Lamination adhesive
Patent Information
- Application Number
- PCT/FR2024/050559
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-05-03
- Filing Date
- 2024-04-30
- Publication Date
- 2024-11-07
Smart Images

Figure IMGF000006_0001 
Figure IMGF000006_0002 
Figure IMGF000007_0001
Abstract
Description
[0001] LAMINATION ADHESIVE FIELD OF THE INVENTION The present invention relates to a polyurethane-type adhesive composition. The invention also relates to a multilayer (or complex) structure, usable in particular in the field of flexible packaging, which comprises at least two layers of material bonded together by a crosslinked layer of the composition according to the invention. The present invention also relates to the use of said multilayer structure for the preparation of flexible packaging for agri-food products. TECHNOLOGICAL BACKGROUND Flexible (or supple) packaging intended, in particular, for packaging agri-food products, generally consists of several thin layers (in the form of sheets or films) whose thickness is between 5 and 150 µm and which are made of different materials such as paper,a metal (for example aluminum) or by thermoplastic polymers. These thin layers are bonded together by gluing, and the corresponding complex (or multi-layer) film, the thickness of which can vary from 20 to 400 µm, makes it possible to combine the properties of the different individual layers of material (also called "supports") and thus offer the consumer a set of characteristics adapted to the final flexible packaging such as, for example, its visual appearance (in particular that of the printed elements presenting the information concerning the packaged product and intended for the consumer, or its transparency), a barrier effect to light or atmospheric humidity or gases, in particular oxygen, food contact without risk of toxicity or organoleptic properties of the packaged food, or appropriate heat resistance (in particular,the adhesive joint formed by crosslinking the adhesive layer connecting the individual layers of the packaging must retain a sufficient level of cohesion after heat treatment, in order to avoid any delamination phenomenon). The various layers of materials that make up the multilayer film are typically combined or assembled by lamination, during industrial laminating (or "lamination") processes. These processes use adhesives (or glues) and equipment (or machines) that are designed for this purpose and that operate continuously with generally very high line speeds, of the order of several hundred meters per minute. The multilayer film thus obtained is often itself referred to as "laminated". These lamination processes firstly comprise a step of coating the adhesive on a first film of material,which consists of depositing a continuous layer of glue with a controlled thickness generally less than 10 µm, corresponding to a quantity of glue (or weight) generally not exceeding 10 g / m, 2This coating step is followed by a laminating step of a second film of material, identical or different from the first, consisting of the application under pressure of this second film on the first film covered with the layer of glue. The complex films are thus finally obtained in very large width and are generally packaged by winding, in the form of large reels of 1 m to 1.50 m in diameter having, like the film they store, up to 2 m in width. These large reels can be stored and transported, for use either directly by food manufacturers, for the packaging of their product, or by converters (or complexers, also known by the English term "converters"). In both cases, the film is cut to reduce its width, and shaped to make bags, themselves intended for the packaging of a product, for example an agri-food product.Two-component polyurethane laminating adhesives with solvent are widely used as glue for the manufacture of multi-layer systems intended for the field of flexible packaging. The implementation of said solvent-based adhesives in the laminating process requires an evaporation step of the organic solvent. This step is carried out before the laminating step by passing the first film covered with glue through an oven following the coating step. Two-component polyurethane laminating adhesives with solvent are supplied to the laminating machine in the form of 2 compositions (or components): - one (called -NCO component) comprising chemical entities carrying isocyanate end groups –NCO, and - the other (called -OH component) comprising chemical entities carrying hydroxyl end groups –OH.The mixing of these 2 components can be carried out at room temperature by the operator of the laminating machine before starting it up, which allows it to function correctly, thanks to an appropriate viscosity obtained where appropriate by adding solvent. At the end of the coating step of the mixture thus obtained on the 1. ère thin layer, and the counter-gluing step of the 2 èmelayer, the isocyanate groups of the -NCO component react with the hydroxyl groups of the -OH component, according to a so-called crosslinking reaction, to form a polyurethane which is in the form of a three-dimensional network with urethane groups, ensuring the cohesion of the adhesive joint between the 2 laminated thin layers. However, polyurethane-based adhesive compositions generally have the disadvantage of using a majority NCO-terminated NCO component comprising significant residual contents of diisocyanate monomers originating from the synthesis reaction of the NCO-terminated polyurethane prepolymer. These residual quantities of diisocyanate monomers (so-called free) of low molecular weight are likely to migrate through the multilayer film, after the implementation of the two-component adhesive, and therefore through the final flexible packaging.Thus, these compounds are likely to form, by hydrolysis, upon contact with water or moisture present in particular in packaged foods, primary aromatic amines (often referred to by the English terms Primary Aromatic Amines or PAA), which are considered very harmful to human health and the environment. Furthermore, certain polyurethane-based adhesive compositions can lead to good cohesion before or after heat treatment of a multilayer film containing it. However, such compositions suffer from a performance problem over time. Indeed, the adhesive composition, once prepared, is not necessarily directly used by the complexers to prepare the multilayer systems, but stored for several days or even several months before use. It is important that the adhesive can be just as effective as a "fresh" adhesive (after preparation) even after storage.In particular, it is important that the adhesive can lead to multilayer structures having good cohesion before and after heat treatment, and this after aging of said adhesive (for example after storage at 23°C for one to several months of the adhesive composition). There is therefore a need for a new adhesive composition responding at least in part to at least one of the problems raised. There is in particular a need to provide an adhesive composition leading to a multilayer structure having good resistance to heat treatment, preferably good thermal resistance with respect to the sterilization and / or pasteurization test, before and after aging of the adhesive composition.More particularly, there is a need for new adhesive compositions having a good compromise between a reduced level of residual monomers, an ability to crosslink at 23°C, good adhesive properties before and after heat treatment and even after aging of the adhesive composition. DESCRIPTION OF THE INVENTION Composition The present invention relates to an adhesive composition comprising an -OH component and an -NCO component characterized in that: - the -NCO component is a composition comprising at least one polyisocyanate; - the -OH component is a composition comprising at least one polyurethane P2 comprising at least one hydroxyl terminal function and at least one silylated terminal function. Preferably, the polyurethane P2 is a polyester polyol-based polyurethane.In the context of the invention, and unless otherwise stated, the term "polyester polyol-based polyurethane" means a polyurethane prepared from at least one polyester polyol, preferably from only polyester polyol(s) as polyol(s). Component -NCO Polyisocyanate The polyisocyanate may be chosen from diisocyanates, triisocyanates, and mixtures thereof.Examples of diisocyanates include the group consisting of isophorone diisocyanate (IPDI), pentamethylene diisocyanate (PDI), hexamethylene diisocyanate (HDI), heptane diisocyanate, octane diisocyanate, nonane diisocyanate, decane diisocyanate, undecane diisocyanate, dodecane diisocyanate, 4,4'-methylenebis(cyclohexylisocyanate) (4,4'-HMDI), norbornane diisocyanate, norbornene diisocyanate, 1,4-cyclohexane diisocyanate (CHDI), methylcyclohexane diisocyanate, ethylcyclohexane diisocyanate, propylcyclohexane diisocyanate, methyldiethylcyclohexane diisocyanate, cyclohexane dimethylene diisocyanate, 1,5- diisocyanato-2-methylpentane (MPDI), 1,6-diisocyanato-2,4,4-trimethylhexane, 1,6- diisocyanato-2,2,4-trimethylhexane (TMDI), 4-isocyanatomethyl-1,8-octane diisocyanate (TIN), (2,5)-bis(isocyanatomethyl)bicyclo[2.2.1]heptane (2,5-NBDI), (2,6)- bis(isocyanatomethyl)bicyclo[2.2.1]heptane (2,6-NBDI), 1,3-bis(isocyanatomethyl)cyclohexane (1,3-H6-XDI), 1,4-bis(isocyanatomethyl)cyclohexane (1,4-H6-XDI), xylylene diisocyanate (XDI) (in particular m-xylylene diisocyanate (m-XDI)), toluene diisocyanate (in particular 2,4-toluene diisocyanate (2,4-TDI) and / or 2,6-toluene diisocyanate (2,6-TDI)), diphenylmethane diisocyanate (in particular 4,4'-diphenylmethane diisocyanate (4,4'-MDI) and / or 2,4'-diphenylmethane diisocyanate (2,4'-MDI)), tetramethylxylylene diisocyanate (TMXDI) (in particular tetramethyl (meta)xylylene diisocyanate), of an allophanate of PDI (n = 5) or of HDI (n = 6) having for example the following formula (Y):. in which p is an integer ranging from 1 to 2, q is an integer ranging from 0 to 9, and preferably 2 to 5, R crepresents a hydrocarbon chain, saturated or unsaturated, cyclic or acyclic, linear or branched, comprising from 1 to 20 carbon atoms, preferably from 6 to 14 carbon atoms, R drepresents a divalent alkylene group, linear or branched, having from 2 to 4 carbon atoms, and preferably a divalent propylene group; and mixtures thereof. The diisocyanates are preferably arylaliphatic or cycloaliphatic diisocyanates. Preferably, the diisocyanates are chosen from isophorone diisocyanate (IPDI), xylylene diisocyanate (XDI) (in particular m-xylylene diisocyanate (m-XDI)) and allophanates of HDI or PDI. Among the triisocyanates, mention may be made, for example, of isocyanurates, biurets, and adducts of diisocyanates and triols. The isocyanurates may be used in the form of a technical mixture of (poly)isocyanurate(s) with a purity greater than or equal to 70% by weight of isocyanurate(s). Examples of diisocyanate trimers include: - hexamethylene diisocyanate (HDI) isocyanurate trimer: , - isocyanurate trimer of isophorone diisocyanate (IPDI): As an example of adducts of diisocyanates and triols that can be used according to the invention, mention may be made of the adduct of meta-xylylene diisocyanate (m-XDI) with a triol. Such adducts can typically be obtained by addition reaction using said compounds. The methods of such an addition reaction are for example described in EP3101044. The triol used is preferably a trimethylolalkane comprising an alkane comprising from 1 to 20 carbon atoms and 3 methylol groups such as, for example, trimethylolmethane, trimethylolethane, trimethylolpropane, tri-methyloln-butane, trimethylolisobutane, trimethylols-butane, trimethylolt-butane, trimethylolpentane, trimethylolhexane, trimethylolheptane, trimethyloloctane, trimethylolnonane, trimethyloldecane, trimethylolundecane, and trimethyloldo-decane.More preferably, among the triols that can be used to obtain the adduct of m-XDI and triol, mention may be made of Glycerol of formula HOH2C-CHOH-CH2OH, Trimethylolmethane (TMM) of formula HC(CH2-OH)3, Trimethylolethane (TME) of formula H3C-C(CH2-OH)3 and Trimethylolpropane (TMP) of formula CH3-CH2-C(CH2-OH)3. Preferably, the adduct of diisocyanates and triols is the adduct of m-XDI and TMP, of the following formula:. Adducts of m-XDI and triol are also commercially available. For example, the adduct of m-XDI and TMP is available, in solution in 75% ethyl acetate, from MITSUI CHEMICALS under the name TAKENATE. ® D-110N. The adduct of m-H6XDI and TMP is also available, in solution in 75% ethyl acetate, from MITSUI CHEMICALS under the name TAKENATE ®D-120N. Polyisocyanates are widely available commercially. For example, mention may be made of “SCURANATE® TX” marketed by the company VENCOREX, corresponding to a 2,4-TDI with a purity of around 95%, “SCURANATE® T100” marketed by the company VENCOREX, corresponding to a 2,4-TDI with a purity greater than 99% by weight, “DESMODUR® I” marketed by the company COVESTRO, corresponding to an IPDI. Preferably, the polyisocyanate is an aliphatic, arylaliphatic or cycloaliphatic polyisocyanate. Preferably, the polyisocyanate is a triisocyanate, and more preferably an adduct of m-XDI and triol. Even more preferably, the polyisocyanate is the adduct of m-XDI and Trimethylolpropane (TMP). Additives The –NCO component may comprise at least one additive selected from the group consisting of plasticizers, catalysts, rheological agents, solvents, pigments, adhesion promoters, moisture absorbers,UV stabilizers (or antioxidants), colorants, fillers, and mixtures thereof. The -NCO component may comprise at least one solvent, preferably in an amount ranging from 10% to 60% by weight, more preferably ranging from 15% to 50% by weight, and even more preferably from 20 to 45% by weight, relative to the total weight of the -NCO component. The solvent may be chosen from organic and alcoholic solvents such as ethyl acetate, methyl ethyl ketone, acetone, xylene, ethanol, isopropanol, tetrahydrofuran, methyl-tetrahydrofuran, or from "ISANE®" (based on isoparaffins, available from TOTAL) or "EXXOL® D80" (based on aliphatic hydrocarbons, available from EXXON MOBIL CHEMICAL). Preferably, the –NCO component comprises ethyl acetate. According to a preferred embodiment, the –NCO component comprises: - from 30% to 90% by weight,more preferably from 40% to 80% by weight of polyisocyanate(s) (dry extract); - from 10% to 60% by weight, more preferably ranging from 15% to 50% by weight of solvent(s); the percentages being percentages by weight relative to the total weight of said -NCO component. The -NCO component can be prepared by simple mixing of the ingredients at 23°C, if necessary with stirring. -OH component The -OH component is a composition comprising at least one polyurethane P2 comprising at least one hydroxyl terminal function and at least one silylated terminal function. The polyurethane P2 is preferably obtained by a process comprising the following steps: E1) the preparation of a composition comprising at least one polyurethane P1 comprising at least one -NCO terminal function and at least one -OH terminal function,by a polyaddition reaction: i) of at least one polyester polyol A1; ii) of at least one polyisocyanate P'; iii) of an optional polyol A2 different from A1; in amounts such that the NCO / OH molar ratio (r1) is less than 1; E2) the reaction of the composition formed in step E1 with at least one aminosilane. Preferably, in step E2), the reaction takes place in amounts such that the NCO / NH molar ratio (r2) ranges from 1.5 to 5.2 and even more preferably from 1.5 to 4.5. Polyester polyol A1 Reaction E1) can be carried out with a polyester polyol A1 or a mixture of different polyester polyols A1. Preferably,in the presence of a mixture of different polyester polyols A1. Polyester polyol A1 may have a number-average molecular weight Mn greater than or equal to 1000 g / mol. Polyester polyol A1 may have a number-average molecular weight ranging from 2400 to 12000 g / mol. greater than or equal to 10000 g / mol. The number-average molecular weight Mn is measured by size exclusion chromatography (or SEC, acronym for "Size Exclusion Chromatography") which is also referred to by the terms gel permeation chromatography (or by the corresponding English acronym GPC). The calibration implemented is usually a PEG (PolyEthyleneGlycol) or PS (PolyStyrene) calibration, preferably PS. The hydroxyl number (denoted IOH) of polyester polyol A1, and more generally of a polyol,(noted IOH) represents the number of hydroxyl functions per gram of polyol and is expressed in the form of the equivalent number of milligrams of potash (KOH) used in the determination of hydroxyl functions, determined by titrimetry according to ISO 14900:2017. The IOH is related to the number-average molecular mass Mn by the relationship: IOH = (56.1 xfx 1000) / Mn f being the average functionality of the polyester polyol Among the polyester polyols, we can for example cite: - polyester polyols of natural origin such as castor oil; - polyester polyols resulting from the polycondensation of: - one or more aliphatic (linear, branched or cyclic) or aromatic polyols such as, for example, monoethylene glycol, diethylene glycol, 1,2-propanediol, 1,3-propanediol, 1,4-butanediol, butenediol, 1,6-hexanediol, cyclohexane dimethanol, tricyclodecane dimethanol, neopentyl glycol, cyclohexane dimethanol, glycerol,trimethylolpropane, 1,2,6-hexanetriol, sucrose, glucose, sorbitol, pentaerythritol, mannitol, N-methyldiethanolamine, triethanolamine, a dimeric fatty alcohol, a trimer fatty alcohol and mixtures thereof, with - one or more polycarboxylic acids or their ester or anhydride derivatives such as 1,6-hexanedioic acid (adipic acid), dodecanedioic acid, azelaic acid, sebacic acid, 1,18-octadecanedioic acid, phthalic acid, isophthalic acid, terephthalic acid, succinic acid, a dimeric fatty acid, a trimer fatty acid and mixtures of these acids, an unsaturated anhydride such as, for example, maleic or phthalic anhydride, or a lactone such as, for example, caprolactone. - estolide polyols resulting from the polycondensation of one or more hydroxy acids, such as ricinoleic acid,on a diol (for example, we can cite “POLYCIN® D-1000” and “POLYCIN® D-2000” available from VERTELLUS). The aforementioned polyester polyols can be prepared conventionally, and are for the most part commercially available. The polyester polyol A1 is preferably a copolyester obtained by a polycondensation reaction: - of at least one aliphatic diol (a); with - at least one aromatic diacid (b) chosen from terephthalic acid, isophthalic acid, phthalic acid, one of their diester or anhydride derivatives, and mixtures thereof; and - at least one aliphatic diacid (c) or one of its diester or anhydride derivatives. The aliphatic diol (a) may be linear or branched and is selected from the group consisting of ethylene glycol (CAS: 107-21-1), diethylene glycol, triethylene glycol, tetraethylene glycol, 1,2-propanediol, dipropylene glycol, tripropylene glycol, tetrapropylene glycol, 1,6-hexanediol, 3-ethyl-2-methyl-1,5-pentanediol, 2-ethyl-3-propyl-1,5-pentanediol, 2,4-dimethyl-3-ethyl-1,5-pentanediol, 2-ethyl-4-methyl-3-propyl- 1,5-pentadiol, 2,3-diethyl-4-methyl-1,5-pentanediol, 3-ethyl-2,2,4-trimethyl-1,5-pentanediol, 2,2-dimethyl-4-ethyl-3-propyl-1,5-pentanediol, 2-methyl-2-propyl-1,5-pentanediol, 2,4-dimethyl-3-ethyl-2-propyl-1,5-pentanediol, 2,3-dipropyl-4-ethyl-2-methyl-1,5-pentanediol, 2-butyl-2-ethyl-1,5-pentanediol, 2-butyl-2,3-diethyl-4-methyl-1,5-pentanediol, 2-butyl-2,4-diethyl-3-propyl-1,5-pentanediol, 3-butyl-2-propyl-1,5-pentanediol, 2-methyl-1,5-pentanediol (CAS: 42856-62-2), 3-methyl-1,5-pentanediol (MPD, CAS: 4457-71-0), 2,2-dimethyl-1,3-pentanediol (CAS: 2157-31-5), 2,2-dimethyl-1,5-pentanediol (CAS: 3121-82-2), 3,3-dimethyl-1,5-pentanediol (CAS: 53120-74-4), 2,3-dimethyl-1,5-pentanediol (CAS: 81554-20-3), 2,2-dimethyl-1,3-propanediol (Neopentylglycol - NPG, CAS: 126-30-7), 2,2-diethyl-1,3-propanediol (CAS: 115-76-4), 2-methyl-2-propyl-1,3-propanediol (CAS: 78-26-2), 2-butyl-2-ethyl-1,3-propanediol (CAS: 115-84-4), 2-methyl-1,3-propanediol (CAS: 2163-42-0), 2-benzyloxy-1,3-propanediol (CAS: 14690-00-7), 2,2-dibenzyl-1,3-propanediol (CAS: 31952-16-6), 2,2-dibutyl-1,3-propanediol (CAS: 24765-57-9), 2,2-diisobutyl-1,3-propanediol, 2,4-diethyl-1,5- pentanediol, 2-ethyl-1,6-hexanediol (CAS: 15208-19-2), 2,5-dimethyl-1,6-hexanediol (CAS: 49623-11-2), 5-methyl-2-(1-methylethyl)-1,3-hexanediol (CAS: 80220-07-1), 1,4-dimethyl-1,4-butanediol, 1,5-hexanediol (CAS: 928-40-5), 3-methyl-1,6-hexanediol (CAS: 4089-71-8), 3-tert-butyl-1,6-hexanediol (CAS: 82111-97-5), 1,3-heptanediol (CAS: 23433-04-7), 1,2-octanediol (CAS: 1117-86-8), 1,3-octanediol (CAS: 23433-05-8), 2,2,7,7-tetramethyl-1,8-octanediol (CAS: 27143-31-3), 2-methyl-1,8-octanediol (CAS: 109359-36-6), 2,6-dimethyl-1,8-octanediol (CAS: 75656-41-6), 1,7-octanediol (CAS: 3207-95-2), 4,4,5,5-tetramethyl-3,6-dioxa-1,8-octanediol (CAS: 76779-60-7), 2,2,8,8-tetramethyl-1,9-Nonanediol (CAS: 85018-58-2), 1,2-nonanediol (CAS: 42789-13-9), 2,8-dimethyl-1,9-nonanediol (CAS: 40326-00-9), 1,5-nonanediol (CAS: 13686-96-9), 2,9-Dimethyl-2,9-dipropyl-1,10-decanediol (CAS: 85018-64-0), 2,9-Dibutyl-2,9-dimethyl-1,10-decanediol (CAS: 85018-65-1), 2,9-Dimethyl-2,9-dipropyl-1,10-decanediol (CAS: 85018-64-0), 2,9-Diethyl-2,9-dimethyl-1,10-decanediol (CAS: 85018-63-9), 2,2,9,9-tetramethyl-1,10-decanediol (CAS: 35449-36-6), 2-nonyl-1,10-decanediol (CAS: 48074-20-0), 1,9-decanediol (CAS: 128705-94-2), 2,2,6,6,10,10-hexamethyl-4,8-dioxa- 1,11-undecanediol (CAS: 112548-49-9), 1-phenyl-1,11-undecanediol (CAS: 109217-58-5), 2-octyl-1,11-undecanediol (CAS: 48074-21-1), 2,10-diethyl-2,10-dimethyl-1,11-undecanediol (CAS: 85018-66-2), 2,2,10,10-tetramethyl-1,11-undecanediol (CAS: 35449-37-7), 1-phenyl-1,11-undecanediol (CAS: 109217-58-5), 1,2-undecanediol (CAS: 13006-29-6), 1,2-dodecanediol (CAS: 1119-87-5), 2,11-dodecanediol (CAS: 33666-71-6), 2,11-diethyl-2,11-dimethyl-1,12-dodecanediol (CAS: 85018-68-4), 2,11-dimethyl-2,11-dipropyl-1,12-dodecanediol (CAS: 85018-69-5), 2,11-dibutyl-2,11-dimethyl-1,12-dodecanediol (CAS: 85018-70-8), 2,2,11,11-tetramethyl-1,12-dodecanediol (CAS: 5658-47-9), 1,11-dodecanediol (CAS: 80158-99-2), 11-methyl-1,7-dodecanediol (CAS: 62870-49-9), 1,4-dodecanediol (CAS: 38146-95-1), 1,3-dodecanediol (CAS: 39516-24-0), 1,10-dodecanediol (CAS: 39516-27-3), 2,11-dimethyl-2,11-dodecanediol (CAS: 22092-59-7), 1,5-dodecanediol (CAS: 20999-41-1), 6,7-dodecanediol (CAS: 91635-53-9), and cyclohexanedimethanol. Preferably, the diol (a) is selected from ethylene glycol, diethylene glycol, trimethylene glycol,hexamethylene glycol, propylene glycol (or propane-1,2-diol), propane-1,3-diol, butanediol (-1,4, -1,3 or -1,2), neopentyl glycol, 2-methyl-1,3-propane diol, hexane diol or cyclohexanedimethanol. According to a preferred variant, the diol (a) is chosen from ethylene glycol and diethylene glycol. Even more preferably, 2 diols (a) are used, consisting, respectively, of ethylene glycol and diethylene glycol. Among the diester derivatives of terephthalic acid, isophthalic acid or phthalic acid which can be used as monomers (b), mention may be made, for example, of dimethyl terephthalate or dimethyl isophthalate. As an example of an anhydride derivative of an aromatic diacid for the monomer (b), mention may be made of phthalic anhydride. Preferably, we use: - either 2 diacids (b) consisting, respectively,by terephthalic acid and isophthalic acid; - or isophthalic acid b). The aliphatic diacid (c) may be linear or branched and is, for example, chosen from adipic acid, azelaic acid, sebacic acid, cyclohexanedicarboxylic acid, dodecanedicarboxylic acid, 1,10-decanedicarboxylic acid and succinic acid. Preferably, adipic acid is used as aliphatic diacid (c). According to a preferred embodiment, the polyester polyol A1 is an amorphous polyester polyol. In the context of the invention, and unless otherwise stated, the term "amorphous polyester polyol" means a polyester polyol whose analysis by differential scanning calorimetry (DSC) shows that it does not have a melting point. According to a preferred embodiment, the polyester polyol A1 is obtained by polycondensation: - of 2 aliphatic diols (a) consisting, respectively,by ethylene glycol and diethylene glycol; with - either 2 diacids (b) consisting, respectively, of terephthalic acid and isophthalic acid; or isophthalic acid as acid b); and - adipic acid as aliphatic diacid (c). When some of the monomers (b) and optionally (c) are diester derivatives, such as, for example, methyl or ethyl diester derivatives, said monomers are, in a 1, ère step, mixed with one or more diol monomers (a), said mixture being brought to a temperature of up to 190°C, so as to carry out, preferably in the presence of a titanium or zinc-based catalyst, a transesterification reaction and eliminate the methanol or ethanol formed. In a 2 èmestep, the monomers (b) and optionally (c) which are diacids are added, mixed with one or more diol monomers (a), the reaction medium being brought to a temperature of up to 230°C, so as to carry out the esterification reaction and eliminate the water formed. Finally, in a 3 èmestep, the pressure is lowered to a value below approximately 5 mbar, and the reaction medium is brought to a higher temperature, up to 250°C, in order to increase the chain length of the polyester polyol to achieve a given IOH. The polyester polyol A1 may be in dry form or in solvent form. The solvent may, for example, be chosen from the group consisting of esters, ketones, aromatic compounds, and mixtures thereof. The solvent may, for example, be chosen from ethyl acetate, butyl acetate, methyl ethyl ketone, methyl isobutyl ketone, acetone, toluene, xylene, and mixtures thereof. When in solvent form, the dry extract content of the polyester polyol A1 preferably ranges from 40% to 70% by weight (relative to the total weight of solvent and polyester polyol A1). Polyisocyanate P' Polyisocyanate P' may be as described previously for the -NCO component.The polyisocyanate P' can be chosen from diisocyanates, triisocyanates, and their mixtures.Examples of diisocyanates include the group consisting of isophorone diisocyanate (IPDI), pentamethylene diisocyanate (PDI), hexamethylene diisocyanate (HDI), heptane diisocyanate, octane diisocyanate, nonane diisocyanate, decane diisocyanate, undecane diisocyanate, dodecane diisocyanate, 4,4'-methylenebis(cyclohexylisocyanate) (4,4'-HMDI), norbornane diisocyanate, norbornene diisocyanate, 1,4-cyclohexane diisocyanate (CHDI), methylcyclohexane diisocyanate, ethylcyclohexane diisocyanate, propylcyclohexane diisocyanate, methyldiethylcyclohexane diisocyanate, cyclohexane dimethylene diisocyanate, 1,5- diisocyanato-2-methylpentane (MPDI), 1,6-diisocyanato-2,4,4-trimethylhexane, 1,6- diisocyanato-2,2,4-trimethylhexane (TMDI), 4-isocyanatomethyl-1,8-octane diisocyanate (TIN), (2,5)-bis(isocyanatomethyl)bicyclo[2.2.1]heptane (2,5-NBDI), (2,6)- bis(isocyanatomethyl)bicyclo[2.2.1]heptane (2,6-NBDI), 1,3-bis(isocyanatomethyl)cyclohexane (1,3-H6-XDI), 1,4-bis(isocyanatomethyl)cyclohexane (1,4-H6-XDI), xylylene diisocyanate (XDI) (in particular m-xylylene diisocyanate (m-XDI)), toluene diisocyanate (in particular 2,4-toluene diisocyanate (2,4-TDI) and / or 2,6-toluene diisocyanate (2,6-TDI)), diphenylmethane diisocyanate (in particular 4,4'-diphenylmethane diisocyanate (4,4'-MDI) and / or 2,4'-diphenylmethane diisocyanate (2,4'-MDI)), tetramethylxylylene diisocyanate (TMXDI) (in particular tetramethyl (meta)xylylene diisocyanate), of an allophanate of PDI (n = 5) or of HDI (n = 6) having for example the following formula (Y):. in which p is an integer ranging from 1 to 2, q is an integer ranging from 0 to 9, and preferably 2 to 5, R crepresents a hydrocarbon chain, saturated or unsaturated, cyclic or acyclic, linear or branched, comprising from 1 to 20 carbon atoms, preferably from 6 to 14 carbon atoms, R drepresents a divalent alkylene group, linear or branched, having from 2 to 4 carbon atoms, and preferably a divalent propylene group; and mixtures thereof. Preferably, the polyisocyanate P' is chosen from toluene diisocyanate (in particular 2,4-toluene diisocyanate (2,4-TDI) and / or 2,6-toluene diisocyanate (2,6-TDI)), diphenylmethane diisocyanate (in particular 4,4'-diphenylmethane diisocyanate (4,4'-MDI) and / or 2,4'-diphenylmethane diisocyanate (2,4'-MDI)), isophorone diisocyanate (IPDI), xylylene diisocyanate (XDI) (in particular m-xylylene diisocyanate (m-XDI)) and allophanates of HDI or PDI. Even more preferably, the polyisocyanate P' is isophorone diisocyanate (IPDI). Optional polyol A2 When an optional polyol A2 is used in step E1), its mass content is lower than that of the polyester polyol A1 (or of the mixture of polyester polyols A1). The hydroxyl functionality of the polyol A2 can range from 2 to 6.The hydroxyl functionality is the average number of hydroxyl functions per mole of polyol. Polyol A2 may be chosen from polyether polyols, polyene polyols, polycarbonate polyols, and mixtures thereof. The polyethers may be chosen from polyoxyalkylene polyols, the alkylene part of which, linear or branched, comprises from 1 to 4 carbon atoms, more preferably from 2 to 3 carbon atoms. Examples of polyoxyalkylene diols or triols include: - polyoxypropylene diols or triols (also referred to as polypropylene glycol (PPG) diols or triols) having a number-average molecular weight (Mn) ranging from 300 to 12,000 g / mol; - polyoxyethylene diols or triols (also referred to as polyethylene glycol (PEG) diols or triols) having a number-average molecular mass (Mn) ranging from 300 to 12000 g / mol; - and mixtures thereof.The above-mentioned polyether polyols can be prepared conventionally and are widely commercially available. They can be obtained by polymerization of the corresponding alkylene oxide in the presence of a basic catalyst (e.g., potash) or a catalyst based on a double metal-cyanide complex. An example of a polyether diol is the polyoxypropylene diol sold under the name "VORANOL® P 400" by the company DOW, with a number-average molecular weight (Mn) of around 400 g / mol and a hydroxyl number ranging from 250 to 270 mg KOH / g.As an example of a polyether triol, mention may be made of the polyoxypropylene triol sold under the name "VORANOL® CP 450" by the company DOW, with a number-average molecular weight (Mn) of around 450 g / mol and a hydroxyl number ranging from 370 to 396 mg KOH / g, or the polyoxypropylene triol sold under the name "VORANOL® CP3355" by the company DOW, with a number-average molecular weight of around 3554 g / mol. The polyene polyols having a molecular weight greater than 200 g / mol may be chosen from polyenes comprising terminal hydroxyl groups, and their corresponding hydrogenated or epoxidized derivatives. The polyene polyols may be chosen from polybutadienes comprising terminal hydroxyl groups, optionally hydrogenated or epoxidized.Preferably, the polyene polyol(s) that can be used according to the invention is (are) chosen from butadiene homopolymers and copolymers comprising terminal hydroxyl groups, optionally hydrogenated or epoxidized. In the context of the invention, and unless otherwise stated, the term "terminal hydroxyl groups" of a polyene polyol means the hydroxyl groups located at the ends of the main chain of the polyene polyol. The hydrogenated derivatives mentioned above can be obtained by total or partial hydrogenation of the double bonds of a polydiene comprising terminal hydroxyl groups, and are therefore saturated or unsaturated. The epoxidized derivatives mentioned above can be obtained by chemoselective epoxidation of the double bonds of the main chain of a polyene comprising terminal hydroxyl groups, and therefore comprise at least one epoxy group in its main chain.Examples of polyene polyols include saturated or unsaturated butadiene homopolymers comprising terminal hydroxyl groups, optionally epoxidized, such as those marketed under the name “POLY BD® or KRASOL®” by the company CRAY VALLEY. The polycarbonate polyols may be chosen from polycarbonate diols or triols, having in particular a number-average molecular weight (M. n ) ranging from 300 to 12000 g / mol. As an example of polycarbonate diol, we can for example cite “CONVERGE® POLYOL 212-10” and “CONVERGE® POLYOL 212-20” marketed by the company NOVOMER respectively with number-average molecular weight (M n) equal to 1000 and 2000 g / mol whose hydroxyl indices are respectively 112 and 56 mg KOH / g. Preferably, step E1) is not carried out with optional polyols A2 (only polyester polyol(s) A1 as polyols). Preferably, the polyurethane P2 is obtained by a process comprising the following steps: E1) the preparation of a composition comprising at least one polyurethane P1 comprising at least one -NCO terminal function and at least one -OH terminal function, by a polyaddition reaction: i) of at least one polyester polyol A1; ii) of at least one polyisocyanate P'; in amounts such that the NCO / OH molar ratio (r1) is less than 1; E2) the reaction of the composition formed in step E1 with at least one aminosilane. Step E1 – synthesis of polyurethane P1 During step E1, the polyaddition reaction can be carried out at a temperature ranging from 50°C to 100°C, preferably from 60° to 80°C.In the context of the invention, and unless otherwise stated, r1 is the NCO / OH molar ratio corresponding to the molar ratio of the number of isocyanate groups (NCO) to the number of hydroxyl groups (OH) carried by all the polyisocyanate(s) and polyol(s) present in the reaction medium of step E1. Preferably, the ratio r1 ranges from 0.25 to 0.95, even more preferably from 0.40 to 0.80. The polyaddition reaction of step E1 can be carried out in the presence or absence of at least one reaction catalyst. The catalyst can be any catalyst known to those skilled in the art for catalyzing the formation of polyurethane by reaction of at least one polyisocyanate with at least one polyol. An amount of up to 0.3% by weight of catalyst(s) relative to the weight of the reaction medium of step E1 can be used. The reaction of step E1 can also be carried out in the presence of a solvent.The solvent may be chosen from the group consisting of esters, ketones, aromatic compounds, and mixtures thereof. The solvent may be added during step E1 or may come from the starting reagents in solution in said solvent. The solvent may, for example, be chosen from the group consisting of esters, ketones, aromatic compounds, and mixtures thereof. The solvent may, for example, be chosen from ethyl acetate, butyl acetate, methyl ethyl ketone, methyl isobutyl ketone, toluene, xylene, and mixtures thereof. The polyurethane P1 is preferably a polyester polyol-based polyurethane. The polyurethane P1 preferably has an NCO group content ranging from 0.10 to 0.90%, more preferably from 0.15 to 0.75%. Step E1 preferably leads to a composition comprising at least one polyurethane P1 as described in the present application, in a mixture with other polymer(s) such as a pre-polymer terminated with at least two OH functions.Step E2 is advantageously carried out before the disappearance of the polyurethane P1 (before all the -NCO functions have reacted). Step E2 is advantageously carried out without isolation of the polyurethane P1. The polyurethane P1 typically has a number-average molecular weight lower than that of the polyurethane P2. Step E2 – Synthesis of the polyurethane P2 Step E2 can be carried out at a temperature below 95°C, for example between 40°C and 80°C. In the context of the invention, and unless otherwise stated, r2 is the NCO / NH molar ratio corresponding to the molar ratio of the number of NCO isocyanate groups to the number of NH functions carried respectively by all the isocyanates (in particular the polyurethane P1), and the aminosilanes (present in the medium of step E2). The ratio r2 preferably ranges from 1.5 to 5.2, more preferably from 1.5 to 4.5.The polyaddition reaction of step E2 may be carried out in the presence or absence of at least one reaction catalyst. The catalyst may be any catalyst known to those skilled in the art. An amount of up to 0.3% by weight of catalyst(s) relative to the weight of the reaction medium of step E2 may be used. The reaction of step E2 may also be carried out in the presence of a solvent. The solvent may be chosen from the group consisting of esters, ketones, aromatic compounds, and mixtures thereof. The solvent may be added during step E1, during step E2 or may come from the starting reagents in solution in said solvent. The solvent may, for example, be chosen from ethyl acetate, butyl acetate, acetone, methyl ethyl ketone, methyl isobutyl ketone, toluene, xylene, and mixtures thereof.Step E2 preferably leads to a composition comprising at least one polyurethane P2 as described in the present application, in a mixture with other polymer(s) such as for example a polymer terminated with at least two OH functions. Aminosilane The aminosilanes contain in particular an amine function as a reactive function with the –NCO function of the polyurethane P1 obtained at the end of step E1. The aminosilane preferably has the following formula (I): (R. 4 O) 3-r (R 3 ) r Si-R 1 -NH-R 2 (I) in which: - R 3 , identical or different, each represents a linear or branched monovalent hydrocarbon radical comprising from 1 to 10 carbon atoms; - R 4 , identical or different, represents a linear or branched monovalent hydrocarbon radical comprising from 1 to 10 carbon atoms, or two R groups 4can form a cycle; - r is an integer equal to 0, 1 or 2, preferably equal to 0 or 1, and even more preferably equal to 0; - R 1 represents a linear or branched divalent alkylene radical comprising from 1 to 12 carbon atoms, preferably from 1 to 6 carbon atoms, R 3 preferentially representing methylene or n-propylene, and - R 2 represents H, a linear or branched alkyl radical, an arylalkyl radical, a cyclic radical comprising from 1 to 20 carbon atoms, or a radical having the following formula (II): in which: - R 7 and R 8 are independently of each other, a hydrogen or a radical chosen from the group consisting of –R 9 , -COOR 9 and –CN; - the radical R 10 is hydrogen, or a radical selected from the group consisting of – CH2-COOR 9 , -COOR 9 , -CONHR 9 , -CON(R 9 )2, -CN; - the radical R 9being a hydrocarbon radical having from 1 to 20 carbon atoms optionally comprising at least one heteroatom. In particular, the radical of formula (II) may be chosen from one of the following radicals: in which R 9 is as defined above. According to a preferred embodiment, the aminosilane of formula (I) is that in which: - R 3 , identical or different, each represents a linear or branched alkyl group comprising from 1 to 10 carbon atoms, preferably from 1 to 5 carbon atoms; - R 4 , identical or different, each represents a linear or branched alkyl comprising from 1 to 10 carbon atoms, preferably from 1 to 5 carbon atoms, - r is an integer equal to 0, 1 or 2, preferably p is 0; - R 1 represents a linear or branched divalent alkylene radical comprising from 1 to 12 carbon atoms, preferably from 1 to 6 carbon atoms, R 1preferentially representing n-propylene, and - R 2represents H. The aminosilanes of formula (I) above are preferably primary aminosilanes such as, for example, 3-aminopropyltrimethoxysilane, 3-aminopropyltriethoxysilane, 3-aminopropyldiethoxymethylsilane, 3-aminopropyldimethoxymethylsilane; secondary aminosilanes such as, for example, N-butyl-3-aminopropyltrimethoxysilane, N-butyl-3-aminopropyltriethoxysilane, N-phenyl-3-aminopropyltrimethoxysilane, N-phenyl-3-aminopropyltriethoxysilane; the products of the Michael addition reaction of primary aminosilanes such as for example 3-aminopropyltrimethoxysilane or 3-aminopropyldimethoxymethylsilane with Michael acceptors such as for example acrylonitrile, acrylic esters, acrylamides, maleic diesters, methylene malonate diesters, itaconic diesters. Preferably, the aminosilane is 3-aminopropyltrimethoxysilane.Aminosilanes may be commercially available, such as, for example, Dynasylan® 1189 marketed by Evonik, or SILQUEST® A1110 marketed by Momentive. Polyester polyol-based polyurethane P2 The –OH component may comprise from 20% to 100% by weight, preferably from 30% to 90% by weight, more preferably from 40% to 80% by weight of polyurethane(s) P2 (solids content) relative to the total weight of said –OH component. The polyurethane P2 may be a single polymer or a polymer blend. The polyurethane P2 may have a mass content of OH groups ranging from 0.10% to 0.5% by weight, preferably from 0.1% to 0.4% by weight relative to the total weight of the polyurethane P2. The –OH component can have a viscosity at 23°C ranging from 500 mPa.s to 2500 mPa.s for a dry extract of 60%. The adhesive composition according to the invention is a multi-component composition comprising at least the aforementioned -NCO and -OH components. Preferably, the adhesive composition is a two-component composition. The amounts of the –NCO and –OH components in said composition may be such that the –NCO / -OH molar equivalent ratio is within a range from 1.2 to 5.0, preferably from 1.5 to 3.0, and even more preferably from 1.5 to 2.5. The term –NCO / -OH molar equivalent ratio is understood to mean the ratio of the equivalent number of –NCO groups (present in the –NCO component) to the equivalent number of –OH groups (present in the –OH component). The adhesive composition may comprise at least one additive selected from the group consisting of plasticizers, catalysts, rheological agents, solvents, pigments, adhesion promoters, moisture absorbers, UV stabilizers (or antioxidants), colorants, fillers, and mixtures thereof.These additives can be found in the –NCO component, in the –OH component or in both. When the adhesive composition is solvent-based, this means that it comprises at least one solvent. Preferably, the composition does not comprise epoxy compounds (i.e. a compound comprising at least one epoxy function). Uses The present invention also relates to a multilayer (complex) structure comprising at least two layers of material bonded together by an adhesive layer, characterized in that said adhesive layer consists of the composition according to the invention, in the crosslinked state. The adhesive layer preferably has a thickness ranging from 1.2 to 5 µm. The adhesive layer can be obtained by crosslinking the composition according to the invention, in an amount preferably ranging from 0.5 to 5 g / m².The materials from which the layers of material surrounding the adhesive layer are made are generally chosen from paper, a metal, such as for example aluminum or thermoplastic polymers such as: - polyethylene (PE), - polypropylene (PP), - a copolymer based on ethylene and propylene, - polyamide (PA), - polyethylene terephthalate (PET), or - an ethylene-based copolymer such as for example a maleic anhydride graft copolymer, a copolymer of ethylene and vinyl acetate (EVA), a copolymer of ethylene and vinyl alcohol (EVOH), a copolymer of ethylene and an alkyl acrylate such as methyl acrylate (EMA) or butyl acrylate (EBA), - polystyrene (PS), - polyvinyl chloride (PVC), - polyvinylidene fluoride (PVDF), - a polymer or copolymer of lactic acid (PLA), or - a polyhydroxyalkanoate (PHA). An individual layer of material may itself consist of several materials.It may be, for example, a layer of thermoplastic polymers obtained by coextrusion of two polymers (there is then no glue between the coextruded layers), the individual layers of thermoplastic polymer may be further coated with a substance (for example based on aluminum oxide or silicon oxide) or metallized (case of PET metallized with aluminum particles) to add an additional barrier effect. The thickness of the 2 layers of material adjacent to the adhesive layer and of the other layers of material implemented in the multilayer structure according to the invention may be capable of varying within a wide range, for example, from 5 to 150 µm. The total thickness of said structure may also be capable of varying within a wide range, for example, from 20 to 400 µm. Preferably, the multilayer structure is in the form of a multilayer film.According to a preferred variant, the film comprises 2 to 4 thin layers of materials, said film then being called, respectively, duplex, triplex or quadruplex. According to one embodiment, said film is chosen from: - a triplex film: PET / ALU / PE (biased polyester) - a triplex film: PET / ALU / cPP (“cast” polypropylene). The invention also relates to a method for manufacturing the multilayer structure (complex) according to the invention comprising the following steps: - mixing the components -OH and -NCO, and optional dilution with an organic solvent, to form an adhesive mixture, then - coating said adhesive mixture on the surface of a first layer of material, then - optional evaporation of the organic solvent in the presence of solvent; - laminating the surface of a second layer on the coated surface of the first layer of material, then - crosslinking said adhesive mixture.The adhesive composition is typically supplied to the complexer in the form of 2 compositions (or components): - one (called the -NCO component) comprising chemical entities carrying isocyanate end groups –NCO, and - the other (called the -OH component) comprising chemical entities carrying hydroxyl end groups –OH. The mixing of these 2 components can be carried out at 23°C if the composition is solvent-based, otherwise between 35 and 60°C, by the operator of the complexing machine prior to its start-up, which allows the correct operation of the latter, thanks to an appropriate viscosity. The viscosity of the adhesive composition thus obtained can be adjusted by simply adding solvent by the operator when it is solvent-based, resulting in a final quantity of dry extract of the adhesive composition which can vary in practice from 30 to 70% weight / weight, preferably from 30 to 55% weight / weight; otherwise by adjusting the application temperature.The coating of said mixture may be carried out on all or part of the surface of a material. In particular, the coating of said mixture may be carried out in the form of a layer with a thickness ranging from 1.5 to 5 µm. The coating is preferably carried out continuously or substantially continuously. The coating and the lamination of the second material are generally carried out within a time interval compatible with the coating process, as is well known to those skilled in the art, i.e. before the adhesive layer loses its ability to bond the two materials. Optionally, the crosslinking of said mixture on the surface of the material may be accelerated by heating the coated material(s) to a temperature of less than or equal to 70°C. The time required to complete this crosslinking reaction and thus ensure the required level of cohesion is generally of the order of 0.5 to 24 hours.The invention also relates to the use of the multilayer structure (complex) according to the invention for the manufacture of flexible packaging. The complexes according to the invention can in fact be used for the manufacture of the most diverse flexible packaging, which is shaped and then closed (after the step of packaging the product intended for the consumer) by heat-sealing techniques (or heat-welding). Preferably, the complex according to the invention is used in food packaging. Packaging intended for food can be heat-treated at temperatures ranging from 90°C to 135°C before use. The multilayer structure is advantageously suitable for the manufacture of flexible packaging intended for the packaging of food products.The adhesive composition according to the invention has at least one of the following advantages: - it advantageously leads (without aging), after crosslinking, to a multilayer structure having good initial adhesion. Preferably, the initial peel strength is greater than or equal to 3N / 15 mm, even more preferably greater than or equal to 4.0 N / 15 mm, for a PET / ALU / cPP triplex film according to the method described in the experimental part; - after aging over time of the composition, it advantageously leads, after crosslinking, to a multilayer structure having good initial adhesion.Preferably, the initial peel force is greater than or equal to 3N / 15 mm, even more preferably greater than or equal to 4.0 N / 15 mm, for a PET / ALU / cPP triplex film according to the method described in the experimental part; - it advantageously leads (without aging), after crosslinking, to a multilayer structure having good resistance to heat treatment, preferably good thermal resistance with respect to the sterilization and / or pasteurization test.Preferably, the peel strength 1 hour after sterilization is greater than or equal to 3N / 15 mm, even more preferably greater than or equal to 4.0 N / 15 mm, for a PET / ALU / cPP triplex film according to the method described in the experimental part; - after aging over time of the composition, this advantageously leads, after crosslinking, to a multilayer structure having good resistance to heat treatment, preferably good thermal resistance with respect to the sterilization and / or pasteurization test.Preferably, the peel strength 1 hour after sterilization is greater than or equal to 3N / 15 mm, even more preferably greater than or equal to 4.0 N / 15 mm, for a PET / ALU / cPP triplex film according to the method described in the experimental part; - it advantageously leads to a low variation in adhesion performance before / after sterilization on an aged and non-aged adhesive; - it is crosslinkable at 23°C for less than 5 days, preferably less than 3 days; - its viscosity is stable over time; - it has a reduced level of residual monomers; - it does not generate aromatic amines (PAA) after migration within the packaging; - it complies with the regulations specific to sterilizable food packaging. All the embodiments described below can be combined with each other.In particular, the various aforementioned constituents of the composition, and in particular the preferred embodiments of the composition, may be combined with each other. In the context of the invention, the term "between x and y" or "ranging from x to y" means an interval in which the limits x and y are included. For example, the range "between 0% and 25%" includes in particular the values 0% and 25%. The invention is now described in the following embodiments which are given purely for illustrative purposes and should not be interpreted to limit its scope. EXAMPLES The following compounds were used in the context of the examples: - Isophorone diisocyanate (IPDI) available from VENCOREX. Its functionality is equal to 2 and its NCO percentage is 37.6% - TAKENATE D-110N (NB) marketed by the company MITSUI CHEMICALS corresponding to an adduct m-XDI / TMP (meta-xylylene diisocyanate and trimethylolpropane) at 75% dry extract in ethyl acetate (NCO percentage is 11 to 12%). - SILQUEST A-1110 available from MOMENTIVE is 3-aminopropyltrimethoxysilane (molar mass = 179g / mol) - Monoethylene glycol available from BASF; - Diethylene glycol available from SABIC; - TYZOR® LA available from Dorf Ketal: titanium chelate - TYZOR® TnBT available from Dork Ketal: (nBuO)4Ti Example 1: preparation of linear amorphous copolyester diol (COPO1) 35.120 g of monoethylene glycol and 154.435 g of diethylene glycol are introduced into a closed 1 liter reactor, equipped with stirring, a distillation column, heating means, a thermometer and connected to a vacuum pump. When the temperature of the reaction mixture reaches 120°C, the following are introduced into the reactor: 76.190 g of adipic acid, 170.035 g of isophthalic acid, 64.165 g of terephthalic acid and 0.035 g of a titanium chelate catalyst (TYZOR® LA from Dorf Ketal). A temperature ramp is then programmed to reach a temperature of 230°C in 3 hours.The acid number (Ia) is then measured. The reaction is stopped when the acid number Ia is less than 25 mg KOH / g. 0.020 g of a titanium-based catalyst (of formula (nBuO)4Ti, TYZOR® TnBT from Dork Ketal) is then introduced, then the reactor is placed under vacuum and the reaction mixture is heated to 240°C. The acid number (Ia) is measured according to ASTM-D4662 and the Brookfield viscosity at 180°C. The reaction is stopped when the Ia is less than 3 mg KOH / g and when the viscosity is between 8000 and 9000 mPa.s. The copolyester diol obtained is then cooled to 200°C and then slowly poured into ethyl acetate at room temperature (23°C) with stirring, to form a 60% weight / weight solution. The IOH of the copolyester diol thus obtained was measured according to ISO 14900:2017 and is equal to 12.5 mg KOH / g. The Brookfield viscosity at 23°C of the product obtained is 2000 mPa.s.Viscosity measurement can be done using a Brookfield viscometer according to ISO 2555:2018. : Preparation of linear amorphous copolyester diol (COPO2) In a closed 1 liter reactor, equipped with stirring, a distillation column, heating means, a thermometer and connected to a vacuum pump, 7.669 g of monoethylene glycol and 202.245 g of diethylene glycol are introduced. When the temperature of the reaction mixture reaches 120°C, 95.555 g of adipic acid and 194.480 g of isophthalic acid are introduced into the reactor. Then a temperature ramp is programmed to reach a temperature of 230°C in 3 hours. The acid number (Ia) is then measured. The reaction is stopped when the acid number Ia is less than 25 mg KOH / g. 0.051 g of a titanium-based catalyst (TYZOR® TnBT) is then introduced, then the reactor is placed under vacuum (reaching 15 mbar in 2 hours) and the reaction mixture is heated to 240°C. Measurements of the Ia and the Brookfield viscosity are carried out at 80°C.The reaction is stopped when the Ia is less than 3 mg KOH / g and when the viscosity is between 6000 and 6500 mPa.s. The copolyester diol obtained is then cooled to 200°C and then slowly poured into ethyl acetate at room temperature with stirring, to form a 75% weight / weight solution. The IOH of the copolyester diol thus obtained was measured and is equal to 42.5 mg KOH / g. The Brookfield viscosity at 23°C of the product obtained is 1100 mPa.s. Example No. 3: Preparation of the OH components (3A, 3B, 3C) OH component – 3A: In a closed 1 liter reactor, equipped with stirring, a condenser, heating means and a thermometer, 213.075 g of copolyester COPO1 (example 1), 213.080 g of copolyester COPO2 (example 2) and 10.565 g of isophorone diisocyanate (IPDI) are introduced. The mixture is then heated to a temperature of 77°C and maintained at this temperature for 13 hours.The reaction progress rate is controlled by measuring the NCO group content by a dibutylamine backflush assay, using hydrochloric acid according to standard NF T52-132. When the measured NCO group content is approximately equal to the desired NCO group content (0.25-0.46% NCO), the mixture is cooled to 55°C and then 4.637g of Silquest® A1110 aminosilane is added. This addition is carried out before all the NCO functions on the intermediate prepolymer have disappeared, so that the aminosilane is grafted onto the prepolymer. The reaction mixture is stirred for 3 hours at this temperature. Then ethyl acetate (non-reactive solvent) is introduced until a dry extract of 60% is obtained. Ethyl acetate does not participate in the reaction and acts as a diluent. After homogenization of the mixture (30 minutes) maintained between 30-50°C, the Brookfield viscosity at 23°C and the dry extract are measured.Component OH – 3B: In a closed 1 liter reactor, equipped with stirring, a condenser, heating means and a thermometer, 190.155 g of copolyester COPO2 (example 2) and 7.495 g of isophorone diisocyanate (IPDI) are introduced. The mixture is then heated to a temperature of 77°C and maintained at this temperature for 10 hours. When the measured NCO group content is approximately equal to the desired NCO group content (0.28-0.71% NCO), the mixture is cooled to 55°C and then 2.34 g of the aminosilane Silquest® A1110 is added. This addition is carried out before the disappearance of all the NCO functions on the intermediate prepolymer, so that the aminosilane is grafted onto the prepolymer. The reaction mixture is stirred for 3 hours at this temperature. Then 249.982 g of copolyester COPO1 (example 1) and ethyl acetate (non-reactive solvent) are introduced until a dry extract of 60% is obtained.Ethyl acetate and COPO1 do not participate in the reaction and act as diluents at this stage. After homogenization of the mixture (30 minutes) maintained between 30-50°C, the Brookfield viscosity at 23°C and the dry extract are measured. Component OH – 3C: In a closed 1 liter reactor, equipped with stirring, a condenser, heating means and a thermometer, 63.599 g of copolyester COPO1 (example 1), 254.457 g of copolyester COPO2 (example 2) and 10.614 g of isophorone diisocyanate (IPDI) are introduced. The mixture is then heated to a temperature of 77°C and maintained at this temperature for 13 hours. When the measured NCO group content is approximately equal to the desired NCO group content (0.27-0.61% NCO), the mixture is cooled to 55°C and then 3.722g of Silquest® A1110 aminosilane is added. This addition is made before all the NCO functions on the intermediate prepolymer have disappeared, so that the aminosilane is grafted onto the prepolymer.The reaction mixture is stirred for 3 hours at this temperature. Then 99.983 g of copolyester COPO1 (example 1) and ethyl acetate (non-reactive solvent) are introduced until a dry extract of 60% is obtained. Ethyl acetate and COPO1 do not participate in the reaction and act as diluents at this stage. After homogenization of the mixture (30 minutes) maintained between 30-50°C, the Brookfield viscosity at 23°C and the dry extract are measured. The compositions of the different -OH components are detailed in the following table:.
[0002] Table 1 – Compositions of components -OH OH (3A) OH (3B) OH (3C) C omposant OH (% by weight) (% by weight) (% by weight) Copolyester COPO1 (example 1)42.61 - 12.72Synthesis Copolyester COPO2 polyurethane (example 2)42.61 38.03 50.89P2 IPDI 2.11 1.50 2.12 Silquest® A1110 0.93 0.47 0.75 Ethyl acetate 11.74 10.00 1ts no (solv 3,53 Solvan ant)reagents added Copolyester COPO1 at the end of (example 1) (dry extract synthesis =60% in 0 50.00 20.00 ethyl acetate) Dry extract 59.93% 60.03% 59.05% %OH of P2 0.187% 0.139% 0.197% %OH of the OH component 0.187% 0.253% 0.243% NCO / OH (molar) synthesis of P2 0.63 0.62 0.62 The measurement of dry extract (before or after aging) is done by weighing before after evaporation of the solvent, in an oven for 3 hours at 105°C, on 3 samples of approximately exactly 1g each. Aging of -OH components Each of the OH components of Example 3, liquid, was placed in an oven at 40°C for 21 days, in a sealed metal pot inerted with nitrogen. This accelerated aging of the -OH component corresponds approximately to storage for 4 to 5 months at 23°C. It therefore makes it possible to simulate storage of the -OH component before use by the user.The viscosity measurement at 23°C is made using a Brookfield viscometer according to ISO 2555 published in 1999 (Brookfield RVT viscometer, a needle adapted to the viscosity range 3 and at a rotation speed of 50 revolutions per minute (rpm). The viscosity and solids results are given in the following table: OH (3A) OH (3B) OH (3C) Initial viscosity of the -OH component at 23°C (mPa.s) 1264 908 748 Initial solids of the -OH component (%) 59.93% 60.03% 59.05% O. H (3A) OH (3B) OH (3C) v ieilli aged aged Viscosity of the -OH component at 23 after aging for 21 days at 40°C (mPa.s)1980 968 938Solid extract of the -OH component after aging for 21 days at 40°C 59,95% 59,43% 59,16%Example No. 4: Preparation of the comparative OH component (4A) OH component – 4A: In a closed 1 liter reactor, equipped with stirring, a condenser, heating means and a thermometer, 371.9 g of copolyester COPO2 (example 2) and 14.235 g of isophorone diisocyanate (IPDI) are introduced. The mixture is then heated to a temperature of 77°C and maintained at this temperature for 13 hours. When the measured NCO group content is approximately equal to zero (NCO groups consumed), the mixture is cooled to 55°C and then 4.615 g of Silquest® A1110 aminosilane is added. The aminosilane will not react because there are no NCO functions present, which have all been consumed, hence no grafting of the aminosilane onto the polymer. Then ethyl acetate (non-reactive solvent) is introduced until a dry extract of 60% is obtained. Ethyl acetate does not participate in the reaction and acts as a diluent.After homogenization of the mixture (30 minutes) maintained between 30-50°C, the Brookfield viscosity at 23°C and the dry extract are measured. The composition of the -OH component is detailed in the following table: Table 2 – Composition of the comparative -OH component (4A) OH (4A) comparative OH component (% by weight) Prepolymer synthesis Copolyester COPO2 (example 2) 74.38 polyurethane IPDI 2.85 Non-reactive solvents Ethyl acetate (solvent) 21.85 added at the end of synthesis Silquest® A1110 0.92 Solids content 61.46% %OH prepolymer 0.285% %OH of the OH component 0.285% NCO / OH (molar) synthesis of the prepolymer 0.60 Aging of the comparative -OH component The OH component of example 4, liquid, was placed in an oven at 40 °C for 21 days, in a sealed metal pot and inerted with nitrogen. This accelerated aging of the -OH component corresponds approximately to storage for 4 to 5 months at 23°C. It therefore makes it possible to simulate storage of the -OH component before use by the user.The viscosity measurement at 23°C is made using a Brookfield viscometer according to ISO 2555 published in 1999 (Brookfield RVT viscometer, a needle adapted to the viscosity range 3 and at a rotation speed of 50 revolutions per minute (rpm). The viscosity and dry extract results are given in the following table: OH (4A) comparative Initial viscosity of the -OH component at 23°C (. mPa.s) 1085 Initial dry extract of the -OH component (%) 61.46% O H (4A) comparatif v ieilli Viscosity of the -OH component at 23°C after aging for 21 days at 40°C (mPa.s) 985 Dry extract of the -OH component after aging for 21 days at 40°C 60,92%Examples 5 to 12: Two-component adhesive compositions An –OH component from Example 3 (3A, 3B, 3C, aged or not) or the -OH component from Comparative Example 4 (4A aged or not) was mixed with the –NCO component with ethyl acetate solvent to fluidify the adhesive mixture and obtain a solids content of 35%, then introduced into the feed tank of the laminating machine at room temperature (23°C) according to a given weight ratio making it possible to achieve a given NCO / OH molar ratio. The -NCO component is as follows: TAKENATE D-110N m-XDI / TMP adduct (in ethyl acetate, solids content=75%) 100,00%Dry extract 75.00% Theoretical %NCO 11.50% The data for the two-component adhesive compositions are reported in Table 3. Similar two-component compositions were prepared with the -OH components of Examples 3 and 4 obtained after aging, in ratios identical to those mentioned for the unaged OH components. Table 3 – Two-component adhesive compositions Ex.11 Ex.12 Ex.5 Ex.6 Ex.7 Ex.8 Ex.9 Ex.10 (comp (compar aratif) ative) Component 3A 3B 3C 3A 3B 3C 4A 4A aged -OH aged aged aged Component Takena Takena Takena Takena Takena Takena Takena Takena Takenate -NCO te te te te te te te te D110N D110N D110N D110N D110N D110N D110N Solvent Acetate ... 1,79 molar – 99 1.75 1.78 1.99 1.75 1.78 1,79NCO / -OH Weight ratio 9.3 / 100 11 / 100 8 / 100 9.5 / 100 9.3 / 100 8 / 100 9.5 / 100 11 / 100 component –NCO / -OH Example 13: PET / ALU / cPP triplex film A triplex film is prepared consisting of a first film of PolyEthylene Terephthalate (PET), a second film of aluminum (ALU) and a third film of cast PolyPropylene (cPP) bonded at each interface by a layer of adhesive composition of Examples 5 to 12. A PET film with a thickness of 12 μm, an ALU film with a thickness of 8 μm and a cPP film with a thickness of 70 μm are used. This triplex film is obtained in two stages: - The manufacture of a PET / ALU duplex by feeding the tank of a Nordmeccanica type laminating machine with a standard two-component adhesive composition marketed by Bostik: HERBERTS HP 1614 + PURBINDER C1. Said laminating machine is equipped with a roller-type coating device with an open tank, operating at room temperature and at a running speed of 50 m / minute.The adhesive layer binding the 2 PET / ALU films has a thickness of approximately 3.5 μm corresponding to approximately 3.5 g / m2 of adhesive composition. - The manufacture of the PET / ALU / cPP triplex is finalized by coating the PET / ALU duplex, ALU side, using a hand-coater, with the two-component adhesive composition according to the invention, for each of examples 5 to 10 and comparative adhesive composition of examples 11 and 12, then lamination of the cPP film which is done manually by applying a 2 kg roller. Immediately after its manufacture, the triplex film is stored at a temperature of 23 °C and under an atmosphere at 50% relative humidity (RH). The samples are subsequently subjected to the following tests after 2 days of crosslinking under these conditions: 23 °C, 50% RH. A. 180° Peel Test The 180° peel test is as described in the French standard NF T 54-122.The principle of this test consists of determining the force required to separate (or peel) two individual layers of film bonded by the two-component adhesive. A rectangular specimen 15 mm wide and approximately 10 cm long is cut from the triplex film. The two individual layers of film included in this strip and the two free ends thus obtained are manually peeled off from the end of this specimen, and over approximately 2 cm, are fixed to two attachment devices connected, respectively, to a fixed part and a mobile part of a traction device which are located on a vertical axis.While a drive mechanism communicates to the moving part a uniform speed of 100 mm / minute, leading to the detachment of the 2 layers whose detached ends move progressively along a vertical axis forming an angle of 180°, the fixed part - connected to a dynamometer - measures the force which is supported by the specimen thus held, and which is expressed in N / 15mm. On the PET / ALU / cPP triplex, the peel test was carried out only between ALU and cPP. B. Sterilization resistance The sterilization resistance is then evaluated on bag-type samples after 2 days of crosslinking at 23°C 50% RH. The bags are made from the A4 triplex (dimensions 21 x 29.7 cm) obtained by hand-coating, in which two rectangular formats of dimensions 14 x 12 cm are cut using a template.These two formats are then superimposed cPP against cPP, and heat sealed on 3 sides at a temperature of 160°C and a pressure of 3 bars for 1 second. 3 grams of distilled water are then added to each bag, the air from which is manually expelled by pressure from the packaging before proceeding to heat seal the 4. èmeand last side of each bag according to the parameters stated above. This sample is placed in an autoclave which is heated to 135°C in the vapor phase for one hour to simulate a sterilization treatment. The sample is then kept at room temperature for 1 hour and the cohesion of the ALU / cPP interface of the film is then measured, using the peel test at 180°C described above. The result is indicated in N / 15 mm in the results tables, for each of the adhesive compositions 5 to 12, before and after aging of the OH component. C. Results: The compositions of examples 5 to 10 (according to the invention) advantageously comply with European (EU 10 / 2011) and American (FDA 177.1390) regulations, in that they do not comprise aromatic isocyanate monomers, and have a quantity of PAA (primary aromatic amines) of less than 2 ppb (Europe) for food packaging.In addition, the performances of the compositions of Examples 5 to 10 (invention) and 11-12 (comparative) are detailed in the following table: Triplex film F1 F2 F3 F4 F5 F6 F7 F8 (PET / ALU) / cPP (comparative) (comparative) Adhesive used at the interface Ex. Ex. Ex.7 Ex. Ex Ex Ex 11 Ex 12 ALU / cPP 5 6 8 9 10 Initial peel strength at the ALU / cPP interface on adhesive with unaged OH component. a) or aged b) 4.36 4.57 4.43 4.83 5.5 3.69 3.69 3.11 (N / 15mm) Peel strength 1H after sterilization at the ALU / cPP interface on adhesive with unaged OH component 4.39 4.42 4.69 a) 4.42 4.99 4.36 2.38 1.94 (N / 15mm) % variation in peel strength 1H after sterilization on adhesive -8% -9% +18% +1% -3% +6%-36% -38% with unaged OH component a) or aged b)a) The unaged -OH component corresponds for film F1 to the OH component (3A), for film F2 to the -OH component (3B), for film F3 to the -OH component (3C), for film F7 to the comparative OH component (4A) b) The aged -OH component corresponds for film F4 to the aged -OH component (3A), for film F5 to the aged -OH component (3B), for film F6 to the aged -OH component (3C), for film F8 to the aged comparative OH component 4A. The results show that films F1, F2, F3, F4, F5 and F6 advantageously have an initial peel strength greater than 3 N / 15 mm, and this for adhesives having an aged or unaged -OH component. More particularly, the adhesives of examples 5 to 10 according to the invention advantageously lead to good resistance to sterilization, whether for adhesives having an unaged -OH component (4.42 / 4.99 / 4.36 N / 15 mm) or with an aged -OH component (4.39 / 4.42 / 4.69 N / 15 mm).The percentage variation in peel strength 1 hour after sterilization on adhesive with OH components having undergone accelerated aging advantageously varies from -3% to +6% (films F4, F5 and F6 according to the invention), which demonstrates a very low variation. Thus, advantageously, the adhesives having undergone accelerated aging as described above maintain good resistance to sterilization, and therefore good adhesive properties. This is important for the end user who can advantageously use a two-component adhesive composition stored for a few months before use. On the other hand, films F7 and F8 (comparative) lead to much higher variations (-36% and -38% respectively).
Claims
CLAIMS 1. Adhesive composition comprising an -OH component and an -NCO component, characterized in that: - the -NCO component is a composition comprising at least one polyisocyanate; - the -OH component is a composition comprising at least one polyurethane P2 comprising at least one hydroxyl terminal function and at least one silylated terminal function.
2. Adhesive composition according to claim 1, characterized in that the polyurethane P2 is a polyester polyol-based polyurethane.
3. Adhesive composition according to any one of claims 1 or 2, characterized in that the polyisocyanate is a triisocyanate, preferably an adduct of m-XDI and triol.
4. Adhesive composition according to any one of claims 1 to 3, characterized in that the polyisocyanate is the adduct of m-XDI and Trimethylolpropane (TMP). 5.Adhesive composition according to any one of claims 1 to 4, characterized in that the polyurethane P2 is obtained by a process comprising the following steps: E1) the preparation of a composition comprising at least one polyurethane P1 comprising at least one -NCO terminal function and at least one -OH terminal function, by a polyaddition reaction: i) of at least one polyester polyol A1; ii) of at least one polyisocyanate P'; iii) of an optional polyol A2 different from A1; in amounts such that the NCO / OH molar ratio (r1) is less than 1; E2) the reaction of the composition formed in step E1 with at least one aminosilane.
6. Adhesive composition according to claim 5, characterized in that the polyester polyol A1 is a copolyester obtained by a polycondensation reaction: - of at least one aliphatic diol (a); with. - at least one aromatic diacid (b) chosen from terephthalic acid, isophthalic acid, phthalic acid, one of their diester or anhydride derivatives, and mixtures thereof; and - at least one aliphatic diacid (c) or one of its diester or anhydride derivatives.
7. Adhesive composition according to any one of claims 5 or 6, characterized in that the polyester polyol A1 is obtained by polycondensation: - of 2 aliphatic diols (a) consisting, respectively, of ethylene glycol and diethylene glycol; with - either 2 diacids (b) consisting, respectively, of terephthalic acid and isophthalic acid; or isophthalic acid as acid b); and - of adipic acid as aliphatic diacid (c).
8. Adhesive composition according to any one of claims 5 to 7, characterized in that the ratio r1 ranges from 0.25 to 0.95, even more preferably from 0.40 to 0.
80. 9.Adhesive composition according to any one of claims 5 to 8, characterized in that the polyurethane P1 has a content of NCO groups ranging from 0.10 to 0.90%, more preferably from 0.15 to 0.75%.
10. Adhesive composition according to any one of claims 5 to 9, characterized in that the NCO / NH molar ratio (r2) ranges from 1.5 to 5.2, more preferably from 1.5 to 4.
5.
11. Adhesive composition according to any one of claims 5 to 10, characterized in that the polyurethane P2 has a mass content of OH groups ranging from 0.10% to 0.50% by weight, preferably from 0.10% to 0.40% by weight relative to the total weight of the polyurethane P2.
12. Adhesive composition according to any one of claims 1 to 11, characterized in that the –OH component has a viscosity at 23°C ranging from 500 mPa.s to 2500 mPa.s for a dry extract of 60%. 13.Adhesive composition according to any one of claims 5 to 12, characterized in that the aminosilane has the following formula (I): (R. 4 O) 3-r (R 3 ) r Si-R 1 -NH-R 2 (I) in which: - R 3 , identical or different, each represents a linear or branched monovalent hydrocarbon radical comprising from 1 to 10 carbon atoms; - R 4 , identical or different, represents a linear or branched monovalent hydrocarbon radical comprising from 1 to 10 carbon atoms, or two R groups 4 can form a cycle; - r is an integer equal to 0, 1 or 2, preferably equal to 0 or 1, and even more preferably equal to 0; - R 1 represents a linear or branched divalent alkylene radical comprising from 1 to 12 carbon atoms, preferably from 1 to 6 carbon atoms, R 3 preferentially representing methylene or n-propylene, and - R 2represents H, a linear or branched alkyl radical, an arylalkyl radical, a cyclic radical comprising from 1 to 20 carbon atoms, or a radical having the following formula (II): in which: - R 7 and R 8 are independently of each other, a hydrogen or a radical chosen from the group consisting of –R 9 , -COOR 9 and –CN; - the radical R 10 is hydrogen, or a radical chosen from the group consisting of –CH2- COOR 9 , -COOR 9 , -CONHR 9 , -CON(R 9 )2, -CN; - the radical R 9being a hydrocarbon radical having from 1 to 20 carbon atoms optionally comprising at least one heteroatom.
14. Multilayer structure comprising at least two layers of material bonded together by an adhesive layer, characterized in that said adhesive layer consists of the adhesive composition according to any one of claims 1 to 13, in the crosslinked state.
15. Method for manufacturing the multilayer structure according to claim 14, comprising the following steps: - mixing the components -OH and -NCO, and optional dilution with an organic solvent, to form an adhesive mixture, then - coating said adhesive mixture on the surface of a first layer of material, then - optional evaporation of the organic solvent in the presence of solvent; - laminating the surface of a second layer on the coated surface of the first layer of material, then - crosslinking said adhesive mixture.
16. Use of the multilayer structure as defined in claim 13, for the manufacture of flexible packaging, preferably flexible food packaging.
Citation Information
Patent Citations
Polyisocyanate composition, two-pack-type curable polyurethane resin, coating material, adhesive, and process for producing polyisocyanate composition
EP3101044A1
Two-component curable solventless-type laminate adhesive and resin cured product
US20190010372A1
Lamination adhesive for sterilisation
WO2020217023A1
Two-component polyurethane adhesive composition for film lamination
WO2023284973A1