Cosmetic, method for producing same, and ultraviolet shielding agent composition
The integration of BMBM into an organic-inorganic composite UV absorber within a layered double hydroxide, combined with specific surfactants, addresses solubility and stability issues in sunscreens, achieving high UV-A protection and reduced metal ion-induced coloring, ensuring effective and safe sunscreen performance.
Patent Information
- Application Number
- PCT/JP2024/015055
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-04-27
- Filing Date
- 2024-04-16
- Publication Date
- 2024-10-31
AI Technical Summary
Current UV protection agents like 4-tert-butyl-4'-methoxydibenzoylmethane (BMBM) have low solubility in cosmetic oils, leading to precipitation and reaction with inorganic powders and metal ions, resulting in coloring issues and reduced UV-A protection efficacy in sunscreens.
An organic-inorganic composite UV absorber is developed, where BMBM is integrated into a layered double hydroxide with a negatively charged intermediate layer, combined with a polyhydric alcohol fatty acid ester type nonionic surfactant and a UV protection ability improver like phosphoric acid or silicone surfactant, enhancing UV-A protection and stability in cosmetic formulations.
The solution provides high UV-A protection, reduces metal ion-induced coloring, and improves safety by maintaining BMBM's effectiveness and stability within the cosmetic, allowing for efficient production of sunscreens with enhanced UV protection.
Smart Images

Figure JPOXMLDOC01-APPB-T000001 
Figure JPOXMLDOC01-APPB-T000002 
Figure JPOXMLDOC01-APPB-T000003
Abstract
Description
Cosmetics, their production method, and ultraviolet protection composition
[0001] The present invention relates to a cosmetic having a high ultraviolet protection effect, a method for producing the same, and an ultraviolet protection agent composition suitable for producing the cosmetic.
[0002] Among the ultraviolet rays that adversely affect the human body, 4-tert-butyl-4'-methoxydibenzoylmethane (cosmetic labeling name: t-butylmethoxydibenzoylmethane, sometimes abbreviated as "BMBM" in this specification) is widely used as an organic ultraviolet absorber for protecting against long-wavelength ultraviolet rays (UV-A) with wavelengths of 320 to 400 nm, due to its excellent UV-A absorbing ability. However, BMBM has low solubility in oils commonly used in cosmetics, making it difficult to incorporate it at high concentrations, and even when dissolved, it has the problem of being prone to crystallization over time, and also has the problem of being prone to discoloration due to reaction with inorganic powders blended into cosmetics and metal ions derived from manufacturing equipment.
[0003] Therefore, development of new UV absorbers that overcome the drawbacks of BMBM has been underway. For example, Patent Document 1 discloses a new UV absorber, an organic-inorganic composite UV absorber, in which the interlayer water in the intermediate layer of a hydrotalcite, a layered double hydroxide consisting of a positively charged base layer and a negatively charged intermediate layer, is replaced with a polar, nonionic organic UV absorber (e.g., BMBM) (see claims 1 and 6). The document also states that this organic-inorganic composite UV absorber protects the organic UV absorber from light and prevents contact of the organic UV absorber with transition metals or skin because the organic UV absorber is confined within the layered crystals of the hydrotalcite (see paragraph 0006). It also discloses that this organic-inorganic composite UV absorber can be used in cosmetics (see claim 9). However, it does not disclose specific examples of cosmetics that use this organic-inorganic composite UV absorber, nor does it disclose any embodiments for use in cosmetics. As described above, the organic-inorganic composite ultraviolet absorber described in Patent Document 1 has excellent UV-A protection capabilities, but in recent years, there has been a demand in the market for the development of sunscreen cosmetics with even higher performance.
[0004] Japanese Patent Application Laid-Open No. 2021-161367
[0005] The present invention was completed against this background technology, and its main object is to provide a cosmetic preparation that has a high sunscreen effect, particularly a high protection effect against ultraviolet A rays (UV-A), is minimally colored, and is highly safe. Another object is to provide a method for efficiently producing the cosmetic preparation, and a still further object is to provide an ultraviolet protection agent composition that is suitable for producing the cosmetic preparation.
[0006] As a result of intensive research to solve the above-mentioned problems, the present inventors have found that, in the case of the organic-inorganic composite ultraviolet absorbers described in Patent Document 1, which contain BMBM as an ultraviolet absorber in an intermediate layer, it is useful to have a specific compound coexist when dispersing the organic-inorganic composite ultraviolet absorber in an oil phase, and have thus completed the present invention.
[0007] Thus, according to the present invention, as a first invention, there is provided a cosmetic comprising, as an oil phase component, an ultraviolet protection agent (A) consisting of a layered double hydroxide having a positively charged base layer composed of divalent metal ions, trivalent metal ions, and hydroxide ions, and a negatively charged intermediate layer between the two base layers, the layered double hydroxide containing organic acid ions and BMBM, and a liquid oil (C) containing at least one ultraviolet protection enhancer (B) selected from the group consisting of polyhydric alcohol fatty acid ester-type nonionic surfactants, polyoxyethylene alkyl ether phosphates or salts thereof, silicone surfactants, polyhydroxy fatty acids, clay minerals, and silica. Also provided is a method for producing the above cosmetic, which comprises the step of mixing components (A), (B), and (C) to prepare an oil-based dispersion. Also provided is a UV protection composition comprising components (A), (B), and (C).
[0008] The cosmetic of the present invention has a high sun protection effect, particularly UV-A protection effect, is less discolored by metal ions, and is also excellent in safety because the possibility of BMBM coming into contact with the skin is reduced. Furthermore, the production method and ultraviolet protection ability improver of the present invention enable the above-mentioned cosmetic to be produced efficiently.
[0009] The cosmetic of the present invention contains, as essential components, an organic-inorganic composite (A), an ultraviolet protection enhancer (B), and a liquid oil (C). Each component will be described in detail below.
[0010] (A: Organic-inorganic composite) The organic-inorganic composite used as component (A) of the present invention is a layered double hydroxide having a positively charged base layer composed of divalent metal ions, trivalent metal ions, and hydroxide ions, and a negatively charged intermediate layer present between the two base layers and containing organic acid ions and BMBM.
[0011] A typical example of layered double hydroxide is hydrotalcite, a type of clay mineral, and the typical composition formula of hydrotalcite is Mg 6 Al 2 (OH) 16 CO3 ・4H 2 Hydrotalcite has a layered crystal structure similar to talc and smectite, and a metal double hydroxide with a regular octahedral structure, in which part of the Mg in magnesium hydroxide is replaced with Al, forms a positively charged base layer (also called a host layer), and CO, which electrically neutralizes the charge, is formed. 3 It is known that ions form an intermediate layer (also called a guest layer), and that the intermediate layer contains water molecules, which are called interlayer water.
[0012] In such hydrotalcite, Mg is replaced with other divalent metals, Al is replaced with other trivalent metals, the ratio of the two is changed, or CO 3 Many layered double hydroxides (sometimes called "hydrotalcite-like compounds") that have a structure similar to hydrotalcite, in which ions are substituted with other anions, are also known, and these are usually represented by the composition formula (1) below. 2+ ) 1-x (M 3+ ) x (OH) 2 ][(A n- ) x / n ・(H 2 O) m ]...(1) (M in the formula 2+ is a divalent metal ion, M 3+ is a trivalent metal ion, A n- represents an n-valent anion, n is an integer of 1 to 6, x is a number in the range of 0.1<x<0.5, and m is a number greater than 0.) Examples of divalent metal ions include Mg 2+ , Zn 2+ , Ca 2+ , Mn 2+ , Ni 2+ , Co 2+ and the like, and preferably Mg 2+ and Zn 2+ The trivalent metal ions are at least one of Fe, 3+ , Al 3+ , Ga 3+ .Cr 3+ , La 3+ , In 3+and the like, and preferably Al 3+ The n-valent anion is CO 3 2- , SO 4 2- , NO 3 - , P.O. 4 3- Examples include:
[0013] Hydrotalcite-like compounds can be easily obtained as precipitates by coprecipitation with an aqueous solution of a mixed divalent and trivalent metal salt and an approximately equivalent amount of alkali. The interlayer anions of hydrotalcite-like compounds have ion-exchange properties, and studies have been conducted on the intercalation of various anions, utilizing this property. However, there have been few reports on the exchange of interlayer water. Patent Document 1 is one of these few reports, and the organic-inorganic composite described in this document is one in which the interlayer water of the hydrotalcite-like compound is replaced with a polar, nonionic organic ultraviolet absorber. In the present invention, one of the organic-inorganic composites described in Patent Document 1, which uses BMBM as the organic ultraviolet absorber, is used as component (A).
[0014] The basic layer of the organic-inorganic composite used as component (A) of the present invention is formed from a double hydroxide of a divalent metal and a trivalent metal. The divalent metal used is Mg, Ca, Zn, Ni, Cu, etc., preferably Mg or Zn. The trivalent metal is Al, Fe, In, etc., preferably Al. The divalent metal and the trivalent metal may be used alone or in combination of two or more.
[0015] The anions forming the intermediate layer of the organic-inorganic composite are organic acid ions with a larger ionic radius than carbonate ions or sulfate ions, preferably with an ionic radius such that the thickness (unit layer thickness) of the intermediate layer is 10 Å or greater, or even 13 Å or greater. If the thickness of the intermediate layer is smaller than the molecular diameter of BMBM (approximately 8.3 Å), it becomes difficult to insert BMBM between the layers, making it difficult to obtain an organic-inorganic composite with a high BMBM content. Specific examples of preferred organic acid ions include ions of higher fatty acids with 10 or more carbon atoms, such as lauric acid, myristic acid, palmitic acid, stearic acid, and behenic acid, as well as ions of ferulic acid and phenylbenzimidazole sulfonic acid, which are known to have ultraviolet absorption capabilities. Among these, stearic acid ions, which have a unit layer thickness as large as 31 Å, are particularly preferred. The anions forming the intermediate layer may be a single component or multiple components.
[0016] The organic-inorganic composite contains BMBM in the intermediate layer. The BMBM is inserted by replacing water molecules originally contained therein, and some water molecules may also be present. The BMBM content in the organic-inorganic composite is preferably 2 to 80% by mass, more preferably 5 to 70% by mass, and particularly preferably 10 to 60% by mass. If the BMBM content is too low, it will be impossible to impart a high UV protection effect to the cosmetic, while if the BMBM content is too high, it will be difficult to insert BMBM between the layers, making production difficult.
[0017] Such an organic-inorganic composite is a known substance from Patent Document 1 (JP 2021-161367 A) and can be produced according to the method described therein. The process is outlined below. (Step 1) A mixed aqueous solution of water-soluble divalent and trivalent metal salts (metal chlorides, nitrates, bromides, sulfates, etc., preferably chlorides and nitrates) is co-precipitated with an alkali (sodium hydroxide, potassium hydroxide, ammonia, sodium carbonate, calcium hydroxide, etc.) in an amount approximately equal to the metal ion equivalent, followed by hydrothermal treatment at 100 to 250°C, preferably 150 to 250°C, for 5 to 20 hours, to produce a hydrotalcite-like compound. (Step 2) Anions in the intermediate layer of the hydrotalcite-like compound are ion-exchanged with organic acid ions. <Third Step> The hydrotalcite-like compound whose unit layer thickness has been increased in the operation of the second step is mixed with an organic solvent solution in which BMBM has been dissolved, and the mixture is heated with stirring at a temperature below the boiling point of the organic solvent, preferably at 50 to 70°C, to replace the interlayer water with BMBM. Specific examples of organic solvents that dissolve BMBM include alcohols such as ethyl alcohol and isopropyl alcohol, and hydrocarbons such as n-hexane and cyclohexane, with alcohols being preferred. The amount of BMBM used in this replacement reaction is 1 to 150 parts by mass, preferably 10 to 100 parts by mass, per 100 parts by mass of the hydrotalcite-like compound. Subsequently, conventional processes such as filtration, washing, drying, pulverization, and classification are appropriately selected and used to obtain the organic-inorganic composite used as component (A).
[0018] Such organic-inorganic composites may be used as is, or, if desired, may be treated with a polyanion (polymeric anion). Specific examples of polyanions that can be used include polyacrylic acid, maleic anhydride-olefin copolymers, polystyrene sulfonic acid, alginic acid, polyphosphoric acid, polysilicic acid (water glass), and carboxymethyl cellulose. These are typically neutralized with an alkali such as NaOH before use. Treatment with a polyanion can be carried out by adding an aqueous solution of the polyanion to a hydrotalcite-like compound dispersed in a polar solvent such as water, and mixing the mixture with stirring. The amount of polyanion used in the treatment is 0.01 to 20% by mass, preferably 0.5 to 10% by mass, relative to the mass of the organic-inorganic composite. Treatment with a polyanion blocks the openings in the intermediate layer of the hydrotalcite-like compound, thereby trapping the BMBM inside.
[0019] Because the organic-inorganic composite of component (A) is a powder containing BMBM between the layers of the layered double hydroxide, the BMBM content in the cosmetic is proportional to the powder blend amount. Therefore, the greater the BMBM content in the organic-inorganic composite, and the greater the content of the organic-inorganic composite in the cosmetic, the greater the BMBM blend amount. Because BMBM is a substance that is difficult to dissolve in oils commonly used in cosmetics, it is difficult to blend BMBM at a concentration above its solubility when dissolving it in an oil using conventional methods. However, according to the present invention, by increasing the BMBM content in the organic-inorganic composite and increasing the blend amount of the organic-inorganic composite, it is possible to blend BMBM at a concentration above its solubility in the oil. Incidentally, the solubility of BMBM in liquid paraffin, which is commonly used as an oil in cosmetics, is 1% by mass at room temperature.
[0020] The cosmetic of the present invention preferably contains 1 to 50% by mass of the organic-inorganic composite of component (A) in the cosmetic. More preferably, it is 2 to 40% by mass, and particularly preferably, it is 5 to 30% by mass. Furthermore, the organic-inorganic composite of component (A) is preferably blended in such a ratio that the amount of BMBM contained therein accounts for 0.5 to 20% by mass of the entire cosmetic, more preferably, the amount of BMBM is 1 to 15% by mass, and particularly preferably, the amount of BMBM is 2 to 10% by mass. If the content of component (A) in the cosmetic is too low, a high UV protection effect cannot be obtained, whereas if it is too high, the solids concentration in the cosmetic becomes high, making it difficult to spread on the skin.
[0021] (B: UV Protection Improver) The organic-inorganic composite of component (A) used in the present invention has the advantages of not precipitating BMBM crystals even when incorporated at high concentrations and of being less likely to discolor due to contact with metal ions, but it still does not have sufficient UV protection effect. Therefore, in the present invention, the UV protection ability of component (A) is enhanced by incorporating, as component (B), at least one UV protection improver selected from the group consisting of polyhydric alcohol fatty acid ester-type nonionic surfactants, polyoxyethylene alkyl ether phosphates or salts thereof, silicone surfactants, polyhydroxy fatty acids, clay minerals, and silica.
[0022] The mechanism by which component (B) improves the UV protection effect is not clear, but in the case of powders such as clay minerals and silica, it is presumed that it functions to prevent the complex of component (A) from aggregating or reagglomerating in liquid oil, and in the case of other organic compounds, it functions to improve the wettability of the complex of component (A) and prevent reagglomeration in liquid oil.
[0023] Examples of polyhydric alcohol fatty acid ester type nonionic surfactants used as component (B) include sucrose fatty acid esters such as sucrose polystearate and sucrose tetrastearate triacetate; glycerin fatty acid esters such as glyceryl stearate and glyceryl diisostearate; polyglycerin fatty acid esters such as polyglyceryl-2 oleate, polyglyceryl-2 isostearate and polyglyceryl-6 polyricinoleate; fatty acid sorbitan esters such as sorbitan isostearate, sorbitan sesquiisostearate, sorbitan oleate and sorbitan sesquioleate; polyoxyethylene sorbitan fatty acid esters such as PEG-4 sorbitan triisostearate; polyoxyethylene glycerin fatty acid esters such as PEG-5 glyceryl stearate; Examples include polyoxyethylene fatty acid esters such as PEG-3 isostearate and PEG-2 stearate, and polyoxyethylene hydrogenated castor oils such as PEG-5 hydrogenated castor oil and PEG-7 hydrogenated castor oil. Among these, polyglyceryl-2 oleate, polyglyceryl-2 isostearate, sorbitan isostearate, sorbitan sesquiisostearate, sorbitan oleate, and sorbitan sesquioleate are preferably used because they have a high rate of improvement in UV protection ability.
[0024] The polyhydric alcohol fatty acid ester nonionic surfactant used as component (B) is preferably lipophilic because it is used by dissolving or dispersing it in the oil used in cosmetics, and its HLB value is usually 8 or less, preferably 2 to 8, and particularly preferably 3 to 6. HLB is an index showing the balance between hydrophilicity and lipophilicity of a nonionic surfactant as a value ranging from 0 to 20, with the closer to 0 the higher the lipophilicity and the closer to 20 the higher the hydrophilicity. Various methods are known for calculating the HLB value, and the values are also listed in catalogs provided by manufacturers.
[0025] Examples of commercially available polyhydric alcohol fatty acid ester nonionic surfactants include NIKKOL SI-15RV (manufactured by Nikko Chemicals Co., Ltd.), which is a sorbitan sesquiisostearate, Cosmol 41V (manufactured by Nisshin Oillio Co., Ltd.), which is a polyglyceryl-2 isostearate, and NIKKOL HEXAGLYN PR-15 (manufactured by Nikko Chemicals Co., Ltd.), which is a polyglyceryl-6 polyricinoleate.
[0026] Examples of polyoxyethylene alkyl ether phosphates or salts thereof used as component (B) include polyoxyethylene lauryl ether phosphate, polyoxyethylene myristyl ether phosphate, polyoxyethylene cetyl ether phosphate, polyoxyethylene stearyl ether phosphate, polyoxyethylene behenyl ether phosphate, and sodium salts thereof. Commercially available polyoxyethylene alkyl ether phosphates or salts thereof include NIKKOL TLP-4, which is trilaureth-4 phosphate, and DLP-10, which is dilaureth-10 phosphate (both manufactured by Nikko Chemicals Co., Ltd.).
[0027] Examples of silicone surfactants used as component (B) include silicone surfactants having a polyoxyalkylene group, such as PEG-3 dimethicone, PEG-8 dimethicone, PEG-9 dimethicone, PEG-10 dimethicone, PEG-9 polydimethylsiloxyethyl dimethicone, lauryl PEG-9 polydimethylsiloxyethyl dimethicone, and cetyl PEG / PPG-10 / 1 dimethicone; and silicone surfactants having a glycerin group, such as polyglyceryl-3 disiloxane dimethicone, polyglyceryl-3 polydimethylsiloxyethyl dimethicone, and lauryl polyglyceryl-3 polydimethylsiloxyethyl dimethicone. The HLB value of the silicone surfactant is preferably 8 or less, more preferably 2 to 8. An HLB value of 3 to 6 is particularly preferred.
[0028] Examples of commercially available silicone surfactants include silicone surfactants having a polyoxyalkylene group such as KF-6016, KF-6011P, KF-6012, KF-6013, KF-6018, KF-6019, KF-6017, KF-6028P, and KF-6038 (all manufactured by Shin-Etsu Chemical Co., Ltd.), ABIL EM-90 and ABIL EM-97 (all manufactured by Evonik Goldschmidt), SH-3772M and SH3775M (all manufactured by Dow-Toray Industries, Inc.), and SILWET L-7604 (manufactured by Momentive Performance Materials, Inc.), and silicone surfactants having a glycerin group such as KF-6104, KF-6105, and KF-6106 (all manufactured by Shin-Etsu Chemical Co., Ltd.).
[0029] Examples of polyhydroxy fatty acids used as component (B) include polyhydroxystearic acid, polyricinoleic acid, etc. Commercially available polyhydroxy fatty acids include, for example, Salacos HS-6C (manufactured by Nisshin Oillio Co., Ltd.), which is polyhydroxystearic acid.
[0030] Examples of clay minerals that can be used as component (B) include water-swelling clay minerals such as bentonite, montmorillonite, hectorite, saponite, (Li / Mg / Na) silicate, and (Al / Mg) silicate; organically modified clay minerals such as disteardimonium hectorite (dimethyl distearyl ammonium hectorite), quaternium-18 hectorite, stearalkonium hectorite (benzyl dimethyl stearyl ammonium hectorite), and distearyl dimethyl ammonium chloride-treated aluminum magnesium silicate; and non-swelling clay minerals such as talc, kaolin, mica, synthetic mica, and sericite. Examples of silica include fumed silica and wet silica. Among these UV protection ability enhancers, organically modified clay minerals are preferred because they provide a high rate of improvement in UV protection effect. Commercially available organically modified clay minerals include Sumecton SAN-P (manufactured by Kunimine Industries Co., Ltd.), which is a quaternium-18 hectorite, Esben WV60 (manufactured by Hojun Co., Ltd.), which is a quaternium-18 bentonite, Benton 38VCG (manufactured by Elementis Japan Co., Ltd.), which is a disteardimonium hectorite, and Benton 27 (manufactured by Elementis Japan Co., Ltd.), which is a stearalkonium hectorite.
[0031] Furthermore, as the UV protection enhancer, a compound having a UV protection index of 1.2 or more, particularly 1.5 or more, as determined by the following evaluation method is preferably used. Examples of compounds having a UV protection index of 1.5 or more include polyhydric alcohol fatty acid ester-type nonionic surfactants, polyoxyethylene alkyl ether phosphates or salts thereof, silicone surfactants, polyhydroxy fatty acids, clay minerals, and silica, with organically modified clay minerals having a particularly high UV protection index.
[0032] (Evaluation method for UV protection index) The base layer is Mg 0.75 Al 0.25 (OH) 213.9 parts by mass of an organic-inorganic composite having a composition and a BMBM content of 36% by mass and 13.9 parts by mass of isotridecyl isononanoate were mixed using a three-roll mill, and then 72.2 parts by mass of isotridecyl isononanoate was added to the resulting mixture to prepare a total of 100 parts by mass of oil dispersion (1). The amount of BMBM contained in this oil dispersion (1) was 5% by mass. The ultraviolet protection factor (UVAPF) of this oil dispersion (1) was measured in accordance with the Colipa (European Fragrance and Cosmetic Industry Federation) guidelines (Method for in vitro determination of UVA protection, 2009), and the value obtained was used as the reference value.
[0033] On the other hand, 13.9 parts by mass of the organic-inorganic composite and 13.9 parts by mass of isotridecyl isononanoate were mixed using a three-roll mill, and 1 part by mass of UV protection performance enhancer was added. The same procedure as above was repeated, except that the amount of isotridecyl isononanoate added was reduced to 71.2 parts by mass, to prepare a total of 100 parts by mass of oil dispersion (2). The UVAPF was measured, and this value was designated UVAPF-1. The amount of BMBM contained in oil dispersion (2) was 5% by mass, and the amount of UV protection performance enhancer was 1% by mass. The ratio of the obtained UVAPF-1 to the reference value (UVAPF-1 / reference value) was calculated, and this ratio was designated the UV protection performance improvement index of the UV protection performance enhancer. An ultraviolet protection performance improvement index of more than 1 indicates that the addition of the ultraviolet protection performance improver has improved ultraviolet protection performance compared to when no ultraviolet protection performance improver is added. For example, an ultraviolet protection performance improvement index of 1.2 indicates that the addition of the ultraviolet protection performance improver has improved ultraviolet protection performance by 20% compared to when no ultraviolet protection performance improver is added.
[0034] In the cosmetic of the present invention, the content of the ultraviolet protection ability enhancer of component (B) is preferably 0.001 to 20% by mass, more preferably 0.01 to 10% by mass, based on the total amount of the cosmetic. Furthermore, in the cosmetic of the present invention, the content of component (B) in the oil phase is preferably 0.01 to 40% by mass, more preferably 0.02 to 20% by mass, based on the total amount of the oil phase. By having the amount of component (B) within this range, a high sunscreen effect is achieved. Furthermore, the mass ratio of component (B) to component (A) [(B) / (A)] is preferably 1 / 99 to 50 / 50, more preferably 2 / 98 to 30 / 70.
[0035] (C: Liquid Oil) In the present invention, a liquid oil (C) is blended as an essential component together with the above-mentioned components (A) and (B). Here, "liquid oil" refers to an oil component that has fluidity at room temperature (25°C) and a semi-solid oil component with a melting point of less than 50°C.
[0036] The liquid oil (C) is not particularly limited as long as it is one that is commonly used in cosmetics, and may be any of animal oil, vegetable oil, and synthetic oil. Specific examples of liquid oils include esters such as triethylhexanoin, tri(caprylic / capric)glyceryl, neopentyl glycol dicaprate, isononyl isononanoate, isotridecyl isononanoate, ethylhexyl palmitate, isopropyl myristate, isopropyl palmitate, octyldodecyl myristate, diisostearyl malate, oligomer esters of dimer acid and dimer diol, pentaerythritol tetraisostearate, diglyceryl tetraisostearate, cetyl isooctanoate, cholesterol fatty acid esters, and jojoba oil; hydrocarbons such as volatile isoparaffin, (C13-15) alkane, (C15-19) alkane, butylene, heavy liquid isoparaffin, liquid paraffin, α-olefin oligomer, squalane, and petrolatum; fats and oils such as olive oil, castor oil, mink oil, and macadamia nut oil; Fatty acids such as isostearic acid and oleic acid; Higher alcohols such as oleyl alcohol and isostearyl alcohol; Silicone oils such as low-polymerization dimethylpolysiloxane, cyclic silicone, high-polymerization dimethylpolysiloxane, methylphenylpolysiloxane, methyl trimethicone, caprylyl trimethicone, cross-linked organopolysiloxane, and fluorine-modified polysiloxane; Fluorine-based oils such as perfluoropolyether; Lanolin derivatives such as lanolin acetate, lanolin fatty acid isopropyl, and lanolin alcohol.
[0037] Among these liquid oils, ester oils have excellent dispersibility for component (A), and when ester oils are used as the liquid oil, cosmetics exhibiting good UVAPF can be easily obtained. Specific examples of ester oils include triethylhexanoin, caprylic / capric triglyceride, neopentyl glycol dicaprate, isononyl isononanoate, isotridecyl isononanoate, ethylhexyl palmitate, and isopropyl myristate.
[0038] The viscosity of the liquid oil at 25°C is usually 0.5 to 5,000 mPa·s, preferably 1 to 500 mPa·s, and more preferably 5 to 500 mPa·s. The viscosity of the liquid oil is measured using a Brookfield viscometer. In particular, an ester oil having a viscosity of 1 to 200 mPa·s at 25°C is preferably used, and its content is preferably 10 to 100 mass% based on the total liquid oil.
[0039] The content of the liquid oil (C) is preferably 7 to 98% by mass, more preferably 10 to 95% by mass, and even more preferably 12 to 90% by mass, of the total cosmetic composition. If the content of component (C) is too low, it becomes difficult to disperse the organic-inorganic composite of component (A), and the ease of spreading also decreases. If the content is too high, the cosmetic composition lacks freshness and feels sticky when used.
[0040] The cosmetic of the present invention may be in any form, such as a lotion (liquid), gel, emulsion, suspension, cream, ointment, aerosol, mist, solid, or solid stick. This cosmetic can be used not only as a sunscreen cosmetic, but also as other cosmetic products imparted with UV protection. Specific examples of other cosmetic products include makeup cosmetics such as foundations and primers, skin care cosmetics such as emulsions, creams, serums, BB creams, and CC creams, and hair cosmetics.
[0041] In addition to the above components (A), (B), and (C), the cosmetic of the present invention may contain other components as appropriate. The other components are not particularly limited as long as they are commonly used in the field of cosmetics, and their amounts are not particularly limited as long as they do not essentially impair the effects of the present invention. Specific examples of other components include solid oils, oil-soluble resins, oil-based gelling agents, UV absorbers (e.g., dimethicodiethyl benzalomalonate, ethylhexyl methoxycinnamate, etc.), UV scattering agents (e.g., titanium oxide, zinc oxide, etc.), polyhydric alcohols (e.g., glycerin, propylene glycol, butanediol, etc.), lower alcohols (e.g., ethanol, isopropyl alcohol, etc.), surfactants, water-soluble polymers, vitamins, moisturizers, fragrances, antioxidants, whitening agents, pH adjusters, chelating agents, preservatives, antifoaming agents, fibers, and various extracts.
[0042] Although component (A) has excellent protection against UV-A, it does not provide sufficient protection against short-wavelength UV, and therefore, when the cosmetic composition of the present invention is used for sunscreen purposes, it is preferable to incorporate an oil-soluble ultraviolet absorber or ultraviolet scattering agent that has excellent protection against short-wavelength ultraviolet (UV-B). Oil-soluble ultraviolet absorbers and ultraviolet scattering agents are described below.
[0043] Examples of oil-soluble UV absorbers that can be blended include cinnamic acid-based UV absorbers such as benzyl paramethoxycinnamate, 2-ethylhexyl paramethoxycinnamate, and glyceryl di-paramethoxycinnamate mono-2-ethylhexanoate; benzophenone-based UV absorbers such as hydroxymethoxybenzophenone, dihydroxymethoxybenzophenone, dihydroxybenzophenone, and tetrahydroxybenzophenone; benzoate ester-based UV absorbers such as paraaminobenzoic acid, ethyl paraaminobenzoate, glyceryl paraaminobenzoate, amyl paradimethylaminobenzoate, octyl paradimethylaminobenzoate, ethyl 4-[N,N-di(2-hydroxypropyl)amino]benzoate, and diethylaminohydroxybenzoylhexylbenzoate; salicylic acid-based UV absorbers such as ethylene glycol salicylate, phenyl salicylate, octyl salicylate, benzyl salicylate, para-tert-butylphenyl salicylate, and homomenthyl salicylate; Examples of the ultraviolet absorber include triazine-based ultraviolet absorbers such as ethylhexyl triazone (2,4,6-tris[4-(2-ethylhexyloxycarbonyl)anilino]1,3,5-triazine) and bis-ethylhexyloxyphenol methoxyphenyl triazine; and other ultraviolet absorbers such as menthyl anthranilate, 2-(2-hydroxy-5-methylphenyl)benzotriazole, 2-ethylhexyl dimethoxybenzylidene dioxoimidazolidinepropionate, octocrylene, and dimethicodiethyl benzalmalonate. Free BMBM can also be contained within a range that does not impair the effects of the present invention.
[0044] When an oil-soluble ultraviolet absorber is blended, its content is 2 to 30% by mass, preferably 5 to 25% by mass, and more preferably 8 to 22% by mass, based on the total mass of the cosmetic.
[0045] Examples of ultraviolet scattering agents that can be added include fine particle metal oxides. More specifically, fine particle titanium oxide, fine particle zinc oxide, fine particle iron oxide, fine particle cerium oxide, fine particle zirconium oxide, etc. The shape of these fine particles is not particularly limited, and may be any of amorphous, granular, spherical, needle-like, spindle-like, plate-like, etc.
[0046] Since UV scattering agents are usually added to the oil phase, it is preferable to use those whose surfaces have been hydrophobized in terms of dispersibility in the oil phase. The method of such surface hydrophobization is not particularly limited, and examples include hydrophobized products using silicone, metal soap, N-acylamino acid salt, perfluoroalkyl compound, etc. as a treating agent. The hydrophobization can be carried out using a single treating agent or a combination of two or more treating agents.
[0047] The ultraviolet scattering agent is typically a fine particle having a number average particle diameter of 5 nm to 100 nm, preferably 8 nm to 85 nm, and more preferably 10 nm to 35 nm. If the number average particle diameter is too small, the ultraviolet protection effect decreases, whereas if the number average particle diameter is too large, the ultraviolet protection effect and transparency decrease.
[0048] When the cosmetic is an emulsion cosmetic such as an oil-in-water or water-in-oil type, the UV scattering agent can be blended in the aqueous phase, but from the viewpoint of the durability of the sunburn prevention effect, it is preferable to blend it in the oil phase.
[0049] In the present invention, a solid oil can be incorporated into the oil phase. By incorporating a solid oil, it is possible to adjust the feel of the cosmetic, such as its staying power and moisturizing effect. Furthermore, by incorporating such a solid oil, it is possible to produce a compact- or stick-shaped oil-based solid cosmetic or a solid W / O type cosmetic, which can be endowed with functions such as portability and ease of use when applying to specific areas. In the present invention, the solid oil is an oil that is solid at room temperature (25°C) and has a melting point of 50 to 120°C, preferably 55 to 105°C.
[0050] Specific examples of such solid oils include hydrocarbon waxes such as paraffin wax, polyethylene wax, ethylene-propylene copolymer, microcrystalline wax, ceresin, ozokerite, and Fischer-Tropsch wax, as well as Japan wax, carnauba wax, candelilla wax, rice wax, beeswax (beeswax), hydrogenated jojoba oil, hardened oil, higher alcohol, and silicone wax.
[0051] The formulation of the cosmetic of the present invention is not particularly limited, and can be, for example, an oil-based cosmetic, a water-in-oil (W / O) emulsion cosmetic, or an oil-in-water (O / W) emulsion cosmetic. Each formulation will be described below.
[0052] (Oily-Based Cosmetic) When the cosmetic of the present invention is an oily cosmetic, it can be in the form of an oily liquid, oily paste, or oily solid, containing component (A), component (B), and component (C) as essential components.
[0053] When the formulation is an oily paste or oily solid, it is preferable to contain one or more selected from an oily gelling agent and a solid oil. Examples of oily gelling agents include dextrin fatty acid esters, sucrose fatty acid esters, starch fatty acid esters, and aluminum stearate. The content of the oily gelling agent and / or solid oil is usually 1 to 30% by mass, preferably 2 to 20% by mass, and more preferably 3 to 15% by mass, of the total cosmetic.
[0054] (Water-in-oil emulsion cosmetic) When the sunscreen cosmetic of the present invention is a water-in-oil emulsion cosmetic, it may contain water, a water-soluble component, and a water-dispersible component that form the aqueous phase, in addition to containing components (A), (B), and (C). From the viewpoint of emulsion stability, water-in-oil emulsion cosmetics may contain a lipophilic surfactant that does not fall under component (B), and it is preferable that the aqueous phase contain an inorganic salt such as sodium chloride or magnesium sulfate in an amount of 0.01 to 3% by mass based on the total weight of the cosmetic.
[0055] In a water-in-oil emulsion cosmetic, the content of the oil phase is preferably 20 to 95% by mass, more preferably 30 to 90% by mass, based on the total cosmetic, and the content of the aqueous phase is preferably 5 to 80% by mass, more preferably 10 to 70% by mass, based on the total cosmetic.
[0056] (Oil-in-water emulsion cosmetic) When the cosmetic of the present invention is an oil-in-water emulsion cosmetic, it may contain water, a water-soluble component, and a water-dispersible component that form the aqueous phase, in addition to the components (A), (B), and (C). In oil-in-water emulsion cosmetics, from the viewpoint of emulsion stability, it is preferable that the aqueous phase contain a hydrophilic surfactant, a water-soluble polymer, and a polyhydric alcohol. Examples of hydrophilic surfactants include anionic surfactants, amphoteric surfactants, and nonionic surfactants with an HLB value of more than 8.
[0057] In the case of an oil-in-water emulsion cosmetic, the content of the aqueous phase is preferably 30 to 80% by mass, more preferably 40 to 75% by mass, based on the total weight of the cosmetic, and the content of the oil phase is preferably 20 to 70% by mass, more preferably 25 to 60% by mass, based on the total weight of the cosmetic.
[0058] (Method for producing cosmetic preparations) The cosmetic preparations of the present invention can be prepared according to conventional methods, but it is preferable to prepare an oily dispersion containing each of the components (A), (B), and (C) in advance, and then add other components as needed and mix them to form an oil phase in which the organic-inorganic composite is dispersed. According to this production method, cosmetics with excellent sun protection effect, feel, and usability can be efficiently produced.
[0059] The method for preparing the oily dispersion is not particularly limited, but it is preferable to use a dispersing machine to produce it from the viewpoint of improving the sunscreen effect. Examples of dispersing machines include roll mills such as two-roll and three-roll mills, ball mills such as ball mills and vibration ball mills, paint shakers, bead mills such as continuous disk bead mills and continuous annular bead mills, Henschel mixers, dispersing mixers, homomixers, high-pressure homogenizers, planetary mixers, kneaders, etc. Among these, it is preferable to use a roll mill because of its high dispersing power and ease of equipment cleaning.
[0060] When preparing an oil-based dispersion using a disperser, the entire amount of components (A), (B), and (C) constituting the dispersion may be added to the disperser. Alternatively, a method may be used in which components (A), (B), and a portion of component (C) are dispersed in advance, and then the resulting mixture is diluted with the remaining component (C). When preparing a dispersion using a kneader such as a three-roll mill, the mass ratio of the amount of component (A) to the total amount of components (B) and (C) during the dispersion process [(A):[(B) + (C)]] is preferably 2:8 to 8:2, and more preferably 4:6 to 7:3. If this mass ratio is small, it is difficult to obtain a fine dispersion. If this mass ratio is too large, the oil agent does not form a continuous phase, making it difficult to obtain a dispersion.
[0061] (UV Protection Composition) The present invention also provides a UV protection composition containing the organic-inorganic composite of component (A). The UV protection composition of the present invention is an oil-based dispersion containing the organic-inorganic composite of component (A) and the UV protection enhancer of component (B) in the liquid oil of component (C), and is suitable for use in preparing cosmetics.
[0062] In the UV protection composition of the present invention, the content of component (A) in the composition is preferably 1 to 70% by mass, more preferably 2 to 50% by mass. The content of component (B) in the composition is preferably 0.01 to 50% by mass, more preferably 0.02 to 40% by mass. The content of component (C) in the composition is preferably 10 to 98% by mass, more preferably 20 to 90% by mass.
[0063] The UV protection composition of the present invention can be produced by mixing the organic-inorganic composite (Component A), the UV protection enhancer (Component B), the liquid oil (Component C), and other components added as needed. The preparation method is the same as the preparation method for the oil dispersion in the cosmetic production method described above.
[0064] The present invention will be explained in more detail below based on examples, but the present invention is not limited to these examples. In the following production examples, examples, and comparative examples, "parts" and "%" represent "parts by mass" and "% by mass relative to the total amount" unless otherwise specified. The cosmetic preparations in the following examples and comparative examples were evaluated as follows:
[0065] (UVAPF Measurement) UVAPF is measured using SPF Analyzer UV-1000S manufactured by Labshere. For the measurement, SPFMASTER-PA01 manufactured by Shiseido Irika Technology Co., Ltd. is used as the sample application plate, and the application amount is 2 mg / cm. 2 Let's say.
[0066] (Coloration test) 20 g of a sample for evaluation was placed in a 30 mL glass bottle, and an iron nail (iron round nail N32) was added thereto. After storing the bottle at 40°C for 1 day, the degree of coloration of the sample was visually observed and evaluated on a 4-point scale based on the following evaluation criteria.
[0067] (Evaluation criteria) A: No change in color of the sample. B: The sample around the nail is slightly discolored red or brown. C: The sample around the nail is deeply discolored red or brown. D: The sample around the nail is widely discolored red or brown.
[0068] Production Example 1 (production of organic-inorganic composite I) 2 L of a mixed solution of 1.5 M / L aqueous magnesium chloride solution and 0.5 M / L aqueous aluminum chloride solution and 2 L of 4.0 M / L aqueous sodium hydroxide solution, using a metering pump, each at a flow rate of 100 mL / min, was supplied under stirring to a 5 L capacity reaction vessel filled with 500 mL of water in advance, the pH was about 9.4-9.6, and the temperature was maintained at about 35 ° C. while carrying out a coprecipitation reaction to obtain a hydrotalcite-like compound. A portion of the precipitate was collected, dissolved in hydrochloric acid, and the amount of Mg and Al was measured by chelate titration, and the atomic ratio of Mg: Al was 3: 1. Furthermore, by comparing the X-ray diffraction pattern of the precipitate with the X-ray diffraction pattern of the hydrotalcite, this hydrotalcite-like compound was found to contain Mg 0.75 Al 0.25 (OH) 2The double hydroxide having the following composition formed the base layer, and chloride ions and water molecules formed the intermediate layer. The reaction mixture was then filtered under reduced pressure, washed with water, and redispersed in water using a chemical stirrer to a total volume of 5 L. One liter of the mixture was then collected, placed in a 1 L autoclave, and hydrothermally treated at 180°C for 15 hours. After cooling to approximately 90°C, the mixture was transferred to a 2 L beaker, and an equimolar aqueous solution of sodium stearate (approximately 90°C) containing Al was added with stirring and reacted for 30 minutes, resulting in ion exchange of the interlayer chloride ions with stearate ions. The mixture was then filtered, washed with warm water (approximately 90°C), dried (approximately 120°C for 3 hours), and sieved through a 100-mesh sieve to obtain a hydrotalcite-like compound powder containing interlayer water and stearate ions as the interlayer anions. (BMBM-free complex) 50 g of this powder was added to 800 mL of ethyl alcohol solution in which 38 g of BMBM had been dissolved, and the mixture was heated at 60 ° C. for 1 hour to replace the interlayer water with BMBM. Subsequently, 0.5 g of maleic anhydride / diisobutylene copolymer sodium salt (Polystar OMR, manufactured by NOF Corporation) was added and stirred for a further 20 minutes. After filtration under reduced pressure, the mixture was washed with alcohol and sieved through a 100 mesh sieve at 120 ° C. for 2 hours to obtain organic-inorganic composite I. The sieved powder was dissolved in hydrochloric acid, and diethyl ether was added to extract the BMBM into diethyl ether. A portion of the extract was taken and the amount of BMBM was measured from the absorption intensity at a wavelength of 357 nm using a spectrophotometer, and the BMBM content was 36%.
[0069] Production Example 2 (Production of organic-inorganic composite II) Organic-inorganic composite II was obtained in the same manner as in Production Example 1, except that 800 mL of ethyl alcohol in which 45 g of BMBM was dissolved was used instead of 800 mL of ethyl alcohol solution in which 38 g of BMBM was dissolved. When analyzed in the same manner as in Production Example 1, the BMBM content was 43%.
[0070] Comparative Example 1 13.9 parts of the organic-inorganic composite I (BMBM content 36%) obtained in Production Example 1 and the same mass of isotridecyl isononanoate were kneaded using a three-roll mill, and 72.2 parts of isotridecyl isononanoate were added and mixed to prepare a total of 100 parts of an oil dispersion. The amount of BMBM contained in this oil dispersion corresponded to 5% of the total. The UVAPF of this composition was measured and found to be 23.6. In the following Examples 1 to 13, this value was used as the reference value to calculate the UV protection performance improvement index of the UV protection performance improver.
[0071] Example 1 In Comparative Example 1, an ultraviolet absorber composition was obtained in the same manner as in Comparative Example 1, except that 1 part by mass of sorbitan sesquiisostearate was added prior to kneading with a three-roll mill, and the amount of isotridecyl isononanoate added was 71.2 parts. The BMBM content of this composition was 5%, and the sorbitan sesquiisostearate content was 1%. The UVAPF of this composition was measured to be 36.5, and the UV protection ability improvement index of sorbitan sesquiisostearate was 1.5. In other words, the coexistence of sorbitan sesquiisostearate improved the UVAPF by 1.5 times compared to the above-mentioned standard value.
[0072] Examples 2 to 13 Ultraviolet absorber compositions were prepared in the same manner as in Example 1, except that the compounds shown in Table 1 were used instead of sorbitan sesquiisostearate, and the UVAPFs of the compositions were measured to calculate the ultraviolet protection ability improvement index for each compound. The results are shown in Table 1.
[0073]
[0074] The results in Table 1 show that the coexistence of polyhydric alcohol fatty acid ester-type nonionic surfactants (Examples 1-3), polyoxyethylene alkyl ether phosphate or its salt (Example 4), silicone-based surfactants (Examples 5 and 6), polyhydroxy fatty acids (Example 7), clay minerals (Examples 8-12), and silica (Example 13) resulted in UVAPFs significantly exceeding the standard value. Among these, sorbitan sesquiisostearate (Example 1), sorbitan oleate (Example 2), trilaureth-4 phosphate (Example 4), PEG-10 dimethicone (Example 5), polyhydroxystearic acid (Example 7), clay minerals (Examples 8-12), and fumed silica (Example 13) significantly improved UV protection, and the organically modified clay minerals (Examples 8 and 9) in particular significantly improved UV protection.
[0075] Examples 14 and 15 and Comparative Examples 2 and 3 <Water-in-oil (W / O) Sunscreen Cosmetics> The water-in-oil sunscreen cosmetics shown in Table 2 were prepared according to the following manufacturing procedure and evaluated using the evaluation methods described above. The results are also shown in Table 2. (Manufacturing Procedure) (1) The components listed in Part A of Table 2 were kneaded using a three-roll mill to prepare an oily dispersion. (2) The components listed in Part B were dissolved or dispersed in the oily dispersion and thoroughly mixed to prepare an oily phase. Note that homosalate (homomenthyl salicylate), octocrylene, and octyl salicylate listed in Part B are oil-soluble UV absorbers. (3) The components listed in Part C were mixed to prepare an aqueous phase. Note that butylene glycol listed in Part C is a humectant. (4) At room temperature (around 25°C), the aqueous phase was added to the oily phase with stirring to prepare a cosmetic.
[0076]
[0077] As is clear from the results in Table 2, the water-in-oil cosmetic compositions of the present invention exhibit excellent UVAPF and are also less likely to discolor due to contact with metals (Examples 14 and 15). In contrast, the cosmetic composition not containing BMBM had a significantly lower UVAPF (Comparative Example 2), and the cosmetic composition containing BMBM dissolved in the oil phase without complexing it showed discoloration due to contact with metals (Comparative Example 3).
[0078] Example 16 and Comparative Example 4 <W / O type emulsion foundation> A W / O type emulsion foundation having the composition shown in Table 3 was prepared according to the same production procedure as in Example 14 and evaluated by the above-mentioned evaluation method. The results are also shown in Table 3. Note that the hydrogen dimethicone-treated zinc oxide fine particles shown in Part B are an ultraviolet scattering agent, and the AL dimyristate-treated titanium oxide is a colorant.
[0079]
[0080] As is clear from the results in Table 3, the W / O type foundation of Example 16 exhibited a high UVAPF and was less likely to discolor due to contact with metals. In contrast, the foundation of Comparative Example 4, which contained BMBM dissolved in the oil phase, had a lower UVAPF than the examples and was also prone to discoloration due to contact with metals.
[0081] Example 17, Comparative Example 5 <Oil-in-water Sunscreen Cosmetic> Oil-in-water sunscreen cosmetics having the compositions shown in Table 4 were prepared using the D-phase emulsification method according to the following manufacturing procedure, and evaluated using the evaluation methods described above. The results are also shown in Table 4. (Manufacturing Procedure) (1) The components of Part A are kneaded using a three-roll mill to prepare an oily dispersion. Note that the triethoxycaprylylsilane-treated titanium dioxide fine particle described in Part A is an ultraviolet scattering agent. (2) In Comparative Example 5, the components of Part B are dissolved and mixed, and then combined with the components of Part A to form the oil phase. (3) The components of Part C are mixed to prepare Phase D (surfactant phase). (4) The oil phase (in the case of Comparative Example 5) or oily dispersion (in the case of Example 17) is mixed into Phase D in small amounts at room temperature to prepare the O / D phase of the gel emulsion. (5) The aqueous phase prepared by mixing the components of Part D is added to the O / D phase and mixed to prepare the cosmetic.
[0082]
[0083] As is clear from the results in Table 4, the sunscreen cosmetic of Example 17 exhibited excellent UVA protection and did not develop discoloration upon contact with metals. In contrast, the sunscreen cosmetic of Comparative Example 5 exhibited good UVA protection but developed significant discoloration upon contact with metals.
[0084] According to the present invention, there are provided a cosmetic preparation that has a high sun protection effect, is less discolored by metal ions, and is highly safe, an efficient method for producing the cosmetic preparation, and an ultraviolet protection agent composition that is useful for preparing the cosmetic preparation.
Claims
1. A cosmetic preparation characterized by comprising as an oil phase component: an ultraviolet protection agent (A) consisting of a layered double hydroxide having a positively charged base layer composed of divalent metal ions, trivalent metal ions, and hydroxide ions, and a negatively charged intermediate layer containing organic acid ions and t-butyl methoxydibenzoylmethane present between the two base layers; and a liquid oil (C) containing at least one ultraviolet protection enhancer (B) selected from the group consisting of polyhydric alcohol fatty acid ester type nonionic surfactants, polyoxyethylene alkyl ether phosphates or salts thereof, silicone surfactants, polyhydroxy fatty acids, clay minerals, and silica.
2. The cosmetic preparation according to claim 1, wherein the divalent metal is at least one selected from magnesium and zinc, and the trivalent metal is aluminum.
3. The cosmetic preparation according to claim 1 or 2, wherein the content of t-butyl methoxydibenzoylmethane in the layered double hydroxide is 2 to 80 mass %.
4. The cosmetic preparation according to claim 1 or 2, wherein the content of said component (A) is 1 to 50 mass%, the content of said component (B) is 0.01 to 20 mass%, and the content of said component (C) is 7 to 98 mass%.
5. The cosmetic preparation according to claim 1 or 2, wherein the organic acid ion is a higher fatty acid ion having 10 or more carbon atoms, a ferulic acid ion, or a phenylbenzimidazole sulfonate ion.
6. The cosmetic preparation according to claim 1 or 2, wherein the ultraviolet protection index of the ultraviolet protection enhancer is 1.2 or more.
7. The cosmetic preparation according to claim 1 or 2, wherein the mass ratio of said component (B) to said component (A) [(B) / (A)] is 1 / 99 to 50 / 50.
8. The cosmetic preparation according to claim 1 or 2, the formulation of which is an oil-based cosmetic preparation, a water-in-oil emulsion cosmetic preparation, or an oil-in-water emulsion cosmetic preparation.
9. A method for producing the cosmetic preparation according to claim 1 or 2, comprising the step of mixing said component (A), said component (B) and said component (C) to prepare an oily dispersion.
10. An ultraviolet protection composition comprising the above component (A) and the above component (B) dispersed or dissolved in the above component (C).
Citation Information
Patent Citations
Preparation method of organic intercalated hydrotalcite ultraviolet absorbent
CN105907366A
External agent for skin
JP1986215315A
Sunburn stopping agent
JP1994009358A
Oil-in-water emulsion cosmetic
JP2012214449A
Ultraviolet absorber
JP2021161367A
Cited By
Cosmetic composition for the photoprotection of the skin and / or hair and its preparation process
FR3171997A1
Cosmetic composition for photoprotection of the skin and / or hair and method for preparing same
WO2026167108A1