Process for aftertreatment of a panel

The method of embedding an electro-optical functional film between adhesive layers in an adhesive pre-composite and attaching it to the pane addresses the sensitivity to mechanical loads, ensuring high optical quality and reliability in composite pane production.

WO2024218224A1PCT designated stage expired Publication Date: 2024-10-24SAINT GOBAIN SEKURIT FRANCE
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
PCT/EP2024/060575
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-04-19
Filing Date
2024-04-18
Publication Date
2024-10-24

AI Technical Summary

Technical Problem

Integrating electro-optical functional films with a liquid crystal-based functional layer into composite pane production is challenging due to sensitivity to mechanical loads, leading to optical defects and quality issues during lamination and handling.

Method used

A method involving an adhesive pre-composite with an electro-optical functional film embedded between two optically transparent adhesive layers, which is applied to the pane to minimize mechanical stress and ensure high optical quality, using a stacking sequence of a pre-composite pane, a first adhesive layer, the electro-optical functional film, and a second adhesive layer, followed by lamination and attachment to the pane.

Benefits of technology

This method prevents uneven contact pressure and local mechanical stress on the electro-optical functional film, reducing the risk of optical defects and enabling reliable, high-quality production of composite panes with electro-optical functionality.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure EP2024060575_24102024_PF_FP_ABST
    Figure EP2024060575_24102024_PF_FP_ABST
Patent Text Reader

Abstract

The invention relates to a process for aftertreatment of a panel (100), in particular laminate panel, which comprises the steps of: a) providing an adhesive prelaminate (1) comprising in the following sequence: - a prelaminate panel (2), - a first adhesive layer (14) composed of an optically transparent adhesive, - an electrooptical functional film (5), - a second adhesive layer (15) composed of an optically transparent adhesive, b) providing the panel (100), in particular laminate panel, c) securing the adhesive prelaminate (1) to a surface (104) of the panel (100) by bonding using the second adhesive layer (15), wherein production of the adhesive prelaminate (1) comprises the steps of: i) providing the prelaminate panel (2), ii) laminating a first adhesive film (3) composed of an optically transparent adhesive onto the prelaminate panel (2) to produce the first adhesive layer (14), iii) laminating the electrooptical functional film (5) onto the first adhesive layer (14), iv) laminating a second adhesive film (4) composed of an optically transparent adhesive onto the electrooptical functional film (5) to produce the second adhesive layer (15).
Need to check novelty before this filing date? Find Prior Art

Description

[0001] Method for reworking a pane

[0002] The present invention lies in the technical field of window manufacturing and relates to a method for post-processing a window, in which the window is provided with an electro-optical functional element in film form. The invention further extends to a window manufactured in particular by the method according to the invention, as well as its use.

[0003] Laminated windows generally consist of two individual panes, typically made of glass, firmly bonded together by a thermoplastic interlayer. Modern laminated windows, particularly windshields in motor vehicles, generally exhibit complex curvatures in horizontal and / or vertical directions in order to meet the specific aerodynamic requirements and design specifications of OEMs such as automobile manufacturers. They increasingly also include electrically controllable functional elements that display information for the driver and / or front passenger, serve as lighting, and / or can change the optical transparency of the window, for example, like a sun visor. In particular, the optical transparency of windows can be switched over large areas, for example in roof windows, rear side windows, or partition windows.

[0004] Electrically controllable functional elements are advantageously provided in the form of electro-optical functional films. Electro-optical functional films with a liquid crystal-based functional layer, in particular, represent an interesting option for implementing electro-optical switching functions in a composite pane in a simple, space-saving, cost-effective, and reliable manner. Further advantages include faster switching and reduced haze effects.

[0005] To date, electro-optical functional films with a liquid crystal-based functional layer have been difficult to integrate into conventional production processes for laminated glass. This poses a significant challenge for simple and cost-effective industrial series production of laminated glass. As practice has shown, functional films with a liquid crystal-based functional layer react very sensitively to mechanical stress of any kind, particularly uneven contact pressure or shear and tensile forces. Even the smallest local deviations in the mechanical stress during the lamination of the laminated glass and in the laminated laminated glass lead to the occurrence of local optical defects in the functional films, which can render the laminated glass optically unusable.

[0006] In the series production of curved laminated glazing, however, it is unavoidable that the individual panes of the laminated glazing do not fit perfectly. Rather, minor shape deviations within the usual dimensional tolerances always occur, leading to locally increased mechanical stresses during lamination. This is not critical for conventional laminated glazing, as the optical quality of the laminated glazing is not impaired. However, locally increased mechanical stresses are sufficient to create undesirable local optical defects (e.g., local discoloration, discoloration, or clouding) in functional films with a liquid crystal-based functional layer. Furthermore, local shape deviations or locally increased mechanical stresses can certainly be desired during the production of laminated glazing.

[0007] However, problems with a deterioration in the optical quality of electro-optical functional films with a liquid crystal-based functional layer due to local mechanical stress can also occur simply through handling and processing the electro-optical functional films. This is particularly true for robot-assisted handling of electro-optical functional films.

[0008] US 2008 / 316381 A1 discloses a pane with an adhered light adjustment film.

[0009] In contrast, the object of the present invention is to create a way to produce a pane with an electro-optical functional element in film form with high optical quality in industrial series production. In particular, this should be possible in a simple manner in existing production facilities with relatively minimal adaptations.

[0010] These and other objects are achieved according to the invention by a method for reworking a pane according to the independent patent claim. Advantageous embodiments of the invention are set out in the subclaims.

[0011] According to the invention, a method for post-processing a pane, preferably a laminated pane, in particular a laminated glass pane, is shown, by which the pane is provided with an electro-optical functional element in film form. The electro-optical functional element is not integrated into the laminated pane, but is a component of an add-on part that is prepared or manufactured in the form of an adhesive pre-laminate. The adhesive pre-laminate is bonded to a surface of the pane.

[0012] The electro-optical functional element is in film form and has a functional layer, preferably based on liquid crystals. Here and below, the electro-optical functional element in film form is referred to simply as an "electro-optical functional film." The optical transparency of the electro-optical functional film is electrically controllable.

[0013] The method according to the invention for reworking a pane, in particular a composite pane, comprises the following steps, which are carried out, for example, in the specified order according to the alphabetical designation:

[0014] Step a)

[0015] Providing an adhesive pre-composite, which is in the form of a stacking sequence and comprises in this order: a pre-composite pane (e.g. thin glass pane), a first adhesive layer made of an optically transparent adhesive, an electro-optical functional film, a second adhesive layer made of an optically transparent adhesive.

[0016] Step b)

[0017] Providing a pane, in particular a composite pane, which is to be subjected to post-processing.

[0018] Step c)

[0019] Attaching the adhesive pre-bond to a surface of the pane by bonding it with the second adhesive layer. For this purpose, the adhesive pre-bond is applied to the surface of the pane, with the second adhesive layer being applied to the surface of the pane.

[0020] For ease of reference, the pane used in the pre-composite process is referred to here and below as the "pre-composite pane." The pane subjected to post-processing within the scope of the invention is referred to as the "pane" or "composite pane." The pre-composite pane is different from the pane to be post-processed and can be customized.

[0021] For the purposes of this invention, the term "adhesive pre-bond" refers to a stack of different layers that are adhesively bonded together. The adhesive pre-bond is a prefabricated (one-piece or monolithic) attachment for attachment to a surface of the pane, i.e., the adhesive pre-bond is manufactured as a product prior to attachment to the pane.

[0022] According to the invention, the adhesive pre-composite is produced in the form of a laminate. Its production comprises the following steps, which are carried out, for example, in the specified order according to the Roman numeral numbering: i) providing the pre-composite pane, ii) laminating a first adhesive film made of an optically transparent adhesive to the pre-composite pane to produce the first adhesive layer, iii) laminating the electro-optical functional film to the first adhesive layer, iv) laminating a second adhesive film made of an optically transparent adhesive to the electro-optical functional film to produce the second adhesive layer.

[0023] In the above embodiment, the optically transparent adhesive is used in the form of adhesive films that can be easily laminated. Such adhesive films are commercially available from various manufacturers. The adhesive films form the adhesive layers in the pre-laminated assembly.

[0024] In one embodiment of the invention, the process steps for laminating the pre-composite are performed in the specified order. In one embodiment of the invention, the process steps for laminating the pre-composite are performed in a different order. In one embodiment of the invention, two or more process steps for laminating the pre-composite are performed simultaneously.

[0025] The term "lamination" in the context of the present invention describes the application of pressure and / or vacuum (lower than ambient pressure) and / or heating of the respective layer sequence to be produced. For example, lamination can be carried out by applying mechanical pressure and simultaneous evacuation. In one embodiment of the invention, the adhesive films are laminated by applying mechanical pressure and optionally simultaneous evacuation, whereby no temperature increase occurs.

[0026] In one embodiment of the invention, a polymeric cover film (protective film), which consists, for example, of polyethylene terephthalate (PET), is arranged on the second adhesive layer or adhesive film. Before performing step c), i.e., before attaching the adhesive pre-composite to the pane, the cover film is removed again, exposing the second adhesive layer and allowing the pre-composite to be bonded to the pane using the second adhesive layer.

[0027] In one embodiment of the invention, during the production of the adhesive pre-laminate in the form of a laminate, the amount of dust in the immediate vicinity of the pre-laminate is reduced. Various measures are known to those skilled in the art for this purpose, such as applying ionized compressed air to the room in which the lamination takes place or lamination in a clean room. Dust can impair the optical quality of the adhesive pre-laminate, so it is advantageous to reduce the amount of dust.

[0028] For laminating the adhesive pre-laminate, conventional methods for laminating composite panes can be used. Vacuum lamination is particularly well-known and common. This process involves lamination in a heatable and evacuatable chamber within, for example, approximately 60 minutes at a reduced pressure of 0.01 mbar to 800 mbar. Roller lamination involves pressing in a calender between at least one pair of rollers or one roller and a solid substrate. This is well known to those skilled in the art, so it need not be discussed in detail here.

[0029] The adhesive pre-laminate can be bonded to the pane using the second adhesive layer in any way as long as it is ensured that a solid connection is created between the pre-laminate and the pane.

[0030] In one embodiment of the invention, in step c), to attach the adhesive pre-composite to the pane, the adhesive pre-composite is subjected to pressure in the direction of the pane surface, so that the second adhesive layer made of an optically transparent adhesive is subjected to pressure. In one embodiment of the invention, in step c), to attach the adhesive pre-composite to the pane, the second adhesive layer made of an optically transparent adhesive is physically and / or chemically solidified (cured), in particular by exposure to heat and / or electromagnetic radiation, in particular UV radiation.

[0031] The present invention thus advantageously demonstrates a way to prevent uneven contact pressure on the electro-optical functional film. In particular, damage to the electro-optical functional film can be prevented even before it is attached to the pane by embedding the electro-optical functional film in an adhesive pre-laminate between two adhesive layers made of an optically transparent adhesive and additionally protecting it from local mechanical stress by the pre-laminate pane. When attaching the adhesive pre-laminate to the pane, local load peaks can also be avoided by the pre-laminate pane, so that no uneven compressive forces act on the electro-optical functional film. The risk of local defects in the electro-optical functional film is minimized.The pre-composite pane also enables simple and reliable automated handling of the pre-composite, for example, using a robot-assisted gripper (e.g., a suction lifter). These are major advantages of the present invention.

[0032] In one embodiment of the invention, the first adhesive layer made of an optically transparent adhesive and / or the second adhesive layer made of an optically transparent adhesive have a layer thickness in the range of 0.2 to 2 mm. Such layer thicknesses have proven advantageous for the adhesive pre-bond, ensuring sufficient adhesive function and, at the same time, good and reliable protection for the electro-optical functional film against local mechanical stress.

[0033] In one embodiment of the invention, the electro-optical functional film comprises a functional layer based on a liquid crystal. The invention can be used particularly advantageously with electro-optical functional films based on liquid crystals, since these are particularly susceptible to optical damage due to local compressive stress.

[0034] In one embodiment of the invention, after step c), the connecting parts of the electro-optical functional element are at least partially covered by an encapsulation. This measure can protect the connecting parts from damage, particularly during transport and installation of the pane. The encapsulation contains or consists of, for example, a thermoplastic elastomer (TPE) or polyurethane (PU).

[0035] The pane produced by the method according to the invention is usually used to separate an interior space from an external environment. The pane is preferably a composite pane. The composite pane comprises a first pane with an outer side and an inner side, and a second pane with an inner side and an outer side, which are firmly connected to one another by at least one thermoplastic intermediate layer. The first pane can also be referred to as the outer pane, and the second pane as the inner pane. The surfaces or sides of the two individual panes are referred to, from the outside inwards, as side I, side II, side III and side IV. When installed, the outer pane faces the external environment. Advantageously, the adhesive pre-composite is bonded to side IV, i.e. to the surface of the inner pane facing the interior space.

[0036] In one embodiment of the invention, the optically transparent adhesive of the two adhesive films is curable, meaning it can be irreversibly cured. Typically, it is a plastic that is cured into a polymer-crosslinked state. This significantly distinguishes the curable adhesive from a thermoplastic, which, while also optically transparent, can be reversibly softened by applying heat. In contrast, the curable adhesive can no longer be returned to a flowable state once it has cured.

[0037] In one embodiment of the invention, in step c), for attaching the pre-composite to the pane by adhesive bonding, the optically transparent adhesive of the second adhesive layer and, optionally, also of the first adhesive layer, is cured. In one embodiment, the curable, optically transparent adhesive is cured by heat, exposure to electromagnetic radiation, preferably UV radiation, and / or chemically. Curing preferably occurs by applying heat or increasing the temperature and / or UV radiation.

[0038] During the production of the adhesive pre-composite by lamination, at least no (irreversible) curing of the optically transparent adhesive of the second adhesive layer, by which the pre-composite is adhered to the pane, occurs. In one embodiment of the invention, during lamination of the adhesive pre-composite, the optically transparent adhesive of the first adhesive layer is cured, whereas the optically transparent adhesive of the second adhesive layer is not cured. In one embodiment of the invention, during lamination of the adhesive pre-composite, neither the optically transparent adhesive of the first adhesive layer nor the optically transparent adhesive of the second adhesive layer are cured.

[0039] The electro-optical functional film can, in principle, be designed in any desired manner. Examples of electrically switchable or controllable functional films include SPD (suspended particle device), liquid crystal-based functional films, in particular guest-host films, PDLC (polymer dispersed liquid crystal), electrochromic, or electroluminescent functional films, and are known per se to those skilled in the art. The electro-optical functional film can also be a polymeric electrically conductive layer, for example, containing at least one conjugated polymer or a polymer provided with conductive particles. The electro-optical functional film generally contains at least one carrier film with a functional layer.

[0040] The invention can be used particularly advantageously in electro-optical functional films with a functional layer made of a liquid crystalline material, which are commercially available, for example, under the term "light control films" (Light Control Film), for example from Dai Nippon Printing Co., Ltd., Japan, under the product name LCF005(EU).

[0041] The optically transparent adhesive can, in principle, be chosen freely. Optically transparent adhesives are particularly well-known under the acronym LOCA (liquid optically clear adhesive) and OCA (optical clear adhesive) in tape or film form. These are often used in touch-sensitive displays, for example, to firmly bond them to an LCD panel or to firmly bond plastic covers to the touch-sensitive displays. After application, the LOCA or OCA in film form is often cured using UV radiation. Optically transparent adhesives are freely available commercially from a variety of suppliers.

[0042] The optically transparent adhesive of the first adhesive layer and the optically transparent adhesive of the second adhesive layer can be the same or different from each other; preferably, they are the same. In one embodiment, the electro-optical functional film and the two adhesive films have the same dimensions when laminating the pre-laminate, i.e., they have the same area. However, they can also have different dimensions, in which case the adhesive pre-laminate is cut to size after lamination.

[0043] The optically transparent adhesive can, for example, contain or consist of polyurethane (PU), polyacrylate, polyacetate resin, casting resin, or a copolymer or mixture thereof. Advantageously, the optically transparent adhesive consists of a casting resin, in particular based on polyurethane, polyacrylate, or silicone. In one embodiment of the invention, the optically transparent adhesive is based on polyacrylate or polyurethane. These are common and proven materials for optically transparent adhesives that are readily available commercially, including in film form.

[0044] Each individual pane (i.e., pane or composite pane or pre-composite pane) preferably contains or consists of glass, particularly preferably flat glass, float glass, quartz glass, borosilicate glass, soda-lime glass, aluminosilicate glass, or clear plastics, preferably rigid clear plastics, in particular polyethylene, polypropylene, polycarbonate, polymethyl methacrylate, polystyrene, polyamide, polyester, polyvinyl chloride, and / or mixtures thereof. Particularly preferably, each pane contains or consists of glass, in particular soda-lime glass. Suitable glasses are known, for example, from EP 0 847 965 B1.

[0045] In one embodiment of the invention, the pre-laminated pane contains or consists of glass. In one embodiment of the invention, the pre-laminated pane has a maximum thickness of 0.5 mm (thin glass pane). This has the advantage that the pre-laminated pane is very thin while still providing sufficient and reliable protection for the electro-optical functional film. The pre-laminated pane also makes the pre-laminated pane easy to handle, for example, using a robot-assisted suction lifter.

[0046] In one embodiment of the invention, the pane, in particular a composite pane, contains or consists of glass. The thickness of each individual pane of the composite pane can vary widely and be adapted to the requirements of the individual case. Panes with standard thicknesses of 1.0 mm to 25 mm and more preferably 1.4 mm to 2.1 mm are used. The size of the panes can vary widely and depends on their use. The composite pane can have any three-dimensional shape and be planar or slightly or strongly curved in one or more directions of space. The layer(s) made of a thermoplastic material for connecting the individual panes preferably contain or consist of polyvinyl butyral (PVB), ethylene vinyl acetate (EVA), thermoplastic polyurethane (TPU) and / or polyethylene terephthalate (PET).The thermoplastic material is formed by one or more thermoplastic films arranged one above the other, wherein the thickness of a thermoplastic film is preferably from 0.25 mm to 1 mm, typically 0.38 mm or 0.76 mm.

[0047] The invention further extends to a pane, preferably a composite pane, which is produced in particular by the method according to the invention. The pane, in particular a composite pane, comprises an adhesive pre-composite bonded to a pane surface, wherein the adhesive pre-composite comprises, as a stacking sequence in the following order: a pre-composite pane, a first adhesive layer made of an optically transparent adhesive, an electro-optical functional film, a second adhesive layer made of an optically transparent adhesive, through which the

[0048] Pre-laminated is glued to the pane.

[0049] The above statements regarding the method according to the invention apply analogously to the pane according to the invention, in particular the composite pane. With regard to features of the pane according to the invention, reference is made to the statements regarding the method according to the invention. Features of optional embodiments of the method according to the invention correspond analogously to features of optional embodiments of the pane according to the invention.

[0050] Furthermore, the invention extends to the use of the pane according to the invention, in particular a composite pane, in buildings or in means of transport for land, air, or water traffic, in particular in motor vehicles, for example as a windshield, rear window, side windows, and / or roof window. According to the invention, the use of the composite pane in motor vehicles is preferred, particularly preferably as a windshield, side window, or roof window.

[0051] The various embodiments of the invention can be implemented individually or in any combination. In particular, the features mentioned above and explained below can be used not only in the specified combinations, but also in other combinations or on their own, without departing from the scope of the present invention.

[0052] The invention is explained in more detail below using exemplary embodiments, with reference to the accompanying figures. They show, in simplified form and not to scale:

[0053] Fig. 1A-1C Cross-sectional views of intermediate products for producing a pre-composite in a vacuum laminator,

[0054] Fig. 2A-2C Cross-sectional views of intermediate products for producing the pre-composite in a roll laminator,

[0055] Fig. 3 is a cross-sectional view illustrating the attachment of the pre-composite to a composite pane,

[0056] Fig. 4 is a flow chart illustrating the method according to the invention.

[0057] The method according to the invention is explained by way of example in Figures 1 to 3 using the post-processing of a composite pane designated overall by the reference number 100 (see Figure 3).

[0058] Consider first Figure 3, in which the composite pane 100 is shown on the right. The composite pane comprises a first pane 101 and a second pane 102, which are firmly connected to one another by a thermoplastic intermediate layer 103. The composite pane 100 can, for example, be installed in a building or motor vehicle and separates an interior space from an external environment. For example, the composite pane 100 is the windshield of a motor vehicle. The first pane 101 and the second pane 102 are each made of glass, preferably soda-lime glass, and are transparent to visible light. The thermoplastic used in the composite pane 100 is preferably made of polyvinyl butyral (PVB), ethylene-vinyl acetate (EVA), thermoplastic polyurethane (TPU) and / or polyethylene terephthalate (PET).

[0059] In the present exemplary embodiment, the first pane 101 is the outer pane and the second pane 102 is the inner pane. The outer surface of the first pane 101 faces the outside environment and is simultaneously the outer surface of the composite pane 100. The inner surface of the second pane 102 faces the building or vehicle interior and is simultaneously the inner surface of the composite pane 100. It is understood that the composite pane 100 can have any suitable geometric shape and / or curvature. As a windshield, the composite pane 100 typically has a convex curvature. The different surfaces of the two panes 101, 102 are usually referred to - from outside to inside - as Side I, Side II, Side III and Side IV.

[0060] In Figure 3, an adhesive pre-composite 1 is shown on the left side, which is attached, for example, to a surface 104, which is the inner surface of the second pane 102 (side IV) of the composite pane 100.

[0061] The production of the adhesive pre-composite 1 is explained below. Consider Figures 1A and 2A first. Figure 1A illustrates, using a cross-sectional view, the production of a first intermediate product for forming an adhesive pre-composite 1 in a vacuum laminator. Figure 1B illustrates the production of the same first intermediate product in a roller laminator. The adhesive pre-composite 1 is formed as a (layer) laminate in each case.

[0062] Accordingly, a pre-laminated pane 2 is first prepared. The pre-laminated pane 2 consists of glass, in particular soda-lime glass, and has a layer thickness of, for example, 0.5 mm. A first adhesive film 3 is laminated onto the pre-laminated pane 2. The first adhesive film 3 consists of an optically transparent adhesive, for example, based on polyacrylate or polyurethane. The thickness of the first adhesive film 3 is in the range of 0.2 to 2 mm and is, for example, 1 mm.

[0063] As illustrated in Figure 1A, the lamination can take place in a vacuum laminator 6. For this purpose, the pre-laminated sheet 2 and the first adhesive film 3 are introduced into a vacuum chamber 7, which can be evacuated. In the vacuum chamber 7 there are two horizontal laminating plates 8, 8', which can be positioned vertically towards one another so that intermediate layers are pressed together by applying pressure and, if necessary, heating. This is symbolically represented by arrows in Figure 1A. As illustrated in Figure 1A, the pre-laminated sheet 2 rests on a lower laminating plate 8', and the first adhesive film 3 is arranged on an upper laminating plate 8. By positioning the two laminating plates 8, 8', the pre-laminated sheet 2 and the first adhesive film 3 are pressed and laminated together, thereby producing a first intermediate product 11 of the pre-laminated sheet 1.For example, lamination takes place at a reduced pressure in the vacuum chamber 8 of 0.01 mbar to 800 mbar.

[0064] As illustrated in Figure 2A, the lamination can equally well be carried out in a roller laminator 9 between laminating rollers 10. For this purpose, the first adhesive film 3 is arranged on the pre-laminated sheet 2 and successively pressed by laminating rollers 10, whereby the first intermediate product 11 of the pre-laminated sheet 1 is produced. In the schematic representation in Figure 2A, only a single laminating roller 10 is shown, although it is understood that roller laminators typically have several laminating rollers. As a rule, pressing takes place in a calender between at least one pair of rollers. However, it is also possible for the pressing to take place between at least one laminating roller 10 and a solid base, which is shown schematically in Figure 2A.A relative movement is caused between the laminating roller(s) 10 and the layers, for example by the laminating rollers 10 rolling along the layers, as symbolically represented by an arrow in Figure 2A.

[0065] In one embodiment, the optically transparent adhesive of the first adhesive film 3 is not (irreversibly) cured during lamination. In an alternative embodiment, the optically transparent adhesive of the first adhesive film 3 is cured.

[0066] The further processing of the first intermediate product 11 of the adhesive pre-composite 1 is described below, whereby for the sake of simplicity only the steps carried out in each case are explained and otherwise reference is made to the above explanations regarding Figures 1A and 2A.

[0067] Reference is now made to Figures 1B and 2B, which in turn relate to the vacuum laminator 6 and the roller laminator 9. As illustrated in Figure 1B, the first intermediate product 11 obtained in Figure 1A is further processed. The (laminated) first intermediate product 11 is arranged on the lower laminating plate 8'. An electro-optical functional film 5 with a functional layer based on liquid crystals is arranged on the upper laminating plate 8. By advancing the two laminating plates 8, 8', the first intermediate product 11 and the electro-optical functional film 5 are pressed together, producing a second intermediate product 12 of the pre-composite 1. As illustrated in Figure 2B, the lamination can equally well be carried out in the roller laminator 9.For this purpose, the first intermediate product 11 is brought into position and the electro-optical functional film 5 is pressed between the laminating rollers 10 or between a laminating roller 10 and a solid base, whereby the second intermediate product 12 of the adhesive pre-composite 1 is produced.

[0068] Reference is now made to Figures 1C and 2C, which in turn relate to the vacuum laminator 6 and the roller laminator 9. As illustrated in Figure 1C, the second intermediate product 12 obtained in Figure 1B is further processed. The second intermediate product

[0069] 12 is arranged on the lower laminating plate 8'. A second adhesive film 4 is arranged on the upper laminating plate 8, which here is constructed, for example, analogously to the first adhesive film 3. On the second adhesive film 4, specifically on the side of the second adhesive film 4 facing away from the second intermediate product 12, there is a cover film 13 (protective film) made of polymeric material, e.g., polyethylene terephthalate. By advancing the two laminating plates 8, 8', the second intermediate product 12 and the combination of the second adhesive film 4 and the cover film

[0070] 13, whereby the adhesive pre-composite 1 is produced.

[0071] As illustrated in Figure 2C, the lamination can also be performed in the roller laminator 9. For this purpose, the second intermediate product 12 is positioned and pressed onto the second adhesive film 4 with the applied cover film 13, thereby producing the adhesive pre-composite 1.

[0072] During lamination, the layers of the pre-composite 1 are bonded together adhesively, which is possible because the adhesive films 3, 4 have adhesive properties. There is no (irreversible) curing of at least the second adhesive film 4, since this serves to adhere it to the composite pane 100.

[0073] Here, for example, the electro-optical functional film 5 and the two adhesive films 3, 4 have the same dimensions, i.e., they have the same surface area. This can be easily achieved by cutting them to the desired size before lamination. However, it is also possible to cut the laminated pre-composite 1 accordingly.

[0074] It is understood that during the lamination of the pre-composite 1, individual or multiple process steps can be carried out simultaneously and / or in a different order. Let us now look again at Figure 3. On the left side of Figure 3, the adhesive pre-composite 1 produced by the previously described process steps is shown. The pre-composite 1 comprises the pre-composite pane 2, a first adhesive layer 14 formed from the first adhesive film 3, a second adhesive layer 15 formed from the second adhesive film 4, the electro-optical functional film 5, and the cover film 13. The cover film 13 is optional and can also be omitted. It serves to protect the second adhesive layer 15. The electro-optical functional film 5 is embedded between the two adhesive layers 14, 15, such that the electro-optical functional film 5 is well protected from mechanical influences by the two adhesive layers 14, 15 and the pre-composite pane 2.

[0075] The composite pane 100 is shown on the right-hand side of Figure 3. In the present exemplary embodiment, the adhesive pre-composite 1 is arranged on a surface 104, which is the inner surface of the second pane 102 (side IV). The pre-composite 1 is handled by means of a robot-assisted gripping element 105 (e.g. suction lifter) and positioned on the composite pane 100 such that the second adhesive layer 15 preferably has direct contact with the surface 104. The cover film 13 is removed beforehand. The pre-composite 1 is pressed against the composite pane 100 by the gripping element 105, whereby a firm adhesive bond between the pre-composite 1 and the composite pane 100 can be achieved. Advantageously, the two adhesive layers 14, 15 are additionally cured by heating and / or electromagnetic radiation, such as UV radiation. The pre-composite 1 and the composite pane 100 are thus permanently and firmly connected to each other.In addition, connection parts of the electro-optical functional film 5 not shown in the figures can be covered by encapsulation.

[0076] In Figure 4, the method according to the invention is illustrated again using a flowchart. It comprises the following steps in this order: a) Providing an adhesive pre-composite (1), which comprises in this order: a pre-composite pane (2), a first adhesive layer (14) made of an optically transparent adhesive, an electro-optical functional film (5), and a second adhesive layer (15) made of an optically transparent adhesive, b) Providing the pane (100), in particular a composite pane, c) Attaching the adhesive pre-composite (1) to a surface (104) of the pane (100) by adhering it using the second adhesive layer (15), wherein production of the adhesive pre-composite (1) comprises the following steps: i) Providing the pre-composite pane (2), ii) Laminating a first adhesive film (3) made of an optically transparent adhesive onto the pre-composite pane (2) to produce the first adhesive layer (14),iii) laminating the electro-optical functional film (5) onto the first adhesive layer (14), iv) laminating a second adhesive film (4) made of an optically transparent adhesive onto the electro-optical functional film (5) to produce the second adhesive layer (15).

[0077] From the above, it follows that the invention provides a method for post-processing a pane, preferably a composite pane, by which the pane can be provided with an electro-optical functional film, wherein uneven mechanical loading of the electro-optical functional film is avoided, so that optically impairing damage to the electro-optical functional film can be avoided and the pane has a high optical quality. The method according to the invention can be easily implemented in the industrial series production of panes, in particular composite panes. The panes, in particular composite panes, with electro-optical functional films can be produced simply, cost-effectively, and with high optical quality.

[0078] List of reference symbols

[0079] 1 pre-composite

[0080] 2 pre-laminated panes

[0081] 3 first adhesive film

[0082] 4 second adhesive film

[0083] 5 electro-optical functional film

[0084] 6 Vacuum laminator

[0085] 7 Vacuum chamber

[0086] 8, 8' laminating board

[0087] 9-roll laminator

[0088] 10 Laminating roller

[0089] 11 first intermediate product

[0090] 12 second intermediate product

[0091] 13 Cover film

[0092] 14 first adhesive layer

[0093] 15 second adhesive layer

[0094] 100 composite panes

[0095] 101 first disc

[0096] 102 second disc

[0097] 103 Intermediate layer

[0098] 104 Surface

[0099] 105 gripping organ

Claims

Patent claims 1. A method for post-processing a pane (100), in particular a composite pane, comprising the following steps: a) providing an adhesive pre-composite (1), which comprises in this order: a pre-composite pane (2), a first adhesive layer (14) made of an optically transparent adhesive, an electro-optical functional film (5), a second adhesive layer (15) made of an optically transparent adhesive, b) providing the pane (100), in particular a composite pane, c) attaching the adhesive pre-composite (1) to a surface (104) of the pane (100) by adhering it using the second adhesive layer (15), wherein production of the adhesive pre-composite (1) comprises the following steps: i) providing the pre-composite pane (2), ii) laminating a first adhesive film (3) made of an optically transparent adhesive onto the pre-composite pane (2) to produce the first adhesive layer (14),iii) laminating the electro-optical functional film (5) onto the first adhesive layer (14), iv) laminating a second adhesive film (4) made of an optically transparent adhesive onto the electro-optical functional film (5) to produce the second adhesive layer (15).

2. The method according to claim 1, wherein a polymeric cover film (13) is arranged on the second adhesive layer (15), which is removed before carrying out step c).

3. Method according to one of claims 1 or 2, wherein in step c) the pre-composite (1) is subjected to pressure in the direction of the surface (104) of the pane (100).

4. Method according to one of claims 1 to 3, wherein in step c) the second adhesive layer (15) made of an optically transparent adhesive is cured physically and / or chemically, in particular by the action of heat and / or electromagnetic radiation, in particular UV radiation.

5. Method according to one of claims 1 to 4, wherein during the production of the adhesive pre-composite (1) the amount of dust in the immediate vicinity of the pre-composite (1) is reduced, for example by production in a clean room and / or use of at least one dust cleaning device.

6. Method according to one of claims 1 to 5, wherein the pre-laminated pane (2) is a glass pane.

7. Method according to one of claims 1 to 6, wherein the pre-composite pane (2) has a maximum pane thickness of 0.5 mm.

8. Method according to one of claims 1 to 7, wherein the first adhesive layer (14) made of an optically transparent adhesive and / or the second adhesive layer (15) made of an optically transparent adhesive has a layer thickness in the range of 0.2 to 2 mm.

9. A method according to any one of claims 1 to 8, wherein the optically transparent adhesive is based on acrylate or polyurethane.

10. Method according to one of claims 1 to 9, wherein the electro-optical functional film (5) comprises a functional layer based on a liquid crystal.

11. Method according to one of claims 1 to 10, in which the pane (100), in particular a composite pane, consists of glass, in particular of soda-lime glass.

12. Method according to one of claims 1 to 11, wherein after step c) one or more connection parts of the electro-optical functional film (5) are covered by an encapsulation. 13 Pane (100), in particular a composite pane, with a pre-composite (1) glued to a surface (104), the pre-composite (1) comprising as a stacking sequence in this order: a pre-composite pane (2), a first adhesive layer (14) made of an optically transparent adhesive, an electro-optical functional film (5), a second adhesive layer (15) made of an optically transparent adhesive, by means of which the pre-composite (1) is glued to the pane (100).

14. Use of the pane (100), in particular a composite pane, according to claim 13 in buildings or in means of transport for traffic on land, in the air or for Water, especially in motor vehicles, for example as windshields, rear windows, side windows and / or roof windows.

Citation Information

Patent Citations

  • Glazing comprising a substrate furnished with a multiplicity of thin layers providing thermal insulation and / or solar protection

    EP0847965B1

  • Light-adjusting film

    US20080316381A1