Crystalline polyoxyalkylene-based polymer and curable composition comprising same
The crystalline polyoxyalkylene polymer with reactive silicon groups addresses the weakness in elastic modulus and strength of conventional polymers, enhancing the mechanical properties of cured products in sealants and adhesives through a specialized curable composition.
Patent Information
- Application Number
- PCT/JP2024/008926
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-04-27
- Filing Date
- 2024-03-08
- Publication Date
- 2024-10-31
AI Technical Summary
Conventional polyoxyalkylene polymers with reactive silicon groups used in curable compositions often result in cured products with inadequate elastic modulus and strength, limiting their mechanical properties in applications such as sealants and adhesives.
Development of a crystalline polyoxyalkylene polymer with a reactive silicon group, specifically designed to enhance the elastic modulus and strength of the cured product, combined with a silanol condensation catalyst and optional amorphous polyoxyalkylene polymer, silane coupling agent, and (meth)acrylic acid ester polymer in a curable composition.
The crystalline polyoxyalkylene polymer significantly improves the elastic modulus and strength of the cured product, making it suitable for demanding applications like sealing and adhesion, while the curable composition ensures effective crosslinking and mechanical stability.
Smart Images

Figure JPOXMLDOC01-APPB-T000001
Abstract
Description
Crystalline polyoxyalkylene polymer and curable composition containing same
[0001] The present invention relates to a crystalline polyoxyalkylene polymer and a curable composition containing the same.
[0002] It is known that polymers containing at least one reactive silicon group in the molecule can produce rubber-like cured products. This is because the reactive silicon group is hydrolyzed by moisture to form a crosslinked network of siloxane bonds. This reaction proceeds even at room temperature.
[0003] Such polymer main chain structures include polyoxyalkylene, polyacrylic acid ester, polyisobutylene, etc. These polymers have already been produced industrially and are widely used in applications such as sealants, adhesives, paints, and waterproofing materials (see Patent Documents 1 to 4).
[0004] Among these, polymers whose main chain structure is polyoxyalkylene have a wide range of applications because they have a relatively low viscosity at room temperature, making them easy to handle, and the mechanical properties of the resulting cured products are good.
[0005] Japanese Patent Application Publication No. 52-073998 Japanese Patent Application Publication No. 63-006041 Japanese Patent Application Publication No. 55-009669 Japanese Patent Application Publication No. 2003-206410
[0006] However, the above-mentioned conventional techniques leave room for improvement in the modulus of elasticity and strength of the resulting cured product.
[0007] An object of one aspect of the present invention is to provide a polyoxyalkylene polymer that can provide a cured product having excellent elastic modulus and strength, and a curable composition containing the same.
[0008] The present inventors have conducted extensive research to solve the above problems, and as a result have found that the problems can be solved by making the polyoxyalkylene polymer having a reactive silicon group into a crystalline polymer.
[0009] The crystalline polyoxyalkylene polymer (A) according to one embodiment of the present invention has a reactive silicon group represented by general formula (1): —Si(R 1 ) 3-a (X) a (1) In the formula, R 1 each independently represents a hydrocarbon group having 1 to 20 carbon atoms which may have a substituent, the substituent may have a heteroatom, each X independently represents a hydroxyl group or a hydrolyzable group, and a is 1, 2 or 3.
[0010] A curable composition according to one aspect of the present invention contains a crystalline polyoxyalkylene polymer (A) and a silanol condensation catalyst (B).
[0011] According to one aspect of the present invention, there are provided a polyoxyalkylene polymer capable of providing a cured product excellent in elastic modulus and strength, and a curable composition containing the same.
[0012] An embodiment of the present invention will be described below, but the present invention is not limited to this embodiment.
[0013] [1. Crystalline Polyoxyalkylene Polymer (A)] [1.1. Structure and Properties of Crystalline Polyoxyalkylene Polymer (A)] The crystalline polyoxyalkylene polymer (A) according to one embodiment of the present invention has a reactive silicon group represented by general formula (1). The reactive silicon group is a functional group that forms a siloxane bond by a chemical reaction such as hydrolysis. -Si(R 1 ) 3-a (X) a (1)
[0014] In the formula, R 1 each independently represents a hydrocarbon group having 1 to 20 carbon atoms which may have a substituent. The substituent may have a heteroatom. Each X independently represents a hydroxyl group or a hydrolyzable group. a is 1, 2, or 3.
[0015] R 1 is a hydrocarbon group having 1 to 20 carbon atoms. 1The number of carbon atoms is preferably 1 to 12, more preferably 1 to 6, and even more preferably 1 to 4. The hydrocarbon group may be an unsubstituted hydrocarbon group or a hydrocarbon group having a substituent.
[0016] The substituent may have a heteroatom. The heteroatom refers to an atom of a type other than carbon atoms and hydrogen atoms. Suitable examples of heteroatoms include N, O, S, P, Si, and halogen atoms (F, Cl, Br, I, etc.). In this specification, a substituent having a heteroatom is referred to as a heteroatom-containing substituent. In the heteroatom-containing substituent, the total number of carbon atoms and heteroatoms is preferably 1 to 10, more preferably 1 to 6, and even more preferably 1 to 4.
[0017] Preferred examples of the heteroatom-containing substituent include a hydroxyl group, a mercapto group, a halogen atom (such as Cl, Br, I, or F), a nitro group, a cyano group, an alkoxy group (such as a methoxy group, an ethoxy group, an n-propyloxy group, or an isopropyloxy group), an alkylthio group (such as a methylthio group, an ethylthio group, an n-propylthio group, or an isopropylthio group), an acyl group (such as an acetyl group, a propionyl group, or a butanoyl group), an acyloxy group (such as an acetyloxy group, a propionyloxy group, or a butanoyloxy group), a substituted or unsubstituted amino group (such as an amino group, a methylamino group, an ethylamino group, a dimethylamino group, or a diethylamino group), and a substituted or unsubstituted aminocarbonyl group (such as an aminocarbonyl group, a methylaminocarbonyl group, an ethylaminocarbonyl group, a dimethylaminocarbonyl group, or a diethylaminocarbonyl group).
[0018] R 1 When R has a heteroatom-containing substituent, 1 The total number of carbon atoms and hetero atoms in the whole is preferably 2 to 30, more preferably 2 to 18, even more preferably 2 to 10, and particularly preferably 2 to 6.
[0019] R 1Specific examples of the alkyl group include alkyl groups (methyl, ethyl, n-propyl, isopropyl, n-butyl, isobutyl, sec-butyl, tert-butyl, n-pentyl, n-hexyl, n-heptyl, n-octyl, 2-ethyl-n-hexyl, n-nonyl, n-decyl, n-undecyl, n-dodecyl, n-tridecyl, n-tetradecyl, n-pentadecyl, n-hexadecyl, n-octadecyl, n-nonadecyl, and n-icosyl groups); alkenyl groups (vinyl cycloalkyl groups (cyclopropyl, cyclobutyl, cyclopentyl, cyclohexyl, cycloheptyl, cyclooctyl, etc.); aryl groups (phenyl, naphthalen-1-yl, naphthalen-2-yl, o-phenylphenyl, m-phenylphenyl, p-phenylphenyl, etc.); and aralkyl groups (benzyl, phenethyl, naphthalen-1-ylmethyl, naphthalen-2-ylmethyl, etc.).
[0020] Groups in which one or more hydrogen atoms contained in these hydrocarbon groups are substituted with the above-mentioned heteroatom-containing substituents are also included in R 1 It is preferable as.
[0021] R 1 Suitable examples of R include alkyl groups (e.g., methyl and ethyl groups); alkyl groups having a heteroatom-containing substituent (e.g., chloromethyl and methoxymethyl groups); cycloalkyl groups (e.g., cyclohexyl groups); aryl groups (e.g., phenyl groups); and aralkyl groups (e.g., benzyl groups). 1 are each independently selected from the group consisting of a methyl group, a methoxymethyl group, and a chloromethyl group. More preferably, R 1 are each independently selected from the group consisting of a methyl group and a methoxymethyl group. 1 is a methyl group.
[0022] a is 1, 2, or 3. Preferably, a is 2 or 3. A more preferably a is 3, since this improves the curability of the curable composition and the strength of the cured product.
[0023] X is a hydroxyl group or a hydrolyzable group. Examples of the hydrolyzable group include a halogen atom, an alkoxy group, an acyloxy group, a ketoximate group, an amino group, an amide group, an acid amide group, an aminooxy group, a mercapto group, and an alkenyloxy group. Among the above, an alkoxy group is preferred because it is mildly hydrolyzable and easy to handle. The alkoxy group is preferably independently selected from a methoxy group and an ethoxy group, and more preferably a methoxy group.
[0024] Specific examples of the reactive silicon group represented by formula (1) include trimethoxysilyl, triethoxysilyl, tris(2-propenyloxy)silyl, triacetoxysilyl, dimethoxymethylsilyl, diethoxymethylsilyl, dimethoxyethylsilyl, (chloromethyl)dimethoxysilyl, (chloromethyl)diethoxysilyl, (methoxymethyl)dimethoxysilyl, (methoxymethyl)diethoxysilyl, (N,N-diethylaminomethyl)dimethoxysilyl, and (N,N-diethylaminomethyl)diethoxysilyl. From the viewpoint of the mechanical properties of the cured product, dimethoxymethylsilyl, trimethoxysilyl, triethoxysilyl, and (methoxymethyl)dimethoxysilyl groups are preferred. From the viewpoint of the activity of the reactive silicon group, trimethoxysilyl, (chloromethyl)dimethoxysilyl, and (methoxymethyl)dimethoxysilyl groups are preferred, with trimethoxysilyl being more preferred.
[0025] The main chain of the crystalline polyoxyalkylene polymer (A) is -R 3 It has a repeating unit represented by —O—. 3 is a divalent branched alkylene group having 1 to 14 carbon atoms. 3 Specific examples of the repeating unit represented by -O- include -CH 2 CH (CH 3 ) O—, —CH 2 CH(C 2 H 5 ) O—, —CH 2 CH(CH=CH 2 ) O—, —CH 2 CH(C 6 H 5) O—, —CH 2 CH(C 6 H 4 CH 3 ) O—, —CH 2 CH (CH 2 F) O—, —CH 2 CH (CH 2 Cl)O—, —CH 2 CH (CH 2 Br)O—, —CH 2 CH (CH 2 OH)O-, -CH 2 CH (CH 2 O.C. 4 H 9 ) O—, —CH 2 CH (CH 2 O.C. 6 H 13 ) O—, —CH 2 CH (CH 2 OCH 2 CH=CH 2 ) O—, —CH 2 CH (CH 2 O.C. 6 H 5 ) O—, —CH 2 CH (CH 2 OCH 2 CH 2 Cl)O—, —CH 2 CH(C 6 H 4 Among the above, —CH 2 CH (CH 3 ) O—, —CH 2 CH(C 2 H 5 ) O— and —CH 2 CH(C 6 H 5 )O—, and —CH 2 CH (CH 3 )O— is more preferred. In one embodiment, the polyoxyalkylene polymer (A) is a polyoxypropylene polymer.
[0026] Among all the repeating units constituting the main chain of the crystalline polyoxyalkylene polymer (A), -R 3The proportion of repeating units represented by —O— is preferably 50% or more, more preferably 70% or more, and even more preferably 90% or more. 3 In one embodiment, the crystalline polyoxyalkylene polymer (A) may have two or more kinds of repeating units represented by —O—. 2 CH (CH 3 The proportion of repeat units represented by )O- can be 50% or more, 70% or more, or 90% or more.
[0027] The crystallinity of a polyoxyalkylene polymer is determined by the isotacticity of the main chain. Specifically, a polyoxyalkylene polymer with a high mm-triad content can be said to be crystalline (in this specification, the "m" in "mm-triad" stands for "meso"). When the polyoxyalkylene polymer is a polyoxypropylene polymer, the mm-triad content can be calculated by the method described in J. AM. CHEM. SOC., vol. 127, pp. 11566-11567 (2005).
[0028] The mm-triad content of the crystalline polyoxyalkylene polymer (A) is preferably 5% or more, more preferably 25% or more, even more preferably 50% or more, and particularly preferably 75% or more, from the viewpoint of the elastic modulus and strength of the cured product.
[0029] The isotactic structures of the crystalline polyoxyalkylene polymer (A) may be distributed anywhere in the main chain. The isotactic structures and atactic structures may be randomly distributed in the main chain. Alternatively, the isotactic structures and atactic structures may form blocks (isotactic structure-atactic structure-isotactic structure, atactic structure-isotactic structure-atactic structure, etc.). By forming blocks in this manner, the resulting cured product may exhibit better mechanical properties.
[0030] The main chain of the crystalline polyoxyalkylene polymer (A) may be linear or branched.
[0031] The number average molecular weight of the crystalline polyoxyalkylene polymer (A) is not particularly limited. The lower limit of the number average molecular weight is preferably 1,000 or more, more preferably 2,000 or more, and even more preferably 3,000 or more. The upper limit of the number average molecular weight is preferably 500,000 or less, more preferably 400,000 or less, and even more preferably 300,000 or less. The number average molecular weight of the crystalline polyoxyalkylene polymer (A) is determined as a polystyrene-equivalent molecular weight by GPC. When the number average molecular weight is within the above range, the polymer can be easily produced and the production cost is not excessively increased. Furthermore, when the number average molecular weight is within the above range, a cured product with high elastic modulus and strength can be obtained.
[0032] The molecular weight distribution (Mw / Mn) of the crystalline polyoxyalkylene polymer (A) is not particularly limited, but generally, a smaller value is considered preferable. The molecular weight distribution is preferably 3.5 or less, more preferably 3.0 or less, even more preferably 2.5 or less, and particularly preferably 2.0 or less.
[0033] The crystalline polyoxyalkylene polymer (A) may be used alone or in combination of two or more different types.
[0034] [1.2. Production method of crystalline polyoxyalkylene polymer (A)] Examples of methods for polymerizing the main chain of the crystalline polyoxyalkylene polymer (A) include those described in J. AM. CHEM. SOC., vol. 127, pp. 11566-11567 (2005), J. AM. CHEM. SOC., vol. 130, pp. 17658-17659 (2008), CHEM. REV., vol. 114, pp. 8129-8152 (2014), and J. AM. CHEM. SOC., vol. 139, pp. 11048-11054 (2017). If the terminal of the obtained crystalline polyoxyalkylene polymer is not a hydroxyl group, it is preferable to convert it to a hydroxyl group in order to introduce a reactive silicon group.
[0035] (Method 1 for Introducing Reactive Silicon Groups) Reactive silicon groups can be introduced by utilizing the terminal hydroxyl groups of a polyoxyalkylene polymer. For example, reactive silicon groups can be introduced by the following first process. 1. An alkali metal salt or double metal cyanide complex catalyst is reacted with a polyoxyalkylene polymer having a terminal hydroxyl group. This results in a polyoxyalkylene polymer having a terminal metaloxy group. 2. An electrophile having a carbon-carbon unsaturated bond is reacted with a polyoxyalkylene polymer having a terminal metaloxy group. This results in a polyoxyalkylene polymer having a terminal carbon-carbon unsaturated bond. 3. A reactive silicon group-containing compound that reacts with carbon-carbon unsaturated bonds is reacted with a polyoxyalkylene polymer having a terminal carbon-carbon unsaturated bond. This results in a polyoxyalkylene polymer having a terminal reactive silicon group.
[0036] The alkali metal salt in step 1 is not particularly limited. Examples of alkali metal salts include sodium hydroxide, sodium alkoxide, potassium hydroxide, potassium alkoxide, lithium hydroxide, lithium alkoxide, cesium hydroxide, and cesium alkoxide. Among the above, from the viewpoints of ease of handling and solubility, sodium hydroxide, sodium methoxide, sodium ethoxide, sodium tert-butoxide, potassium hydroxide, potassium methoxide, potassium ethoxide, and potassium tert-butoxide are preferred, with sodium methoxide and sodium tert-butoxide being more preferred. Furthermore, from the viewpoint of availability, sodium methoxide is preferred. An alkali metal salt dissolved in a solvent may be used in the reaction.
[0037] There is no particular limitation on the electrophilic agent having a carbon-carbon unsaturated bond in step 2. Examples of the electrophilic agent having a carbon-carbon unsaturated bond include organic halides having a carbon-carbon unsaturated bond and epoxy compounds having a carbon-carbon unsaturated bond.
[0038] An organic halide having a carbon-carbon unsaturated bond and a metaloxy group form an ether bond through a halogen substitution reaction, thereby introducing a carbon-carbon unsaturated bond into the terminal portion of the polyoxyalkylene polymer.
[0039] Specific examples of organic halides having a carbon-carbon unsaturated bond include vinyl chloride, allyl chloride, methallyl chloride, vinyl bromide, allyl bromide, methallyl bromide, vinyl iodide, allyl iodide, and methallyl iodide. Among these, allyl chloride and methallyl chloride are preferred because they are easy to handle. Furthermore, methallyl chloride, methallyl bromide, and methallyl iodide are preferred because they improve the average number of reactive silicon groups introduced relative to the number of terminals of the main chain of the polyoxyalkylene polymer.
[0040] The organic halide having a carbon-carbon unsaturated bond may be a halogenated hydrocarbon compound having a carbon-carbon triple bond. When such an electrophile is used in step 2, a polyoxyalkylene polymer having a terminal carbon-carbon triple bond is obtained. When a reactive silicon group is introduced into a polyoxyalkylene polymer having a terminal carbon-carbon triple bond, a polyoxyalkylene polymer having a carbon-carbon double bond adjacent to the reactive silicon group is obtained.
[0041] Examples of halogenated hydrocarbon compounds having a carbon-carbon triple bond include propargyl chloride, 1-chloro-2-butyne, 4-chloro-1-butyne, 1-chloro-2-octyne, 1-chloro-2-pentyne, 1,4-dichloro-2-butyne, 5-chloro-1-pentyne, 6-chloro-1-hexyne, propargyl bromide, 1-bromo-2-butyne, 4-bromo-1-butyne, 1-bromo-2-octyne, 1-bromo-2-pentyne, 1,4-dibromo-2-butyne, 5-bromo-1-pentyne, 6-bromo-1-hexyne, propargyl iodide, 1-iodo-2-butyne, 4-iodo-1-butyne, 1-iodo-2-octyne, 1-iodo-2-pentyne, 1,4-diiodo-2-butyne, 5-iodo-1-pentyne, and 6-iodo-1-hexyne. Of the above, propargyl chloride, propargyl bromide, and propargyl iodide are preferred.
[0042] As the organic halide having a carbon-carbon unsaturated bond, a halogenated hydrocarbon compound having a carbon-carbon triple bond and a halogenated hydrocarbon compound having a carbon-carbon double bond may be used in combination.
[0043] An epoxy compound having a carbon-carbon unsaturated bond and a metaloxy group form an ether bond through a ring-opening addition reaction of the epoxy group. This results in a polyoxyalkylene polymer having both a carbon-carbon unsaturated bond and a metaloxy group at its terminal portion. In the ring-opening addition reaction, by adjusting the amount of epoxy compound used relative to the metaloxy group or the reaction conditions, it is possible to add one or more epoxy compounds having one carbon-carbon unsaturated bond to one metaloxy group.
[0044] The epoxy compound having a carbon-carbon unsaturated bond is not particularly limited. From the viewpoint of reactivity, allyl glycidyl ether, methallyl glycidyl ether, glycidyl acrylate, glycidyl methacrylate, and butadiene monoxide are preferred, and allyl glycidyl ether is more preferred.
[0045] As described above, when a polyoxyalkylene polymer having a terminal metaloxy group is reacted with an epoxy compound having a carbon-carbon unsaturated bond, a metaloxy group is newly generated at the terminal of the polyoxyalkylene polymer. Therefore, after the reaction with the epoxy compound having a carbon-carbon unsaturated bond, the polyoxyalkylene polymer may be reacted with an organic halide having a carbon-carbon unsaturated bond.
[0046] In step 3, it is preferable to subject a polyoxyalkylene polymer having a terminal carbon-carbon unsaturated bond to a hydrosilane compound having a reactive silicon group through a hydrosilylation reaction. Advantages of using a hydrosilylation reaction include ease of implementation, ease of adjusting the amount of reactive silicon group introduced, and stable physical properties of the resulting polymer.
[0047] Specific examples of hydrosilane compounds having a reactive silicon group include halosilanes, alkoxysilanes, acyloxysilanes, ketoximate silanes, and isopropenyloxysilane (deacetone-containing). Examples of halosilanes include trichlorosilane, dichloromethylsilane, chlorodimethylsilane, dichlorophenylsilane, (chloromethyl)dichlorosilane, (dichloromethyl)dichlorosilane, bis(chloromethyl)chlorosilane, (methoxymethyl)dichlorosilane, (dimethoxymethyl)dichlorosilane, and bis(methoxymethyl)chlorosilane. Examples of alkoxysilanes include trimethoxysilane, triethoxysilane, dimethoxymethylsilane, diethoxymethylsilane, dimethoxyphenylsilane, ethyldimethoxysilane, methoxydimethylsilane, ethoxydimethylsilane, (chloromethyl)methylmethoxysilane, (chloromethyl)dimethoxysilane, (chloromethyl)diethoxysilane, bis(chloromethyl)methoxysilane, (methoxymethyl)methylmethoxysilane, (methoxymethyl)dimethoxysilane, bis(methoxymethyl)methoxysilane, (methoxymethyl)diethoxysilane, (ethoxymethyl)diethoxysilane, Examples of acyloxysilanes include diacetoxymethylsilane and diacetoxyphenylsilane. Examples of ketoximate silanes include bis(dimethylketoximate)methylsilane and bis(cyclohexylketoximate)methylsilane. Examples of acyloxysilanes include diacetoxymethylsilane and diacetoxyphenylsilane. Examples of ketoximate silanes include bis(dimethylketoximate)methylsilane and bis(cyclohexylketoximate)methylsilane.Examples of isopropenyloxysilanes (deacetone type) include triisopropenyloxysilane, (chloromethyl)diisopropenyloxysilane, and (methoxymethyl)diisopropenyloxysilane.
[0048] The hydrosilylation reaction in step 3 is preferably carried out in the presence of a hydrosilylation catalyst. Examples of hydrosilylation catalysts include metals such as cobalt, nickel, iridium, platinum, palladium, rhodium, and ruthenium, and complexes thereof. More specific examples include platinum supported on a support such as alumina, silica, or carbon black; chloroplatinic acid; chloroplatinic acid complexes composed of chloroplatinic acid and alcohols, aldehydes, or ketones; platinum-olefin complexes (Pt(CH 2 =CH 2 ) 2 (PPh 3 ), Pt(CH 2 =CH 2 ) 2 Cl 2 etc.); platinum-vinylsiloxane complexes (Pt{(vinyl)Me 2 SiOSiMe 2 (vinyl)}, Pt{Me(vinyl)SiO} 4 platinum-phosphine complexes (Ph(PPh etc.); 3 ) 4 , Pt(PBu 3 ) 4 etc.); platinum-phosphite complexes (Pt{P(OPh) 3} 4 From the viewpoint of reaction efficiency, platinum catalysts are preferred, and chloroplatinic acid and platinum-vinylsiloxane complexes are more preferred.
[0049] (Method 2 for Introducing Reactive Silicon Groups) The second process for introducing reactive silicon groups into the terminal hydroxyl groups of a crystalline polyoxyalkylene polymer is as follows: 1. A compound having both a reactive silicon group and an isocyanate group is allowed to act on a polyoxyalkylene polymer having a terminal hydroxyl group, thereby introducing the reactive silicon group via a urethane bond.
[0050] The compound having both a reactive silicon group and an isocyanate group is not particularly limited. Specific examples of such compounds include (3-isocyanatepropyl)trimethoxysilane, (3-isocyanatepropyl)dimethoxymethylsilane, (3-isocyanatepropyl)triethoxysilane, (3-isocyanatepropyl)diethoxymethylsilane, (isocyanatemethyl)trimethoxysilane, (isocyanatemethyl)triethoxysilane, (isocyanatemethyl)dimethoxymethylsilane, and (isocyanatemethyl)diethoxymethylsilane.
[0051] The urethanization reaction in step 1 may be carried out in the presence of a urethanization catalyst. Any conventionally known urethanization catalyst can be used (e.g., catalysts listed in Polyurethanes: Chemistry and Technology, Part I, Table 30, Chapter 4, Saunders and Frisch, Interscience Publishers, New York, 1963). Specific examples of such catalysts include organotin compounds, bismuth compounds, and base catalysts (e.g., organic amines).
[0052] (Method 3 for Introducing Reactive Silicon Groups) The third process for introducing reactive silicon groups into the terminal hydroxyl groups of a crystalline polyoxyalkylene polymer is as follows: 1. A polyoxyalkylene polymer having a terminal hydroxyl group is reacted with an excess amount of a polyisocyanate compound, thereby obtaining a polymer having an isocyanate group at its terminal. 2. A polymer having an isocyanate group at its terminal is reacted with a compound having both a group reactive with an isocyanate group (such as an amino group) and a reactive silicon group.
[0053] Examples of the polyisocyanate compound in step 1 include aliphatic polyisocyanates (aromatic polyisocyanates such as toluene (tolylene) diisocyanate, diphenylmethane diisocyanate, and xylylene diisocyanate; isophorone diisocyanate, and hexamethylene diisocyanate).
[0054] Examples of the compound having both a group reactive with an isocyanate group and a reactive silicon group in step 2 include amino group-containing silanes, hydroxy group-containing silanes, and mercapto group-containing silanes. Examples of amino group-containing silanes include γ-aminopropyltrimethoxysilane, γ-aminopropyldimethoxymethylsilane, γ-aminopropyltriethoxysilane, N-(β-aminoethyl)-γ-aminopropyltrimethoxysilane, N-(β-aminoethyl)-γ-aminopropyldimethoxymethylsilane, N-(β-aminoethyl)-γ-aminopropyltriethoxysilane, γ-(N-phenyl)aminopropyltrimethoxysilane, γ-(N-phenyl)aminopropyldimethoxymethylsilane, N-ethylaminoisobutyltrimethoxysilane, N-ethylaminoisobutyldimethoxymethylsilane, N-cyclohexylaminomethyltrimethoxysilane, and N-cyclohexylaminomethyldimethoxymethylsilane. Examples of hydroxy group-containing silanes include γ-hydroxypropyltrimethoxysilane and γ-hydroxypropyldimethoxymethylsilane. Examples of mercapto group-containing silanes include γ-mercaptopropyltrimethoxysilane and γ-mercaptopropyldimethoxymethylsilane.
[0055] (Method 4 for Introducing Reactive Silicon Groups) The fourth process for introducing reactive silicon groups into terminal hydroxyl groups of a crystalline polyoxyalkylene polymer is as follows: 1. An alkali metal salt or double metal cyanide complex catalyst is allowed to act on a polyoxyalkylene polymer having terminal hydroxyl groups, thereby obtaining a polyoxyalkylene polymer having terminal metaloxy groups. 2. An electrophile having a carbon-carbon unsaturated bond is allowed to act on a polyoxyalkylene polymer having terminal metaloxy groups, thereby obtaining a polyoxyalkylene polymer having terminal carbon-carbon unsaturated bonds. 3. A compound having both a mercaptan group and a reactive silicon group is allowed to act on a polyoxyalkylene polymer having terminal carbon-carbon unsaturated bonds, thereby introducing reactive silicon groups via sulfide bonds.
[0056] Steps 1 and 2 are as explained in (Method 1 for introducing reactive silicon groups).
[0057] Examples of the compound having both a mercaptan group and a reactive silicon group in step 3 include (3-mercaptopropyl)methyldimethoxysilane, (3-mercaptopropyl)trimethoxysilane, (3-mercaptopropyl)methyldiethoxysilane, (3-mercaptopropyl)triethoxysilane, (mercaptomethyl)methyldimethoxysilane, (mercaptomethyl)trimethoxysilane, (mercaptomethyl)methyldiethoxysilane, and (mercaptomethyl)triethoxysilane.
[0058] In step 3, the addition reaction of the mercaptan group to the carbon-carbon unsaturated bond may be carried out in the presence of a radical initiator. Conventionally known radical initiators can be used. Specific examples of radical initiators include azo initiators and peroxide initiators. In particular, catalysts with low activity toward reactive silicon groups are preferred, and from this perspective, azo initiators are preferred. Examples of azo initiators include 2,2'-azobis(isobutyronitrile) (AIBN), 2,2'-azobis(2-methylbutyronitrile) (V-59), and 2,2'-azobis(1-methylcyclohexanecarbonitrile) (V-40).
[0059] [2. Curable Composition] A curable composition according to one embodiment of the present invention comprises a crystalline polyoxyalkylene polymer (A) and a silanol condensation catalyst (B). The curable composition may further comprise, as an optional component, one or more components selected from the group consisting of an amorphous polyoxyalkylene polymer (C), a silane coupling agent (D), and a (meth)acrylic acid ester polymer (E) having a reactive silicon group. The crystalline polyoxyalkylene polymer (A) is as described in Section [1]. In this section, the other components will be described in detail.
[0060] [2.1. Silanol Condensation Catalyst (B)] Examples of the silanol condensation catalyst (B) include organotin compounds, metal carboxylates, amine compounds, carboxylic acids, alkoxy metals, and titanium compounds.
[0061] Examples of organotin compounds include dibutyltin dilaurate, dibutyltin dioctanoate, dibutyltin bis(butyl maleate), dibutyltin diacetate, dibutyltin oxide, dibutyltin bis(acetylacetonate), dioctyltin bis(acetylacetonate), dioctyltin dilaurate, dioctyltin distearate, dioctyltin diacetate, dioctyltin oxide, a reaction product of dibutyltin oxide with a silicate compound, a reaction product of dioctyltin oxide with a silicate compound, and a reaction product of dibutyltin oxide with a phthalate ester.
[0062] Examples of metal carboxylates include tin carboxylate, bismuth carboxylate, titanium carboxylate, zirconium carboxylate, iron carboxylate, potassium carboxylate, and calcium carboxylate. Examples of carboxylic acids contained in metal carboxylates include 2-ethylhexanoic acid, neodecanoic acid, oleic acid, and naphthenic acid. Examples of metals contained in metal carboxylates include tin, bismuth, iron, titanium, vanadium, calcium, potassium, barium, manganese, nickel, cobalt, and zirconium. Specific examples of metal carboxylates include iron 2-ethylhexanoate (divalent), iron 2-ethylhexanoate (trivalent), titanium 2-ethylhexanoate (tetravalent), vanadium 2-ethylhexanoate (trivalent), calcium 2-ethylhexanoate (divalent), potassium 2-ethylhexanoate (monovalent), barium 2-ethylhexanoate (divalent), manganese 2-ethylhexanoate (divalent), nickel 2-ethylhexanoate (divalent), cobalt 2-ethylhexanoate (divalent), zirconium 2-ethylhexanoate (tetravalent), iron neodecanoate (divalent), iron neodecanoate (trivalent), titanium neodecanoate (tetravalent), vanadium neodecanoate (trivalent), calcium neodecanoate (divalent), potassium neodecanoate (monovalent), barium neodec ... Examples of suitable oleic acids include zirconium decanoate (tetravalent), iron oleate (divalent), iron oleate (trivalent), titanium oleate (tetravalent), vanadium oleate (trivalent), calcium oleate (divalent), potassium oleate (monovalent), barium oleate (divalent), manganese oleate (divalent), nickel oleate (divalent), cobalt oleate (divalent), zirconium oleate (tetravalent), iron naphthenate (divalent), iron naphthenate (trivalent), titanium naphthenate (tetravalent), vanadium naphthenate (trivalent), calcium naphthenate (divalent), potassium naphthenate (monovalent), barium naphthenate (divalent), manganese naphthenate (divalent), nickel naphthenate (divalent), cobalt naphthenate (divalent), and zirconium naphthenate (tetravalent).
[0063] Examples of the amine compound include amines (octylamine, 2-ethylhexylamine, laurylamine, stearylamine, etc.); nitrogen-containing heterocyclic compounds (pyridine, 1,8-diazabicyclo[5,4,0]undecene-7 (DBU), 1,5-diazabicyclo[4,3,0]nonene-5 (DBN), etc.); guanidines (guanidine, phenylguanidine, diphenylguanidine, etc.); biguanides (butylbiguanide, 1-o-tolylbiguanide, 1-phenylbiguanide, etc.); amino group-containing silane coupling agents; and ketimine compounds.
[0064] Examples of carboxylic acids include acetic acid, propionic acid, butyric acid, 2-ethylhexanoic acid, lauric acid, stearic acid, oleic acid, linoleic acid, neodecanoic acid, and versatic acid.
[0065] Examples of alkoxy metals include aluminum compounds (such as aluminum tris(acetylacetonate) and diisopropoxyaluminum ethylacetoacetate) and zirconium compounds (such as zirconium tetrakis(acetylacetonate)).
[0066] Examples of titanium compounds include tetrabutyl titanate, tetrapropyl titanate, titanium tetrakis(acetylacetonate), bis(acetylacetonato)diisopropoxytitanium, and diisopropoxytitanium bis(ethylacetoacetate).
[0067] Examples of the silanol condensation catalyst (B) other than those mentioned above include fluorine anion-containing compounds, photoacid generators, photobase generators, and thermal base generators.
[0068] The silanol condensation catalyst (B) may be used alone or in combination of two or more different types.
[0069] The lower limit of the content of the silanol condensation catalyst (B) in the curable composition is preferably 0.001 parts by weight or more, more preferably 0.01 parts by weight or more, based on 100 parts by weight of the total content of the polymers having a hydrolyzable silyl group. The upper limit of the content of the silanol condensation catalyst (B) in the curable composition is preferably 20 parts by weight or less, more preferably 15 parts by weight or less, and even more preferably 10 parts by weight or less, based on 100 parts by weight of the total content of the polymers having a hydrolyzable silyl group. In one embodiment, the total content of the polymers having a hydrolyzable silyl group is the total content of the crystalline polyoxyalkylene polymer (A) and the optionally contained amorphous polyoxyalkylene polymer (C) and (meth)acrylic acid ester polymer (E). When a polymer having a hydrolyzable silyl group other than these is contained in the curable composition, the content of the polymer is also included in the total content of the polymers having a hydrolyzable silyl group.
[0070] [2.2. Amorphous Polyoxyalkylene Polymer (C)] The mm-triad content of the amorphous polyoxyalkylene polymer (C) is preferably less than 5%.
[0071] The amorphous polyoxyalkylene polymer (C) has a reactive silicon group represented by the general formula (2): —Si(R 2 ) 3-b (Y) b (2)
[0072] In the formula, R 2 each independently represents a hydrocarbon group having 1 to 20 carbon atoms which may have a substituent. The substituent may have a heteroatom. Each Y independently represents a hydroxyl group or a hydrolyzable group. b is 1, 2, or 3.
[0073] R 2 For an explanation of R in Section [1] 1 The explanation for X in section [1] is incorporated herein by reference. The explanation for Y is incorporated herein by reference. Y is preferably an alkoxy group, more preferably a methoxy group.
[0074] b is 1, 2, or 3. Preferably, b is 2 or 3. More preferably, b is 3, since the curability of the curable composition and the strength of the cured product are good.
[0075] Examples of the reactive silicon group represented by formula (2) include those exemplified for the crystalline polyoxyalkylene polymer (A). Specific examples include trimethoxysilyl, triethoxysilyl, tris(2-propenyloxy)silyl, triacetoxysilyl, dimethoxymethylsilyl, diethoxymethylsilyl, dimethoxyethylsilyl, (chloromethyl)dimethoxysilyl, (chloromethyl)diethoxysilyl, (methoxymethyl)dimethoxysilyl, (methoxymethyl)diethoxysilyl, (N,N-diethylaminomethyl)dimethoxysilyl, and (N,N-diethylaminomethyl)diethoxysilyl. From the viewpoint of the mechanical properties of the cured product, the dimethoxymethylsilyl, trimethoxysilyl, triethoxysilyl, and (methoxymethyl)dimethoxysilyl groups are preferred. From the viewpoint of the activity of the reactive silicon group, a trimethoxysilyl group, a (chloromethyl)dimethoxysilyl group, or a (methoxymethyl)dimethoxysilyl group is preferred, with a trimethoxysilyl group being more preferred.
[0076] The main chain of the amorphous polyoxyalkylene polymer (C) has a structure represented by —R 4 It has a repeating unit represented by —O—. 4 is a divalent functional group having 1 to 14 carbon atoms, and preferably a divalent functional group having 2 to 4 carbon atoms. 4 is preferably an alkylene group. The alkylene group may be linear or branched. 4 Specific examples of the repeating unit represented by -O- include -CH 2 O-, -CH 2 CH 2 O-, -CH 2 CH (CH 3 ) O—, —CH 2 C(CH 3 ) (CH 3 ) O—, —CH 2 CH 2 CH 2 CH 2Among the above, —CH 2 CH 2 O-, -CH 2 CH (CH 3 )O— is preferred, and —CH 2 CH (CH 3 )O— is more preferred. In one embodiment, the polyoxyalkylene polymer (C) is a polyoxypropylene polymer.
[0077] Among all the repeating units constituting the main chain of the amorphous polyoxyalkylene polymer (C), -R 3 The proportion of repeating units represented by —O— is preferably 50% or more, more preferably 70% or more, and even more preferably 90% or more. 3 In one embodiment, the amorphous polyoxyalkylene polymer (C) may have two or more kinds of repeating units represented by —O—. 2 CH (CH 3 The proportion of repeat units represented by )O- can be 50% or more, 70% or more, or 90% or more.
[0078] The main chain of the amorphous polyoxyalkylene polymer (C) may be linear or branched.
[0079] The number average molecular weight of the amorphous polyoxyalkylene polymer (C) is not particularly limited. The lower limit of the number average molecular weight is preferably 5,000 or more, more preferably 10,000 or more, even more preferably 12,000 or more, and particularly preferably 13,000 or more. The upper limit of the number average molecular weight is preferably 100,000 or less, more preferably 40,000 or less, even more preferably 25,000 or less, and particularly preferably 20,000 or less. The number average molecular weight of the amorphous polyoxyalkylene polymer (C) is determined as a polystyrene-equivalent molecular weight by GPC. When the number average molecular weight is within the above range, the polymer can be easily produced and the production cost is not excessively increased. Furthermore, when the number average molecular weight is within the above range, a cured product with high strength can be obtained.
[0080] The molecular weight distribution (Mw / Mn) of the amorphous polyoxyalkylene polymer (C) is not particularly limited, but is preferably narrow. The molecular weight distribution is preferably 1.6 or less, more preferably 1.4 or less, even more preferably 1.3 or less, and particularly preferably 1.2 or less. The number average molecular weight and weight average molecular weight of the amorphous polyoxyalkylene polymer (C) are determined as polystyrene-equivalent molecular weights by GPC.
[0081] (Method for producing amorphous polyoxyalkylene polymer (C)) The main chain of the amorphous polyoxyalkylene polymer (C) can be formed by a conventionally known method. For example, it can be formed by polymerizing an epoxy compound with an initiator having a hydroxyl group. This results in a polyoxyalkylene polymer having a hydroxyl group at its terminal. A polymerization method using a composite metal cyanide complex catalyst (such as a zinc hexacyanocobaltate glyme complex) is preferred because the molecular weight distribution (Mw / Mn) of the resulting polymer is narrow.
[0082] The initiator having a hydroxyl group is not particularly limited. Examples of initiators having a hydroxyl group include ethylene glycol, propylene glycol, glycerin, pentaerythritol, low molecular weight polyoxypropylene glycol, low molecular weight polyoxypropylene triol, butanol, allyl alcohol, methanol, ethanol, propanol, butanol, pentanol, hexanol, low molecular weight polyoxypropylene monoallyl ether, and low molecular weight polyoxypropylene monoalkyl ether. In order to obtain a polyoxyalkylene polymer (C) whose main chain is branched, an initiator having three or more hydroxyl groups may be used. Examples of such initiators include glycerin, pentaerythritol, and low molecular weight polyoxypropylene triol.
[0083] The epoxy compound is not particularly limited. Examples of the epoxy compound include alkylene oxides (ethylene oxide, propylene oxide, etc.) and glycidyl ethers (methyl glycidyl ether, butyl glycidyl ether, etc.). Preferably, the epoxy compound is propylene oxide.
[0084] The reactive silicon group can be introduced into the amorphous polyoxyalkylene polymer (C) by any of the methods described in Section [1] in connection with the crystalline polyoxyalkylene polymer (A). Among these, a preferred method involves subjecting a polyoxyalkylene polymer having a terminal carbon-carbon unsaturated bond to a hydrosilylation reaction with a hydrosilane compound having a reactive silicon group. Advantages of this method include its simplicity, ease of adjustment of the amount of reactive silicon group introduced, and stable physical properties of the resulting polymer.
[0085] The amorphous polyoxyalkylene polymer (C) may be a commercially available product, specific examples of which include SAT350, SAT400, S203H, S303H, EST280, SAX530, SAX580, SAX590, S810, S257, S258, S227, S327, MA452, and MA480 (all manufactured by Kaneka Corporation).
[0086] The amorphous polyoxyalkylene polymer (C) may be used alone or in combination of two or more different types.
[0087] The lower limit of the weight ratio ((A) / (C)) of the crystalline polyoxyalkylene polymer (A) to the amorphous polyoxyalkylene polymer (C) in the curable composition is preferably 1 / 99 or more, more preferably 10 / 90 or more, and even more preferably 20 / 80 or more. The upper limit of (A) / (C) is preferably 99 / 1 or less, more preferably 90 / 10 or less, and even more preferably 80 / 20 or less.
[0088] [2.3. Silane Coupling Agent (D)] Specific examples of the silane coupling agent (D) include amino group-containing silanes, isocyanate group-containing silanes, mercapto group-containing silanes, and epoxy group-containing silanes. Examples of amino group-containing silanes include γ-aminopropyltrimethoxysilane, γ-aminopropylmethyldimethoxysilane, N-β-aminoethyl-γ-aminopropyltrimethoxysilane, N-β-aminoethyl-γ-aminopropylmethyldimethoxysilane, N-phenyl-γ-aminopropyltrimethoxysilane, and (2-aminoethyl)aminomethyltrimethoxysilane. Examples of isocyanate group-containing silanes include γ-isocyanatepropyltrimethoxysilane, γ-isocyanatepropyltriethoxysilane, γ-isocyanatepropylmethyldimethoxysilane, α-isocyanatemethyltrimethoxysilane, and α-isocyanatemethyldimethoxymethylsilane. Examples of mercapto group-containing silanes include γ-mercaptopropyltrimethoxysilane, γ-mercaptopropyltriethoxysilane, and γ-mercaptopropylmethyldimethoxysilane.Examples of epoxy group-containing silanes include γ-glycidoxypropyltrimethoxysilane and β-(3,4-epoxycyclohexyl)ethyltrimethoxysilane.
[0089] As the silane coupling agent (D), a condensate or reaction product of the silane coupling agent (D) may be used. Examples of the condensate of the silane coupling agent (D) include a condensate of aminosilane and a condensate of aminosilane and another alkoxysilane. Examples of the reaction product of the silane coupling agent include a reaction product of aminosilane and epoxysilane, and a reaction product of aminosilane and a (meth)acrylic group-containing silane. Specific examples of such silane coupling agents (D) include Dynasylan 1146 and Dynasylan 1124 (EVONIK).
[0090] The silane coupling agent (D) may be used alone or in combination of two or more different types.
[0091] The lower limit of the content of the silane coupling agent (D) in the curable composition is preferably 0.1 parts by weight or more, more preferably 0.5 parts by weight or more, based on 100 parts by weight of the total content of the polymers having a hydrolyzable silyl group. The upper limit of the content of the silane coupling agent (D) in the curable composition is preferably 20 parts by weight or less, more preferably 10 parts by weight or less, based on 100 parts by weight of the total content of the polymers having a hydrolyzable silyl group. In one embodiment, the total content of the polymers having a hydrolyzable silyl group is the total content of the crystalline polyoxyalkylene polymer (A) and the optionally contained amorphous polyoxyalkylene polymer (C) and (meth)acrylic acid ester polymer (E). When a polymer having a hydrolyzable silyl group other than these is contained in the curable composition, the content of the polymer is also included in the total content of the polymers having a hydrolyzable silyl group.
[0092] [2.4. (Meth)acrylic acid ester polymer (E) having a reactive silicon group] The curable composition may further contain a (meth)acrylic acid ester polymer (E) having a reactive silicon group. In this specification, (meth)acrylic refers to acrylic and / or methacrylic. When the curable composition contains a (meth)acrylic acid ester polymer (E) having a reactive silicon group, the weather resistance of the cured product and the adhesion of the curable composition are improved.
[0093] The (meth)acrylic acid ester monomer constituting the main chain of the (meth)acrylic acid ester polymer (E) is not particularly limited. Specific examples of the monomer include methyl (meth)acrylate, ethyl (meth)acrylate, n-propyl (meth)acrylate, isopropyl (meth)acrylate, n-butyl (meth)acrylate, isobutyl (meth)acrylate, tert-butyl (meth)acrylate, n-pentyl (meth)acrylate, n-hexyl (meth)acrylate, cyclohexyl (meth)acrylate, n-heptyl (meth)acrylate, n-octyl (meth)acrylate, 2-ethylhexyl (meth)acrylate, Nonyl (meth)acrylate, decyl (meth)acrylate, dodecyl (meth)acrylate, phenyl (meth)acrylate, toluyl (meth)acrylate, benzyl (meth)acrylate, 2-methoxyethyl (meth)acrylate, 3-methoxybutyl (meth)acrylate, 2-hydroxyethyl (meth)acrylate, 2-hydroxypropyl (meth)acrylate, stearyl (meth)acrylate, glycidyl (meth)acrylate, (3-trimethoxysilyl)propyl (meth)acrylate, p) (3-dimethoxymethylsilyl)propyl acrylate, (2-trimethoxysilyl)ethyl (meth)acrylate, (2-dimethoxymethylsilyl)ethyl (meth)acrylate, trimethoxysilylmethyl (meth)acrylate, (dimethoxymethylsilyl)methyl (meth)acrylate, ethylene oxide adducts of (meth)acrylic acid, trifluoromethylmethyl (meth)acrylate, 2-trifluoromethylethyl (meth)acrylate, 2-perfluoroethylethyl (meth)acrylate, 2-perfluoroethyl-2-perfluorobutylethyl (meth)acrylate, perfluoroethyl (meth)acrylate, trifluoromethyl (meth)acrylate, bis(trifluoromethyl)methyl (meth)acrylate, 2-trifluoromethyl-2-perfluoroethylethyl (meth)acrylate, 2-perfluorohexylethyl (meth)acrylate, 2-perfluorodecylethyl (meth)acrylate, and 2-perfluorohexadecylethyl (meth)acrylate.
[0094] The main chain of the (meth)acrylic acid ester polymer (E) may have a repeating unit derived from a (meth)acrylic monomer other than a (meth)acrylic acid ester monomer. Examples of such a (meth)acrylic monomer include acrylic acid monomers (e.g., acrylic acid, methacrylic acid), monomers having an amide group (e.g., N-methylol acrylamide, N-methylol methacrylamide), monomers having an epoxy group (e.g., glycidyl acrylate, glycidyl methacrylate), and monomers having a nitrogen-containing group (e.g., diethylaminoethyl acrylate, diethylaminoethyl methacrylate).
[0095] The main chain of the (meth)acrylic acid ester polymer (E) may have a repeating unit derived from a vinyl monomer. The vinyl monomer is not particularly limited. Examples of the vinyl monomer include styrene monomers (styrene, vinyltoluene, α-methylstyrene, chlorostyrene, styrenesulfonic acid and its salts, etc.); fluorine-containing vinyl monomers (perfluoroethylene, perfluoropropylene, vinylidene fluoride, etc.); silicon-containing vinyl monomers (vinyltrimethoxysilane, vinyltriethoxysilane, etc.); maleic acid monomers (maleic anhydride, maleic acid, monoalkyl esters of maleic acid, dialkyl esters of maleic acid, etc.); fumaric acid monomers (fumaric acid, monoalkyl esters of fumaric acid, dialkyl esters of fumaric acid, etc.); maleimide monomers (maleimide, methylmaleimide, ethylenediamine diol ... Examples of the vinyl monomer include ethylmaleimide, propylmaleimide, butylmaleimide, hexylmaleimide, octylmaleimide, dodecylmaleimide, stearylmaleimide, phenylmaleimide, and cyclohexylmaleimide; vinyl monomers having a nitrile group (acrylonitrile, methacrylonitrile, and the like); vinyl monomers having an amide group (acrylamide, methacrylamide, and the like); vinyl ester monomers (vinyl acetate, vinyl propionate, vinyl pivalate, vinyl benzoate, vinyl cinnamate, and the like); alkenyl monomers (ethylene, propylene, and the like); conjugated diene monomers (butadiene, isoprene, and the like); vinyl chloride, vinylidene chloride, allyl chloride, and allyl alcohol. These vinyl monomers may be used alone or in combination of two or more different types.
[0096] From the viewpoint of the physical properties of the resulting polymer, the repeating units constituting the main chain of the (meth)acrylic acid ester polymer (E) are preferably one or more types selected from the group consisting of styrene-based monomers and (meth)acrylic acid-based monomers, more preferably one or more types selected from the group consisting of acrylic acid ester monomers and methacrylic acid ester monomers, and even more preferably one or more types selected from the group consisting of acrylic acid ester monomers.
[0097] Of all the repeating units constituting the main chain of the (meth)acrylic acid ester-based polymer (E), the proportion of repeating units derived from (meth)acrylic acid ester monomers is preferably 50% or more, more preferably 70% or more, and even more preferably 90% or more.
[0098] The lower limit of the number of reactive silicon groups contained in the (meth)acrylic acid ester polymer (E) is preferably 1.0 or more on average per molecule, and more preferably 1.27 or more from the viewpoint of the mechanical properties of the cured product. The upper limit of the number of reactive silicon groups is preferably 5.0 or less, and more preferably 3.0 or less from the viewpoint of the stability of the polymer.
[0099] The (meth)acrylic acid ester polymer (E) has a reactive silicon group represented by the general formula (3): —SiR 5 3-c Z c (3)
[0100] In the formula, R 5 each independently represents a hydrocarbon group having 1 to 20 carbon atoms. The substituent may have a heteroatom. Each Z independently represents a hydroxyl group or a hydrolyzable group. c is 1, 2, or 3.
[0101] R 5 is a hydrocarbon group having 1 to 20 carbon atoms. 5 The number of carbon atoms is preferably 1 to 12, more preferably 1 to 6, and even more preferably 1 to 4. The hydrocarbon group may be an unsubstituted hydrocarbon group or a hydrocarbon group having a substituent.
[0102] R 5Specific examples of the alkyl group include alkyl groups (methyl, ethyl, n-propyl, isopropyl, n-butyl, isobutyl, sec-butyl, tert-butyl, n-pentyl, n-hexyl, n-heptyl, n-octyl, 2-ethyl-n-hexyl, n-nonyl, n-decyl, n-undecyl, n-dodecyl, n-tridecyl, n-tetradecyl, n-pentadecyl, n-hexadecyl, n-octadecyl, n-nonadecyl, and n-icosyl groups); alkenyl groups (vinyl cycloalkyl groups (cyclopropyl, cyclobutyl, cyclopentyl, cyclohexyl, cycloheptyl, cyclooctyl, etc.); aryl groups (phenyl, naphthalen-1-yl, naphthalen-2-yl, o-phenylphenyl, m-phenylphenyl, p-phenylphenyl, etc.); and aralkyl groups (benzyl, phenethyl, naphthalen-1-ylmethyl, naphthalen-2-ylmethyl, etc.).
[0103] R 5 Suitable examples of R include alkyl groups (e.g., methyl and ethyl groups); alkyl groups having a heteroatom-containing substituent (e.g., chloromethyl and methoxymethyl groups); cycloalkyl groups (e.g., cyclohexyl groups); aryl groups (e.g., phenyl groups); and aralkyl groups (e.g., benzyl groups). 5 are each independently selected from the group consisting of a methyl group, a methoxymethyl group, and a chloromethyl group. More preferably, R 5 are each independently selected from the group consisting of a methyl group and a methoxymethyl group. 5 is a methyl group.
[0104] Z is a hydroxyl group or a hydrolyzable group. Examples of the hydrolyzable group include a halogen atom, an alkoxy group, an acyloxy group, a ketoximate group, an amino group, an amide group, an acid amide group, an aminooxy group, a mercapto group, and an alkenyloxy group. Among the above, an alkoxy group is preferred because it is mildly hydrolyzable and easy to handle. The alkoxy group is preferably independently selected from a methoxy group and an ethoxy group, and more preferably a methoxy group.
[0105] c is 1, 2 or 3. Preferably, c is 2 or 3.
[0106] Specific examples of the reactive silicon group represented by formula (3) include trimethoxysilyl, triethoxysilyl, tris(2-propenyloxy)silyl, triacetoxysilyl, dimethoxymethylsilyl, diethoxymethylsilyl, dimethoxyethylsilyl, (chloromethyl)dimethoxysilyl, (chloromethyl)diethoxysilyl, (methoxymethyl)dimethoxysilyl, (methoxymethyl)diethoxysilyl, (N,N-diethylaminomethyl)dimethoxysilyl, and (N,N-diethylaminomethyl)diethoxysilyl. From the viewpoint of the mechanical properties of the cured product, dimethoxymethylsilyl, trimethoxysilyl, triethoxysilyl, and (methoxymethyl)dimethoxysilyl groups are preferred. From the viewpoint of the activity of the reactive silicon group, trimethoxysilyl and (methoxymethyl)dimethoxysilyl groups are preferred, with trimethoxysilyl groups being more preferred.
[0107] The number average molecular weight of the (meth)acrylic acid ester polymer (E) is not particularly limited. The lower limit of the number average molecular weight is preferably 500 or more, more preferably 1,000 or more. The upper limit of the number average molecular weight is preferably 100,000 or less, more preferably 50,000 or less, and even more preferably 30,000 or less. The number average molecular weight of the (meth)acrylic acid ester polymer (E) is determined as a polystyrene-equivalent molecular weight by GPC.
[0108] The molecular weight distribution (Mw / Mn) of the (meth)acrylic acid ester polymer (E) is not particularly limited, but is preferably narrow. The molecular weight distribution is preferably 2.5 or less, more preferably 2.0 or less, even more preferably 1.5 or less, and particularly preferably 1.2 or less. The number average molecular weight and weight average molecular weight of the (meth)acrylic acid ester polymer (E) are determined as polystyrene-equivalent molecular weights by GPC.
[0109] The (meth)acrylic acid ester-based polymer (E) may be used alone or in combination of two or more different types.
[0110] (Method for Producing (Meth)acrylic Acid Ester Polymer (E)) There are no particular limitations on the method for introducing reactive silicon groups into the (meth)acrylic acid ester polymer (E). For example, the following methods 1 to 4 can be mentioned. Method 1: A method in which a compound having both a polymerizable unsaturated group and a reactive silicon group is copolymerized with the above-mentioned monomer. The (meth)acrylic acid ester polymer (E) obtained by this method has reactive silicon groups introduced randomly into its main chain. Method 2: A method in which a (meth)acrylic acid ester polymer is polymerized using a mercaptosilane compound having a reactive silicon group as a chain transfer agent. The (meth)acrylic acid ester polymer (E) obtained by this method has reactive silicon groups introduced at the end of its main chain. Method 3: A method in which a compound having both a polymerizable unsaturated group and a reactive functional group is copolymerized with the above-mentioned monomer. Then, a compound having both a functional group reactive with the reactive functional group and a reactive silicon group is reacted. A specific example of this method is copolymerizing the above-mentioned monomer with 2-hydroxyethyl acrylate, followed by reacting the hydroxyl groups in the main chain with an isocyanate silane having a reactive silicon group. Another specific example is copolymerizing the above-mentioned monomer with glycidyl acrylate, followed by reacting the epoxy groups in the main chain with an aminosilane compound having a reactive silicon group. ● Method 4: A method of modifying the terminal functional groups of a (meth)acrylic acid ester polymer synthesized by living radical polymerization to introduce reactive silicon groups. (Meth)acrylic acid ester polymers obtained by living radical polymerization are easily modified with functional groups at the polymer terminals. By modifying these terminal functional groups, reactive silicon groups can be introduced at the terminals of the main chain. This method produces polymers with narrow molecular weight distributions. The molecular weight distribution is preferably 1.6 or less, more preferably 1.4 or less, and even more preferably 1.2 or less. The number-average molecular weight and weight-average molecular weight of the (meth)acrylic acid ester polymer (E) are determined as polystyrene-equivalent molecular weights by GPC.
[0111] In Method 1, examples of the compound having both a polymerizable unsaturated group and a reactive silicon group include 3-(trimethoxysilyl)propyl (meth)acrylate, 3-(dimethoxymethylsilyl)propyl (meth)acrylate, 3-(triethoxysilyl)propyl (meth)acrylate, (trimethoxysilyl)methyl (meth)acrylate, (dimethoxymethylsilyl)methyl (meth)acrylate, (triethoxysilyl)methyl (meth)acrylate, (diethoxymethylsilyl)methyl (meth)acrylate, and 3-((methoxymethyl)dimethoxysilyl)propyl (meth)acrylate. From the viewpoint of availability, trimethoxysilylpropyl (meth)acrylate and (dimethoxymethylsilyl)propyl (meth)acrylate are preferred among the above.
[0112] In Method 2, examples of the mercaptosilane compound having a reactive silicon group include 3-mercaptopropyltrimethoxysilane, 3-mercaptopropyldimethoxymethylsilane, 3-mercaptopropyltriethoxysilane, mercaptomethyltrimethoxysilane, (mercaptomethyl)dimethoxymethylsilane, and mercaptomethyltriethoxysilane.
[0113] In Method 3, examples of the compound having both a polymerizable unsaturated group and a reactive functional group include isocyanate silane compounds (3-isocyanate propyl trimethoxy silane, 3-isocyanate propyl dimethoxy methyl silane, 3-isocyanate propyl triethoxy silane, isocyanate methyl trimethoxy silane, isocyanate methyl triethoxy silane, isocyanate methyl dimethoxy methyl silane, isocyanate methyl diethoxy methyl silane, etc.); epoxy silane compounds (3-glycidoxypropyl trimethoxy silane, 3-glycidoxypropyl triethoxy silane, 3-glycidoxypropyl dimethoxy methyl silane, glycidoxymethyl triethoxy methyl silane, etc.); trimethoxysilane, glycidoxymethyltriethoxysilane, glycidoxymethyldimethoxymethylsilane, glycidoxymethyldiethoxymethylsilane, etc.); aminosilane compounds (3-aminopropyltrimethoxysilane, 3-aminopropyltriethoxysilane, 3-aminopropyldimethoxymethylsilane, aminomethyltrimethoxysilane, aminomethyltriethoxysilane, aminomethyldimethoxymethylsilane, N-cyclohexylaminomethyltriethoxysilane, N-cyclohexylaminomethyldiethoxymethylsilane, N-phenylaminomethyltrimethoxysilane, (2-aminoethyl)aminomethyltrimethoxysilane, etc.).
[0114] Examples of modification reactions that can be used in Method 4 include the following: - A (meth)acrylic acid ester polymer having a terminal reactive group is obtained by polymerization. Next, a compound having both a functional group reactive with the terminal reactive group and a reactive silicon group is reacted. - A (meth)acrylic acid ester polymer having a terminal reactive group is obtained by polymerization. Next, a compound having both a functional group reactive with the terminal reactive group and a double bond is reacted. This introduces a double bond to the polymer terminal. Next, a reactive silicon group is introduced by a hydrosilylation reaction or the like.
[0115] Methods 1 to 4 may be combined in any manner. For example, by combining Method 2 and Method 3, a (meth)acrylic acid ester polymer (E) having reactive silicon groups both in the main chain and at the terminals can be obtained.
[0116] [2.5. Other Components] The curable composition may contain components other than those described above. Examples of such components include fillers, adhesion promoters, plasticizers, solvents, diluents, anti-sagging agents, antioxidants, light stabilizers, UV absorbers, physical property modifiers, tackifier resins, compounds having epoxy groups, photocurable substances, oxygen-curable substances, epoxy resins, and other resins. Furthermore, the curable composition may contain additives for adjusting the physical properties of the curable composition or the cured product. Examples of such additives include surface modifiers, foaming agents, curability modifiers, flame retardants, silicates, radical inhibitors, metal deactivators, antiozonants, phosphorus-based peroxide decomposers, lubricants, pigments, and mildew inhibitors.
[0117] Hereinafter, the total content of curable polymers refers to the total content of substances that are crosslinked and contribute to the formation of a cured product. The curable polymers include polymers having hydrolyzable silyl groups and other curable polymers (such as epoxy resins). In one embodiment, the total content of curable polymers is the total content of the crystalline polyoxyalkylene polymer (A) and the optionally contained amorphous polyoxyalkylene polymer (C), (meth)acrylic acid ester polymer (E), and epoxy resin.
[0118] (Filler) Examples of fillers include ground calcium carbonate, colloidal calcium carbonate, magnesium carbonate, diatomaceous earth, clay, talc, titanium oxide, fumed silica, precipitated silica, crystalline silica, fused silica, anhydrous silicic acid, hydrous silicic acid, carbon black, ferric oxide, fine aluminum powder, zinc oxide, activated zinc white, PVC powder, PMMA powder, glass fiber, and filament.
[0119] The content of the filler in the curable composition is preferably 1 to 600 parts by weight, more preferably 10 to 300 parts by weight, based on 100 parts by weight of the total content of the curable polymer. Only one type of filler may be used, or two or more different types may be used in combination.
[0120] To lower the specific gravity of the curable composition, organic or inorganic balloons may be blended as a filler. Balloons refer to hollow spherical fillers. Examples of balloon materials include inorganic materials (glass, shirasu, silica, etc.) and organic materials (phenolic resin, urea resin, polystyrene, saran, etc.).
[0121] The content of the balloons in the curable composition is preferably 0.1 to 100 parts by weight, more preferably 1 to 20 parts by weight, based on 100 parts by weight of the total content of the curable polymer. Only one type of balloon may be used, or two or more different types may be used in combination.
[0122] (Plasticizer) Examples of plasticizers include phthalate ester compounds (dibutyl phthalate, diisononyl phthalate (DINP), diheptyl phthalate, di(2-ethylhexyl) phthalate, diisodecyl phthalate (DIDP), butyl benzyl phthalate, etc.); terephthalate ester compounds (bis(2-ethylhexyl)-1,4-benzenedicarboxylate, etc.); and non-phthalate ester compounds (1,2-cyclohexanedicarboxylic acid diisononyl ester, etc.). Specific examples of products include Hexamol DINCH (BASF), etc.); aliphatic polycarboxylic acid ester compounds (dioctyl adipate, dioctyl sebacate, dibutyl sebacate, diisodecyl succinate, acetyl tributyl citrate, etc.); unsaturated fatty acid ester compounds (butyl oleate, methyl acetylricinoleate, etc.); alkylsulfonic acid phenyl esters (specific product examples include Mesamoll (LANXESS), etc.); phosphate ester compounds; trimellitic acid ester compounds; hydrocarbon oils (chlorinated paraffins, alkyl diphenyls, partially hydrogenated terphenyls, etc.); process oils; and epoxy plasticizers (epoxidized soybean oil, epoxy benzyl stearate, etc.).
[0123] The plasticizer may be a polymer plasticizer. Examples of the polymer plasticizer include vinyl polymers, polyester plasticizers, polyether polyols (such as polyethylene glycol and polypropylene glycol having a number average molecular weight of 500 or more), derivatives of polyether polyols in which the hydroxy groups are converted into ester groups, ether groups, or the like, polystyrenes, polybutadiene, polybutene, polyisobutylene, butadiene-acrylonitrile, and polychloroprene.
[0124] The content of the plasticizer in the curable composition is preferably 5 to 150 parts by weight, more preferably 10 to 120 parts by weight, and even more preferably 20 to 100 parts by weight, based on 100 parts by weight of the total content of the curable polymer. If the content is 5 parts by weight or more, the effect as a plasticizer can be expected to be sufficient. If the content is 150 parts by weight or less, sufficient mechanical strength can be imparted to the cured product. Only one type of plasticizer may be used, or two or more different types may be used in combination.
[0125] (Solvent and diluent) Examples of solvents and diluents include aliphatic hydrocarbons, aromatic hydrocarbons, alicyclic hydrocarbons, halogenated hydrocarbons, alcohols, esters, ketones, and ethers. In order to avoid polluting the surrounding air when the curable composition is used indoors, the boiling point of the solvent is preferably 150°C or higher, more preferably 200°C or higher, and particularly preferably 250°C or higher. Only one type of solvent and / or diluent may be used, or two or more different types may be used in combination.
[0126] (Anti-sagging agent) By blending an anti-sagging agent into the curable composition, sagging of the curable composition can be prevented and workability can be improved. Examples of the anti-sagging agent include polyamide waxes, hydrogenated castor oil derivatives, and metal soaps (calcium stearate, aluminum stearate, barium stearate, etc.).
[0127] The content of the anti-sagging agent in the curable composition is preferably 0.1 to 20 parts by weight, based on 100 parts by weight of the total content of the curable polymer. Only one type of anti-sagging agent may be used, or two or more different types may be used in combination.
[0128] (Antioxidant) By incorporating an antioxidant into the curable composition, the weather resistance of the cured product is improved. Examples of antioxidants include hindered phenols, monophenols, bisphenols, and polyphenols. Specific examples of products include BHT, Irganox 245, Irganox 1010, Irganox 1035, Irganox 1076, Irganox 1135, Irganox 1330, Irganox 1520, and SONGNOX 1076. In addition, a hindered amine light stabilizer may be incorporated as an antioxidant. Specific examples of products include Tinuvin 622LD, Tinuvin 144, Tinuvin 292, CHIMASSORB944LD, and CHIMASSORB119FL (all manufactured by BASF); ADK STAB LA-57, ADK STAB LA-62, ADK STAB LA-67, ADK STAB LA-63, and ADK STAB LA-68 (manufactured by ADEKA Corporation); SANOL LS-2626, SANOL LS-1114, and SANOL LS-744 (manufactured by Sankyo Lifetech Co., Ltd.); and NOCRAC CD (manufactured by Ouchi Shinko Chemical Industry Co., Ltd.). Further examples of antioxidant products include SONGNOX 4120, NOUGARD 445, and OKABEST CLX050.
[0129] Specific examples of antioxidants are also described in Japanese Patent Application Laid-Open Nos. 4-283259 and 9-194731.
[0130] The content of the antioxidant in the curable composition is preferably 0.1 to 10 parts by weight, more preferably 0.2 to 5 parts by weight, based on 100 parts by weight of the total content of the curable polymer. Only one type of antioxidant may be used, or two or more different types may be used in combination.
[0131] (Light Stabilizer) By blending a light stabilizer in the curable composition, photo-oxidative degradation of the cured product can be prevented. Examples of light stabilizers include benzotriazole-based, hindered amine-based, and benzoate-based. Among the above, hindered amine-based stabilizers are preferred. Specific examples of hindered amine light stabilizers include Tinuvin 123, Tinuvin 144, Tinuvin 249, Tinuvin 292, Tinuvin 312, Tinuvin 622LD, Tinuvin 765, Tinuvin 770, Tinuvin 880, Tinuvin 5866, Tinuvin B97, CHIMASSORB 119FL, and CHIMASSORB 944LD (all manufactured by BASF); ADK STAB LA-57, LA-62, LA-63, LA-67, and LA-68 (manufactured by ADEKA Corporation); SANOL LS-292, LS-2626, LS-765, LS-744, and LS-1114 (manufactured by Sankyo Lifetech Co., Ltd.); SABOSTAB UV91, SABOSTAB UV119, SONGSORB CS5100, and SONGSORB Examples include CS622, SONGSORB CS944 (both SONGWON), and Nocrac CD (Ouchi Shinko Chemical Industry Co., Ltd.).
[0132] The content of the light stabilizer in the curable composition is preferably 0.1 to 10 parts by weight, more preferably 0.2 to 5 parts by weight, based on 100 parts by weight of the total content of the curable polymer. Only one type of light stabilizer may be used, or two or more different types may be used in combination.
[0133] (UV absorber) By incorporating a UV absorber into the curable composition, the surface weather resistance of the cured product is improved. Examples of UV absorbers include benzophenone-based, benzotriazole-based, salicylate-based, triazine-based, substituted acrylonitrile-based, and metal chelate-based. Among these, benzotriazole-based are preferred. Specific examples of benzotriazole-based UV absorbers include Tinuvin 234, Tinuvin 326, Tinuvin 327, Tinuvin 328, Tinuvin 329, Tinuvin 350, Tinuvin 571, Tinuvin 900, Tinuvin 928, Tinuvin 1130, and Tinuvin 1600 (all manufactured by BASF); and SONGSORB 3290 (manufactured by SONGWON). Specific examples of triazine-based UV absorbers include Tinuvin 400, Tinuvin 405, Tinuvin 477, and Tinuvin 1577ED (all manufactured by BASF), and SONGSORB CS400 and SONGSORB 1577 (manufactured by SONGWON).Specific examples of benzophenone-based UV absorbers include SONGSORB 8100 (manufactured by SONGWON).
[0134] Alternatively, a product containing a mixture of antioxidants, light stabilizers, and UV absorbers may be used, such as Addworks IBC760 (Clariant).
[0135] The content of the ultraviolet absorber in the curable composition is preferably 0.1 to 10 parts by weight, more preferably 0.2 to 5 parts by weight, based on 100 parts by weight of the total content of the curable polymer. Only one type of ultraviolet absorber may be used, or two or more different types may be used in combination.
[0136] (Physical property modifier) By blending a physical property modifier with the curable composition, it becomes possible to adjust the tensile properties of the cured product, for example, by increasing the hardness of the cured product to improve tensile strength, or by decreasing the hardness to improve elongation at break.
[0137] Examples of the physical property adjuster include alkylalkoxysilanes (phenoxytrimethylsilane, methyltrimethoxysilane, dimethyldimethoxysilane, trimethylmethoxysilane, n-propyltrimethoxysilane, etc.); arylalkoxysilanes (diphenyldimethoxysilane, phenyltrimethoxysilane, etc.); alkylisopropenoxysilanes (dimethyldiisopropenoxysilane, methyltriisopropenoxysilane, γ-glycidoxypropylmethyldiisopropenoxysilane, etc.); trialkylsilylborates (tris(trimethylsilyl)borate, tris(triethylsilyl)borate, etc.); silicone varnish; and polysiloxanes.
[0138] In particular, compounds that generate monovalent silanol groups (preferably trimethylsilanol groups) upon hydrolysis can reduce the modulus of the cured product without increasing the stickiness of the surface of the cured product. Examples of such compounds include alcohol derivatives of silicone compounds (examples of alcohols include hexanol, octanol, phenol, trimethylolpropane, glycerin, pentaerythritol, and sorbitol). Specific examples include phenoxytrimethylsilane and tris((trimethylsiloxy)methyl)propane.
[0139] The content of the physical property adjuster in the curable composition is preferably 0.1 to 10 parts by weight, more preferably 0.5 to 5 parts by weight, based on 100 parts by weight of the total content of the curable polymer. Only one type of physical property adjuster may be used, or two or more different types may be used in combination.
[0140] (Tackifying Resin) By blending a tackifying resin into the curable composition, the adhesiveness and adhesion to the substrate are improved. Examples of tackifying resins include terpene resins, aromatic modified terpene resins, hydrogenated terpene resins, terpene-phenol resins, phenol resins, modified phenol resins, xylene-phenol resins, cyclopentadiene-phenol resins, coumarone-indene resins, rosin resins, rosin ester resins, hydrogenated rosin ester resins, xylene resins, low-molecular-weight polystyrene resins, styrene copolymer resins, styrene block copolymers and hydrogenated products thereof, petroleum resins (C5 hydrocarbon resins, C9 hydrocarbon resins, C5C9 hydrocarbon copolymer resins, etc.), hydrogenated petroleum resins, and DCPD resins.
[0141] The content of the tackifier resin in the curable composition is preferably 2 to 100 parts by weight, more preferably 5 to 50 parts by weight, and even more preferably 5 to 30 parts by weight, based on 100 parts by weight of the total content of the curable polymer. If the content is 2 parts by weight or more, sufficient adhesion and bonding effects to the substrate can be expected. If the content is 100 parts by weight or less, the viscosity of the curable composition does not become too high, making it easy to handle. Only one type of tackifier resin may be used, or two or more different types may be used in combination.
[0142] (Epoxy Group-Containing Compound) By incorporating an epoxy group-containing compound into the curable composition, the restoration properties of the cured product are improved. Examples of epoxy group-containing compounds include epoxidized unsaturated fats and oils, epoxidized unsaturated fatty acid esters, alicyclic epoxy compounds, epichlorohydrin derivatives, and mixtures thereof. More specific examples include epoxidized soybean oil, epoxidized linseed oil, bis(2-ethylhexyl)-4,5-epoxycyclohexane-1,2-dicarboxylate (E-PS), epoxy octyl stearate, and epoxy butyl stearate.
[0143] The content of the compound having an epoxy group in the curable composition is preferably 0.5 to 50 parts by weight, based on 100 parts by weight of the total content of the curable polymer. Only one type of compound having an epoxy group may be used, or two or more different types may be used in combination.
[0144] (Photocurable substance) By blending a photocurable substance into a curable composition, a film of the photocurable substance is formed on the surface of the cured product, which can reduce stickiness of the surface of the cured product and improve weather resistance. Known photocurable substances include organic monomers, oligomers, resins, and compositions containing them. Representative examples of photocurable substances include monomers, oligomers, or mixtures thereof having one or more (meth)acrylic unsaturated groups; polyvinyl cinnamate; and azido resins.
[0145] The content of the photocurable substance in the curable composition is preferably 0.1 to 20 parts by weight, more preferably 0.5 to 10 parts by weight, based on 100 parts by weight of the total content of the curable polymer. If the content is 0.1 part by weight or more, a sufficient effect of improving weather resistance can be expected. If the content is 20 parts by weight or less, the cured product does not become too hard, and cracking can be prevented. Only one type of photocurable substance may be used, or two or more different types may be used in combination.
[0146] (Oxygen-Curable Substance) An oxygen-curable substance is, for example, an unsaturated compound that can react with oxygen in the air. By incorporating an oxygen-curable substance into a curable composition, a film of the photo-curable substance is formed on the surface of the cured product, which reduces stickiness of the cured product surface and prevents adhesion of dirt and dust. Examples of oxygen-curable substances include drying oils (tung oil, linseed oil, etc.); alkyd resins obtained by modifying drying oils; acrylic polymers, epoxy resins, or silicone resins modified with drying oils; and liquid polymers obtained by polymerizing or copolymerizing diene compounds such as butadiene, chloroprene, isoprene, and 1,3-pentadiene (1,2-polybutadiene, 1,4-polybutadiene, polymers of C5 to C8 dienes, etc.).
[0147] The content of the oxygen-curable substance is preferably 0.1 to 20 parts by weight, more preferably 0.5 to 10 parts by weight, based on 100 parts by weight of the total content of the curable polymer. If the content is 0.1 part by weight or more, a sufficient effect of improving contamination can be expected. If the content is 20 parts by weight or less, the mechanical strength of the cured product is less likely to be impaired. Only one type of oxygen-curable substance may be used, or two or more different types may be used in combination. Furthermore, an oxygen-curable substance and a photo-curable substance may be used in combination (see, for example, JP-A-3-160053).
[0148] (Epoxy Resin) A curable composition containing an epoxy resin is particularly preferred as an adhesive (particularly an adhesive for exterior wall tiles). Examples of the epoxy resin include bisphenol A type epoxy resins and novolac type epoxy resins.
[0149] The contents of the epoxy resin, crystalline polyoxyalkylene polymer (A) and amorphous polyoxyalkylene polymer (C) are preferably in a range of a weight ratio such that the total content of the crystalline polyoxyalkylene polymer (A) and amorphous polyoxyalkylene polymer (C) / the content of the epoxy resin = (100 / 1) to (1 / 100). If the amount of epoxy resin is too small, it is difficult to obtain the effects of improving the impact strength and toughness inherent in the epoxy resin cured product. If the amount of epoxy resin is too large, the strength of the cured product tends to be insufficient.
[0150] When an epoxy resin is blended into the curable composition, the curable composition may further contain an epoxy resin curing agent for curing the epoxy resin. The epoxy resin curing agent is not particularly limited, and a commonly used epoxy resin curing agent can be used.
[0151] The content of the epoxy resin curing agent in the curable composition is preferably 0.1 to 300 parts by weight, based on 100 parts by weight of the epoxy resin content.
[0152] 3. Preparation and Use of Curable Compositions 3.1. Preparation of Curable Compositions The curable composition may be a one-component curable composition or a two-component curable composition. In a one-component curable composition, all components are blended as a single composition. A one-component curable composition is stored sealed before use and hardens after use due to moisture in the air. In a two-component curable composition, the components are blended separately into two compositions: a base agent and a curing agent. The curing agent contains components such as a curing catalyst, filler, plasticizer, and water. In a two-component curable composition, the base agent and curing agent are mixed before use. From the viewpoint of workability, a one-component curable composition is preferred.
[0153] In one-component curable compositions, all components are blended as a single composition. Therefore, it is preferable to dehydrate and dry components containing moisture before use, or to dehydrate them by reducing the pressure while kneading with other components. In addition, the inclusion of an alkoxysilane compound further improves the storage stability of the curable composition. Examples of alkoxysilane compounds include n-propyltrimethoxysilane, vinyltrimethoxysilane, phenyltrimethoxysilane, vinylmethyldimethoxysilane, γ-mercaptopropylmethyldimethoxysilane, γ-mercaptopropylmethyldiethoxysilane, and γ-glycidoxypropyltrimethoxysilane.
[0154] The content of the dehydrating agent (particularly a silicon compound capable of reacting with water, such as vinyltrimethoxysilane) is preferably 0.1 to 20 parts by weight, more preferably 0.5 to 10 parts by weight, based on 100 parts by weight of the total content of the curable polymer.
[0155] [3.2. Uses of Curable Composition] The curable composition can be used for pressure-sensitive adhesives, sealing materials for buildings, ships, automobiles, roads, etc., adhesives, waterproofing materials, waterproof coating materials, mold release agents, vibration-insulating materials, vibration-damping materials, sound-insulating materials, foam materials, paints, spray materials, etc. The cured product obtained by curing the curable composition according to one embodiment of the present invention has excellent flexibility and adhesiveness. Therefore, among the above-mentioned uses, it is more preferable to use it as a sealant or adhesive.
[0156] Further examples of applications of the curable composition include electrical and electronic component materials (such as solar cell backside sealing materials), electrical and electronic components (such as insulating coating materials for electric wires and cables), electrical insulating materials for devices, acoustic insulating materials, elastic adhesives, binders, contact adhesives, spray-type sealants, crack repair materials, tiling adhesives, adhesives for asphalt waterproofing materials, powder coatings, casting materials, medical rubber materials, medical adhesives, medical adhesive sheets, medical device sealants, dental impression materials, food packaging materials, and exterior materials (such as sizing boards). Examples of suitable applications include joint sealants for glass and laminated glass (such as glass panels), coatings, anti-slip coatings, buffer materials, primers, conductive materials for electromagnetic wave shielding, thermally conductive materials, hot melt materials, potting agents for electrical and electronic applications, films, gaskets, concrete reinforcement materials, temporary adhesives, molding materials, rust-preventing and waterproofing sealants for the edges (cut sections) of wired glass and laminated glass, and liquid sealants used in automobile parts, large vehicle parts (trucks, buses, etc.), train parts, aircraft parts, marine parts, electrical parts, and machine parts. Examples of applications for automobile parts include the bonding and attachment of plastic covers, trim, flanges, bumpers, windows, interior parts, exterior parts, and the like. Furthermore, when combined with a primer, the curable composition adheres to a variety of substrates, including glass, porcelain, wood, metal, and resin moldings. Therefore, it can also be used in various types of sealing or adhesive compositions.
[0157] Specific application examples of the curable composition as an adhesive or sealant include adhesives for interior panels, adhesives for exterior panels, tile adhesives, stone veneer adhesives, ceiling finishing adhesives, floor finishing adhesives, wall finishing adhesives, adhesives for vehicle panels, adhesives for assembling electrical, electronic, and precision equipment, adhesives for bonding leather, textile products, fabrics, paper, boards, and rubber, reactive post-crosslinking pressure-sensitive adhesives, sealants for direct glazing, sealants for double-glazing, sealants for SSG construction, sealants for working joints in buildings, and materials for civil engineering and bridges. Furthermore, the curable composition can also be used as an adhesive material such as an adhesive tape or adhesive sheet.
[0158] The present invention is not limited to the above-described embodiments, and various modifications are possible within the scope of the claims. Embodiments obtained by appropriately combining the technical means disclosed in different embodiments are also included in the technical scope of the present invention.
[0159] [4. Summary] The present invention includes the following aspects. <1> A crystalline polyoxyalkylene polymer (A) having a reactive silicon group represented by general formula (1): —Si(R 1 ) 3-a (X) a (1) In the formula, R 1 each independently represent a hydrocarbon group having 1 to 20 carbon atoms which may have a substituent, the substituent may have a heteroatom, each X independently represents a hydroxyl group or a hydrolyzable group, and a is 1, 2, or 3. <2> The crystalline polyoxyalkylene polymer (A) according to <1>, wherein X represents an alkoxy group. <3> The crystalline polyoxyalkylene polymer (A) according to <2>, wherein X represents a methoxy group. <4> The crystalline polyoxyalkylene polymer (A) according to any one of <1> to <3>, wherein the crystalline polyoxyalkylene polymer (A) is a polyoxypropylene polymer. <5> A curable composition comprising the crystalline polyoxyalkylene polymer (A) according to any one of <1> to <4>, and a silanol condensation catalyst (B). <6> The curable composition according to <5>, further comprising an amorphous polyoxyalkylene polymer (C) having a reactive silicon group represented by general formula (2): —Si(R 2 ) 3-b (Y) b (2) In the formula, R 2each independently represent a hydrocarbon group having 1 to 20 carbon atoms which may have a substituent, the substituent may have a heteroatom, each Y independently represents a hydroxyl group or a hydrolyzable group, and b is 1, 2, or 3. <7> The curable composition according to <6>, in which Y represents an alkoxy group. <8> The curable composition according to <7>, in which Y represents a methoxy group. <9> The curable composition according to any one of <6> to <8>, in which the amorphous polyoxyalkylene polymer (C) is a polyoxypropylene polymer. <10> The curable composition according to any one of <6> to <9>, in which the weight ratio ((A) / (C)) of the crystalline polyoxyalkylene polymer (A) to the amorphous polyoxyalkylene polymer (C) is 1 / 99 to 99 / 1. <11> The curable composition according to any one of <5> to <10>, further comprising a silane coupling agent (D). <12> A sealant comprising the curable composition according to any one of <5> to <10>. <13> An adhesive comprising the curable composition according to any one of <5> to <10>. <14> A cured product obtained by curing the curable composition according to any one of <5> to <10>.
[0160] An example of the present invention will be described below, but the present invention is not limited to the following example.
[0161] Synthesis Example 1: Synthesis of crystalline polyoxypropylene polymer A crystalline polyoxypropylene polymer having a reactive silicon group was synthesized by the following procedure. 1. The main chain of the crystalline polyoxypropylene polymer was synthesized by the method described in J. AM. CHEM. SOC., vol. 127, pp. 11566-11567 (2005). The peak top molecular weight of the obtained polymer was 59,000. The terminals of the obtained polymer were acetyl groups and hydroxyl groups. 1The reaction mixture was confirmed by H NMR. 2. Sodium ethoxide dissolved in ethanol was added to the obtained polymer, and the mixture was allowed to react for 2 hours. This reaction was carried out under vacuum at 130°C while removing volatile components. 3. The reaction solution was neutralized with aqueous hydrochloric acid and recrystallized in acetone. This resulted in a crystalline polyoxypropylene polymer having hydroxyl groups at the ends of its molecular chains. 4. 50 ppm of dibutyltin bis(isooctylmercaptopropionate) (Neostan U-360, Nitto Kasei Co., Ltd.) was added to the obtained polymer. 5. The reaction mixture was heated to 90°C, and (3-isocyanatopropyl)triethoxysilane (Tokyo Chemical Industry Co., Ltd.) was added dropwise. The mixture was allowed to react in this state for 5 hours. This resulted in a crystalline polyoxypropylene polymer having triethoxysilyl groups at the ends of its molecular chains. 1 The number of triethoxysilyl groups calculated from the H NMR spectrum was about 1.8 per molecule.
[0162] The peak top molecular weight in step 1 is a polystyrene-equivalent molecular weight measured by GPC. Specific measurement conditions are as follows: Liquid delivery system: HLC-8120GPC (Tosoh Corporation) Column: TSK-GEL H type (Tosoh Corporation) Solvent: chloroform
[0163] The mm-triad content of the obtained polyoxypropylene polymer was 99% or more. This indicates that a crystalline polyoxypropylene resin was obtained. The mm-triad content was determined by the method described in J. AM. CHEM. SOC., vol. 127, pp. 11566-11567 (2005), 13 Confirmed by C NMR.
[0164] Synthesis Example 2: Synthesis of Amorphous Polyoxypropylene Polymer An amorphous polyoxypropylene polymer having reactive silicon groups was synthesized according to the following procedure. 1. Propylene oxide was polymerized to obtain amorphous polypropylene oxide having hydroxyl groups at the ends of the molecular chain. A polyoxypropylene diol with a molecular weight of approximately 2,000 was used as the initiator. A zinc hexacyanocobaltate glyme complex was used as the catalyst. The number-average molecular weight of the resulting polymer was 14,500. 2. A methanol solution of NaOMe was added to the resulting polymer. The methanol was then distilled off. The amount of NaOMe added was 1.2 molar equivalents relative to the amount of hydroxyl groups in the polymer. 3. Allyl chloride was added to convert the terminal hydroxyl groups to allyl groups. Unreacted allyl chloride was then removed by devolatilization under reduced pressure. 4. 100 parts by weight of the crude polymer, 300 parts by weight of n-hexane, and 300 parts by weight of water were mixed and stirred. The water was then removed by centrifugation. 5. 300 parts by weight of water was mixed and stirred with the hexane solution of the obtained polymer. The water was then removed by centrifugation. The hexane was then removed by devolatilization under reduced pressure. In this manner, a polypropylene oxide-based polymer having an allyl group at the molecular end was obtained. The number-average molecular weight of this polymer was approximately 14,500. 6. The obtained polymer was reacted with methyldimethoxysilane at 90°C for 5 hours. In this manner, a polyoxypropylene-based polymer having methyldimethoxysilyl groups at the molecular chain end was obtained. The amount of methyldimethoxysilane added was 0.8 molar equivalents relative to the allyl groups contained in the polymer. A 2-propanol solution of platinum vinylsiloxane complex (platinum content: 3 wt%) was used as the catalyst. The amount of catalyst added was 150 ppm based on 100 parts by weight of the polymer used in the reaction. 1 The number of methyldimethoxysilyl groups calculated from the 1 H NMR spectrum was approximately 1.6 per molecule.
[0165] The number average molecular weight in step 1 is a polystyrene-equivalent molecular weight measured by GPC. Specific measurement conditions are as follows: Liquid delivery system: HLC-8120GPC (Tosoh Corporation) Column: TSK-GEL H type (Tosoh Corporation) Solvent: Tetrahydrofuran
[0166] The mm-triad content of the obtained polyoxypropylene polymer was less than 5%, which proves that an amorphous polyoxypropylene resin was indeed obtained.
[0167] Example 1 A cured product was prepared according to the following procedure. 1. A crystalline polyoxypropylene polymer and an amorphous polyoxypropylene polymer were added to a mayonnaise jar. Both of these polyoxypropylene polymers contained reactive silicon groups. 2. 100 parts by weight of tetrahydrofuran was added to a total of 100 parts by weight of polyoxypropylene polymers. The mixture was then mixed while heating in a 70°C oven. 3. The mixture was removed from the oven, and a silanol condensation catalyst and water were added. The mixture was then stirred with a spatula, and the curable composition was poured into a mold. Dibutyltin dilaurate (Neostan U-100, Nitto Kasei Co., Ltd.) was used as the silanol condensation catalyst. 4. The tetrahydrofuran was evaporated in a 50°C oven. The mixture was then cured at 70°C for 20 to 33 hours. In this manner, a cured product was obtained.
[0168] Comparative Example 1 A cured product was produced by the following procedure. 1. A silanol condensation catalyst and water were added to an amorphous polyoxyalkylene polymer, and the mixture was stirred and poured into a mold. Dibutyltin dilaurate (Neostan U-100, Nitto Kasei Co., Ltd.) was used as the silanol condensation catalyst. 2. The mixture was aged for one week at a constant temperature and humidity of 23°C and 55%. In this way, a cured product was obtained.
[0169] Comparative Example 2 In Example 1, the crystalline polyoxypropylene polymer used was changed to a crystalline polyoxypropylene polymer having no reactive silicon group. Specifically, the crystalline polyoxypropylene polymer was changed to the crystalline polyoxypropylene polymer obtained in Step 2 of Synthesis Example 1. A cured product was obtained in the same manner as in Example 1 except for the above.
[0170] [Method for measuring mechanical properties of cured product] From the obtained sheet-like cured product (thickness: approximately 1 mm), No. 3 dumbbell-shaped test pieces as specified in JIS K 7113 were punched out. These test pieces were subjected to a tensile test to measure their mechanical properties. Specifically, the elastic modulus (stress at 50% elongation, stress at 100% elongation, stress at break) and elongation at break (elongation relative to the distance between chucks before the test) were measured. The results are shown in Table 1. The measurement conditions were as follows: an autograph (AG-2000A, Shimadzu Corporation), a measurement temperature of 23°C, and a tensile speed of 500 mm / min.
[0171] [Results] The results are shown in Table 1.
[0172] The cured product of Example 1 was obtained by curing a curable composition containing a crystalline polyoxyalkylene polymer having a reactive silicon group. The cured product of Comparative Example 1 was obtained by curing a curable composition not containing a crystalline polyoxyalkylene polymer. The cured product of Comparative Example 2 was obtained by curing a curable composition containing a crystalline polyoxyalkylene polymer not having a reactive silicon group.
[0173] Comparing the results of Example 1 and Comparative Example 1, the cured product of Example 1 had higher stresses at 50% elongation and 100% elongation than the cured product of Comparative Example 1, and was therefore stronger at the same elongation. Furthermore, the cured product of Example 1 had a higher stress at break than the cured product of Comparative Example 1, and required a large force to break. This suggests that the addition of a crystalline polyoxyalkylene polymer improves the modulus of elasticity and strength of the cured product.
[0174] A comparison of the results of Example 1 and Comparative Example 1 suggests that the effect of incorporating a crystalline polyoxyalkylene polymer is exerted by the fact that the crystalline polyoxyalkylene polymer has a reactive silicon group.
[0175] The curable composition according to one embodiment of the present invention can be used as a sealant, adhesive, or the like.
Claims
1. A crystalline polyoxyalkylene polymer (A) having a reactive silicon group represented by the general formula (1): -Si(R 1 ) 3-a (X) a (1) In the formula, R 1 each independently represents a hydrocarbon group having 1 to 20 carbon atoms which may have a substituent, the substituent may have a heteroatom, each X independently represents a hydroxyl group or a hydrolyzable group, and a is 1, 2 or 3.
2. The crystalline polyoxyalkylene polymer (A) according to claim 1, wherein the X is an alkoxy group.
3. The crystalline polyoxyalkylene polymer (A) according to claim 2, wherein the X is a methoxy group.
4. The crystalline polyoxyalkylene polymer (A) according to claim 1, wherein the crystalline polyoxyalkylene polymer (A) is a polyoxypropylene polymer.
5. A curable composition comprising the crystalline polyoxyalkylene polymer (A) according to claim 1 and a silanol condensation catalyst (B).
6. The curable composition according to claim 5, further comprising an amorphous polyoxyalkylene polymer (C) having a reactive silicon group represented by general formula (2): -Si(R 2 ) 3-b (Y) b (2) In the formula, R 2 each independently represents a hydrocarbon group having 1 to 20 carbon atoms which may have a substituent, the substituent may have a heteroatom, each Y independently represents a hydroxyl group or a hydrolyzable group, and b is 1, 2 or 3.
7. The curable composition according to claim 6, wherein Y is an alkoxy group.
8. The curable composition according to claim 7, wherein Y is a methoxy group.
9. The curable composition according to claim 6, wherein the amorphous polyoxyalkylene polymer (C) is a polyoxypropylene polymer.
10. The curable composition according to claim 6, wherein the weight ratio ((A) / (C)) of the crystalline polyoxyalkylene polymer (A) to the amorphous polyoxyalkylene polymer (C) is 1 / 99 to 99 / 1.
11. The curable composition according to claim 5 or 6, further comprising a silane coupling agent (D).
12. A sealant comprising the curable composition according to claim 5 or 6.
13. An adhesive comprising the curable composition according to claim 5 or 6.
14. A cured product obtained by curing the curable composition according to claim 5 or 6.
Citation Information
Patent Citations
Room temperature-curable composition
JP1991160053A
Curable composition
JP1992283259A
Curable composition
JP1997194731A
Curable composition
JP2003206410A
Information processing apparatus, information processing system, information processing method, and information processing program
JP2025073998A