Printing method for infiltration of high-viscosity mixture solution containing particles into porous material, infiltration-inducing method, and automation method using same
The automated method for infiltrating high-viscosity ceramic slurries into porous materials addresses the inefficiencies of manual processes by using an automated printing and penetration induction technique, ensuring uniformity and enabling mass production with improved ceramic product quality.
Patent Information
- Application Number
- PCT/KR2024/005111
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-04-21
- Filing Date
- 2024-04-17
- Publication Date
- 2024-10-24
AI Technical Summary
Conventional methods for infiltrating high-viscosity ceramic slurries into porous materials, such as sponges, are inefficient and prone to variability in quality due to manual processes, making mass production challenging and difficult to maintain uniformity.
An automated method involving a printing process to apply a high-viscosity mixture onto a film, which is then used to penetrate a porous material using a pair of pressure rollers with adjustable gaps, ensuring consistent application and infiltration.
This method enables uniform and consistent infiltration of the high-viscosity mixture into porous materials, reducing waste and allowing for mass production with improved mechanical properties of the resulting ceramic products.
Smart Images

Figure KR2024005111_24102024_PF_FP_ABST
Abstract
Description
Printing method for infiltrating a high viscosity mixture containing particles into a porous material, infiltration-inducing method and automated method using the same
[0001] The present invention relates to a printing method, a penetration-inducing method, and an automated method using the same for infiltrating a high-viscosity mixture containing particles such as ceramic powder into a porous material for the purpose of manufacturing artificial bones, etc., and more specifically, to a printing method for forming a film on which a mixture is applied by applying a high-viscosity mixture containing particles to a film in a predetermined shape and thickness, and to an penetration-inducing method for arranging a porous material such as a sponge between a pair of films on which a mixture is applied and compressing the porous material to infiltrate the mixture applied to the film into the porous material, thereby automating a series of processes for infiltrating a high-viscosity mixture containing particles into a porous material.
[0002] Generally, porous materials similar to the structure of natural cancellous bone have high specific surface area and porosity, and a three-dimensional interconnected open pore structure. This structure is well known to be the most suitable structure for cell attachment and osteogenesis and is widely used in the field of hard tissue engineering. Therefore, various methods for manufacturing cancellous bone-mimicking artificial bone grafts are being studied, and the most widely known methods include sponge replication, gel casting, pore formation using volatile organic compounds, and salt leaching. Among them, sponge replication has the advantage of being able to produce an excellent structure as a bone graft because it is easy to control the pore size and easily forms three-dimensionally interconnected open pores.
[0003] This sponge replication method involves mixing ceramic powder of several to several tens of micrometers in size with a liquid, infiltrating a ceramic slurry into a sponge, heating the sponge in which the ceramic slurry is synthesized at a high temperature to vaporize the sponge and sinter the ceramic, ultimately producing a porous ceramic that forms artificial bone. As a related prior art document, Republic of Korea Patent Publication No. 10-2013-0073302 (published on July 3, 2013, hereinafter referred to as “prior art document 1”) has been proposed.
[0004] In prior art document 1, a slurry for reinforcing a bone is coated on a sponge and dried to form a sponge with a reinforced bone, a ceramic slurry composed of a bioceramic powder, a dispersant, and a freezing medium is infiltrated into the sponge with the reinforced bone, and freeze-dried to form a porous ceramic green body, and then the porous ceramic green body is heat-treated to manufacture a bioceramic porous body.
[0005] In the case of the above prior art document 1, the mechanical properties of the ceramic porous body are improved by filling a ceramic slurry into a sponge having a reinforced basic structure, and the ceramic slurry is formed with a low viscosity in the range of 0.1 to 1.5 Pa·s so that the ceramic slurry can be naturally absorbed into the sponge.
[0006] However, in the case of ceramic slurry for manufacturing artificial bones for special purposes, the viscosity of the ceramic slurry is approximately 600,000 cP (600 Pa·s), so it is not naturally absorbed into the sponge due to surface tension. Accordingly, a method of manually infiltrating the ceramic slurry into the sponge with steel using a rod has been used in the past.
[0007] The conventional method of manually permeating ceramic slurry into a sponge has the problem that the quality of the porous ceramic varies depending on the skill of the worker, and above all, it is difficult to maintain a consistent quality even for the same skilled worker due to fatigue accumulation when working for a long time, and mass production is impossible.
[0008] The present invention has been devised to solve the above problems, and the purpose of the present invention is to provide a printing method, a penetration induction method, and an automated method using the same, which enable mass production by automating a series of operations for infiltrating a high-viscosity mixture containing particles into a porous material, and can always infiltrate a constant amount of the mixture into the porous material to implement uniform quality.
[0009] Another object of the present invention is to provide a printing method, a penetration-inducing method, and an automation method using the same that can reduce consumption of a mixed solution.
[0010] Another object of the present invention is to provide a printing method, a penetration-inducing method, and an automated method using the same, which can uniformly infiltrate a mixed solution into a porous material through stepwise compression of a film and a porous material.
[0011] The present invention, which achieves the above-described purpose and performs the task of eliminating the conventional defects, relates to a printing method for applying a high-viscosity mixed solution containing particles to a film (20), and is characterized by including a step (S110) of placing a coating frame (110) having a cavity (111) formed therein to form a coating area on a table (101); a film placing step (S120) of placing a film (20) under the coating frame (110); a mixture supply step (S130) of supplying a certain amount of the mixed solution onto the coating frame (110); and a mixture application step (S140) of dispersing the mixed solution on the coating frame (110) and guiding it into the cavity (111) to fill it.
[0012] In addition, the film placement step (S120) may include a film fixing step (S121) of placing and fixing a film (20) on a vacuum table (140) equipped with a plurality of suction holes (141); and a film adhesion step (S122) of raising the film (20) located at the lower portion of the application frame (110) to adhere the upper surface of the film (20) to the application frame (110).
[0013] In addition, the mixture application step (S140) may include a blade application step (S141) in which the blade (131) of the scraper (130) is applied to the application mold (110); and a relative movement step (S142) in which the application mold (110) and the film (20) are moved laterally so that the blade (131) guides the mixture to the cavity (111) by the relative movement of the scraper (130), the application mold (110), and the film (20).
[0014] In particular, after the above-mentioned mixed solution application step (S140), a film separation step (S150) may be further included in which the film (20) located at the lower portion of the application mold (110) is lowered to separate the film (20) from the application mold (110).
[0015] And, after the film separation step (S150), the film arrangement step (S120), the mixture supply step (S130), and the mixture application step (S140) are repeated, but the relative movement step (S142) of the mixture application step (S140) can change the movement direction of the application frame (110) and the film (20) to opposite sides.
[0016] Meanwhile, a method for inducing penetration of a high viscosity mixed solution containing particles into a porous material is characterized by including a porous material preparation step (S210) of stacking films (20) on the upper and lower portions of a porous material (10) and placing them on a conveyor (240); and a penetration inducing step (S220) of forcibly infiltrating the mixed solution (21) into the porous material (10) by inserting the porous material (10) with the films (20) placed on the upper and lower portions between a pair of pressure rollers (211, 212) and compressing the porous material (10).
[0017] In addition, the above-described penetration induction step (S220) may include a gap adjustment step (S221) for adjusting the gap between a pair of pressure rollers (211, 212); a compression step (S222) for compressing a porous material (10) having a film (20) disposed on the upper and lower portions by feeding it between a pair of pressure rollers (211, 212) onto a conveyor (240) disposed on one side of the pressure rollers (211, 212); and a relocation step (S223) for moving it to a conveyor (240) disposed on the other side of the pressure rollers (211, 212).
[0018] In particular, the above-described penetration induction step (S220) may further include a re-pressure step (S224) in which, after the above-described rearrangement step (S223), the porous material (10) with the film (20) arranged on the upper and lower sides is re-introduced between a pair of pressure rollers (211, 212) by a conveyor (240) arranged on the other side of the pressure rollers (211, 212) and re-pressurized.
[0019] In addition, the above penetration induction step (S220) is performed repeatedly multiple times, and it is preferable that the gap adjustment step (S221) gradually narrows the gap between a pair of pressure rollers (211, 212).
[0020] Meanwhile, an automated method for permeating a high-viscosity mixture containing particles of the present invention into a porous material may include a printing step (100) of applying a high-viscosity mixture containing particles to a designed application area on the upper portion of a film (20); and a permeation inducing step (S200) of arranging a pair of films (20) on which a mixture (21) is applied on the upper and lower portions of a porous material (10) and vertically compressing the film (20) and the porous material (10) to forcibly permeate the mixture (21) into the porous material (10).
[0021] In addition, the application area may be formed by a cavity (111) of an application mold (110) including a central area (111-1) that provides an area corresponding to the shape of the porous material (10); and a rear protrusion area (111-2) that provides an area that protrudes in the rear and both sides from the rear ends of the central area (111-1).
[0022] In addition, the cavity (111) may further include an inclined protrusion region (111-3) that protrudes on both sides of the central region (111-1) and extends in the front-back direction, and is formed in a triangular structure so that the rear end gradually approaches the central region (111-1).
[0023] According to the printing method, penetration-inducing method and automation method using the same of the present invention, a constant amount of the mixture is always applied to the film to penetrate the porous material, so that a constant quality can be maintained regardless of the skill level or condition of the worker.
[0024] In particular, the series of operations of applying the mixture to a film and penetrating it into a porous material can be automated to enable mass production and further improve quality.
[0025] Furthermore, since the mixture applied by one side scraper in the preceding application process and the remaining mixture is guided to the cavity by the other side scraper in the subsequent application process, unnecessary consumption of the mixture can be prevented.
[0026] In addition, by adjusting the gap between the pressure rollers according to the process progression sequence using a gap adjustment mechanism, the film and the porous material can be compressed step by step, thereby uniformly permeating the mixed solution into the porous material, thereby manufacturing a high-quality porous support.
[0027] FIG. 1 is a perspective view of a printing device for implementing a printing method according to an embodiment of the present invention;
[0028] Figure 2 is a front view of a printing device for implementing a printing method according to an embodiment of the present invention;
[0029] Figure 3 is a perspective view of a coating mold for implementing a printing method according to an embodiment of the present invention;
[0030] Figure 4 is an exemplary diagram showing the cavity shape of a coating mold for implementing a printing method according to an embodiment of the present invention.
[0031] Figure 5 is a block diagram illustrating a printing method according to an embodiment of the present invention in a time series manner.
[0032] Figures 6a to 6q are exemplary views showing a process of applying a mixture to a film according to a printing method according to an embodiment of the present invention.
[0033] Figure 7 is a perspective view of a penetration induction device for implementing a penetration induction method according to an embodiment of the present invention.
[0034] Figure 8 is a perspective view showing the operating structure of the pressure roller of the penetration induction device for implementing the penetration induction method according to an embodiment of the present invention.
[0035] Figure 9 is a side view showing the operating structure of the pressure roller of the penetration induction device for implementing the penetration induction method according to an embodiment of the present invention.
[0036] Figure 10 is a perspective view showing a state in which a conveyor of a penetration induction device for implementing a penetration induction method according to an embodiment of the present invention is installed on both sides of a pressure roller.
[0037] Figure 11 is a block diagram illustrating a penetration induction method according to an embodiment of the present invention in a time series manner.
[0038] Figure 12 is an example diagram showing a state in which a pair of films coated with a mixed solution are placed on the upper and lower parts of a porous material.
[0039] Figures 13a to 13d are exemplary diagrams showing a process of compressing a film and a porous material to infiltrate a mixed solution into a porous material using a penetration-inducing method according to an embodiment of the present invention.
[0040] Figure 14 is a block diagram illustrating a time series of an automation method according to an embodiment of the present invention.
[0041] Figure 15 is an image showing the results of an experiment on the degree of penetration according to the shape of a cavity formed in a coating mold using the penetration induction method of the present invention.
[0042] Hereinafter, a preferred embodiment of the present invention will be described in detail based on the matters illustrated in the drawings. However, if it is determined that a specific description of a related known function or configuration may unnecessarily obscure the gist of the present invention, the detailed description will be omitted.
[0043] Before describing the printing method of the high viscosity mixed liquid containing the particles of the present invention, a printing device (100) for implementing the printing method will be described. However, the printing device (100) described below is presented as one example of a device for implementing the present invention, and the dispenser height, dispenser pressure, size of the porous material, speed of the conveying mechanism, etc. are also presented as examples, and therefore, it will be apparent to those skilled in the art that they can be flexibly changed depending on the intended porous support.
[0044] As shown in FIGS. 1 to 4, a printing device (100) for implementing the printing method of the present invention includes a coating frame (110), a dispenser (120), and a scraper (130).
[0045] The above-mentioned application mold (110) is arranged on the upper part of the film (20) to allow the mixture to be applied to the film (20) without flowing, and is provided with one or more cavities (111) that form an application area.
[0046] Meanwhile, the cavity (111) penetrates the flat-plate coating mold (110) and includes a central region (111-1) and a rear protruding region (111-2) so that the mixed solution (21) on the film (20) can uniformly penetrate the entire porous material (10) in consideration of the shape of the porous material (10) that is deformed due to the compression of the pressure rollers (211, 212) to be described later.
[0047] The above central region (111-1) is formed with the same shape and size as the porous material (10) before deformation.
[0048] For example, as shown in Fig. 11, when the porous material (10) is formed into a 90 mm x 120 mm rectangular shape, the central region (111-1) can also be formed into a 90 mm x 120 mm rectangular hole.
[0049] The above rear protrusion area (111-2) is formed to protrude in the rear and both sides from both rear ends of the central area (111-1) so that the mixed solution that penetrates the portion that is stretched due to compression of the porous material (10) is applied onto the film (20).
[0050] Meanwhile, the mixture applied to the film (20) by the rear protrusion area (111-2) is pushed backward when the film (20) and the porous material (10) are pressed by the pressure rollers (211, 212) described later, and in addition, the mixture flows toward the center due to the cohesive force caused by the viscosity of the mixture in the central area (111-1) and comes into contact with the elongated portion of the porous material (10) and penetrates into the porous material (10), so that the mixture (21) can be uniformly penetrated even into the elongated portion.
[0051] In addition, inclined protrusion regions (111-3) that enable the mixed solution to penetrate evenly to the end edges of the porous material (10) may be formed on both sides of the central region (111-1), and an auxiliary protrusion region (111-4) that further protrudes rearward may be formed on the outer lower side of the rear protrusion region (111-2).
[0052] The above-mentioned inclined protrusion area (111-3) protrudes outward from both sides of the central area (111-1) and extends in the front-back direction, and is formed into a triangular structure with the rear end gradually approaching the central area (111-1).
[0053] The mixture applied to the film (20) by these inclined protrusion areas (111-3) supplements the mixture that penetrates into both edges of the porous material (10), thereby inducing the mixture (21) to smoothly penetrate even the end edges of the porous material (10).
[0054] The coating frame (110) configured as described above is installed in a horizontal position on the table (101) of the printing device (100).
[0055] The above dispenser (120) supplies a certain amount of the mixture onto the application frame (110), is provided in the printing device (100) so as to be positioned vertically above the application frame (110), and is preferably configured as a line dispenser (120) that supplies the mixture (21) in a linear structure so that the mixture (21) is applied evenly onto the application frame (110).
[0056] A dispenser (120) like this can be connected to a mixed solution storage tank (not shown) to receive the mixed solution (21).
[0057] In addition, the dispenser (120) is connected to a hydraulic cylinder (121) for the dispenser, and the hydraulic cylinder (121) for the dispenser is configured to move the dispenser (120) up and down while being extended by hydraulic pressure to adjust the gap between the application frame (110) and the dispenser (120).
[0058] In addition, the hydraulic cylinder (121) for the dispenser is mounted on a dispenser height fine-adjuster (122), and the dispenser height fine-adjuster (122) includes a screw-type drive shaft (122a) in a vertical position connected to a handle (122b), a pair of guide rods (122c) arranged in a parallel position on both sides of the screw-type drive shaft (122a), and a vertical movement block (122d) connected to the hydraulic cylinder (121) for the dispenser, which is combined with the screw-type drive shaft (122a) and the guide rods (122c) and moves up and down by the rotation of the screw-type drive shaft (122a).
[0059] A dispenser height fine adjuster (122) of this type moves the vertical movement block (122d), the hydraulic cylinder for the dispenser (121), and the dispenser (120) up and down by the rotation of the screw-type drive shaft (122a) by the operation of the handle (122b), so that the height of the dispenser (120) can be finely adjusted.
[0060] The scraper (130) above guides and disperses the mixed solution supplied to the application mold (110) into the cavity (111) so that the mixed solution is uniformly filled in the cavity (111) at a constant thickness. It includes a blade (131) that guides the mixed solution into the cavity (111) while moving relative to the application mold (110) while being in close contact with it, and is installed in the printing device (100) adjacent to the dispenser (120).
[0061] Meanwhile, the blade (131) is made of a polymer material so as to be elastically deformable, and is installed in an inclined position so as to form an acute angle with the application mold (110).
[0062] The scrapers (130) as described above are positioned on both sides of the dispenser (120), and the blades (131) of the scrapers (130) on both sides of the dispenser (120) are provided symmetrically and inclined to each other so that, regardless of the relative movement direction of the application frame (110) and the scrapers (130), the blade (131) of one of the scrapers (130) is always in close contact with the application frame (110) and functions to guide the mixed liquid into the cavity (111).
[0063] That is, when one of the scrapers (130) on both sides guides the mixture into the cavity (111) by the relative movement of the application mold (110) and the scraper (130) and the mixture is filled into the cavity (111) and the application of the mixture to the film (20) is completed, the other scraper (130) guides the mixture remaining on the application mold (110) and the mixture newly supplied from the dispenser (120) into the cavity (111) and fills them in the next application process, so that continuous application work is possible without having to return the scraper (130) to the origin position after the application work to one film (20) is completed.
[0064] In this way, the scraper (130) provided on both sides of the dispenser (120) is connected to a hydraulic cylinder (132) for the scraper, and the hydraulic cylinder (132) for the scraper is installed in a scraper height fine adjuster (133) so as to adjust the gap between the scraper (130) and the application frame (110) through the up and down movement of the scraper (130).
[0065] Meanwhile, since the hydraulic cylinder (132) for the scraper and the scraper height fine adjuster (133) can be configured with substantially the same structure as the hydraulic cylinder (121) for the dispenser and the dispenser height fine adjuster (122), a description of the specific configuration of the hydraulic cylinder (132) for the scraper and the scraper height fine adjuster (133) is omitted.
[0066] The above vacuum table (140) has a plurality of suction holes (141) formed on the upper surface and is connected to a vacuum pump (not shown) so that when the vacuum pump is in operation, air is sucked in through the suction holes (141) and the film (20) placed on the upper surface is tightly fixed.
[0067] In addition, a lifting mechanism (150) made of a hydraulic cylinder is provided at the bottom of the vacuum table (140), so that the film (20) can be brought into contact with or separated from the application mold (110) through the up and down movement of the vacuum table (140) by the lifting mechanism (150).
[0068] In addition, a transport mechanism (160) formed of a linear stage extending in the Y-axis direction of the coordinate system shown in FIG. 1 is provided at the lower portion of the above-described elevator mechanism (150), and the transport mechanism (160) is connected to the elevator mechanism (150) and the table (101) so that the film (20) and the coating frame (110) are moved laterally according to the process sequence through the lateral movement of the elevator mechanism (150) and the table (101).
[0069] As illustrated in FIG. 5, the printing method of the high viscosity mixture containing the particles of the present invention is sequentially performed including a coating frame placement step (S110), a film placement step (S120), a mixture supply step (S130), and a mixture application step (S140).
[0070] The above-mentioned coating frame mounting step (S110) is performed by fixing the coating frame (110) in a horizontal position on the table (101) of the printing device (100) in which a cavity (111) forming a coating area is formed.
[0071] As shown in FIGS. 6a and 6b, the film placement step (S120) is a process of placing a film (20) at the bottom of a coating mold (110), and includes a film fixing step (S121) of placing and fixing the film (20) on a vacuum table (140) equipped with a plurality of suction holes (141), and a film adhesion step (S122) of raising the film (20) located at the bottom of the coating mold (110) to adhere the upper surface of the film (20) to the coating mold (110).
[0072] The above film fixing step (S121) may be performed by operating the vacuum table (140) to adsorb and fix the film (20) to the vacuum table (140), and the above film adhesion step (S122) may be performed by operating the elevating mechanism (150) to elevate the vacuum table (140) so that the upper surface of the film (20) is adhered to the application mold (110).
[0073] The above mixture supply step (S130) is a process of supplying a certain amount of mixture onto the application mold (110), and as shown in FIGS. 6c and 6d, the method may be performed by moving the lifting mechanism (150), the vacuum table (140), and the table (101) laterally using the transport mechanism (160) so that the dispenser (120) is positioned at one end of the cavity (111), lowering the dispenser (120) so that the dispenser (120) is positioned at a height of about 3 cm from the surface of the application mold (110), and then discharging the mixture using the dispenser (120).
[0074] At this time, the appropriate pressure applied to the end of the dispenser (120) when discharging the mixed liquid can be formed to be approximately 470 kPa.
[0075] Meanwhile, when the coating mold (110) is provided with two cavities (111a, 111b), the dispenser (120) is positioned at the left end of the left cavity (111a) or at the right end of the right cavity (111b). In the following description, the dispenser (120) is assumed to be positioned at the left end of the left cavity (111a). In this case, the discharge of the mixed solution by the dispenser (120) is performed until the dispenser (120) reaches the right end of the right cavity (111b).
[0076] As illustrated in FIGS. 6e and 6h, the mixture application step (S140) is a process of dispersing the mixture supplied onto the application mold (110) by the dispenser (120) and guiding it into the cavity (111) to fill it, and includes a blade adhesion step (S141) in which the scraper (130) is lowered to bring the blade (131) into contact with the application mold (110), and a relative movement step (S142) in which the scraper (130), the application mold (110), and the film (20) are moved laterally so that the blade (131) guides the mixture into the cavity (111) by the relative movement of the scraper (130), the application mold (110), and the film (20).
[0077] Meanwhile, the blade contact step (S141) is performed by operating the hydraulic cylinder (132) for the scraper so that the blade (131) of the scraper (130a) located on the left side of the dispenser (120) touches the application mold (110) to lower the scraper (130a), and then further lowering the scraper (130a) by about 1.0 mm using the scraper height fine adjuster (133) so that the tip of the blade (131) is deformed and comes into contact with the upper surface of the application mold (110).
[0078] Meanwhile, if the blade (131) presses the application mold (110) excessively, there is a problem that the friction between the scraper (130) and the application mold (110) increases, causing the surface of the application mold (110) to wear out and the mixture inside the application mold (110) to be lost. Therefore, it is preferable to lower the blade (131) by about 1.0 mm from the time it touches the application mold (110) so that the blade (131) is pressed against the application mold (110) with an appropriate pressure.
[0079] This blade adhesion step (S141) can be performed simultaneously with the process of lowering the dispenser (120).
[0080] The above relative movement step (S142) can be performed by operating the transport mechanism (160) to move the lifting mechanism (150) and the vacuum table (140) in the left direction, thereby implementing the relative movement of the scraper (130), the application frame (110), and the film (20).
[0081] This relative movement step (S142) is performed until the tip of the blade (131) of the left scraper (130a) reaches the right end of the right cavity (111b), and when the tip of the blade (131) of the left scraper (130a) reaches the right end of the right cavity (111b), the transport mechanism (160) is stopped, and the hydraulic cylinder (132) for the scraper and the hydraulic cylinder (121) for the dispenser are operated to raise the left scraper (130a) and the dispenser (120) and separate them from the application mold (110).
[0082] Meanwhile, the appropriate transport speed of the transport mechanism (160) can be implemented at approximately 25 mm / s.
[0083] When the application of the mixture (21) is completed through the above process, a film separation step (S150) is performed in which the film (20) located at the bottom of the application frame (110) is lowered to separate the film (20) from the application frame (110).
[0084] As illustrated in FIG. 6i, the film separation step (S150) is performed by operating the lifting mechanism (150) to lower the vacuum table (140) so as to separate the film (20) on which the mixed solution (21) is applied from the application frame (110), and it is preferable to maintain the vacuum state of the vacuum table (140) to maintain the fixed state of the film (20).
[0085] Meanwhile, after the film (20) is completely separated from the application mold (110) by lowering the vacuum table (140), the vacuum of the vacuum table (140) is released to separate the film (20) on which the mixed solution (21) is applied from the vacuum table (140).
[0086] After the film separation step (S150), the film arrangement step (S120), the mixture supply step (S130), and the mixture application step (S140) are repeated, but in the relative movement step (S142) of the mixture application step (S140), the movement direction of the application frame (110) and the film (20) is changed to the opposite side, and the right scraper (130b) is used to induce dispersion and filling of the mixture, thereby performing the application process for a new film (20).
[0087] That is, as shown in Fig. 6j, when the removal of the film (20) on which the mixed solution (21) has been applied is completed, a new film (20) is fixed by vacuum on the vacuum table (140), and the vacuum table (140) is raised so that the upper surface of the film (20) is brought into close contact with the application frame (110).
[0088] As shown in FIG. 6k, the lifting mechanism (150), vacuum table (140), and table (101) are moved laterally using the transport mechanism (160) so that the dispenser (120) is positioned at the right end of the right cavity (111b).
[0089] As shown in FIG. 6l, the dispenser (120) is positioned at a point about 3 cm above the application frame (110), and the hydraulic cylinder for the dispenser (121) and the hydraulic cylinder for the scraper (132) are operated so that the blade (131) of the right scraper (130b) touches the application frame (110) to lower the dispenser (120) and the right scraper (130b), and then the scraper (130) is further lowered by about 1.0 mm using the scraper height fine adjuster (133) connected to the right scraper (130b).
[0090] As shown in FIG. 6m, the dispenser (120) is operated to discharge the mixed solution onto the surface of the application mold (110), and the transfer mechanism (160) is operated to move the vacuum table (140) and the table (101) to the right so that the mixed solution is applied in a flat manner on the application mold (110).
[0091] In the previous process, the mixture remaining on the application mold (110) and the mixture discharged from the dispenser (120) are distributed while being guided into the cavity (111) by the blade (131) of the right scraper (130b) and filled to a certain thickness inside the cavity (111).
[0092] As shown in Fig. 6n, when the dispenser (120) reaches the left end of the left cavity (111a), the operation of the dispenser (120) is stopped to stop the discharge of the mixed liquid.
[0093] As shown in Fig. 6o, when the tip of the blade (131) of the right scraper (130b) reaches the left end of the left cavity (111a), the transport mechanism (160) is stopped.
[0094] As shown in Fig. 6p, the right scraper (130b) and the dispenser (120) are raised and separated from the application frame (110) using the hydraulic cylinder (132) for the scraper and the hydraulic cylinder (121) for the dispenser.
[0095] As shown in Fig. 6q, the lifting mechanism (150) is operated to lower the vacuum table (140), thereby separating the film (20) on which the mixed solution (21) is applied from the application frame (110).
[0096] As described above, the present invention can improve productivity by allowing the mixture to be applied to the film (20) regardless of the relative movement direction of the application mold (110) and the two scrapers (130a, 130b), and in particular, the mixture remaining on the application mold (110) in the preceding process can be used in the subsequent process, thereby reducing unnecessary waste of the mixture.
[0097]
[0098] Before describing the method for inducing penetration of a high viscosity mixed liquid containing particles of the present invention, a penetration-inducing device (200) for implementing the above-described penetration-inducing method will be described. However, the penetration-inducing device (200) described below is presented as one example of a device for implementing the present invention, and the porous material thickness, the gap between the pressure rollers, the motor rotation speed, the rotation speed of the end of the reducer, the conveyor belt speed, etc. are also presented as examples, and therefore, it will be readily apparent to those skilled in the art that they can be flexibly changed depending on the intended porous support.
[0099] As shown in FIGS. 7 to 10, a penetration induction device (200) for implementing the penetration induction method of the present invention includes a pair of pressure rollers (211, 212) and a conveyor (240).
[0100] The above pair of pressure rollers (211, 212) are configured to be adjacent to each other vertically and rotate in different directions to press and transport the film (20) and the porous material (10).
[0101] Meanwhile, a spur gear (211a, 212a) is provided at one end of the pressure roller (211, 212) so that a pair of pressure rollers (211, 212) rotate in conjunction with the meshing of the spur gears (211a, 212a), and the other end of the lower pressure roller (212) is connected to a driving unit (220) composed of a motor (221) and a reducer (222), so that the lower pressure roller (212) rotates by the operation of the driving unit (220) and rotates the upper pressure roller (211).
[0102] In addition, the upper pressure roller (211) is connected to a gap adjustment mechanism (230), and the gap adjustment mechanism (230) is configured to move the upper pressure roller (211) up and down to adjust the gap between the upper pressure roller (211) and the lower pressure roller (212).
[0103] The above gap adjustment mechanism (230) includes a drive unit (231) composed of a motor (231a) and a reducer (231b), an elevation shaft (232) that is coupled to both ends of the upper pressure roller (211) in a vertical position and rotates to induce up and down movement of the upper pressure roller (211), and a power transmission means (233) that connects the drive unit (231) and the elevation shaft (232) to transmit the power of the drive unit (231) to the elevation shaft (232).
[0104] At this time, the lifting shaft (232) is configured to have threads formed on the outer surface to raise or lower the upper pressure roller (211) depending on the direction of rotation, and the power transmission means (233) is configured to be a combination of multiple gears to transmit power generated from the driving unit (231) to both lifting shafts (232).
[0105] The above conveyor (240) is composed of a belt conveyor, and includes a belt guard (241) that supports the belt from below to prevent sagging and cutting of the belt, and a tension controller (242) that adjusts the tension of the belt.
[0106] Meanwhile, the tension controller (242) is connected to a driven roller (240b) provided at the outer end of the conveyor (240) and moves the driven roller (240b) closer to or further away from the driving roller (240a) to adjust the tension of the belt.
[0107] That is, the tension adjuster (242) may include a bracket (242a) that is coupled to both ends of the driven roller (240b) to support the driven roller (240b) and move together with it, and a screw-type drive shaft (242b) that is coupled to the bracket (242a) and moves the bracket (242a) while rotating by a handle operation to adjust the position of the driven roller (240b).
[0108] A conveyor (240) like this is provided on both sides of the pressure rollers (211, 212), and the porous material (10) fed between the pressure rollers (211, 212) by one conveyor (240) is fed to the other conveyor (240) after being compressed, and is fed back between the pressure rollers (211, 212) by the operation of the other conveyor (240), thereby easily implementing multiple compression processes.
[0109] Meanwhile, the pressure rollers (211, 212) and the conveyors (240) on both sides can be configured to share a drive unit (220) so that the pressure rollers (211, 212) and the conveyors (240) on both sides are driven by a single drive unit (220).
[0110] That is, the output shaft of the reducer (222) of the drive unit (220) is directly connected to the lower pressure roller (212) through a coupler, and is connected to the drive roller (240a) of the conveyor (240) arranged on both sides of the pressure rollers (211, 212) through belts (222a, 222b), so that the pressure rollers (211, 212) and the two conveyors (240) operate together when the drive unit (220) operates.
[0111] As illustrated in Fig. 12, the method for inducing penetration of a high viscosity mixed solution containing particles of the present invention is sequentially performed, including a porous material preparation step (S210) and a penetration induction step (S220).
[0112] As illustrated in FIG. 11 and FIG. 13a, the porous material preparation step (S210) is a process of stacking films (20) on the upper and lower parts of a porous material (10) and placing them on a conveyor (240). The film (20) on which the mixture (21) is applied is placed on the upper and lower parts of a porous material (10) made of a polyurethane sponge having a thickness of about 5 mm, and the film (20) is placed on the upper and lower parts of the porous material (10) so that the mixture (21) applied to the film (20) faces the porous material (10), and the porous material (10) on which the film (20) is stacked on the upper and lower parts is placed on a conveyor (240).
[0113] In the following description, it is assumed that the film (20) is placed on the left conveyor (240a) of the pressure roller (211, 212) through the porous material preparation step (S210).
[0114]
[0115] The above-mentioned penetration induction step (S220) is a process in which a porous material (10) having a film (20) disposed on the upper and lower portions is compressed by inserting the mixed solution (21) between a pair of pressure rollers (211, 212) and forcibly infiltrating the porous material (10), and includes a gap adjustment step (S221), a compression step (S222), and a rearrangement step (S223).
[0116] The above gap adjustment step (S221) is a process for adjusting the gap between a pair of pressure rollers (211, 212), and the gap between the upper pressure roller (211) and the lower pressure roller (212) is adjusted using a gap adjustment mechanism (230). In order to induce penetration of the mixed solution (21) by compressing a porous material (10) having a thickness of 5 mm, the gap between the pressure rollers (211, 212) can be gradually reduced so that the gap becomes 1.125 mm during the first compression, 1 mm during the second compression, 0.875 mm during the third compression, and 0.75 mm during the fourth compression.
[0117] As illustrated in Fig. 13b, the pressing step (S222) is a process of pressing a porous material (10) with a film (20) arranged vertically by feeding it between a pair of pressing rollers (211, 212). When the driving unit (220) is operated to rotate the lower pressing roller (212) clockwise, the upper pressing roller (211) rotates counterclockwise, and when the conveyors (240) on both sides operate together, the porous material (10) of the left conveyor (240a) is fed between the upper pressing roller (211) and the lower pressing roller (212).
[0118] At this time, it is preferable that the motor rotation speed of the drive unit (220) is 1 / 10 (rotations / s), the reduction gear end rotation speed is 1 / 50 (rotations / s), and the conveyor (240) speed is 4.4 (mm / s).
[0119] Meanwhile, as the film (20) and the porous material (10) are pressed together by the upper pressure roller (211) and the lower pressure roller (212), the mixture (21) of the film (20) penetrates into the porous material (10), and the mixture (21) applied to the film (20) includes a central region (111-1), a rear protruding region (111-2), and an inclined protruding region (111-3) due to the cavity (111) formed in the application mold (110), so that the mixture (21) can even penetrate into the deformed portion of the porous material (10) that is deformed to be extended in the direction of travel due to the pressing.
[0120] As illustrated in Fig. 13c, the above-described rearrangement step (S223) is performed by moving the porous material (10) discharged from the pressure roller (211, 212) to the right conveyor (240b) and arranging it.
[0121] Meanwhile, after the above-mentioned repositioning step (S223), a re-compression step (S224) may be performed in which the porous material (10) that has been first compressed and placed on the right conveyor (240b) is re-introduced between the pressure rollers (211, 212) and re-compression is performed.
[0122] As illustrated in FIG. 13d, the re-pressing step (S224) is performed by operating the driving unit (220) in the reverse direction so that the lower pressure roller (212) rotates counterclockwise to transport the porous material (10) of the right conveyor (240b) in the left direction, thereby feeding the porous material (10) between the upper pressure roller (211) and the lower pressure roller (212).
[0123] The penetration induction step (S220) configured as above is repeatedly performed multiple times, and as exemplified above, the gap between a pair of pressure rollers (211, 212) is gradually narrowed from 1.125 mm → 1 mm → 0.875 mm → 0.75 mm to gradually pressurize the porous material (10).
[0124] An automated method for permeating a high viscosity mixture containing particles according to the present invention into a porous material is configured using the printing method and the permeation induction method configured as described above.
[0125] As illustrated in FIG. 14, an automated method for permeating a high-viscosity mixture containing particles according to an embodiment of the present invention into a porous material includes a printing step (100) of applying a high-viscosity mixture containing particles to a designed application area on the upper portion of a film according to the printing method, and a permeation inducing step (S200) of arranging a pair of films (20) on which a mixture (21) is applied according to the permeation inducing method on the upper and lower portions of a porous material (10) and vertically compressing the films (20) and the porous material (10) to forcibly permeate the mixture (21) into the porous material (10).
[0126] As described above, the present invention manufactures a film (20) coated with a mixture (21) using a printing method, and presses the porous material (10) disposed on the upper and lower portions of the film (20) coated with the mixture (21) in multiple stages according to a penetration-inducing method to allow the mixture (21) to penetrate the porous material (10), and by automating this series of processes, mass production of a porous support is possible, and uniformity of quality can be ensured.
[0127] Meanwhile, Fig. 15 shows the results of an experiment in which a polyurethane sponge was pressurized according to the penetration inducing method of the present invention to penetrate the mixture (however, the sponge area was approximately 11700 mm² and the thickness was 1.1 mm). (a) shows that protruding regions were formed only on the rear sides based on the central region (111-1) of the cavity (111), and it can be confirmed that the mixture was not sufficiently penetrated into the rear corners. (b) shows that a rear protruding region (111-2) was formed so as to protrude both rearward and on both sides based on the central region (111-1) of the cavity (111), and it can be confirmed that the mixture was relatively sufficiently penetrated. (c) shows that the protruding regions on both sides of the rear protruding region (111-2) were further protruded downward to form an auxiliary protruding region (111-4) and at the same time form an inclined protruding region (111-3), and it can be confirmed that stably penetrated with almost no unpenetrated region.
[0128]
[0129] It will be understood by those skilled in the art that the printing method, infiltration-inducing method, and automation method using the same for infiltrating a high-viscosity mixture containing particles according to the present invention described above into a porous material can be implemented in other specific forms without changing the technical idea or essential features of the present invention.
[0130] Therefore, it should be understood that the embodiments described above are exemplary in all respects and not restrictive, and the scope of the present invention is indicated by the claims described below rather than the detailed description described above, and all changes or modifications derived from the meaning and scope of the claims and equivalent concepts should be interpreted as being included in the scope of the present invention.
Claims
1. A printing method for applying a high viscosity mixture containing particles to a film (20), A coating frame mounting step (S110) of mounting a coating frame (110) having a cavity (111) formed to form a coating area on a table (101); Film placement step (S120) of placing a film (20) on the lower part of the above application mold (110); A mixture supply step (S130) for supplying a certain amount of mixture onto the above-mentioned application mold (110); and A mixture application step (S140) of dispersing the mixture on the above application mold (110) and filling it by guiding it into the cavity (111); A method for printing a high viscosity mixed solution containing particles characterized by including .
2. In paragraph 1, The above film placement step (S120) is A film fixing step (S121) of placing and fixing a film (20) on a vacuum table (140) equipped with a plurality of suction holes (141); and A film adhesion step (S122) of raising the film (20) located at the bottom of the application mold (110) and adhesion the upper surface of the film (20) to the application mold (110); A method for printing a high viscosity mixed solution containing particles characterized by including .
3. In paragraph 1, The above mixture application step (S140) is Blade adhesion step (S141) of adhesion of the blade (131) of the scraper (130) to the application mold (110); and A relative movement step (S142) in which the application mold (110) and the film (20) are moved laterally so that the blade (131) guides the mixture into the cavity (111) by the relative movement of the scraper (130), the application mold (110), and the film (20); A method for printing a high viscosity mixed solution containing particles characterized by including .
4. In paragraph 3, After the above mixture application step (S140), A film separation step (S150) of lowering the film (20) located at the bottom of the application mold (110) and separating the film (20) from the application mold (110); A method for printing a high viscosity mixture containing particles, characterized in that it further comprises:
5. In paragraph 4, After the above film separation step (S150), A method for printing a high viscosity mixed solution containing particles, wherein the film arrangement step (S120), the mixed solution supply step (S130), and the mixed solution application step (S140) are repeated, but the relative movement step (S142) of the mixed solution application step (S140) is characterized in that the movement direction of the application frame (110) and the film (20) is changed to the opposite side.
6. A method for inducing penetration of a high viscosity mixture containing particles into a porous material. A porous material preparation step (S210) of stacking a film (20) on the upper and lower parts of a porous material (10) and placing it on a conveyor (240); and A penetration induction step (S220) in which a porous material (10) having a film (20) arranged at the upper and lower portions is inserted between a pair of pressure rollers (211, 212) and pressed while forcing the mixed solution (21) into the porous material (10); A method for inducing penetration of a high viscosity mixture containing particles into a porous material, the method comprising:
7. In paragraph 6, The above penetration induction step (S220) is A gap adjustment step (S221) for adjusting the gap between a pair of pressure rollers (211, 212); A pressing step (S222) in which a porous material (10) with a film (20) arranged on the upper and lower sides is fed between a pair of pressing rollers (211, 212) and pressed by a conveyor (240) arranged on one side of the pressing rollers (211, 212); and A relocation step (S223) of moving to a conveyor (240) arranged on the other side of the pressure roller (211, 212); A method for inducing penetration of a high viscosity mixture containing particles into a porous material, the method comprising:
8. In paragraph 7, The above penetration induction step (S220) is After the above relocation step (S223), A re-pressing step (S224) in which the porous material (10) with the film (20) arranged on the upper and lower sides is re-introduced between a pair of pressure rollers (211, 212) by a conveyor (240) arranged on the other side of the pressure rollers (211, 212) and re-pressed; A method for inducing penetration of a high viscosity mixture containing particles into a porous material, the method comprising:
9. In paragraph 7, The above penetration induction step (S220) is A method for inducing penetration of a high viscosity mixture containing particles into a porous material, wherein the gap adjustment step (S221) is performed repeatedly over multiple times, and the gap between a pair of pressure rollers (211, 212) is gradually narrowed.
10. A printing step (100) of applying a high viscosity mixture containing particles to the upper part of the film (20) to the designed application area; and A penetration induction step (S200) in which a pair of films (20) coated with a mixture (21) are placed on the upper and lower portions of a porous material (10) and the films (20) and the porous material (10) are pressed upward and downward to force the mixture (21) into the porous material (10); An automated method for infiltrating a high viscosity mixture containing particles into a porous material, the mixture characterized by including:
11. In paragraph 1 or paragraph 10, The above application area is, A central region (111-1) providing a region corresponding to the shape of the above porous material (10); and A rear protrusion area (111-2) that provides an area that protrudes backward and in both directions from both sides of the rear end of the central area (111-1); An automated method for permeating a high viscosity mixture containing particles into a porous material, characterized in that the mixture is formed by a cavity (111) of a coating mold (110) including the particles.
12. In paragraph 11, The above cavity (111) is An inclined protrusion area (111-3) that protrudes from both sides of the central area (111-1) and extends in the front-back direction, and is formed in a triangular structure so that the rear end gradually approaches the central area (111-1); An automated method for infiltrating a high viscosity mixture containing particles into a porous material, the mixture characterized by further including:
Citation Information
Patent Citations
Method and apparatus for calibrating print head pressure and applying an accurate print pressure during production
KR1020100015539A
Method for manufacturing silicon filter
KR1020170080932A
Continuous process for producing electrodes for supercapacitors having high energy densities
KR1020180067618A
Foaming printing method
KR102362294B1
Conductor for PTC heater and heat dissipation material integrated manufacturing device using stencil technique and manufacturing method using the same
KR102454475B1