Dry particle emulsions

The production of silk fibroin fibre particles with specific geometry through alkaline hydrolysis and milling allows for the formation of stable Pickering emulsions at low silk loadings, addressing the inefficiencies and toxicity issues of existing methods, and enabling scalable industrial applications.

WO2024216331A1PCT designated stage expired Publication Date: 2024-10-24DEAKIN UNIVERSITY
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
PCT/AU2024/050364
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-04-18
Filing Date
2024-04-17
Publication Date
2024-10-24

AI Technical Summary

Technical Problem

Current methods for producing stable Pickering emulsions using silk fibroin require lengthy, chemical-intensive processes and high silk concentrations, making them unsuitable for industrial applications due to toxicity concerns and inefficiency.

Method used

Development of silk fibroin fibre particles with a specific aspect ratio and width, produced through alkaline hydrolysis, cutting, and dry milling, which can form stable Pickering emulsions at low silk loadings, using a scalable and short process.

Benefits of technology

The method enables the production of stable Pickering emulsions with low silk concentrations, overcoming the limitations of traditional processes by ensuring particle geometry is suitable for industrial-scale applications and safety standards.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure AU2024050364_24102024_PF_FP_ABST
    Figure AU2024050364_24102024_PF_FP_ABST
Patent Text Reader

Abstract

The present invention provides a method of producing silk fibroin fibre particles wherein at least 90% of the particles have an aspect ratio of between 2.5 and 40 and wherein the average width of the particles is at least 800 nm, the method comprising: (i) providing degummed and partially hydrolysed silk fibroin fibres by subjecting a silk starting material to alkaline hydrolysis; (ii) cutting the degummed and partially hydrolysed silk fibroin fibres until the cut silk fibres will pass through a 2 mm grid; and (iii) milling the cut silk fibres to produce silk fibroin fibre particles, wherein 90% of the particles have an aspect ratio of between 2.5 and 40 and wherein the average width of the particles is at least 800 nm.
Need to check novelty before this filing date? Find Prior Art

Description

[0001]Dry Particle Emulsions Technical Field The present invention relates to the preparation and use of modified silk fibroin fibre particles which can be used in the preparation of a wide range of oil in water and water in oil Pickering emulsions (PE). The modified silk fibroin fibre particles may be used as emulsifiers in the formation of Pickering emulsions useful in a number of applications particularly in the cosmetics, pharmaceutical, biomedical, medtech and food industries given the safety profile of silk as a protein material. The applicants have found that Pickering emulsions produced using the modified silk fibroin fibre particles of the present invention are stable and can be produced with quite low loadings of silk compared to the disperse phase which is emulsified. In addition emulsions of the present invention can typically be formed with much lower loadings of silk compared to traditional chemical emulsifiers. Background of Invention Emulsions are found in a wide variety of products in everyday use including foods, cosmetics and pharmaceuticals. An emulsion can be understood to be a mixture of two or more liquids in which one of the liquids is present in the form of droplets of microscopic size or finer which are distributed throughout the other liquid. Simple emulsions are either oil droplets distributed in continuous water phase (called an oil in water emulsion (O / W)) or water droplets distributed in continuous oil phase (a water in oil emulsion (W / O)). Merely by way of example milk is an everyday example of an oil in water emulsion in which the fat phase of the milk forms tiny droplets within the water phase. In contrast to this margarine is an example of a water in oil emulsion as it consists of tiny droplets of water dispersed throughout a blend of vegetable oils. The presence of emulsions in society and their extensive use in the food, cosmetics and pharmaceutical industry has lead to them being extensively studied in order to be able to provide stable emulsions. Thus whilst it is well known that a simple emulsion can be temporarily produced by subjecting a mixture of oil and water to high shear (such as by rapid mixing). Emulsions of this type are formed in essence by breaking up the dispersed phase into fine droplets within the continuous phase but require significant energy input to produce the required increase in interfacial area between the two phase. Unfortunately it is also well known that these emulsions are very unstable and tend to break down quite quickly leading to separation of oil and water phases unless an additive is used to stabilise the emulsion. In order to stabilise emulsions and extend the life of any products that are in the form of an emulsion there has been significant research conducted into the identification and development of emulsifiers that help stabilise the emulsion once formed. Accordingly there are now a wide range of natural and synthetic emulsifiers in use in various industries. In general emulsifiers work as they create a physical barrier that keeps the droplets from coalescing with each other which would ultimately lead to phase separation. In general, a typical emulsifier consists of a hydrophilic (water loving) head group and a hydrophobic (oil loving) tail group. As such emulsifiers are attracted to both the water phase and the oil phase and when added to a mixture containing both water and oil they tend to congregate at the surface of the droplets in the mixture such that the water loving head group is present in the water phase and the oil loving tail group is present in the oil phase. As such in the case of an oil in water emulsion the emulsifier sits around the oil droplet with the hydrophilic head group extending out into the water phase and the hydrophilic tail group extending around and into the oil droplet. Given the broad range of applications of emulsions in food, cosmetics and pharmaceuticals a potential concern is the safety profile of any emulsifier used. Accordingly, in the formation of emulsions there is always a concern that the emulsifier used may be having an unintended effect in the final formulation. As such research is constantly being carried out to identify new emulsifiers. Historically most commonly used emulsifiers have been compounds that are soluble in either the dispersed phase or the continuous phase and as a result of their amphiphilic nature accumulate at the interface between the continuous phase and the dispersed phase. In this role they “stabilise” the emulsion as they prevent the droplets of the dispersed phase from coalescing. Pickering emulsions have garnered interest in more recent times. A Pickering emulsion is an emulsion which is stabilised by solid particles as the emulsifier rather than by a compound that dissolves in the continuous or dispersed phases. As a result of their unique properties Pickering emulsions have the potential to find application in a number of areas in which emulsions are used. Whilst there has been significant research carried out to date most Pickering emulsions are formed using inorganic particles like silica and the like. There are relatively few organic materials that will form insoluble particles that can be used to form Pickering emulsion. Such number is limited as it has been found that it is important for Pickering emulsion particles to have a water contact angle close to 90 deg. Accordingly, most organic particles need to be modified to increase or decrease contact angle to form Pickering emulsions. One area of research into the identification of potential emulsifiers in the formation of Pickering emulsions is an analysis of naturally occurring materials where these are perceived to be less likely to lead to any undesirable side effects. As such groups have conducted research into naturally occurring cellulose, peptides and proteins to determine if they have the ability to be used as emulsifiers in the formation of Pickering emulsions. An example of a naturally occurring material that has previously been reported to be able to be used in the formation of Pickering emulsions are silk fibres. Silk is a naturally occurring fibre that is produced by a wide variety of arthropods with the most commercially significant being silk produced by the Bombyx mori silkworm reared using Mulberry tree leaves. In its natural form silk is predominantly made up of an insoluble protein known as fibroin which is coated by a smaller amount of a water soluble protective layer known as sericin and it may also contain small amounts of other substances. Whilst the process of silk manufacture varies from country to country almost all processes involve one or more steps in which the silk is treated to remove the gummy protein sericin leaving the “degummed” fibre made of fibroin protein. This typically involves heating of the fibres in alkali at elevated temperature. Silk has been previously reported as an emulsifier in the form of a silk nanofibers. Unfortunately the reported nanofibre production requires a long, chemical intensive process route to convert silk fibre into solution. For example the reported procedure requires at least 72 hours of dialysis to remove toxic materials like LiBr used for dissolution of silk, then a further 24 plus hours for nano particles formation from solution and then a further more than 24 hrs to get self-assembled nanofibres. Accordingly, the produced nanofibers are not commercially attractive due to the time taken to produce the fibres and the use of toxic materials such as LiBr in their manufacture which makes their use problematic in foods, cosmetics and medtech, pharmaceuticals and biopharmaceuticals. In a further attempt to use silk in the formation of emulsions it has been reported that emulsions can be formed using ball milled silk particles obtained using a standard silk isolation process in which silk has been treated to remove the water soluble sericin. The reported literature suggests that whilst this material may be used in the formation of emulsions there is a requirement that the emulsion contain at least 10% silk in order to provide a suitable stable emulsion. In addition the reported emulsion contained droplets with a droplet size of 100 micron or higher which is undesirable. Many previous processes for the generation of potential emulsifiers have focused on the production of nano scale particles which were believed to be required for the production of a stable emulsion. A skilled worker in the field would generally not have expected to be able to form a strong emulsion with strong stability with micron size particles as it was believed that the presence of nanometre particles was required for the formation of a strong emulsion. The present invention demonstrates that if proper aspect ratio is maintained then micron size particles produced using simple, scalable and short processes are able to produce good emulsions. Accordingly, it would be desirable to provide alternative silk based emulsifiers that could find application in the preparation of Pickering emulsions in a wide variety of industries due to its consumer acceptance (being a natural product) and its status of being Generally recognised as safe (GRAS) by regulatory bodies such as the FDA. Summary of Invention As a result of the desire to provide alternative silk based emulsifiers , the applicants have identified a relatively straightforward process that can be utilised to modify silk to make it suitable for use as an emulsifier in the preparation of Pickering emulsions that find use in a number of industrial applications. The applicants have identified that a specific combination of processing steps when carried out in combination produce silk fibroin fibre particles with a suitable particle geometry which enables them to be used to form stable Pickering emulsions at relatively low loadings of silk in the final emulsion. In particular the applicants have found that silk fibroin fibre particles wherein at least 90% of the particles have an aspect ratio of between 2.5 and 40 and wherein the average width of the particles is at least 800 nm are particularly suitable for use in the formation of stable Pickering emulsions. Accordingly, the present invention provides silk fibroin fibre particles wherein at least 90% of the particles have an aspect ratio of between 2.5 and 40 and wherein the average width of the particles is at least 800 nm. As stated above these particles are found to be able to be used in the formation of Pickering emulsions at quite low loadings of silk. The applicants have also developed a process for the production of particles of this type. Accordingly, in yet an even further aspect the present invention provides a method of producing silk fibroin fibre particles wherein at least 90% of the particles have an aspect ratio of between 2.5 and 40 and wherein the average width of the particles is at least 800 nm, the method comprising: (i) providing degummed and partially hydrolysed silk fibroin fibres by subjecting a silk starting material to alkaline hydrolysis, (ii) cutting the degummed and partially hydrolysed silk fibroin fibres until the cut silk fibres will pass through a 2 mm grid; and (iii) dry milling the cut silk fibres to produce silk fibroin fibre particles wherein at least 90% of the particles have an aspect ratio of between 2.5 and 40 and wherein the average width of the particles is at least 800 nm. The process has been found to produce silk fibroin fibre particles with the desired properties on a consistent basis and is applicable to industrial scale up relatively easily. In yet an even further aspect the present invention provides a method of producing an emulsion the method comprising a) combining silk fibroin fibre particles wherein at least 90% of the particles have an aspect ratio of between 2.5 and 40 and wherein the average width of the particles is at least 800 nm with a first component to form a dispersed mixture of the silk fibroin fibre particles in the first component; (b) adding a second component which is immiscible with the first component to the mixture; and (c) subjecting the product of step (b) to high shear to form an emulsion. In yet an even further aspect still the present invention provides a formulation in the form of an emulsion comprising (a) silk fibroin fibre particles wherein at least 90% of the particles have an aspect ratio of between 2.5 and 40 and wherein the average width of the particles is at least 800 nm, (b) an organic diluent, (c) water and (d) one or more active ingredients. Description of the Drawings Figures 1(a) and Fig 1(b) Mulberry silk from B.mori silkworm hydrolysed using 3g / L sodium carbonate before cutter milling at different magnifications. Figures 2(a) and Fig 2(b) Mulberry silk from B.mori silkworm hydrolysed using 6g / L sodium carbonate before cutter milling at different magnifications. Figures 3(a) and Fig 3(b) Mulberry silk from B.mori silkworm hydrolysed using 15g / L sodium carbonate before cutter milling at different magnifications. Figures 4(a) 4(b) and 4(c) Snippets after Cutter milling (4a):M-3 (mulberry silk particles formed after a treatment of 3g / L sodium carbonate); (4b): M-10 mulberry silk particles formed after a treatment of 10g / L sodium carbonate; ( 4c) M-30 (mulberry silk particles formed after a treatment of 30g / L sodium carbonate). Figures 5 and 6 (a) to (d) 5(a) and 6(a) M-3-AJM; 5(b) and 6(b) M-6-AJM; 5(c) and 6(c) M-10-AJM; 5 (d) and 6(d) M-30-AJM. Figures 5 are low magnification and Figures 6 higher magnification for the same sample. Figure 7 shows the gel image from example 3. Figure 8 shows d.5 (µm) based on volume based size distribution of emulsion droplets for emulsions prepared from different alkali hydrolysis and silk particle loading. Figure 9 Volume based size distribution of emulsion droplets for M-6-AJM based emulsions for different particle loading. Figure 10 SEM images of emulsion from M-6-AJM particles (Row 1: 0.25 % silk; Row 2: 0.5 %silk; Row 3: 1 %silk; Row 4: 2 % silk; oil: 30 %. The images show how droplet size decrease as the silk content is increased (i.e. Oil to Silk ratio decrease). Figure 11 Emulsion droplet size vs Oil: silk ratio; size of droplets were measured based on volume based size distribution. Figure 12 Shear Thinning Behaviour of Emulsion prepared from 1 % silk and 30 % oil for M-6-AJM based emulsion. Figure 13 Stability of Emulsion on storage and application of mechanical force. Detailed Description In this specification, a number of terms are used that are well known to a skilled addressee. Nevertheless, for the purposes of clarity, a number of terms will be defined. Throughout this specification, unless the context requires otherwise, the word “comprise”, or variations such as “comprises” or “comprising”, will be understood to imply the inclusion of a stated element or integer or group of elements or integers but not the exclusion of any other element or integer or group of elements or integers. It is to be noted that where a range of values is expressed, it will be clearly understood that this range encompasses the upper and lower limits of the range, and all numerical values or sub-ranges in between these limits as if each numerical value and sub-range is explicitly recited. The statement "about X% to Y%" has the same meaning as "about X% to about Y%," unless indicated otherwise. The term “about” as used in the specification means approximately or nearly and in the context of a numerical value or range set forth herein is meant to encompass variations of + / - 10% or less, + / - 5% or less, + / - 1% or less, or + / - 0.1% or less of and from the numerical value or range recited or claimed. It is also to be noted that, as used herein, the singular forms “a”, “an” and “the” include plural aspects unless the context already dictates otherwise. An “emulsion” is a mixture of two or more liquids that are normally immiscible (unmixable or unblendable), with one of the liquids forming the dispersed phase and the other liquid forming the dispersion medium. Two liquids can form a number of different types of emulsions. By way of example, oil and water can form an oil-in-water emulsion where the oil is the dispersed phase and the water is the dispersion medium. Alternatively, they can form a water-in-oil emulsion where water is the dispersed phase and oil is the dispersion medium. Multiple emulsions are also possible such as a water- in-oil-in-water emulsion or an oil-in-water-in-oil emulsion. In circumstances where there are multiple similar phases in the same emulsion (like the two oil phases in an oil-in- water-in-oil emulsion) each phase may contain a different solute. As used herein the term “stable emulsion” refers to an emulsion that in which there is less than a 5% increase in mean droplet size over the first two weeks of storage at ambient temperature. As used herein the term “miscibility” and derivations thereof such as “miscible” refers to the property or ability of two substances to mix in all proportions, or put another way, their ability to fully dissolve in each other at any concentration. Accordingly as used herein the term “water-immiscible” means that there are certain proportions of the substance where it does not dissolve in water. For example, butanone (methyl ethyl ketone) is significantly soluble in water but is still classed as water-immiscible as these two solvents are not soluble in each other in all proportions. As used herein the term “oil” refers to any nonpolar chemical substance that is both hydrophobic and lipophilic, and may include triesters of glycerol and fatty acids. Oils are typically liquids at room temperature. The term “aspect ratio” of a particle is typically defined as the ratio of its longest dimension to its shortest dimension. For example the aspect ratio of a circle is 1. It is to be appreciated, however, that in assessing the aspect ratio of certain particles and fibres of the present invention that there may be a weak spot where the width is very small. To overcome these anomalies in assessing this value the aspect ratio is determined to be the ratio of the length of the longest dimension to its average width where width is measured perpendicular to its longitudinal axis. Determining aspect ratio in this way provides a more accurate assessment of the aspect ratio as it takes into account variations of the width of a fibre or particle along its length as well as removing the anomaly that would be caused by a fibre containing a weak point where it is typically very narrow at a single point which is not representative of dimensions of the fibre as a whole. As used herein the term “average width” refers to the width of a fibre when three or more measurements are taken of the width of the fibre perpendicular to its longitudinal axis and the average of these measurements is determined. The measurements are typically taken at regular points along the longitudinal axis such as 25% of the way along the longitudinal axis, 50% of the way along the longitudinal axis and 75% of the way along the longitudinal axis. As would be clear to a skilled worker in the art in describing particles made by milling there is typically some degree of variation in the particles dimensions as a whole with there generally being a distribution of particles. Accordingly in describing the particles of the present invention we have referred to language such as “wherein at least 90% of the particles have an aspect ratio of between 2.5 and 40.” For the avoidance of doubt in this and related phrases the 90% refers to the number percentage of the particles such that 90% of the total number of particles used for measurements having an aspect ratio of between 2.5 and 40. Put another way for every 100 particles, 90 will have an aspect ratio of between 2.5 and 40. As discussed above the present invention provides novel silk fibroin fibre particles, methods for their production, methods for the use of particles of this type in the formation of emulsions and formulations in the form of an emulsion containing the particles. Silk Fibroin Particles of the invention As discussed above silk is a naturally occurring fibre that is produced by a wide variety of arthropods. In its natural form silk is predominantly made up of an insoluble protein known as fibroin which is coated by a smaller amount of a water soluble protective layer known as sericin and it may also contain small amounts of other substances. During processing the sericin is removed and the remaining fibron fibres are processed in the textile industry. Whilst this form of silk fibre is well known it cannot readily be used in the formation of emulsion due to its size and properties. Accordingly a significant amount of research has been conducted in order to identify modifications to silk fibroin fibres that may make them suitable for use in the formation of Pickering emulsions. The applicants have found that silk fibroin fibre particles wherein at least 90% of the particles (by number) have an aspect ratio of between 2.5 and 40 and wherein the average width of the particles is at least 800 nm are particularly suitable as emulsifiers in the formation of Pickering emulsions. In one embodiment at least 90% of the silk fibroin fibre particles (by number) have an aspect ratio of less than 35. In one embodiment at least 90% of the silk fibroin fibre particles (by number) have an aspect ratio of less than 30. In one embodiment at least 90% of the silk fibroin fibre particles (by number) have an aspect ratio of less than 25. In one embodiment at least 90% of the silk fibroin fibre particles (by number) have an aspect ratio of less than 20. In one embodiment at least 90% of the silk fibroin fibre particles (by number) have an aspect ratio of less than 15. In one embodiment at least 90% of the silk fibroin fibre particles (by number) have an aspect ratio of less than 10. In one embodiment at least 90% of the silk fibroin fibre particles (by number) have an aspect ratio between 2.5 and 35. In one embodiment at least 90% of the silk fibroin fibre particles (by number) have an aspect ratio between 7.5 and 35. In one embodiment at least 90% of the silk fibroin fibre particles (by number) have an aspect ratio between 7.5 and 30. In one embodiment at least 90% of the silk fibroin fibre particles (by number) have an aspect ratio between 7.5 and 25. In one embodiment at least 90% of the silk fibroin fibre particles (by number) have an aspect ratio between 7.5 and 20. In one embodiment at least 90% of the silk fibroin fibre particles (by number) have an aspect ratio between 7.5 and 15. In one embodiment at least 90% of the silk fibroin fibre particles (by number) have an aspect ratio between 7.5 and 10. As will be appreciated the applicants have found that the aspect ratio alone does not provide a particle with desired properties. The applicants have found that the combination of the aspect ratio and the width of the particles is important in ensuring adequate particle performance to form a good stable emulsion. As such the silk fibroin fibre particles are also of a defined width in order to create the required Pickering emulsion. In general the applicants have found that it is necessary that the average width of the particles be at least 800 nm. In one embodiment the average width of the particles is at least 900 nm. In one embodiment the average width of the particles is at least 1000 nm. In one embodiment the average width of the particles is at least 1100 nm In one embodiment the average width of the particles is at least 1200 nm. In one embodiment the average width of the particles is at least 1500 nm. In one embodiment the average width of the particles is at least 2000 nm. In one embodiment the average width of the particles is from 1000 nm to 5000 nm. In one embodiment the average width of the particles is from 1000 nm to 4000 nm. In one embodiment the average width of the particles is from 1000 nm to 3000 nm. In one embodiment the average width of the particles is from 1000 nm to 2500 nm. In one embodiment the average width of the particles is from 1200 nm to 2500 nm. The silk fibroin fibre particles are also preferably of a defined length in order to create the required Pickering emulsion. Typically the silk fibroin fibre particles have an average length of less than 40 ^m. In one embodiment the silk fibroin fibre particles have an average length of less than 35 ^m. In one embodiment the silk fibroin fibre particles have an average length of less than 30 ^m. In one embodiment the silk fibroin fibre particles have an average length of less than 25 ^m. In one embodiment the silk fibroin fibre particles have an average length of less than 20 ^m. In one embodiment the silk fibroin fibre particles have an average length of less than 15 ^m. In one embodiment the silk fibroin fibre particles have an average length of less than 10 ^m. In one embodiment the silk fibroin fibre particles have an average length of less than 8 ^m. In one embodiment the silk fibroin fibre particles have an average length of less than 6 ^m. In one embodiment the silk fibroin fibre particles have an average length of less than 5 ^m. In one embodiment the average length is from 2 ^m to 40 ^m. In one embodiment the average length is from 2 ^m to 35 ^m. In one embodiment the average length is from 2 ^m to 30 ^m. In one embodiment the average length is from 2 ^m to 25 ^m. In one embodiment the average length is from 2 ^m to 20 ^m. In one embodiment the average length is from 2 ^m to 15 ^m. In one embodiment the average length is from 2 ^m to 10 ^m. In one embodiment the average length is from 3 ^m to 10 ^m. In one embodiment the average length is from 4 ^m to 10 ^m. In one embodiment the average length is from 4 ^m to 8 ^m. In order to provide a pickering emulsion with the desired properties it is desirable that all the silk fibroin fibre particles have the stated aspect ratio and average width as described above. Nevertheless as will be appreciated by a skilled worker in the field a working emulsion can be produced as long as a sufficient number or percentage of the particles meet this criteria. As such the applicants have typically found that an acceptable emulsion can be formed if at least 90 % of the particles (by number) have an aspect ratio of between 2.5 and 40 and wherein the average width of the particles is at least 800 nm. Formation of Silk Fibroin Fibre particles of the invention As discussed above the method of the present invention provides a method of producing silk fibroin fibre particles wherein at least 90% of the particles particles (by number) have an aspect ratio of between 2.5 and 40 and wherein the average width of the particles is at least 800 nm the method comprising (i) providing degummed and partially hydrolysed silk fibroin fibres by subjecting a silk starting material to alkaline hydrolysis (ii) cutting the degummed and partially hydrolysed silk fibroin fibres until the cut silk fibres will pass through a 2 mm grid; and (iii) dry milling the cut silk fibres to produce silk fibroin fibre particles wherein at least 90% of the particles have an aspect ratio of between 2.5 and 40 and wherein the average width of the particles is at least 800 nm. The degummed and partially hydrolysed silk fibroin fibres typically have an onset of thermal degradation below 275oC and above 260oC as observed by DSC measurement. In addition the degummed and partially hydrolysed silk fibroin fibres typically have a beta sheet content of at least 45% as measured by FTIR. The first step in the method of formation of the Silk fibroin fibre particles of the invention is the provision of degummed and partially hydrolysed silk fibroin fibres. The applicants have found that the provision of silk fibroin fibres that are partially hydrolysed (and thus of lower molecular weight) is important to ensure that the particles have the required degree of brittleness in order to ensure that the remaining steps of the process provide the desired particles. The level of hydrolysis of a silk fibroin fibre particle is typically determined by the conditions that have been used in the degumming process with more forcing conditions typically leading to a higher level of hydrolysis. Commercially available degummed silk fibres or fibres degummed using standard degumming process used in the textile industry do not have the sufficient hydrolysis during degumming and hence cannot be used for particle production with required size and morphology. Hence additional hydrolysis is required to get further hydrolysis and reduction of molecular weight to improve brittleness and thus enable subsequent steps of particle production. As such in order to provide silk fibroin fibre particles with the required level of hydrolysis it is typically necessary to treat either raw silk, degummed silk or a combination thereof to produce degummed and partially hydrolysed silk fibroin fibres. In one embodiment the step of providing degummed and partially hydrolysed silk fibroin fibres comprises heating a starting material selected from raw silk, degummed silk or a combination thereof in an alkali solution at a temperature of from 100oC to 135oC. In one embodiment the starting material is raw silk. In another embodiment the starting material is degummed silk. In yet an even further embodiment the starting material is a combination of raw silk and degummed silk. Examples of Silk material that may be used as starting materials in the present invention include the Shell of Green or stifled Cocoon after removing the pupae, reeled silk filament from silk reeling factory, degummed silk from spun silk industry, waste cut cocoon and reeling waste from the silk reeling sector, degummed silk waste from spun silk industry, and raw silk or degummed silk based silk fabric waste. The type of silk starting material can also vary widely. Examples include silk from B.mori (Mulberry), A.assama (Muga silk). S.C ricini (Eri silk) and A. Pernyi (Tasar). The amount of starting material present in the alkali solution may vary. In one embodiment the starting material is present in an amount of 10 to 100 g per L of alkali solution. In one embodiment the starting material is present in an amount 20 to 100 g per L of alkali solution. In yet another embodiment the starting material is present in an amount of in an amount of 40 to 100 g per L of alkali solution. As will be appreciated by a skilled addressee the standard industry method for the removal of sericin involves treatment of silk with alkali at elevated temperatures typically of between 90oC to 100oC for from 5 to 90 minutes. Unfortunately, the applicants have found that this will not produce silk fibroin fibres having the required level of hydrolysis on a consistent basis. As will also be appreciated the process is a combination of temperature, time and alkali concentration with all three variables interacting with each other. Thus, for example, the higher the temperature the shorter the time that is required in order to provide silk fibroin fibre particles of the required degree of hydrolysis. A skilled worker will typically modify one or more of these variables based on the equipment available and the desired timeline of the process step. Nevertheless as stated above the temperature is from 100oC to 135oC. It is found that whilst the process works at the ends of this range neither point is optimal. For example working at the top end of the range runs the risk of degrading or reducing the molecular weight of the silk fibre more than needed as the heating is conducted for too long whereas operating at the lower end of the range elongates the time required for the process to achieve the desired level of hydrolysis in the fibre. As such in one embodiment the temperature is from 105oC to 130oC. In yet an even further embodiment the temperature is from 110oC to 130oC. In yet an even further embodiment the temperature is from 115oC to 130oC. In yet an even further embodiment the temperature is from 120oC to 130oC. in one embodiment the temperature is about 125oC. As will be appreciated as the alkali solution is typically an aqueous solution and the temperatures discussed above exceed the boiling point of the solution the heating step is conducted in a sealed vessel. The vessel may be of any suitable type and a skilled worker in the field could easily choose a suitable vessel based on the production parameters they wish to use such as volume and the like. The heating is carried out for a time period that is sufficient to provide degummed and partially hydrolysed silk fibroin fibres having the required degree of hydrolysis. In general as discussed above selection of the time will depend upon the other variables used and the starting material used. This may involve some routine experimentation based on the starting material of choice but once determined will be relatively consistent. It is anticipated, however, that the heating will be carried out for from 10 minutes to 240 minutes. Once again it is anticipated that lower temperatures will require a longer heating period whereas higher temperatures will require a shorter heating period. In one embodiment the heating is carried out for from 15 minutes to 180 minutes. In one embodiment the heating is carried out for from 20 minutes to 150 minutes. In one embodiment the heating is carried out for from 25 minutes to 120 minutes. In one embodiment the heating is carried out for from 30 minutes to 90 minutes. In one embodiment the heating is carried out for from 45 minutes to 75 minutes. In one embodiment the heating is carried out for from 50 minutes to 70 minutes. In one embodiment the heating is carried out for from 55 minutes to 65 minutes. In one embodiment the heating is carried out for about 60 minutes. The alkali solution used may be any suitable alkali solution known in the art. Examples of alkali solutions that may be used include sodium carbonate, sodium bicarbonate, potassium carbonate, potassium bicarbonate, sodium hydroxide and potassium hydroxide. In general, however, it is found to be preferable if the alkali is a mild alkali such as sodium carbonate or sodium bicarbonate. In one embodiment the alkali is sodium carbonate. In one embodiment the alkali is sodium bicarbonate. It is particularly desirable that the alkali is sodium carbonate as this alkali is the alkali of choice for the degumming of silk in the commercial silk industry and so silk processors typically have ready amounts of sodium carbonate on hand and are also well versed in its use in relation to materials safety and handling. In choosing an alkali solution the solution is typically chosen so that the alkali solution has a pH of greater than 9.0. In one embodiment the alkali solution has a pH of greater than 10.0. In one embodiment the alkali solution has a pH of greater than 11.0. In one embodiment the alkali solution has a pH of from 9.00 to 12.00. In one embodiment the alkali solution has a pH of from 10.00 to 12.00. In one embodiment the alkali solution has a pH of from 11.00 to 12.00. A skilled addressee in the field would readily be able to vary the pH of an alkali solution to fall within this range once a suitable alkali was chosen. In table 1 below we outline examples of different alkali at different concentrations. The amount of alkali can vary depending upon the specific alkali source chosen. In circumstances where the alkali is sodium carbonate the amount of alkali in the alkali solution is typically from 3g / L to 50g / L. In one embodiment the amount of alkali in the alkali solution is from 3g / L to 35g / L. In one embodiment the amount of alkali in the alkali solution is from 3g / L to 10g / L. In one embodiment the amount of alkali in the alkali solution is from 5g / L to 8g / L. In one embodiment the amount of alkali in the alkali solution is about 6g / L. It is typical that during the heating step the alkali solution is agitated. This can be carried out in a wide variety of ways depending upon the apparatus chose. Following completion of the heating step the alkali solution is typically cooled and the silk fibroin fibres isolated by filtration. Following heating the degummed and now partially hydrolysed silk fibroin fibres may then be washed to remove any residue from the heating step. As will be appreciated there are a number of potential washing steps that may be used. Washing steps that may be used either alone or in combination may include (a) a warm water washing step (b) a cold water washing step (c) a mild acid washing step to remove basic residue from the heating step. Any washing regime may incorporate one or more of these steps. If a warm water washing step is used the water is typically at a temperature of from 40oC to 80oC. In one embodiment the warm water wash is at a temperature of from 50oC to 70oC. In one embodiment the warm water wash is at a temperature of from 55oC to 65oC. If a cold water washing step is used the water is typically at a temperature of from 5oC to 20oC. In one embodiment the cold water wash is at a temperature of from 10oC to 20oC. In one embodiment the cold water wash is at a temperature of from 15oC to 20oC. If a mild acid washing step is used the wash is typically dilute acetic acid. The dilute acid wash is typically at a temperature is of from 10oC to 30oC. In one embodiment the acid wash is at a temperature of from 15oC to 25oC. In one embodiment the acid wash is at a temperature of about 20oC. If an acid wash is used the silk fibres are typically washed with the dilute acid until the pH of the washing liquor is 7 which indicates that all residual alkali has been removed. Once the degummed and partially hydrolysed silk fibroin fibres have been isolated and washed (if necessary) they are then dried prior to subjection to the remaining steps of the process. The drying may be carried out in any way well known in the art although it is typical that the drying is carried out using oven drying typically at a temperature of from 70oC to 80oC or air drying. Following drying the degummed and partially hydrolysed silk fibroin fibres typically have a beta sheet content of greater than 45% as measured by FTIR. In one embodiment the degummed and partially hydrolysed silk fibroin fibres have a beta sheet content of from 45% to 65% as measured by FTIR. In one embodiment the degummed and partially hydrolysed silk fibroin fibres have a beta sheet content of from 50% to 65% as measured by FTIR. In one embodiment the degummed and partially hydrolysed silk fibroin fibres have a beta sheet content of from 55% to 65% as measured by FTIR. Without wishing to be bound by theory it is felt that the level of beta sheet content is required so that the silk fibroin fibres are sufficiently brittle so that they are suitable for the milling step carried out later in the process. The degummed and partially hydrolysed silk fibroin fibres are then cut until the cut silk fibres will pass through a 2 mm grid. The cutting may be carried out in any way known in the art although typically cutting comprises passing the degummed and partially hydrolysed silk fibroin fibres through a fibre cutting machine or a cutter mill to form cut silk fibres of the desired dimension if required repeatedly before passing through the grid. A cutter mill is piece of equipment that consists of a series of uniformly spaced knives (typically 2 to 12 in number) which are attached to a horizontal rotor (rotating knives) which act against a series of stationary knives that are attached to the casing body of the mill. The bottom of the mill typically has a screen or grid attached which controls the residence time of the material inside the mill head as once the fibre particles are small enough to pass through the grid they fall out the bottom of the mill. As would be appreciated by a skilled worker in the field the size of particles produced by a cutter mill are typically determined by the rotor size, the gap between the sets of knives and the size of the screen or grid. A skilled worker will readily be able to modify these variables to produce cut silk of the required size. As will also be appreciated, however, given that the silk fibroin fibres are typically relatively thin there is the possibility that some of them may contact the screen in a lengthwise fashion and pass through the grid. The final step in the process is milling of the silk fibres to produce silk fibroin fibre particles wherein at least 90% of the particles have an aspect ratio of between 2.5 and 40 and wherein the average width of the particles is at least 800 nm. The milling may be carried out using any suitable milling apparatus such as a mechanical mill or a jet mill. It is typically found, however that it is preferable to use a jet mill rather than a mechanical mill due to the specific properties of a jet mill. As would be appreciated by a skilled worker a mechanical mill typically requires many moving parts with varying chambers for pulverization and classification. In contrast a jet micronizing mill relies mainly on a single chamber to pulverize and classify the material thoroughly. As would be appreciated by a person of skill in the art there are different designs of air jet mill and all are encompassed here which include both spiral air jet mills and fluidised bed air jet mills. Indeed jet mills involve no moving parts at all in the milling chamber, and instead rely on air, gas or steam jets to break up the particles into the desired particle sizes. In operation these high-velocity jets are used to drive the material around the grinding chamber, creating collisions between particles of the materials which breaks them into smaller particles. Once the desired particle size has been reached, the particles are then small enough to be able to escape out of the circular air flow and are funnelled out of a chamber and conveyed to a collection system. As there are no moving parts jet mills do not typically lead to heat generation which means that the silk fibres are not degraded during the milling process. Whilst each jet mill is somewhat different a skilled user of any specific apparatus will be able to readily modify the operating parameters such as feed in rate, air pressure and number of passes, to arrive at silk particles with the required dimensions. Nevertheless to assist the reader we note that the jet mill pressure is typically from 50-150 kg / cm2. In one embodiment the jet mill pressure is from 60-140 kg / cm2. In one embodiment the jet mill pressure is from 70-130 kg / cm2.. In one embodiment the jet mill pressure is from 80-120 kg / cm2. In addition it is possible to pass the material through the jet mill a number of times in order to produce the required particles. In one embodiment the cut silk fibres are passed through the jet mill once. In one embodiment the cut silk fibres are passed through the jet mill two times. In one embodiment the cut silk fibres are passed through the jet mill three times. Following jet milling the particles may be stored for later use. The particles are stable, dry and have a long shelf life and as such can be stored for a significant period of time. This makes the particles particularly suitable for industrial application as they are amenable to shipment and storage. Use of the particles of the invention to form an emulsion As stated previously the particles may be used as an emulsifier in the formation of a Pickering emulsion in which the particles act as an emulsifier. The applicants have found that the particles can be used in the formation of either an oil in water emulsion or a water in oil emulsion depending upon the way in which the emulsion is formed. As such the particles are inherently very flexible emulsifiers that can be used in the formulation of a wide variety of emulsions. Accordingly the present invention provides method of producing an emulsion the method comprising (a) combining silk fibroin fibre particles wherein at least 90% of the particles have an aspect ratio of between 2.5 and 40 and wherein the average width of the particles is at least 800 nm with a first component to form a mixture of the silk fibroin fibre particles in the first component; (b) adding a second component which is immiscible with the first component to the mixture; (c) subjecting the product of step (b) to high shear form an emulsion. In certain embodiments the emulsion is a stable emulsion as specified herein. As can be seen the first step in the process is combining silk fibroin fibre particles wherein at least 90% of the particles have an aspect ratio of between 2.5 and 40 and wherein the average width of the particles is at least 800 nm with a first component to form a well dispersed mixture of the silk fibroin fibre particles in the first component. The amount of silk fibroin fibre particles and first component used will depend upon the desired amounts of these two components in the final emulsion. An advantage of the particles of the present invention is that they can be reversibly dried and re-suspended in either a water phase or an oil phase. The amount of silk fibroin fibre particles in the final emulsion is typically from 0.1 to 10% w / w. and the amount of silk fibroin fibre particles mixed with the first component is selected to achieve this range in the final emulsion. In one embodiment the amount of silk fibroin fibre particles in the final emulsion is from 0.1 to 8% w / w. In one embodiment the amount of silk fibroin fibre particles in the final emulsion is from 0.1 to 6% w / w. In one embodiment the amount of silk fibroin fibre particles in the final emulsion is from 0.1 to 4% w / w. In one embodiment the amount of silk fibroin fibre particles in the final emulsion is from 0.1 to 3% w / w. In one embodiment the amount of silk fibroin fibre particles in the final emulsion is from 0.5 to 3% w / w. In one embodiment the amount of silk fibroin fibre particles in the final emulsion is from 1.0 to 3% w / w.. In one embodiment the amount of silk fibroin fibre particles in the final emulsion is from 1.5 to 2.5% w / w. Depending upon the nature of the emulsion to be formed the first component may be water or a water immiscible component. In one embodiment the first component is water. In one embodiment the first component is a water immiscible component. In embodiments where the first component is a water immiscible component the water-immiscible component may take any number of forms with the identity of the water-immiscible component typically being selected on the basis of the desired end- use application of emulsion, the cost, availability, and properties of the material. For example where the emulsion is intended to be used as a food additive it is advantageous to attempt to use a food-grade water-immiscible component. In principle, any water-immiscible component may be used with a water-immiscible liquid being preferred. In some embodiments, the water-immiscible component is an oil or a combination of oils. The oil may be an organic oil or a mineral oil. Examples of oils that may be used include C6-C18 hydrocarbons, triglycerides, natural oils, petroleum-based oils, and silicone oils. In some embodiments the oil is a natural oil selected from the group consisting of almond oil, apricot kernel oil, avocado oil, coconut oil, olive oil, safflower oil, sesame oil, soybean oil, sunflower oil, rapeseed oil, hemp oil, canola oil, cocoa butter, peanut oil, wheat germ oil, and other vegetable oils. The oil may also be sandalwood oil or an essential oil such as lavender oil, tea tree oil, frankincense oil, peppermint oil, eucalyptus oil, lemon oil, lemongrass oil, orange oil, rosemary oil, bergamot oil, and cedarwood oil. In some embodiments the water-immiscible component is a solvent or a combination of solvents. Examples of suitable solvents that may be used include carbon tetrachloride, chloroform, cyclohexane, 1,2-dichloroethane, dichloromethane, diethyl ether, dimethyl formamide, ethyl acetate, heptane, hexane, cyclohexane, methyl-tert-butyl ether, pentane, toluene, and 2,2,4-trimethylpentane or a combination thereof. In one embodiment the water-immiscible component is hexane or cyclohexane. The amount of first component in the final emulsion may vary widely from as low as 5%w / w up to 90%w / w. Nevertheless the amount of first component is typically from 10 to 70% w / w and the amount of first component mixed with the silk fibroin fibre particles is selected to achieve this range in the final emulsion. In one embodiment the amount of first component in the final emulsion is from 10 to 60% w / w. In one embodiment the amount of first component in the final emulsion is from 10 to 50% w / w. In one embodiment the amount of first component in the final emulsion is from 10 to 40% w / w. In one embodiment the amount of first component in the final emulsion is from 20 to 40% w / w. In one embodiment the amount of silk fibroin fibre particles in the final emulsion is from 25 to 35% w / w. In one embodiment the amount of first component in the final emulsion is from 28 to 32% w / w. In one embodiment the amount of first component in the final emulsion is about 30% w / w. Accordingly to get these amounts requires mixing from 0.1 to 10 parts by weight of the silk fibroin fibre particles with from 5 to 90 parts by weight of the first component. Following combination of the silk fibroin fibre particles with the first component the resulting mixture is typically gently agitated to ensure mixing of the silk fibroin fibre particles with the first component. Once the mixtures of silk fibroin fibre particles and first component has been produced the next step in the process is the addition of a second component which is immiscible with the first component. The identity of the second component will depend upon the identity of the first component. If the first component is water then the second component is a water immiscible component. If the first component is a water immiscible component then the second component is water. In one embodiment the first component is water. In one embodiment the first component is a water immiscible component. It is preferred that the first component is a water immiscible component and the second component is water. The amount of second component in the final emulsion may vary widely from as low as 10%w / w up to 95%w / w.. In one embodiment the amount of second component in the final emulsion is from 20% w / w to 90% w / w. In one embodiment the amount of second component in the final emulsion is from 30% w / w to 90 % w / w. In one embodiment the amount of second component in the final emulsion is from 30% w / w to 80% w / w. In one embodiment the amount of second component in the final emulsion is from 40% w / w to 80% w / w. In one embodiment the amount of second component in the final emulsion is from 50% w / w to 80% w / w. In one embodiment the amount of second component in the final emulsion is from 60% w / w to 80% w / w. In one embodiment the amount of second component in the final emulsion is from 65% w / w to 75% w / w. In one embodiment the amount of second component in the final emulsion is about 70% w / w. Emulsion Formation The mixture containing the first component, second component and silk fibroin fibre particles is then subjected to high shear to produce the desired emulsion. The applicants have found that the droplets in the final emulsion produced by the methods of the present invention typically are fine droplets which facilitate their use in many formulations. In one embodiment the method produces emulsions wherein 90 % of the droplets in the emulsion are less than 50 ^M. In another embodiment the method produces emulsions wherein 90 % of the droplets in the emulsion are less than 20 ^M. There are a number of known technologies that may be used to subject a liquid mixture to high shear. Examples of techniques for providing high shear that produce the necessary shear forces include high-pressure homogenisation, microfluidisation, hydrodynamic cavitation and ultrasonication. In one embodiment of the method of the invention in step (c), the mixture is subjected to high shear by sonication of the mixture comprising silk fibroin fibre particles, first component and second component. The sonication frequency used may vary greatly although it is typically in the range of from 20kHz to 200kHz. In one embodiment the sonication is carried out at a frequency of from 20kHz to 200kHz. In one embodiment the sonication is carried out at a frequency of from 20kHz to 150kHz. In one embodiment the sonication is carried out at a frequency of from 20kHz to 100kHz. In one embodiment the sonication is carried out at a frequency of from 20kHz to 40kHz. As will be appreciated by a skilled worker in the field sonication frequency is merely one variable in the sonication process. In general, the threshold energy density is a better way of determining the sonication step. The threshold energy density (E) may be defined as: E=(P X t) / V; Where P = Power input (W), t = time (s) and V (mL) is the processed volume. In certain embodiments, the sonication is carried out at an energy density of greater than 20 J / mL. In certain embodiments the sonicator is a 400W sonicator. The sonicator may be operated at various power levels. In certain embodiments the sonicator is operated at a power of from 50% to 100%. The sonication may be carried out for any period of time necessary to achieve the desired phase inversion. In one embodiment the sonication is carried out for from 1 second to 600 seconds. In one embodiment the sonication is carried out for from 5 seconds to 300 seconds. In one embodiment the sonication is carried out for from 10 seconds to 200 seconds. In one embodiment the sonication is carried out for from 15 seconds to 100 seconds. In one embodiment the sonication is carried out for from 20 second to 50 seconds. The sonicator may also be pulsed in order to maximise shear. The pulse may vary from 50 to 100. In one embodiment the pulse is 50. In one embodiment the pulse is 60. In one embodiment the pulse is 70. In one embodiment the pulse is 80. In one embodiment the pulse is 90. In one embodiment the pulse is 100. In one aspect the sonication is carried out in a continuous fashion whereby the mixture is passed through a sonication zone in order to produce the desired emulsion. In one embodiment the residence time in the sonication zone is 1 second to 600 seconds. In one embodiment the residence time in the sonication zone is 5 seconds to 300 seconds. In one embodiment the residence time in the sonication zone is 10 seconds to 200 seconds.. In one embodiment the residence time in the sonication zone is 15 seconds to 100 seconds. In one embodiment the residence time in the sonication zone is 20 second to 50 seconds. In one embodiment the sonication is carried out for about 5 seconds. In one embodiment the sonication is carried out for about 10 seconds. In one embodiment the sonication is carried out for about 15 seconds. In one embodiment the sonication is carried out for about 20 seconds. In one embodiment the sonication is carried out for about 25 seconds. In one embodiment the sonication is carried out for about 30 seconds. In one embodiment the sonication is carried out for about 35 seconds. In one embodiment the sonication is carried out for about 40 seconds. In one embodiment the sonication is carried out for about 45 seconds. In one embodiment the sonication is carried out for about 50 seconds. In one embodiment the sonication is carried out for about 55 seconds. In one embodiment the sonication is carried out for about 60 seconds. In one embodiment of the process of the invention in step (c) the mixture is subjected to high shear by the subjection of the mixture comprising silk fibroin fibre particles, first component and second component. to high-pressure homogenisation. In one embodiment the high-pressure homogenisation is carried out at a pressure of from 100 to 2000 bar. In one embodiment the high-pressure homogenisation is carried out at a pressure of from 500 to 1500 bar. In one embodiment the high-pressure homogenisation is carried out at a pressure of from 500 to 1000 bar In one embodiment the high-pressure homogenisation is carried out at a pressure of about 600 bar. In one embodiment the high-pressure homogenisation is carried out at a pressure of about 700 bar. In one embodiment the high-pressure homogenisation is carried out at a pressure of about 800 bar. In one embodiment the high-pressure homogenisation is carried out at a pressure of about 900 bar. In one embodiment the high-pressure homogenisation is carried out at a temperature of from 10°C to 90°C. In one embodiment the high-pressure homogenisation is carried out at a temperature of from 10°C to 70°C. In one embodiment the high-pressure homogenisation is carried out at a temperature of from 10°C to 50°C. In one embodiment the high-pressure homogenisation is carried out at a temperature of from 20°C to 50°C. In one embodiment the high-pressure homogenisation is carried out at a temperature of from 20°C to 30°C. In certain embodiments the high-pressure homogenisation involves multiple passes of the mixture through the homogeniser. In one embodiment the mixture is passed 6 times through the homogeniser. In one embodiment the mixture is passed 5 times through the homogeniser. In one embodiment the mixture is passed 4 times through the homogeniser. In one embodiment the mixture is passed 3 times through the homogeniser. In one embodiment the mixture is passed 2 times through the homogeniser. In one embodiment the is passed a single time through the homogeniser. The flow rate of the mixture through the high-pressure homogeniser will be dependent on a number of variables including the exact parameters and scale of the homogeniser equipment, however, the flow rate is typically in the range of from 10 to 28000 L / h. In one embodiment of the process of the invention in step (c) the mixture is subjected to high shear by the subjection of the mixture comprising silk fibroin fibre particles, first component and second component to shear mixing. The shear mixing may be carried out in a number of ways. The shear mixer typically has a rotation speed of from 1000 to 30000 rpm. In one embodiment the shear mixer has a rotation speed of from 5000 to 25000 rpm. In one embodiment the shear mixer has a rotation speed of from 10000 to 20000 rpm. In one embodiment the shear mixer has a rotation speed of from 12000 to 18000 rpm. In one embodiment the shear mixer has a rotation speed of from 14000 to 16000 rpm. In one embodiment the shear mixer has a rotation speed of about 15000 rpm. The shear mixing is typically carried out for from 5 minutes to 18015 minutes. In one embodiment the shear mixing is carried out for from 6 minutes to 14 minutes. In one embodiment the shear mixing is carried out for from 7 minutes to 13 minutes. In one embodiment the shear mixing is carried out for from 8 minutes to 12 minutes. In one embodiment the shear mixing is carried out for from 9 minutes to 11 minutes. In one embodiment the shear mixing is carried out for about 10 minutes. The end result of the method of the invention is an emulsion which may be used in a number of industrial formulations. Formulations of the Invention The present inventions also pertains to novel formulations that can be produced using the methods of the present invention. Accordingly the present invention provides a formulation in the form of an emulsion comprising (a) silk fibroin particles wherein at least 90% of the particles have an aspect ratio of between 2.5 and 40 and wherein the average width of the particles is at least 800 nm, (b) a water immiscible component, (c) water and (d) one or more active ingredients. The amount of silk fibroin fibre particles in the formulations of the invention is typically from 0.1 to 10% w / w. In one embodiment the amount of silk fibroin fibre particles in the formulations of the invention is from 0.1 to 8% w / w. In one embodiment the amount of silk fibroin fibre particles in the formulations of the invention is from 0.1 to 6% w / w. In one embodiment the amount of silk fibroin fibre particles in the formulations of the invention is from 0.1 to 4% w / w. In one embodiment the amount of silk fibroin fibre particles in the formulations of the invention is from 0.1 to 3% w / w. In one embodiment the amount of silk fibroin fibre particles in the formulations of the invention is from 0.5 to 3% w / w. In one embodiment the amount of silk fibroin fibre particles in the formulations of the invention is from 1.0 to 3% w / w.. In one embodiment the amount of silk fibroin fibre particles in the formulations of the invention is from 1.5 to 2.5% w / w. . In one embodiment the amount of silk fibroin fibre particles in the formulations of the invention is from 0.5 to 1.2% w / w. The formulations of the invention contain a water immiscible component. In some embodiments, the water-immiscible component is an oil or a combination of oils. The oil may be an organic oil or a mineral oil. Examples of oils that may be used include C6-C18 hydrocarbons, triglycerides, natural oils, petroleum-based oils, and silicone oils. In some embodiments the oil is a natural oil selected from the group consisting of almond oil, apricot kernel oil, avocado oil, coconut oil, olive oil, safflower oil, sesame oil, soybean oil, sunflower oil, rapeseed oil, hemp oil, canola oil, cocoa butter, peanut oil, wheat germ oil, and other vegetable oils. The oil may also be sandalwood oil or an essential oil such as lavender oil, tea tree oil, frankincense oil, peppermint oil, eucalyptus oil, lemon oil, lemongrass oil, orange oil, rosemary oil, bergamot oil, and cedarwood oil. In some embodiments the water-immiscible component is a solvent or a combination of solvents. Examples of suitable solvents that may be used include carbon tetrachloride, chloroform, cyclohexane, 1,2-dichloroethane, dichloromethane, diethyl ether, dimethyl formamide, ethyl acetate, heptane, hexane, cyclohexane, methyl-tert-butyl ether, pentane, toluene, and 2,2,4-trimethylpentane or a combination thereof. In one embodiment the water-immiscible component is hexane or cyclohexane. The amount of water immiscible component in the formulation may vary widely from as low as 5%w / w up to 90%w / w. Nevertheless, the amount of water immiscible component is typically from 10%w / w to 70% w / w. In one embodiment the amount of water immiscible component in the formulation is from 10%w / w to 60% w / w. In one embodiment the amount of water immiscible component in the formulation is from 10%w / w to 50% w / w. In one embodiment the amount of water immiscible component in the formulation is from 10%w / w to 40% w / w. In one embodiment the amount of water immiscible component in the formulation is from 20%w / w to 40% w / w. In one embodiment the amount of water immiscible component in the formulation is from 20%w / w to 35% w / w. In one embodiment the amount of water immiscible component in the formulation is from 28%w / w to 32% w / w. In one embodiment the amount of water immiscible component in the formulation is about 30% w / w. The amount of water in the formulation may vary widely from as low as 10%w / w up to 90%w / w. In one embodiment the amount of water in the formulation is from 20% w / w to 90% w / w. In one embodiment the amount of water in the formulation is from 30% w / w to 90 % w / w. In one embodiment the amount of water in the formulation is from 30% w / w to 80% w / w. In one embodiment the amount of water in the formulation is from 40% w / w to 80% w / w. In one embodiment the amount of water in the formulation is from 50% w / w to 80% w / w. In one embodiment the amount of water in the formulation is from 60% w / w to 80% w / w. In one embodiment the amount of water in the formulation is from 65% w / w to 75% w / w. In one embodiment the amount of water in the formulation is about 70% w / w. The formulations of the present invention also contain one or more active agents. The active agent may be any type of active agent and may include a cosmetic agent, a therapeutic agent or a nutraceutical agent. The active agent may be present in either the dispersed phase or the continuous phase. Examples of active agents include anaesthetics, antibiotics (eg, erythromycin and tetracycline), salicylic acid , anti-allergic agents, anti-fungal agents, anti-helminthic anti-irritants, anti-inflammatory agents, antimicrobial agents, antibacterial agents, analgesics, nitric oxide synthase inhibitors, insect repellents, skin cooling Agents, chelating agents, perfumes, vitamins, or any mixture thereof. The formulations of the invention may also contain a number of other additives such as preservatives, self-blackening agents, skin penetration enhancers, colorants (including dyes, lakes and pigments, which may be untreated or chemically surface treated to improve wettability or some other property), demulcents, emollients, wetting agents, lubricants, skin protectants, humectants, pH adjusters, preservatives, stabilizers, surfactants, thickeners, plasticizers, viscosity improvers, or any mixture thereof. The invention will now be illustrated by way of examples; however, the examples are not to be construed as being limitations thereto. Examples Materials: Silk materials of the following forms can be used for particle production including shell of Green or stifled Cocoon after removing the pupae, reeled Silk filament from silk reeling factory, degummed silk from spun silk industry, waste cut cocoon and reeling waste from the silk reeling sector, degummed silk waste of various types from spun silk industry and raw silk or degummed silk based silk fabric waste. A wide variety of silk types may be used including silk from B.mori (Mulberry), A.assama (Muga silk) and S.C ricini (Eri silk) and A. Pernyi (Tasar). B.mori was used because it is widely available compared to other type of silk. Silk materials were supplied by Automatic Reeling mill Ramgrah, India and Rudrasagar Silk Mill India. Chemicals for emulsion formation were purchased from New Directions Australia Pty Ltd and other chemicals were from Sigma Aldrich Australia and were used as received. Example 1: Degumming of Silk Silk cocoon shells were cut into pieces. In place of cocoon shells, raw silk filaments can also be used. The cocoon pieces / raw silk filaments were degummed to remove sericin gum using an Ahiba dyeing machine. For this 20 g silk and 300 mL alkaline solution (2g / L Sodium carbonate, using deionised water containing 0.5g / L of soap) were used in each beaker. Beakers are closed and airtight. Temperature was 98 deg C, time of treatment 30 min. the heating rate was 4 deg C per min and cooling rate was 2 deg C per min. The breakers were rotated slowly @5 rev / min. The degummed silk was removed once the temperature dropped to 40 deg C. The degummed silk fibres were rinsed with warm water and then with cold water till all residual alkali could be removed and pH of the washed liquor turned to 7. Degummed silk fibres were dried in fume hood or in an oven at 80 deg C till dry and kept for future use. Example 2: Alkali hydrolysis of silk Degummed silk either obtained from the procedure of example 1 or obtained commercially was hydrolysed using a similar procedure discussed above for degumming in example 1. No soap was used and Sodium Carbonate concentration was 3g / L -30g / L to hydrolyse silk to different degrees. Sample hydrolysed with 3g / L sodium carbonate is termed as M-3 and for 6g / L as M-6 and so on. Temperature was 125 deg C. Time of treatment was 1 hr. The heating rate, silk to liquor ratio and rotational speed of beakers were same as used in degumming. The hydrolysed silk was rinsed thoroughly with warm water followed by cold water. Silk was then washed in dilute solution of acetic acid to neutralise residual alkali and washed again till the pH of washed liquor was 7. Note: Degumming and hydrolysis can be performed simultaneously if instead of degummed silk raw silk is used for hydrolysis. Sample descriptions were as follows: M-3 : Mulberry silk from B.mori silkworm hydrolysed using 3g / L sodium carbonate. M-6: Mulberry silk from B.mori silkworm hydrolysed using 6g / L sodium carbonate. M-10: Mulberry silk from B.mori silkworm hydrolysed using 10g / L sodium carbonate. M-15: Mulberry silk from B.mori silkworm hydrolysed using 15g / L sodium carbonate. M-30: Mulberry silk from B.mori silkworm hydrolysed using 30g / L sodium carbonate. In a similar way “Mg” stands for Muga and “E” for Eri silk. % Mass loss due to hydrolysis of degummed silk is presented in Table 2 The general trend of weight loss is Muga<Eri<Mulberry silk. Detailed studies were conducted with Mulberry silk only and optimum hydrolysis conditions were determined using concentrations such as 6g / L and 15g / L which were not done for Muga and Eri silk. From weight loss results it is clear that there is substantial weight loss when alkali concentration was 10g / L and more than 50% when it was 15 g / L or more. this is not ideal for commercial applications. It was observed that when alkali concentration was high as 30g / L, the materials turns extremely brittle and fibres were fragmented and it was difficult to rinse without losing even remaining samples. Long fibres were retained for M-3 and M-6 samples and to a large extent for M-10 and rinsing was easy. SEM images obtained using the procedure outlined in example 9 below of Hydrolysed silk (M-3, M-6 and M-15) before cutter milling are shown in Figures 1 to 3. As can be seenM15 is demonstrating significant brittleness even before cutting. Example 3: MW analysis of alkaline treated fibres Sample were prepared using the procedure in example 2 to produce silk that had been alkali treated under various conditions. The samples tested were as follows: (1) dressed silk slivers, (2) Water only treated (0g / L Na2CO3, control) treated fibres, (3) 3g / L Na2CO3 treated fibres, (4) 6g / L Na2CO3 treated fibres, (5) 10g / L Na2CO3 treated fibres, (6) 15g / L Na2CO3 treated fibres, (7) 30g / L Na2CO3 treated fibres. The basic procedure for the MW analysis was as follows. Samples were dissolved for 3 hours in 9.3 M LiBr. Samples were loaded into 0.3 to 3 mL Slide-a-Lyzer dialysis cassettes (7 kDa MWCO) and dialysed overnight against dH2O. Protein concentration for each sample was determined using Pierce Rapid Gold BCA Assay kit. The procedure was modified to using commercially available silk fibroin to make the standard curve. Samples were diluted to an equal concentration to load onto the SDS- PAGE gel. MW distribution of the fibroin smear was visualised using Origin 2021b by plotting the pixel intensity of the lanes and comparing to the relative migration of the bands in the protein standard lane. This is shown in figure 7. As can be seen relative to the control the dressed fibres and 0 g / L treated fibres (lanes 1 and 2) show significant staining at higher molecular weights since the dark smear is even right down the lane. Lane 3 (3 g / L) shows higher molecular weight fractions have been hydrolysed, with the majority of the staining in the bottom half of the gel. Lane 4 (6 g / L) shows significant hydrolysis with practically now high MW fractions and smearing mostly below the 66 kDa band of the standards. Lanes 5-7 show very high levels of hydrolysis, with no detectable protein staining above 30 kDa. Example 4: Cutter milling A cutter mill (Pulverisette 19 from Fritsch) was used for chopping partially hydrolysed silk filaments from example 2. It has five “V” shaped blades fitted on a rotor rotating at 2888 rpm. These blades in combination with three fixed blades cut the fibres until they become fine enough to pass through a 2 mm grid. Some snippets longer than 2 mm could also pass through the grid due to the small diameter of silk fibres (10–20 μm). SEM images obtained using the procedure outlined in example 9 below of Hydrolysed silk (M-3, M-6 and M-15) after cutter milling are shown in Figure 4. Example 5: Air Jet Milling A Sturtevant laboratory air jet mill (2 inch dia) with grinding air pressure 100- 110 kg / cm2was used. Feed air pressure was about 30-40 Kg / cm2. Snippets prepared by the cutter mill as detailed in example 3 were fed manually or using a powder hopper (K-Tron, made in USA) at a feed rate of 50-200 g / h. Only one pass was used. Compressed air was pre dried before feeding to the milling chamber. Sample descriptors were as follows: M-3-AJM: Air jet milled particles of snippets of M-3 silk. M-6-AJM: Air jet milled particles of snippets of M-6 silk. M-10-AJM: Air jet milled particles of snippets of M-10 silk. M-15-AJM: Air jet milled particles of snippets of M-15 silk. M-30-AJM: Air jet milled particles of snippets of M-30 silk. In a similar way “Mg” stands for Muga and “E” for Eri silk. SEM images obtained using the procedure outlined in example 9 below of particles after jet milling is shown in figure 5. It was found that M-3-AJM samples even after milling remained highly fibrous with high aspect ratio. These are difficult to process through the jet mill and there is lack of flow like any powder materials and they remains fluffy after jet milling. They could be used for emulsion formation but dispersion was not easy. In contrast other samples prepared with higher alkali concentration could be handled like powder and could be dispersed during emulsification. Example 6: Emulsion formation- Oil In water Formulation Silk fibre particles after Air Jet Milling were used to form Oil-in-water (O / W) Pickering emulsion. The following mass fraction was used for formation of emulsion . • Silk: 0.25-2 part • Oil: Caprylic / Capric Triglyceride: (30-50) • Preservative (Phenoxyethanol): 1 part • Water: to make total to 100 Silk may be added either to oil phase or to water phase and stirred well using a lab stirrer (IKA RW 20) for 1-2 min at 300 rpm till silk fibre particles were completely dispersed without any clumps. Oil and water phases were then added mixed and preservative added to the mix. The water phase was buffered to pH5 using sodium acetate and acetic acid. To understand influence of pH in formation of emulsions, water phase with pH3 and pH7 were also used. To obtain pH7 buffered solution,Na2HPO4 and NaH2PO4 were used. Example 7: Sonication assisted emulsification The mixture from example 6 is sonicated using a 500 W sonicator. For a total mass of 10 g mixture in a 15 mL Eppendorf tube, 2 mm dia titanium sonicator horn was used to produce emulsion. 30 pulses were used. Sonicator power was kept at 100% and pulse 70%. For 50g and above mixture, 19 mm horn was used and power was kept at 50% and 40-60 pulses were used till complete homogenisation was noticed. Example 8: Emulsion by shear mixing The mixture obtained from example 6 was subjected to shear mixing. An IKA T 25 DIGITAL stator rotor with a rotor diameter of 18mm was used. RPM of 5000-20000 was tried for emulsion formation. Time was 2 min and material emulsified was 100 g. Few drops of RMOT 100 Antifoam was used as foam was produced during the homogenisation. An emulsion was formed but not as fine as the emulsion formed by sonication. Example 9: Emulsion by high pressure homogenisation The mixture of example 6 was subjected to high pressure homogenisation. A Planda Plus High Pressure homogenizer (GEA) with 1000 bar pressure. The material was processed three times. Prior to High pressure homogenisation, shear mixing was used at 5000 RPM as a pre-treatment. Under these conditions an emulsion formed but it was not as fine as the emulsion formed by sonication. Example 10: Scanning Electron microscopy The morphology of the silk fibres, snippets and jet milled particles was observed from the Scanning Electron Microscopy images taken by Zeiss Supra 55VP SEM. Samples were fixed on the stub using carbon tap and then gold-coated (thickness ~5 nm) with a Leica ACE600 sputter coater before imaging. Secondary electron detector mode was used to capture images at an accelerating voltage of 5 kV at different magnifications. Example 11: Optical microscopy Morphology was observed and length distribution of silk snippets was obtained with the help of an optical microscope (Olympus DP71, Japan). Magnifications of 10x and 20x were used by placing a drop of a suspension of very low concentration on a glass slide. For higher magnification, in the case of snippets the suspension was diluted in ethanol and then dried on a glass slide. Example 12: Determination of Fibre particle size distribution from microscopy The SEM images of dried particles ) particles were analysed with Image-Pro Plus software. Width of a fibre particle was measured in 3 different spots along the length of the particle and average determined to be used as the width of that particle. Length of that particle was also measured. Then Length to width ratio was determined as the aspect ratio of the particle. Distribution of length, width and aspect ratio was then obtained from measurements from approximately 200 particles taking number of images from different spots and marking about 10 particles at random from each image. Same approach was used to measure length distribution of snippets from the optical microscopy images. Measurements were made Here are my measurements from the 3, 6 and 10 g / L samples. The sample size is 200 fibres in each group but each fibre width was measured 3 x which is why the N number is 600 for width. The results are shown in tables 3 to 5 below. Table 3 3g / L Table 4 6g / L Table 5 10 g / L Example 13: Oil Droplet Size distribution of an emulsion A Malvern Instruments Mastersizer 3000, which is a laser diffraction based particle size analyser, was used to measure droplet size of oil in O / W emulsion. The Hydro MV unit was used for the controlled, automated wet dispersion of samples. The dispersion medium was DI water. Two drops of 5% Nonidet P-40 was used to facilitate dispersion .Refractive index of 1.450 and absorbance of 0.001 were used for oil phase as this is required to measure droplet size. After the emulsion drops were put into the MV unit, 30 second was allowed once obscuration was achieved followed by stirring at 1500 RPM for 2 min for stabilization.. 10 measurements were made and average readings were taken. The gradual change of readings over 10 measurement was also used to indicate the stability of the emulsion droplet. Figure 8 shows d.5 of volume based size distribution of droplets for emulsions prepared from different alkali hydrolysis and silk particle loading. Fig.9 shows the volume based Size distribution of emulsion droplet for M- 6-AJM based emulsions for different particle loading. Example 14: Silk particle Size distribution For silk particle size distribution, microscopy was used to determine relative particle sizes. Example 15: Differential Scanning calorimetry Calorimetry measurement of silk particles was carried out by DSC Q200 (TA Instruments, USA).8-10 mg of samples were placed in an aluminium pan, and a similar empty pan was taken as the reference. Heating was done from room temperature to 350°C at a rate of 100C / min in a nitrogen atmosphere. Example 16: Degree of Crystallinity based on FTIR The proportion of crystalline (β-sheet and turn) and amorphous (α- helix and random coil) motifs was measured in silk fibre and fibre particles using a LUMOS Fourier transform infrared (FTIR) microscope (Bruker, Billerica,MA, USA). Scans were taken in absorbance mode over the range of 4000 to 600 cm−1. A total of 5 measurements were taken for each sample. The amide I region (1705 to 1595 cm−1) was subjected to deconvolution and curve fitting using 12 known conformational positions. The relative peak area of each of these 12 deconvoluted peaks was used to determine the % content of side chain, β-sheet, random coil, α-helix and β- turn. The % peak area values were expressed as the mean ± standard deviation. The averaged scan of all samples was also plotted after deconvolution. Example 17: Emulsion Stability Stability of the emulsion was studied by observing any separation of oil when stored at room temperature and in an oven at 400C for a period up to 6 months. Digital photographs were taken at given time points. Chage in emulsion and serum layers was observed. Emulsion stability was also measured by centrifuging the emulsion at 4000 g force for 2 minutes at 200C. while centrifugal force squeezed out the water and increase the serum layer, the emulsion is considered stable if emulsion part is not broken and oil not separated from the Pickering emulsion capsules. An example of emulsion stability is shown in figure 13. Fig.13 shows no separation of oil after one month of storage. The serum layer seen is common in all pickering emulsion. There was no separation of oil and breakage of emulsion layer even after 6 months and till last observed. Storage temperature of 400C did not have impact on stability. To understand stability of emulsion when subjected to mechanical force that may apply during transport and application, emulsion was centrifuged at 4000g force for 2 minutes. While water is squeezed out and density of droplets increased there was no separation of oil as can be seen from the image. The SEM images of oil droplets show that there was no change in size indicating no breakage of emulsion. There was no evidence of coalescence of drops as may happens in unstable emulsions when there will be increase in size of drops and eventually separates out oil later. That did not happen. Example 18: Rheology of Emulsions The rheological measurements of emulsion samples were evaluated by Discovery HR-3 Rheometer (TA instruments) with a 40mm / 2° cone to parallel geometry and a Peltier plate with a fixed gap of 49μm. To determine storage modulus (G’) and loss modulus (G”), the frequency sweep of the suspensions was carried out at 25°c and 0.01≤ω≤100 rad / s with 0.1% strain. The shear thinning behaviour of an emulsion of the invention is shown in figure 10. Example 19 Confocal staining The oil droplet size and the arrangement of silk particles around the oil droplets was visualised using a Stellaris 5 Laser Scanning Confocal Microscope (Leica Microsystems, Wetzlar, Germany). Silk particle were stained overnight in DMSO containing 1 mg / mL of Fluorescein 5(6)-isothiocyanate (Sigma-Aldrich). Unbound stain was removed by centrifuging at 7,000 x g for 5 min, removing the supernatant and replacing with an equal volume of dH2O. A total of 3 wash steps was used. The oil phase was stained separately using Nile Red at a final concentration of 4 µg / mL (Sigma-Aldrich). The stained particles and oil were then combined to make emulsions as shown in example 6. Emulsions were then imaged using 2 laser channels for the different stains: the fluorescein stained particles were excited with 495 nm light while the Nile red was excited at 515 nm. Fluorescence images were collected at 525 nm (for fluorescein isothiocyanate) and 638 (for Nile red). Example 20: Skin care formulation A skin care formulation was created according to the following recipe. Phase A - Silk fibre particles : 1 part, Caprylic / Capric Triglyceride: 13 part, Isopropyl Myristate: 12 parts, Sandalwood oil: 0.5-2 parts. Phase B - Hyaluronic Acid: .1 part, Carbomer: 0.5 part, Sodium Chloride: 0.1 part, Water: remaining to make it 100 parts (when combined with phase A). Phase C -Phenoxyethanol 1 part. Mixing components in Phase A with overhead stirring at 500 RPM for 5 minutes to disperse silk in oil phase. Mix Phase B till carbomer and Hyaluronic acid are completely dissolved in water phase. Add Phase B to Phase A and emulsify using sonication. Add phase C and add Sodium carbonate solution dropwise to adjust pH is 5.5 and mix using the overhead stirrer. The subject headings used herein are included only for the ease of reference of the reader and should not be used to limit the subject matter found throughout the disclosure or the claims. The subject headings should not be used in construing the scope of the claims or the claim limitations. The description provided herein is in relation to several embodiments which may share common characteristics and features. It is to be understood that one or more features of one embodiment may be combinable with one or more features of the other embodiments. In addition, a single feature or combination of features of the embodiments may constitute additional embodiments. All methods described herein can be performed in any suitable order unless indicated otherwise herein or clearly contradicted by context. The use of any and all examples, or exemplary language (e.g., "such as") provided herein, is intended merely to better illuminate the example embodiments and does not pose a limitation on the scope of the claimed invention unless otherwise claimed. No language in the specification should be construed as indicating any non-claimed element as essential. It will be apparent to the person skilled in the art that while the invention has been described in some detail for the purposes of clarity and understanding, various modifications and alterations to the embodiments and methods described herein may be made without departing from the scope of the inventive concept disclosed in this specification. Those skilled in the art will appreciate that the invention described herein is susceptible to variations and modifications other than those specifically described. It is to be understood that the invention includes all such variations and modifications. The invention also includes all of the steps, features, compositions and compounds referred to, or indicated in this specification, individually or collectively, and any and all combinations of any two or more of the steps or features. Future patent applications may be filed in Australia or overseas on the basis of the present application, for example by claiming priority from the present application, by claiming a divisional status and / or by claiming a continuation status. It is to be understood that the following provisional claims are provided by way of example only and are not intended to limit the scope of what may be claimed in any such future application. Furthermore, the claims should not be considered to limit the understanding of (or exclude other understandings of) the invention inherent in the present disclosure. Features may be added to or omitted from the provisional claims at a later date, so as to further define the invention.

Claims

Claims:

1. Silk fibroin fibre particles wherein at least 90% of the particles have an aspect ratio of between 2.5 and 40 and wherein the average width of the particles is at least 800 nm.

2. Silk fibroin fibre particles according to claim 1 wherein 90% of the particles have an aspect ratio of between 7.5 and 35.

3. Silk fibroin fibre particles according to claim 1 or 2 wherein 90% of the particles have an aspect ratio of between 7.5 and 20. . Silk fibroin fibre particles according to any one of claimsto 3 wherein the average width of the particles is at least 1000 nm.

5. Silk fibroin fibre particles according to any one of claimsto 4 wherein the average width of the particles is at least 1200 nm. Silk fibroin fibre particles according to any one of claimsto 5 wherein the average length of the particles is less than 35 ^m.

7. A method of producing silk fibroin fibre particles wherein at least 90% of the particles have an aspect ratio of between 2.5 and 40 and wherein the average width of the particles is at least 800 nm, the method comprising: (i) providing degummed and partially hydrolysed silk fibroin fibres by subjecting a silk starting material to alkaline hydrolysis; (ii) cutting the degummed and partially hydrolysed silk fibroin fibres until the cut silk fibres will pass through a 2 mm grid; and (iii) dry milling the cut silk fibres to produce silk fibroin fibre particles, wherein 90% of the particles have an aspect ratio of between 2.5 and 40 and wherein the average width of the particles is at least 800 nm.

8. A method according to claim 7 wherein step (i) comprises heating a starting material selected from raw silk, degummed silk or a combination thereof in an alkali solution at a temperature of from 100oC to 135oC.

9. A method according to claim 8 wherein the heating is carried out for a period of from 10 to 240 minutes.

10. A method according to claim 8 or claim 9 wherein the heating is carried out for a period of from 30 to 90 minutes.

11. A method according to any one of claim 8 to 10 wherein the alkali solution is a sodium carbonate solution.

12. A method according to claim 11 wherein in step the alkali solution is at a concentration of from 3g / L to 50g / L.

13. A method according to any one of claims 11 to 12 wherein in step (i) the alkali solution is at a concentration of from 3g / L to 35g / L.

14. A method according to any one of claims 11 to 13 wherein in step (i) the alkali solution is at a concentration of from 3g / L to 10g / L.

15. A method according to any one of claims 11 to 14 wherein in step (i) the alkali solution is at a concentration of from 5g / L to 8g / L.

16. A method according any one of claims 8 to 15 wherein the starting material is degummed silk.

17. A method according to claim 16 wherein in step (i) the degummed silk is present in an amount of 10 to 100 g per L of alkali solution.

18. A method according to claim 16 wherein in step (i) the amount of degummed silk is present in an amount of 20 to 100 g per L of alkali solution.

19. A method according to claim 16 wherein in step (i) the amount of degummed silk is present in an amount of 40 to 100 g per L of alkali solution.

20. A method according to any one of claims 7 to 19 wherein the degummed and partially hydrolysed silk fibroin fibres have a beta sheet content in the range of from 45% to 75%.

21. A method according to any one of claims 7 to 20 wherein in step (ii) cutting the degummed and partially hydrolysed silk fibroin fibres comprises passing the fibres through a fibre cutting machine or a cutter mill to form cut silk fibres.

22. A method according to any one of claims 7 to 21 wherein in step (iii) milling of the cut silk fibres is carried out in a jet mill.

23. A method of producing an emulsion the method comprising: (a) combining silk fibroin fibre particles wherein at least 90% of the particles have an aspect ratio of between 2.5 and 40 and wherein the average width of the particles is at least 800 nm with a first component to form a mixture of the silk fibroin fibre particles in the first component; (b) adding a second component which is immiscible with the first component to the mixture; (c) subjecting the product of step (b) to high shear to form an emulsion.

24. A method according to claim 23 wherein the first component is a water immiscible component.

25. A method according to claim 23 wherein the water immiscible component is an oil or organic solvent.

26. A method according to any one of claims 23 to 25 wherein the second component is water.

27. A method according to any one of claims 23 to 26 wherein the emulsion comprises: (a) from 0.1 to 4% w / w of silk fibroin fibre particles; (b) from 10 to 80% w / w of first component; and (c) from 19.9 to 90 %w / w of the second component.

28. A method according to any one of claims 23 to 27 wherein step (c) comprises sonication.

29. A method according to claim 28 wherein the sonication is at a frequency of from 20kHz to 200kHz.

30. A method according to claim 28 or claim 29 wherein the sonication is carried out for a period of from 1 second to 600 seconds.

31. A method according to any one of claims 23 to 30 wherein 90% of the droplets in the emulsion are less than 50 ^M based on volume based size distribution.

32. A method according to any one of claims 23 to 31 wherein 90% of the droplets in the emulsion are less than 20 ^M based on volume based size distribution 33. A formulation in the form of an emulsion comprising (a) silk fibroin fibre particles wherein at least 90% of the particles have an aspect ratio of between 2.5 and 40 and wherein the average width of the particles is at least 800 nm, (b) a water immiscible component (c) water and (d) one or more active ingredients.

34. A formulation according to claim 33 wherein the formulation comprises from 0.1 to 4%w / w of silk fibroin fibre particles.

35. A formulation according to claim 33 or 34 wherein the formulation comprises from 0.5 to 1.2% w / w of silk fibroin fibre particles.

36. A formulation according to any one of claims 33 to 35 wherein the formulation comprises from 10 to 80%w / w of a water immiscible component.

37. A formulation according to any one of claims 33 to 36 wherein the formulation comprises from 19.9 to 40% w / w of a water immiscible component.

38. A formulation according to any one of claims 33 to 37 wherein the formulation comprises from 20 to 35% w / w of a water immiscible component.

39. A formulation according to any one of claims 33 to 38 wherein the formulation comprises from 35 to 90% w / w of water.

40. A formulation according to any one of claims 33 to 39 wherein the formulation comprises from 55 to 80% w / w of water.

41. A formulation according to any one of claims 33 to 40 wherein the formulation comprises from 65 to 75% w / w of water.

42. A formulation according to any one of claims 33 to 41 wherein 90% of the droplets in the emulsion are less than 50 ^M measured based on volume based size distribution.

43. A formulation according to any one of claims 33 to 42 wherein 90% of the droplets in the emulsion are less than 20 ^M measured based on volume based size distribution.

Citation Information

Patent Citations

  • Methods of producing and using silk microfibers

    US9925301B2

  • Silk fibroin-based microneedles and methods of making the same

    WO2012054582A2

  • Compositions comprising low molecular weight silk fibroin fragments and plasticizers

    WO2018081805A1