Wash-resistant textile hydrophobisation
The polymer, formed by radical polymerization with specific monomers and an organometallic complex, addresses the limitations of existing fluorine-free siloxane-based polymers by providing long-lasting and reactivatable hydrophobic coatings for textiles, ensuring excellent water-repellent performance even after repeated washing and stress.
Patent Information
- Application Number
- PCT/EP2024/060335
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-04-17
- Filing Date
- 2024-04-17
- Publication Date
- 2024-10-24
AI Technical Summary
Current fluorine-free siloxane-based polymers for textile hydrophobization lack sufficient washing permanence and reactivatability, failing to maintain excellent hydrophobic properties under mechanical and chemical stress.
A polymer is developed through radical polymerization of a mixture containing specific monomers, including an active monomer such as glycidyl methacrylate, which interacts with an organometallic complex to create a wash-resistant and thermally reactivatable hydrophobic coating for textiles.
The polymer achieves superior hydrophobic properties with high washing permanence and thermal reactivation capabilities, significantly surpassing existing fluorine-free alternatives by maintaining hydrophobicity even after multiple wash cycles and mechanical stress.
Smart Images

Figure EP2024060335_24102024_PF_FP_ABST
Abstract
Description
[0001]CO12401 / WI 1 Wash-resistant textile hydrophobic treatment The present invention relates to the field of textile hydrophobic treatment using fluorine-free siloxane copolymers, their production and use, as well as the textiles coated therewith. Long-lasting textile hydrophobic treatment is essential for many functional and outdoor textiles and is promoted by many outdoor brands. Important criteria here are a water-repellent effect and the durability of the coating. This so-called DWR (durable water resistance) finish is often based on per- and polyfluorinated alkyl compounds (PFAS), which have long been established in the field. The outstanding property profile of a fluorocarbon coating obtained in this way is expressed, for example, in high hydrophobicity, which even withstands washing of the textile (wash permanence).In addition, hydrophobicity that decreases over time can be reactivated, for example, by thermal treatment of the coated (finished) textiles. However, the high persistence of PFAS, especially their toxic transformation and degradation products, requires the use of fluorine-free alternatives. A number of alternative technologies are already commercially available and demonstrate good water-repellent properties. Commercially available silicones, for example, represent an excellent hydrophobic alternative. Textile hydrophobization using copolymers based on acrylate, acid, and siloxane acrylate monomers is known, for example, from CO12401 / WI 2 US 2022 / 0275124 A1. Although these polymers are well suited for hydrophobizing textiles, they do not exhibit sufficient wash permanence.A group of authors describes in Progress in Organic Coatings Volume 150, January 2021, 105968, an analogous use of copolymer dispersions based on acrylates and siloxane acrylate monomers as fluorocarbon substitutes for textile coatings. Although the silicones previously used in textile coatings, such as those described above, can provide excellent hydrophobicity to a textile, this effect is significantly reduced under mechanical and / or chemical stress (e.g., after use or washing of the textile). Reactivation of the hydrophobic effect similar to fluorocarbon has not yet been possible with siloxane-based textile coatings. It would therefore be desirable to provide fluorine-free siloxane-based polymers that enable excellent, reactivatable hydrophobicity of textiles while simultaneously exhibiting high wash durability.Surprisingly, it has been shown that the use of a special active monomer as an anchor group within the copolymer achieves excellent hydrophobicity of textiles. The interaction of these anchor groups with an organometallic complex added during textile hydrophobicization also makes the treated textile exceptionally wash-resistant: the textile coating according to the invention is easily reactivated, i.e., a decrease in hydrophobicity can be very easily maximized again through thermal activation. The ability to thermally renew the hydrophobic effect of siloxane-based coatings was unexpected given the fluorocarbon substitutes previously available in the field and was therefore particularly surprising.The need for fluorocarbon substitutes for textile coating with outstanding hydrophobic properties could thus surprisingly be met by means of a first aspect of the present invention, which is directed to a polymer obtainable by radical polymerization of a starting mixture comprising: (i) at least one monomer of the following chemical formula (I). [Formula I], wherein R1 is H or a hydrocarbon radical having 1-6 C atoms, preferably having 1-3 C atoms, more preferably having 1-2 C atoms; R2 is a hydrocarbon moiety having 1-10 C atoms, preferably 1-8 C atoms, more preferably 3-6 C atoms; and R3, R4 and R5 are the same or different and are each independently CH3, C2H5, n-propyl, isopropyl, OC2H5, on-propyl, O-isopropyl, O-Si(CH3)3, O-Si(C2H5)3, O-Si-(n-propyl)3 or O-Si-(iso-propyl)3, preferably CH3, O-Si(CH3)3, O-Si(C2H5)3, or O-Si-(iso-propyl)3, more preferably O-Si(CH3)3;and (ii) at least one active monomer selected from the group consisting of esters and amides of an unsaturated carboxylic acid, wherein the carboxylic acid preferably has up to 6 C atoms, more preferably up to 4 C atoms, in particular selected from esters and amides of acrylic acid or methacrylic acid, more preferably selected from N-methylolacrylamide (NMA), N-methylolmethacrylamide, glycidyl methacrylate and alkyl ethers or esters of N-methylolacrylamide (NMA), N-methylolmethacrylamide and glycidyl methacrylate and (iii) optionally one or more monomers of the following chemical formula (II); [Formula II], wherein CO12401 / WI 5 R6 is H or a hydrocarbon radical having 1-6 C atoms, preferably having 1-3 C atoms, more preferably having 1-2 C atoms; R7 is a hydrocarbon radical having 1-30 C atoms, preferably 1-20 C atoms, more preferably having 1-10 C atoms. By copolymerizing the active monomer (ii), the polymers according to the invention achieve hydrophobic properties that are superior to the prior art, which are expressed in particular by high wash durability and the possibility of thermal reactivation in the event of loss of hydrophobicity. In order to keep the number of pages of the description of the present invention too long, only the preferred embodiments of the individual features are listed below. However, the skilled reader should understand this type of disclosure to mean that any combination of different levels of preference is explicitly disclosed and explicitly desired.In a preferred embodiment, R1 is H or methyl, preferably methyl. R2 can be an alkyl moiety or an alkenyl moiety, preferably an alkyl moiety, more preferably an ethyl or n-propyl moiety, in particular an n-propyl moiety. R2 can also comprise at least one heteroatom selected from the group consisting of O, P, N and S, preferably O and N, more preferably O. R2 can also be an alkyl moiety or an alkenyl moiety interrupted by a CO12401 / WI6 ether group and / or an amine group. R2 is preferably unsubstituted or substituted by a substituent selected from the group consisting of methyl, ethyl, n-propyl, isopropyl, -OH, -SH, -NH2, =O, -F, -Cl, -Br and -I. At least one of R3, R4 and R5 is in particular selected from O-Si(CH3)3, O-Si(C2H5)3, O-Si-(n-propyl)3 or O-Si-(iso-propyl)3, preferably O-Si(CH3)3, O-Si(C2H5)3, or O-Si-(iso-propyl)3, more preferably O-Si(CH3)3.In a preferred embodiment, R3, R4 and R5 are identical. For example, the monomer of the chemical formula (I) is tris(trimethylsiloxy)silylpropyl methacrylate, or (bis(trimethylsiloxy)methyl)silylpropyl methacrylate, preferably tris(trimethylsiloxy)silylpropyl methacrylate (CLA30). Even if it is already clear from the general chemical formula (I) that these monomers in particular do not comprise any siloxane repeating units, it should be emphasized that the at least one monomer of the chemical formula (I) does not represent a polymeric structure, in particular not a polysiloxane. The mentioned esters of the active monomer can be, for example, the esters of C1-C10 alkylcarboxylic acids. The mentioned ethers of the active monomer can be, for example, the C1-C 10-Alkyl ether. It is preferred that the active monomer is an ester of unsaturated carboxylic acids, in particular an ester of unsaturated carboxylic acids having up to 6 C atoms, more preferably having up to 4 C atoms. The active monomer is particularly preferably an ester of acrylic acid or methacrylic acid, in particular methacrylic acid. CO12401 / WI 7 The active monomer is, for example, N-methylolacrylamide (NMA), N-methylolmethacrylamide, or glycidyl methacrylate. In a particularly preferred embodiment, the active monomer is glycidyl methacrylate. In a preferred embodiment, the starting mixture comprises precisely one monomer according to chemical formula (I) and / or precisely one active monomer (ii). More preferably, the starting mixture comprises precisely one monomer according to chemical formula (I) and / or precisely one active monomer (ii) and / or precisely one monomer according to chemical formula (II). In a preferred embodiment, R6 is H or methyl, more preferably methyl.R7 can be an alkyl or alkenyl radical, in particular an alkyl radical. R7 can also be linear or branched. For example, R7 is a linear alkyl radical having 1-20 C atoms, in particular having 1-10 C atoms. R7 can comprise at least one heteroatom selected from the group consisting of O, P, N, and S, preferably O and N, more preferably O. R7 is preferably unsubstituted or substituted by a substituent selected from the group consisting of -OH, -SH, -NH2, =O, -F, -Cl, -Br, and -I.In a preferred embodiment, R7 is selected from the group consisting of methyl, ethyl, propyl, allyl, butyl, butenyl, pentyl, pentenyl, hexyl, hexenyl, heptyl, heptenyl, octyl, CO12401 / WI 8 octenyl, nonyl, noneyl, decyl, decenyl, undecyl, undecenyl, Dodecyl, dodecenyl, tridecyl, tridecenyl, tetradecyl, tetradecenyl, pentadecyl, pentadecenyl, hexadecyl, hexadecenyl, heptadecyl, heptadecenyl, octadecyl and octadecenyl radical, preferably methyl, ethyl, propyl, Allyl, butyl, butenyl, pentyl, pentenyl, hexyl, Hexenyl, heptyl, heptenyl, octyl, octenyl, undecyl, undecenyl, octadecyl, and octadecenyl radicals, in particular methyl, ethyl, propyl, butyl, pentyl, hexyl, heptyl, octyl, undecyl, and octadecyl radicals. The monomer of chemical formula (II) is preferably an acrylic acid ester, for example methyl methacrylate, stearyl methacrylate, lauryl methacrylate, or capryl methacrylate, preferably methyl methacrylate.In the event that the starting mixture further comprises (iv) at least one auxiliary monomer, this is selected, for example, from the group consisting of styrene, (meth)acrylic acid, butyl (meth)acrylate, lauryl (meth)acrylate, stearyl (meth)acrylate. In a particular embodiment, the starting mixture comprises precisely one auxiliary monomer (iv). The starting mixture may additionally comprise at least one solvent (v), which is, for example, water. Preferably, the starting mixture further comprises an emulsifier system (vi), which comprises, for example, an ionic, a non-ionic component, and a superhydrophobe. The ionic component can be a cationic or anionic component. CO12401 / WI 9 Suitable cationic components are all those commonly used, such as quaternary alkylammonium salts.Suitable anionic components are all those commonly used, such as alkyl sulfates with a chain length of 8 to 18 carbon atoms, alkyl or alkylaryl ether sulfates with 8 to 18 carbon atoms in the hydrophobic moiety and up to 60 ethylene or propylene oxide units, alkyl or alkylarylsulfonates with 8 to 18 carbon atoms, esters and half-esters of sulfosuccinic acid with monohydric alcohols or alkylphenols, for example sodium dodecyl sulfate (SDS). The non-ionic component is selected, for example, from the group consisting of ethoxylated isotridecyl alcohol (IT8), IT20, and IT16, preferably IT8. A suitable superhydrophobe is selected, for example, from the group consisting of hexadecane, cetyl alcohol, pentanol, and octanol, preferably hexadecane. The emulsifier system can also comprise at least one protective colloid.Suitable protective colloids include, for example, partially saponified polyvinyl alcohols, polyvinylpyrrolidones, polyvinyl acetals, as well as starches and celluloses and their carboxymethyl, methyl, hydroxyethyl, and hydroxypropyl derivatives. Further usable emulsifiers and protective colloids can be found in "McCutchen's Detergents and Emulsifiers," North American Edition, 1979. The starting mixture may further comprise at least one reaction initiator (vii), which may be thermally or CO12401 / WI 10 redox-initiated. The reaction initiator is preferably at least partially water-soluble. A thermally initiated reaction initiator is known to decompose after thermal treatment into reactive components that initiate the polymerization reaction. As is known in the art, redox-initiated reaction initiators are combinations of oxidizing and reducing compounds used to initiate radical polymerizations.The reaction initiator is preferably a peroxide, which is preferably selected from the group consisting of sodium, potassium, and ammonium salts of peroxodisulfuric acid, hydrogen peroxide, di-t-butyl peroxide (DTBP), t-butyl hydroperoxide (TBHP), potassium peroxodiphosphate, t-butyl peroxopivalate, cumene hydroperoxide, isopropylbenzene monohydroperoxide, dilauroyl peroxide, dibenzoyl peroxide, dicumyl peroxide, preferably TBHP; or an azo initiator, such as azobis(isobutyronitrile) (AIBN) or 2,2'-azobis(2-methylpropionamidine) dihydrochloride (V-50), preferably V-50. It has been found preferable to use the reaction initiator in combination with a redox system. As redox reaction initiator combinations, the above-mentioned initiators are used in conjunction with a reducing agent.Suitable reducing agents are sulfites and bisulfites of monovalent cations, for example, sodium sulfite, and derivatives of sulfoxylic acid, such as zinc or alkali formaldehyde sulfoxylates, for example, sodium hydroxymethanesulfinate and ascorbic acid, especially sodium hydroxymethanesulfinate. CO12401 / WI 11 Redox reaction initiator combinations have the advantage that the polymerization reaction can be initiated at lower temperatures. In addition to reduced energy consumption, the monomers can also be protected from possible thermal decomposition. Additionally, small amounts of a metal compound soluble in the polymerization medium can be introduced, the metal component of which is redox-active under the polymerization conditions, such as those based on iron or vanadium, for example, ferric ammonium sulfate.Particularly preferred initiators are peroxodisulfate salts, especially ammonium peroxodisulfates, optionally in combination with reducing agents, especially sodium hydroxymethanesulfinate. When conducting the reaction using the miniemulsion polymerization technique, predominantly oil-soluble initiators can also be used, such as cumene hydroperoxide, isopropylbenzene monohydroperoxide, dibenzoyl peroxide, or azobisisobutyronitrile. Preferred reaction initiators for miniemulsion polymerizations are potassium persulfate, ammonium persulfate, azobisisobutyronitrile, and dibenzoyl peroxide. An overview of suitable initiators in addition to those described above can be found in "Handbook of Free Radical Initiators," ET Denisov, TG Denisova, TS Pokidova, 2003, Wiley Verlag. In the polymer according to the invention, the amount of at least one monomer of the chemical formula (I) can be 40-99.9 wt.%, preferably 50-99.9 wt.%, more preferably 60-99.9 wt.-%, based on the total weight of the at least one monomer according to CO12401 / WI 12 formula (I), the at least one active monomer (ii), optionally the at least one monomer according to formula (II), and optionally the at least one auxiliary monomer (iv). In the polymer according to the invention, the amount of the at least one active monomer (ii) can be 0.1-15 wt.%, preferably 0.5-10 wt.%, more preferably 1-6 wt.%, based on the total weight of the at least one monomer according to formula (I), optionally the at least one monomer according to formula (II), the at least one active monomer (ii) and optionally the at least one auxiliary monomer (iv). In the polymer according to the invention, the amount of the at least one monomer of the chemical formula (II) can be 1-60 wt.%, preferably 3-50 wt.%, more preferably 5-40 wt.%, based on the total weight of the at least one monomer according to formula (I), the at least one monomer according to formula (II), the at least one active monomer (ii) and optionally.of the at least one auxiliary monomer (iv). In the polymer according to the invention, the amount of the at least one auxiliary monomer (iv) can be 1-30 wt. %, preferably 5-25 wt. %, more preferably 10-20 wt. %, based on the total weight of the at least one monomer of the formula (I), optionally of the at least one monomer of the formula (II), of the at least one active monomer (ii) and of the at least one auxiliary monomer (iv). In the polymer according to the invention, the amount of the at least one solvent (v) can be 40-90 wt. %, preferably 50-80 wt. %, based on the total amount of the starting mixture. CO12401 / WI 13 In the polymer according to the invention, the amount of the emulsifier system (vi) can be 0.3-2.5 wt. %, preferably 0.5-2 wt. %, based on the total amount of the starting mixture. In the polymer according to the invention, the amount of reaction initiator (vii) may be 0.1-5 wt.%, preferably 0.1-2 wt.%, based on the total amount of the starting mixture.As already explained, the polymer is obtainable by radical polymerization of a starting mixture. Radical polymerization within the meaning of the present invention can be described as a chain polymerization in which the two C atoms of the ethylenically unsaturated C2 unit of one monomer are each covalently bonded to a C atom of an ethylenically unsaturated C2 unit of any other monomer. The double bonds of these C2 units are converted into single bonds. This bonding reaction is initiated by reaction initiators that release radicals (INIT∙). The radicals bind to the ethylenically unsaturated C2 units (C=C) to form a primary radical (INIT-CC∙), which in turn undergoes chain polymerization with further ethylenically unsaturated C2 units. Ultimately, the backbone of the resulting copolymer is formed from the covalently bonded C2 units.Radical polymerization is carried out in particular in an aqueous medium. The starting mixture preferably has the properties typical for radical polymerization. The radical polymerization is preferably an emulsion polymerization, wherein the starting mixture is an emulsion, in particular a CO12401 / WI 14 miniemulsion polymerization, wherein the starting mixture is a miniemulsion. An emulsion polymerization within the meaning of the present invention can be described as a special process for the above-mentioned radical polymerization. Here, water-insoluble monomers are emulsified in water with the aid of an emulsifier system, the monomers being located within the micelles formed by the emulsifiers. Using water-soluble reaction initiators, the monomers are polymerized within the micelles to form so-called latex particles.A polymer dispersion is ultimately obtained from the emulsion used. Miniemulsion polymerization differs from emulsion polymerization in that a superhydrophobe can also be added to stabilize the monomer-containing micelles. Furthermore, the mixture is subjected to an intensive homogenization step, for example, by ultrasonic treatment (e.g., ultrasonic finger) and / or pressure treatment (e.g., high-pressure homogenizer). This allows the formation of significantly smaller and more monodisperse micelles. Ideally, only the monomers within a micelle polymerize independently of the other micelles. The result here, too, is a polymer dispersion, whereby the individual so-called latex particles are significantly smaller and more monodisperse compared to a polymer dispersion following emulsion polymerization. The micelles have, for example, an average diameter of 50–350 nm.The micelle size can be determined using colloid analysis methods known to those skilled in the art, such as dynamic light scattering (DLS). CO12401 / WI 15 In contrast to emulsion polymerization, in which the size of the polymer latex particles is essentially determined by kinetic processes and the stability of the micelles, miniemulsion polymerization is based on the monomer already being completely contained within micelles prior to polymerization and thus no longer needing to diffuse into the micelles during polymerization. In other words, the latex particles formed can be viewed as polymerized copies of the monomer-filled micelles present at the beginning. This means that the size of the latex particles is determined exclusively by the dispersion process and the stability of the monomer-filled micelles.As a result, this process has several advantages over traditional emulsion polymerizations: ^ Since the monomer does not have to be transported through the continuous, usually aqueous phase, it is possible to polymerize even completely water-insoluble monomers in miniemulsions. ^ The size of the latex particles usually corresponds to that of the previously formed monomer-filled micelles and can be adjusted quite precisely via the amount and type of emulsifier system used. ^ Each monomer-filled micelle is homogeneous in terms of its composition. Especially for copolymerizations, the monomer ratio in each micelle is the same and is not subject to diffusion differences between the monomers. ^ The amounts of emulsifier system used are lower because the miniemulsion is only kinetically, but not thermodynamically, stabilized.A particular advantage of the present invention is that the polymer according to the invention can be used directly (i.e., without prior CO12401 / WI 16 purification) for treating textiles. Textiles within the meaning of the present invention are understood to be textile substrates, i.e., substrates formed from fibers. The polymer according to the invention preferably comprises no acid monomer, in particular no carboxylic acid monomer, such as acrylic acid, no phosphoric acid monomer, and / or no sulfuric acid monomer. The present invention further provides a hydrophobizing composition comprising (a) the polymer according to the invention; (b) at least one organometallic complex; and (c) optionally at least one auxiliary agent. The hydrophobizing composition is, in particular, a hydrophobizing dispersion.An organometallic complex within the meaning of the present invention is a compound in which an organic radical or an organic compound is directly bonded to a metal atom. The hydrophobizing composition may further contain a diluent, such as water. In this case, the amount of polymer is preferably 0.1-30 wt. %, more preferably 0.5-10 wt. %, based on the total amount of the hydrophobizing composition comprising the CO12401 / WI 17 polymer according to the invention, the at least one organometallic complex, the optional at least one auxiliary substance, and the diluent. The amount of the organometallic complex may then be 0.01-2.0 wt. %, preferably 0.01-1.5 wt. %, more preferably 0.03-1.0 wt. %, based on the total amount of the hydrophobizing composition comprising the polymer according to the invention, the at least one organometallic complex, the optional at least one auxiliary substance, and the diluent.In a preferred embodiment, the organometallic complex is an amine, alcoholate, carboxylic or phosphoric acid salt or chelate, preferably an alcoholate or carboxylic acid salt, of a metal selected from the group consisting of Pb, Zn, Zr, Sb, Fe, Cd, Sn, Ti, Ba, Ca, Mn, V, Al or Co, preferably Zn, Zr, Ti and Al, more preferably Zr and Ti. The carboxylic acid salt is, for example, a naphthenate, octoate, hexoate, laurate, acetate, formate, citrate or lactate, preferably an acetate. Preferably, the organometallic complex is selected from the group consisting of zinc, tin and zirconium octoate; Aluminum alcoholate, such as Al-tri-sec.-butanolate, Al-di-sec.-butanolate mono-acetylacetonate, Al-mono-sec.-butanolate-di-acetylacetonate, Al-di-sec.-butanolate-monoacetoacetic acid ethyl ester, Al-mono-sec.-butanolate-di-acetoacetic acid ethyl ester, Al-di-sec.-butanolate- mono-acetate and Al-mono-sec.-butoxide diacetate; alkyl titanate; alkyl zirconate; zinc, tin, zirconium, ferric and cobalt naphthenate; zinc and zirconium formate; tin, zinc and zirconium acetate; dibutyltin dicaprylate, dilaurate, diacetate and maleate; dioctyltin diformate, dibenzoate and dicrotonate; alkanolamine titanate and zirconate; titanium phosphate; titanium acetylacetonate; butyl titanate; ethyl citrate zirconate; and trialkoxyvanadate, such as trimethoxyvanadate, tri-n-butoxyvanadate and CO12401 / WI 18 triheptoxyvanadate, preferably from butyl titanate, zirconium octoate and zirconium acetate. Due to the presence of, among other things, at least one organometallic complex, the textile substrates treated with the hydrophobic composition according to the invention exhibit superior properties compared to the prior art. The substrates treated in this way are not only characterized by outstanding, wash-permanent hydrophobicity, but can also be thermally reactivated.Should the hydrophobicity decrease (for example, due to mechanical and / or chemical stress on the textile substrate during use and / or washing), it can be maximized again by thermal treatment of the substrate. This thermal treatment is preferably carried out in an oven, by ironing, and / or by treatment in a commercially available tumble dryer. The coated textile can be exposed to an activation temperature in the range of 50-200°C, preferably 80-180°C, more preferably 120-180°C, with the activation time being in particular 1-30 minutes, preferably 1-15 minutes. A particular advantage of the present invention is that the polymer according to the invention can be used directly for the treatment of textile substrates, i.e., can be included in the hydrophobicizing composition without prior purification. Surprisingly, the hydrophobicizing effect is not reduced as a result.Since an additional purification step of the polymer is unnecessary, the economic efficiency of the hydrophobing approach according to the invention is significantly improved. CO12401 / WI 19 Suitable auxiliaries are, for example, surface-active substances, such as wetting agents or surfactants, dispersants, fragrances, dyes, solvents, antifoams, adhesion promoters, or release agents. The amount of the auxiliaries in the hydrophobing composition is preferably 0.1-10 wt. %, more preferably 0.5-5 wt. %, based on the total weight of the hydrophobing composition. The present invention further provides a redispersible polymer powder obtainable by drying the polymer according to the invention.To produce such polymer powders, for example, which are redispersible in water, the aqueous dispersions resulting from the radical polymerization of the starting mixture are preferably dried in a manner known to those skilled in the art, for example by the spray-drying process. Drying the polymer to powder form significantly reduces the volume of the product; thus, lower transport costs can be achieved. Furthermore, polymers dried in this way are particularly stable in storage and can be easily converted into a dispersion, i.e., redispersed, before use by mixing with a suitable solvent, such as water.The present invention further provides a process for hydrophobizing a textile substrate, comprising the following steps in the specified order: (A) providing the textile substrate; CO12401 / WI 20 (B) wetting the textile substrate with the hydrophobing composition according to the invention as described above; and (C) thermally treating the wetted textile substrate obtained after step (B). The textile substrate comprises, for example, at least one natural fiber or at least one synthetic fiber or a mixture thereof. Examples of such natural fibers are cotton, linen, hemp, wool, such as sheep's wool, alpaca, angora wool, cashmere, mohair, yak wool, or merino wool, silk, and mixtures thereof, preferably cotton. Examples of synthetic fibers are viscose, polyester, polyethylene terephthalate, polyamide, polyethylene, polypropylene, elastane, and mixtures thereof, preferably polyester and polyamide.In a particular embodiment, the textile comprises cotton and / or polyester and / or polyamide. Particular preference is given to a textile which is a blend of cotton and at least one synthetic fiber, such as a blend of cotton and polyester, or a textile made of polyester, polyamide, or a blend of polyamide and polyester. The wetting of the textile substrate with the hydrophobing composition in step (B) can be carried out in any manner suitable for the treatment of textiles, for example by dipping, brushing, pouring, spraying, rolling, printing, padding, or foam application. The wetting is, in particular, complete wetting. Complete wetting within the meaning of the invention means that 70-100% of the total surface of the textile is brought into contact with the CO12401 / WI 21 hydrophobing dispersion, preferably 80-100%, more preferably 90-100%.Preferably, the wetted textile substrate obtained after step (B) is dried for 1-5 hours, preferably for 2-4 hours, at 10-40 °C, in particular at 20-30 °C, or for 1-15 minutes, preferably for 1-5 minutes at 80-150 °C, in particular at 100-130 °C, before the thermal treatment in step (C). The thermal treatment in step (C) can be carried out for 1-60 minutes, preferably for 1-45 minutes, more preferably for 1-30 minutes, at 50-200 °C, preferably at 80-180 °C, more preferably at 100-180 °C. The present invention further provides a production process for the polymer according to the invention. In this case, the starting mixture described in detail above, comprising (i) at least one monomer of the following chemical formula (I). [Formula I], wherein R1 is H or a hydrocarbon radical having 1-6 C atoms, preferably having 1-3 C atoms, more preferably having 1-2 C atoms; CO12401 / WI 22 R2 is a hydrocarbon moiety having 1-10 C atoms, preferably 1-8 C atoms, more preferably 3-6 C atoms; and R3, R4 and R5 are the same or different and are each independently CH3, C2H5, n-propyl, iso-propyl, OC2H5, on-propyl, O-iso-propyl, O-Si(CH3)3, O-Si(C2H5)3, O-Si-(n-propyl)3 or O-Si-(iso-propyl)3, preferably CH3, O-Si(CH3)3, O-Si(C2H5)3, or O-Si-(iso-propyl)3, more preferably O-Si(CH3)3;and (ii) at least one active monomer selected from the group consisting of esters and amides of an unsaturated carboxylic acid, wherein the carboxylic acid preferably has up to 6 C atoms, more preferably up to 4 C atoms, in particular selected from esters and amides of acrylic acid or methacrylic acid, more preferably selected from N-methylolacrylamide (NMA), N-methylolmethacrylamide, glycidyl methacrylate and alkyl ethers or esters of N-methylolacrylamide (NMA), N-methylolmethacrylamide and glycidyl methacrylate. and (iii) optionally one or more monomers of the following chemical formula (II) CO12401 / WI 23; [Formula II], wherein R6 is H or a hydrocarbon radical having 1-6 C atoms, preferably 1-3 C atoms, more preferably 1-2 C atoms; R7 is a hydrocarbon radical having 1-30 C atoms, preferably 1-20 C atoms, more preferably 1-10 C atoms; radically polymerized, this preferably taking place in an aqueous medium. As already mentioned, the process is preferably an emulsion polymerization, in particular a miniemulsion polymerization. The process comprises in particular the following steps in the order given: (α) providing the starting mixture according to the invention, which further comprises water (v) and an emulsifier system (vi); (β) homogenizing the provided starting mixture, preferably by stirring, dispersing, treating with ultrasound and / or treating with pressure; (γ) adding at least one reaction initiator (vii), optionally in combination with a redox system as described above,to the homogenized reaction mixture at a temperature of 0-100 °C, preferably 5-80 °C, more preferably 30-80 °C, over a period of several hours, preferably in the range of 2-8 hours, more preferably 4-6 hours; (δ) reacting the reaction mixture obtained according to (γ) and admixed with initiator at a temperature of 30-60 °C, preferably 40-55 °C, over a period of several hours, preferably in the range of 2-8 hours, more preferably 4-6 hours; and (ε) cooling the reacted reaction mixture obtained according to (δ) to room temperature. The pH of the emulsifier system is, for example, from 2 to 9, preferably from 4 to 8; in a particularly preferred embodiment, from 4 to 6. The pH can be adjusted before the start of the reaction using hydrochloric acid, acetic acid, sodium hydroxide solution, or EDTA solution. The polymerization can be carried out discontinuously or continuously, with all or individual components of the reaction mixture being introduced,with partial initial charging and subsequent metering of individual components of the reaction mixture, or by the metering method without initial charging. All metering is preferably carried out in proportion to the consumption of the respective component. Batch polymerization is particularly preferred. CO12401 / WI 25 The homogenization in step (β) can be carried out until the resulting emulsion has a particle size in the range of 50-500 nm, preferably 100-350 nm, measured by colloid analysis methods known in the art, such as dynamic light scattering (DLS) or static light scattering (LLS). It can be particularly advantageous for the cooled reaction mixture obtained after (ε) to be purified or used without further purification. The present invention further provides a coated textile substrate obtainable by the hydrophobization process according to the invention,as detailed above. The textile substrate (coated textile) thus treated exhibits excellent, wash-permanent, hydrophobic properties. It was particularly surprising that the textile thus treated is thermally reactivatable. Thermal reactivatability means that a decreasing hydrophobicity of the textile – e.g., due to mechanical and / or chemical stress, such as during use or washing of the textile – can be increased, in particular maximized, by thermal treatment. This thermal treatment is preferably carried out in an oven, by ironing and / or by treatment in a commercially available tumble dryer. CO12401 / WI 26 The coated textile can be exposed to an activation temperature in the range of 50-200 °C, preferably 80-180 °C, more preferably 100-180 °C, with the activation duration being in particular 1-120 min, preferably 1-30 min.particularly preferably 1-15 min. All symbols of the above formulas have their meanings independently of one another. In all formulas, the silicon atom is tetravalent. Working examples The present invention and the associated surprising technical advantages are further illustrated by the following working examples. 1. Analysis methods used Particle size determination: The particle sizes are determined on a Zetasizer Nano-S particle size measuring device, Malvern, software version 8.01, using dynamic light scattering (Mie measurement method). For this purpose, dispersions are diluted with filtered and degassed water to 0.1 wt% to a maximum of 0.5 wt%. The stated values always refer to the value D(50). D(50) is to be understood as the volume-average particle diameter.in which 50% of all measured particles have a volume-average diameter smaller than the specified value D(50). The measurements are carried out at 25 °C with the following specified settings: Refractive index of water (Dispersant RI) at 1.330; Viscosity (cP) at 0.8872; Refractive index of the disperse phase (Material RI) at 1.55; Material absorption at 0.010; Duration Used at 50 s; Measurement Position at 0.85 mm. Evaluating the hydrophobicity of the treated textiles: The hydrophobicity of the treated textiles can be evaluated either by measuring the contact angle with water or by conducting the so-called spray test. Determination of the contact angle with water: The measurement is carried out using a DSA25E contact angle measuring device from Krüss.which is equipped with a curved sample table with a magnetic holder. The measurement is evaluated using the ADVANCE software from Krüss. After clamping the fabrics, the contact angle with water is determined several times by applying 0.2 µl of water using the automated double dosing unit, and the average value is determined. The higher the measured contact angle, the more hydrophobic the treated textile is towards water. Testing using a spray test according to AATCC Test Method No. 22-2005: The textiles are sprinkled with deionized water. The result, which results from comparing the sprinkled textile surface with the rating images in the method description, indicates approximately what percentage of the area remained unwetted. A spray test value of 100% means a completely unwetted textile. The higher the spray test value, the more hydrophobic the treated textile is.the more hydrophobic the treated textile is towards water. CO12401 / WI 28 2. Preparation of the silicone acrylate dispersions The preparation of inventive hydrophobing compositions (Examples 2-5) and of a comparative dispersion without inventive active monomer (ii) (Example 1) is described below. In addition, a further non-inventive comparative example is presented as Example 6, in which a textile hydrophobing agent is prepared based on amine-containing silicone oils customary in the art. Example 1: (Comparative example; not according to the invention) 0.02 g of SDS (sodium dodecyl sulfate) and 0.48 g of IT8 (ethoxylated isotridecanol) are dissolved in water at 40°C with stirring. 4.95 g of stearyl methacrylate, 19.8 g of WACKER CLA 30 (3-[tris(trimethylsilyloxy)silyl]propyl methacrylate) and 0.36 g of hexadecane are added and mixed homogeneously at 40°C, then dispersed for 15 minutes using an Ultraturrax. The pre-emulsion is then further emulsified for 15 minutes using an ultrasonic finger (10 Wh) while stirring until a miniemulsion with a particle size of approximately 300 nm is obtained. The resulting miniemulsion is then subjected to radical polymerization. For this purpose, 157 µl of acetic acid (diluted; 10 wt%), 140 µl of NaOH solution (2 wt%), and 30 µl of FAS (ferrous ammonium sulfate) 1 wt% are dissolved in water and 20 ml of water are placed in a 250 ml laboratory reactor. The previously prepared miniemulsion is then added and heated to 50°C while stirring. When the temperature is reached, 0.4 ml of a 10 wt% TBHP solution (tert-butyl hydroperoxide) and 0.4 ml of a 5 wt% aqueous sodium formaldehyde sulfoxylate solution are added over four hours. The course of the reaction is monitored and controlled based on the resulting solids content. For this purpose, a 1 ml aliquot is taken from the stirred vessel and precipitated in ethanol. The resulting solid is centrifuged and dried. The reaction is polymerized for a total of 5.5 h at 50 °C until complete conversion is achieved and then cooled to room temperature. The resulting dispersion is used as received. It should be noted that Example 1 is the hydrophobic dispersion described in the prior art (Organic Coatings Volume 150, January 2021, 105968). Example 2: (according to the invention) 0.02 g of SDS and 0.48 g of IT8 are dissolved in water (53 ml) at 40 °C with stirring. 16.8 g WACKER CLA 30, 0.63 g glycidyl methacrylate and 0.36 g of hexadecane are added and mixed homogeneously at 40°C, then dispersed for 15 minutes on an Ultraturrax. The pre-emulsion is then further emulsified for 15 minutes using an ultrasonic finger (10 wt%) while stirring until a mini-emulsion with a particle size of approximately 220 nm is obtained. The resulting mini-emulsion is then radically polymerized. For this purpose, 157 µl of acetic acid (diluted; 10 wt%), 140 µl of NaOH solution (2 wt%), and 30 µl of FAS (1 wt%) are dissolved in water and 20 ml of water are placed in a 250 ml laboratory reactor. The previously prepared mini-emulsion is then added and heated to 50°C while stirring. When the temperature is reached, 0.4 ml of a 10 wt% TBHP solution and 0.4 ml of a 5 wt% aqueous sodium formaldehyde sulfoxylate solution is added over four hours. The course of the reaction is monitored and controlled based on the resulting solids content. For this purpose, a 1 ml aliquot is taken from the stirred vessel and precipitated in ethanol. The resulting solid is centrifuged and dried. CO12401 / WI 30 The reaction is polymerized for a total of 5.5 h at 50 °C until complete conversion is achieved and then cooled to room temperature. The resulting dispersion is used as received. Example 3: (according to the invention) 0.02 g SDS and 0.48 g IT8 are dissolved in water (53 ml) at 40 °C with stirring. 2.17 g methyl methacrylate, 16.93 g WACKER CLA 30, 0.63 g glycidyl methacrylate, and 0.36 g of hexadecane are added and mixed homogeneously at 40°C, then dispersed for 15 minutes on an Ultraturrax. The pre-emulsion is then further emulsified for 15 minutes using an ultrasonic finger (10 wt%) while stirring until a mini-emulsion with a particle size of approximately 250 nm is obtained. The resulting mini-emulsion is then radically polymerized. For this purpose, 157 µl of acetic acid (diluted; 10 wt%), 140 µl of NaOH solution (2 wt%), and 30 µl of FAS (1 wt%) are dissolved in water and 20 ml of water are placed in a 250 ml laboratory reactor. The previously prepared mini-emulsion is then added and heated to 50°C while stirring. When the temperature is reached, 0.4 ml of a 10 wt% TBHP solution and 0.4 ml of a 5 wt% aqueous sodium formaldehyde sulfoxylate solution is added over four hours. The reaction is monitored and controlled based on the resulting solids content. For this purpose, a 1 ml aliquot is taken from the stirred vessel and precipitated in ethanol. The resulting solid is centrifuged and dried. The reaction is polymerized for a total of 5.5 h at 50 °C until complete conversion is achieved and then cooled to room temperature. The resulting dispersion is used as received. CO12401 / WI 31 Example 4: (according to the invention) 0.02 g SDS and 0.48 g IT8 are dissolved in water (53 ml) at 40 °C with stirring. 3.10 g methyl methacrylate, 13.0 g WACKER CLA 30, 0.63 g glycidyl methacrylate and 0.36 g of hexadecane are added and mixed homogeneously at 40°C, then dispersed for 15 minutes on an Ultraturrax. The pre-emulsion is then further emulsified for 15 minutes using an ultrasonic finger (10 wt%) while stirring until a mini-emulsion with a particle size of approximately 200 nm is obtained. The resulting mini-emulsion is then radically polymerized. For this purpose, 157 µl of acetic acid (diluted; 10 wt%), 140 µl of NaOH solution (2 wt%), and 30 µl of FAS (1 wt%) are dissolved in water and 20 ml of water are placed in a 250 ml laboratory reactor. The previously prepared mini-emulsion is then added and heated to 50°C while stirring. When the temperature is reached, 0.4 ml of a 10 wt% TBHP solution and 0.4 ml of a 5 wt% aqueous sodium formaldehyde sulfoxylate solution is added over four hours. The reaction is monitored and controlled based on the resulting solids content. For this purpose, a 1 ml aliquot is taken from the stirred vessel and precipitated in ethanol. The resulting solid is centrifuged and dried. The reaction is polymerized for a total of 5.5 h at 50 °C until complete conversion is achieved and then cooled to room temperature. The resulting dispersion is used as received. Example 5: (according to the invention) 0.02 g of SDS and 0.48 g of IT8 are dissolved in water (53 ml) at 40 °C with stirring. 4.03 g of methyl methacrylate, 9.24 g of WACKER CLA 30, 0.63 g of glycidyl methacrylate, and 0.36 g of hexadecane are added and mixed homogeneously at 40°C. Dispersed for 15 minutes on a CO12401 / WI 32 Ultraturrax. The pre-emulsion is then further emulsified for 15 minutes using an ultrasonic finger (10 w / w) while stirring until a mini-emulsion with a particle size of approximately 200 nm is obtained. The resulting mini-emulsion is then radically polymerized. For this purpose, 157 µl of acetic acid (diluted; 10 w / w%), 140 µl of NaOH solution (2 w / w%), and 30 µl of FAS (1 w / w%) are dissolved in water and 20 ml of water are placed in a 250 ml laboratory reactor. The previously prepared mini-emulsion is then added and heated to 50°C while stirring. When the temperature is reached, 0.4 ml of a 10 w / w% TBHP solution and 0.4 ml of a 5 wt% aqueous sodium formaldehyde sulfoxylate solution is added over four hours. The reaction is monitored and controlled based on the resulting solids content. For this purpose, a 1 ml aliquot is taken from the stirred vessel and precipitated in ethanol. The resulting solid is centrifuged and dried. The reaction is polymerized for a total of 5.5 h at 50 °C until complete conversion is achieved and then cooled to room temperature. The resulting dispersion is used as received. Example 6 (not according to the invention): 12.6 g of an organopolysiloxane with the functional groups - (CH2)3NH(CH2)2NH2 and a viscosity of 1000 mm, 2 / s at 20 °C and an amine number of 0.3 mequiv. / g, 2.2 g of a dimethylpolysiloxane with a viscosity of 5 mm / s at 25 °C, 2.2 g of MQ methylsilicone resin, and 3 g of ethylene glycol monohexyl ether are placed at room temperature and mixed. Then, 6 g of diethylene glycol monobutyl ether, 0.25 g of acetic acid, and 73.75 g of demineralized water are stirred in successively at room temperature. A slightly cloudy emulsion is obtained. CO12401 / WI 33 3. Preparation of the test specimens and determination of the hydrophobic properties: Preparation of the test specimens: In the working examples, the corresponding dispersions or emulsions for finishing textiles are diluted with water to an active content of 1 wt.%, partially mixed with 0.7 wt.% zirconium acetate solution (16 wt.%) (Examples 1b, 2b, 3, 4, 5, 6b) and then applied to the textile sample. When finishing via a padder, the corresponding dispersions or emulsions areEmulsions for finishing textiles diluted with water to an active content of 10 wt.%, partially mixed with 0.7 wt.% zirconium acetate solution (16 wt.%) (Examples 1b, 2b, 3, 4, 5, 6b) and then applied to a textile sample. The textile samples used are 20 cm x 20 cm pieces of an unfinished fabric with the following compositions: ^ Polyester (PES)-cotton (CO) twill (214 g / m2; 65 wt.% PES, 35 wt.% CO) ^ Polyester (128 g / m2) ^ Polyamide / TAFT (66 g / m2) The textile samples (= finishing) are treated as follows: The fabric is dipped into the hydrophobing composition ten times so that the entire CO12401 / WI 34 fabric piece is completely wetted.The fabric is then dried for 2 hours at room temperature and then conditioned for at least 72 hours in a climatic chamber at 23°C and 60% humidity to ensure it is sufficiently conditioned for determining its hydrophobicity using a spray test and contact angle measurement. Alternatively, the fabric can be coated using a padder at 3 bar roller pressure. The fabric is then dried for 2 minutes at 130°C in a stenter and then conditioned for at least 72 hours in a climatic chamber at 23°C and 60% humidity to ensure it is sufficiently conditioned for determining its hydrophobicity using a spray test and contact angle measurement. Spray test after finishing: A spray test is carried out for all treated textiles after finishing (including the conditioning described above) (result: "after finishing"). The textiles are then dried on the clothesline overnight in the climatic chamber.Testing wash permanence: To test wash permanence, the treated textiles are washed and spun for 40 minutes at 40°C with approximately 2 kg of fiber in a Miele PROFESSIONAL WS 5426 household washing machine using the easy-care wash program following the drying process described above. One capful of a 3+1 color detergent from the Spee Power Caps brand by Henkel is added as a detergent surfactant. The textiles are then dried and conditioned for at least 24 hours in a climate-controlled room at 23°C and 60% humidity. To remove the CO12401 / WI 35 wash crease, the test samples can optionally be ironed with a Tristar iron on the "Cotton / Linen" setting. The crease-free, washed samples are then tested again for hydrophobicity using the spray test method and by contact angle measurement (result: "after washing").Activation: The coated textiles can be activated in various ways, and reactivation can also occur after washing. Treatment can be carried out in a drying cabinet at 150-180°C for 5-15 minutes, in a stenter at 130-180°C for 1-5 minutes, in a standard household condenser tumble dryer at 90-120°C for 30-120 minutes, or by ironing at maximum heat. The samples activated in this way are retested for hydrophobicity using the spray test method and by contact angle measurement (result: "after washing and activation"). The "washing" and "activation" sequence is repeated several times and accompanied by hydrophobicity measurements, allowing conclusions to be drawn about the reactivatability of the hydrophobicity of the textiles treated according to the invention. 4. Results Table 1 shows the results of the spray tests on textile polyester-cotton twill samples which were treated with the hydrophobing compositions of Examples 1-6 CO12401 / WI 36.In some cases, zirconium acetate was added to the hydrophobic composition. Table 1: Spray test results of all examples on polyester-cotton twill. after 1st after 10th execution washing washing dispersion addition after 1st washing and and and No. Zr(OAc) example activation activation activation 1a 1 no 0% 0% 0% 0% 1b 1 yes 50% 0% 0% 0% 2a 2 no 0% 0% 0% 0% 2b 2 yes 100% <50% 90% 50% 3 3 yes 100% <50% 80% 50% 4 4 yes 100% <50% 90% 50% 5 5 yes 100% <50% 80 50% 6a 6 no 80% - 90% 0% 0% 6b 6 yes 100% 80% 80% 0% The results of Comparative Examples 1a and 1b, which represent the state of the art, clearly demonstrate that the absence of the active monomer (ii) according to the invention results in unsatisfactory hydrophobicity of the textile – even directly after finishing without washing. Furthermore, the textiles coated in this way do not exhibit any particular wash permanence.Surprisingly, only the polymers according to the invention containing the active monomer (ii)—and only in combination with the organometallic complex in the hydrophobicizing composition—lead to the desired effect, namely high hydrophobicity of the treated textiles (see Examples 2a and 2b), which is also reactivatable. CO12401 / WI 37 Examples 2b, 3, 4, and 5 clearly demonstrate that the interaction of the active monomer (ii) and the organometallic complex results in coated textiles with outstanding hydrophobicity. Even after mechanical and chemical stress during washing, the reduced, but still sufficient, hydrophobic properties can be maximized again by thermally activating the textile. The fact that this is possible without restriction even after the tenth wash cycle underscores the extraordinary wash permanence of the textiles coated with the hydrophobicizing composition according to the invention.Such properties could not be achieved even with the amine-containing silicone oils commonly used in the art (see Examples 6a and 6b). Table 2 summarizes the results obtained in a similar way for textile samples made of pure synthetic fibers. Table 2: Spray test results of working examples 2b and 3 on other textiles. after after 10. Finish after 1. Wash Working example Wash and and and Activation Activation Activation 2b on polyamide 100% 100% 100% 2b on polyester 100% 100% 100% 3 on polyester 100% 100% 100% The outstanding hydrophobicity of the textiles finished according to the invention and the possibility of reactivating the hydrophobicity after stress from washing are confirmed for these textile samples and the results from Table 1 are even exceeded CO12401 / WI 38.The hydrophobicity of the coating and its wash resistance due to the active monomer (ii) mean that the outstanding water-repellent effect is partially retained even after ten washes (see Examples 2b and 3). In addition to the spray test, the contact angles were also determined for the coated textile samples from Table 1 (see Table 3). Table 3: Results of the contact angle measurement for all examples on polyester-cotton twill. Design Dispersion Addition Contact angle Contact angle Example No.Zr(OAc) after washing after activation 1a 1 no 132.7° (±1.38)° 129.85° (±1.75)° 1b 1 yes 126.47° (±3.10)° 131.72°(±2.85)° drop sinks drop sinks 2a 2 no on on 2b 2 yes 142°(±4.47)° 162(±2.76)° 3 3 yes 148°(±5.94)° 164°(±2.40)° 4 4 yes 149°(±3.47)° 161°(±1.63)° 5 5 yes 141°(±5.99)° 161°(±3.02)° 6a 6 no 117.60° (±2.29)° 121.87° (±1.69) 6b 6 ja 120.61° (±1.49)° 131.06° (±1.22) The textiles coated according to the invention (Examples 2-5) exhibit even greater hydrophilicity (indicated by higher contact angles) than the comparative examples, even after washing. Furthermore, the surprising effect becomes clear: only in the textiles coated according to the invention could the hydrophobicity reduced by washing be increased again by thermal activation. CO12401 / WI 39 The present invention is further characterized by the following points: 1.Polymer obtainable by radical polymerization of a starting mixture comprising: (i) at least one monomer of the following chemical formula (I). [Formula I], wherein R1 is H or a hydrocarbon radical having 1-6 C atoms, preferably having 1-3 C atoms, more preferably having 1-2 C atoms; R2 is a hydrocarbon moiety having 1-10 C atoms, preferably 1-8 C atoms, more preferably 3-6 C atoms; and R3, R4 and R5 are the same or different and are each independently CH3, C2H5, n-propyl, iso-propyl, OC2H5, on-propyl, O-iso-propyl, O-Si(CH3)3, O-Si(C2H5)3, O-Si-(n-propyl)3 or O-Si-(iso-propyl)3, preferably CH3, O-Si(CH3)3, O-Si(C2H5)3, or O-Si-(iso-propyl)3, more preferably O-Si(CH3)3;CO12401 / WI 40 and (ii) at least one active monomer selected from the group consisting of esters and amides of an unsaturated carboxylic acid, wherein the carboxylic acid preferably has up to 6 C atoms, more preferably up to 4 C atoms, in particular selected from esters and amides of acrylic acid or methacrylic acid, more preferably selected from N-methylolacrylamide (NMA), N-methylolmethacrylamide, glycidyl methacrylate and alkyl ethers or esters of N-methylolacrylamide (NMA), N-methylolmethacrylamide and glycidyl methacrylate. and (iii) optionally one or more monomers of the following chemical formula (II); [Formula II], wherein R6 is H or a hydrocarbon radical having 1-6 C atoms, preferably 1-3 C atoms, more preferably 1-2 C atoms; CO12401 / WI 41 R7 is a hydrocarbon radical having 1-30 C atoms, preferably 1-20 C atoms, more preferably 1-10 C atoms. 2. Polymer according to point 1, wherein R1 is H or methyl, preferably methyl. 3. Polymer according to one of the preceding points, wherein R2 is an alkyl unit or an alkenyl unit, preferably an alkyl unit, more preferably an ethyl or n-propyl unit, in particular an n-propyl unit. 4. Polymer according to any one of the preceding points, wherein R2 comprises at least one heteroatom selected from the group consisting of O, P, N, and S, preferably O and N, more preferably O. 5. Polymer according to any one of the preceding points, wherein R2 is an alkyl moiety or an alkenyl moiety interrupted by an ether group and / or an amine group. 6.Polymer according to one of the preceding points, wherein R2 is unsubstituted or substituted by a substituent selected from the group consisting of methyl, ethyl, n-propyl, isopropyl, -OH, -SH, -NH2, =O, -F, -Cl, -Br and -I. 7. Polymer according to one of the preceding points, wherein R3, R4 and R5 are the same. 8. Polymer according to one of the preceding points, wherein the monomer of the chemical formula (I) is tris(trimethylsiloxy)silylpropyl methacrylate, or (bis(trimethylsiloxy)methyl)silylpropyl methacrylate, preferably tris(trimethylsiloxy)silylpropyl methacrylate (CLA30). 9. Polymer according to one of the preceding points, wherein the esters of the active monomer are the esters of C1-C10 alkylcarboxylic acids. 10. Polymer according to one of the preceding points, wherein the ethers of the active monomer are C1-C. 10-alkyl ethers. 11. Polymer according to one of the preceding points, wherein the active monomer is N-methylolacrylamide (NMA), N-methylolmethacrylamide or glycidyl methacrylate, preferably glycidyl methacrylate. CO12401 / WI 42 12. Polymer according to one of the preceding points, wherein R6 is H or methyl, more preferably methyl. 13. Polymer according to point 1 or 2, wherein R7 is an alkyl or alkenyl radical, in particular an alkyl radical. 14. Polymer according to one of the preceding points, wherein R7 is linear or branched. 15. Polymer according to one of the preceding points, wherein R7 is a linear alkyl radical having 1-20 C atoms, in particular having 1-10 C atoms. 16. Polymer according to any one of the preceding points, wherein R7 comprises at least one heteroatom selected from the group consisting of O, P, N and S, preferably O and N, more preferably O. 17.A polymer according to any one of the preceding points, wherein R7 is unsubstituted or substituted with a substituent selected from the group consisting of -OH, -SH, -NH2, =O, -F, -Cl, -Br, and -I. 18.Polymerisat nach einem der vorhergehenden Punkte, wobei R7 bevorzugt ausgewählt ist aus der Gruppe, bestehend aus Methyl-, Ethyl-, Propyl-, Allyl-, Butyl-, Butenyl-, Pentyl-, Pentenyl-, Hexyl-, Hexenyl-, Heptyl-, Heptenyl-, Octyl, Octenyl, Nonyl-, Noneyl-, Decyl-, Decenyl-, Undecyl-, Undecenyl-, Dodecyl-, Dodecenyl-, Tridecyl-, Tridecenyl-, Tetradecyl-, Tetradecenyl-, Pentadecyl-, Pentadecenyl-, Hexadecyl-, Hexadecenyl-, Heptadecyl-, Heptadecenyl-, Octadecyl- und Octadecenyl-Rest, bevorzugt Methyl-, Ethyl-, Propyl-, Allyl-, Butyl-, Butenyl-, Pentyl-, Pentenyl-, Hexyl-, Hexenyl-, Heptyl-, Heptenyl-, Octyl, Octenyl, Undecyl-, Undecenyl-, Octadecyl- und Octadecenyl-Rest, insbesondere Methyl-, Ethyl-, Propyl-, Butyl-, Pentyl-, Hexyl-, Heptyl-, Octyl-, Undecyl- und Octadecyl-Rest. 19.Polymer according to one of the preceding points, wherein the monomer of chemical formula (II) is an acrylic acid ester, for example methyl methacrylate, stearyl methacrylate, lauryl methacrylate, or capryl methacrylate, preferably methyl methacrylate. 20. Polymer according to one of the preceding points, wherein the starting mixture is an emulsion, preferably a miniemulsion. 21. Polymer according to one of the preceding points, wherein the starting mixture comprises precisely one monomer according to chemical formula (I) and / or precisely one active monomer (ii). CO12401 / WI 43 22. Polymer according to one of the preceding points, wherein the radical polymerization is a radical polymerization in an aqueous medium. 23. Polymer according to one of the preceding points, wherein the starting mixture further comprises (iv) at least one auxiliary monomer selected from the group consisting of styrene, (meth)acrylic acid, butyl (meth)acrylate, lauryl (meth)acrylate, stearyl (meth)acrylate. 24.Polymer according to one of the preceding points, wherein the starting mixture comprises precisely one auxiliary monomer (iv). 25. Polymer according to one of the preceding points, wherein the starting mixture further comprises (v) at least one solvent, preferably water. 26. Polymer according to one of the preceding points, wherein the starting mixture further comprises (vi) an emulsifier system, which preferably comprises an ionic, a non-ionic component, and a superhydrophobe. 27. Polymer according to point 26, wherein the ionic component is a cationic or anionic component, wherein the cationic component is preferably a quaternary alkylammonium salt, or the anionic component is preferably sodium dodecyl sulfate (SDS). 28. Polymer according to point 26 or 27, wherein the non-ionic component is selected from the group consisting of ethoxylated isotridecyl alcohol IT8, IT20, and IT16, preferably IT8. 29.Polymer according to any one of points 26-28, wherein the superhydrophobic agent is selected from the group consisting of hexadecane, cetyl alcohol, pentanol, and octanol, preferably hexadecane. 30. Polymer according to any one of the preceding points, wherein the starting mixture further comprises (vii) at least one reaction initiator, which may be thermally or redox-initiated. 31. Polymer according to point 30, wherein the reaction initiator is a peroxide, which is preferably selected from the group consisting of sodium, potassium, and ammonium salts of peroxodisulfuric acid, hydrogen peroxide, di-t-butyl peroxide (DTBP), t-butyl hydroperoxide (TBHP), potassium peroxodiphosphate, t-butyl peroxopivalate, cumene hydroperoxide, isopropylbenzene monohydroperoxide, dilauroyl peroxide, dibenzoyl peroxide, and dicumyl peroxide, preferably TBHP; or an azo initiator, such as azobis(isobutyronitrile) (AIBN) or 2,2'-azobis(2-methylpropionamidine) dihydrochloride (V-50), preferably V-50. CO12401 / WI 44 32.A hydrophobizing composition comprising (a) the polymer according to any one of the preceding points; (b) at least one organometallic complex; and (c) optionally at least one auxiliary agent. 33. The hydrophobizing composition according to point 32, wherein the hydrophobizing composition further contains a diluent, preferably water, and the amount of the polymer is 0.1-30 wt.%, preferably 0.5-10 wt.%, based on the total weight of the hydrophobizing composition; and / or the amount of the organometallic complex is 0.01-2.0 wt.%, preferably 0.01-1.5 wt.%, more preferably 0.03-1.0 wt.%, based on the total weight of the hydrophobizing composition. 34.Hydrophobing composition according to item 32 or 33, wherein the organometallic complex is an amine, alcoholate, carboxylic or phosphoric acid salt or chelate, preferably an alcoholate or carboxylic acid salt, of a metal selected from the group consisting of Pb, Zn, Zr, Sb, Fe, Cd, Sn, Ti, Ba, Ca, Mn, V, Al or Co, preferably from Zn, Zr, Ti and Al, more preferably from Zr and Ti. 35. Hydrophobing composition according to item 34, wherein the carboxylic acid salt is a naphthenate, octoate, hexoate, laurate, acetate, formate, citrate or lactate, preferably an acetate. 36. Hydrophobing composition according to any one of items 32-35, wherein the organometallic complex is selected from the group consisting of zinc, tin and zirconium octoate; Aluminum alcoholate, such as Al-tri-sec.-butanolate, Al-di-sec.-butanolate-mono-acetyl-acetonate, Al-mono-sec.-butanolate-di-acetylacetonate, Al-di-sec.-butanolate-monoacetoacetic acid ethyl ester, Al-mono-sec.-butanolate-di-acetoacetic acid ethyl ester, Al-di-sec.-butoxide mono-acetate and Al mono-sec-butoxide di-acetate; alkyl titanate; alkyl zirconate; zinc, tin, zirconium, ferric and cobalt naphthenate; zinc and zirconium formate; tin, zinc and zirconium acetate; dibutyltin dicaprylate, dilaurate, diacetate and maleate; dioctyltin diformate, dibenzoate and dicrotonate; alkanolamine titanate and zirconate; titanium phosphate; titanium acetylacetonate; butyl titanate; ethyl citrate zirconate; and trialkoxyvanadate, such as trimethoxyvanadate, tri-n-butoxyvanadate and triheptoxyvanadate, preferably from butyl titanate, zirconium octoate and zirconium acetate. CO12401 / WI 45 37. Hydrophobic composition according to any one of items 32-36, wherein the polymer is present in the hydrophobic composition without prior purification. 38.Hydrophobicizing composition according to any one of points 32-37, wherein the auxiliary agent is selected from the group consisting of surface-active substances, such as crosslinking agents or surfactants, dispersants, fragrances, dyes, solvents, antifoams, adhesion promoters, or release agents; and / or wherein the amount of auxiliary agent in the hydrophobicizing composition is 0.1-10 wt. %, preferably 0.5-5 wt. %, based on the total weight of the hydrophobicizing composition. 39. Redispersible polymer powder obtainable by drying the polymer according to any one of points 1-31. 40. A process for hydrophobicizing a textile substrate, comprising the following steps in the given order: (A) providing the textile substrate; (B) wetting the textile substrate with the hydrophobicizing composition according to any one of points 32-38; and (C) thermally treating the wetted textile substrate obtained after step (B). 41.Method according to item 40, wherein the textile substrate comprises at least one natural fiber, at least one synthetic fiber, or a mixture thereof. 42. Method according to item 41, wherein the natural fiber is selected from the group consisting of cotton, linen, hemp, wool, such as sheep's wool, alpaca, angora, cashmere, mohair, yak, or merino wool, silk, and mixtures thereof, preferably cotton. 43. Method according to item 41 or 42, wherein the synthetic fiber is selected from the group consisting of viscose, polyester, polyethylene terephthalate, polyamide, polyethylene, polypropylene, elastane, and mixtures thereof, preferably polyester and polyamide. 44. Method according to any one of items 40-43, wherein the textile substrate comprises cotton, polyester, and / or polyamide. 45.The process according to any one of items 40-44, wherein the textile substrate is a blend of cotton and at least one synthetic fiber, such as a blend of cotton and polyester, or wherein the textile is a polyester, a polyamide, or a blend of polyamide and polyester. CO12401 / WI 46 46. The process according to any one of items 40-45, wherein the wetting of the textile substrate with the hydrophobing composition in step (B) is carried out in any manner suitable for the treatment of textiles, for example by dipping, brushing, pouring, spraying, rolling, printing, padding, or foam application. 47. The process according to any one of items 40-46, wherein the wetted textile substrate obtained after step (B) is dried for 1-5 hours, preferably for 2-4 hours, at 10-40°C, in particular at 20-30°C, or for 1-15 minutes, preferably for 1-5 minutes, at 80-150°C, in particular at 100-130°C, before the thermal treatment in step (C).A process according to any one of items 40-47, wherein the thermal treatment in step (C) is carried out for 1-60 min, preferably 1-45 min, more preferably 1-30 min, at 50-200°C, preferably 80-180°C, more preferably 100-180°C. 49. A process for producing the polymer according to any one of items 1-31, wherein a starting mixture comprising (i) at least one monomer of the following chemical formula (I). [Formula I], wherein R1 is H or a hydrocarbon radical having 1-6 C atoms, preferably having 1-3 C atoms, more preferably having 1-2 C atoms; R2 is a hydrocarbon moiety having 1-10 C atoms, preferably 1-8 C atoms, more preferably 3-6 C atoms; and R3, R4 and R5 are the same or different and are each independently CH3, C2H5, n-propyl, isopropyl, OC2H5, on-propyl, O-isopropyl, O-Si(CH3)3, O-Si(C2H5)3, O-Si-(n-propyl)3 or O-Si-(iso-propyl)3, preferably CH3, O-Si(CH3)3, O-Si(C2H5)3, or O-Si-(iso-propyl)3, more preferably O-Si(CH3)3;and (ii) at least one active monomer selected from the group consisting of esters and amides of an unsaturated carboxylic acid, wherein the carboxylic acid preferably has up to 6 C atoms, more preferably up to 4 C atoms, in particular selected from esters and amides of acrylic acid or methacrylic acid, more preferably selected from N-methylolacrylamide (NMA), N-methylolmethacrylamide, glycidyl methacrylate and alkyl ethers or esters of N-methylolacrylamide (NMA), N-methylolmethacrylamide and glycidyl methacrylate. and (iii) optionally one or more monomers of the following chemical formula (II); [Formula II], wherein R6 is H or a hydrocarbon radical having 1-6 C atoms, preferably 1-3 C atoms, more preferably 1-2 C atoms; R7 is a hydrocarbon radical having 1-30 C atoms, preferably 1-20 C atoms, more preferably 1-10 C atoms; CO12401 / WI 48 radically polymerized, this preferably taking place in an aqueous medium. 50. Process according to item 49, wherein the process is an emulsion polymerization, preferably a miniemulsion polymerization. 51. Process according to item 49 or 50, wherein the process comprises the following steps in the order given: (α) providing the starting mixture according to the invention as described in any one of items 1-31, which further comprises water (v) and an emulsifier system (vi); (ß) homogenizing the prepared starting mixture, preferably by stirring, dispersing, treating with ultrasound and / or treating with pressure;(γ) adding at least one reaction initiator (vii), optionally in combination with a redox system, to the homogenized reaction mixture at a temperature of 0-100°C, preferably 5-80°C, more preferably 30-80°C, over a period of several hours, preferably in the range of 2-8 hours, more preferably 4-6 hours; (δ) reacting the initiator-added reaction mixture obtained according to (γ) at a temperature of 30-60°C, preferably 40-55°C, over a period of several hours, preferably in the range of 2-8 hours, more preferably 4-6 hours; and (ε) cooling the reacted reaction mixture obtained according to (δ) to room temperature. 51. Coated textile substrate obtainable by a process according to any one of items 40-48.;
Claims
CO12401 / WI 49 Claims 1. Polymer obtainable by radical polymerization of a starting mixture which comprises: (i) at least one monomer of the following chemical formula (I) [Formula I], wherein R1 is H or a hydrocarbon radical having 1-6 C atoms; R2 is a hydrocarbon moiety having 1-10 C atoms; and R3, R4 and R5 are the same or different and each independently is CH3, C2H5, n-propyl, iso-propyl, OC2H5, on-propyl, O-iso-propyl, O-Si(CH3)3, O-Si(C2H5)3, O-Si-(n-propyl)3 or O-Si-(iso-propyl)3; and CO12401 / WI 50 (ii) at least one active monomer selected from the group consisting of esters and amides of an unsaturated carboxylic acid.
2. The polymer according to claim 1, wherein R1 is H or methyl; and / or wherein R2 is an alkyl moiety or an alkenyl moiety.
3. The polymer according to claim 1 or 2, wherein at least one of R3, R4, and R5 is selected from O-Si(CH3)3, O-Si(C2H5)3, O-Si-(n-propyl)3, or O-Si-(isopropyl)3.
4. The polymer according to any one of the preceding claims, which further comprises (iii) one or more monomers of the following chemical formula (II) [Formula II], wherein R6 is H or a hydrocarbon radical having 1-6 C atoms; R7 is a hydrocarbon radical having 1-30 C atoms. CO12401 / WI 51 5. Polymer according to one of the preceding claims, wherein the starting mixture further comprises (iv) at least one auxiliary monomer selected from the group consisting of styrene, methyl (meth)acrylate, (meth)acrylic acid and butyl (meth)acrylate; and / or wherein the starting mixture further comprises (v) at least one solvent; and / or wherein the starting mixture further comprises (vi) an emulsifier system; and / or wherein the starting mixture further comprises (vii) at least one reaction initiator.
6. Hydrophobizing composition comprising (a) the polymer according to one of the preceding claims; (b) at least one organometallic complex; and (c) optionally at least one auxiliary substance.
7. Hydrophobizing composition according to claim 6, wherein the hydrophobizing composition further comprises a diluent and the amount of polymer is 0.1-30 wt.-%, based on the total weight of the hydrophobing composition; and / or the amount of the organometallic complex is 0.01-2.0 wt.%, based on the total weight of the hydrophobing composition.
8. The hydrophobing composition according to claim 6 or 7, wherein the organometallic complex is an amine, alcoholate, carboxylic or phosphoric acid salt, or chelate of a metal selected from the group consisting of Pb, Zn, Zr, Sb, Fe, Cd, Sn, Ti, Ba, Ca, Mn, V, Al, or Co. CO12401 / WI 52 9. The hydrophobing composition according to any one of claims 6-8, wherein the polymer is present in the hydrophobing composition without prior purification.
10. The hydrophobing composition according to any one of claims 6-9, wherein the auxiliary agent is selected from the group consisting of surface-active substances, such as wetting agents or surfactants, dispersants, fragrances, dyes, solvents, antifoams, adhesion promoters, or release agents; and / or wherein the amount of auxiliary agent in the hydrophobing composition is 0.1-10 wt. %, based on the total weight of the hydrophobing composition.
11. A redispersible polymer powder obtainable by drying the polymer according to any one of claims 1-5. 12.A process for hydrophobizing a textile substrate, comprising the following steps in the specified order: (A) providing the textile substrate; (B) wetting the textile substrate with the hydrophobizing composition according to any one of claims 6-10; and (C) thermally treating the wetted textile substrate obtained after step (B).
13. The process for hydrophobizing according to claim 12, wherein the wetted textile substrate obtained after step (B) is dried for 1-5 hours before the thermal treatment in step (C). CO12401 / WI 53 wherein the thermal treatment in step (C) is carried out for 1-60 min at 50-200 °C.
14. A process for preparing the polymer according to any one of claims 1-5, wherein a starting mixture comprising (iv) at least one monomer of the following chemical formula (I) [Formula I], wherein R1 is H or a hydrocarbon radical having 1-6 C atoms; R2 is a hydrocarbon moiety having 1-10 C atoms; and R3, R4 and R5 are the same or different and each independently is CH3, C2H5, n-propyl, iso-propyl, OC2H5, on-propyl, O-iso-propyl, O-Si(CH3)3, O-Si(C2H5)3, O-Si-(n-propyl)3 or O-Si-(iso-propyl)3; and CO12401 / WI 54 (v) at least one active monomer selected from the group consisting of esters and amides of an unsaturated carboxylic acid and (vi) optionally one or more monomers of the following chemical formula (II) [Formula II], wherein R6 is H or a hydrocarbon radical having 1-6 C atoms; R7 is a hydrocarbon radical having 1-30 C atoms; is radically polymerized, preferably in an aqueous medium.
15. A coated textile substrate obtainable by a hydrophobicization process according to claim 12 or 13.
Citation Information
Patent Citations
Preparation of an aqueous dispersion of acrylate-siloxane copolymer particles
US20220275124A1
Acrylic ester electrostatic flocking binding agent and preparation method thereof
CN103214993A
Anticorrosion and antifouling type coating resin and method for preparing same
CN108727545A
Curable compositions for paints and painted products
JP4790140B2
Organosilicone copolymers
US20090186982A1
Cited By
Wash-resistant textile hydrophobisation
EP4698569A1