Microelectromechanical polymer structure oxide coatings
The micro-lens encapsulation layer with a metal oxide or silicon-containing layer addresses the challenges of energy efficiency and stability in LED pixels by providing a robust barrier against environmental factors, ensuring the longevity and optical compatibility of micro-LEDs in augmented and virtual reality applications.
Patent Information
- Application Number
- PCT/US2024/025869
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-04-24
- Filing Date
- 2024-04-23
- Publication Date
- 2024-10-31
AI Technical Summary
Current LED pixel technologies face challenges in achieving high energy efficiency, brightness, and longevity, particularly in augmented and virtual reality applications, where micron-scale LEDs with micro-lenses are needed but require effective encapsulation to prevent oxygen and moisture ingress while maintaining optical and mechanical stability.
A micro-lens encapsulation layer with a thickness of 1 nm to 100 nm, composed of a metal oxide or silicon-containing layer, is deposited using atomic layer deposition, providing a barrier against oxygen and moisture while retaining optical compatibility and stability up to 200 °C, and is applied over micro-lenses to enhance mechanical stability and prevent thermal damage.
The solution enhances the thermal stability and mechanical durability of micro-LED pixels, maintaining optical properties and ensuring the longevity of micro-lens geometry, while allowing for efficient light emission and reduced manufacturing costs through a low-temperature deposition process.
Smart Images

Figure US2024025869_31102024_PF_FP_ABST
Abstract
Description
MICROELECTROMECHANICAL POLYMER STRUCTURE OXIDE COATINGSBACKGROUNDField
[0001] Embodiments of the present disclosure generally relate to LED pixels and methods of fabricating LED pixels.Description of the Related Art
[0002] Light emitting diode (LED) panels use an array of LEDs, with individual LEDs providing the individually controllable pixel elements. Such LED panels can be used for a computer, touch panel device, personal digital assistant (PDA), cell phone, television monitor, and the like.
[0003] An LED panel that uses micron-scale LEDs based on lll-V semiconductor technology (also called micro-LEDs) would have a variety of advantages as compared to OLEDs, e.g., higher energy efficiency, brightness, and lifetime, as well as fewer material layers in the display stack which can simplify manufacturing. Augmented Reality (AR) and Virtual Reality (VR) LED panels may use micro-LEDs with micro-lenses. Accordingly what is needed in the art are LED pixels and a method of fabricating LED pixels.SUMMARY
[0004] In one embodiment, a device is provided. The device includes a micro-lens encapsulation layer. The device includes a backplane, at least three micro-LEDs disposed on the backplane, and subpixel isolation (SI) structures disposed on the backplane to define wells of at least three subpixels. At least three of the subpixels have a color conversion material disposed in the wells. An encapsulation layer is disposed over the subpixel isolation structures and the subpixels. A plurality of micro-lens are disposed over the encapsulation layer, in which each micro-lens of the plurality of micro-lens is disposed over a respective well of at least three subpixels. A micro-lens encapsulation layer having a thickness of about 1 nanometer (nm) to about 100 nm is disposed onthe micro-lenses, in which the micro-lens encapsulation layer is a metal oxide layer or a silicon-containing layer.
[0005] In another embodiment, a method of depositing a micro-lens encapsulation layer is provided. The method includes depositing a resist over an encapsulation layer of a pixel, in which the encapsulation layer is disposed over encapsulate subpixel isolation structures above micro-LEDs and a backplane. The method includes patterning the resist disposed over the encapsulation layer. A micro-lens is formed from the resist using a modification process. A micro-lens encapsulation layer is deposited on the micro-lens, in which the micro-lens encapsulation layer has a thickness of about 1 nanometer (nm) to about 100 nm disposed on the micro-lenses. The micro-lens encapsulation layer is a metal oxide layer or a silicon-containing layer.
[0006] In another embodiment, a method of depositing a micro-lens encapsulation layer is provided. The method includes depositing a resist over an encapsulation layer of a pixel, in which the encapsulation layer is disposed over encapsulate subpixel isolation structures above micro-LEDs and a backplane. The method includes patterning the resist disposed over the encapsulation layer. A micro-lens is formed from the resist using an atomic layer deposition process. A micro-lens encapsulation layer is deposited on the micro-lens, in which the micro-lens encapsulation layer has a thickness of about 1 nanometer (nm) to about 100 nm disposed on the micro-lenses. The microlens encapsulation layer is a metal oxide layer or a silicon-containing layer.BRIEF DESCRIPTION OF THE DRAWINGS
[0007] So that the manner in which the above recited features of the present disclosure can be understood in detail, a more particular description of the disclosure, briefly summarized above, may be had by reference to embodiments, some of which are illustrated in the appended drawings. It is to be noted, however, that the appended drawings illustrate only exemplary embodiments of the disclosure and are therefore not to be considered limiting of its scope, may admit to other equally effective embodiments.
[0008] Figure 1 is a schematic, cross-sectional view of a pixel having a micro-lens arrangement according to embodiments.
[0009] Figure 2 is a flow diagram of a method of depositing a micro-lens encapsulation layer according to embodiments.
[0010] Figures 3A-3D are schematic, cross-sectional views of a pixel during the method according to embodiments.
[0011] Figure 4 is a flow diagram of a method of atomic layer deposition according to embodiments.
[0012] To facilitate understanding, identical reference numerals have been used, where possible, to designate identical elements that are common to the figures. It is contemplated that elements and features of one embodiment may be beneficially incorporated in other embodiments without further recitation.DETAILED DESCRIPTION
[0013] Embodiments of the present disclosure generally relate to LED pixels and a method of fabricating LED pixels. The method includes a method of depositing a micro-lens encapsulation layer. The device includes a micro-lens encapsulation layer disposed on the micro-lenses. The micro-lens encapsulation layer is a metal oxide layer or a silicon-containing layer disposed on the micro-lenses. The encapsulation layer has a thickness of about 1 nm to about 100 nm. The thickness of about 1 nanometers (nm) to about 100 nm allows the metal oxide layer or silicon-containing layer to be optically compatible. The composition of the metal oxide layer or the silicon-containing layer provides a barrier to oxygen and moisture ingress while remaining stable at temperatures up to 200 °C. The micro-lens encapsulation layer is deposited via an atomic layer deposition (ALD) process operating at a temperature of about 50 °C to about 100 °C, e.g., about 50 °C to about 90 °C or about 70 °C to about 85 °C. In some embodiments, the ALD process can be performed at a temperature of 80 °C or less to allow the micro-lenses to retain their geometry and optical properties as the micro-lens encapsulation layer is deposited.
[0014] Figure 1 is a schematic, cross-sectional view of a pixel 100. The pixel 100 includes at least three micro-LEDs disposed on a backplane 102. An isolation material 106 may be disposed between the micro-LEDs 104. The micro-LEDs 104 are integrated with backplane circuitry so that each micro-LED 104 can be individually addressed. For example, the circuity of the backplane 102 can include a thin-film transistor (TFT) active matrix array with a TFT and a storage capacitor (not illustrated) for each micro-LED, column address and row address lines, column and row drivers, to drive the micro-LEDs 104. Alternatively, the micro-LEDs 104 can be driven by a passive matrix in the backplane circuitry. The backplane 102 can be fabricated using conventional complementary metal-oxide-semiconductor (CMOS) processes.
[0015] An optional interfacial layer 108 is disposed over, and in some embodiments directly on, the micro-LEDs 104. Subpixel isolation (SI) structures 110 may be disposed over the interfacial layer 108. The adjacent subpixel isolation structures define the respective wells 113 of at least three subpixels. The micro-LEDs 104 are disposed in each well 113 between the adjacent SI structures 110. For example, a first sub-pixel 114a includes a first micro-LED 104a, a second sub-pixel 114b includes a second micro-LED 104b, and a third sub-pixel 114c includes a third micro-LED 104c. Although the pixel 100 is described as including three micro-LEDs, it is to be understood that the pixel 100 may have hundreds, thousands, millions, or more LEDs. Although the micro-LEDs 104 are illustrated as micro-LEDs, this is for example purposes only, in which any style of LED may be utilized. In some embodiments, the LEDs may be any size including, but not limited to, mini and macro LEDs. In some embodiments, the micro-LEDs 104 emit UV light. In other embodiments, the micro-LEDs 104 emit light of other wavelengths. Each well 113 has a width from about 0.5 pm to about 40 pm, such as about 1 pm to about 30 pm. The SI structures 110 have a width from about 0.1 pm to about 15 pm such as 0.5 pm to 10 pm. The SI structures 110 may include organic material, such as epoxy-based photoresist, or inorganic material, such as a reflective metal, or a combination of both.
[0016] The subpixels 112 may include a red subpixel 112a with a red color conversion material disposed in the well 113 of the red subpixel 112a, a green subpixel 112b with a green color conversion material disposed in the well 113 of the green subpixel 112b, and a blue subpixel 112c with a blue color conversion material disposed in the well 113 of the blue subpixel 112c. When a micro-LED 104a of the red subpixel 112a is turned on, the red color conversion material will convert the UV light, about 370 nm to about 425 nm, and / or blue, green, or red light, emitted from micro-LED 104a into red light. When a micro-LED 104c of the blue subpixel 112c is turned on, the blue color conversion material will convert the UV light emitted from micro-LED 104c into blue light. When a micro-LED 104b of the blue subpixel 112b is turned on, the green color conversion material will convert the UV light emitted from micro- LED 104b into green light. In one embodiment, the pixel 100 includes a fourth subpixel 112d. A fourth subpixel 112d may not include a color conversion material, e.g., color-conversion-layer-free, or may be a sacrificial material. In some embodiments, which may be combined with other embodiments of the disclosure, the at least three subpixels include a similar color conversion material. In some embodiments, which may be combined with other embodiments of the disclosure, the at least three subpixels include a different color conversion material. The fourth subpixel 112d may be later filled with a color conversion material.
[0017] In some embodiments, the color conversion material may include quantum dots (QDs). The quantum dots may be sized to produce wavelengths corresponding to different colors. In one embodiment, the red color conversion material of the red subpixel 112a may include quantum dots approximately 6 nm in size. The blue color conversion material of the blue subpixel 112b may include quantum dots approximately 4 nm in size. The green color conversion material of the green subpixel 112c may include quantum dots approximately 2 nm in size. In other embodiments, the color conversion material may include nanostructures, photoluminescent materials, or organic substances.
[0018] An encapsulation layer 122 is disposed over the subpixel isolation structures 110 and the subpixels 112. In some embodiments, which may be combined with other embodiments of the disclosure, the pixel 100 may include a UV blocking layer disposed over the encapsulation layer 122. In some embodiments, a light filter layer 130 can be disposed over the encapsulation layer 122 and below the micro-lenses 128. In some embodiments, a passivation layer 132 is disposed on the light filter layer 130 with the microlenses 128 disposed on the passivation layer 132 and over each of the wells 113 of the subpixels 110. The light filter layer 130 can be selective for photons of certain wavelengths. In some embodiments, the light filter layer 130 is a UV blocking layer, a UV reflecting layer, a blue light blocking layer, a blue light reflecting layer, or combinations thereof. The light filter layer 130 may include a UV blocking material, a UV reflecting material, a blue light blocking material, a blue light reflecting material, or combinations thereof.
[0019] In some embodiments, the encapsulation layer 122, the light filter layer 130, and / or the passivation layer 132 can include an inorganic silicon- containing layer, or a organosilicon-containing layer. In some embodiments, the inorganic silicon-containing layer may include silicon nitrides. In some embodiments, the organosilicon-containing layer may include hexamethyldisiloxane (HMDSO). In some embodiments, the organosilicon- containing layer includes an epoxy-based polymeric material. In some embodiments, the organosilicon-containing layer includes a photoresist.
[0020] In some embodiments, each of the encapsulation layer 122, the light filter layer 130, and / or the passivation layer 132 can have a thickness of about 0.1 pm to about 1 pm, e.g., about 0.1 pm to about 0.8 pm, about 0.2 pm to about 0.5 pm, about 0.5 pm to about 0.9 pm, or about 0.9 pm to about 1 pm. For example, the organosilicon-containing layer can have a thickness of about 1 pm to about 3 pm, e.g., about 1.1 pm to about 2.8 pm, about 1.2 pm to about 2.5 pm, about 1 .5 pm to about 1 .9 pm, or about 1.5 pm to about 1.6 pm.
[0021] The micro-lenses 128 are disposed on the encapsulation layer 122 and over each of the wells 113 of the subpixels 112. The micro-lenses 128include a resist material. The resist material may be a photoresist material or a polymeric material, e.g., epoxy resin, acrylated polyesters, silicones, siloxanes, or the like.
[0022] A micro-lens encapsulation layer 126 is disposed on the micro-lenses 128. The micro-lens encapsulation layer 126 is a metal oxide layer or a silicon- containing layer that has a thickness of about 1 nm to about 100 nm to allow the metal oxide layer to be optically compatible and provide a barrier to oxygen and moisture ingress. The metal oxide layer includes aluminum oxide, titanium oxide, hafnium oxide, tantalum oxide, or combinations thereof. The silicon- containing layer includes silicon oxide, silicon nitride, or the like. Without being bound by theory, the micro-lens encapsulation layer of a metal oxide or a silicon oxide can provide enhanced mechanical stability to prevent damage to the micro-lens while still retaining transparency for the emission of one or more wavelengths of light through the micro-lens encapsulation layer.
[0023] The micro-lens encapsulation layer 126 has a thickness of about 1 nm to about 100 nm, e.g., about 1 nm, about 10 nm, about 20 nm, about 30 nm, about 40 nm, about 50 nm, about 60 nm, about 70 nm, about 80 nm, about 90 nm, about 100 nm, or the like. The micro-lens encapsulation layer 126 may provide thermal stability from about -50 °C to about 200 °C, e.g., about -50 °C, about -40 °C, about -30 °C, about -20 °C, about -10 °C, about 0 °C, about 10 °C, about 20 °C, about 30 °C, about 40 °C, about 50 °C, about 60 °C, about 70 °C, about 80 °C, about 90 °C, about 100 °C, about 110 °C, about 120 °C, about 130 °C, about 140 °C, about 200 °C, or the like. Without being bound by theory, micro-lens encapsulation layer having a thickness of about 1 nm to about 100 nm can provide for enhanced thermal stability up to about 200 °C.
[0024] Figure 2 is a flow diagram of a method 200 of forming a micro-lens encapsulation layer 126. Figures 3A-3D are schematic, cross-sectional views of the pixel 100 during the method 200. At operation 201 , as shown in Figure 3A, a resist 301 is deposited. The resist 301 is deposited over the encapsulation layer 122. At operation 202, as shown in Figure 3B, the resist 301 is patterned. The resist may include a polymer containing material. Asshown in Figure 3B, the resist 301 is patterned such that the resist 301 remains disposed over each of the wells 113 of the subpixels 112, thereby preventing damage to the each of the wells 113 of the subpixels 112 during a later processing operation. The resist 301 may be patterned via grayscale lithography, laser etching, or a plasma etching procedure, nanoimprint lithography, or combinations thereof.
[0025] At operation 203, as shown in Figure 3C, the micro-lenses 128 are formed. The micro-lenses 128 are formed by a modification process. The modification process is a grayscale lithography process or a thermal reflow process. The thermal reflow process may include a process of heating the plurality of resists 301 at about 100 °C to about 200 °C, e.g., about 100 °C, about 120 °C, about 140 °C, about 160 °C, about 180 °C, about 200 °C, or the like, to form the micro-lenses 128. In some embodiments, the micro-lenses 128 have a spherical or aspheric shape after the modification process. In some embodiments, the micro-lenses 128 comprises a total transmittance of about 80% to about 95%, e.g., about 80% to about 95%, about 85% to about 94%, about 90% to about 93%, or about 91 % to about 92%.
[0026] At operation 204, as shown in Figure 3D, a micro-lens encapsulation layer 126 is deposited over the micro-lenses 128. The micro-lens encapsulation layer 126 includes a metal oxide layer or a silicon-containing layer as described herein. In some embodiments, the micro-lenses encapsulation layer 126 can have a spherical or aspheric shape after being deposited over the micro-lenses 128. In some embodiments, the micro-lenses encapsulation layer 126 comprises a total transmittance of about 80% to about 100%, e.g., about 80% to about 99%, about 85% to about 98%, about 90% to about 98%, or about 95% to about 100%.
[0027] Figure 4 is a flow diagram of a method 400 of depositing a micro-lens encapsulation layer 126 using an ALD process. At operation 401 , a first precursor is introduced in a processing chamber for a first predetermined period of time. The first precursor may include any reactive precursor capable of bonding to or reacting with the plurality of micro-lenses. The first precursor mayinclude trimethylamine (TMA), hafnium chloride, tert-butyllim ido-tris- ethylmethylamido-tantalum (TBTEMT), bis(diisopropylamino)disilane (BDIPADS), and / or titanium isopropxide (Ti[OCH(CH3)2]4). The first predetermined period of time may range from 0.1 s to about 10 s, e.g., about 0.1 s to about 5 s, about 0.1 s to about 1 s, or about 0.1 s to about 0.5 s. For example, at operation 401 a first precursor of trimethyl aluminum (TMA) can be introduced to the chamber for a first predetermined amount of time of about 0.1 s. Without being bound by theory, a first predetermined amount of time of about 0.1 s to about 10 s can provide a film having a uniform thickness on the plurality of micro-lenses.
[0028] At operation 402, a first purge gas may be introduced to purge the first precursor from the chamber. The first purge gas may include any inert gas capable of diluting and / or purging the first precursor from the chamber. For example, and without limitation, the first purge gas may include nitrogen, argon, helium, xenon, or a combination thereof. The first purge gas may be introduced for a second predetermined period of time at a flow rate of about 100 seem to about 500 seem, e.g., about 100 seem to about 450 seem, about 150 seem to about 400 seem, about 200 seem to about 400 seem, or about 250 seem to about 350 seem. The second predetermined period of time may range from about 5 s to about 20 s, e.g., about 5 s to about 18 s, about 6 s to about 15 s, about 8 s to about 13 s, or about 9 s to about 11 s. For example, the second predetermined period of time may be 10 s. Without being bound by theory, a second predetermined period of time of about 1 s to about 20 s can provide saturation of the surface, thereby purging the first precursor from the surface.
[0029] At operation 403, a second precursor is introduced in a processing chamber for a third predetermined period of time. The second precursor may include any reactive precursor capable of bonding to or reacting with the first precursor bonded to the micro-lens. The second precursor may include water vapor. Without being bound by theory, a second precursor of water vapor can allow for low-temperature processing. The third predetermined period of time may range from 0.1 s to about 10 s, e.g., about 0.1 s to about 5 s, about 0.1 sto about 1 s, or about 0.1 s to about 0.5 s. For example, the second precursor may be introduced into the process chamber for a period of 0.2 s. Without being bound by theory, a first predetermined amount of time of about 0.1 s to about 10 s can provide a film having a uniform thickness on the plurality of micro-lenses.
[0030] At operation 404, a second purge gas may be introduced to purge the second precursor from the chamber. The second purge gas may include any of the first inert gas, as described in the present disclosure. The second purge gas can include an inert gas capable of diluting and / or purging the second precursor from the chamber. For example, and without limitation, the second purge gas may include nitrogen, argon, helium, xenon, or a combination thereof. In some embodiments, which may be combined with other embodiments described herein, the second purge gas is the same as the first purge gas. In some embodiments, which may be combined with other embodiments described herein, the second purge gas is different than the first purge gas.
[0031] The second purge gas may be introduced for a fourth predetermined period of time. The fourth predetermined period of time may range from about 5 s to about 20 s. For example, the fourth predetermined period of time may be 10 s. Without being bound by theory, a second predetermined period of time of about 5 s to about 20 s can provide saturation of the surface, thereby purging the second precursor from the surface.
[0032] At operation 405, the processes above may be iteratively cycled until a desired thickness of the deposited chemical is achieved. In some embodiments, the process may be cycled for about 10 cycles to about 500 cycles, e.g., about 10 cycles to about 400 cycles, about 20 cycles to about 300 cycles, or about 20 cycles to about 250 cycles. For example, the processes of operations 401 , 402, 403, and 404 may be iteratively cycled to deposit an aluminum oxide encapsulation layer of about 1 nm to about 10 nm, e.g., about 1 nm to about 8 nm, about 2 nm to about 7 nm, or about 2 nm to about 5 nm. In some embodiments, which may be combined with other embodimentsdescribed herein, each iterative cycle may deposit 0.01 nm per cycle to about 0.5 nm per cycle of aluminum oxide, e.g., e.g., about 0.01 nm per cycle to about 0.4 nm per cycle, about 0.05 nm per cycle to about 0.3 nm per cycle, about 0.07 nm per cycle to about 0.2 nm per cycle, or about 0.09 nm per cycle to about 0.011 nm per cycle. The deposition process may be repeated to provide a thickness of aluminum oxide of about 1 nm to about 100 nm. For example, the processes may be iteratively cycled 50 times at a deposition rate of about 0.1 nm per cycle to produce a 5 nm thick encapsulation layer of aluminum oxide on the micro-lens. As a further example, the processes may be iteratively cycled 20 times at a deposition rate of about 0.1 nm per cycle to produce a 2 nm thick encapsulation layer of aluminum oxide on the micro-lens.
[0033] Overall, the present disclosure provides devices and methods of manufacturing thereof having a micro-lens encapsulation layer deposited over a micro-lens. The micro-lens encapsulation layer can include a metal oxidepolymer, e.g., aluminum oxide or a silica containing material, that can improve thermal stability of devices to up to about 200 °C. Moreover, the micro-lens encapsulation layer can be about 2 nm thick, while still providing thermal stability and retaining a percent transmittance of greater than about 80%. The present disclosure also provides a low temperature deposition process for depositing a micro-lens encapsulation layer, thereby reducing thermal damage to a device during the manufacturing processes. While the foregoing is directed to embodiments of the present disclosure, other and further embodiments of the disclosure may be devised without departing from the basic scope thereof, and the scope thereof is determined by the claims that follow.
Claims
What is claimed is:
1. A device, comprising: a backplane; at least three micro-LEDs disposed on the backplane; subpixel isolation (SI) structures disposed on the backplane to define wells of at least three subpixels, wherein the at least three of the subpixels have a color conversion material disposed in the wells; an encapsulation layer disposed over the SI structures and the subpixels; a plurality of micro-lens disposed over the encapsulation layer, each micro-lens of the plurality of micro-lens disposed over a respective well of the at least three subpixels; and a micro-lens encapsulation layer having a thickness of about 1 nanometer (nm) to about 100 nm disposed on the micro-lenses, wherein the micro-lens encapsulation layer is a metal oxide layer or a silicon-containing layer.
2. The device of claim 1 , wherein the micro-lens encapsulation layer is selected from aluminum oxide, titanium oxide, hafnium oxide, tantalum oxide, silicon oxide, and silicon nitride.
3. The device of claim 1 , wherein the metal oxide layer is aluminum oxide.
4. The device of claim 1 , wherein the thickness of the micro-lens encapsulation layer is 1 nm to about 10 nm.
5. The device of claim 4, wherein the thickness of the micro-lens encapsulation layer is about 2 nm.
6. The device of claim 1 , wherein the at least three subpixels have a different color conversion material.
7. The device of claim 6, wherein the at least three subpixels have a similar color conversion material.
8. The device of claim 1 , further comprising a fourth subpixel, wherein a respective well of the fourth subpixel comprises a sacrificial material.
9. A method, comprising: depositing a resist over an encapsulation layer of a pixel, the encapsulation layer disposed over subpixel isolation structures above micro-LEDs and a backplane; patterning the resist disposed over the encapsulation layer; forming a micro-lens from the resist using a modification process; and depositing a micro-lens encapsulation layer on the micro-lens, the micro-lens encapsulation layer having a thickness of about 1 nanometer (nm) to about 100 nm disposed on the micro-lenses, wherein the micro-lens encapsulation layer is a metal oxide layer or a silicon-containing layer.
10. The method of claim 9, wherein the modification process is a thermal reflow process.11 . The method of claim 9, wherein depositing the micro-lens encapsulation layer comprises using an atomic layer deposition process.
12. The method of claim 11 , wherein the atomic layer deposition process is iteratively cycled for about 10 cycles to about 500 cycles.
13. The method of claim 12, wherein each iterative cycle deposits an encapsulation layer of about 0.1 nm.
14. The method of claim 11 , wherein the atomic layer deposition process is iteratively cycled for about 10 cycles to about 250 cycles.
15. The method of claim 14, wherein the micro-lens encapsulation layer comprises a thickness of about 1 nm to about 25 nm.
16. The method of claim 11 , wherein the atomic layer deposition process is performed at a temperature of about 50 °C to about 100 °C.
17. The method of claim 9, wherein the micro-lens encapsulation layer is selected from aluminum oxide, titanium oxide, hafnium oxide, tantalum oxide, silicon oxide, and silicon nitride.
18. A method, comprising: depositing a resist over an encapsulation layer of a pixel, the encapsulation layer disposed over subpixel isolation structures above micro-LEDs and a backplane; patterning the resist disposed over the encapsulation layer; forming a micro-lens from the resist using an atomic layer deposition process; and depositing a micro-lens encapsulation layer on the micro-lens, the micro-lens encapsulation layer having a thickness of about 1 nanometer (nm) to about 100 nm disposed on the micro-lenses, wherein the micro-lens encapsulation layer is a metal oxide layer or a silicon-containing layer.
19. The method of claim 18, wherein the atomic layer deposition process is iteratively cycled for about 10 cycles to about 500 cycles.
20. The method of claim 18, wherein each iterative cycle deposits an encapsulation layer of about 0.1 nm.
Citation Information
Patent Citations
Micro LED micro-display chip and manufacturing method thereof
CN115472730A
Solid state image sensor and method of the same
KR1020030016850A
Method for transferring wafer and apparatus for transferring wafer
KR1020230124483A
Display panel and manufacturing method thereof, and display device
US20200335723A1
Image display device
US20210005583A1