasma irradiation steps (e) and (f). While plasma irradiation can achieve a desired step height between the surface of the insulating film 102, 202 of the semiconductor substrate 100, 200 and the tip surfaces of the electrodes 103, 203, depending on the plasma output, it may worsen the surface roughness of the insulating film 102, 202 or the tip surfaces of the electrodes 103, 203. In hybrid bonding, poor surface roughness of the bonding surfaces can lead to poor hybrid bonding. Therefore, this manufacturing method reduces the surface roughness of the surfaces and tip surfaces that would otherwise be roughened by plasma irradiation by polishing in advance. This manufacturing method therefore makes it possible to reduce poor hybrid bonding. Furthermore, in the polishing steps (c) and (d), it is possible to reduce the surface roughness of the organic insulating film surface and the tip surface of the electrode on the semiconductor substrate 100, 200 while achieving a desired step height between the organic insulating film surface and the tip surface of the electrode. However, it is difficult to adjust a fine step height by polishing. Therefore, if the desired step height cannot be obtained in the polishing steps (c) and (d), the step height can be further adjusted by performing plasma irradiation steps (e) and (f) after the polishing steps (c) and (d).
[0052] In the method for manufacturing a semiconductor device according to this embodiment, in the polishing steps (c) and (d), polishing is preferably performed so that the surface roughness Ra of each of the surfaces of the insulating films 102 and 202 and the electrodes 103 and 203 is 5 nm or less, preferably 1 nm or less, which makes it possible to more reliably reduce bonding defects in hybrid bonding.
[0053] In the semiconductor device manufacturing method according to this embodiment, the resin material contained in the insulating film 102, 202 may include bismaleimide, polyimide, a polyimide precursor, polyamideimide, benzocyclobutene (BCB), polybenzoxazole (PBO), or a PBO precursor. These materials are liquid or soluble in a solvent, which facilitates the preparation of the insulating film 102, 202 by, for example, spin coating, and facilitates the formation of a thin film. Furthermore, these materials have high heat resistance, which allows them to withstand the high temperatures encountered when bonding the semiconductor chip 10 (semiconductor substrate 100) to the semiconductor substrate 200, thereby enabling more reliable bonding of the substrates.
[0054] Although the embodiments of the present disclosure have been described in detail above, the present disclosure is not limited to the above embodiments and can be applied to various embodiments. For example, although the above describes a semiconductor device manufacturing method using a CoW bonding process as an example of hybrid bonding, the semiconductor device manufacturing method according to the present embodiment may also be applied to a wafer-to-wafer (W2W) bonding process. In this case, the semiconductor substrate 100 and the semiconductor substrate 200 that have undergone steps (e) and (f) are bonded by hybrid bonding without performing step (g) of dicing the first semiconductor substrate into individual pieces.
[0055] The present invention will be described in more detail below with reference to examples, but the present invention is not limited to these examples. In the following examples (experimental examples), a semiconductor substrate having an organic insulating film and an electrode on one surface of a substrate body was prepared, and plasma was irradiated onto the semiconductor substrate to test whether the step between the surface of the organic insulating film and the tip surface of the electrode could be adjusted.
[0056] First, a test wafer corresponding to the semiconductor substrate 100 was prepared. In this preparation, a first polyimide material and a second polyimide material were prepared as materials for the organic insulating film used in the test wafer. The first polyimide material has a glass transition temperature after hardening of 290°C and a coefficient of linear expansion (CTE) of 100 ppm / °C (10 ―6 The second polyimide material had a glass transition temperature after curing of 267°C, a coefficient of linear expansion (CTE) of 75 ppm / °C, and a modulus of elasticity of 3.1 GPa. The linear expansion coefficient of copper used in the electrodes was 16.8 ppm / °C (10 ―6 / °C) and the elastic modulus was 120 GPa.
[0057] Next, as Experimental Example 1, as shown in FIG. 3, a number of electrodes 103, which were copper pillars (Cu) measuring 10 μm square and 6 μm high, were fabricated by a semi-additive method on a substrate body 101, which was a silicon substrate. The first polyimide material described above was then spin-coated onto the substrate body 101 to cover the electrodes 103, and baked at 375° C. for 2 hours in a nitrogen atmosphere to harden (see FIG. 3A). The hardened semiconductor substrate 100 was then placed in a reduced-pressure chamber, and argon plasma was applied to the semiconductor substrate 100 under the following plasma conditions (see FIG. 3B). RF power (plasma power): 500 W (watts); treatment time (plasma treatment time): 120 seconds; Ar flow rate (flow rate of plasma gas): 8.45×10 -2 P.A.M. 3 / sec(50sccm)
[0058] After plasma irradiation was completed, the step D between the surface of the organic insulating film and the tip surface of the electrode, the surface roughness Ra of the surface of the organic insulating film, and the surface roughness Ra of the tip surface of the electrode were measured, and the following results were obtained. Step D between the surface of the organic insulating film and the tip surface of the electrode: 72.4 nm Surface roughness Ra of the surface of the organic insulating film: 1.5 nm Surface roughness Ra of the tip surface of the electrode: 2.6 mm According to the test under the plasma conditions of Experimental Example 1, it was confirmed that the step D was 40 nm to 80 nm, which is the range in which the compression bonding properties of hybrid bonding are good (when the elastic modulus is 2.5 GPa). It was also confirmed that the surface roughness Ra of the organic insulating film and the electrode could be kept to low values.
[0059] Next, in Experimental Examples 2 to 6, the first polyimide material having an elastic modulus of 2.5 GPa was used as is, and plasma was irradiated onto the semiconductor substrate 100 under different plasma conditions. Conditions other than the plasma irradiation conditions were the same as in Experimental Example 1. The plasma conditions and test results for Experimental Examples 2 to 6 were as shown in Table 1 below. Note that the evaluation A for the compression bondability in Table 1 indicates that, as described above, the step D was within the range in which the compression bondability of hybrid bonding was good.
[0060] Next, in Experimental Examples 7 to 10, a second polyimide material with an elastic modulus of 3.1 GPa was used, and plasma was irradiated onto the semiconductor substrate under different plasma conditions. Conditions other than the elastic modulus of the organic insulating film material and the plasma irradiation conditions were the same as in Experimental Example 1. The plasma conditions and test results for Experimental Examples 7 to 10 are shown in Table 2 below. When the elastic modulus was 3.1 GPa, if the step D was in the range of 15 nm to 50 nm, the compression bonding properties of the hybrid bonding were good, and this was given an evaluation of A. Furthermore, in Experimental Examples 7 to 10, it was confirmed that the surface roughness Ra of the organic insulating film and the electrode could also be kept low.
[0061] Next, Experimental Examples 11 to 17 were conducted as further experimental examples. In Experimental Examples 11 to 17, a first polyimide material having an elastic modulus of 2.5 GPa was used as in Experimental Example 1, and plasma was irradiated onto the semiconductor substrate 100 under different plasma conditions. Conditions other than the plasma irradiation conditions were the same as in Experimental Example 1. The plasma conditions and test results for Experimental Examples 11 to 17 were as shown in Table 3 below. In Experimental Examples 11 to 17, tests were conducted under significantly different plasma conditions compared to Experimental Example 1 and the like.
[0062] As shown in Experimental Examples 11 to 17, it was confirmed that the step D and surface roughness Ra could be changed (i.e., various adjustments could be made) by changing the plasma conditions. Note that for those in which the step D was insufficient (e.g., Experimental Example 15) and those in which the step D was too large (e.g., Experimental Example 17), it was considered possible to use them for hybrid bonding by adjusting the step D and surface roughness Ra to the desired value by performing a process such as CMP before the plasma treatment.
[0063] As described above, according to the above experimental examples, it was confirmed that when plasma is irradiated toward both the organic insulating film and the electrode, the amount of etching by the plasma can be varied depending on the difference in elastic modulus between the two, etc. Furthermore, it was confirmed that in the plasma treatment of such an organic insulating film, by changing the plasma conditions depending on the materials of the organic insulating film and the electrode or the difference in elastic modulus between the two, etc., it is possible to easily provide a desired step between the surface of the organic insulating film of the semiconductor substrate and the tip surface of the electrode in a hybrid bonding method using an organic insulating film.
[0064] 1...semiconductor device, 10...semiconductor chip, 20...semiconductor substrate, 100, 200...semiconductor substrate, 101, 201...substrate body, 101a, 201a...one surface, 102, 202...insulating film, 102a, 202a...surface, 102b...insulating film portion, 103, 203...electrode, 103a, 203a...tip surface, D...step.
Claims
1. A method for manufacturing a semiconductor device, comprising: a step of preparing a first semiconductor substrate having a first substrate body, and a first organic insulating film and a first electrode provided on one surface of the first substrate body; and a step of irradiating a surface of the first semiconductor substrate with plasma, wherein in the step of irradiating with plasma, at least the first organic insulating film is etched by the plasma so that the surface of the first organic insulating film is closer to the first substrate body than the tip surface of the first electrode.
2. The method for manufacturing a semiconductor device according to claim 1, wherein in the step of irradiating the plasma, the first semiconductor substrate is irradiated with argon plasma.
3. In the plasma irradiation step, the flow rate of the plasma gas is 3.38×10 -2 P.A.M. 3 / sec (20 sccm) to 1.69 Pa m 3 3. The method for manufacturing a semiconductor device according to claim 1, wherein the flow rate of the gas is 1000 sccm / sec (1000 sccm).
4. The method for manufacturing a semiconductor device according to any one of claims 1 to 3, wherein in the step of irradiating the plasma, a plasma output is 10 W to 1000 W.
5. The method for manufacturing a semiconductor device according to any one of claims 1 to 4, wherein in the step of irradiating the substrate with plasma, the plasma treatment time is 30 seconds or more.
6. The method for manufacturing a semiconductor device according to any one of claims 1 to 5, wherein the first organic insulating film has an elastic modulus of 7.5 GPa or less.
7. The method for manufacturing a semiconductor device according to any one of claims 1 to 6, wherein in the step of irradiating with plasma, the surface of the first semiconductor substrate is irradiated with plasma so that a step distance between the surface of the first organic insulating film and the tip face of the first electrode is 40 nm or more and 100 nm or less.
8. A method for manufacturing a semiconductor device according to any one of claims 1 to 6, wherein in the step of irradiating plasma, the surface of the first semiconductor substrate is irradiated with plasma so that a step distance between the surface of the first organic insulating film and the tip face of the first electrode is 60 nm or more and 80 nm or less.
9. A method for manufacturing a semiconductor device according to any one of claims 1 to 8, further comprising a step of polishing the first organic insulating film and the first electrode provided on the one surface of the first semiconductor substrate, the step of polishing the first semiconductor substrate being carried out before the step of irradiating with plasma.
10. The method for manufacturing a semiconductor device according to claim 9, wherein in the step of polishing the first semiconductor substrate, polishing is performed so that the surfaces of the first organic insulating film and the first electrode have a surface roughness Ra of 5 nm or less.
11. A method for manufacturing a semiconductor device according to any one of claims 1 to 10, further comprising the steps of: preparing a second semiconductor substrate having a second substrate body, and a second organic insulating film and a second electrode provided on one surface of the second substrate body; aligning the second electrode of the second semiconductor substrate with the first electrode of the first semiconductor substrate; and heating and pressurizing the first semiconductor substrate and the second semiconductor substrate to bond the first organic insulating film and the second organic insulating film to each other and to bond the first electrode and the second electrode to each other.
12. A method for manufacturing a semiconductor device as described in claim 11, further comprising a step of irradiating a surface of the second semiconductor substrate with plasma, wherein in the step of irradiating the second semiconductor substrate with plasma, at least the second organic insulating film is etched by the plasma so that the surface of the second organic insulating film is closer to the second substrate body than the tip surface of the second electrode.
13. The method for manufacturing a semiconductor device according to any one of claims 1 to 12, wherein the resin material contained in the first organic insulating film includes bismaleimide, polyimide, a polyimide precursor, polyamideimide, benzocyclobutene (BCB), polybenzoxazole (PBO), or a PBO precursor.
Citation Information
Patent Citations
Method for etching, and manufacturing of semiconductor device using the method
JP2000340549A
Active matrix substrate, method for manufacturing same, and display device using same
JP2004038047A
Organic el display and its manufacturing method
JP2006085916A
Active matrix type display device and manufacturing method for active matrix type display device
JP2006106575A
Liquid crystal display device and method of manufacturing the same
JP2009015199A