Method and apparatus for double-sided copper foil patterned lithiophilic preparation
The method of oxidizing copper substrates and patterning lithium deposition using a cooled barrier mask and laser ablation addresses the defects in existing lithium deposition techniques, enhancing lithium application on copper substrates and improving battery performance and lifespan.
Patent Information
- Application Number
- PCT/US2024/023780
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-04-24
- Filing Date
- 2024-04-10
- Publication Date
- 2024-10-31
AI Technical Summary
Current lithium deposition technologies on copper substrates result in transition zones, surface defects, and internal resistance issues in thin film lithium batteries, leading to performance problems and shorter battery lifespan.
A method involving a cooled barrier mask with defined openings, oxidation of the copper substrate to form copper oxide, and subsequent lithium deposition, with precise temperature control and patterning using laser ablation to enhance edge quality and minimize defects.
This approach improves lithium application on copper substrates by reducing defects and enhancing edge quality, resulting in higher performance and longer battery lifespan by minimizing dendrite formation and internal resistance.
Smart Images

Figure US2024023780_31102024_PF_FP_ABST
Abstract
Description
METHOD AND APPARATUS FOR DOUBLE-SIDED COPPER FOIL PATTERNED LITHIOPHILIC PREPARATIONBACKGROUNDField
[0001] Embodiments described herein generally relate to metal electrodes, more specifically lithium-containing anodes, high performance electrochemical devices, such as primary and secondary electrochemical devices, including the aforementioned lithium-containing electrodes, and methods for fabricating the same.Description of the Related Art
[0002] Rechargeable electrochemical storage systems are increasing in importance for many fields of everyday life. High-capacity energy storage devices, such as lithium-ion (Li-ion) batteries and capacitors, are used in a growing number of applications, including portable electronics, medical, transportation, grid- connected large energy storage, renewable energy storage, and uninterruptible power supply (UPS). In each of these applications, smaller battery sizes are crucial for continued innovation. Thin film lithium batteries have high potential as smaller batteries, but present difficulties in the manufacturing process.
[0003] Thin film lithium batteries typically employ a thin film of lithium deposited on or over a copper substrate or web. Current lithium deposition technology can lead to a transition zone at each edge of the lithium film in which the lithium film transitions from nominal thickness to zero (bare copper). This transition zone of unwanted lithium can cause internal resistance issues in the formed energy storage device.
[0004] Application of lithium on a copper substrate via evaporation or melt deposition can lead to surface defects, surface impurities, visible copper oxide, and other undesirable qualities. These undesirable qualities can lead to battery performance issues, shorter battery lifespan, or battery failure.
[0005] Thus, there is a need for an improved process of applying lithium to a copper substrate.SUMMARY
[0006] Embodiments described herein generally relate to metal electrodes, more specifically lithium-containing anodes, high performance electrochemical devices, such as primary and secondary electrochemical devices, including the aforementioned lithium-containing electrodes, and methods for fabricating the same.
[0007] In at least one aspect, a method of forming a lithium layer on a copper substrate is provided. The method includes applying a barrier mask to the copper substrate, wherein the barrier mask is cooled and the barrier mask comprises two or more barrier mask segments, each barrier mask segment defining an opening. The method also includes oxidizing the copper substrate to form copper oxide, wherein the oxidizing comprises introducing oxygen to a first side of the copper substrate through the opening defined by each barrier mask segment and applying heat to a second side of the copper substrate. The method further includes depositing lithium on the copper oxide.
[0008] Embodiments may include one or more of the following. The barrier mask is cooled using water. The barrier mask is made from stainless steel. The oxidizing is performed until the copper oxide has a thickness from about 500 nm to about 600 nm. Heat is applied until the copper substrate reaches a temperature greater than or equal to 230°C. The barrier mask forms an air-tight seal with the copper substrate. The barrier mask thickness is between about 40 pm to 60 pm.
[0009] In another aspect, a method of forming a lithium layer on a copper substrate is provided. The method includes applying a barrier mask to the copper substrate, wherein the barrier mask is cooled. The method also includes oxidizing the copper substrate to create copper oxide, wherein the oxidizing comprises applying heat to a first side of the copper substrate and introducing oxygen to a second side of the copper substrate. The method further includes depositing lithium on the copper oxide and patterning the lithium.
[0010] Embodiments may include one or more of the following. The patterning is performed via a laser ablation process. The barrier mask is cooled using water. The water is supplied to the barrier mask such that a center area of the coppersubstrate in a center of the barrier mask and an edge area of the copper substrate covered by the barrier mask have a temperature differential of 50°C. The barrier mask is made from stainless steel. The barrier mask forms an air-tight seal with the copper substrate. The copper substrate is oxidized for less than one second. The oxidizing is performed until the copper oxide has a thickness from about 500 nm to about 600 nm.
[0011] In another aspect, an integrated processing tool is provided. The tool includes a first processing chamber configured to perform oxidization of a continuous sheet of copper substrate to form copper oxide, wherein the processing chamber comprises a cooled barrier mask. The tool also includes a second processing chamber configured to deposit lithium on the continuous sheet of copper substrate.
[0012] Embodiments may include one or more of the following. The tool further includes a third processing chamber configured to pattern the deposited lithium. The third processing chamber is configured to perform laser ablation. The cooled barrier mask comprises a plurality of barrier mask segments. The cooled barrier mask forms an air-tight seal with the continuous sheet of copper substrate.BRIEF DESCRIPTION OF THE DRAWINGS
[0013] So that the manner in which the above recited features of the present disclosure can be understood in detail, a more particular description of the disclosure, briefly summarized above, may be had by reference to embodiments, some of which are illustrated in the appended drawings. It is to be noted, however, that the appended drawings illustrate only typical embodiments of this disclosure and are therefore not to be considered limiting of its scope, for the disclosure may admit to other equally effective embodiments.
[0014] Figure 1 illustrates a processing sequence in accordance with one or more embodiments of the present disclosure.
[0015] Figures 2A-2E illustrate various stages of applying a lithium coating to a copper substrate in accordance with one or more embodiments of the present disclosure.
[0016] Figure 3 illustrates a processing sequence in accordance with one or more embodiments of the present disclosure.
[0017] Figures 4A-4D illustrate various stages of applying a lithium coating to a copper substrate in accordance with one or more embodiments of the present disclosure.
[0018] Figure 5 illustrates a schematic view of an integrated processing tool in accordance with one or more embodiments of the present disclosure.DETAILED DESCRIPTION
[0019] Embodiments described herein generally relate to metal electrodes, more specifically lithium-containing anodes, high performance electrochemical devices, such as primary and secondary electrochemical devices, including the aforementioned lithium-containing electrodes, and methods for fabricating the same.
[0020] One method of applying lithium to copper involves evaporating lithium on copper. However, evaporating lithium onto copper may result in issues in edge quality and application uniformity. The width of the copper substrate may also be limited. In devices with poor edge quality, lithium exposure can result in dendrite formation. Lithium deposition with higher edge quality generally has straight edges without cracks. Dendrites are basically whiskers of lithium that grow inside batteries, and can cause batteries to lose power more quickly, short out, or even in some instances to catch fire. Dendrites are typically blocked by the porous separator membrane, which is positioned in between the lithium metal anode and the cathode. However, some dendrites grow so fast and rigid that these dendrites actually pierce the porous membrane separator positioned between the electrodes, which in turn, short the lithium battery, and in some instances, lead to spontaneous combustion. Thus, there is a need for an improved method of applying lithium to a copper substrate.
[0021] Metallic lithium (Li) wetting is temperature and material dependent. Higher temperatures generally correspond to increased wetting. Materials such as titanium (Ti) and lithium fluoride (LiF) are not lithiophilic. Copper oxide (e.g., CU2O)and nickel (Ni) are examples of more lithiophilic materials. Materials that are more lithiophilic can be utilized as a surface coating for copper films to increase the wettability of the copper film. Therefore, formation of copper oxide on a copper film can increase the wettability of the copper film.
[0022] Described herein are systems and methods of applying lithium to copper films while maximizing edge quality and minimizing surface defects, surface impurities, visible copper oxide, and other undesirable qualities of lithium coated on copper.
[0023] In at least one implementation, barrier masks, heat sources, and oxidizers are used to prepare patterned lithiophilic copper oxide on copper substrates, for example, copper foils. The barrier masks may be fluid cooled barrier masks. In at least one implementation, the barrier masks clamp a copper substrate forming “window” openings of exposed copper material. Infrared heat is applied to the exposed copper material while the copper substrate physically contacting the barrier mask is conductively cooled. An oxidizing gas, for example, oxygen gas, is introduced at a precise pressure, web temperature, and time duration to yield patterned copper oxide with defined edges.
[0024] In at least one implementation, the barrier mask described enables rapid thermal processing (“RTP”) application to high volume web conversion from copper to double-side-patterned copper oxide. Conventional oxidation furnaces suffer from oxidizer migration and web temperature drift such that lithiophilic copper oxide edge definition lacks precise control. This inability to tune lithiophilic copper oxide thickness, composition, and pattern compromises lithium wetting properties, metallic lithium thickness, and area edge definition among other things. In addition, selective copper web thermal oxidation via precise surface temperature control is difficult to achieve due to high substrate thermal conductivity. In at least one implementation, the barrier mask described enables application of lamp or laserbased RTP to prepare copper oxide with properties of optimum lithium wetting without excess heat inducing oxidation outside the barrier window. Alternative approaches such as selective lithium removal after deposition involve massive equipment complexity and are less economical.
[0025] In at least one implementation, precise patterned copper oxidation, for example, less than one micron thick, serving as a lithiophilic layer in combination with commensurate metallic lithium dosing via, for example, a molten lithium atomizer or droplet dispensing - can produce solid metal anodes for LiB’s at lower manufacturing cost compared to thermal evaporation of an equivalent metal thickness. Further, material produced using this method can be made in longer lengths at higher purity than can be using roller lithium.
[0026] Figure 1 illustrates a processing sequence 100 in accordance with one or more embodiments of the present disclosure. Figures 2A-2E illustrate various stages of applying a lithium coating to a copper substrate in accordance with one or more embodiments of the present disclosure. With reference to Figures 2A-2E, views of some embodiments of a lithium coated copper substrate at various stages of manufacture are provided to illustrate the method of Figure 1 .
[0027] In operation 110, a barrier mask 210 is applied to a copper substrate 220 as shown in Figure 2A. The barrier mask 210 includes a plurality of sidewalls 218. The plurality of sidewalls 218 define an opening 213. The copper substrate 220 has a first surface 223 and a second surface 221 , opposite the first surface 223. The copper substrate 220 has edge portions 222, which are covered by the barrier mask 210, and a center portion 224, which is exposed by the opening 213 and not covered by the barrier mask 210. The copper substrate 220 may be in the form of a web-based substrate, panels, or discrete sheets. The copper substrate 220 may be or include a foil, a film, or a thin plate. The copper substrate 220 may be or include strips of plastic material, metal, paper, polymer materials, or a combination thereof. The copper substrate 220 may be or include a polymer sheet coated with copper material. The copper substrate 220 may be or include a copper foil.
[0028] The barrier mask 210 may be made of any suitable material that is compatible with process conditions. In one or more embodiments, the barrier mask 210 is made of a material that has a low thermal conductivity. In one or more embodiments, the barrier mask 210 is made of stainless steel.
[0029] The barrier mask 210 has a height 212, a width 214, and a length 216. The height 212 of the barrier mask 210 may range from 500pm to 750 pm. In oneor more embodiments which can be combined with other embodiments, the height 212 of the barrier mask 210 is 500 pm. The width 214 of the barrier mask 210 may range from 1 mm to 2 mm. In one or more embodiments which can be combined with other embodiments, the width 214 of the barrier mask 210 is 1 mm. The length 216 of the barrier mask 210 may range from 1 mm to 2 mm. In one or more embodiments which can be combined with other embodiments, the length 216 of the barrier mask 210 is 1 mm. The barrier mask 210 has a thickness 211. The thickness 211 of the barrier mask 210 may range from 40 pm to 60 pm. In one or more embodiments which can be combined with other embodiments, the thickness 211 of the barrier mask 210 is 40 pm. Although the barrier mask 210 is shown as rectangular in Figure 2A, the barrier mask 210 may have any regular or irregular shape.
[0030] In one or more embodiments which can be combined with other embodiments, the barrier mask 210 may be flush with the first surface 223 of the copper substrate 220. In one or more embodiments which can be combined with other embodiments, pressure may be applied to the barrier mask 210, such that there is an air-tight seal between the barrier mask 210 and the first surface 223 of the copper substrate 220.
[0031] The copper substrate 220 has a thickness 226. The thickness 226 may range from 10 pm to 18 pm. In one or more embodiments which can be combined with other embodiments, the thickness 266 may be 18 pm.
[0032] In operation 120, the copper substrate 220 is oxidized to form copper oxide as shown in Figure 2B. Pressurized oxygen is supplied to the process chamber 230 via an oxygen source 240. The oxygen is supplied to the surface of the copper substrate 220 that is to be oxidized, for example, the first surface 223 of the copper substrate 220. The opposite surface of the copper substrate 220, for example, the second surface 221 , that is not oxidized during the immediate process, is heated by a heat source 250. During operation 120, copper oxide is formed in the center portion 224, but not the edge portions 222 of the copper substrate 220.
[0033] In one or more embodiments which can be combined with other embodiments, the oxygen source 240 may include any oxygen-containing gas. In one or more embodiments, the oxygen source may include pure oxygen (O2).
[0034] In one or more embodiments which can be combined with other embodiments, the heat source 250 may be an infrared heat source or a heat lamp.
[0035] The barrier mask 210 is configured to allow cooling fluid (not shown) to flow through the barrier mask 210 such that the edge portions 222 of the copper substrate 220 have a lower temperature during operation 120 than the center portion 224 of the copper substrate 220. During operation 120, cooling fluid is supplied to the barrier mask 210 at a flowrate sufficient to create a temperature differential in a range from about 310°C to about 331 °C between the edge portions 222 and the center portion 224. In one or more embodiments which can be combined with other embodiments, the cooling fluid is supplied at a flowrate sufficient to maintain a 50°C or greater difference between the edge portions 222 and the center portion 224. The cooling fluid may be a cooling liquid or a cooling gas. Suitable examples of the cooling fluid include but are not limited to water, inert liquids, clean dry air, inert gases (e.g., argon or nitrogen), or a combination thereof.
[0036] In one or more embodiments which can be combined with other embodiments, the heat source 250 is operated to create a rapid heat transfer through the center portion 224. In one or more embodiments which can be combined with other embodiments, the heat source 250 is operated such that the heat flux through the center portion 224 is about 1 ,800,000 W / m2The heat source 250 may be operated to produce a heat flux such that the temperature of the copper substrate 220 in the center portion 224 is between 322°C and 331 °C. The heat source 250 may be operated to produce a heat flux such that the temperature of the copper substrate 220 in the center portion 224 reaches a minimum of 230°C.
[0037] In one or more embodiments which can be combined with other embodiments, the length of operation 120 is adjusted based on the thickness 226 of the copper substrate 220. In one or more embodiments which can be combined with other embodiments, the length of operation 120 is adjusted based on the targeted thickness 262 of a copper oxide layer 260 (as shown in Figure 2C) on thecopper substrate 220. In one or more embodiments, the length of the operation 120 is adjusted based on visual cues from the process. Operation 120 may be performed until a green tint appears on the surface of the copper. In one or more embodiments which can be combined with other embodiments, operation 120 is performed for less than one second. In one or more embodiments, operation 120 may be performed for 0.6 seconds.
[0038] In operation 120, the oxygen may be supplied at a pressure ranging from 0.2 kPa to 22 kPa.
[0039] In operation 130, the barrier mask 210 is removed such that the copper substrate 220 and the copper oxide layer 260 can be further processed. The thickness 262 of the copper oxide layer 260 may range from 500 nm to 900 nm. In one or more embodiments which can be combined with other embodiments, the thickness 262 of the copper oxide layer 260 is about 500 nm to about 600 nm.
[0040] In operation 140, a lithium layer 270 is deposited on the copper oxide layer 260 as shown in Figure 2C. The lithium layer 270 may have a thickness 272 ranging from 1 pm to 20 pm. Without being limited by theory, since the copper oxide layer 260 is more lithiophilic than the copper substrate 220, the deposited lithium preferentially adheres to the copper oxide layer 260.
[0041] In operation 150, the lithium layer 270 is patterned. In one or more embodiments which can be combined with other embodiments, the lithium layer 270 is patterned with a patterning tool 280 to form patterned lithium layers 270’. In some embodiments (not shown), a plurality of patterning tools 280 are utilized in operation 150. Figures 2D and 2E illustrate the lithium layers 270 on the copper oxide layers 260 after patterning. Figure 2D is a perspective view of the copper substrate 220, and Figure 2E is a top-down view of the copper substrate 220. In one or more embodiments which can be combined with other embodiments, the patterning tool 280 is a tool capable of laser ablation, micro-machining, or other form of patterning. In one or more embodiments which can be combined with other embodiments, patterning the lithium layer 270 includes using a laser having a pulse width in the picosecond range. Specifically a laser with a wavelength in the infrared(IR) range can be used to provide a picosecond-based laser, for example, a laser with a pulse width on the order of the picosecond (10’12seconds).
[0042] In operation 150, some or all of the lithium layer 270 may be removed to form the patterned lithium layers 270’. In operation 150, some or all of the copper oxide layer 260 may be removed to form the patterned copper oxide layer 260’. The patterning process may run in a single pass only, or in multiple passes.
[0043] In Figures 2D-2E, the patterned lithium layers 270’ are shown as regular rectangles. In other embodiments, the patterned lithium layers 270’ may be any regular or irregular shape. In one or more embodiments which can be combined with other embodiments, further processing of the copper substrate 220 and the patterned lithium layers 270’ may take place after completion of processing sequence 100.
[0044] Figure 3 illustrates a processing sequence 300 in accordance with one or more embodiments of the present disclosure. Figures 4A-4D illustrate various stages of applying a lithium coating to a copper substrate in accordance with one or more embodiments of the present disclosure. With reference to Figures 4A-4D, views of some embodiments of a lithium coated copper substrate at various stages of manufacture are provided to illustrate the method of Figure 3. In operation 310, a barrier mask 410 is applied to a copper substrate 420. The barrier mask 410 has an exterior edge portion 417 and interior edge portions 419, which define a plurality of openings 413a-d. The copper substrate 420 has a first surface 423 and a second surface 421 , opposite the first surface. The copper substrate 420 has edges 422, which are covered by the exterior edge portions 417 and interior edge portions 419, and a center portion 424, which is not covered by the barrier mask 410. Each center portion 424 is surrounded by a barrier mask segment 415. In Figure 4A, each barrier mask segment 415 is made of exterior edge portions 417 and interior edge portions 419 of the barrier mask 410. In other embodiments, some of the barrier mask segments 415 may include only interior edge portions 419 of the barrier mask 410, while other barrier mask segments 415 include interior edge portions 419 and exterior edge portions 417 of the barrier mask 410.
[0045] The barrier mask 410 may be made of any suitable material that is compatible with process conditions. In one or more embodiments, the barrier mask 410 is made of stainless steel, a material that has a low thermal conductivity. In one or more embodiments, the barrier mask 410 is made of stainless steel.
[0046] The barrier mask segments 415 have a height 412, a width 414, and a length 416. The height 212 of the barrier mask segment 415 may range from 500 pm to 800 pm. In one or more embodiments which can be combined with other embodiments, the height 412 of the barrier mask segment 415 is 500 pm. The width 414 of the barrier mask segment 415 may range from 0.4 to 0.6. In one or more embodiments which can be combined with other embodiments, the width 414 of the barrier mask segment 415 is 0.4 mm. The length 416 of the barrier mask segment 415 may range from 0.4 mm to 0.6 mm. In one or more embodiments which can be combined with other embodiments, the length 416 of the barrier mask segment 415 is 0.4 mm. The exterior edge portions 417 of the barrier mask 410 have a thickness 411 . The thickness 411 of the exterior edge portions 417 of the barrier mask 410 may range from 0.1 mm to 0.2 mm. In one or more embodiments which can be combined with other embodiments, thickness 411 of the exterior edge portions 417 of the barrier mask 410 is 0.2 mm. Although the barrier mask segments 415 are shown as rectangular in Figure 4A, the barrier mask segments 415 may have any regular or irregular shape. Although, in Figure 4A, there are four barrier mask segments 415, any number of barrier mask segments 415 may be utilized. In one or more embodiments which can be combined with other embodiments, there may be 4 to 8 barrier mask segments 415.
[0047] In one or more embodiments which can be combined with other embodiments, the barrier mask 410 may be flush with the first surface 423 of the copper substrate 420. In one or more embodiments which can be combined with other embodiments, pressure may be applied to the barrier mask 410, such that there is an air-tight seal between the barrier mask 410 and the first surface 423 of the copper substrate 420.
[0048] The copper substrate 420 has a thickness 426. The thickness 426 may range from 10 pm to 18 pm. In one or more embodiments which can be combined with other embodiments, the thickness 466 may be 18 pm.
[0049] In operation 320, the copper substrate 420 is oxidized to form copper oxide as shown in Figure 4B. Pressurized oxygen is supplied to the process chamber 430 via an oxygen source 440. The oxygen is supplied to the side of the copper substrate 420 that is to be oxidized. The opposite surface of the copper substrate 420, for example the second surface 421 that is not oxidized during the immediate process, is heated by a heat source 450. During operation 320, copper oxide is formed in the center portions 424, but not the edges 422 of the copper substrate 420.
[0050] In one or more embodiments which can be combined with other embodiments, the oxygen source 440 may include any oxygen-containing gas. In one or more embodiments, the oxygen source may include pure oxygen (O2).
[0051] In one or more embodiments which can be combined with other embodiments, the heat source 450 may be an infrared heat source or a heat lamp.
[0052] The barrier mask 410 is configured to allow cooling fluid (not shown) to flow through the barrier mask 410 such that the edges 422 of the copper substrate 420 have a lower temperature during operation 320 than the center portions 424 of the copper substrate 420. During operation 320, cooling fluid is supplied to the barrier mask 410 at a flowrate sufficient to create a 225°C to 234°C temperature differential between the edges 422 and the center portions 424. In one or more embodiments which can be combined with other embodiments, the cooling water is supplied at a flowrate sufficient to maintain a 50°C or greater difference between the edges 422 and the center portions 424. The cooling fluid may be a cooling liquid or a cooling gas. Suitable examples of the cooling fluid include but are not limited to water, inert liquids, clean dry air, inert gasses (e.g., argon or nitrogen), or a combination thereof.
[0053] In one or more embodiments, the heat source 450 is operated to create a rapid heat transfer through the center portions 424. In one or more embodiments which can be combined with other embodiments, the heat source 450 is operated such that the heat flux through the center portions 424 is about 1 ,800,000 W / m2The heat source 450 may be operated to produce a heat flux such that the temperature of the copper substrate 420 in the center portions 424 is between229°C and 234°C. The heat source 450 may be operated to produce a heat flux such that the temperature of the copper substrate 420 in the center portion 424 reaches a minimum of 231 °C.
[0054] In one or more embodiments which can be combined with other embodiments, the length of operation 320 is adjusted based on the thickness 426 of the copper substrate 420. In one or more embodiments which can be combined with other embodiments, the length of operation 320 is adjusted based on the thickness 462 of copper oxide layers 460 (as shown in Figure 4C) on the copper substrate 420. In one or more embodiments which can be combined with other embodiments, operation 320 is performed for less than one second. In one or more embodiments, operation 320 may be performed for 0.6 seconds.
[0055] In operation 320, the oxygen may be supplied at a pressure ranging from 0.2 kPa to 22 kPa.
[0056] In operation 330, the barrier mask 410 is removed such that the copper substrate 420 and the copper oxide layers 460 can be further processed. The thicknesses 462 of the copper oxide layers 460 may range from 1 nm to 900 nm. In one or more embodiments which can be combined with other embodiments, the thicknesses 462 of the copper oxide layers range from about 500 nm to about 600 nm.
[0057] In operation 340, lithium layers 470 are deposited on the copper oxide layers 460. The lithium layers 470 may have thicknesses 472 ranging from 1 pm to 18 pm. Without being limited by theory, since the copper oxide layers 460 are more lithiophilic than the copper substrate 420, the deposited lithium preferentially adheres to the copper oxide layers 460. Since the barrier mask segments 415 form lithium layers 470 in the shape of the barrier mask segments 415, patterning is not necessary in processing sequence 300. In one or more embodiments which can be combined with other embodiments, further processing of the copper substrate 420 and lithium layers 470 may take place after completion of processing sequence 300.
[0058] Figure 5 illustrates a schematic view of an integrated processing tool 500 in accordance with one or more embodiments of the present disclosure. In certain embodiments, the integrated processing tool 500 comprises a plurality of processing modules or chambers 520, 530, 560 arranged in a line, each configured to perform one processing operation to a continuous sheet of material 510. In one or more embodiments which can be combined with other embodiments, the processing chambers 520, 530, 560 are stand-alone modular processing chambers wherein each modular processing chamber is structurally separated from the other modular processing chambers. Therefore, each of the stand-alone modular processing chambers, can be arranged, rearranged, replaced, or maintained independently without affecting each other. In certain embodiments, the processing chambers 520, 530, 560 are configured to process a single side of the continuous sheet of material 510 as is shown in FIG. 5. In other embodiments, the processing chambers 520, 530, 560 are configured to process both sides of the continuous sheet of material 510. Although the integrated processing tool 500 is configured to process a horizontally oriented continuous sheet of material 510, the integrated processing tool 500 may be configured to process substrates positioned in different orientations, for example, a vertically oriented continuous sheet of material 510. In certain embodiments, the continuous sheet of material 510 is a flexible conductive substrate. In certain embodiments, the continuous sheet of material 510 may be or include the copper substrate 220, 420.
[0059] In certain embodiments, the integrated processing tool 500 comprises a transfer mechanism 505. The transfer mechanism 505 may comprise any transfer mechanism capable of moving the continuous sheet of material 510 through the processing region of the processing chambers 520, 530, 560. The transfer mechanism 505 may comprise a common transport architecture. The common transport architecture may comprise a reel-to-reel system with a common take-up reel 514 and a feed reel 512 for the system. The take-up reel 514 and the feed reel 512 may be individually heated. The take-up reel 514 and the feed reel 512 may be individually heated using an internal heat source positioned within each reel or an external heat source. The common transport architecture may further comprise one or more intermediate transfer reels 513a, 513b, 516a, 516b, 518a, 518b, 519a, 519b positioned between the take-up reel 514 and the feed reel 512. Although theintegrated processing tool 500 is depicted as having multiple processing regions, in certain embodiments, it may be advantageous to have a single or shared processing region in which each process is performed. For embodiments having discrete processing regions, modules, or chambers, the common transport architecture may be a reel-to-reel system where each chamber or processing region has an individual take-up-reel and feed reel and one or more optional intermediate transfer reels positioned between the take-up reel and the feed reel. The common transport architecture may comprise a track system. The track system extends through the processing regions or discrete processing regions. The track system is configured to transport either a substrate or discrete substrates.
[0060] The integrated processing tool 500 may comprise the feed reel 512 and the take-up reel 514 for moving the continuous sheet of material 510 through the different processing chambers: a first processing chamber 520 to oxidize the continuous sheet of material 510 to form a copper oxide (e.g., CU2O) layer 515 as described in operations 120 and 320, a second processing chamber 530 to deposit a thin film of lithium metal 517 on the copper oxide layer 515, as described in operation 140, 340, and optionally a third processing chamber 560 to pattern the thin film of lithium metal 517 as described in operation 150. In one or more embodiments which can be combined with other embodiments, the finished copper substrate 220, 420 will not be collected on take-up reel 514 as shown in the figures, but may go directly for integration with other components, for example, a separator and positive electrodes, to form battery cells.
[0061] The integrated processing tool 500 may comprise the feed reel 512 and the take-up reel 514 for moving the continuous sheet of material 510 through the different processing chambers: a first processing chamber 520 to oxidize the continuous sheet of material 510 to form the copper oxide layer 515 as described in operations 120 and 320, a second processing chamber 530 to deposit a lithium layer 270, 470 on the copper oxide 260, 460 in operation 140, 340, and a third processing chamber 560 to pattern, for example, by laser ablation, the lithium layer 270 in operation 150. In one or more embodiments which can be combined with other embodiments, the finished copper substrate 220, 420 will not be collected on take-up reel 514 as shown in the figures, but may go directly for integration withother components, for example, a separator and positive electrodes, to form battery cells.
[0062] The first processing chamber 520 is configured to oxidize the continuous sheet of material 510 to form the copper oxide layer 515 as described, for example, in operation 120, 320. The copper oxide layer 515 may be or include the copper oxide layers 260, 460 as described. Oxidization of the copper substrate 220 is described above. The first processing chamber 520 has a processing region 542 that includes an oxidation source 544a for delivering an oxidizing gas to the continuous sheet of material 510. Any suitable oxidizing gas may be used. In at least one implementation, the oxidation source 544a includes oxygen gas. The first processing chamber 520 further includes a barrier mask 550 positioned in between the oxidation source 544a and the continuous sheet of material 510. The barrier mask 550 may be or include the barrier mask 210 or the barrier mask 410. In one or more embodiments, the first processing chamber 520 further includes a heating source 548 for applying heat to the continuous sheet of material 510 during the oxidation process. The heating source 548 may be or include the heat source 250. In some embodiments where the processing chamber 520 is configured to process both the frontside and the backside of the continuous sheet of material 510, the processing region 542 further includes a second oxidation source and a second barrier mask positioned to process the underside of the continuous sheet of material 510.
[0063] In one or more embodiments, the heating source 548 is positioned below the continuous sheet of material 510 to heat the underside of the continuous sheet of material 510 as the frontside of the continuous sheet of material 510 is oxidized similar to the positioning of the heat source 250 shown in Figure 2B. In one or more other embodiments, the heating source 548 may be positioned at other suitable locations within the processing region 542, for example, above the continuous sheet of material 510 in the processing region 542. It is contemplated that more than one heating source 548, and / or other heating module locations may be used. In one or more embodiments, the heating source 548 is an infrared heating source. In one or more embodiments, the heating source 548 includes a lamp or lamp array, a laser source, a resistive heating source, or a combination thereof.
[0064] The second processing chamber 530 is configured for depositing a thin film of lithium metal 517 over the continuous sheet of material 510 as described, for example, in operations 140, 340. The thin film of lithium metal 517 may be or include the patterned lithium layer 270’ or the lithium layer 470. In one or more embodiments, the thin film of lithium metal 517 forms on the oxidized portions of the continuous sheet of material 510, for example, the copper oxide layer 515. In one or more embodiments, where the copper oxide layer 515 is patterned to expose portions of the copper in between portions of the copper oxide layer 515, the thin film of lithium metal 517 preferentially deposits on the portions of the copper oxide layer 515 relative to the exposed copper portions of the continuous sheet of material 510.
[0065] The second processing chamber 530 has a processing region 552 that includes a lithium deposition source 554 positioned to process the frontside of the continuous sheet of material 510. In some embodiments where the processing chamber 530 is configured to process both the frontside and the backside of the continuous sheet of material 510, the processing region 552 further includes a second lithium deposition source positioned to process the backside of the continuous sheet of material 510. The lithium deposition source 554 is configured to perform any suitable lithium deposition process for depositing the thin film of lithium metal 517.
[0066] In one or more embodiments, deposition of the thin film of lithium metal 517 is performed using a molten lithium atomizer or lithium droplet dispensing system. The molten lithium atomizer may perform a centripetal (centrifugal) atomizing method to create small droplets of molten lithium. In at least one implementation, the molten lithium atomizer includes a long porous cylinder with molten lithium contained inside and is located in a position relative to the substrate, for example, the continuous sheet of material 510, such that a portion of the atomized spray from the outside of the cylinder is incident on the substrate. The cylinder is rotated about its axis at rotational speed co and droplets of lithium leave the surface with velocity (=cor), where r is the radius of the cylinder). A portion of these droplets strike the substrate surface where they solidify creating a thin film.The droplets which are not incident on the substrate are collected and returned to a lithium crucible to be recirculated thru the cylinder.
[0067] In one or more embodiments, deposition of the thin film of lithium metal 517 may be by PVD processes, such as evaporation, a slot-die process, a transfer process, a lamination process, thermal evaporation, or a three-dimensional lithium printing process, or any other method of depositing lithium. In one or more embodiments, the second processing chamber 530 for depositing the thin film of lithium metal may include a PVD system, such as an electron-beam evaporator, a thin film transfer system (including large area pattern printing systems such as gravure printing systems), a lamination system, a thermal evaporation system, a slot-die deposition system, a molten lithium atomizer, or a lithium droplet dispensing system.
[0068] The third processing chamber 560 is configured for patterning the thin film of lithium metal on the continuous sheet of material 510, as described, for example in operation 150. The patterning may be performed by any processing chamber capable of laser ablation, micro-machining, mask-assisted bead blasting, or other form of patterning.
[0069] The third processing chamber 560 has a processing region 562 that includes a patterning tool 572 positioned to process the frontside of the continuous sheet of material 510. The patterning tool 572 may be or include the patterning tool 280. In some embodiments where the third processing chamber 560 is configured to process both the frontside and the backside of the continuous sheet of material 510, the processing region 562 further includes a second patterning tool positioned to process the backside of the continuous sheet of material 510.
[0070] In one or more embodiments which can be combined with other embodiments, the patterning tool 572 is a tool capable of laser ablation, micromachining, mask-assisted bead blasting, or other form of patterning. In one or more embodiments which can be combined with other embodiments, patterning the thin film of lithium metal 517 includes using a laser having a pulse width in the picosecond range. Specifically a laser with a wavelength in the infrared (IR) rangecan be used to provide a picosecond-based laser, for example, a laser with a pulse width on the order of a picosecond (10’12seconds).
[0071] In one or more embodiments which can be combined with other embodiments, additional processing chambers may be added to the integrated processing tool 500 to perform further processing of the continuous sheet of material 510. In some embodiments additional processing chambers may be configured to form a protective film on the lithium metal. The protective film may be an ion conducting material as described herein. The protective film can be formed by dip-coating, slot-die coating, gravure coating, laminating, or printing.
[0072] In one or more embodiments which can be combined with other embodiments, additional chambers can provide for deposition of an electrolyte soluble binder or the additional chambers can provide for formation of electrode material (positive or negative electrode material). In one or more embodiments which can be combined with other embodiments, additional chambers provide for cutting of the electrode. In one or more embodiments which can be combined with other embodiments, a wet / dry station is included. The wet / dry station may be suitable for cleaning residues and fragments, or for removing a mask, subsequent to laser patterning of the web. In one or more embodiments which can be combined with other embodiments, a metrology station is included as a component of the integrated processing tool 500.
[0073] In one or more embodiments which can be combined with other embodiments, the processing regions 542, 552, 562 remain under vacuum and / or at a pressure below atmosphere during processing. In one embodiment, the processing regions 542, 552, 562 remain at atmospheric pressure during processing. In one or more embodiments which can be combined with other embodiments, the processing regions 542, 552, 562 remain under an inert gas atmosphere during processing. In one or more embodiments which can be combined with other embodiments, the inert gas atmosphere is an argon gas atmosphere. In one or more embodiments which can be combined with other embodiments, the inert gas atmosphere is a nitrogen gas (N2) atmosphere.
[0074] The integrated processing tool 500 further includes a system controller 590 operable to control various aspects of the integrated processing tool 500. The system controller 590 facilitates the control and automation of the integrated processing tool 500 and can include a central processing unit (CPU), memory, and support circuits (or I / O). Software instructions and data can be coded and stored within the memory for instructing the CPU. The system controller 590 can communicate with one or more of the components of the integrated processing tool 500 via, for example, a system bus. A program (or computer instructions) readable by the system controller 590 determines which tasks are performable on a substrate. In some aspects, the program is software readable by the system controller 590, which can include code to control processing of the substrate. Although shown as a single system controller 590, it should be appreciated that multiple system controllers can be used with the aspects described herein.
[0075] While the foregoing is directed to embodiments of the present disclosure, other and further embodiments of the disclosure may be devised without departing from the basic scope thereof, and the scope thereof is determined by the claims that follow.
Claims
Claims:
1. A method of forming a lithium layer on a copper substrate, the method comprising: applying a barrier mask to the copper substrate, wherein the barrier mask is cooled and the barrier mask comprises two or more barrier mask segments, each barrier mask segment defining an opening; oxidizing the copper substrate to form copper oxide, wherein the oxidizing comprises introducing oxygen to a first side of the copper substrate through the opening defined by each barrier mask segment and applying heat to a second side of the copper substrate; and depositing lithium on the copper oxide.
2. The method of claim 1 , wherein the barrier mask is cooled using water.
3. The method of claim 1 , wherein the barrier mask is made from stainless steel.
4. The method of claim 1 , wherein the oxidizing is performed until the copper oxide has a thickness from about 500 nm to about 600 nm.
5. The method of claim 1 , wherein the heat is applied until the copper substrate reaches a temperature greater than or equal to 230°C.
6. The method of claim 1 , wherein the barrier mask forms an air-tight seal with the copper substrate.
7. The method of claim 1 , wherein a thickness of the barrier mask is between about 40 pm to 60 pm.
8. A method of forming a lithium layer on a copper substrate, the method comprising:applying a barrier mask to the copper substrate, wherein the barrier mask is cooled; oxidizing the copper substrate to create copper oxide, comprising applying heat to a first side of the copper substrate and introducing oxygen to a second side of the copper substrate; depositing lithium on the copper oxide; and patterning the lithium.
9. The method of claim 8, wherein the patterning is performed via a laser ablation process.
10. The method of claim 8, wherein the barrier mask is cooled using water.
11. The method of claim 10, wherein the water is supplied to the barrier mask such that a center area of the copper substrate in a center of the barrier mask and an edge area of the copper substrate covered by the barrier mask have a temperature differential of 50°C.
12. The method of claim 8, wherein the barrier mask is made from stainless steel.
13. The method of claim 8, wherein the barrier mask forms an air-tight seal with the copper substrate.
14. The method of claim 8, wherein the copper substrate is oxidized for less than one second.
15. The method of claim 8, wherein the oxidizing is performed until the copper oxide has a thickness from about 500 nm to about 600 nm.
16. An integrated processing tool comprising:a first processing chamber configured to perform oxidization of a continuous sheet of copper substrate to form copper oxide, wherein the first processing chamber comprises a cooled barrier mask; and a second processing chamber configured to deposit lithium on the continuous sheet of copper substrate.
17. The integrated processing tool of claim 16, further comprising a third processing chamber configured to pattern the deposited lithium.
18. The integrated processing tool of claim 17, wherein the third processing chamber is configured to perform laser ablation.
19. The integrated processing tool of claim 16, wherein the cooled barrier mask comprises a plurality of barrier mask segments.
20. The integrated processing tool of claim 16, wherein the cooled barrier mask forms an air-tight seal with the continuous sheet of copper substrate.
Citation Information
Patent Citations
Depositing mask, film formation method using it, and film formation device using it
JP2005044592A
Composition comprising lactic acid bacteria derived from green tea for improving liver function
KR1020230161153A
Method for producing a substrate, which is coated with an alkali metal, by means of a promoter layer, and a coated substrate
US20200099039A1
Electrode for use in an electrical energy storage apparatus and a method for manufacturing an electrode for use in an electrical energy storage apparatus
US20200303746A1
Contact cooling of a projection mask
US5142120A