Method for producing nonwoven fabric sheet, device for producing nonwoven fabric sheet, and nonwoven fabric sheet
The method of adjusting low-viscosity liquid material viscosity and applying it to nonwoven fabric sheets addresses the neck-in issue, ensuring consistent and strong sheet production, overcoming the limitations of traditional extrusion molding techniques.
Patent Information
- Application Number
- PCT/JP2023/042002
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-04-11
- Filing Date
- 2023-11-22
- Publication Date
- 2024-10-17
AI Technical Summary
The existing methods for manufacturing nonwoven fabric sheets using extrusion molding face challenges when dealing with low-viscosity molten resin, as they often result in neck-in phenomena, leading to sheets with undesired shapes and dimensions.
A method and apparatus that adjust the viscosity of the liquid material to 100,000 mPa·s or less, using a combination of heating and solvent mixing, and apply it to nonwoven fabric using a coating machine, followed by impregnation and solidification to produce sheets with desired shapes, incorporating a solvent evaporation step for enhanced efficiency.
This approach allows for stable production of nonwoven fabric sheets with improved strength and shape consistency, even with low-viscosity materials, expanding the range of applicable raw materials and enhancing handling ease.
Smart Images

Figure JP2023042002_17102024_PF_FP_ABST
Abstract
Description
Nonwoven fabric sheet manufacturing method, nonwoven fabric sheet manufacturing apparatus, and nonwoven fabric sheet
[0001] The present invention relates to a method for manufacturing a nonwoven fabric sheet, an apparatus for manufacturing a nonwoven fabric sheet, and a nonwoven fabric sheet.
[0002] A widely known method for producing a sheet is to melt raw materials in an extruder and extrude the resulting molten resin into a sheet shape from an extrusion die (T die) (see, for example, Patent Document 1 (JP 2020-146853 A)).
[0003] Japanese Patent Application Laid-Open No. 2020-146853
[0004] Incidentally, a predetermined distance (air gap) is provided between the extrusion die (T-die) and the cooling roll for the extruded molten resin. In the air gap, the weight, tension, speed, etc. of the molten resin cause a phenomenon called neck-in, in which the width of the obtained film becomes narrower than the die width.
[0005] At this time, if the viscosity of the molten resin is low, the amount of neck-in tends to be large, which may make it difficult to produce a sheet with the desired shape.
[0006] Therefore, an object of the present invention is to provide a method and apparatus for manufacturing a nonwoven fabric sheet that can produce a sheet of a desired shape when manufacturing a sheet made of a resin material, even if the viscosity of the liquid material containing the raw material is low. Other objects and novel features will become apparent from the description of this specification and the accompanying drawings.
[0007] One embodiment of a method for manufacturing a nonwoven fabric sheet includes: (a) preparing a liquid material containing raw materials and having a viscosity of 100,000 mPa·s or less; (b) applying the liquid material to a nonwoven fabric in the form of a sheet using a coating machine; (c) impregnating the nonwoven fabric with the liquid material; (d) solidifying the liquid material impregnated into the nonwoven fabric to obtain a nonwoven fabric sheet; and (e) winding up the nonwoven fabric sheet.
[0008] One embodiment of the nonwoven fabric sheet manufacturing apparatus includes a raw material container that adjusts and stores a liquid material containing raw materials and having a predetermined viscosity, a nonwoven fabric discharge section that feeds out the nonwoven fabric, a coating machine that applies the liquid material to the nonwoven fabric, an impregnation area that impregnates the nonwoven fabric with the liquid material, a solidification area that solidifies the liquid material to form a nonwoven fabric sheet, and a sheet winding section that winds up the nonwoven fabric sheet.
[0009] In the above-described method and apparatus for producing a nonwoven fabric sheet, the liquid material is adjusted so that its viscosity is 100,000 mPa·s or less.
[0010] According to one embodiment, in the production of a nonwoven fabric sheet, even when a liquid material with a viscosity that would result in a large neck-in amount is used when an extrusion molding die (T-die) is used, the nonwoven fabric sheet can be stably produced.
[0011] Fig. 1 is a diagram showing a schematic configuration of a nonwoven fabric sheet manufacturing apparatus according to embodiment 1. Fig. 2 is a diagram illustrating a case where a gravure roll is applied as a coating machine in Fig. 1. Fig. 3 is a diagram showing a schematic configuration of a nonwoven fabric sheet manufacturing apparatus according to embodiment 2. Fig. 4 is a diagram showing the chemical structural formula of glucomannan. Fig. 5 is a diagram showing the chemical structural formula of cellulose. Fig. 6 is a diagram showing a schematic configuration of a moisture recovery device using a nonwoven fabric sheet. Fig. 7 is a diagram showing a schematic configuration of a moisture recovery device using a nonwoven fabric sheet.
[0012] Hereinafter, the present embodiment will be described in detail with reference to the drawings. In all the drawings for explaining the embodiment, the same reference numerals are used to designate components having the same functions, and repeated description thereof will be omitted.
[0013] First Embodiment <Nonwoven Fabric Sheet Manufacturing Apparatus> FIG. 1 is a diagram showing a schematic configuration of a nonwoven fabric sheet manufacturing apparatus according to the present embodiment.
[0014] The nonwoven fabric sheet manufacturing apparatus 10 shown in Figure 1 includes a raw material container 11 that prepares and stores a liquid material LM containing raw materials and having a viscosity of 100,000 mPa·s or less, a nonwoven fabric discharge section 12 that feeds out the nonwoven fabric NW, a coating machine 13 that applies the liquid material LM to the nonwoven fabric NW fed out from the nonwoven fabric discharge section 12, an impregnation area 14 that impregnates the nonwoven fabric NW with the sheet-like liquid material SLM applied to the nonwoven fabric NW, a solidification area 15 that solidifies the liquid material SLM impregnated into the nonwoven fabric NW to form a nonwoven fabric sheet 50, and a sheet winding section 16 that winds up the nonwoven fabric sheet 50 after the solidification area 15.
[0015] The raw material container 11 is a container for preparing and storing a liquid material containing the raw material and having a viscosity of 100,000 mPa·s or less. The liquid material stored in the raw material container 11 can also be referred to as a coating liquid to be applied onto the nonwoven fabric NW by a coating machine 13 described later.
[0016] This raw material container 11 contains raw material and adjusts it to a liquid material with a viscosity of 100,000 mPa·s or less. For example, if the above viscosity is satisfied by heating and melting the raw material, only the raw material can be stored in the raw material container 11. In this case, viscosity adjustment can be achieved by providing a heating unit that heats the raw material to the above viscosity. An example of this heating unit is a heat source such as a heater. The raw material is heated by this heat source and maintained at that temperature within the raw material container 11.
[0017] The raw material can also be mixed with a solvent to adjust the viscosity to 100,000 mPa·s or less. For example, when the raw material must be heated to an extremely high temperature to be heated and melted as described above, and when it is difficult to achieve a viscosity of 100,000 mPa·s even after heating and melting, the raw material can be dissolved using a solvent to adjust the viscosity to 100,000 mPa·s or less. Even for raw materials whose viscosity becomes 100,000 mPa·s or less when heated and melted, the viscosity can be adjusted using a solvent.
[0018] In this way, when mixing the raw material and the solvent to form a raw material solution, for example, a solvent supply section that supplies the solvent to this raw material container 11 is provided, and the amount of solvent supplied is adjusted so that the raw material solution (liquid material) falls within the above-mentioned viscosity range.
[0019] The viscosity of the liquid material here is the viscosity of the coating liquid to be applied by the coater 13, and is preferably 10 to 80,000 mPa·s, and more preferably 100 to 10,000 mPa·s.
[0020] The nonwoven fabric discharge unit 12 is a component that feeds out the nonwoven fabric NW. Here, the nonwoven fabric NW is a substrate for coating with the liquid material. In this nonwoven fabric discharge unit, the nonwoven fabric NW is wound in a roll shape, and the nonwoven fabric NW can be continuously fed to the coating machine 13, where the liquid material can be coated on the surface of the nonwoven fabric NW.
[0021] The coater 13 is a device that coats the nonwoven fabric NW with the liquid material sent from the raw material container 11 by a pump or the like. This coater 13 can be a known coater used in sheet formation, such as a die coater, gravure coater, bar coater, or blade coater that performs a contact coating process. The coater 13 can coat the nonwoven fabric NW with the liquid material in a uniform width. These coaters can be selected, for example, depending on the viscosity of the liquid material.
[0022] 1 illustrates a case where a die coater is used as the coater 13. In this case, a slot die type die coater is preferred, in which a liquid material is extruded from a die head and coated onto the nonwoven fabric NW. In this case, a back roll 17 is provided at a position opposite the slit through which the liquid material is discharged in the coater 13, with the substrate interposed therebetween.
[0023] 2 illustrates an example in which a gravure coater is used as the coater 13. Fig. 2 is a diagram illustrating a configuration in which a gravure coater is used to coat a liquid material LM onto a substrate BM in the sheet manufacturing apparatus 10. Here, the cross-sectional structure of the gravure coater is shown so that the internal configuration can be seen.
[0024] 2 is a vertical coating machine with a chamber (tank) 13a arranged vertically (parallel to the direction of gravity). This coater has a chamber (tank) 13a for storing liquid material LM, a coating roll (gravure roll) CR partially immersed in the chamber (tank) 13a, a blade 13b for preventing the liquid material LM from splashing and for adjusting the amount of liquid on the roll surface, and a second blade 13c for preventing the coating liquid from leaking from the gap between the liquid material in the chamber (tank) and the coating roll (gravure roll) CR.
[0025] The first blade 13b is disposed on the rotation direction side of the coating roll CR so that the angle and pressing pressure of the first blade 13b can be adjusted to adjust the amount of liquid material LM adhering to the surface of the coating roll CR. Then, the liquid material LM adhering to the surface of the coating roll CR is transferred to the surface of the substrate BM, thereby forming a sheet-like liquid material SLM.
[0026] The chamber (tank) 13a of the gravure coater may be either vertical or horizontal. If it is horizontal, the second blade 13c for preventing leakage of the coating liquid is not required, and the gravure coater can be configured to have only the first blade 13b for preventing the liquid material LM from splashing and adjusting the amount of liquid on the roll surface.
[0027] The impregnation area 14 is an area where the sheet-like liquid material SLM coated by the coater 13 is impregnated into the nonwoven fabric NW. In this impregnation area 14, the sheet-like liquid material SLM is allowed to penetrate into the gaps between the fibers of the nonwoven fabric NW. For example, impregnation rolls 14a may be provided to sandwich the nonwoven fabric NW coated with the sheet-like liquid material SLM from above and below, thereby impregnating the nonwoven fabric NW with the sheet-like liquid material SLM. In this case, while FIG. 1 shows an example in which two sets of impregnation rolls 14a are provided, one set, or three or more sets may also be provided. Furthermore, the impregnation rolls 14a may be configured to apply pressure to the nonwoven fabric NW coated with the sheet-like liquid material SLM to promote impregnation.
[0028] Depending on the relationship between the viscosity of the liquid material LM used and the basis weight of the nonwoven fabric NW, the liquid material LM may be applied from the coating machine 13 onto the nonwoven fabric NW while the liquid material LM is being impregnated into the nonwoven fabric NW. If sufficient impregnation can be achieved in this manner, it is not necessary to provide an impregnation member such as an impregnation roll 14a.
[0029] The solidification region 15 is a region where the nonwoven fabric NW impregnated with the sheet-like liquid material SLM in the impregnation region 14 is solidified to form the nonwoven fabric sheet 50, and it is the raw material that solidifies at this time. In this solidification region 15, if the liquid material consists only of the raw material, the temperature of the liquid material (raw material) impregnated into the nonwoven fabric NW is lowered to solidify it. At this time, for example, the temperature of the raw material impregnated into the nonwoven fabric NW can be naturally lowered at room temperature, such as about 25°C, without providing any special cooling means, and the raw material can be solidified. Alternatively, a cooling means may be provided to actively lower the temperature of the raw material impregnated into the nonwoven fabric NW to solidify it.
[0030] Furthermore, when the liquid material is a raw material solution obtained by mixing a raw material and a solvent, the solvent is evaporated from the liquid material impregnated into the nonwoven fabric NW by heating or the like, thereby solidifying the material. In this case, the solvent can be evaporated naturally at room temperature or the like without providing a special heating means. Alternatively, a heating means such as a heater may be provided to actively increase the temperature of the liquid material impregnated into the nonwoven fabric NW, thereby promoting the evaporation of the solvent and solidifying the material.
[0031] As described above, by solidifying the liquid material impregnated into the nonwoven fabric NW, a nonwoven fabric sheet 50 in which the nonwoven fabric NW and the raw material are integrated is obtained.
[0032] The sheet winding unit 16 is a member that can wind up the obtained nonwoven fabric sheet 50 and store it as a roll of nonwoven fabric sheet. The nonwoven fabric sheet 50 wound here can be made into a roll of nonwoven fabric sheet product. Furthermore, if necessary, this nonwoven fabric sheet can be further processed to make a sheet product.
[0033] Furthermore, it is preferable to provide a feed roll 18 between the nonwoven fabric discharge section 12 and the sheet winding section 16 so that the nonwoven fabric NW can be stably fed out. The feed roll 18 sandwiches the nonwoven fabric NW (or the nonwoven fabric sheet 50 impregnated with the liquid material after the liquid material has been applied) and feeds it to the subsequent stage.
[0034] <Sheet Manufacturing Method> Next, a description will be given of a sheet manufacturing method in Embodiment 1. This sheet manufacturing method includes the steps of preparing a liquid material containing raw materials and having a viscosity of 100,000 mPa·s or less (step (a)), after step (a), applying the liquid material to a nonwoven fabric in the form of a sheet using a coater (step (b)), after step (b), impregnating the nonwoven fabric with the liquid material (step (c)), after step (c), solidifying the liquid material impregnated into the nonwoven fabric to obtain a nonwoven fabric sheet (step (d)), and after step (d), winding up the nonwoven fabric sheet (step (e)).
[0035] Hereinafter, a sheet manufacturing method using the sheet manufacturing apparatus 10 described with reference to FIG. 1 will be described as a specific apparatus configuration.
[0036] First, a step of preparing a liquid material containing raw materials and having a viscosity of 100,000 mPa·s or less is carried out (step (a)).
[0037] In this viscosity adjusting step, as described above, a liquid material containing the raw material and having a viscosity of 100,000 mPa·s or less is prepared in raw material container 11. For example, when the above viscosity is satisfied by heating and melting the raw material, only the raw material is stored in raw material container 11, and the raw material is heated to the above viscosity to adjust the viscosity.
[0038] Furthermore, when mixing the raw material with a solvent to adjust the viscosity to 100,000 mPa s or less, the supply amount of the solvent is adjusted so that the raw material solution (liquid material) obtained by mixing the raw material with the solvent has a viscosity within the above range. In this case, temperature adjustment such as heating may be combined as necessary.
[0039] The viscosity of the liquid material in step (a) is the viscosity of the coating liquid for coating by the coater 13, as described above, and is preferably 10 to 50,000 mPa·s, and more preferably 100 to 10,000 mPa·s.
[0040] Next, after the step (a), a step of applying the liquid material in the form of a sheet onto the nonwoven fabric using a coating machine is carried out (step (b)).
[0041] In this embodiment, a nonwoven fabric discharge section 12 is provided, and a liquid material LM is applied in sheet form onto the nonwoven fabric NW sent out from this nonwoven fabric discharge section 12 using a coating machine 13, thereby obtaining a sheet-shaped liquid material SLM (coated body).
[0042] The nonwoven fabric NW used here is not particularly limited, and any known nonwoven fabric can be used without limitation. Examples of this nonwoven fabric NW include inorganic fibers such as carbon fiber, glass fiber, and metal fiber, and chemical fibers such as nylon (polyamide), tetron, rayon, cupra, acetate, vinylon, acrylic, polyethylene terephthalate (polyester), polypropylene, aramid, polyester, polyimide, and polyacrylic. Natural fibers such as cellulose fiber, cotton, linter, kapok, flax, hemp, ramie, silk, and wool can also be used. Carbon fiber, glass fiber, and chemical fibers are preferred because they have relatively high rigidity and can increase the rigidity of the nonwoven fabric sheet 50 and improve the strength of the sheet itself.
[0043] The average fiber diameter of the fibers constituting the nonwoven fabric is preferably 0.1 μm to 0.5 mm, more preferably 0.4 μm to 200 μm. The average fiber length of the fibers is preferably 1 mm to 200 mm. The thickness of the nonwoven fabric is preferably 10 μm to 5 mm, more preferably 20 μm to 3 mm.
[0044] The basis weight of the nonwoven fabric NW is 0.1 to 10,000 g / m 2 is preferably 0.2 to 5000 g / m 2is more preferable. By setting the basis weight of the fibers in this range, not only can the voids in the nonwoven fabric NW be sufficiently impregnated with the liquid material, but also the strength of the nonwoven fabric sheet 50 can be maintained. It is preferable to select the basis weight of the nonwoven fabric NW appropriately after comprehensively considering the design strength, such as the tensile strength, bending strength, and fatigue strength, and the heat resistance of the nonwoven fabric sheet 50 impregnated with the liquid material.
[0045] In this case, the coating amount of the liquid material is adjusted according to the amount of raw material to be impregnated into the nonwoven fabric NW, and the thickness of the sheet-shaped liquid material SLM is determined. That is, when the liquid material consists only of raw material, all of the impregnated liquid material LM solidifies to form the nonwoven fabric sheet 50, so the coating amount is applied so that it corresponds to the impregnation amount. Also, when the liquid material is a raw material solution obtained by mixing raw material and solvent, the solvent from the impregnated liquid material LM evaporates, and the remaining raw material components solidify to form the nonwoven fabric sheet 50. Therefore, the coating amount of the liquid material LM is determined and applied taking into account the amount of raw material components.
[0046] When applying the liquid material LM, the thickness of the sheet-like liquid material SLM to be applied varies depending on various factors such as the conveying speed of the nonwoven fabric NW, the viscosity of the liquid material LM used, and the amount of liquid material LM discharged in the coating machine 13, so these application conditions can be adjusted to achieve the desired thickness.
[0047] The viscosity of the liquid material LM is set to 100,000 mPa·s or less as described above. The conveying speed of the nonwoven fabric NW is, for example, preferably 1 to 500 m / min, and more preferably 5 to 300 m / min.
[0048] It is preferable to select the coater 13 depending on the viscosity of the liquid material LM. For example, when the viscosity of the liquid material LM is 1000 mPa·s or more, it is preferable to use a die coater as the coater 13, and when the viscosity of the liquid material LM is less than 1000 mPa·s, it is preferable to use a gravure coater as the coater 13. Furthermore, when the viscosity of the liquid material LM is 10000 mPa·s or more, it is preferable to use a device having a screw shape, such as a single-screw extruder or a twin-screw extruder, instead of a pump.
[0049] Next, after the step (b), a step of impregnating the nonwoven fabric NW with the liquid material LM is carried out (step (c)).
[0050] In this embodiment, the sheet-like liquid material SLM formed by coating on the nonwoven fabric NW is allowed to soak into gaps between the fibers of the nonwoven fabric NW in the impregnation region 14. This impregnation operation can be performed, for example, by providing impregnation rolls 14a and sandwiching the nonwoven fabric NW coated with the sheet-like liquid material SLM from above and below, thereby impregnating the nonwoven fabric NW with the sheet-like liquid material SLM.
[0051] As described above, the impregnation roll 14a may be configured to apply pressure to the nonwoven fabric NW coated with the sheet-like liquid material SLM to promote impregnation. In this case, the pressure applied by the impregnation roll 14a is preferably 0.01 to 100 MPa, and more preferably 0.1 to 50 MPa.
[0052] As mentioned above, depending on the relationship between the viscosity of the liquid material LM used and the basis weight of the nonwoven fabric NW, the liquid material LM may be applied from the coating machine 13 onto the nonwoven fabric NW while the liquid material LM is being impregnated into the nonwoven fabric NW. If sufficient impregnation can be achieved in this manner, it is not necessary to provide an impregnation member such as the impregnation roll 14a.
[0053] Furthermore, after the step (c), a step (d) is carried out in which the liquid material impregnated into the nonwoven fabric NW is solidified to obtain a nonwoven fabric sheet 50.
[0054] In this embodiment, the liquid material impregnated in the nonwoven fabric NW is solidified to obtain a nonwoven fabric sheet 50 in which the nonwoven fabric NW and the liquid material (raw material) are integrated. Here, the solidification of the liquid material (raw material) is performed in a solidification region 15.
[0055] When the liquid material is composed of only raw materials, the temperature of the liquid material impregnated into the nonwoven fabric NW is lowered to solidify it. At this time, for example, the temperature of the raw material can be naturally lowered at room temperature or the like without providing a cooling means, and the raw material can be solidified. Alternatively, a cooling means may be provided to actively lower the temperature of the raw material and solidify it.
[0056] The solidification temperature is specific to the raw material used, and should be below the melting point or glass transition point of the raw material. By setting the temperature at this level, the liquid raw material solidifies and a sheet is obtained.
[0057] Furthermore, when the liquid material is a raw material solution obtained by mixing a raw material and a solvent, the solvent is evaporated from the liquid material impregnated into the nonwoven fabric NW by heating or the like, thereby solidifying the liquid material. At this time, the solvent may be evaporated naturally at room temperature or the like, but in order to improve manufacturing efficiency, it is preferable to provide a heating means such as a heater to heat the nonwoven fabric NW impregnated with the liquid material, thereby accelerating the evaporation of the solvent and solidifying the liquid material. In this manner, the nonwoven fabric sheet 50 can be formed.
[0058] After this solidification, the nonwoven fabric sheet 50 is wound up (step (e)). Here, the nonwoven fabric sheet 50 is wound up into a roll by the sheet winding unit 16. In this way, nonwoven fabric sheets can be continuously obtained as products.
[0059] By adopting the configuration of the above embodiment, even when a low-viscosity liquid material is used as the raw material, it is possible to prevent the sheet from being significantly different from the desired shape, such as necking, and the limitations on the raw materials that can be used are greatly relaxed, making it possible to provide a manufacturing technology for nonwoven fabric sheets with a wide range of applications. Furthermore, the nonwoven fabric sheets obtained in this manner are stronger than sheets made only from the raw material, and are easier to handle, which is preferable.
[0060] Second Embodiment <Nonwoven Fabric Sheet Manufacturing Apparatus> FIG. 3 is a diagram showing a schematic configuration of a nonwoven fabric sheet manufacturing apparatus according to another embodiment.
[0061] Similar to the sheet manufacturing apparatus 10 described above, the sheet manufacturing apparatus 20 shown in Figure 3 includes a raw material container 11 that prepares and stores a liquid material containing raw materials and having a viscosity of 100,000 mPa·s or less, a nonwoven fabric discharge section 12 that feeds out the nonwoven fabric NW, a coating machine 13 that applies the liquid material to the nonwoven fabric NW fed out from the nonwoven fabric discharge section 12, an impregnation area 14 that impregnates the nonwoven fabric NW with the liquid material applied to the nonwoven fabric NW, a solidification area 15 that solidifies the liquid material impregnated into the nonwoven fabric NW to form a nonwoven fabric sheet 50, and a sheet winding section 16 that winds up the nonwoven fabric sheet 50 after the solidification area 15.
[0062] The sheet manufacturing apparatus 20 differs from the sheet manufacturing apparatus 10 in that it further includes a drying processing section 21. Hereinafter, a description of the same components will be omitted, and different components will be described in detail.
[0063] As described above, this sheet manufacturing apparatus 20 includes the same components as those of the sheet manufacturing apparatus 10, and is provided with a drying processing unit 21. The drying processing unit 21 is disposed in the solidification area 15 and is a member that dries the solvent contained in the liquid material impregnated into the nonwoven fabric NW. That is, this second embodiment is an embodiment in which a raw material solution (liquid material) obtained by mixing a raw material and a solvent is used as the liquid material.
[0064] This drying treatment section 21 is provided to efficiently volatilize the solvent contained in the liquid material impregnated into the nonwoven fabric NW in step (d). Typically, a heated atmosphere is created inside the drying treatment section 21 to promote the evaporation of the solvent. To create a heated atmosphere, for example, gas (air, etc.) heated to a set temperature by a heat source such as a heater may be introduced into the drying treatment section 21. At this time, it is preferable to continue the operation of introducing the heated gas so that the temperature inside the drying treatment section 21 can be maintained near the set temperature.
[0065] This heating temperature can be set optimally depending on the solvent used. For example, when water or a lower alcohol is used as the solvent, the heating temperature is preferably 50 to 90°C. However, the upper limit should be a temperature below the boiling point of the solvent. By setting the temperature within this range, the efficiency of solvent evaporation can be significantly improved, and situations such as the generation of bubbles in the sheet due to the boiling of the solvent can be avoided. Furthermore, in order to promote evaporation and drying, a configuration may be provided in which a blower can blow air onto the sheet-shaped liquid material SLM.
[0066] Furthermore, when the drying treatment section 21 is provided, a solvent recovery mechanism may be provided to cool, liquefy, and recover the volatilized solvent generated in the drying treatment section 21. By providing this solvent recovery mechanism, the solvent can be reused. Furthermore, the recovered solvent can be recycled and reused as a solvent for dissolving the raw material again. By recycling in this manner, costs can be reduced and the nonwoven fabric sheet can be efficiently produced in the manufacturing operation of the nonwoven fabric sheet of this embodiment.
[0067] <Method for Manufacturing Nonwoven Fabric Sheet> In the present embodiment, the nonwoven fabric sheet manufacturing apparatus 20 used differs from the nonwoven fabric sheet manufacturing apparatus 10 described above in that it does or does not have a drying processing section 21. Therefore, the basic operations in the method for manufacturing a nonwoven fabric sheet are the same as those in the first embodiment.
[0068] In this embodiment 2, in addition to the operations of embodiment 1, the liquid material impregnated into the nonwoven fabric NW is heated by a drying processing unit 21 to volatilize and dry the solvent contained in the liquid material, thereby efficiently integrating the nonwoven fabric and the raw material into a nonwoven fabric sheet 50. This drying process is performed in a solidification area 15.
[0069] This drying process is preferably performed by heating to a temperature that promotes the evaporation of the solvent used, as described above, and the optimum temperature is set depending on the solvent used. For example, when water or a lower alcohol is used as the solvent, the heating temperature is preferably 50 to 90°C. However, the upper limit should be a temperature below the boiling point of the solvent. By setting the temperature within this range, the evaporation efficiency of the solvent can be significantly improved, and situations such as the generation of bubbles in the sheet due to the boiling of the solvent can be avoided. Furthermore, to promote evaporation and drying, a configuration may be provided in which a fan can blow air onto the sheet-shaped liquid material SLM.
[0070] Furthermore, by providing a solvent recovery mechanism as described above, the solvent evaporated in the drying treatment unit 21 can be cooled and liquefied, and the solvent can be recovered. The solvent recovered in this way can be recycled and reused as a solvent for the raw material.
[0071] <Raw Materials> Next, the raw materials used in Embodiments 1 and 2 will be described. The raw materials are not particularly limited, and as described above, any liquid material having a viscosity of 100,000 mPa·s or less may be used as a liquid material for coating by the coater 13. This liquid material may be prepared by melting the raw materials, or by mixing and dissolving the raw materials in a solvent.
[0072] Examples of this raw material include low-viscosity liquid resins such as so-called injection grades and spinning grades that are injected from a die when molding resins.
[0073] Furthermore, biodegradable materials can also be used as raw materials. Water-soluble materials are suitable as biodegradable materials in the present invention, and since they can be easily dissolved in water as a solvent to obtain a low-viscosity liquid material, they are excellent not only in terms of moldability but also in terms of low environmental impact.
[0074] Examples of raw materials that can be used in this embodiment include polysaccharides and gelatin. Examples of polysaccharides include glucomannan, cellulose-based materials, pectin, starch, isomaltodextrin, agar, etc. These may be used alone or in combination of two or more. In particular, it is preferable to contain at least one selected from glucomannan, cellulose-based materials, gelatin, and agar.
[0075] Glucomannan is a water-soluble polysaccharide that makes up approximately 10% of the tubers of konjac, and can be extracted by purifying konjac flour with alcohol. Glucomannan has the chemical structure shown in Figure 4, and is a polysaccharide in which D-glucose and D-mannose are linked together in a β-1,4 bond in a ratio of 1:1.6 (n indicates the number of repeating units). It has one branch for every 50-60 sugars, and has a high molecular weight, sometimes exceeding 1 million.
[0076] The glucomannan used here preferably has a molecular weight in the range of 20 to 2,000,000. Glucomannan having such a molecular weight has a viscosity of 1,000 to 20,000 mPa·s when added to water at 1% by mass and melted.
[0077] Furthermore, glucomannan has many hydroxyl groups and can be easily dissolved in alcohols as a solvent to reduce the viscosity.
[0078] Cellulose-based materials are materials that contain cellulose or cellulose in part. Cellulose is a naturally occurring polymer in which many β-glucose molecules are polymerized in a linear chain via glycosidic bonds. It has the chemical structure shown in Figure 6 and the molecular formula (C 6 H 10 O 5 ) n Examples of cellulose-based materials include carboxymethyl cellulose and cellulose nanofiber.
[0079] The cellulosic material used here preferably has a molecular weight in the range of 1,000 to 500,000. A cellulosic material having such a molecular weight will have a viscosity of 50 to 50,000 mPa·s when heated to 20 to 60° C. and melted.
[0080] Furthermore, cellulose-based materials have many hydroxyl groups, and can be dissolved in alcohols as a solvent, making it easy to reduce the viscosity.
[0081] Gelatin is a fibrous protein called collagen, and agar is obtained by freezing and drying the solidified mucus of red algae.It is insoluble in water as it is, but can be melted and made less viscous by heating.
[0082] Furthermore, the liquid material may contain a filler. Examples of the filler include inorganic substances such as alumina, silica, aluminum hydroxide, and boehmite, as well as cellulose (including cellulose nanofibers), carbon fibers, carbon nanotubes, carbon nanofibers, graphene, fullerene, and aramid fibers. Cellulose in which the hydrophilic groups have been substituted with hydrophobic groups may also be used.
[0083] (Embodiment 3) <Nonwoven Fabric Sheet> The nonwoven fabric sheet of this embodiment is a sheet-like material formed by impregnating and solidifying the above-mentioned low-viscosity liquid material into a nonwoven fabric NW. As described above, this low-viscosity liquid material is obtained by melting a raw material or dissolving a raw material in a solvent, and the raw material preferably contains at least one material selected from, for example, glucomannan, a cellulose-based material, gelatin, and agar.
[0084] The nonwoven fabric sheet 50 is made of a nonwoven fabric NW and an impregnating material containing a low-viscosity liquid material that has been impregnated and solidified into the nonwoven fabric NW. The nonwoven fabric sheet 50 may have a surface that has undergone various treatments. The thickness of the nonwoven fabric sheet can be any thickness, and is preferably 10 μm to 5 mm, and more preferably 20 μm to 3 mm, for example.
[0085] The ratio of nonwoven fabric to solidified material (raw material) in this nonwoven fabric sheet 50 can be any ratio. For example, it is preferable that the ratio of solidified raw material to the entire nonwoven fabric sheet is 5% by volume or more and 90% by volume or less. In this way, by increasing the ratio of raw material relative to nonwoven fabric, it is possible to effectively utilize the properties derived from the solidified portion made of the raw material. In this case, the ratio of this raw material can be calculated using the following formula (1): Raw material ratio [%] = (volume of solidified raw material) / (volume of nonwoven fabric sheet) ... (1)
[0086] In this case, increasing the proportion of nonwoven fabric can improve the strength of the nonwoven fabric sheet 50. The proportion of this composition can be determined depending on the purpose of the nonwoven fabric sheet 50, and can be adjusted by appropriately selecting the nonwoven fabric and liquid material to be used.
[0087] Furthermore, this nonwoven fabric sheet can be a multilayer sheet with other layers provided on its surface, in which case all layers may be the nonwoven fabric sheet of this embodiment, or some layers may be the nonwoven fabric sheet of this embodiment and the remaining layers may be sheets other than those of this embodiment (which may be sheets composed of nonwoven fabric or nonwoven fabric sheets not composed of nonwoven fabric). In other words, it is sufficient that the sheet has one or more layers of the nonwoven fabric sheet used in this embodiment.
[0088] The nonwoven fabric sheet will be specifically described below when glucomannan is used as a raw material. When glucomannan is added at 0.5% by mass to water used as a solvent, it becomes a liquid material with a viscosity of 10,000 mPa·s.
[0089] The liquid material obtained by adding the liquid material to the solvent in this manner can be used, for example, to manufacture a nonwoven fabric sheet using the nonwoven fabric sheet manufacturing apparatus 10 shown in Figure 1. In this case, for example, the nonwoven fabric NW has a width of 50 cm, a thickness of 2 mm, and a basis weight of 500 g / cm. 2 A nonwoven fabric made of polyethylene (PE) with a porosity of 50% is used, and the liquid material LM is applied onto the nonwoven fabric NW at a conveying speed of 0.1 m / s and a discharge rate of 3000 mL / min from a coating machine 13 (die coater) with a slit width of 1 mm for discharging the liquid material LM.
[0090] In the impregnation region 14, the nonwoven fabric NW on which the sheet-like liquid material SLM was formed was sandwiched between impregnation rolls 14a from above and below with a pressure of 1 MPa applied, and the liquid material LM was impregnated into the nonwoven fabric NW. The nonwoven fabric NW was allowed to solidify by natural cooling at room temperature and transported by feed rolls 19 to form a nonwoven fabric sheet 50. This nonwoven fabric sheet 50 having a thickness of 2 mm was wound up by the sheet winding unit 16 to obtain a roll-like nonwoven fabric sheet 50.
[0091] The glucomannan nonwoven fabric sheet thus obtained can be used as a water-absorbent sheet, taking advantage of the hygroscopicity of the raw material.
[0092] The glucomannan sheet obtained in this way can be used as a water-absorbent sheet by utilizing the hygroscopicity of the raw material. An example of its use as a water-absorbent sheet will be explained using Figures 6 and 7. In these figures, the arrows indicate the transfer of thermal energy.
[0093] 6 and 7 show an example of the application of a glucomannan nonwoven fabric sheet 50 as a water-absorbing sheet using sunlight. The moisture recovery device 100 shown here is composed of a heat collector 101, a heat storage tank 102, an inclined plate 103, and a moisture recovery container 104.
[0094] The heat collector 101 is a device that can extract thermal energy from, for example, sunlight and transfer it to the heat storage tank 102. The heat storage tank 102 stores the heat collected by the heat collector 101, and the stored heat can be used to heat the nonwoven fabric sheet 50 at a desired timing. The inclined plate 103 is a plate-like body that is arranged at an angle above the nonwoven fabric sheet 50. This inclined plate 103 cools and liquefies the water vapor released from the nonwoven fabric sheet 50 and guides it to the moisture collection container 104. The moisture collection container 104 is a container that stores the liquefied water guided to the inclined plate 103.
[0095] This moisture recovery device 100 is used, for example, as follows. First, as shown in Figure 6, during the day, thermal energy from sunlight is collected by a heat collector 101, and the collected thermal energy is stored in a heat storage tank 102. Here, the nonwoven fabric sheet 50 is exposed to the external atmosphere, but absorbs moisture (water vapor) contained in the air. As described above, the glucomannan nonwoven fabric sheet 50 has excellent moisture absorption properties and can retain a large amount of moisture.
[0096] Then, at night after the sun has set, as shown in FIG. 7 , the thermal energy stored in the heat storage tank 102 is used to heat the nonwoven fabric sheet 50. This heating is performed to a temperature at which the nonwoven fabric sheet 50 will release (desorb) the moisture it has absorbed, preferably 80 to 100°C. The moisture released from the nonwoven fabric sheet 50 diffuses upward, comes into contact with the inclined plate 103, and liquefies on its surface. The liquefied moisture flows downward along the slope of the inclined plate 103, is guided to the moisture recovery container 104, and is finally stored in the moisture recovery container 104.
[0097] The present invention has been specifically described above using embodiments and examples, but the present invention should not be construed as being limited to these embodiments and examples, and it goes without saying that the present invention can be modified in various ways without departing from the spirit of the invention.
[0098] REFERENCE SIGNS LIST 10, 20 Sheet manufacturing apparatus 11 Raw material container 12 Nonwoven fabric discharge section 13 Coating machine 14 Impregnation area 15 Solidification area 16 Sheet winding section 17 Back roll 18 Feed roll 21 Drying processing section 50 Nonwoven fabric sheet LM Liquid material NW Nonwoven fabric SLM Sheet-like liquid material
Claims
1. A method for producing a nonwoven fabric sheet, comprising: (a) preparing a liquid material containing raw materials and having a viscosity of 100,000 mPa·s or less; (b) after the step (a), applying the liquid material in the form of a sheet onto a nonwoven fabric using a coating machine; (c) after the step (b), impregnating the nonwoven fabric with the liquid material; (d) after the step (c), solidifying the liquid material impregnated into the nonwoven fabric to obtain a nonwoven fabric sheet; and (e) after the step (d), winding up the nonwoven fabric sheet.
2. A method for producing a nonwoven fabric sheet according to claim 1, wherein the nonwoven fabric is made of a material containing at least one material selected from the group consisting of polyester, polypropylene, polyethylene, rayon, nylon, polyethylene terephthalate, aramid glass fiber, and carbon fiber.
3. In the method for producing a nonwoven fabric sheet according to claim 1, the nonwoven fabric has a basis weight of 0.1 g / m 2 ~10000g / m 2 A method for producing a nonwoven fabric sheet, the range being:
4. A method for producing a nonwoven fabric sheet according to claim 1, wherein in step (c), the impregnation of the liquid material is carried out by impregnation rolls disposed above and below the nonwoven fabric.
5. The method for producing a nonwoven fabric sheet according to claim 4, wherein in step (c), the nonwoven fabric is pressed by the impregnated roll.
6. The method for producing a nonwoven fabric sheet according to claim 5, wherein the pressure applied by the impregnated roll is 0.01 to 100 MPa.
7. The method for producing a nonwoven fabric sheet according to claim 1, wherein the raw material is a powdered filler containing at least one selected from the group consisting of glucomannan, a cellulose-based material, gelatin and agar.
8. The method for producing a nonwoven fabric sheet according to claim 1, wherein the liquid material contains the raw material and a solvent, and step (d) includes a drying process for volatilizing the solvent by heating.
9. The method for producing a nonwoven fabric sheet according to claim 8, wherein the solvent is water or alcohol.
10. A nonwoven fabric sheet manufacturing apparatus comprising: a raw material container for preparing and storing a liquid material containing raw materials and having a viscosity of 100,000 mPa·s or less; a nonwoven fabric discharge section for feeding out nonwoven fabric; a coater for coating the liquid material in a sheet form onto the nonwoven fabric fed out from the nonwoven fabric discharge section; an impregnation area for impregnating the nonwoven fabric with the coated liquid material; a solidification area for solidifying the liquid material impregnated into the nonwoven fabric to form a sheet; and a sheet winding section for winding up the nonwoven fabric sheet obtained by solidifying the liquid material.
11. An apparatus for manufacturing a nonwoven fabric sheet according to claim 10, further comprising, in said solidification area, a drying treatment section for volatilizing the solvent in said sheet by heating.
12. An apparatus for manufacturing a nonwoven fabric sheet according to claim 11, wherein the liquid material contains the raw material and a solvent, and the solidification area has a recovery section for recovering the evaporated solvent.
13. A nonwoven sheet comprising: a nonwoven fabric; and an impregnated material containing at least one material selected from glucomannan, a cellulosic material, gelatin, and agar, impregnated and solidified in the nonwoven fabric.
14. The nonwoven fabric sheet according to claim 13, wherein the nonwoven fabric sheet has a multi-layer structure in which two or more layers are laminated, and the nonwoven fabric sheet has one or more layers.
Citation Information
Patent Citations
Die for extrusion molding and extrusion molding apparatus
JP2020146853A
Method for preparing wear-resistant water-absorption-type non-woven fabric
CN108018716A
Waterborne polyurethane superfine fiber synthetic leather and preparation method thereof
CN112111976A
Dandelion fluff-based antibacterial hemostatic dressing
CN112706477A
Manufacture of hydrolyzable cleaning article and manufacturing device therefor
JP2000300463A