Liquid molding compound and preparation method therefor
By preparing a liquid molding adhesive containing paraffin oil, the problem of adhesive residue during the peeling process of pyrolytic tape in semiconductor packaging is solved, and the effect of no adhesive residue is achieved.
Patent Information
- Application Number
- PCT/CN2023/092801
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-04-26
- Filing Date
- 2023-05-08
- Publication Date
- 2024-10-31
AI Technical Summary
In the semiconductor packaging process, adhesive residue is prone to occur during the pyrolysis tape stripping process, affecting packaging quality.
A liquid molding compound is used, whose ingredients include fillers (such as silica), epoxy resins, curing agents (such as methyl endomethine tetrahydrophthalic anhydride), and dyes (such as carbon black) , accelerator (such as DBU) and paraffin oil, prepared through mixing, dispersion treatment and defoaming treatment. The paraffin oil precipitates under heating conditions to form a barrier layer to avoid residual glue.
It effectively avoids the occurrence of residual glue during the peeling process of pyrolytic tape, ensuring the integrity and quality of the package.
Smart Images

Figure CN2023092801_31102024_PF_FP_ABST
Abstract
Description
Liquid mold sealant and preparation method thereof
[0001] CROSS-REFERENCE TO RELATED APPLICATIONS
[0002] This disclosure claims priority to Chinese patent application No. 2023104622775, filed on April 26, 2023, entitled “A liquid mold sealant and its preparation method,” the entire contents of which are incorporated herein by reference. Technical Field
[0003] The present disclosure relates to the field of semiconductor packaging technology, and in particular to a liquid molding compound and a preparation method thereof. Background Art
[0004] In recent years, demands for smaller, thinner, and more multifunctional IT equipment, such as mobile phones, have increased the need for higher-density mounting technology in semiconductor devices (semiconductor packages).
[0005] Fan-out wafer-level packaging (FOWLP) is a key enabler for the industry's transition from transistor scaling to system scaling and integration. The FOWLP process involves applying thermal release tape to a carrier wafer, then picking up a known good die (KGD) and placing it on the carrier. Molding then occurs, followed by substrate debonding, RDL redistribution bumping, and finally package dicing. However, the current thermal release tape removal process can easily leave adhesive residue on the carrier wafer.
[0006] Summary of the Invention
[0007] By utilizing one or more embodiments of the present disclosure, the technical problem in the prior art that residual adhesive easily occurs during the thermal tape stripping process is solved.
[0008] In a first aspect of the present disclosure, a liquid mold sealant is provided, comprising the following components, calculated by mass fraction: 83% to 88% filler, 6% to 9% epoxy resin, 6% to 9% curing agent, 0.1% to 0.2% colorant, 0.1% to 0.3% accelerator, and 0.3% to 0.6% paraffin oil.
[0009] In a second aspect of the present disclosure, a method for preparing the liquid mold sealant described in the first aspect is provided, comprising: obtaining the components of the liquid mold sealant; mixing the components of the liquid mold sealant and performing a dispersion treatment to obtain an intermediate product; and defoaming the intermediate product to obtain the liquid mold sealant. BRIEF DESCRIPTION OF THE DRAWINGS
[0010] In order to more clearly illustrate the technical solutions in the embodiments of the present disclosure, a brief introduction will be given below to the drawings required for use in the description of the embodiments. Obviously, the drawings described below are some embodiments of the present disclosure. For ordinary technicians in this field, other drawings can be obtained based on these drawings without any creative work.
[0011] FIG1 shows a flow chart of a method for preparing liquid molding compound according to some embodiments of the present disclosure. DETAILED DESCRIPTION
[0012] To make the objectives, technical solutions, and advantages of the embodiments of the present disclosure more clear, the technical solutions of the present disclosure will be clearly and completely described below in conjunction with the drawings in the embodiments of the present disclosure. Obviously, the described embodiments are part of the embodiments of the present disclosure, not all of the embodiments. Based on the embodiments of the present disclosure, all other embodiments obtained by ordinary technicians in this field without making any creative efforts shall fall within the scope of protection of the present disclosure.
[0013] Various embodiments of the present disclosure may be presented in the form of a range; it should be understood that the description in the form of a range is merely for convenience and brevity and should not be construed as a rigid limitation on the scope of the present disclosure; therefore, the range description should be considered to have specifically disclosed all possible sub-ranges and single numerical values within the range. For example, the range description from 1 to 6 should be considered to have specifically disclosed sub-ranges, such as from 1 to 3, from 1 to 4, from 1 to 5, from 2 to 4, from 2 to 6, from 3 to 6, etc., as well as single numbers within the range, such as 1, 2, 3, 4, 5 and 6, regardless of the range. In addition, whenever a numerical range is indicated in the present disclosure, it is intended to include any quoted number (fractional or integer) within the indicated range. Unless otherwise specified, the various raw materials, reagents, instruments and equipment used in the present disclosure can be purchased commercially or can be prepared by existing methods.
[0014] In the present disclosure, unless otherwise specified, the directional words used, such as "upper" and "lower", specifically refer to the directions of the drawings in the accompanying drawings. In addition, in the description of the present disclosure, the terms "including", "comprising", etc. mean "including but not limited to". In the present disclosure, relational terms such as "first" and "second" are merely used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply that there is any such actual relationship or order between these entities or operations. In the present disclosure, "and / or" describes the association relationship of associated objects, indicating that three relationships may exist. For example, A and / or B can mean: A exists alone, A and B exist at the same time, and B exists alone. Wherein A and B can be singular or plural. In the present disclosure, "at least one" refers to one or more, and "plurality" refers to two or more. "At least one", "at least one of the following" or similar expressions refer to any combination of these items, including any combination of single or plural items. For example, "at least one of a, b, or c", or "at least one of a, b, and c", can both mean: a, b, c, a~b (i.e., a and b), a~c, b~c, or a~b~c, where a, b, c can be single or multiple, respectively.
[0015] In a first aspect, the present disclosure provides a liquid mold sealant, comprising: the following components, calculated by mass fraction, 83% to 88% filler, 6% to 9% epoxy resin, 6% to 9% curing agent, 0.1% to 0.2% colorant, 0.1% to 0.3% accelerator, and 0.3% to 0.6% paraffin oil.
[0016] The above components can be prepared or purchased from the market. The functions of each component are as follows: the filler can be selected from silicon dioxide, which acts as an inorganic filler to reduce the material expansion coefficient and increase the material strength; the epoxy resin is used as the material matrix, and the naphthalene epoxy resin itself has greater rigidity. After curing, the epoxy resin has a larger storage modulus than other epoxy resins. The epoxy resin includes a polycyclic aromatic epoxy resin. Specifically, the polycyclic aromatic epoxy resin can be selected from at least one of dihydroanthracene epoxy resin and HP6000 (Nippon Kayaku); the curing agent reacts with the epoxy resin under a certain temperature and the action of an accelerator, and the system changes from a fluid state to a solid state. The curing agent includes an acid anhydride curing agent. Specifically, the acid anhydride curing agent can be selected from at least one of methyl-endimethylene tetrahydrophthalic anhydride (methyl nadic anhydride) and tetrahydrophthalic anhydride; the dye mainly plays a dyeing role, and the dye can be selected from carbon black; the accelerator is equivalent to a catalytic effect, which does not work at room temperature and can promote the reaction at a certain temperature. The accelerator includes an amine accelerator. Specifically, the amine accelerator can be selected from DBU and pyridine At least one of the following: paraffin oil does not participate in the reaction of other components, has a certain dilution effect, and at the same time, can be well dispersed in the system. It is easy to precipitate on the surface of the colloid at a certain temperature to form a barrier layer, thereby achieving peeling without residual glue.
[0017] In some embodiments, the liquid mold sealant includes: the following components, calculated by mass fraction, filler 84% to 87%, epoxy resin 7% to 8%, curing agent 7% to 8%, colorant 0.12% to 0.18%, accelerator 0.15% to 0.25%, and paraffin oil 0.4% to 0.5%.
[0018] In some embodiments, the liquid mold sealant includes: the following components, calculated by mass fraction, filler 85% to 86%, epoxy resin 7.3% to 7.7%, curing agent 7.3% to 7.7%, colorant 0.14% to 0.16%, accelerator 0.18% to 0.22%, and paraffin oil 0.43% to 0.47%.
[0019] As shown in FIG1 , in a second aspect, the present disclosure provides a method for preparing the liquid mold sealant described in the first aspect, the method comprising: S1. obtaining the components of the liquid mold sealant; S2. mixing the components of the liquid mold sealant and performing a dispersion treatment to obtain an intermediate product; S3. performing a defoaming treatment on the intermediate product to obtain the liquid mold sealant.
[0020] In S1, the liquid mold sealant comprises the following components, by mass: 83% to 88% filler, 6% to 9% epoxy resin, 6% to 9% curing agent, 0.1% to 0.2% colorant, 0.1% to 0.3% accelerator, and 0.3% to 0.6% paraffin oil. In S2, the components of the liquid mold sealant are added to a mixing cup and stirred in a centrifugal mixer for a suitable time until the system is initially mixed and uniformly distributed. The initially mixed material is then added to a three-roller drum for dispersion to obtain a uniformly dispersed intermediate product. The stirring time is 100 to 150 seconds, the rotation speed is 900 rpm, and the revolution speed is 1300 rpm. The feed gap of the three rollers is 100 to 200 μm, and the discharge gap is 200 to 400 μm. In S3, a centrifugal mixer is used to vacuum degas the uniformly dispersed intermediate product to obtain a liquid mold sealant; wherein, the centrifugal mixer has a vacuum degassing time of 60 to 100 seconds, a rotation speed of 100 r / min, and a revolution speed of 1200 r / min.
[0021] The present disclosure will be further described below with reference to specific examples. It should be understood that these examples are intended to illustrate the present disclosure only and are not intended to limit the scope of the present disclosure. Experimental methods in the following examples where specific conditions are not specified are generally measured in accordance with national standards. If no corresponding national standards are available, the methods were performed in accordance with commonly used international standards, conventional conditions, or conditions recommended by the manufacturer.
[0022] Example 1: A liquid mold sealant comprises, by mass fraction, 85.3% silicon dioxide, 7% dihydroanthracene epoxy resin, 7% methyl nadic anhydride, 0.1% carbon black, 0.2% DBU, and 0.4% paraffin oil.
[0023] Example 2: A liquid mold sealant comprises, by mass fraction, 85.1% silicon dioxide, 7% dihydroanthracene epoxy resin, 7% methyl nadic anhydride, 0.1% carbon black, 0.2% DBU, and 0.6% paraffin oil.
[0024] Example 3: A liquid mold sealant comprises, by mass fraction, 85.4% silicon dioxide, 7% dihydroanthracene epoxy resin, 7% methyl nadic anhydride, 0.1% carbon black, 0.2% DBU, and 0.3% paraffin oil.
[0025] Comparative Example 1: A liquid mold sealant comprising, by mass fraction, 85.7% silicon dioxide, 7% dihydroanthracene epoxy resin, 7% methyl nadic anhydride, 0.1% carbon black, and 0.2% DBU.
[0026] Comparative Example 2: A liquid mold sealant comprising, by mass fraction, 85.6% silicon dioxide, 7% dihydroanthracene epoxy resin, 7% methyl nadic anhydride, 0.1% carbon black, 0.2% DBU, and 0.1% paraffin oil.
[0027] Comparative Example 3: A liquid mold sealant comprising, by mass fraction, 85% silicon dioxide, 7% dihydroanthracene epoxy resin, 7% methyl nadic anhydride, 0.1% carbon black, 0.2% DBU, and 0.7% paraffin oil.
[0028] Comparative Example 4: A liquid mold sealant comprising, by mass fraction, 82% silicon dioxide, 12% dihydroanthracene epoxy resin, 5% methyl nadic anhydride, 0.1% carbon black, 0.2% DBU, and 0.7% paraffin oil.
[0029] Comparative Example 5: A liquid mold sealant, comprising, by mass fraction: 85.3% silicon dioxide, 7% dihydroanthracene epoxy resin, 7% methyl nadic anhydride, 0.1% carbon black, 0.2% DBU, and 0.4% glycerol.
[0030] The liquid molding sealants provided in Examples 1 to 3 and Comparative Examples 1 to 5 were used to package semiconductors, and the residual adhesive after the thermal tape was peeled off is shown in Table 1.
[0031] Table 1
[0032] In Table 1, grade A means that the adhesive residue occupies 100% of the wafer surface, grade B means that the adhesive residue occupies more than 50% of the wafer surface, grade C means that the adhesive residue occupies less than 50% of the wafer surface, and grade D means that there is no adhesive residue at all.
[0033] As shown in Table 1, when the liquid mold sealant provided by some embodiments of the present disclosure is used for semiconductor packaging, no residual glue will appear during the peeling process of the pyrolytic tape. A comparison of Comparative Example 1 with the embodiment shows that when no paraffin oil is added, a more serious residual glue situation will occur. A comparison of Comparative Examples 1 and 2 with the embodiment shows that when a small amount of paraffin oil is added, the residual glue situation will be improved to a certain extent, but residual glue still exists. Only when the addition amount reaches at least 0.2% can the residual glue situation be effectively eliminated. A comparison of Comparative Example 2 with the embodiment shows that when the addition amount of paraffin oil is greater than 0.6%, although residual glue will not appear during the peeling process, the pyrolytic tape will not be well bonded to the colloid before heating. A comparison of Comparative Example 4 with the embodiment shows that when the ratio of each component is not within the range of the present disclosure, the product cannot meet the physical property requirements of use. A comparison of Comparative Example 5 with the embodiment shows that using other substances such as glycerol to replace paraffin oil cannot improve the residual glue situation.
[0034] The above-mentioned technical solution provided by some embodiments of the present disclosure has the following advantages compared with the prior art: the liquid mold sealant, by adding paraffin oil, takes advantage of the fact that paraffin oil has low surface activity and does not participate in the reaction between epoxy resin and curing agent. Paraffin oil is easily compatible with epoxy resin, but is easily precipitated under heating conditions. The precipitated paraffin oil forms a spacer layer on the surface of the colloid and the pyrolytic tape. The paraffin oil in the spacer layer has almost no adhesion to the acrylic glue on the pyrolytic tape, so that the pyrolytic tape can be easily peeled off at a certain temperature, achieving the effect of no residual glue.
[0035] The foregoing description is merely a list of specific embodiments of the present disclosure to enable those skilled in the art to understand and implement the present disclosure. Various modifications to these embodiments will be readily apparent to those skilled in the art, and the general principles defined herein may be implemented in other embodiments without departing from the spirit or scope of the present disclosure. Therefore, the present disclosure is not limited to the embodiments shown herein, but is intended to be construed in the broadest manner consistent with the principles and novel features claimed herein.
Claims
1. A liquid mold sealant, comprising: The following ingredients, calculated by mass fraction, are filler 83% to 88%, epoxy resin 6% to 9%, curing agent 6% to 9%, colorant 0.1% to 0.2%, accelerator 0.1% to 0.3%, and paraffin oil 0.3% to 0.6%.
2. The liquid molding compound according to claim 1, wherein: The liquid mold sealant comprises the following components, measured by mass fraction, 84% to 87% of filler, 7% to 8% of epoxy resin, 7% to 8% of curing agent, 0.12% to 0.18% of dye, 0.15% to 0.25% of accelerator, and 0.4% to 0.5% of paraffin oil.
3. The liquid molding compound according to claim 2, wherein: The liquid mold sealant comprises the following components, measured by mass fraction, 85% to 86% of filler, 7.3% to 7.7% of epoxy resin, 7.3% to 7.7% of curing agent, 0.14% to 0.16% of dye, 0.18% to 0.22% of accelerator, and 0.43% to 0.47% of paraffin oil.
4. The liquid molding compound according to any one of claims 1 to 3, wherein: The viscosity of the paraffin oil is 300 cP to 700 cP.
5. The liquid molding compound according to any one of claims 1 to 3, wherein: The filler includes silicon dioxide.
6. The liquid molding compound according to any one of claims 1 to 3, wherein: The epoxy resin includes a polycyclic aromatic epoxy resin.
7. The liquid molding compound according to claim 6, wherein: The polycyclic aromatic epoxy resin includes at least one of dihydroanthracene epoxy resin and HP6000.
8. The liquid molding compound according to any one of claims 1 to 3, wherein: The curing agent includes at least one of methyl endomethylene tetrahydrophthalic anhydride and tetrahydrophthalic anhydride.
9. The liquid molding compound according to any one of claims 1 to 3, wherein: The promoter includes at least one of DBU and pyridine.
10. A method for preparing the liquid molding compound according to any one of claims 1 to 9, wherein: The method comprises: Obtaining the components of the liquid molding compound; Mixing the components of the liquid molding compound and dispersing them to obtain an intermediate product; and The intermediate product is subjected to defoaming treatment to obtain a liquid mold sealing adhesive.
Citation Information
Patent Citations
High-temperature movable label hot melt adhesive and preparation method thereof
CN113249066A
Liquid molding compound and preparation method thereof
CN115772374A
Thermosetting resin compositions
US5739184A