Anisotropic graphite composite and manufacturing method therefor
The anisotropic graphite composite, formed by laminating anisotropic graphite with a metal and/or resin adhesive layer and optimizing its structure through cutting and surface peeling, addresses the inefficiencies and brittleness of conventional composites, achieving superior heat transfer and structural reliability for electronic applications.
Patent Information
- Application Number
- PCT/JP2024/014349
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-04-14
- Filing Date
- 2024-04-09
- Publication Date
- 2024-10-17
AI Technical Summary
Conventional anisotropic graphite composites have limitations in heat transfer efficiency, and they are structurally brittle, prone to collapse, which affects their reliability as heat transfer elements in electronic devices.
An anisotropic graphite composite is created by laminating layers of anisotropic graphite and an adhesive layer containing metal and/or resin, with the crystal orientation plane of the graphite layer arranged parallel to the XY plane, and the adhesive layers alternately bonded in the Z-axis direction, followed by cutting and surface peeling to enhance heat transfer efficiency and structural integrity.
The resulting composite achieves excellent heat transfer performance with a thermal resistance value of 10 mm² K/W or less, providing long-term reliability and improved strength for use in electronic equipment and components.
Smart Images

Figure JP2024014349_17102024_PF_FP_ABST
Abstract
Description
Anisotropic graphite composite and its manufacturing method
[0001] The present invention relates to an anisotropic graphite composite and a method for producing the same.
[0002] Graphite is widely used as an element for effectively transferring and dissipating heat generated by electronic equipment and devices.
[0003] In particular, anisotropic graphite, which has a graphite structure in which six-membered rings are connected by covalent bonds and each graphite structure is bonded by van der Waals forces, has high thermal conductivity. Anisotropic graphite is useful as a heat transfer element that suppresses hot spots that occur in electronic devices and electronic components, which are heat sources, and efficiently transfers heat from the heat source to a cooler.
[0004] Furthermore, anisotropic graphite is structurally brittle and prone to crumbling. To solve this strength issue, a technique has been proposed in which an anisotropic graphite composite formed by laminating anisotropic graphite with layers made of metal, resin, or the like is used as a heat transfer element. For example, Patent Document 1 proposes a technique in which an inorganic material layer is formed on the surface of anisotropic graphite.
[0005] Japanese Patent Publication No. 5930604
[0006] However, the above-described conventional anisotropic graphite composites have room for improvement in terms of heat transfer efficiency.
[0007] In view of the above circumstances, an object of one aspect of the present invention is to provide an anisotropic graphite composite having excellent heat transfer efficiency and a method for producing the same.
[0008] The present inventors have conducted extensive research to solve the above-mentioned problems, and as a result have completed the present invention. That is, one embodiment of the present invention is a graphite composite including (a) anisotropic graphite and (b) an adhesive layer containing a metal and / or a resin, wherein an X axis, a Y axis orthogonal to the X axis, and a Z axis perpendicular to the X-Y plane are defined, and the crystal orientation plane of the graphite layer in the anisotropic graphite is arranged parallel to the X-Y plane, and (a) the anisotropic graphite and (b) the adhesive layer containing a metal and / or a resin are alternately stacked in the Z axis direction and bonded to each other, and the thermal resistance value of the composite measured on a surface parallel to the X-Z plane or the Y-Z plane is 10 mm 2 It is an anisotropic graphite composite with a K / W or less.
[0009] Another embodiment of the present invention is a method for producing an anisotropic graphite composite including (a) anisotropic graphite and (b) an adhesive layer containing a metal and / or a resin, wherein an X axis, a Y axis orthogonal to the X axis, and a Z axis perpendicular to the X-Y plane are defined, and a crystal orientation plane of a graphite layer in the anisotropic graphite is arranged parallel to the X-Z plane, the method comprising: a bonding step of alternately stacking and bonding (a) anisotropic graphite and (b) the adhesive layer containing a metal and / or a resin in the Z axis direction; a cutting step of cutting the obtained bonded body; and a surface peeling step of peeling off a surface parallel to the X-Z plane or the Y-Z plane of the bonded body obtained in the cutting step after cutting.
[0010] According to one embodiment of the present invention, it is possible to provide an anisotropic graphite composite having excellent heat transfer performance and long-term reliability as a heat transfer element, and a method for manufacturing the same.
[0011] 1 is a schematic diagram showing an outline of the configuration of an anisotropic graphite composite according to one embodiment of the present invention; 2 is a diagram showing images of the surfaces of an anisotropic graphite composite according to an example and a comparative example of the present invention, observed with a scanning electron microscope (SEM); 3 is a diagram showing an image of a cross section of a bonded body of anisotropic graphite according to a comparative example of the present invention;
[0012] An embodiment of the present invention will be described below, but the present invention is not limited thereto. The present invention is not limited to the respective configurations described below, and various modifications are possible within the scope of the claims. Furthermore, embodiments or examples obtained by appropriately combining the technical means disclosed in different embodiments or examples are also included in the technical scope of the present invention. Furthermore, new technical features can be formed by combining the technical means disclosed in each embodiment. All academic literature and patent documents described in this specification are incorporated herein by reference. Furthermore, unless otherwise specified in this specification, the term "A to B" representing a numerical range means "greater than or equal to A (including and greater than A) and less than or equal to B (including and less than B)."
[0013] [1. Anisotropic Graphite Composite] An anisotropic graphite composite according to one embodiment of the present invention (hereinafter, may be referred to as "the composite") is a graphite composite including (a) anisotropic graphite and (b) an adhesive layer containing a metal and / or a resin, wherein an X axis, a Y axis orthogonal to the X axis, and a Z axis perpendicular to the X-Y plane are defined, and the crystal orientation plane of the graphite layer in the anisotropic graphite is arranged parallel to the X-Y plane, and (a) the anisotropic graphite and (b) the adhesive layer containing a metal and / or a resin are alternately stacked in the Z axis direction and bonded to each other, and the thermal resistance value measured on a surface of the composite parallel to the X-Z plane or the Y-Z plane is 10 mm 2 K / W or less.
[0014] The composite has the above-described structure and therefore has excellent heat transfer efficiency.
[0015] <1-1. Structure of Anisotropic Graphite Composite> The structure of the present composite will be described in detail with reference to FIG. 1. FIG. 1 is a schematic diagram showing the general configuration of the present composite. As shown in FIG. 1, the present composite 100 includes (a) anisotropic graphite 10 and (b) adhesive layer 20 containing a metal and / or a resin. When an X axis, a Y axis perpendicular to the X axis, and a Z axis perpendicular to the X-Y plane are defined, the crystal orientation plane 11 of the graphite layer in (a) anisotropic graphite 10 is arranged parallel to the X-Y plane, and (a) anisotropic graphite 10 and (b) adhesive layer 20 containing a metal and / or a resin are alternately stacked in the Z-axis direction and bonded to each other.
[0016] (Thickness of Anisotropic Graphite Composite) The thickness of the composite is not particularly limited, but is preferably 1 mm or less, and more preferably 0.5 mm or less. By controlling the thickness of the composite to 1 mm or less, an anisotropic graphite composite with superior heat transfer efficiency can be provided. The lower limit of the thickness of the composite is not particularly limited, but may be, for example, 0.01 mm or more. In this specification, the thickness of the composite refers to the thickness in the direction perpendicular to the cut surface formed in the cutting step described below (for example, when a cut surface parallel to the X-Z plane is formed, the thickness is the thickness in the Y-axis direction, and when a cut surface parallel to the Y-Z plane is formed, the thickness is the thickness in the X-axis direction).
[0017] The thickness of the (a) anisotropic graphite in the Z-axis direction (the thickness of each layer of the (a) anisotropic graphite) in the composite is not particularly limited, but is preferably 10 μm to 1 mm, from the viewpoint of providing a composite with more excellent heat transfer efficiency, more preferably 50 μm to 500 μm, and even more preferably 50 μm to 300 μm.
[0018] The thickness of the (b) metal and / or resin-containing adhesive layer in the present composite in the Z-axis direction (the thickness of each of the (b) metal and / or resin-containing adhesive layers) is not particularly limited, but is preferably 0.1 μm to 1 mm from the viewpoint of providing a composite with better heat transfer efficiency, more preferably 0.5 μm to 300 μm, and even more preferably 1.0 μm to 150 μm or less.
[0019] <1-2. (a) Anisotropic Graphite> The present composite contains (a) anisotropic graphite. In this specification, anisotropic graphite has a block-like structure in which many layers (in other words, graphite layers) having a graphite structure in which six-membered carbon rings are connected by covalent bonds are stacked. The block-like (a) anisotropic graphite has high thermal conductivity in a direction parallel to the crystal orientation plane of the graphite layer. The "anisotropy" of anisotropic graphite means that, due to the orientation of the graphite layers, the thermal conductivity of the anisotropic graphite differs greatly in the directions parallel to and perpendicular to the crystal orientation plane of the graphite layer.
[0020] The anisotropic graphite (a) according to one embodiment of the present invention has a block-like shape in which many layers (i.e., graphite layers) having a graphite structure in which six-membered rings are connected by covalent bonds are stacked. The anisotropic graphite (a) in the block shape has high thermal conductivity in a direction parallel to the crystal orientation plane of the graphite layers.
[0021] The type of (a) anisotropic graphite according to one embodiment of the present invention is not particularly limited as long as it has high thermal conductivity in the plane direction of a graphite structure in which six-membered rings are connected by covalent bonds. Specifically, examples of (a) anisotropic graphite that can be used include polymer-decomposed anisotropic graphite obtained by decomposing (e.g., pyrolyzing) a polymer, graphene oxide, HOPG (Highly Oriented Pyrolytic Graphite), pyrolytic anisotropic graphite obtained by heat-treating Kish graphite, extruded anisotropic graphite obtained by extruding expanded graphite, and molded anisotropic graphite obtained by molding expanded graphite. (a) Anisotropic graphite has high thermal conductivity in the plane direction of the graphite structure in which six-membered rings are connected by covalent bonds, and anisotropic graphite composites containing (a) anisotropic graphite have superior heat transfer performance. Therefore, it is preferable to use polymer-decomposed anisotropic graphite or pyrolytic anisotropic graphite as the (a) anisotropic graphite, and it is more preferable to use polymer-decomposed anisotropic graphite.
[0022] (Method for Producing Anisotropic Graphite) The method for producing (a) anisotropic graphite according to one embodiment of the present invention is not particularly limited, and for example, a so-called polymer pyrolysis method can be adopted, in which a polymer film (e.g., a polyimide film) is heat-treated in an inert gas atmosphere or under reduced pressure. Such a polymer pyrolysis method makes it possible to produce polymer-decomposed anisotropic graphite. More specifically, a method for producing (a) anisotropic graphite using the polymer pyrolysis method includes a carbonization step in which a polymer film (e.g., a polyimide film) is heat-treated at a temperature of about 1400°C to obtain a carbonaceous film, a graphitization step in which the carbonaceous film obtained in the carbonization step is heat-treated at a temperature of about 2900°C to graphitize it, thereby obtaining a film-like anisotropic graphite, and a rolling step in which the obtained film-like anisotropic graphite is rolled.
[0023] (Carbonization Step) (a) The carbonization step in the method for producing anisotropic graphite is a step of carbonizing (carbonizing) a polymer film by heat treating it at a temperature of about 1400° C. The carbonization step is preferably carried out in a vacuum atmosphere, under reduced pressure, or in an inert gas, and nitrogen is preferably used as the inert gas.
[0024] The temperature (maximum temperature) at which the polymer film is heat-treated in the carbonization step is, for example, preferably 1200°C to 1600°C, and more preferably 1300°C to 1500°C.
[0025] (Graphitization Step) (a) The graphitization step of anisotropic graphite is a step of graphitizing the carbonaceous film obtained in the carbonization step by heat treating the carbonaceous film at a temperature of about 2900° C. The graphitization step is preferably carried out under reduced pressure or in an inert gas, and argon or helium can be suitably used as the inert gas, and argon with a small amount of helium added can be more suitably used.
[0026] In the graphitization step, the temperature (maximum temperature) at which the carbonaceous film obtained in the carbonization step is heat-treated is, for example, preferably 2400° C. or higher, preferably 2600° C. or higher, preferably 2800° C. or higher, preferably 2900° C. or higher, or preferably 3000° C. or higher. There is no particular limitation on the upper limit of the maximum temperature, but it is preferably 3300° C. or lower, more preferably 3200° C. or lower.
[0027] (Rolling Step) (a) The rolling step in the method for producing anisotropic graphite is a step of rolling the film of anisotropic graphite obtained in the graphitization step. In this specification, the film of anisotropic graphite obtained in the graphitization step and prior to being subjected to the rolling step may be referred to as the anisotropic graphite film before rolling, and the film of anisotropic graphite after being subjected to the rolling step may be referred to as the anisotropic graphite film after rolling.
[0028] In the rolling step, the method for rolling the anisotropic graphite film is not particularly limited, and examples thereof include a method of applying pressure using a single plate press or a roll press.
[0029] <1-3. (b) Adhesive layer containing metal and / or resin> The composite includes an adhesive layer containing (b) a metal and / or resin. In this specification, the "adhesive layer containing (b) a metal and / or resin" may be referred to as the "adhesive layer (b)."
[0030] (b) The adhesive layer may contain only a metal, may contain only a resin, or may contain both a metal and a resin.
[0031] The metal that can be contained in the (b) adhesive layer is not particularly limited, but is preferably one or more selected from nickel, titanium, iron, chromium, tungsten, and stainless steel, because they are partially compatible with graphite at high temperatures and have good adhesive properties. Among these, nickel is particularly preferred as the metal contained in the (b) adhesive layer, because it has strong adhesive strength and excellent heat transfer performance.
[0032] The resin that can be contained in the (b) adhesive layer is not particularly limited, but is preferably one or more resins selected from acrylic resins, silicone resins, urethane resins, polyimide resins, polyamideimide resins, and epoxy resins, because these resins have the advantage of easily adhering to graphite.
[0033] <1-4. Physical properties of anisotropic graphite composite> (Thermal resistance value) The thermal resistance value of this composite is 10 mm 2 The thermal resistance of the anisotropic graphite composite is 10 mm 2 The thermal resistance of the anisotropic graphite composite in this specification is measured by the method described in the Examples.
[0034] The thermal resistance of this composite is 10 mm 2 However, from the viewpoint of providing a composite having a superior heat transfer efficiency, it is preferable that the heat transfer efficiency is 9 mm 2 It is preferable that the thickness is 8 mm or less. 2 K / W or less is more preferable, and 7 mm 2 It is more preferable that the thickness is 6.5 mm or less. 2The lower limit of the thermal resistance of the composite is not particularly limited, but for example, 2 It can be K / W or more.
[0035] 2. Manufacturing Method of Anisotropic Graphite Composite A manufacturing method of an anisotropic graphite composite according to one embodiment of the present invention (hereinafter, sometimes referred to as "this manufacturing method") will be described. This manufacturing method is a manufacturing method of a composite of anisotropic graphite including (a) anisotropic graphite and (b) an adhesive layer containing a metal and / or a resin, wherein an X axis, a Y axis orthogonal to the X axis, and a Z axis perpendicular to the X-Y plane are defined, and the crystal orientation plane of the graphite layer in the anisotropic graphite is arranged parallel to the X-Y plane, and the manufacturing method includes the following steps: a bonding step of alternately stacking and bonding (a) anisotropic graphite and (b) the adhesive layer containing a metal and / or a resin in the Z-axis direction; a cutting step of cutting the resulting bonded body; and a surface peeling step of peeling off the surface parallel to the X-Z plane or the Y-Z plane of the bonded body obtained in the cutting step.
[0036] Specific embodiments of (a) anisotropic graphite and (b) an adhesive layer containing a metal and / or a resin used in this production method are as described above in the section [1. Anisotropic graphite composite].
[0037] <2-1. Bonding Step> This production method includes a bonding step in which (a) anisotropic graphite and (b) adhesive layers containing a metal and / or a resin are alternately stacked in the Z-axis direction and bonded together. The bonding step can also be said to be a step of obtaining a bonded body of anisotropic graphite to be subjected to the cutting step, in other words, a bonded body before cutting.
[0038] In the bonding step, there are no particular limitations on the method for bonding a laminate (hereinafter, sometimes simply referred to as a "laminate") formed by alternately stacking (a) anisotropic graphite and (b) adhesive layers containing a metal and / or a resin in the Z-axis direction. However, a method of applying a load to the laminate to apply pressure along the Z-axis direction and heating the laminate (hereinafter, referred to as "Method A") can be suitably applied.
[0039] (Lamination Method) In Method A, when laminating (b) a metal forming an adhesive layer containing a metal and / or a resin with (a) anisotropic graphite, the metal can be laminated by (i) directly laminating the metal on (a) anisotropic graphite. More specifically, the metal may be laminated on (a) anisotropic graphite by a coating method, a vacuum deposition method, a CVD method, a sputter deposition method, or the like, or a sheet-shaped metal sheet may be laminated.
[0040] Furthermore, in method A, when (b) a resin forming an adhesive layer containing a metal and / or a resin and (a) anisotropic graphite are laminated together, the resin may be laminated by applying it to (a) anisotropic graphite, or a sheet-like resin sheet may be laminated.
[0041] (Pressure) In Method A, the pressure to be applied to the laminate is not particularly limited as long as it can bond (a) anisotropic graphite and (b) an adhesive layer containing a metal and / or a resin. For example, it is 0.05 to 10 kg / cm. 2 It is preferable to pressurize the laminate with a load of 0.1 to 5 kg / cm 2 It is more preferable to pressurize the laminate with a load of 1000 kJ / cm.sup.2 or more. Pressurizing with the above pressure can provide an anisotropic graphite composite having excellent adhesive strength between the anisotropic graphite particles.
[0042] (Heating) In Method A, the laminate is preferably heated in a vacuum, in an inert gas such as nitrogen and / or argon, in a reducing gas such as hydrogen, or in a mixed gas of an inert gas and a reducing gas. In particular, heating in Method A is preferably performed in an inert gas, because this allows the laminate to be produced without destroying the crystal structure of the anisotropic graphite, and as a result, an anisotropic graphite composite having excellent thermal conductivity can be provided.
[0043] In Method A, the temperature to which the laminate is heated is not particularly limited, but is preferably 700 to 1700° C., and more preferably 1000 to 1600° C. Heating at the above temperatures can provide an anisotropic graphite composite having excellent adhesive strength between the anisotropic graphite particles.
[0044] <2-2. Cutting Step> This manufacturing method includes a cutting step of cutting the bonded body obtained in the bonding step before cutting. The cutting step can also be considered a step of obtaining a cut bonded body, which is a bonded body of anisotropic graphite that is subjected to the surface peeling step. The cutting step can also be considered a step of cutting the bonded body along a plane parallel to the X-Z plane or Y-Z plane of the bonded body (i.e., so that a cut surface parallel to the X-Z plane or Y-Z plane is formed) so that the thickness of the cut bonded body in a direction perpendicular to the X-Z plane or Y-Z plane (in other words, perpendicular to the cut surface) is a desired thickness.
[0045] In the cutting step, the method for cutting the bonded body before cutting is not particularly limited, and any known technique such as a diamond cutter, a wire saw, or machining can be appropriately selected. In particular, it is preferable to cut the bonded body before cutting using a wire saw in the cutting step, since this makes it easy to provide a thinner (thin film) bonded body and an anisotropic graphite composite.
[0046] When the bonded body before cutting is cut using a wire saw in the cutting step, cutting the bonded body before cutting is preferably done under conditions of a cutting speed of 1.0 mm / min or less and 0.01 mm / min or more, more preferably 0.5 mm / min or less and 0.01 mm / min or more, because this reduces the formation of saw marks (irregularities) on the cut surface (surface parallel to the X-Z plane or the Y-Z plane) of the bonded body after cutting, making the cut surface smoother, and as a result, it is possible to provide an anisotropic graphite composite with better heat transfer efficiency.
[0047] <2-3. Surface Peeling Step> This production method includes a surface peeling step in which a surface parallel to the X-Z plane or the Y-Z plane of the cut bonded body obtained in the cutting step is peeled off. Here, the surface parallel to the X-Z plane or the Y-Z plane of the cut bonded body refers to the surface (cut surface) along which the bonded body is cut in the cutting step. The surface peeling step can also be said to be a step in which an anisotropic graphite composite after surface peeling is obtained. The "anisotropic graphite composite" obtained by this production method refers to this anisotropic graphite composite after surface peeling.
[0048] In the surface peeling step, the method for peeling the surface of the bonded body after cutting is not particularly limited, but an example is a method in which an easily peelable adhesive tape is adhered to the surface of the anisotropic graphite composite before surface peeling (a surface parallel to the X-Z plane or the Y-Z plane), and the adhesive tape is then peeled off. The adhesive tape that can be used in this method is not particularly limited, and any common adhesive tape can be used, but suitable examples include mending tape manufactured by 3M having an acrylic adhesive layer, and polyimide tape having a silicone adhesive layer.
[0049] In the course of intensive research to provide an anisotropic graphite composite with excellent heat transfer efficiency, the present inventors discovered that in a conventional anisotropic graphite composite (manufactured without a surface exfoliation step), on the surface in the X-Z or Y-Z plane that comes into contact with a heat source, (i) the edges of each graphite layer forming the anisotropic graphite composite present on the surface are covered with fine deposits, and (ii) the edges are oriented in a direction approximately parallel to the X-Z or Y-Z plane. The present inventors believed that the above (i) and (ii) reduced the heat transfer efficiency of conventional anisotropic graphite composites, and conducted further intensive research to provide an anisotropic graphite composite that does not suffer from the above (i) and (ii). As a result, the present inventors have found that, by further carrying out a surface peeling step after the cutting step, (I) fine deposits present on the surface of the anisotropic graphite composite before the surface peeling can be removed, and (II) an anisotropic graphite composite can be provided in which the edges of each graphite layer forming the anisotropic graphite composite are oriented in a substantially vertical direction, and that this anisotropic graphite composite after the surface peeling has excellent heat transfer efficiency, thereby completing the present invention.
[0050] In other words, the anisotropic graphite composite obtained by the present production method (present composite) can also be said to be an anisotropic graphite composite in which (I) there are almost no fine deposits on the surface in the X-Z plane or the Y-Z plane, and (II) the ends of each graphite layer forming the anisotropic graphite composite are oriented in a substantially vertical direction.
[0051] The state of the edges of each graphite layer forming the anisotropic graphite composite can be observed using, for example, a scanning electron microscope (SEM).
[0052] 3. Others An embodiment of the present invention may include the following configuration.
[0053] [1] A graphite composite comprising (a) anisotropic graphite and (b) an adhesive layer containing a metal and / or a resin, wherein an X axis, a Y axis perpendicular to the X axis, and a Z axis perpendicular to the X-Y plane are defined, and the crystal orientation plane of the graphite layer in the anisotropic graphite is arranged parallel to the X-Y plane, and (a) the anisotropic graphite and (b) the adhesive layer containing a metal and / or a resin are alternately stacked in the Z axis direction and bonded to each other, and the thermal resistance value measured on a surface of the composite parallel to the X-Z plane or the Y-Z plane is 10 mm 2 K / W or less of anisotropic graphite composite.
[0054] [2] The anisotropic graphite composite according to [1], wherein the metal is at least one selected from the group consisting of nickel, titanium, iron, chromium, tungsten, and stainless steel.
[0055] [3] The anisotropic graphite composite according to [1], wherein the resin is at least one selected from the group consisting of an acrylic resin, a silicone resin, a urethane resin, a polyimide resin, a polyamide-imide resin, and an epoxy resin.
[0056] [4] The thermal resistance value is 8 mm 2 [4] The anisotropic graphite composite according to any one of [1] to [3], wherein the anisotropic graphite composite has a tensile strength of 1000 kJ / W or less.
[0057] [5] The anisotropic graphite composite according to any one of [1] to [4], wherein the anisotropic graphite (a) is polymer-decomposed anisotropic graphite or pyrolytic anisotropic graphite.
[0058] [6] A method for producing an anisotropic graphite composite including (a) anisotropic graphite and (b) an adhesive layer containing a metal and / or a resin, wherein an X axis, a Y axis orthogonal to the X axis, and a Z axis perpendicular to the X-Y plane are defined, and a crystal orientation plane of a graphite layer in the anisotropic graphite is arranged parallel to the X-Z plane, the method comprising: a bonding step of alternately stacking and bonding (a) anisotropic graphite and (b) the adhesive layer containing a metal and / or a resin in the Z axis direction; a cutting step of cutting the obtained bonded body; and a surface peeling step of peeling off a surface parallel to the X-Z plane or the Y-Z plane of the bonded body obtained in the cutting step after cutting.
[0059] [7] The method for producing an anisotropic graphite composite according to [6], wherein the cutting step includes a step of cutting the anisotropic graphite composite using a wire saw at a cutting speed of 1.0 mm / min or less.
[0060] [8] The method for producing an anisotropic graphite composite according to [6] or [7], wherein the metal is at least one selected from the group consisting of nickel, titanium, iron, chromium, tungsten, and stainless steel.
[0061] [9] The method for producing an anisotropic graphite composite according to any one of [6] to [8], wherein the resin is at least one selected from the group consisting of an acrylic resin, a silicone resin, a urethane resin, a polyimide resin, a polyamide-imide resin, and an epoxy resin.
[0062]
[10] The method for producing an anisotropic graphite composite according to any one of [6] to [9], wherein the anisotropic graphite (a) is polymer-decomposed anisotropic graphite or pyrolytic anisotropic graphite.
[0063] Hereinafter, one embodiment of the present invention will be described in detail with reference to examples and comparative examples, but the technical scope of the present invention is not limited to these examples.
[0064] [Method for Measuring Thermal Resistance Values] The thermal resistance values of the composites and adhesive bodies obtained in the Examples and Comparative Examples were measured as follows: A sample measuring 10 mm long x 10 mm wide was cut out from the composite or adhesive body of any thickness obtained. The thermal resistance value (thermal resistance value in the thickness direction of the composite or adhesive body) of the obtained sample was measured using a resin thermal resistance measuring device (manufactured by Hitachi Technology and Services Co., Ltd.) at a sample temperature of 50°C and a constant load of 20 N.
[0065] Example 1 A polyimide film (Apical NPI manufactured by Kaneka) having a thickness of 75 μm and a size of 250 mm length × 310 mm width and a natural graphite sheet having a thickness of 200 μm and a size of 260 mm length × 320 mm width were alternately laminated in an amount of 100 sheets each to obtain a laminate having a thickness of 27.5 mm. A graphite weight was placed on the obtained laminate, and a weight of 5 g / cm 2 The polyimide film was carbonized by heating it to 1400°C at a heating rate of 0.5°C / min and holding it at 1400°C for 10 minutes, thereby obtaining a carbonized film.
[0066] Next, the obtained carbonized film was laminated again with 100 natural graphite sheets having a thickness of 200 μm and a size of 260 mm length × 320 mm width, to obtain a laminate having a thickness of 27.5 mm. A graphite weight was placed on the obtained laminate, and a weight of 5 g / cm 2 The carbonized film was graphitized by placing the film in a graphitization furnace under a load of 1.0 kg / cm2, raising the temperature to 2900°C at a heating rate of 3.3°C / min, and holding the film at 2900°C for 10 minutes, thereby obtaining an anisotropic graphite film.
[0067] One hundred of the obtained anisotropic graphite films (thickness: 300 μm) were stacked, and the laminate was sandwiched between a polyimide film, a Teflon (registered trademark) film, a cushioning rubber material, and an iron plate on the top and bottom, and rolled by applying a pressure of 20 MPa at room temperature using a single-plate press, to obtain a rolled anisotropic graphite film (thickness: 200 μm).
[0068] The rolled anisotropic graphite film was cut into 400 sheets measuring 40 mm long x 40 mm wide. These 400 anisotropic graphite films were alternately stacked with 399 sheets of nickel foil, each 5 μm thick and 40 mm long x 40 mm wide, to obtain a laminate. This laminate was heated in argon gas at 0.4 kg / cm 2 While applying a pressure of 1000 kJ / min, the temperature was increased to 1340°C at a heating rate of 2.0°C / min and maintained at 1340°C for 30 minutes, thereby bonding the anisotropic graphite film and the nickel foil by heat fusion, thereby producing an anisotropic graphite / nickel bonded body A-1 (thickness: 60 mm, size: length 40 mm x width 40 mm) in which adhesive layers made of anisotropic graphite and nickel were alternately laminated. For the obtained bonded body A-1, the plane parallel to the crystal orientation plane of the graphite layer of the anisotropic graphite was defined as the X-Y plane, and the thickness direction was defined as the Z axis.
[0069] The obtained bonded body A was cut in a direction parallel to the Y-Z plane using a wire saw (Model WSD-K2, manufactured by Takatori Corporation) at a cutting speed of 0.5 mm / min to obtain an anisotropic graphite / nickel bonded body B-1 (bonded body after cutting) having a thickness of 0.25 mm (X axis) and a size of 40 mm (Y axis) x 60 mm (Z axis) (cutting step). Further, this bonded body B-1 was cut into samples having a thickness of 0.25 mm (X axis direction) and a size of 10 mm (Y axis) x 10 mm (Z axis). The thermal resistance value (thermal resistance value in the X axis direction) of the obtained bonded body B-1 sample was measured, and the thermal resistance value was 10.8 mm. 2 The bonded structure B-1 had a surface parallel to the Y-Z plane and a thickness of 100 mm. The bonded structure B-1 had ... surface parallel to the Y-Z plane and a thickness of 100 mm. The surface of the bonded structure B-1 parallel to the Y-Z plane was observed using a scanning electron microscope (SEM). An image obtained by SEM at a magnification of 500 times is shown in FIG. 2 (top). As shown in FIG. 2 (top), on the surface parallel to the Y-Z plane of the bonded structure B-1, the ends of the graphite particles forming each graphite layer were covered with fine deposits, and further, the ends were oriented in a direction approximately parallel to the Y-Z plane.
[0070] For the sample of the bonded body B-1, mending tape (manufactured by 3M) was attached to both surfaces parallel to the YZ plane and then carefully peeled off to obtain an anisotropic graphite / nickel composite C-1 (graphite composite after surface peeling) (surface peeling step). The thermal resistance value (thermal resistance value in the X-axis direction) of the obtained composite C-1 was measured, and the thermal resistance value was 5.7 mm 2 The composite C-1 had a surface parallel to the Y-Z plane, and the surface was observed using a scanning electron microscope (SEM). An image obtained by SEM at a magnification of 500 times is shown in FIG. 2 (lower diagram). As shown in FIG. 2 (lower diagram), on the surface parallel to the Y-Z plane of composite C-1, the ends of the graphite particles forming each graphite layer were oriented in a direction approximately perpendicular to the Y-Z plane.
[0071] Example 2 The bonded body A-1 obtained in Example 1 was cut in a direction parallel to the Y-Z plane using a wire saw (Model WSD-K2, manufactured by Takatori Corporation) at a cutting speed of 0.5 mm / min to obtain an anisotropic graphite / nickel bonded body B-2 having a thickness of 0.30 mm (X axis) and a size of 40 mm (Y axis) x 60 mm (Z axis) (cutting step). Visual inspection of the cut surface of the obtained bonded body B-2 revealed no saw marks from the wire saw. Furthermore, this bonded body B-2 was cut into samples having a thickness of 0.30 mm (X axis) and a size of 10 mm (Y axis) x 10 mm (Z axis). The thermal resistance value (thermal resistance value in the X axis direction) of the obtained bonded body B-2 sample was measured, and the thermal resistance value was 15.0 mm. 2 It was K / W.
[0072] For the sample of the bonded body B-2, mending tape (manufactured by 3M) was attached to both surfaces parallel to the YZ plane and then carefully peeled off to obtain an anisotropic graphite / nickel composite C-2 (graphite composite after surface peeling) (surface peeling step). The thermal resistance value (thermal resistance value in the X-axis direction) of the obtained composite C-2 was measured, and the thermal resistance value was 6.2 mm 2The results are shown in Table 1. Furthermore, the surface of composite C-2 parallel to the YZ plane was observed using a scanning electron microscope (SEM). On the surface of composite C-2 parallel to the YZ plane, the ends of the graphite particles forming each graphite layer were oriented in a direction approximately perpendicular to the YZ plane (not shown).
[0073] Comparative Example 1 The bonded body A-1 obtained in Example 1 was cut at an angle perpendicular to the X axis using a wire saw (Model WSD-K2, manufactured by Takatori Corporation) at a cutting speed of 1.5 mm / min to obtain an anisotropic graphite / nickel bonded body B-3 having a thickness of 0.40 mm (X axis) and a size of 40 mm (Y axis) x 60 mm (Z axis). The cut surface of the obtained bonded body B-3 was visually inspected, and the results are shown in Figure 3. As shown in Figure 3, saw marks from the wire saw were observed on the cut surface of the bonded body B-3. Furthermore, this bonded body B-3 was cut into a sample having a thickness of 0.40 mm (X axis) and a size of 10 mm (Y axis) x 10 mm (Z axis). The thermal resistance value (thermal resistance value in the X axis direction) of the obtained bonded body B-3 sample was measured, and the thermal resistance value was 24.6 mm. 2 It was K / W.
[0074] [Summary] The composites of Examples 1 and 2 obtained through the cutting process and the surface peeling process both had a thermal resistance of 10 mm 2 On the other hand, it can be seen from Comparative Example 1 that the heat transfer performance of the obtained composite is poor when the surface peeling step is not performed.
[0075] According to one embodiment of the present invention, an anisotropic graphite composite having excellent heat transfer efficiency can be provided. Such an anisotropic graphite composite can be suitably used in fields such as electronic devices and electronic components.
[0076] 10 Anisotropic graphite 11 Crystal orientation plane of graphite layer of anisotropic graphite 20 Adhesive layer 100 Anisotropic graphite composite
Claims
1. An anisotropic graphite composite comprising (a) anisotropic graphite and (b) an adhesive layer containing a metal and / or resin, with an X axis, a Y axis perpendicular to the X axis, and a Z axis perpendicular to the X-Y plane, the crystal orientation plane of the graphite layer in the anisotropic graphite (a) is arranged parallel to the X-Y plane, the anisotropic graphite (a) and the adhesive layer containing a metal and / or resin (b) are alternately laminated in the Z-axis direction and bonded to each other, and the thermal resistance value of the anisotropic graphite composite measured on a surface parallel to the X-Z plane or the Y-Z plane is 10 mm 2 K / W or less.
2. The anisotropic graphite composite according to claim 1, wherein the metal is at least one selected from the group consisting of nickel, titanium, iron, chromium, tungsten, and stainless steel.
3. The anisotropic graphite composite according to claim 1, wherein the resin is at least one selected from the group consisting of acrylic resin, silicone resin, urethane resin, polyimide resin, polyamideimide resin, and epoxy resin.
4. The thermal resistance is 8 mm 2 2. The anisotropic graphite composite of claim 1, wherein the anisotropic graphite composite has a hardness of 0.1 K / W or less.
5. The anisotropic graphite composite according to claim 1, wherein the anisotropic graphite (a) is polymer-decomposed anisotropic graphite or pyrolytic anisotropic graphite.
6. A method for producing an anisotropic graphite composite comprising (a) anisotropic graphite and (b) an adhesive layer containing a metal and / or resin, the method comprising: an X-axis, a Y-axis perpendicular to the X-axis, and a Z-axis perpendicular to the X-Y plane; a crystal orientation plane of a graphite layer in the anisotropic graphite (a) is arranged parallel to the X-Y plane; and the method comprises: a bonding step of alternately stacking and bonding the anisotropic graphite (a) and the adhesive layer containing a metal and / or resin (b) in the Z-axis direction; a cutting step of cutting the bonded body obtained in the bonding step; and a surface peeling step of peeling off a surface parallel to the X-Z plane or the Y-Z plane of the bonded body obtained after cutting in the cutting step.
7. The method for producing an anisotropic graphite composite according to claim 6, wherein the cutting step includes a step of cutting the bonded body using a wire saw at a cutting speed of 1.0 mm / min or less.
8. The method for producing an anisotropic graphite composite according to claim 6, wherein the metal is at least one selected from the group consisting of nickel, titanium, iron, chromium, tungsten, and stainless steel.
9. The method for producing an anisotropic graphite composite according to claim 6, wherein the resin is at least one selected from the group consisting of acrylic resin, silicone resin, urethane resin, polyimide resin, polyamideimide resin, and epoxy resin.
10. The method for producing an anisotropic graphite composite according to claim 6, wherein the anisotropic graphite (a) is polymer-decomposed anisotropic graphite or pyrolytic anisotropic graphite.
Citation Information
Patent Citations
Graphite thermal conductor and cold plate using the same
JP1995109171A
Carbon nano-tube based thermal boundary surface material, and method for manufacturing and using the same
JP2018163147A
Heat conductive sheet and method of manufacturing the same
JP2020140982A
Heat conductive sheet
US10724810B1
Methods for Reducing Thermal Resistance of Carbon Nanotube Arrays or Sheets
US20140227477A1