Film deposition method
The film forming method addresses the environmental and step-related challenges of ALD by using ultrasonic bonding and polymerization to create dense films on substrates with uneven surfaces, reducing the number of processing steps and environmental impact.
Patent Information
- Application Number
- PCT/JP2024/013678
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-04-12
- Filing Date
- 2024-04-02
- Publication Date
- 2024-10-17
AI Technical Summary
Atomic layer deposition (ALD) for forming dense films on uneven substrate surfaces involves a large number of steps and significant environmental impact due to the use of multiple raw material gases.
A film forming method that involves immersing a substrate in a solution containing a polymerization initiator, applying ultrasonic waves to bond the initiator group to the substrate, and then immersing it in a solution with a polymerizable monomer for polymerization, reducing the environmental burden and allowing for the formation of dense films with fewer steps.
This method enables the formation of dense, high-quality polymer films on substrates with uneven surfaces while minimizing environmental impact and allowing for the use of fewer processing steps compared to traditional ALD methods.
Smart Images

Figure JP2024013678_17102024_PF_FP_ABST
Abstract
Description
Film forming method
[0001] The present disclosure relates to a film formation method.
[0002] Patent Document 1 discloses a technique for selectively preparing self-assembled monolayers (SAMs) on portions of a substrate surface using a compound containing a hydrogen-bonding group and a polymerizable diacetylene group. Patent Document 2 discloses a technique for recess-etching a SiN film in an ONON stacked structure.
[0003] JP 2021-520640 A JP 2022-94914 A
[0004] In semiconductor manufacturing, atomic layer deposition (ALD) is used to form dense films, particularly on uneven substrate surfaces. However, because this atomic layer deposition process involves alternately introducing multiple source gases in a reduced-pressure environment, it requires many steps and places a heavy burden on the environment.
[0005] The present disclosure provides a film formation method that can reduce the environmental impact when forming a dense film.
[0006] A film formation method according to one aspect of the present disclosure is a film formation method for forming a polymer film on a surface of a substrate in a solution, the film formation method comprising the steps of: immersing a substrate in a first solution containing a polymerization initiator; applying ultrasound to the first solution to bond polymerization initiation groups to the surface of the substrate; immersing the substrate having the polymerization initiation groups bonded to its surface in a second solution containing a polymerizable monomer; and growing the polymer on the surface of the substrate by a polymerization reaction of the polymerizable monomer initiated by the polymerization initiation groups.
[0007] According to one aspect of the present disclosure, it is possible to reduce the environmental impact when forming a dense film.
[0008] 7 is a diagram showing one step (first immersion step) of the film formation method; FIG. 8 is a diagram showing one step (ultrasonic wave application step) of the film formation method; FIG. 9 is a diagram showing one step (second immersion step) of the film formation method; FIG. 10 is a diagram showing one step (polymerization step) of the film formation method; SEM image showing a state in which a thin film has been formed on a substrate; SEM image showing a state in which two thin film layers have been laminated on a substrate; An image of a laminate structure in which two types of thin films are laminated in the horizontal direction; An image of the laminate structure of one of the thin films in FIG. 7 being removed.
[0009] Hereinafter, embodiments of the present disclosure will be described with reference to the drawings. Note that common parts in the drawings may be denoted by the same or corresponding reference numerals, and descriptions thereof may be omitted.
[0010] <Substrate Processing Method> The film formation method of the present disclosure is a film formation method for forming a polymer film on the surface of a substrate in a solution.
[0011] The material of the substrate is not particularly limited. Examples of the material of the substrate include silicon (Si), silicon oxide (SiO 2 ), silicon nitride (Si 3 N 4 ), glass epoxy, etc.
[0012] The form of the substrate is not particularly limited, and examples of the form of the substrate include a substrate obtained by processing a wafer made of single crystal silicon (Si) in a semiconductor device manufacturing process, a substrate in which an insulating layer such as a silicon oxide film (silicon oxide) and / or a silicon nitride film (silicon nitride) is formed on silicon, and a glass epoxy substrate (glass substrate) used in manufacturing flat panel displays.
[0013] The substrate may have a silicon-on-carbon (SOC) film formed on it, or may have a silicon-on-glass (SOG) film formed on top of the SOC film formed on it.
[0014] The polymer film refers to a thin film made of a polymer of a monomer. The polymer film may be a single layer or a laminate of two or more layers. In this specification, the thin film refers to a single layer having a thickness of 1 μm or less.
[0015] The film forming method of the present disclosure includes a step of immersing a substrate in a first solution containing a polymerization initiator (hereinafter referred to as a first immersion step). In the first immersion step, as shown in Fig. 1, a substrate 3 is immersed in a solution 2 in which a polymerization initiator 4 is dissolved in an organic solvent in a reaction vessel 1. Here, the solution 2 in which the polymerization initiator 4 is dissolved is an example of the first solution.
[0016] The polymerization initiator is not particularly limited, but for example, an organic compound having a chlorine-substituted alkyl group or a bromine-substituted alkyl group at one end and a polymerization initiating group at the other end can be used. As such an organic compound, it is preferable to use a sulfonyl chloride compound having a chlorine-substituted alkyl group or a bromine-substituted alkyl group at the end. In the sulfonyl chloride compound, the polymerization initiating group is -SO 2 It is a chlorosulfonyl group represented by Cl.
[0017] When the polymerization initiator is a sulfonyl chloride compound, the number of chlorine or bromine atoms substituted on the alkyl group may be at least 1. In addition, between the chlorine-substituted alkyl group or bromine-substituted alkyl group and the chlorosulfonyl group, any organic group such as a cyclic organic compound such as an aromatic hydrocarbon or an alicyclic hydrocarbon, an alkyl group, an imino group, or an ether bond may be present.
[0018] In this case, the alkyl group preferably has 1 to 3 carbon atoms, more preferably 1, and may be branched. An example of a group having an imino group is N-(2-chloroethyl)sulfamoyl chloride. An example of a group having an ether bond is chloromethoxysulfonyl chloride.
[0019] Examples of such sulfonyl chloride compounds include trichloromethanesulfonyl chloride, tribromomethanesulfonyl chloride, and trichloromethylphenylsulfonyl chloride. Among these, trichloromethanesulfonyl chloride is preferred. These compounds may be used alone or in combination of two or more.
[0020] The first solution is a solution in which a polymerization initiator is dissolved in an organic solvent. The organic solvent is not particularly limited, but is preferably an aprotic organic solvent from the viewpoint of deactivating radical species generated upon irradiation with ultrasonic waves, as described below. Examples of such an aprotic organic solvent include tetrahydrofuran, dioxane, xylene, toluene, and benzene. Among these, it is preferable to use tetrahydrofuran.
[0021] The concentration of the polymerization initiator in the first solution is preferably 0.1% by mass or more and 20% by mass or less, more preferably 0.5% by mass or more and 10% by mass or less, and even more preferably 1% by mass or more and 5% by mass or less, relative to the organic solvent.
[0022] In the film forming method of the present disclosure, when the substrate is made of silicon and / or silicon oxide, the substrate may be pre-treated with ozone before being immersed in the first solution.
[0023] Specifically, when the material of the substrate 3 is silicon or silicon oxide, the substrate 3 is immersed in ozone (O 3 ) atmosphere. As a result, polar groups such as hydroxyl groups are bonded to the surface of the substrate 3, and when the first immersion step is carried out in this state, the polymerization initiation groups 4 such as chlorosulfonyl groups are more likely to bond to the surface of the substrate 3 to which polar groups such as hydroxyl groups are bonded.
[0024] The film formation method of the present disclosure includes a step of applying ultrasonic waves to a first solution to bond polymerization initiating groups to the surface of a substrate (hereinafter referred to as an ultrasonic wave application step). In the ultrasonic wave application step, as shown in Fig. 2, a substrate 3 is immersed in a solution 2 in which a polymerization initiator is dissolved in a reaction vessel 1, and ultrasonic waves 5 are applied to the solution 2, whereby polymerization initiating groups 4 are bonded to the surface of the substrate 3.
[0025] In this specification, "ultrasound" refers to sound waves with frequencies above the audible range (16 kHz to 3000 kHz). Ultrasound is highly directional and does not spread easily, so it is not easily attenuated in liquids. Furthermore, ultrasound has the property of creating a local high-temperature, high-pressure field in liquids through cavitation (the generation and collapse of bubbles in liquid), thereby generating microfluidics.
[0026] It should be noted that a complex uneven pattern may be formed on the surface of the substrate 3. In this case, the ultrasonic waves 5 propagate through the solution 2 and reach the uneven portions, causing cavitation. As a result, even if the surface of the substrate 3 is uneven, a uniform film can be formed on the uneven portions.
[0027] The conditions for ultrasonic irradiation are not particularly limited, but it is preferable to irradiate the material with ultrasonic waves having a frequency of 16 to 3000 kHz and an output of 50 to 600 W for 10 to 90 minutes.
[0028] The polymerization initiating group is a polymerization initiating group derived from a polymerization initiator. For example, when the polymerization initiator is a sulfonyl chloride compound, the polymerization initiating group is the above-mentioned chlorosulfonyl group.
[0029] The polymerization initiator group is preferably one that selectively bonds to the surface of the substrate having a predetermined polar group. For example, by previously providing a region (polar region) having a polar group such as a hydroxyl group and a region (non-polar region) not having a polar group on the surface of the substrate, the polymerization initiator group can be bonded only to the polar region on the surface of the substrate.
[0030] When the polymerization initiator is a sulfonyl chloride compound, the chlorosulfonyl group, which is the polymerization initiator group, is highly reactive with hydroxyl groups, and can therefore be selectively bonded to the surface of the substrate to which hydroxyl groups are bonded.
[0031] The film formation method of the present disclosure includes a step of immersing a substrate having polymerization initiation groups bonded to its surface in a second solution containing a polymerizable monomer (hereinafter referred to as a second immersion step). In the second immersion step, as shown in Fig. 3, the substrate 3 having polymerization initiation groups 4 bonded to its surface is immersed in a solution 2 in which a polymerizable monomer 8 is dissolved in an organic solvent in a reaction vessel 1. Here, the solution 2 in which the polymerizable monomer 8 is dissolved is an example of the second solution.
[0032] The second solution may be prepared in the reaction vessel 1 after the ultrasonic wave application process, and the substrate 3 after the ultrasonic wave application process may be immersed in the second solution in the reaction vessel 1, or the second solution may be prepared in a reaction vessel other than the reaction vessel 1, and the substrate 3 after the ultrasonic wave application process may be immersed in the second solution in the other reaction vessel.
[0033] The polymerizable monomer is not particularly limited, but for example, a radical polymerizable monomer having one or more carbon-carbon unsaturated double bonds in one molecule can be used.
[0034] The monomer having one or more carbon-carbon unsaturated double bonds in one molecule is not particularly limited, but examples thereof include styrene, vinyl chloride, methyl methacrylate, dicyclopentadiene dimethacrylate, dicyclopentadiene diacrylate, trimethylolpropane trimethacrylate, trimethylolpropane triacrylate, ethylene glycol dimethacrylate, ethylene glycol diacrylate, diethylene glycol dimethacrylate, diethylene glycol diacrylate, glycerin dimethacrylate, glycerin diacrylate, pentaerythritol triacrylate, and methacrylic anhydride. Among these, ethylene glycol dimethacrylate is preferred.
[0035] The concentration of the polymerizable monomer in the second solution is preferably 0.1% by volume or more and 40% by volume or less, more preferably 0.5% by volume or more and 20% by volume or less, and even more preferably 1% by mass or more and 10% by mass or less, relative to the organic solvent.
[0036] In the second immersion step, radical active species may be generated on the surface of the substrate to which the polymerization initiating groups are bonded. Specifically, as shown in Fig. 3, the substrate 3 is immersed in a solution 2 in which a polymerizable monomer 8 is dissolved in a reaction vessel 1, and then irradiated with UV or the like, whereby radicals 7 are generated on the surface of the substrate 3 to which the polymerization initiating groups 4 are bonded, and the polymerization initiating groups 4 become radical active species.
[0037] The film formation method of the present disclosure includes a step (polymerization step) of growing a polymer on the surface of a substrate by a polymerization reaction of a polymerizable monomer initiated by a polymerization initiation group. In the polymerization step, as shown in Fig. 4, a substrate 3 having a surface to which a polymerization initiation group 4 is bonded is immersed in a solution 2 in which a polymerizable monomer is dissolved in a reaction vessel 1, and a polymerization reaction of the polymerizable monomer occurs. With the polymerizable monomer 8 bound to the surface of the substrate 3 initiated by the polymerization initiation group 4, a polymer (a polymer of the polymerizable monomer 8) grows on the surface of the substrate 3.
[0038] The polymerization reaction conditions are not particularly limited, but the polymerization time is, for example, 3 minutes to 5 hours, preferably 10 minutes to 3 hours, and more preferably 30 minutes to 2 hours. The polymerization temperature is, for example, 3° C. to 80° C., preferably 5° C. to 60° C., and more preferably 10° C. to 40° C. During the polymerization reaction, the second solution may be stirred or may be irradiated with the above-mentioned ultrasonic waves.
[0039] The type of polymerization reaction is not particularly limited, but is preferably a living radical polymerization reaction. A living radical polymerization reaction is a reaction that does not involve side reactions that deactivate the terminals of a polymer, such as chain transfer reactions and termination reactions. When the polymerization reaction is a living radical polymerization reaction, a polymer of uniform length is obtained, and the terminals of the polymer can be further modified with a polymer, so that the degree of polymerization is easily controlled and a sharp molecular weight distribution is obtained.
[0040] In order to carry out a living radical polymerization reaction in the polymerization step, it is preferable to convert the polymerization initiating groups 4 into radical active species in the second immersion step as described above. In addition, in the polymerization step, the living radical polymerization reaction can be carried out by irradiating the substrate 3 with UV or the like.
[0041] As described above, the film formation method of the present disclosure provides a semiconductor manufacturing process that requires low energy and requires fewer steps by growing a polymer through a polymerization reaction of a polymerizable monomer on the surface of a substrate to which a polymerization initiator group is bonded by applying ultrasonic waves to the first solution. Therefore, the film formation method of the present disclosure can be carried out without using a reduced pressure environment like ALD, and can form a dense film with fewer steps, thereby contributing to reducing the environmental impact.
[0042] Furthermore, even if the polymerizable monomer is a low-molecular-weight monomer, it is possible to form a film on the surface or inside of a fine pattern having grooves or holes with dimensions of about several tens of nanometers. A low-molecular-weight polymerizable monomer refers to a molecule whose size is such that even if the degree of polymerization reaches about 100, the film thickness upon formation is less than several tens of nanometers. Furthermore, by polymerizing a low-molecular-weight monomer, an isotropic and dense film can be formed, enabling high-quality film formation.
[0043] Specifically, the ultrasonic application step can bond the polymerization initiation groups 4 to the side surface 9 of the substrate 3, and the polymerization step can form a film of polymers of the polymerizable monomer 8 (heterogeneous polymers 81, 82) in the horizontal direction starting from the polymerization initiation groups 4 (see FIG. 7). Furthermore, both of the films of the heterogeneous polymers 81, 82 can become fine thin films on the nanoscale.
[0044] Furthermore, by selecting polymerizable monomers such that polymer 81 is decomposed by plasma (e.g., oxygen plasma) but polymer 82 is not decomposed by plasma, when substrate 3 is irradiated with plasma, the film of polymer 81 is removed and a film of polymer 82 remains (see FIG. 8 ). This makes it possible to form a thin film on substrate 3 that has a nanoscale space between side surface 9 and the remaining polymer 82.
[0045] The film forming method of the present disclosure will be further described below using examples.
[0046] Example 1 Approximately 40 mL of tetrahydrofuran (THF) as an organic solvent and 1 g of trichloromethanesulfonyl chloride as a polymerization initiator were placed in a 50 mL vial and stirred to prepare a solution in which the polymerization initiator was dissolved in the organic solvent (first solution).
[0047] A silicon (Si) substrate was placed in a vial, and the vial was placed in an ultrasonic irradiation device containing 1.5 L of water. The vial was then irradiated with ultrasonic waves under a nitrogen atmosphere at a frequency of 430 kHz, an output of 80 W, and for 30 minutes.
[0048] After the ultrasonic irradiation, 2 mL of ethylene glycol dimethacrylate was added as a polymerizable monomer to the vial (second solution), and the vial was left to stand for 45 minutes (polymerization reaction), after which the substrate was taken out of the vial, washed with THF, and dried.
[0049] The cross section of the substrate after drying was observed with a scanning electron microscope (SEM), and it was confirmed that a dense thin film was formed on the surface of the substrate in Example 1.
[0050] Example 2: A silicon (Si) substrate was coated with silicon oxide (SiO 2 ) substrate was used instead, the same operations and observations were carried out as in Example 1. As a result, it was confirmed that in Example 2, a dense thin film was formed on the surface of the substrate.
[0051] Example 3 A silicon (Si) substrate was preliminarily treated with ozone (O 3 The substrates were subjected to the same operations and observations as in Example 1, except that they were exposed to the ozone gas (treated with ozone). As a result, it was confirmed that a dense thin film was formed on the surface of the substrate in Example 3.
[0052] [Example 4] Silicon oxide (SiO 2 ) The substrate was subjected to the same procedure and observation as in Example 2, except that it was exposed to ozone gas before being placed in the vial (ozone treatment). As a result, it was confirmed that a dense thin film was formed on the surface of the substrate in Example 4 (see FIG. 5).
[0053] [Example 5] After the polymerization reaction, 2 mL of ethylene glycol dimethacrylate was further added as a polymerizable monomer and allowed to stand for 45 minutes (polymerization reaction), and the other operations and observations were carried out in the same manner as in Example 4. As a result, it was confirmed that a dense thin film was formed on the surface of the substrate in Example 5 (see FIG. 6).
[0054] From Examples 1 to 5, it was found that a dense thin film can be formed on the surface of a substrate by applying ultrasound to the first solution to bond polymerization initiation groups to the surface of the substrate, and then growing a polymer through a polymerization reaction of a polymerizable monomer on the surface of the substrate (see FIG. 5). Furthermore, in Example 5, it was found that multiple dense thin films can be stacked on the surface of the substrate by repeating the polymerization reaction of the polymerizable monomer (see FIG. 6).
[0055] The above-disclosed embodiments include, for example, the following aspects.
[0056] (Appendix 1) A film formation method for forming a polymer film on a surface of a substrate in a solution, comprising the steps of: immersing a substrate in a first solution containing a polymerization initiator; applying ultrasonic waves to the first solution to bond polymerization initiation groups to the surface of the substrate; immersing the substrate having the polymerization initiation groups bonded to its surface in a second solution containing a polymerizable monomer; and growing the polymer on the surface of the substrate by a polymerization reaction of the polymerizable monomer initiated by the polymerization initiation groups.
[0057] (Supplementary Note 2) The film forming method according to Supplementary Note 1, wherein the polymerization initiation group selectively bonds to a surface of a substrate having a predetermined polar group.
[0058] (Supplementary Note 3) The film forming method according to Supplementary Note 1 or 2, wherein the polymerization reaction is a living radical polymerization reaction.
[0059] (Supplementary Note 4) The film forming method according to any one of Supplementary Notes 1 to 3, further comprising generating radical active species on the surface of the substrate to which the polymerization initiation group is bonded.
[0060] (Supplementary Note 5) The film forming method according to any one of Supplementary Notes 1 to 4, wherein the substrate is made of silicon or silicon oxide, and the substrate is pre-treated with ozone before being immersed in the first solution.
[0061] (Supplementary Note 6) The film forming method according to any one of Supplementary Notes 1 to 5, wherein the surface of the substrate has irregularities formed thereon.
[0062] Although the embodiments of the present disclosure have been described above, the present disclosure is not limited to these embodiments, and various modifications and changes are possible within the scope of the disclosure described in the claims.
[0063] This application claims priority based on Japanese Patent Application No. 2023-065122, filed on April 12, 2023, the entire contents of which are incorporated herein by reference.
[0064] REFERENCE SIGNS LIST 1 Reaction vessel 2 Solution 3 Substrate 4 Polymerization initiator (polymerization initiation group) 5 Ultrasonic wave 6 UV 7 Radical 8 Polymerizable monomer 81 Polymer 82 Polymer 9 Side
Claims
1. A film formation method for forming a polymer film on a surface of a substrate in a solution, comprising the steps of: immersing a substrate in a first solution containing a polymerization initiator; applying ultrasonic waves to the first solution to bond polymerization initiating groups to the surface of the substrate; immersing the substrate with the polymerization initiating groups bonded to its surface in a second solution containing a polymerizable monomer; and growing the polymer on the surface of the substrate by a polymerization reaction of the polymerizable monomer starting from the polymerization initiating groups.
2. The film forming method according to claim 1, wherein the polymerization initiating group selectively bonds to a surface of a substrate having a predetermined polar group.
3. The film forming method according to claim 1, wherein the polymerization reaction is a living radical polymerization reaction.
4. The film forming method according to claim 1, further comprising generating radical active species on the surface of the substrate to which the polymerization initiating group is bonded.
5. The film forming method according to claim 1, wherein the substrate is made of silicon or silicon oxide, and the substrate is preliminarily treated with ozone before being immersed in the first solution.
6. The film forming method according to any one of claims 1 to 5, wherein the surface of the substrate has projections and recesses.
Citation Information
Patent Citations
Manufacturing method of base board with metallic film, base board with metallic film, manufacturing method of metallic pattern material, and metallic pattern material
JP2008104909A
Polymerization initiating group-attached inorganic oxide particle and method for manufacturing the same, as well as polymer-modified inorganic oxide particle obtained by using this inorganic oxide particle and method for manufacturing the same
JP2010168468A
Hydrophilic coating film forming method
JP2018001087A
Method for forming polymer brush layer
WO2018225693A1