Towel fabric and method for manufacturing same

The implementation of silospun spun yarn with a secondary twist in the opposite direction addresses the challenges of pile raising and texture in towel fabrics, resulting in enhanced absorbency and durability, and environmental benefits by eliminating the need for water-soluble fibers or glue in the manufacturing process.

WO2024225182A1PCT designated stage expired Publication Date: 2024-10-31IZAWA TOWEL CO LTD
View PDF 11 Cites 0 Cited by

Patent Information

Application Number
PCT/JP2024/015528
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-04-25
Filing Date
2024-04-19
Publication Date
2024-10-31

AI Technical Summary

Technical Problem

Conventional towel fabrics face challenges with pile raising properties and achieving a soft, puffy texture while maintaining water absorbency and durability.

Method used

The use of silospun spun yarn as warp pile yarn, characterized by a twist coefficient of 0 to 3.0, with a secondary twist in the opposite direction to the primary twist, anchored to both warp and weft yarns, creating a non-twisted or lightly twisted yarn structure that enhances napping properties and breathability.

Benefits of technology

The towel fabric exhibits improved pile standing, softness, water absorption, and durability, with reduced fluff shedding and maintained texture after washing, along with environmental benefits from not requiring water-soluble fibers or glue in production.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure JP2024015528_31102024_PF_FP_ABST
    Figure JP2024015528_31102024_PF_FP_ABST
Patent Text Reader

Abstract

The problem to be solved by the present invention is to provide: a towel fabric that has good raising properties of pile, a soft and bulging texture, and water absorbency; and a method for manufacturing the towel fabric. The present invention is a towel fabric, in which warp pile yarns are locked to warp yarns and weft yarns, wherein the warp pile yarns are silo-spun spun yarns (19) and are spun yarns with no twist or a loose twist to which a secondary twist has been applied in an untwisting direction, which is a direction opposite the direction of a primary twist of a plurality of roving yarns (12a, 12b). Because of a twisting tendency of the primary twist and migration of the primary twist, there is entanglement between fibers, and because yarns are untwisted or loosely twisted, constituent fibers are present in a free state; consequently, the pile yarns have good raising properties and have a soft and bulging texture.
Need to check novelty before this filing date? Find Prior Art

Description

Towel fabric and its manufacturing method

[0001] The present invention relates to a towel fabric using siro spun yarn for pile yarn, and a method for manufacturing the same.

[0002] Traditionally, towel fabrics have been basically made by using warp pile yarns, warp yarns, and weft yarns to create pile fabrics. To ensure good water absorption, towel fabrics have a relatively high basis weight (mass per unit area), and thick, high-fineness yarns are used as constituent yarns. Patent Document 1 proposes using synthetic sirospun yarn to create a figured pile yarn. Patent Documents 2 and 3 propose using loosely twisted sirospun yarn to create a pile knitted fabric.

[0003] Japanese Patent Laid-Open No. 10-088440 Japanese Patent Laid-Open No. 2019-137941 Japanese Patent Laid-Open No. 2019-137942

[0004] However, the above-mentioned prior art has problems with pile raising and soft, fluffy texture, and further improvements are required.

[0005] To provide a towel fabric having good pile raising property, soft and fluffy texture, and water absorbency, and a method for manufacturing the same, as a result of extensive studies to make the most of the characteristics of towel fabric.

[0006] A towel fabric according to one aspect of the present invention includes warp yarns, weft yarns, and warp pile yarns, with the warp pile yarns being engaged with the warp yarns and weft yarns, wherein the warp pile yarns are sirospun yarns, and the sirospun yarns are single yarns of untwisted or loosely twisted spun yarns to which a secondary twist has been applied in the opposite direction to the primary twist direction of a plurality of rovings, i.e., in the untwisting direction, and the sirospun yarns are characterized in that they have a twist coefficient K of 0 to 3.0, where the twist coefficient (K) is calculated using the following formula (Equation 1): Where t: number of twists (twists / 25.4mm), S: cotton count (British cotton count)

[0007] A method for manufacturing towel fabric according to one aspect of the present invention is the method for manufacturing towel fabric described above, characterized in that the warp pile yarn is a sirospun yarn, and a secondary twist is applied in the opposite direction to the primary twist direction of multiple roving yarns with the same twist direction to form a single untwisted or loosely twisted spun yarn.

[0008] A towel according to one embodiment of the present invention is a towel fabric comprising warp yarns, weft yarns, and warp pile yarns, with the warp pile yarns being engaged with the warp yarns and weft yarns, and the warp pile yarns are sirospun yarns that are untwisted or loosely twisted spun yarns to which a secondary twist has been added in the opposite direction (untwisting direction) to the primary twist direction of multiple roving yarns, thereby providing a towel fabric with good pile standing properties, a soft and fluffy texture, and water absorbency, as well as a method for manufacturing the same. That is, the yarn structure has a secondary twist applied in the opposite direction (untwisting direction) to the primary twist direction of multiple rovings, and as a result, the twist tendency of the primary twist and migration of the primary twist (the phenomenon in which single fibers are twisted inward or outward) remain, there is entanglement of the fibers, it is an untwisted yarn or a loosely twisted yarn, and each constituent fiber exists in a free state, so the pile yarn has good pileability and a soft, fluffy texture.

[0009] FIG. 1 is a schematic perspective view of a sirospun spinning device according to one embodiment of the present invention. FIG. 2 is a schematic explanatory diagram of a towel fabric according to one embodiment of the present invention. FIG. 3 is a woven fabric structure diagram of the fiber towel fabric according to the same embodiment. FIG. 4 is a side photograph (magnification: 50x) of the pile portion of the towel fabric according to Example 1 of the present invention. FIG. 5 is a plan photograph (magnification: 10x) of the towel fabric according to Example 1 of the present invention. FIG. 6 is a side photograph (magnification: 50x) of the pile portion of the towel fabric according to Example 2 of the present invention. FIG. 7 is a plan photograph (magnification: 10x) of the towel fabric according to Example 2 of the present invention. FIG. 8 is a side photograph (magnification: 50x) of the pile portion of the ol fabric according to Comparative Example 1. FIG. 9 is a plan photograph (magnification: 10x) of the towel fabric according to Comparative Example 1.

[0010] The present invention focuses on the fact that warp pile yarns (hereinafter also referred to as pile yarns), which account for approximately 70% of the constituent yarns of towel fabric, are important yarns that determine the pile standing property, the texture of the towel fabric, and functionality such as shedding, and has conducted research and made the following findings. That is, the towel fabric of the present invention comprises warp yarns, weft yarns, and warp pile yarns, and the warp pile yarns are engaged with the warp yarns and weft yarns. The warp pile yarns are sirospun yarns, and a secondary twist is applied in the opposite direction to the primary twist direction of the multiple rovings, i.e., in the untwisting direction, and the warp pile yarns are made of untwisted or loosely twisted spun yarns. The inventors have found that this has the following advantages: (1) The warp pile yarns are sirospun yarns, and a secondary twist is applied in the opposite direction to the primary twist direction of the multiple rovings, the number of twists being equal to or greater than the number of twists in the primary twist. As a result, although a secondary twist is applied, the twist tendency of the primary twist remains, and migration (the phenomenon in which single fibers are twisted inward or outward) from the primary twist also remains, and there is entanglement between the fibers. Because the pile yarn is either untwisted or loosely twisted, each constituent fiber exists in a free state, has good pileability, and results in a pile yarn with a soft, fluffy texture. The soft, fluffy texture provides a gentle contact with the skin and allows for efficient wiping of sweat and moisture (texture effect, wiping effect). (2) Because the pile yarn is either untwisted or loosely twisted, the constituent fibers are more likely to absorb moisture, and at the same time, this swelling promotes air movement, improving breathability (water absorption effect, ventilation effect). (3) The entanglement of the constituent fibers reduces shedding (pilling reduction effect), minimizes texture change with washing, and maintains the original soft, fluffy texture (washing texture durability effect). (4) When producing spun yarn, there is no need to use water-soluble fibers (e.g., water-soluble vinylon), glue, etc., which reduces costs. Furthermore, if water-soluble fibers (e.g., water-soluble vinylon), glue, etc. are used and then removed after the fabric is made, voids are created, which reduces the fluffiness (volume) and increases the amount of fluff. (5) When producing spun yarn, there is no need to use water-soluble fibers (e.g., water-soluble vinylon), glue, etc., which reduces the environmental impact of factory wastewater containing these materials.

[0011] The present invention uses Sirospun spun yarn as the warp pile yarn. Sirospun yarn is a yarn formed by separately drafting multiple rovings at regular intervals and then twisting them together to form a two-ply yarn. Compared to two-ply yarns formed by twisting multiple yarns together, Sirospun spun yarn has fibers arranged more regularly on the yarn surface and has less fuzz. Therefore, it can be used as a warp pile yarn in single yarn form. Furthermore, due to the unique yarn structure of Sirospun spun yarn, even when used as a no-twist or loosely twisted yarn, the fibers are entangled with each other, which facilitates winding and reduces yarn breakage during weaving, resulting in good weaving processability. Note that the term "multiple rovings" refers to two or more rovings, and it is known to use two or three rovings. An example of two rovings will be described below.

[0012] The twist coefficient K of the sirospun yarn of the present invention is preferably 0 to 3.5, more preferably 0 to 3.3, and even more preferably 0 to 3.0. The twist coefficient (K) is calculated using the following formula (Math 1): where t: number of twists (twists / 25.4 mm), S: cotton count (British cotton count). This makes the pile yarn either untwisted or loosely twisted.

[0013] It is preferable that the sirospun yarn has a secondary twist in the opposite direction to the primary twist direction of the two rovings, the number of twists being equal to or greater than the number of twists in the primary twist. For example, if the primary twist directions of the two rovings are both Z-direction, the secondary twist is S-direction, and the number of twists in the secondary twist is the same as or greater than the number of twists in the primary twist. This allows each constituent fiber to exist in a more free state, resulting in good pile standing and a pile yarn with a soft, fluffy texture.

[0014] The Sirospun spun yarn is preferably 100% cotton. 100% cotton provides a soft, fluffy texture and is also water-absorbent. Natural fibers including hemp and wool, regenerated fibers including rayon, acetate, and polyester, semi-synthetic fibers, and chemical fibers may be blended to the extent that these properties are not impaired. The blend ratio of these fibers other than cotton is preferably 30% by mass or less. There are no particular restrictions on the yarn count of the Sirospun spun yarn, but thin yarns of 100 to 40 count are preferably used for thin fabrics, 30 to 16 count for medium-weight fabrics, and thick yarns of 12 to 8 count for heavy fabrics.

[0015] The sirospun yarn is preferably mercerized. Mercerization involves immersing the yarn in an aqueous solution of caustic soda (sodium hydroxide) and tensioning it to improve firmness, stiffness, shape memory, luster, strength, shrink resistance, and dyeability. This is thought to be due to the fact that part of the cotton's crystalline structure changes from type I to type II via alkali cellulose, and the structure around the crystals is also rearranged. Mercerization itself is well known, as described in the Fiber Dictionary. Mercerizing the sirospun yarn of the present invention, which is untwisted or loosely twisted in the untwisted direction, synergistically improves pile raising, soft and fluffy texture, water absorbency, and shape memory, resulting in a high-quality towel fabric. The concentration of caustic soda (sodium hydroxide) in the aqueous solution is preferably 15% by mass or more, more preferably 20% by mass or more. The tension treatment is preferably carried out by setting the speed ratio of the supply roller to the take-up roller at about 1 to 1.1 and impregnating the material in a tensioned state with an aqueous solution of caustic soda (sodium hydroxide).

[0016] The method for manufacturing a towel fabric of the present invention includes the following steps: (1) Two rovings with the same twist direction are subjected to a second twist in the opposite direction (untwisting direction) to the primary twist to produce a non-twisted or loosely twisted spun yarn. Preferably, a second twist is added that is equal to or greater than the number of twists in the primary twist. This results in a single sirospun spun yarn, which is then used as the warp pile yarn to manufacture the towel fabric. (2) The warp and weft yarns of the towel fabric may be any yarn, such as open-end spun yarn, air spun yarn, ring spun yarn, long-fiber composite spun yarn, or tying spun yarn. (3) After the towel fabric is woven, it is bleached, scoured, dyed, etc. according to conventional methods to produce the towel fabric.

[0017] The Sirospun spun yarn is preferably cotton with a micronaire of 4 to 7 and an average fiber length of 28 to 45 mm. Micronaire refers to the mass micrograms (μg) per inch (25.4 mm). Cotton with a micronaire of 4 to 7 and an average fiber length of 28 to 45 mm has a high crimp and high crimp strength. Therefore, when applied to the Sirospun spun yarn of the present invention, the twist tendency of the primary twist and migration of the primary twist (the phenomenon in which single fibers are twisted inward or outward) tend to remain, the fibers tend to entangle with each other, and because it is a non-twisted or loosely twisted yarn, each constituent fiber exists in a free state. Therefore, the pile yarn has good nap-raising properties and a soft, fluffy texture. Specific examples shown in Table 1 below are preferred. Among these, Shankar 6 from India is more preferred.

[0018]

[0019] The towel of the present invention is suitable for use as a bath towel (towel after bathing), bath towel, face towel, towel handkerchief (handkerchief), hand towel, wash towel, hand towel, bath mat, sports towel, beach towel (body towel), etc. The fabric blend ratio, yarn type, yarn usage, mass per unit (basis weight), etc. are appropriately set according to the required properties such as shedding resistance and water absorbency. The basis weight can be controlled by changing the pile length (long to short) of the pile yarn to control the basis weight (large to small). Here, an example of a preferable basis weight that can exert the effects of the present invention is a basis weight of 100 to 250 g / m for thin fabrics. 2The medium weight fabric has a basis weight of 250 to 500 g / m 2 The thickness is 500 to 1000 g / m 2 In addition, 100 g / m 2 Those that are less than 1000 g / m are thin and have no bulk. 2 Anything over that is too thick and heavy, and neither is desirable.

[0020] In addition, while cotton is the most suitable material for towels in this invention in terms of texture, absorbency, moisture absorption, and ease of handling, small amounts of linen, rayon, cupra, acetate, or wool may also be blended with cotton. Rayon, cupra, and acetate blends offer moisture absorption, while wool offers warmth. The woven fabric is desized using a jet dyeing machine in accordance with the cotton processing process, and then scoured under standard cotton scouring conditions (a constant temperature of 95-98°C, a 50-minute hold time, and a dilute caustic soda solution and alcohol ethoxylate-added bath). Following scouring, the fabric is then bleached under standard conditions (98°C, 50 minutes, and a hydrogen peroxide solution). The fabric is then dehydrated and set in a tenter for finishing (off-white finish). This bleaching process also involves hot water treatment. If it is desired to incorporate crimped synthetic fiber yarns, the crimp of the false-twisted yarn is expressed during the scouring process, and the fabric is then finished as is.

[0021] Next, if dyeing is performed after scouring and bleaching, cotton is dyed with a reactive dye (60-80°C, 40 minutes). Polyester fibers are dyed with a disperse dye (130°C, 40 minutes). When dyeing fabrics containing cotton and polyester, in addition to solid dyeing using this two-bath process, disperse and reactive dyes can be used separately to dye different colors or chambray (shades). Printing is also possible on scoured and bleached off-white fabric. In the case of pre-dyed polyester yarn, crimping can be developed simultaneously with scouring, and the yarn can be bleached, dyed, and woven to produce pre-dyed towel fabric. In the case of pre-dyed cotton yarn, the yarn can be scoured, bleached, dyed, and woven to produce pre-dyed towel fabric. In this way, the present invention allows for the commercialization of products with excellent color and design properties through a variety of dyeing methods.

[0022] The following description will be made with reference to the drawings. In the following drawings, the same reference numerals indicate the same parts. Figure 1 is a schematic perspective view of a Sirospun spinning device according to one embodiment of the present invention. In this Sirospun spinning device 10, two roving bobbins 11a, 11b are hung per spindle from a creel (roving supplying device), and rovings 12a, 12b supplied from the two roving bobbins 11a, 11b are sent in parallel to a drafting device 15 through a two-mouth trumpet guide 13 provided upstream (on the roving bobbin side) of a back roller 14. The rovings 12a, 12b are then drafted at a predetermined interval between the back roller 14 and an apron 16, and between the apron 16 and a front roller 17, to form fleeces 18a, 18b. The fleeces 18a, 18b are spun from the front roller 17 and twisted downstream of the front roller 17 by a twisting mechanism caused by the rotation of the spindle 21 to form a single spun yarn 19, which is then passed through a snail wire 20 and a traveler 21 and wound onto a bobbin 22. For example, the twist directions of the primary twist of the two rovings 12a, 12b are both in the Z direction, the twist direction by the spindle 21 is in the S direction, and they are twisted in the untwisting direction. In addition, the number of twists by the spindle 21 (secondary twist number) is set to be the same as or greater than the number of twists in the primary twist.

[0023] 2 is a schematic diagram of a towel fabric 1 according to one embodiment of the present invention. This towel fabric 1 is composed of warp pile yarns 2a, 2b, weft ground yarns 3, and warp ground yarns 4a, 4b. The warp pile yarns 2a, 2b form loop piles while being fixed to the ground weave composed of the weft ground yarns 3 and the warp ground yarns 4a, 4b. The obtained towel fabric 1 is cut to a predetermined size and the edges are processed to form towels.

[0024] Figure 3 is a woven fabric diagram of a towel fabric according to one embodiment of the present invention. This woven fabric is a three-pick terry motion weave. The warp pile yarns cross over every three weft ground yarns. The warp ground yarns G and the warp pile yarns P are arranged alternately. The weft yarns 1 to 3 indicate the order. In Figure 3, as viewed from the warp, black and "x" indicate floating yarns, and white indicates sinking yarns.

[0025] The following provides a more detailed explanation using examples. The present invention is not limited to the following examples. <Evaluation of the texture of finished towel fabric> (1) Evaluation of soft texture The softness of the texture is expressed as the volume per 1 g of towel fabric, and is determined by the bulkiness using the following formula. The higher the value, the softer and better the texture. The thickness was measured in accordance with JIS L-1096 (2010) 8.5 bulkiness test, and the basis weight was measured by precisely weighing the weight of a 1 m square. Measurements were taken at five points and the average value was expressed. Bulkiness (cm 3 / g) = thickness (mm) / basis weight (g / m 2 ) × 1000 (2) Evaluation of fluffy texture The towel fabric was compressed at a constant speed using a compression measuring device: KES-G5 (manufactured by Kato Tech Co., Ltd.), and the compression work: WC = (gf.cm 2 ) was determined. Measurements were taken at five locations and the average value was expressed. The WC value is the energy required to compress the fabric, and the larger the value, the better the towel is compressed, the greater the volume and fluffiness, and the better the result. (3) Evaluation of Washing Durability of Texture The towel fabric was washed 20 times in a washing machine according to JIS L-0217 (1995), Method 103. After drying, the compression work: WC = (gf.cm 2 ) was measured at five locations and the average value was expressed. The smaller the difference in WC value before and after washing, the less the loss of fluffy texture due to washing, and the more durable and better the product. (4) Evaluation of water drainage in washing A 35cm wide towel fabric was cut to a length of 80g, and the weight was accurately measured to one decimal place and immersed in water for 20 minutes. The wet towel fabric was then taken out and centrifuged in the spin tub of the washing machine for 4 minutes, the weight was accurately measured and the residual moisture content (%) of the towel fabric was calculated using the following formula. The smaller the value, the better the water drainage. Better the water drainage tends to be, which leads to a faster subsequent drying speed. Three measurements were taken and the average value was expressed. Residual moisture content (%) of fabric = (weight of fabric after immersion in water and spin-drying (W 1 )) - (Weight of fabric before immersion in water (W 0 )) / (Weight of fabric before immersion in water (W 0)) × 100 (5) Evaluation of shedding of fuzz due to washing of towel fabric The shedding of fuzz due to washing was measured in accordance with JIS L0217 (1995), method 103. The fuzz shedding rate (%) was calculated using the following formula; the smaller the value, the less fuzz shedding and the better the result. The number of measurements was 5, and the average value was used. Fuzz shedding rate (%) = (weight of fuzz that fell off after washing (g)) / (weight of towel before washing (g) 0)) x 100 (6) Water Absorbency Evaluation (Modified Larose Method) Five measurements were taken according to the modified Larose method of JIS L 1907 (2010), and the average value was calculated. The Larose Index (Water Absorbency Index) was calculated according to the following formula: Larose Index (Water Absorbency Index) = 2545V x 1411W + 79, where V is the maximum water absorption rate (ml / s), W is the amount of water absorbed at the maximum water absorption rate (ml). The higher the value, the faster and more water is absorbed from the skin, which is preferable. (7) Water Absorption Rate (Drop Method) The water absorption rate of terry cloth was measured according to the Vuillet method of JIS L 1907 (2010). The test outline involved dropping a single drop of water onto the terry cloth from a height of 10 cm, and measuring the water absorption time (seconds) until the mirror-like surface of the drop disappeared three times, and then calculating the average value. The shorter the time, the faster and better the water absorption. <Test Method for Rewetting Rate> The rewetting rate is described in Patent Publication No. 6991633, proposed by the present applicant. This test method involves dropping water onto a fabric test specimen, allowing it to absorb the water, absorbing it with filter paper, and evaluating the fabric's ability to retain the water. This test method, known as the rewetting rate, is consistent with the assessment of water absorbency perceived by humans when using fiber fabrics such as towels. The lower the rewetting rate, the greater the fabric's water absorbency and the better it is evaluated to be. (1) Test Environment and Other Conditions: The test environment was standard conditions, with a temperature of 20±4°C and a relative humidity of 65±4% RH. The filter paper used was stored for at least 24 hours under standard conditions, with a temperature of 20±4°C and a relative humidity of 65±4% RH. The test specimens used were stored for at least 24 hours under standard conditions, with a temperature of 20±4°C and a relative humidity of 65±4% RH. The dripped water was at a temperature of 20±15°C (5-35°C). (2) Operating Procedure: The size of the fiber towel fabric test specimen 1 was 10 cm long and 10 cm wide. The test specimen 1 was placed on a sample stand (not shown). The filter paper used was 110 mm in diameter and 0.22 mm thick, made from α-cellulose according to JIS P 3801 Type 1 standard, and the weight of the filter paper was measured. The filter paper used was Advantec Co., Ltd., product name "Circular Qualitative Filter Paper No. 1." 0.8 ml of water was measured into a pipette and dropped onto the test specimen 1. The test specimen 1 was allowed to absorb the water after waiting for 5 seconds. The filter paper was placed on top, and a load of 1.3 kg (1274 Pa) was placed on top of it. The load was then removed after waiting for 5 seconds.The weight of the filter paper after water absorption was measured. (3) Calculation of water re-wetting rate This was calculated using the following formula: W = [(B - A) / A] x 100 Where W: water re-wetting rate (%) A: weight (g) of filter paper before measurement B: weight (g) of filter paper after water absorption <Pile pileability> A side photograph (magnification 50x) of the pile portion of the towel fabric was observed using an optical microscope.

[0026] (Example 1) (1) Warp Pile Yarns Warp pile yarns were produced using the Sirospun spinning device shown in Figure 1. Shankar 6 cotton from India was used. The twist direction of the first twist of two rovings 12a, 12b was the Z direction, and the twist direction by the spindle 21 was the S direction, and they were twisted in the untwisting direction. The roving fineness was 5 g / 6 yards (9113 decitex), and the Z-direction twist number of the roving was 5 turns / inch (twist factor K = 1 in cotton count). The resulting spun yarn had a cotton count of 20 and a twist factor of 11.7 turns / inch (twist factor K = 2.6). (2) Warp Ground Yarns The warp ground yarns used Indian cotton filling as the cotton, and were ring-spun 40-count two-ply yarns with twist factors of 3.8 for the first twist and 2.2 for the second twist. (3) Weft yarns For the weft yarns, Indian cotton filling was used, and ring-spun yarn No. 20 single yarns with a twist coefficient of 4.0 were used. (4) Weaving of towel fabric The warp pile yarns and warp yarns were sized, and a pile loom was used to weave the fabric shown in Figure 2 with the weave shown in Figure 3. The warp density was 34 threads / inch, the weft density was 56 threads / inch, and the basis weight was 463 g / m 2 The fabric blend ratio is 100% cotton. (5) Scouring and finishing of towel fabric Next, this gray fabric was desized in a liquid jet dyeing machine in the usual manner similar to cotton processing (55°C x 20 minutes, amylase, surfactant-added bath). Next, it was scoured in the same machine at 98°C for 50 minutes in a diluted caustic soda, alcohol ethoxylate-added bath. Next, it was bleached in a hydrogen peroxide bath at 98°C for 50 minutes in the usual manner, and set at 135°C in a tenter and finished (off-white finish). The pile length was 1.15 cm.

[0027] Example 2 The same procedure as in Example 1 was carried out, except that the warp pile yarns were immersed in an aqueous solution of 200 g / L of caustic soda (sodium hydroxide), tensioned, and mercerized.

[0028] Comparative Example 1 The same procedure as in Example 1 was carried out, except that the twist directions of the two rovings 12a, 12b used as warp pile yarns were both in the Z direction, and the twist direction by the spindle 21 was also in the Z direction. The resulting spun yarn had a cotton count of 20 and a twist rate of 14 turns / inch (twist coefficient K = 3.1). The results are shown in Table 2.

[0029]

[0030] As is clear from Table 2, the towel fabrics of Examples 1 and 2 were superior to Comparative Example 1 in bulkiness, total and post-wash compression work (WC), pilling rate, improved Larose method water absorption index, water absorption rate, wet-back rate, and nap standing (Figures 4, 6, and 8). These results confirm that the towel fabric of one embodiment of the present invention is a towel fabric with excellent pile standing, a soft and fluffy texture, and water absorbency, which could not be achieved with conventional technology. Furthermore, the towel fabric of Example 2 (with mercerized pile yarn) had the highest compression work (WC) and drainage property (residual moisture content) after 20 washes, and also had good firmness, stiffness, shape memory, gloss, strength, shrink resistance, and dyeability.

[0031] The towel fabric of the present invention is suitable for use as a fabric for face towels, bath towels, towel handkerchiefs, sports towels, bathrobes, towel blankets, and the like, as well as for clothing, socks, rugs, bedding, and the like.

[0032] REFERENCE SIGNS LIST 1 towel fabric 2a, 2b warp pile yarn 3 weft yarn 4a, 4b warp yarn 10 sirospun spinning device 11a, 11b roving bobbin 12a, 12b roving 13 trumpet guide 14 back roller 15 draft device 16 apron 17 front roller 18a, 18b fleece 19 spun yarn 20 snell wire 21 spindle 22 bobbin

Claims

1. A towel fabric comprising warp yarns, weft yarns and warp pile yarns, the warp pile yarns being engaged with the warp yarns and weft yarns, the warp pile yarns being sirospun yarns, the sirospun yarns being single yarns of untwisted or loosely twisted spun yarns to which a secondary twist has been applied in the opposite direction to the primary twist direction of a plurality of roving yarns, i.e., in the untwisting direction, the sirospun yarns having a twist coefficient K of 0 to 3.0, the twist coefficient (K) being calculated by the following formula (Math 1): Where, t: number of twists (twists / 25.4mm), S: cotton count (British cotton count) 2. The towel fabric according to claim 1, wherein the silospun yarn is 100% cotton.

3. The towel fabric according to claim 1, wherein the sirospun yarn is cotton having a micronaire of 4 to 7 μg and an average fiber length of 28 to 45 mm, where micronaire refers to the average mass per inch (25.4 mm), in micrograms (μg).

4. The towel fabric according to claim 1, wherein the silo spun yarn is mercerized.

5. The towel fabric according to claim 1, wherein the silospun yarn has a cotton count of 8 or more and less than 40.

6. A method for manufacturing a towel fabric according to any one of claims 1 to 5, wherein the warp pile yarn is a sirospun spun yarn, and a secondary twist is applied in the opposite direction to the primary twist direction of multiple roving yarns having the same twist direction to produce a single untwisted or loosely twisted spun yarn.

7. The method for producing towel fabric according to claim 6, wherein the silo spun yarn is mercerized by immersing the yarn in an alkaline aqueous solution and subjecting it to tension treatment.

8. The method for manufacturing a towel fabric according to claim 6, wherein the number of twists in the secondary twist of the sirospun yarn is the same as or greater than the number of twists in the primary twist.

Citation Information

Patent Citations

  • Grandrelle yarn for pile yarn and woven or knitted fabric composed of grandrelle yarn for pile yarn

    JP1998088440A

  • Soft twist spun yarn and method for producing soft twist spun yarn

    JP2019137941A

  • Fabric comprising spun yarn containing cotton fiber as raw material

    JP2019137942A

  • Method and apparatus for testing water absorption of textile fabrics

    JP6991633B1

  • Production of raw yarn for pile fabric

    JP1985052638A