Composition for forming surface-modified layer, and method for forming resist pattern

The surface-modified layer forming composition addresses the adhesion challenges in miniaturized lithography by using specific resin components to improve resist film adhesion, reducing pattern collapse and residue, and enhancing lithography properties.

WO2024228374A1PCT designated stage expired Publication Date: 2024-11-07TOKYO OHKA KOGYO CO LTD
View PDF 9 Cites 0 Cited by

Patent Information

Application Number
PCT/JP2024/016568
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-05-01
Filing Date
2024-04-26
Publication Date
2024-11-07

AI Technical Summary

Technical Problem

In the manufacturing of semiconductor and liquid crystal display devices, the miniaturization of patterns through advanced lithography technology poses challenges in achieving sufficient adhesion of resist films to inorganic substrates, leading to pattern collapse and residue issues during exposure and development.

Method used

A surface-modified layer forming composition is developed, comprising a resin component with specific structural units, which improves the adhesion of resist films to substrates by forming a modified layer between the support and the resist film, enhancing the resist film's adhesion and preventing pattern collapse.

Benefits of technology

The composition effectively improves the adhesion of resist films to substrates, reducing pattern collapse and residue formation, thereby enhancing the lithography properties and resolution of resist patterns in miniaturized devices.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure JP2024016568_07112024_PF_FP_ABST
    Figure JP2024016568_07112024_PF_FP_ABST
Patent Text Reader

Abstract

A surface-modified-layer-forming composition for forming a surface-modified layer provided between a support and a resist film, the surface-modified-layer-forming composition containing a resin component (G) having a structural unit (g0) represented by general formula (g0-1), and a resin component (P) having a structural unit (p0) represented by general formula (p0-1). R represents a hydrogen atom, a C1–5 alkyl group, or a C1–5 halogenated alkyl group, Yg0 is a divalent linking group, Rg0 is an epoxy-group-containing group, Yp0 is a divalent linking group; and Rp0 is a C2–20 chain hydrocarbon group that may have a substituent.
Need to check novelty before this filing date? Find Prior Art

Description

Composition for forming surface modification layer and method for forming resist pattern

[0001] The present invention relates to a composition for forming a surface modification layer and a method for forming a resist pattern. This application claims priority based on Japanese Patent Application No. 2023-075761, filed on May 1, 2023, the contents of which are incorporated herein by reference.

[0002] In recent years, advances in lithography technology have led to rapid advances in the miniaturization of patterns in the manufacturing of semiconductor devices and liquid crystal display devices. A common method for achieving this miniaturization is to shorten the wavelength (increase the energy) of the exposure light source.

[0003] Resist materials are required to have lithography properties such as sensitivity to these exposure light sources, resolution capable of reproducing fine-sized patterns, etc. To satisfy these requirements, a chemically amplified resist composition containing a base component whose solubility in a developer changes with the action of acid and an acid generator component that generates acid upon exposure has been used.

[0004] When forming a resist pattern on an inorganic substrate, adhesion between a support such as a silicon wafer and a resist film becomes an issue. Insufficient adhesion between the support and the resist film can cause the resist pattern to collapse. One method for improving the adhesion of the resist film to the support is to provide a surface modification layer between the support and the resist film. For example, Patent Document 1 describes a surface modification material containing an epoxy resin with a mass average molecular weight of 1,000 to 50,000.

[0005] JP 2011-197425 A

[0006] As patterns become increasingly finer, improvements in various lithography properties, such as resistance to pattern collapse, and pattern resolution are more strongly required in lithography technology than ever before. Conventionally, in order to prevent pattern collapse, methods have been used to improve the adhesion of a resist pattern to a support, such as a silicon wafer, by treating the support with hexamethyldisilazane (HMDS) or by providing an organic anti-reflective coating. However, when a resist pattern of isolated lines with fine dimensions is formed, pattern collapse may not be sufficiently suppressed due to insufficient adhesion of the resist film to the support. Furthermore, residues after exposure and development of the resist film may not be sufficiently suppressed.

[0007] The present invention has been made in consideration of the above circumstances, and an object of the present invention is to provide a composition for forming a surface modification layer, which can improve the adhesion of a resist film to a support, and a method for forming a resist pattern using the composition for forming a surface modification layer.

[0008] In order to solve the above problems, the present invention employs the following configuration. That is, a first aspect of the present invention is a composition for forming a surface modification layer for forming a surface modification layer provided between a support and a resist film, the composition containing a resin component (G) having a structural unit (g0) represented by the following general formula (g0-1), and a resin component (P) having a structural unit (p0) represented by the following general formula (p0-1).

[0009] [wherein R represents a hydrogen atom, an alkyl group having 1 to 5 carbon atoms, or a halogenated alkyl group having 1 to 5 carbon atoms; Yg 0 represents a divalent linking group; Rg 0 represents an epoxy group-containing group.

[0010] [wherein R represents a hydrogen atom, an alkyl group having 1 to 5 carbon atoms, or a halogenated alkyl group having 1 to 5 carbon atoms; Yp 0 represents a divalent linking group; Rp 0 represents a chain hydrocarbon group having 2 to 20 carbon atoms, which may have a substituent.

[0011] A second aspect of the present invention is a method for forming a resist pattern, comprising: a step (i) of forming a surface modification layer on a support using the composition for forming a surface modification layer according to the first aspect; a step (ii) of forming a resist film on the surface modification layer formed on the support using a resist composition; a step (iii) of exposing the resist film; and a step (iv) of developing the exposed resist film to form a resist pattern.

[0012] According to the present invention, it is possible to provide a composition for forming a surface modification layer, which is capable of improving the adhesion of a resist film to a support, and a method for forming a resist pattern using the composition for forming a surface modification layer.

[0013] In this specification and claims, "aliphatic" is a relative concept to aromatic, and is defined as meaning a group, compound, etc. that does not have aromaticity. "Alkyl group" includes linear, branched, and cyclic monovalent saturated hydrocarbon groups, unless otherwise specified. The same applies to alkyl groups in alkoxy groups. "Alkylene group" includes linear, branched, and cyclic divalent saturated hydrocarbon groups, unless otherwise specified. "Halogen atom" includes fluorine, chlorine, bromine, and iodine atoms. "Structural unit" means a monomer unit that constitutes a polymer compound (resin, polymer, copolymer). When it is written that "may have a substituent," it means a case where a hydrogen atom (-H) is replaced with a monovalent group, or a case where a methylene group (-CH 2 The term "exposure" encompasses both cases where the radical (-) is substituted with a divalent group.

[0014] An "acid-decomposable group" is a group having acid decomposability in which at least a part of the bond in the structure of the acid-decomposable group can be cleaved by the action of an acid. Examples of acid-decomposable groups whose polarity increases by the action of an acid include groups that decompose by the action of an acid to generate a polar group. Examples of polar groups include a carboxy group, a hydroxyl group, an amino group, and a sulfo group (-SO 3More specific examples of the acid-decomposable group include groups in which the polar group is protected with an acid-dissociable group (for example, groups in which the hydrogen atom of an OH-containing polar group is protected with an acid-dissociable group).

[0015] The term "acid-dissociable group" refers to either (i) a group having acid dissociability in which the bond between the acid-dissociable group and the atom adjacent to the acid-dissociable group can be cleaved by the action of an acid, or (ii) a group in which a portion of the bond is cleaved by the action of an acid, followed by a decarboxylation reaction, in which the bond between the acid-dissociable group and the atom adjacent to the acid-dissociable group can be cleaved. The acid-dissociable group constituting the acid-decomposable group must be a group with lower polarity than the polar group generated by dissociation of the acid-dissociable group. Thus, when the acid-dissociable group is dissociated by the action of an acid, a polar group with higher polarity than the acid-dissociable group is generated, thereby increasing the polarity. As a result, the polarity of the entire component (A1) increases. The increase in polarity relatively changes the solubility in the developer, increasing the solubility when the developer is an alkaline developer and decreasing the solubility when the developer is an organic developer.

[0016] A "base component" is an organic compound that has film-forming ability. Organic compounds used as base components are broadly classified into non-polymers and polymers. As non-polymers, those with a molecular weight of 500 or more and less than 4000 are usually used (hereinafter referred to as "low molecular weight compounds"). Hereinafter, when referring to "resin," "high molecular weight compound," or "polymer," it refers to a polymer with a molecular weight of 1000 or more. The molecular weight of the polymer is the weight average molecular weight in terms of polystyrene measured by GPC (gel permeation chromatography).

[0017] The term "derived structural unit" refers to a structural unit formed by cleavage of a multiple bond between carbon atoms, for example, an ethylenic double bond. In the "acrylic acid ester", the hydrogen atom bonded to the carbon atom at the α-position may be substituted with a substituent. The substituent (R αx ) is an atom or group other than a hydrogen atom. αx ) is substituted with a substituent containing an ester bond, or αxThis also includes α-hydroxyacrylic esters in which the α-position carbon atom of an acrylic ester is substituted with a hydroxyalkyl group or a group that modifies the hydroxyl group. Unless otherwise specified, the α-position carbon atom of an acrylic ester refers to the carbon atom to which the carbonyl group of acrylic acid is bonded. Hereinafter, acrylic esters in which the hydrogen atom bonded to the α-position carbon atom has been replaced with a substituent may be referred to as α-substituted acrylic esters.

[0018] The term "derivative" is used to refer to a compound in which the hydrogen atom at the α-position of the target compound has been substituted with another substituent such as an alkyl group or a halogenated alkyl group, as well as derivatives thereof. Examples of such derivatives include a compound in which the hydrogen atom of the hydroxyl group of a target compound in which the hydrogen atom at the α-position may be substituted with a substituent has been substituted with an organic group; a compound in which the hydrogen atom at the α-position of the target compound may be substituted with a substituent to which a substituent other than a hydroxyl group is bonded; and the like. Unless otherwise specified, the α-position refers to the first carbon atom adjacent to the functional group. Examples of substituents that can be used to replace the hydrogen atom at the α-position of hydroxystyrene include R αx The same can be mentioned.

[0019] In this specification and claims, some structures represented by chemical formulas may have asymmetric carbon atoms, and may exist as enantiomers or diastereoisomers. In such cases, a single chemical formula represents all of the isomers. These isomers may be used alone or as a mixture.

[0020] (Surface modification layer forming composition) The surface modification layer forming composition according to the first aspect of the present invention is used to form a surface modification layer provided between a support and a resist film. The surface modification layer forming composition of this embodiment contains a resin component (G) (hereinafter also referred to as "(G) component") having a structural unit (g0) represented by the general formula (g0-1) described below, and a resin component (P) (hereinafter also referred to as "(P) component") having a structural unit (p0) represented by the general formula (p0-1) described below.

[0021] <Resin Component (G): Component (G)> The component (G) contains a polymeric compound having a structural unit (g0) represented by general formula (g0-1) described below.

[0022] <Structural Unit (g0)> The structural unit (g0) is a structural unit represented by the following general formula (g0-1).

[0023] [wherein R represents a hydrogen atom, an alkyl group having 1 to 5 carbon atoms, or a halogenated alkyl group having 1 to 5 carbon atoms; Yg 0 represents a divalent linking group; Rg 0 represents an epoxy group-containing group.

[0024] In the formula (g0-1), the alkyl group having 1 to 5 carbon atoms for R is preferably a linear or branched alkyl group having 1 to 5 carbon atoms, and specific examples include a methyl group, an ethyl group, a propyl group, an isopropyl group, an n-butyl group, an isobutyl group, a tert-butyl group, a pentyl group, an isopentyl group, and a neopentyl group. The halogenated alkyl group having 1 to 5 carbon atoms is a group in which some or all of the hydrogen atoms of the alkyl group having 1 to 5 carbon atoms have been substituted with halogen atoms. A fluorine atom is particularly preferred as the halogen atom. R is preferably a hydrogen atom, an alkyl group having 1 to 5 carbon atoms, or a fluorinated alkyl group having 1 to 5 carbon atoms, and from the perspective of industrial ease of availability, a hydrogen atom or a methyl group is most preferred.

[0025] In the formula (g0-1), Yg 0 Examples of the divalent linking group in include a divalent hydrocarbon group which may have a substituent, and a divalent linking group containing a hetero atom.

[0026] Divalent hydrocarbon group which may have a substituent: The divalent hydrocarbon group which may have a substituent may be an aliphatic hydrocarbon group or an aromatic hydrocarbon group.

[0027] Aliphatic hydrocarbon group: An aliphatic hydrocarbon group refers to a hydrocarbon group that does not have aromaticity. The aliphatic hydrocarbon group may be saturated or unsaturated, and is usually preferably saturated. Examples of the aliphatic hydrocarbon group include linear or branched aliphatic hydrocarbon groups, and aliphatic hydrocarbon groups that contain a ring in their structure.

[0028] ...Straight-chain or branched-chain aliphatic hydrocarbon group The straight-chain aliphatic hydrocarbon group preferably has 1 to 10 carbon atoms, more preferably 1 to 6 carbon atoms, even more preferably 1 to 4 carbon atoms, and most preferably 1 to 3 carbon atoms. As the straight-chain aliphatic hydrocarbon group, a straight-chain alkylene group is preferred, and specifically, a methylene group [—CH 2 -], ethylene group [-(CH 2 ) 2 -], trimethylene group [-(CH 2 ) 3 -], tetramethylene group [-(CH 2 ) 4 -], pentamethylene group [-(CH 2 ) 5 The branched chain aliphatic hydrocarbon group preferably has 2 to 10 carbon atoms, more preferably 3 to 6 carbon atoms, even more preferably 3 or 4 carbon atoms, and most preferably 3 carbon atoms. As the branched chain aliphatic hydrocarbon group, a branched chain alkylene group is preferred, and specifically, -CH(CH 3 ) -, -CH(CH 2 CH 3 ) -, -C(CH 3 ) 2 -, -C(CH 3 ) (CH 2 CH 3 ) -, -C(CH 3 ) (CH 2 CH 2 CH 3 ) -, -C(CH 2 CH 3 ) 2 alkylmethylene groups such as -; -CH(CH 3 ) CH 2 -, -CH(CH 3 ) CH(CH 3) -, -C(CH 3 ) 2 CH 2 -, -CH(CH 2 CH 3 ) CH 2 -, -C(CH 2 CH 3 ) 2 -CH 2 alkylethylene groups such as -; -CH(CH 3 ) CH 2 CH 2 -, -CH 2 CH (CH 3 ) CH 2 alkyltrimethylene groups such as -; -CH(CH 3 ) CH 2 CH 2 CH 2 -, -CH 2 CH (CH 3 ) CH 2 CH 2 The alkyl group in the alkylalkylene group is preferably a linear alkyl group having 1 to 5 carbon atoms.

[0029] The linear or branched aliphatic hydrocarbon group may or may not have a substituent, such as a fluorine atom, a fluorinated alkyl group having 1 to 5 carbon atoms and substituted with a fluorine atom, or a carbonyl group.

[0030] ...Aliphatic hydrocarbon groups containing a ring in their structure. Examples of aliphatic hydrocarbon groups containing a ring in their structure include cyclic aliphatic hydrocarbon groups (groups obtained by removing two hydrogen atoms from an aliphatic hydrocarbon ring) that may contain a heteroatom-containing substituent in the ring structure, groups in which the cyclic aliphatic hydrocarbon group is bonded to the end of a linear or branched aliphatic hydrocarbon group, and groups in which the cyclic aliphatic hydrocarbon group is interposed in the linear or branched aliphatic hydrocarbon group. Examples of the linear or branched aliphatic hydrocarbon groups include those described above. The cyclic aliphatic hydrocarbon group preferably has 3 to 20 carbon atoms, more preferably 3 to 12 carbon atoms. The cyclic aliphatic hydrocarbon group may be a polycyclic group or a monocyclic group. The monocyclic alicyclic hydrocarbon group is preferably a group obtained by removing two hydrogen atoms from a monocycloalkane. The monocycloalkane preferably has 3 to 6 carbon atoms, and specific examples include cyclopentane and cyclohexane. The polycyclic alicyclic hydrocarbon group is preferably a group in which two hydrogen atoms have been removed from a polycycloalkane, and the polycycloalkane preferably has 7 to 12 carbon atoms, specifically adamantane, norbornane, isobornane, tricyclo[5.2.1.0] 2,6 ]decane, tetracyclododecane, and the like.

[0031] The cyclic aliphatic hydrocarbon group may or may not have a substituent. Examples of the substituent include an alkyl group, an alkoxy group, a halogen atom, a halogenated alkyl group, a hydroxyl group, and a carbonyl group. The alkyl group as the substituent is preferably an alkyl group having 1 to 5 carbon atoms, and more preferably a methyl group, an ethyl group, a propyl group, an n-butyl group, or a tert-butyl group. The alkoxy group as the substituent is preferably an alkoxy group having 1 to 5 carbon atoms, and more preferably a methoxy group, an ethoxy group, an n-propoxy group, an iso-propoxy group, an n-butoxy group, or a tert-butoxy group, and even more preferably a methoxy group or an ethoxy group. The halogen atom as the substituent is preferably a fluorine atom. Examples of the halogenated alkyl group as the substituent include groups in which some or all of the hydrogen atoms of the alkyl group are substituted with the halogen atoms. The cyclic aliphatic hydrocarbon group may have some of the carbon atoms constituting its ring structure substituted with a substituent containing a heteroatom. The substituent containing a hetero atom includes —O—, —C(═O)—O—, —S—, and —S(═O) 2 -, -S(=O) 2 —O— is preferred.

[0032] Aromatic Hydrocarbon Group The aromatic hydrocarbon group is a hydrocarbon group having at least one aromatic ring. This aromatic ring is not particularly limited as long as it is a cyclic conjugated system having 4n+2 π electrons, and may be monocyclic or polycyclic. The aromatic ring preferably has 5 to 30 carbon atoms, more preferably 5 to 20 carbon atoms, even more preferably 6 to 15 carbon atoms, and particularly preferably 6 to 12 carbon atoms. However, this number of carbon atoms does not include the number of carbon atoms in the substituents. Specific examples of aromatic rings include aromatic hydrocarbon rings such as benzene, naphthalene, anthracene, and phenanthrene; and aromatic heterocycles in which some of the carbon atoms constituting the aromatic hydrocarbon ring are substituted with heteroatoms. Examples of heteroatoms in aromatic heterocycles include oxygen atoms, sulfur atoms, and nitrogen atoms. Specific examples of aromatic heterocycles include pyridine rings and thiophene rings. Specific examples of the aromatic hydrocarbon group include groups in which two hydrogen atoms have been removed from the aromatic hydrocarbon ring or aromatic heterocycle (arylene groups or heteroarylene groups); groups in which two hydrogen atoms have been removed from an aromatic compound containing two or more aromatic rings (e.g., biphenyl, fluorene, etc.); and groups in which one hydrogen atom of a group in which one hydrogen atom has been removed from the aromatic hydrocarbon ring or aromatic heterocycle (aryl group or heteroaryl group) has been substituted with an alkylene group (e.g., groups in which one further hydrogen atom has been removed from the aryl group in an arylalkyl group such as a benzyl group, phenethyl group, 1-naphthylmethyl group, 2-naphthylmethyl group, 1-naphthylethyl group, or 2-naphthylethyl group). The alkylene group bonded to the aryl group or heteroaryl group preferably has 1 to 4 carbon atoms, more preferably 1 or 2 carbon atoms, and particularly preferably 1 carbon atom.

[0033] In the aromatic hydrocarbon group, a hydrogen atom contained in the aromatic hydrocarbon group may be substituted with a substituent. For example, a hydrogen atom bonded to an aromatic ring in the aromatic hydrocarbon group may be substituted with a substituent. Examples of the substituent include an alkyl group, an alkoxy group, a halogen atom, a halogenated alkyl group, and a hydroxyl group. The alkyl group as the substituent is preferably an alkyl group having 1 to 5 carbon atoms, and more preferably a methyl group, an ethyl group, a propyl group, an n-butyl group, or a tert-butyl group. Examples of the alkoxy group, halogen atom, and halogenated alkyl group as the substituent include those exemplified as the substituent substituting a hydrogen atom contained in the cyclic aliphatic hydrocarbon group. The halogen atom as the substituent is preferably a bromine atom or an iodine atom, and more preferably an iodine atom.

[0034] Divalent linking group containing a hetero atom: Examples of the divalent linking group containing a hetero atom include -O-, -C(=O)-O-, -O-C(=O)-, -C(=O)-, -O-C(=O)-O-, -C(=O)-NH-, -NH-, -NH-C(=NH)- (H may be substituted with a substituent such as an alkyl group or an acyl group), -S-, and -S(=O). 2 -, -S(=O) 2 -O-, general formula -Y 21 -O-Y 22 -, -Y 21 -O-, -Y 21 -C(=O)-O-, -C(=O)-O-Y 21 -, -[Y 21 -C(=O)-O] m” -Y 22 -, -Y 21 -OC(=O)-Y 22 - or -Y 21 -S(=O) 2 -O-Y 22 -, wherein Y 21 and Y 22are each independently a divalent hydrocarbon group which may have a substituent, O is an oxygen atom, and m" is an integer of 1 to 3. When the divalent linking group containing a hetero atom is -C(=O)-NH-, -C(=O)-NH-C(=O)-, -NH-, or -NH-C(=NH)-, the H may be substituted with a substituent such as an alkyl group or an acyl group. The substituent (alkyl group, acyl group, etc.) preferably has 1 to 10 carbon atoms, more preferably 1 to 8, and particularly preferably 1 to 5 carbon atoms. General formula -Y 21 -O-Y 22 -, -Y 21 -O-, -Y 21 -C(=O)-O-, -C(=O)-O-Y 21 -, -[Y 21 -C(=O)-O] m” -Y 22 -, -Y 21 -OC(=O)-Y 22 - or -Y 21 -S(=O) 2 -O-Y 22 -Middle, Y 21 and Y 22 are each independently a divalent hydrocarbon group which may have a substituent. Examples of the divalent hydrocarbon group include the same as those described above. 21 As Y, a linear aliphatic hydrocarbon group is preferred, a linear alkylene group is more preferred, a linear alkylene group having 1 to 5 carbon atoms is even more preferred, and a methylene group or an ethylene group is particularly preferred. 22 is preferably a linear or branched aliphatic hydrocarbon group, more preferably a methylene group, an ethylene group or an alkylmethylene group. The alkyl group in the alkylmethylene group is preferably a linear alkyl group having 1 to 5 carbon atoms, more preferably a linear alkyl group having 1 to 3 carbon atoms, and most preferably a methyl group. 21 -C(=O)-O] m” -Y 22 In the group represented by -, m" is an integer of 1 to 3, preferably 1 or 2, and more preferably 1. That is, the group represented by the formula -[Y 21 -C(=O)-O] m”-Y 22 The group represented by - includes the group represented by the formula -Y 21 -C(=O)-O-Y 22 Among them, groups represented by the formula -(CH 2 ) a’ -C(=O)-O-(CH 2 ) b’ In the formula, a' is an integer of 1 to 10, preferably an integer of 1 to 8, more preferably an integer of 1 to 5, even more preferably 1 or 2, and most preferably 1. b' is an integer of 1 to 10, preferably an integer of 1 to 8, more preferably an integer of 1 to 5, even more preferably 1 or 2, and most preferably 1.

[0035] Yg 0 As the alkyl group, an ester bond [-C(=O)-O-, -O-C(=O)-], an ether bond (-O-), a linear or branched alkylene group, or a combination of two or more of these is preferred, and an ester bond [-C(=O)-O-, -O-C(=O)-] is more preferred.

[0036] Rg in general formula (g0-1) 0 The epoxy group-containing group in Rg is not particularly limited as long as it is a group containing an epoxy ring. 0 Examples of the epoxy group-containing group in the formula (rg-1) include a group represented by the following general formula (rg-1) and an alicyclic epoxy group.

[0037] [In the formula, Rg 01 ~Rg 03 each independently represents a hydrogen atom or an alkyl group. * represents a bond.

[0038] In the formula (rg-1), Rg 01 ~Rg 03 The alkyl group in Rg may be linear or branched, but is preferably a linear alkyl group. 01 ~Rg 03 The linear alkyl group in Rg preferably has 1 to 5 carbon atoms, more preferably 1 to 3 carbon atoms, and is further preferably a methyl group or an ethyl group, with a methyl group being particularly preferred. 01 ~Rg 03The branched alkyl group in Rg preferably has 3 to 5 carbon atoms, and more preferably 3 carbon atoms. 01 ~Rg 03 is preferably a hydrogen atom or a methyl group, more preferably a hydrogen atom. 01 ~Rg 03 It is more preferable that all of are hydrogen atoms.

[0039] The alicyclic epoxy group is an alicyclic group containing an epoxy group. Examples of the alicyclic epoxy group include a group represented by the following general formula (rg-2), a group represented by the following formula (rg-3), and a group represented by the following formula (rg-4).

[0040] [In the formula, Rg 04 ~Rg 06 each independently represents a hydrogen atom or an alkyl group; g4 and g5 each independently represent an integer of 1 to 20. * represents a bond.

[0041] In the formula (rg-2), Rg 04 ~Rg 06 The alkyl group in Rg may be linear or branched, but is preferably a linear alkyl group. 04 ~Rg 06 The linear alkyl group in Rg preferably has 1 to 5 carbon atoms, more preferably 1 to 3 carbon atoms, and is further preferably a methyl group or an ethyl group, with a methyl group being particularly preferred. 04 ~Rg 06 The branched alkyl group in Rg preferably has 3 to 5 carbon atoms, and more preferably 3 carbon atoms. 04 ~Rg 06 is preferably a hydrogen atom or a methyl group, more preferably a hydrogen atom. 04 ~Rg 06 It is more preferable that all of are hydrogen atoms.

[0042] In formula (rg-2), g4 is preferably an integer of 1 to 5, more preferably an integer of 1 to 3, even more preferably 1 or 2, and particularly preferably 2. In formula (rg-2), g5 is preferably an integer of 1 to 5, more preferably an integer of 1 to 3, even more preferably 1 or 2, and particularly preferably 1.

[0043] The structural unit (g0) is preferably a group represented by general formula (g0-1-1) shown below.

[0044] [wherein R represents a hydrogen atom, an alkyl group having 1 to 5 carbon atoms, or a halogenated alkyl group having 1 to 5 carbon atoms; Yg 01 represents a single bond or a divalent linking group; Rg 01 represents an epoxy group-containing group.

[0045] R in the formula (g0-1-1) is the same as R in the general formula (g0-1).

[0046] Yg in the formula (g0-1-1) 01 As the divalent linking group, Yg 0 The divalent linking group in the formula Yg may be the same as the divalent linking group in the formula Yg. 01 is preferably a single bond, a linear or branched alkylene group, or a combination of a linear or branched alkylene group and an ester bond or an ether bond, more preferably a single bond or a linear or branched alkylene group, and even more preferably a single bond. The linear or branched alkylene group preferably has 1 to 5 carbon atoms, more preferably 1 to 3 carbon atoms, and even more preferably an ethylene group or a methylene group.

[0047] Rg in the formula (g0-1-1) 01 As the Rg in the formula (g0-1), 0 The same as Rg 01 is preferably a group represented by any one of the above formulae (rg-1) to (rg-4).

[0048] Specific examples of the structural unit (g0) are shown below, but the structural unit is not limited to these. α represents a hydrogen atom, a methyl group, or a trifluoromethyl group.

[0049]

[0050] The structural unit (g0) contained in the component (G) may be one type or two or more types. The proportion of the structural unit (g0) in the component (G) is preferably 10 mol% or more, more preferably 20 mol% or more, even more preferably 30 mol% or more, even more preferably 40 mol% or more, particularly preferably 50 mol% or more, and may even be 100 mol%, relative to the total (100 mol%) of all structural units constituting the component (G). When the proportion of the structural unit (g0) is equal to or greater than the preferred lower limit, the crosslinking efficiency with the support is increased, and the adhesion between the resist film and the support is further improved. The proportion of the structural unit (g0) in the component (G) is, relative to the total (100 mol%) of all structural units constituting the component (G), for example, 10 to 90 mol%, preferably 20 to 80 mol%, more preferably 30 to 80 mol%, even more preferably 40 to 80 mol%, and particularly preferably 50 to 80 mol%. When the proportion of the structural unit (g0) is no more than the above preferred upper limit, a good balance with the other structural units can be achieved, and various favorable lithography properties can be achieved when a resist pattern is formed.

[0051] <<Other Structural Units>> The component (G) may contain other structural units in addition to the structural unit (g0). Examples of other structural units include the structural unit (a11) derived from (α-substituted) acrylic acid or (α-substituted) methyl acrylate, the structural unit (a10) represented by the following general formula (a10-1), a structural unit (a2) containing a lactone-containing cyclic group, and the structural unit (a8) derived from a compound represented by the below-mentioned general formula (a8-1). Of these, the structural unit (a11) and the structural unit (a10) are particularly preferred.

[0052] Structural Unit (a11): The component (G) may include a structural unit (a11). The structural unit (a11) is preferably a structural unit represented by general formula (a11-1) shown below.

[0053] [In the formula, R represents a hydrogen atom, an alkyl group having 1 to 5 carbon atoms, or a halogenated alkyl group having 1 to 5 carbon atoms; 11 represents a hydrogen atom or a methyl group.

[0054] R in the formula (a11-1) is the same as R in the general formula (g0-1). R is preferably a hydrogen atom, an alkyl group having 1 to 5 carbon atoms, or a fluorinated alkyl group having 1 to 5 carbon atoms, and particularly preferably a hydrogen atom or a methyl group.

[0055] In the formula (a11-1), Ra 11 is preferably a hydrogen atom.

[0056] Specific examples of the structural unit (a11) are shown below, but the structural unit is not limited to these. α represents a hydrogen atom, a methyl group, or a trifluoromethyl group.

[0057]

[0058] When the component (G) contains the structural unit (a11), the structural unit (a11) may be of one type or of two or more types. The component (G) may or may not contain the structural unit (a11). When the component (G) contains the structural unit (a11), the proportion of the structural unit (a11) in the component (G) is, relative to the total (100 mol%) of all structural units constituting the component (G), for example, 1 to 50 mol%, preferably 5 to 40 mol%, more preferably 10 to 30 mol%, and even more preferably 10 to 20 mol%. When the proportion of the structural unit (a11) is within the above-mentioned preferred range, various lithography properties are improved when a resist pattern is formed on a surface modification layer formed using the surface modification layer-forming composition of this embodiment.

[0059] Structural Unit (a10): The component (G) may include a structural unit (a10). The structural unit (a10) is a structural unit represented by the following general formula (a10-1).

[0060] [In the formula, R is a hydrogen atom, an alkyl group having 1 to 5 carbon atoms, or a halogenated alkyl group having 1 to 5 carbon atoms. x1 is a single bond or a divalent linking group. x1 is an aromatic hydrocarbon group which may have a substituent. ax1 is an integer of 1 or greater.

[0061] R in the formula (a10-1) is the same as R in the general formula (g0-1). R is preferably a hydrogen atom, an alkyl group having 1 to 5 carbon atoms, or a fluorinated alkyl group having 1 to 5 carbon atoms, and particularly preferably a hydrogen atom or a methyl group.

[0062] In the formula (a10-1), Ya x1 As the divalent linking group, Yg 0 Examples of the divalent linking group include the same as the divalent linking group in the above formula.

[0063] Ya x1 is preferably a single bond, an ester bond [-C(=O)-O-, -O-C(=O)-], an ether bond (-O-), a linear or branched alkylene group, or a combination of two or more of these, and more preferably a single bond or an ester bond [-C(=O)-O-, -O-C(=O)-].

[0064] In the formula (a10-1), Wa x1 is an aromatic hydrocarbon group which may have a substituent. x1 The aromatic hydrocarbon group in the formula (n) is an aromatic ring which may have a substituent. ax1 Examples of the aromatic ring include a group in which 4n+1) hydrogen atoms have been removed. The aromatic ring here is not particularly limited as long as it is a cyclic conjugated system having 4n+2 π electrons. The aromatic ring preferably has 5 to 30 carbon atoms, more preferably 5 to 20 carbon atoms, even more preferably 6 to 15 carbon atoms, and particularly preferably 6 to 12 carbon atoms. Specific examples of the aromatic ring include aromatic hydrocarbon rings such as benzene, naphthalene, anthracene, and phenanthrene; and aromatic heterocycles in which some of the carbon atoms constituting the aromatic hydrocarbon ring are substituted with heteroatoms. Examples of heteroatoms in the aromatic heterocycle include oxygen atoms, sulfur atoms, and nitrogen atoms. Specific examples of the aromatic heterocycle include pyridine rings and thiophene rings. Wa x1 The aromatic hydrocarbon group in (n) is selected from aromatic compounds containing an aromatic ring which may have two or more substituents (for example, biphenyl, fluorene, etc.). ax1 Also included are groups in which one or more hydrogen atoms have been removed. x1Examples of the aryl group include benzene, naphthalene, anthracene, and biphenyl (n ax1 A group in which (n +1) hydrogen atoms have been removed is preferred, and a group in which (n +1) hydrogen atoms have been removed from benzene or naphthalene is preferred. ax1 A group in which (n +1) hydrogen atoms have been removed from benzene is more preferred, ax1 A group in which 1) hydrogen atoms have been removed is more preferred.

[0065] Wa x1 The aromatic hydrocarbon group in may or may not have a substituent. Examples of the substituent include an alkyl group, an alkoxy group, a halogen atom, and a halogenated alkyl group. Examples of the alkyl group, alkoxy group, halogen atom, and halogenated alkyl group as the substituent include Ya x1 Examples of the substituent include the same as those exemplified as the substituent of the cyclic aliphatic hydrocarbon group in Wa. The substituent is preferably a linear or branched alkyl group having 1 to 5 carbon atoms, more preferably a linear or branched alkyl group having 1 to 3 carbon atoms, further preferably an ethyl group or a methyl group, and particularly preferably a methyl group. x1 The aromatic hydrocarbon group in the formula (I) preferably does not have a substituent.

[0066] In the formula (a10-1), n ax1 is an integer of 1 or more, preferably an integer of 1 to 10, more preferably an integer of 1 to 5, even more preferably 1, 2 or 3, and particularly preferably 1 or 2.

[0067] Specific examples of the structural unit (a10) are shown below. In each of the following formulas, R α represents a hydrogen atom, a methyl group, or a trifluoromethyl group.

[0068]

[0069]

[0070]

[0071] When the component (G) contains the structural unit (a10), the structural unit (a10) may be of one type or of two or more types. The component (G) may or may not contain the structural unit (a10). When the component (G) contains the structural unit (a10), the proportion of the structural unit (a10) in the component (G) is preferably 20 to 80 mol%, more preferably 25 to 70 mol%, even more preferably 30 to 60 mol%, and particularly preferably 30 to 50 mol%, relative to the total (100 mol%) of all structural units constituting the component (G). When the proportion of the structural unit (a10) is within the above-mentioned preferred range, various lithography properties are improved when a resist pattern is formed on a surface modification layer formed from the surface modification layer-forming composition of this embodiment.

[0072] The component (G) contained in the composition for forming a surface modification layer of the present embodiment may be used alone or in combination of two or more types.

[0073] Examples of the component (G) include polymeric compounds comprising a repeating structure of the structural unit (g0); polymeric compounds containing a repeating structure of the structural unit (g0) and the structural unit (a10); and polymeric compounds containing a repeating structure of the structural unit (g0) and the structural unit (a11).

[0074] In polymeric compounds having a repeating structure of the structural unit (g0) and the structural unit (a10), the proportion of the structural unit (g0) relative to the total (100 mol%) of all structural units constituting the polymeric compound is preferably 20 to 80 mol%, more preferably 30 to 70 mol%, even more preferably 40 to 70 mol%, and particularly preferably 50 to 60 mol%. The proportion of the structural unit (a10) relative to the total (100 mol%) of all structural units constituting the polymeric compound is preferably 20 to 80 mol%, more preferably 30 to 70 mol%, even more preferably 30 to 60 mol%, and particularly preferably 40 to 50 mol%.

[0075] In polymeric compounds having a repeating structure of the structural unit (g0) and the structural unit (a11), the proportion of the structural unit (g0) relative to the total (100 mol%) of all structural units constituting the polymeric compound is preferably 20 to 80 mol%, more preferably 30 to 80 mol%, even more preferably 40 to 80 mol%, and particularly preferably 50 to 80 mol%. The proportion of the structural unit (a11) relative to the total (100 mol%) of all structural units constituting the polymeric compound is preferably 20 to 80 mol%, more preferably 20 to 70 mol%, even more preferably 20 to 60 mol%, and particularly preferably 20 to 50 mol%.

[0076] The component (G) can be produced by dissolving the monomers that derive each structural unit in a polymerization solvent, and then adding a radical polymerization initiator such as azobisisobutyronitrile (AIBN) or dimethyl azobisisobutyrate (e.g., V-601) to the solution and polymerizing. Alternatively, the component (G) can be produced by dissolving a monomer that derives the structural unit (g0) and a monomer that derives any structural unit (e.g., structural unit (a10), structural unit (a11) or the like) in a polymerization solvent, adding a radical polymerization initiator such as those described above to polymerize, and then carrying out a deprotection reaction. During the polymerization, for example, HS-CH 2 -CH 2 -CH 2 -C(CF 3 ) 2 By using a chain transfer agent such as —OH in combination, it is possible to obtain a chain with —C(CF 3 ) 2 An —OH group may be introduced.

[0077] The weight average molecular weight (Mw) of component (G) (based on polystyrene standards measured by gel permeation chromatography (GPC)) is, for example, preferably 1,000 to 50,000, more preferably 2,000 to 40,000, even more preferably 3,000 to 30,000, and particularly preferably 3,000 to 20,000. When the weight average molecular weight of component (G) is within the above range, the adhesion of the resist film to the support is improved. The dispersity (Mw / Mn) of component (G) is not particularly limited, but is preferably 1.0 to 4.0, and more preferably 1.0 to 3.0. Here, Mn represents the number average molecular weight.

[0078] Specific examples of the component (G) are shown below, but are not limited to these. In each of the following formulas, R α represents a hydrogen atom, a methyl group, or a trifluoromethyl group.

[0079]

[0080] <Resin Component (P): Component (P)> The component (P) contains a polymeric compound having a structural unit (p0) represented by general formula (p0-1) described below.

[0081] <Structural Unit (p0)> The structural unit (p0) is a structural unit represented by the following general formula (p0-1).

[0082] [wherein R represents a hydrogen atom, an alkyl group having 1 to 5 carbon atoms, or a halogenated alkyl group having 1 to 5 carbon atoms; Yp 0 represents a divalent linking group; Rp 0 represents a chain hydrocarbon group having 2 to 20 carbon atoms, which may have a substituent.

[0083] R in the formula (p0-1) is the same as R in the general formula (g0-1). R is preferably a hydrogen atom, an alkyl group having 1 to 5 carbon atoms, or a fluorinated alkyl group having 1 to 5 carbon atoms, and particularly preferably a hydrogen atom or a methyl group.

[0084] In the formula (p0-1), Yp 0 As the divalent linking group, Yg 0 The same as above can be mentioned. 0As the alkyl group, an ester bond [-C(=O)-O-, -O-C(=O)-], an ether bond (-O-), a linear or branched alkylene group, or a combination of two or more of these is preferred, and an ester bond [-C(=O)-O-, -O-C(=O)-] is more preferred.

[0085] In the formula (p0-1), Rp 0 The chain hydrocarbon group in Rp may be saturated or unsaturated, but is preferably saturated. 0 The chain hydrocarbon group in Rp is preferably a linear or branched alkyl group, more preferably a linear alkyl group. 0 The linear alkyl group in Rp preferably has 2 to 16 carbon atoms, more preferably 2 to 14 carbon atoms, still more preferably 2 to 10 carbon atoms, and particularly preferably 2 to 8 carbon atoms. 0 The branched alkyl group in the formula (I) preferably has 3 to 16 carbon atoms, more preferably 3 to 16 carbon atoms, even more preferably 3 to 10 carbon atoms, and particularly preferably 3 to 8 carbon atoms.

[0086] Rp 0 The chain hydrocarbon group in Rp may have a substituent. 0 The substituent that the chain hydrocarbon group in the formula (I) may have may be a monovalent substituent that substitutes a hydrogen atom (—H) that the hydrocarbon chain has, and may be a methylene group (—CH 2 -) may be a divalent substituent that substitutes a hydrogen atom. Examples of the substituent that substitutes a hydrogen atom include a fluorine atom, a carboxy group, and a hydroxy group. 0 The chain hydrocarbon group in the formula (I) preferably does not have a substituent substituting a hydrogen atom. Examples of divalent substituents substituting methylene groups constituting the hydrocarbon chain include -O-, -C(=O)-O-, -O-C(=O)-, -C(=O)-, -O-C(=O)-O-, -C(=O)-NH-, -NH-, -NH-C(=NH)- (H may be substituted with a substituent such as an alkyl group or an acyl group), -S-, -S(=O) 2 -, -S(=O) 2 As the divalent substituent, —O— is preferred.

[0087] Rp 0 As for -(CH 2 ) p2 -CH 3 (p2 is an integer of 1 to 19), or -(CH 2 ) p1 -O-CH 3 (p1 is an integer of 1 to 19) is preferable. p1 and p2 are each preferably an integer of 1 to 15, more preferably an integer of 1 to 13, even more preferably an integer of 1 to 9, and particularly preferably an integer of 1 to 7.

[0088] As the structural unit (p0), a structural unit represented by the following general formula (p0-1-1) (hereinafter also referred to as "structural unit (p01)") or a structural unit represented by the following general formula (p0-1-2) (hereinafter also referred to as "structural unit (p02)") is preferred.

[0089] [wherein R represents a hydrogen atom, an alkyl group having 1 to 5 carbon atoms, or a halogenated alkyl group having 1 to 5 carbon atoms; Yp 01 and Yp 02 each independently represents a single bond or a divalent linking group; and p1 and p2 each independently represent an integer of 1 to 19.

[0090] R in the formulas (p0-1-1) and (p0-1-2) is the same as R in the general formula (g0-1). R is preferably a hydrogen atom, an alkyl group having 1 to 5 carbon atoms, or a fluorinated alkyl group having 1 to 5 carbon atoms, and particularly preferably a hydrogen atom or a methyl group.

[0091] In the formulas (p0-1-1) and (p0-1-2), Yp 01 and Yp 02 As the divalent linking group, Yg 0 The same as above can be mentioned. 01 and Yp 02As the alkylene group, a single bond, a linear or branched alkylene group, or a combination of a linear or branched alkylene group and an ester bond or an ether bond is preferred, a single bond or a linear or branched alkylene group is more preferred, and a single bond is even more preferred. The linear or branched alkylene group preferably has 1 to 5 carbon atoms, more preferably 1 to 3 carbon atoms, and is even more preferably an ethylene group or a methylene group.

[0092] In the formulae (p0-1-1) and (p0-1-2), p1 and p2 are preferably 1 to 15, more preferably 1 to 13, even more preferably 1 to 9, and particularly preferably 1 to 7.

[0093] Specific examples of the structural unit (p0) are shown below, but the structural unit is not limited to these. α represents a hydrogen atom, a methyl group, or a trifluoromethyl group.

[0094]

[0095]

[0096] The structural unit (p0) contained in the component (P) may be one type, or two or more types. Two or more types of structural unit (p0) are preferred. The component (P) preferably contains one or more types of structural unit (p01) and one or more types of structural unit (p02). When the component (P) contains two or more types of structural unit (p0), the adhesion of the resist film to the support can be further improved, and pattern collapse is less likely to occur even when a fine resist pattern is formed. When the component (P) contains the structural unit (p01) and the structural unit (p02) as the structural unit (p0), the molar ratio of the structural unit (p01) to the structural unit (p02) (structural unit (p01):structural unit (p02)) is typically 10:90 to 90:10, preferably 30:70 to 90:10, more preferably 40:60 to 80:20, and even more preferably 50:50 to 80:20. When the molar ratio of the structural unit (p01) to the structural unit (p02) is within this preferred range, the adhesion of the resist film to the support can be further improved.

[0097] The proportion of the structural unit (p0) in the component (P) is preferably 10 mol% or more, more preferably 20 mol% or more, even more preferably 30 mol% or more, even more preferably 40 mol% or more, particularly preferably 50 mol% or more, and may even be 100 mol%, based on the total (100 mol%) of all structural units constituting the component (P). When the proportion of the structural unit (p0) is at or above the preferred lower limit, adhesion between the resist film and the support is further improved, and residue after resist pattern formation is further reduced. The proportion of the structural unit (p0) in the component (P) is, based on the total (100 mol%) of all structural units constituting the component (P), can be 10 to 90 mol%, preferably 20 to 90 mol%, more preferably 30 to 90 mol%, even more preferably 40 to 90 mol%, and particularly preferably 50 to 90 mol%. When the proportion of the structural unit (g0) is at or below the preferred upper limit, a balance with the other structural units can be achieved, resulting in improved lithography properties when the resist pattern is formed.

[0098] <<Other Structural Units>> The component (P) may contain other structural units in addition to the structural unit (p0) described above. Examples of other structural units include the structural unit (a1) containing an acid-decomposable group whose polarity increases under the action of acid, the structural unit (a11) described above, the structural unit (a10) described above, the structural unit (a2) containing a lactone-containing cyclic group, and the structural unit (a8) derived from a compound represented by general formula (a8-1) described below. Of these, the structural unit (a1) and the structural unit (a11) are particularly preferred.

[0099] Structural Unit (a1): The component (P) may include a structural unit (a1). The structural unit (a1) is a structural unit that contains an acid-decomposable group whose polarity increases when acted upon by an acid.

[0100] Examples of the acid-dissociable group include those that have been proposed as acid-dissociable groups for base resins of chemically amplified resist compositions. Specific examples of acid-dissociable groups that have been proposed as acid-dissociable groups for base resins of chemically amplified resist compositions include the "acetal-type acid-dissociable groups," "tertiary alkyl ester-type acid-dissociable groups," "tertiary alkyloxycarbonyl acid-dissociable groups," and "secondary alkyloxycarbonyl acid-dissociable groups" described below.

[0101] Acetal-Type Acid-Dissociable Group: Among the polar groups, examples of the acid-dissociable group that protects a carboxy group or a hydroxyl group include acid-dissociable groups represented by the following general formula (a1-r-1) (hereinafter, sometimes referred to as "acetal-type acid-dissociable group"):

[0102] [In the formula, Ra' 1 , Ra' 2 is a hydrogen atom or an alkyl group. 3 is a hydrocarbon group, and Ra' 3 is Ra' 1 , Ra' 2 may be bonded to any one of the following to form a ring.]

[0103] In formula (a1-r-1), Ra' 1 and Ra' 2 Among Ra', at least one is preferably a hydrogen atom, and more preferably both are hydrogen atoms. 1 or Ra' 2 When is an alkyl group, examples of the alkyl group include the same alkyl groups as those exemplified as the substituent that may be bonded to the carbon atom at the α-position in the description of the α-substituted acrylic acid ester above, and alkyl groups having 1 to 5 carbon atoms are preferred. Specific examples include linear or branched alkyl groups. More specific examples include a methyl group, an ethyl group, a propyl group, an isopropyl group, an n-butyl group, an isobutyl group, a tert-butyl group, a pentyl group, an isopentyl group, and a neopentyl group. A methyl group or an ethyl group is more preferred, and a methyl group is particularly preferred.

[0104] In formula (a1-r-1), Ra' 3Examples of the hydrocarbon group include a linear or branched alkyl group, and a cyclic hydrocarbon group. The linear alkyl group preferably has 1 to 5 carbon atoms, more preferably 1 to 4 carbon atoms, and even more preferably 1 or 2 carbon atoms. Specific examples include a methyl group, an ethyl group, an n-propyl group, an n-butyl group, and an n-pentyl group. Of these, a methyl group, an ethyl group, or an n-butyl group is preferred, and a methyl group or an ethyl group is more preferred.

[0105] The branched alkyl group preferably has 3 to 10 carbon atoms, and more preferably 3 to 5 carbon atoms. Specific examples include an isopropyl group, an isobutyl group, a tert-butyl group, an isopentyl group, a neopentyl group, a 1,1-diethylpropyl group, and a 2,2-dimethylbutyl group, with an isopropyl group being preferred.

[0106] Ra' 3 When is a cyclic hydrocarbon group, the hydrocarbon group may be an aliphatic hydrocarbon group or an aromatic hydrocarbon group, and may be a polycyclic group or a monocyclic group. As an aliphatic hydrocarbon group that is a monocyclic group, a group in which one hydrogen atom has been removed from a monocycloalkane is preferred. As the monocycloalkane, one having 3 to 6 carbon atoms is preferred, and specific examples thereof include cyclopentane and cyclohexane. As an aliphatic hydrocarbon group that is a polycyclic group, a group in which one hydrogen atom has been removed from a polycycloalkane is preferred, and as the polycycloalkane, one having 7 to 12 carbon atoms is preferred, and specific examples thereof include adamantane, norbornane, isobornane, tricyclo[5.2.1.0 2,6 ]decane, tetracyclododecane, and the like.

[0107] Ra' 3When the cyclic hydrocarbon group described above becomes an aromatic hydrocarbon group, the aromatic hydrocarbon group is a hydrocarbon group having at least one aromatic ring. This aromatic ring is not particularly limited as long as it is a cyclic conjugated system having 4n+2 π electrons, and may be monocyclic or polycyclic. The aromatic ring preferably has 5 to 30 carbon atoms, more preferably 5 to 20 carbon atoms, even more preferably 6 to 15 carbon atoms, and particularly preferably 6 to 12 carbon atoms. Specific examples of aromatic rings include aromatic hydrocarbon rings such as benzene, naphthalene, anthracene, and phenanthrene; and aromatic heterocycles in which some of the carbon atoms constituting the aromatic hydrocarbon ring are substituted with heteroatoms. Examples of heteroatoms in aromatic heterocycles include oxygen atoms, sulfur atoms, and nitrogen atoms. Specific examples of aromatic heterocycles include pyridine rings and thiophene rings. Ra' 3 Specific examples of the aromatic hydrocarbon group in the formula (I) include a group in which one hydrogen atom has been removed from the aromatic hydrocarbon ring or aromatic heterocycle (an aryl group or a heteroaryl group); a group in which one hydrogen atom has been removed from an aromatic compound containing two or more aromatic rings (e.g., biphenyl, fluorene, etc.); and a group in which one hydrogen atom of the aromatic hydrocarbon ring or aromatic heterocycle has been substituted with an alkylene group (e.g., an arylalkyl group such as a benzyl group, a phenethyl group, a 1-naphthylmethyl group, a 2-naphthylmethyl group, a 1-naphthylethyl group, or a 2-naphthylethyl group). The alkylene group bonded to the aromatic hydrocarbon ring or aromatic heterocycle preferably has 1 to 4 carbon atoms, more preferably 1 or 2 carbon atoms, and particularly preferably 1 carbon atom.

[0108] Ra' 3 The cyclic hydrocarbon group in may have a substituent. Examples of the substituent include the above-mentioned Ra x5 etc.

[0109] Ra' 3 But Ra' 1 , Ra' 2 When the cyclic group is bonded to any one of the above to form a ring, the cyclic group is preferably a 4- to 7-membered ring, more preferably a 4- to 6-membered ring. Specific examples of the cyclic group include a tetrahydropyranyl group and a tetrahydrofuranyl group.

[0110] Tertiary alkyl ester acid-dissociable group: Among the above polar groups, examples of the acid-dissociable group protecting the carboxy group include acid-dissociable groups represented by the following general formula (a1-r-2): Of the acid-dissociable groups represented by the following formula (a1-r-2), those constituted by an alkyl group will hereinafter be referred to as "tertiary alkyl ester acid-dissociable groups" for convenience.

[0111] [In the formula, Ra' 4 ~Ra' 6 are each a hydrocarbon group, and Ra' 5 , Ra' 6 may be bonded to each other to form a ring.

[0112] Ra' 4 Examples of the hydrocarbon group of Ra' include a linear or branched alkyl group, a linear or cyclic alkenyl group, and a cyclic hydrocarbon group. 4 The linear or branched alkyl group and the cyclic hydrocarbon group (a monocyclic aliphatic hydrocarbon group, a polycyclic aliphatic hydrocarbon group, and an aromatic hydrocarbon group) in 3 The same as Ra' can be mentioned. 4 The chain or cyclic alkenyl group in Ra' is preferably an alkenyl group having 2 to 10 carbon atoms. 5 , Ra' 6 The hydrocarbon group of Ra' 3 The same can be mentioned.

[0113] Ra' 5 and Ra' 6 When Ra' is bonded to each other to form a ring, preferred examples thereof include a group represented by the following general formula (a1-r2-1), a group represented by the following general formula (a1-r2-2), and a group represented by the following general formula (a1-r2-3). 4 ~Ra' 6 When the groups are not bonded to each other and are independent hydrocarbon groups, preferred examples include groups represented by the following general formula (a1-r2-4).

[0114] [In formula (a1-r2-1), Ra' 10 represents a linear or branched alkyl group having 1 to 12 carbon atoms, some of which may be substituted with a halogen atom or a heteroatom-containing group. 11 is Ra' 10 represents a group which forms an aliphatic cyclic group together with the carbon atom to which it is bonded. In formula (a1-r2-2), Ya is a carbon atom. Xa is a group which forms a cyclic hydrocarbon group together with Ya. Some or all of the hydrogen atoms in this cyclic hydrocarbon group may be substituted. Ra 101 ~Ra 103 are each independently a hydrogen atom, a monovalent linear saturated hydrocarbon group having 1 to 10 carbon atoms, or a monovalent cyclic aliphatic saturated hydrocarbon group having 3 to 20 carbon atoms. Some or all of the hydrogen atoms in the linear saturated hydrocarbon group and the cyclic aliphatic saturated hydrocarbon group may be substituted. 101 ~Ra 103 Two or more of the above may be bonded to each other to form a cyclic structure. In formula (a1-r2-3), Yaa is a carbon atom. Xaa is a group that forms an aliphatic cyclic group together with Yaa. Ra 104 In formula (a1-r2-4), Ra′ is an aromatic hydrocarbon group which may have a substituent. 12 and Ra' 13 are each independently a monovalent chain saturated hydrocarbon group having 1 to 10 carbon atoms. Some or all of the hydrogen atoms of this chain saturated hydrocarbon group may be substituted. 14 is a hydrocarbon group which may have a substituent. * indicates a bond (the same applies hereinafter).

[0115] In the above formula (a1-r2-1), Ra' 10 is a linear or branched alkyl group having 1 to 12 carbon atoms, some of which may be substituted with a halogen atom or a heteroatom-containing group.

[0116] Ra' 10 The linear alkyl group in Ra' has 1 to 12 carbon atoms, preferably 1 to 10 carbon atoms, and particularly preferably 1 to 5 carbon atoms. 10 In the formula (I), the branched alkyl group is the above-mentioned Ra' 3The same can be mentioned.

[0117] Ra' 10 In the above, the alkyl group may be partially substituted with a halogen atom or a heteroatom-containing group. For example, some of the hydrogen atoms constituting the alkyl group may be substituted with a halogen atom or a heteroatom-containing group. Furthermore, some of the carbon atoms (such as methylene groups) constituting the alkyl group may be substituted with a heteroatom-containing group. Examples of the heteroatom include an oxygen atom, a sulfur atom, and a nitrogen atom. Examples of the heteroatom-containing group include (-O-), -C(=O)-O-, -O-C(=O)-, -C(=O)-, -O-C(=O)-O-, -C(=O)-NH-, -NH-, -S-, and -S(=O) 2 -, -S(=O) 2 -O- and the like.

[0118] In formula (a1-r2-1), Ra' 11 (Ra' 10 The aliphatic cyclic group formed together with the carbon atom to which Ra' is bonded in formula (a1-r-1) is 3 Among these, monocyclic alicyclic hydrocarbon groups are preferred, and specifically, cyclopentyl and cyclohexyl groups are more preferred.

[0119] In the formula (a1-r2-2), the cyclic hydrocarbon group formed by Xa together with Ya includes Ra' in the formula (a1-r-1). 3 Examples of the cyclic hydrocarbon group include a group in which one or more hydrogen atoms have been further removed from the cyclic monovalent hydrocarbon group (aliphatic hydrocarbon group) in the formula (I). The cyclic hydrocarbon group formed by Xa together with Ya may have a substituent. Examples of the substituent include the above-mentioned Ra' 3 In formula (a1-r2-2), the substituents that the cyclic hydrocarbon group in formula (a1-r2-2) may have are the same as those in formula (a1-r2-2). 101 ~Ra 103 In the formula, examples of the monovalent chain saturated hydrocarbon group having 1 to 10 carbon atoms include a methyl group, an ethyl group, a propyl group, a butyl group, a pentyl group, a hexyl group, a heptyl group, an octyl group, and a decyl group. 101 ~Ra103 In the above formula, examples of the monovalent aliphatic cyclic saturated hydrocarbon group having 3 to 20 carbon atoms include monocyclic aliphatic saturated hydrocarbon groups such as cyclopropyl group, cyclobutyl group, cyclopentyl group, cyclohexyl group, cycloheptyl group, cyclooctyl group, cyclodecyl group, and cyclododecyl group; 2,6 ]decanyl group, tricyclo[3.3.1.1 3,7 ] decanyl group, tetracyclo[6.2.1.1 3,6 .0 2,7 ] and polycyclic aliphatic saturated hydrocarbon groups such as a dodecanyl group and an adamantyl group. 101 ~Ra 103 Among these, from the viewpoint of ease of synthesis, a hydrogen atom or a monovalent chain saturated hydrocarbon group having 1 to 10 carbon atoms is preferable, and among these, a hydrogen atom, a methyl group, or an ethyl group is more preferable, and a hydrogen atom is particularly preferable.

[0120] The above Ra 101 ~Ra 103 Examples of the substituents that the chain saturated hydrocarbon group or the aliphatic cyclic saturated hydrocarbon group represented by the formula (I) include the above-mentioned Ra x5 The same groups as those shown below can be mentioned.

[0121] Ra 101 ~Ra 103 Examples of the group containing a carbon-carbon double bond formed by two or more of the above being bonded to each other to form a cyclic structure include a cyclopentenyl group, a cyclohexenyl group, a methylcyclopentenyl group, a methylcyclohexenyl group, a cyclopentylidene-ethenyl group, a cyclohexylidene-ethenyl group, etc. Among these, from the viewpoint of ease of synthesis, a cyclopentenyl group, a cyclohexenyl group, and a cyclopentylidene-ethenyl group are preferred.

[0122] In formula (a1-r2-3), the aliphatic cyclic group formed by Xaa together with Yaa is Ra' in formula (a1-r-1). 3 In formula (a1-r2-3), the groups exemplified as the aliphatic hydrocarbon group are preferably monocyclic or polycyclic groups. 104Examples of the aromatic hydrocarbon group in the formula (I) include a group in which one or more hydrogen atoms have been removed from an aromatic hydrocarbon ring having 5 to 30 carbon atoms. 104 is preferably a group in which one or more hydrogen atoms have been removed from an aromatic hydrocarbon ring having 6 to 15 carbon atoms, more preferably a group in which one or more hydrogen atoms have been removed from benzene, naphthalene, anthracene or phenanthrene, still more preferably a group in which one or more hydrogen atoms have been removed from benzene, naphthalene or anthracene, particularly preferably a group in which one or more hydrogen atoms have been removed from benzene or naphthalene, and most preferably a group in which one or more hydrogen atoms have been removed from benzene.

[0123] Ra in formula (a1-r2-3) 104 Examples of the substituent that may be possessed by the group include a methyl group, an ethyl group, a propyl group, a hydroxy group, a carboxy group, a halogen atom, an alkoxy group (e.g., a methoxy group, an ethoxy group, a propoxy group, a butoxy group), an alkyloxycarbonyl group, and the like.

[0124] In formula (a1-r2-4), Ra' 12 and Ra' 13 are each independently a monovalent chain saturated hydrocarbon group having 1 to 10 carbon atoms. 12 and Ra' 13 In the formula (I), the monovalent chain saturated hydrocarbon group having 1 to 10 carbon atoms includes the above-mentioned Ra 101 ~Ra 103 The monovalent saturated chain hydrocarbon group having 1 to 10 carbon atoms in the formula (1) may be substituted in part or in whole. 12 and Ra' 13 Among these, Ra' is preferably an alkyl group having 1 to 5 carbon atoms, more preferably an alkyl group having 1 to 5 carbon atoms, further preferably a methyl group or an ethyl group, and particularly preferably a methyl group. 12 and Ra' 13 When the chain saturated hydrocarbon group represented by the formula (I) is substituted, examples of the substituent include the above-mentioned Ra x5 The same groups as those shown below can be mentioned.

[0125] In formula (a1-r2-4), Ra' 14is a hydrocarbon group which may have a substituent. 14 The hydrocarbon group in the formula (I) includes a linear or branched alkyl group, or a cyclic hydrocarbon group.

[0126] Ra' 14 The linear alkyl group in the formula (I) preferably has 1 to 5 carbon atoms, more preferably 1 to 4 carbon atoms, and even more preferably 1 or 2 carbon atoms. Specific examples include a methyl group, an ethyl group, an n-propyl group, an n-butyl group, and an n-pentyl group. Of these, a methyl group, an ethyl group, or an n-butyl group is preferred, and a methyl group or an ethyl group is more preferred.

[0127] Ra' 14 The branched alkyl group in the formula (I) preferably has 3 to 10 carbon atoms, and more preferably 3 to 5. Specific examples include an isopropyl group, an isobutyl group, a tert-butyl group, an isopentyl group, a neopentyl group, a 1,1-diethylpropyl group, and a 2,2-dimethylbutyl group, with an isopropyl group being preferred.

[0128] Ra' 14 When is a cyclic hydrocarbon group, the hydrocarbon group may be an aliphatic hydrocarbon group or an aromatic hydrocarbon group, and may be a polycyclic group or a monocyclic group. As an aliphatic hydrocarbon group that is a monocyclic group, a group in which one hydrogen atom has been removed from a monocycloalkane is preferred. As the monocycloalkane, one having 3 to 6 carbon atoms is preferred, and specific examples thereof include cyclopentane and cyclohexane. As an aliphatic hydrocarbon group that is a polycyclic group, a group in which one hydrogen atom has been removed from a polycycloalkane is preferred, and as the polycycloalkane, one having 7 to 12 carbon atoms is preferred, and specific examples thereof include adamantane, norbornane, isobornane, tricyclo[5.2.1.0 2,6 ]decane, tetracyclododecane, and the like.

[0129] Ra' 14 As the aromatic hydrocarbon group in 104 Among them, the aromatic hydrocarbon groups Ra' are the same as those in 14is preferably a group in which one or more hydrogen atoms have been removed from an aromatic hydrocarbon ring having 6 to 15 carbon atoms, more preferably a group in which one or more hydrogen atoms have been removed from benzene, naphthalene, anthracene, or phenanthrene, still more preferably a group in which one or more hydrogen atoms have been removed from benzene, naphthalene, or anthracene, particularly preferably a group in which one or more hydrogen atoms have been removed from naphthalene or anthracene, and most preferably a group in which one or more hydrogen atoms have been removed from naphthalene. 14 Examples of the substituent that may be possessed by Ra include 104 Examples of the substituents include the same as those that may be possessed by the group.

[0130] Ra' in formula (a1-r2-4) 14 When Ra' in formula (a1-r2-4) is a naphthyl group, the position at which it is bonded to the tertiary carbon atom in formula (a1-r2-4) may be either the 1st or 2nd position of the naphthyl group. 14 When is an anthryl group, the position at which it is bonded to the tertiary carbon atom in the formula (a1-r2-4) may be any one of the 1st, 2nd, and 9th positions of the anthryl group.

[0131] Specific examples of the group represented by the formula (a1-r2-1) are listed below.

[0132]

[0133]

[0134]

[0135] Specific examples of the group represented by the formula (a1-r2-2) are listed below.

[0136]

[0137]

[0138]

[0139] Specific examples of the group represented by the formula (a1-r2-3) are listed below.

[0140]

[0141] Specific examples of the group represented by the formula (a1-r2-4) are listed below.

[0142]

[0143] Tertiary alkyloxycarbonyl acid dissociable group: Examples of the acid dissociable group that protects the hydroxyl group of the polar group include acid dissociable groups represented by the following general formula (a1-r-3) (hereinafter, for convenience, may be referred to as "tertiary alkyloxycarbonyl acid dissociable group").

[0144] [In the formula, Ra' 7 ~Ra' 9 are each an alkyl group.

[0145] In formula (a1-r-3), Ra' 7 ~Ra' 9 are each preferably an alkyl group having 1 to 5 carbon atoms, more preferably an alkyl group having 1 to 3 carbon atoms. The total number of carbon atoms in each alkyl group is preferably 3 to 7, more preferably 3 to 5, and most preferably 3 to 4.

[0146] Secondary Alkyl Ester-Type Acid-Dissociable Group: Among the above polar groups, examples of the acid-dissociable group that protects the carboxy group include acid-dissociable groups represented by the following general formula (a1-r-4).

[0147] [In the formula, Ra' 10 is a hydrocarbon group. 11a and Ra' 11b are each independently a hydrogen atom, a halogen atom or an alkyl group. 12 is a hydrogen atom or a hydrocarbon group. 10 and Ra' 11a or Ra' 11b and may be bonded to each other to form a ring. 11a or Ra' 11b and Ra' 12 may be bonded to each other to form a ring.

[0148] In the formula, Ra' 10 and Ra' 12The hydrocarbon group in Ra' is 3 In the formula, Ra' 11a and Ra' 11b The alkyl group in Ra' is 1 In the formula, Ra' is the same as the alkyl group in 10 and Ra' 12 and the hydrocarbon group in Ra' 11a and Ra' 11b The alkyl group in may have a substituent. Examples of the substituent include the above-mentioned Ra x5 etc.

[0149] Ra' 10 and Ra' 11a or Ra' 11b may be bonded to each other to form a ring. The ring may be polycyclic or monocyclic, and may be an alicyclic or aromatic ring. The alicyclic and aromatic rings may contain heteroatoms.

[0150] Ra' 10 and Ra' 11a or Ra' 11b and are bonded to each other to form a ring, among the above, a monocycloalkene, a ring in which a portion of the carbon atoms of a monocycloalkene is substituted with a heteroatom (such as an oxygen atom or a sulfur atom), or a monocycloalkadiene is preferred, a cycloalkene having 3 to 6 carbon atoms is preferred, and cyclopentene or cyclohexene is preferred.

[0151] Ra' 10 and Ra' 11a or Ra' 11b The ring formed by bonding these may be a fused ring. Specific examples of such fused rings include indan.

[0152] Ra' 10 and Ra' 11a or Ra' 11b The ring formed by bonding together may have a substituent. Examples of the substituent include the above-mentioned Ra x5 etc.

[0153] Ra' 11aor Ra' 11b and Ra' 12 and may be bonded to each other to form a ring, and the ring may include Ra' 10 and Ra' 11a or Ra' 11b and the ring formed by bonding with each other are exemplified.

[0154] Specific examples of the group represented by the formula (a1-r-4) are listed below.

[0155]

[0156] Examples of the structural unit (a1) include a structural unit derived from an acrylate ester in which the hydrogen atom bonded to the carbon atom at the α-position may be substituted with a substituent, a structural unit derived from acrylamide, a structural unit derived from hydroxystyrene or a hydroxystyrene derivative in which at least some of the hydrogen atoms in the hydroxyl groups are protected with a substituent containing the above-mentioned acid-decomposable group, and a structural unit derived from vinylbenzoic acid or a vinylbenzoic acid derivative in which at least some of the hydrogen atoms in -C(═O)-OH are protected with a substituent containing the above-mentioned acid-decomposable group.

[0157] Of the above, the structural unit (a1) is preferably a structural unit derived from an acrylate ester in which the hydrogen atom bonded to the α-position carbon atom may be substituted with a substituent. Preferred specific examples of such structural unit (a1) include structural units represented by the following general formulas (a1-1), (a1-2), and (a1-3):

[0158] [In the formula, R is a hydrogen atom, an alkyl group having 1 to 5 carbon atoms, or a halogenated alkyl group having 1 to 5 carbon atoms. 1 is a divalent hydrocarbon group which may have an ether bond. a1 is an integer from 0 to 2. 1 is an acid-dissociable group represented by the above general formula (a1-r-1), (a1-r-2) or (a1-r-4). 1 is n a2 + is a monovalent hydrocarbon group. a2 is an integer from 1 to 3.2 represents an acid-dissociable group represented by the above general formula (a1-r-1) or (a1-r-3). 001 represents a single bond or a divalent linking group. 01 is a single bond or a divalent linking group. 01 is an acid-dissociable group represented by the above general formula (a1-r-1), (a1-r-2), or (a1-r-4). q is an integer of 0 to 3. n is an integer of 1 or greater, provided that n≦q×2+4.

[0159] In the formulas (a1-1) to (a1-3), R is the same as R in the formula (g0-1). R is preferably a hydrogen atom, an alkyl group having 1 to 5 carbon atoms, or a fluorinated alkyl group having 1 to 5 carbon atoms, and more preferably a hydrogen atom or a methyl group.

[0160] In the formula (a1-1), Va 1 The divalent hydrocarbon group in may be an aliphatic hydrocarbon group or an aromatic hydrocarbon group. 1 As the divalent hydrocarbon group in the formula (g0-1), 0 Examples of the divalent linking group include the same divalent hydrocarbon groups as those exemplified in the formula (Va). 1 is preferably an aliphatic hydrocarbon group, more preferably a linear or branched alkylene group having 1 to 10 carbon atoms, and even more preferably a linear alkylene group having 1 to 10 carbon atoms.

[0161] In the formula (a1-1), Ra 1 is preferably an acid-dissociable group represented by the above general formula (a1-r-2) or (a1-r-4), and among these, a group represented by the general formula (a1-r2-1) or an acid-dissociable group represented by the general formula (a1-r-4) is more preferred.

[0162] In the formula (a1-2), Wa 1 n in a2The +1-valent hydrocarbon group may be an aliphatic hydrocarbon group or an aromatic hydrocarbon group. The aliphatic hydrocarbon group means a hydrocarbon group that does not have aromaticity, and may be saturated or unsaturated, but is usually preferably saturated. Examples of the aliphatic hydrocarbon group include linear or branched aliphatic hydrocarbon groups, aliphatic hydrocarbon groups containing a ring in the structure, and groups combining linear or branched aliphatic hydrocarbon groups with aliphatic hydrocarbon groups containing a ring in the structure. a2 The +1 valence is preferably 2 to 4, more preferably 2 or 3. 2 is preferably an acid-dissociable group represented by the above general formula (a1-r-1).

[0163] In the formula (a1-3), Ya 001 The divalent linking group in is not particularly limited, but suitable examples include a divalent hydrocarbon group which may have a substituent, and a divalent linking group containing a hetero atom. 001 is preferably an ester bond [-C(=O)-O-, -O-C(=O)-], an ether bond (-O-), a linear or branched alkylene group, an aromatic hydrocarbon group, or a combination thereof, or a single bond. The alkylene group preferably has 1 to 10 carbon atoms, more preferably 1 to 6 carbon atoms, still more preferably 1 to 4 carbon atoms, and particularly preferably 1 to 3 carbon atoms. Among these, Ya 001 The alkyl group is preferably a combination of an ester bond [—C(═O)—O—, —O—C(═O)—] and a linear alkylene group, or a single bond, and more preferably a single bond.

[0164] In the formula (a1-3), Ya 01 The divalent linking group in is not particularly limited, but suitable examples include a divalent hydrocarbon group which may have a substituent, and a divalent linking group containing a hetero atom. 01Among the above, it is preferable that Ya is an ester bond [—C(═O)—O—, —O—C(═O)—], an ether bond (—O—), a linear or branched alkylene group, an aromatic hydrocarbon group, or a combination thereof, or a single bond. 01 The alkyl group is preferably a combination of an ester bond [—C(═O)—O—, —O—C(═O)—] and a linear alkylene group, or a single bond, and more preferably a single bond.

[0165] In the formula (a1-3), Rax 01 is preferably an acid dissociable group represented by the above general formula (a1-r-2) or (a1-r-4), and among these, an acid dissociable group represented by the general formula (a1-r-2) is more preferred, and a group represented by the general formula (a1-r2-1) is even more preferred.

[0166] In the formula (a1-3), q is an integer of 0 to 3. When q is 0, the structure is a benzene structure, when q is 1, the structure is a naphthalene structure, when q is 2, the structure is an anthracene structure, and when q is 3, the structure is a tetracene structure. In the formula (a1-3), n is an integer of 1 or more, preferably 1 to 5, more preferably 1 to 3, and even more preferably 1 or 2. In the formula (a1-3), n≦q×2+4. For example, when q is 1 and the structure is a naphthalene structure, all six hydrogen atoms of the naphthalene may be substituted with hydroxy groups. In the naphthalene, Ya 001 , -Ya 01 -C(=O)-O-Ra 01 The substitution positions of the group and the hydroxy group are not particularly limited.

[0167] Specific examples of the structural unit (a1) are shown below. In each of the following formulas, R α represents a hydrogen atom, a methyl group, or a trifluoromethyl group.

[0168]

[0169]

[0170]

[0171]

[0172]

[0173]

[0174]

[0175]

[0176]

[0177]

[0178]

[0179]

[0180]

[0181]

[0182] As the structural unit (a1), a structural unit represented by the above formula (a1-1) or a structural unit represented by the above formula (a1-3) is preferred, and a structural unit represented by the above formula (a1-1) is more preferred. Among these, a structural unit represented by the above formula (a1-1) is preferred. 1 , Rax 01 ) are preferably acid-dissociable groups represented by the above general formula (a1-r2-1), (a1-r2-3), (a1-r2-4) or (a1-r-4), respectively.

[0183] When the component (P) contains the structural unit (a1), the structural unit (a1) may be of one type, or may contain two or more types. The component (P) may or may not contain the structural unit (a1).

[0184] When the component (P) contains the structural unit (a1), the proportion of the structural unit (a1) in the component (P) is preferably 5 to 80 mol%, more preferably 10 to 75 mol%, even more preferably 30 to 70 mol%, and particularly preferably 30 to 60 mol%, relative to the total (100 mol%) of all structural units constituting the component (P). When the proportion of the structural unit (a1) is at or above the lower limit of the above-mentioned preferred range, residues are less likely to be generated when a resist pattern is formed. In addition, the adhesion of the resist film to the support is further improved, and pattern collapse is less likely to occur even when a fine resist pattern is formed. When the proportion of the structural unit (a1) is at or below the upper limit of the above-mentioned preferred range, a balance with the other structural units can be achieved, resulting in various favorable lithography properties when a resist pattern is formed.

[0185] Structural Unit (a11): The component (P) may include the structural unit (a11). The structural unit (a11) is the same as that described above for the component (G).

[0186] When the component (P) contains the structural unit (a11), the structural unit (a11) may be of one type or of two or more types. The component (P) may or may not contain the structural unit (a11). When the component (G) contains the structural unit (a11), the proportion of the structural unit (a11) in the component (G) relative to the total (100 mol%) of all structural units constituting the component (G) is, for example, 1 to 50 mol%, preferably 5 to 40 mol%, more preferably 10 to 30 mol%, and even more preferably 10 to 20 mol%. When the proportion of the structural unit (a11) is within the above-mentioned preferred range, various lithography properties are improved when a resist pattern is formed on a surface modification layer formed from the surface modification layer-forming composition of this embodiment.

[0187] The component (P) contained in the composition for forming a surface modification layer of the present embodiment may be used alone or in combination of two or more types.

[0188] Examples of the component (P) include polymeric compounds comprising a repeating structure of the structural unit (p0); polymeric compounds containing a repeating structure of the structural unit (p0) and the structural unit (a1); polymeric compounds containing a repeating structure of the structural unit (p0) and the structural unit (a11); polymeric compounds containing a repeating structure of the structural unit (p0), the structural unit (a1) and the structural unit (a11); polymeric compounds containing a repeating structure of the structural unit (p01), the structural unit (a1) and the structural unit (a11); polymeric compounds containing a repeating structure of the structural unit (p02), the structural unit (a1) and the structural unit (a11); polymeric compounds containing a repeating structure of the structural unit (p01), the structural unit (p02) and the structural unit (a11);

[0189] In polymeric compounds having a repeating structure of the structural unit (p0) and the structural unit (a11), the proportion of the structural unit (p0) relative to the total (100 mol%) of all structural units constituting the polymeric compound is preferably 20 to 90 mol%, more preferably 30 to 90 mol%, even more preferably 40 to 90 mol%, and particularly preferably 50 to 90 mol%. The proportion of the structural unit (a11) relative to the total (100 mol%) of all structural units constituting the polymeric compound is preferably 10 to 80 mol%, more preferably 10 to 70 mol%, even more preferably 10 to 60 mol%, and particularly preferably 10 to 50 mol%.

[0190] In polymeric compounds having a repeating structure of the structural unit (p0), the structural unit (a1), and the structural unit (a11), the proportion of the structural unit (p0) is preferably 20 to 80 mol%, and more preferably 30 to 70 mol%, relative to the total (100 mol%) of all structural units constituting the polymeric compound. The proportion of the structural unit (a1) is preferably 5 to 80 mol%, more preferably 10 to 75 mol%, even more preferably 30 to 70 mol%, and particularly preferably 30 to 60 mol%, relative to the total (100 mol%) of all structural units constituting the polymeric compound. The proportion of the structural unit (a11) is preferably 5 to 40 mol%, more preferably 10 to 30 mol%, and even more preferably 10 to 20 mol%, relative to the total (100 mol%) of all structural units constituting the polymeric compound.

[0191] The component (P) can be produced by dissolving the monomers that derive each structural unit in a polymerization solvent, and then adding a radical polymerization initiator such as azobisisobutyronitrile (AIBN) or dimethyl azobisisobutyrate (for example, V-601) to the solution and polymerizing. Alternatively, the component (P) can be produced by dissolving a monomer that derives the structural unit (p0) and a monomer that derives any structural unit (for example, the structural unit (a1), the structural unit (a11) or the like) in a polymerization solvent, adding a radical polymerization initiator such as those described above to polymerize, and then carrying out a deprotection reaction. During the polymerization, for example, HS-CH 2 -CH 2 -CH 2 -C(CF 3 ) 2 By using a chain transfer agent such as —OH in combination, it is possible to obtain a chain with —C(CF 3 ) 2 An —OH group may be introduced.

[0192] The weight-average molecular weight (Mw) of the component (P) (based on polystyrene standards measured by gel permeation chromatography (GPC)) is, for example, preferably 1,000 to 1,000,000, more preferably 100,000 to 600,000, even more preferably 150,000 to 500,000, and particularly preferably 200,000 to 400,000. When the weight-average molecular weight of the component (P) is within the above range, the adhesion of the resist film to the support is improved. The dispersity (Mw / Mn) of the component (P) is not particularly limited, but is preferably 1.0 to 4.0, and more preferably 1.0 to 3.0. Here, Mn represents the number-average molecular weight.

[0193] Specific examples of the component (P) are shown below, but are not limited to these. In each of the following formulas, R α represents a hydrogen atom, a methyl group, or a trifluoromethyl group.

[0194]

[0195]

[0196]

[0197]

[0198]

[0199]

[0200] The content of the component (P) in the composition for forming a surface modification layer of this embodiment is preferably 5 to 70 parts by mass, more preferably 5 to 60 parts by mass, even more preferably 5 to 50 parts by mass, and particularly preferably 10 to 50 parts by mass, relative to 100 parts by mass of the total mass of the components (G) and (P). By setting the content of the component (P) within the above-mentioned preferred range, the adhesion of the resist film to the support can be further improved.

[0201] <Other Components> The composition for forming a surface modification layer of this embodiment may contain other components in addition to the components (G) and (P). Examples of other components include organic solvents.

[0202] Any organic solvent can be used as long as it is capable of dissolving the components (G) and (P) to form a homogeneous solution. Examples of the organic solvent include those typically used as organic solvents in chemically amplified resist compositions.

[0203] Examples of organic solvents include lactones such as γ-butyrolactone; ketones such as acetone, methyl ethyl ketone, cyclohexanone, methyl-n-pentyl ketone, methyl isopentyl ketone, and 2-heptanone; polyhydric alcohols such as ethylene glycol, diethylene glycol, propylene glycol, and dipropylene glycol; compounds having an ester bond such as ethylene glycol monoacetate, diethylene glycol monoacetate, propylene glycol monoacetate, and dipropylene glycol monoacetate, and derivatives of polyhydric alcohols such as monoalkyl ethers of the above polyhydric alcohols or compounds having an ester bond, such as monomethyl ether, monoethyl ether, monopropyl ether, and monobutyl ether, or monophenyl ether [among these, propylene glycol monomethyl ether acetate (PGMEA) and propylene glycol monomethyl ether (PGME) are preferred]; Examples of suitable organic solvents include cyclic ethers such as dioxane, esters such as methyl lactate, ethyl lactate (EL), methyl acetate, ethyl acetate, butyl acetate, methyl pyruvate, ethyl pyruvate, methyl methoxypropionate, and ethyl ethoxypropionate, and aromatic organic solvents such as anisole, ethyl benzyl ether, cresyl methyl ether, diphenyl ether, dibenzyl ether, phenetole, butyl phenyl ether, ethylbenzene, diethylbenzene, pentylbenzene, isopropylbenzene, toluene, xylene, cymene, and mesitylene.

[0204] The organic solvent may be used alone or as a mixed solvent of two or more kinds. For example, the (G) and (P) components may be dissolved in a ketone solvent such as 2-heptanone, and then diluted with a dilution solvent such as PGMEA. The organic solvent may be used, for example, so that the total content of the (G) and (P) components in the surface modification layer-forming composition is 0.01 to 5 mass%, preferably 0.1 to 3 mass%, and more preferably 0.1 to 1 mass%. When the total content of the (G) and (P) components is equal to or greater than the preferred lower limit, the adhesion between the resist film and the support is improved. When the total content of the (G) and (P) components is equal to or less than the preferred upper limit, the surface modification layer-forming composition has an appropriate viscosity and is easily applied uniformly to the support.

[0205] The composition for forming a surface modification layer of this embodiment preferably contains the component (G), the component (P), and an organic solvent, and more preferably consists of the component (G), the component (P), and an organic solvent.

[0206] The surface modification layer-forming composition of this embodiment is used to form a surface modification layer provided between a support and a resist film. Formation of a surface modification layer using the surface modification layer-forming composition of this embodiment can be carried out by applying the surface modification layer-forming composition of this embodiment to a support and baking it, as described below. A resist film can be formed by applying a resist composition to the surface modification layer thus formed and baking it. In this way, a surface modification layer can be formed between a support and a resist film using the surface modification layer-forming composition of this embodiment.

[0207] <Support> The support to which the composition for forming a surface modification layer of this embodiment is applied is not particularly limited, and conventionally known supports can be used. Examples of the support include substrates for electronic components, and substrates on which a predetermined wiring pattern is formed. Specific examples of the support include silicon wafers; substrates made of metals such as copper, chromium, iron, and aluminum; and glass substrates. Examples of materials for the wiring pattern include copper, aluminum, nickel, and gold.

[0208] The support may be a substrate on which a processing layer is formed. Examples of the processing layer include various low-k films such as Si, SiO2, SiON, SiN, p-Si, α-Si, W, W-Si, Al, Cu, and Al-Si, and stopper films thereof. The support may be a substrate or the processing layer on which a hard mask layer is formed. The hard mask layer may be formed of an inorganic material or an organic material. Examples of inorganic materials for forming the hard mask layer include silicon oxide (SiO 2 film), silicon nitride film (Si 3 N 4 Examples of the organic material for forming the hard mask layer include a silicon oxide nitride film (SiON film), a silicon oxynitride film (SiON film), etc. Examples of the organic material for forming the hard mask layer include novolac resin.

[0209] <Resist composition> The resist composition to which the composition for forming a surface modification layer of this embodiment is applied is not particularly limited, and a conventionally known resist composition can be used. Commercially available resist compositions can be used without particular limitation.

[0210] The resist composition is preferably a chemically amplified resist composition. Examples of chemically amplified resist compositions include resist compositions that generate acid upon exposure and whose solubility in a developer changes due to the action of the acid. Such resist compositions contain a base component (A) (hereinafter also referred to as "component (A)") whose solubility in a developer changes due to the action of an acid. The resist composition may further contain (1) an acid generator component (B) (hereinafter also referred to as "component (B)") that generates acid upon exposure; (2) the component (A) may be a component that generates acid upon exposure; or (3) the component (A) may be a component that generates acid upon exposure and may further contain component (B). The resist composition may further contain a base component (D) (hereinafter also referred to as "component (D)"), at least one compound (E) (hereinafter also referred to as "component (E)") selected from the group consisting of organic carboxylic acids, and phosphorus oxo acids and derivatives thereof, a fluorine additive component (F) (hereinafter also referred to as "component (F)"), and an organic solvent component (S) (hereinafter also referred to as "component (S)").

[0211] The resist composition may be a positive resist composition or a negative resist composition. The resist composition may be for an alkaline development process in which an alkaline developer is used for the development treatment during resist pattern formation, or may be for a solvent development process in which a developer containing an organic solvent (organic developer) is used for the development treatment. The resist composition is preferably for an alkaline development process.

[0212] <<Base Component (A)>> The component (A) preferably contains a resin component (A1) (hereinafter also referred to as “component (A1)”) whose solubility in a developer changes under the action of an acid.

[0213] Regarding the Component (A1): The component (A1) preferably contains the structural unit (a1) described above. Examples of other structural units that the component (A1) may contain include the structural unit (a10) described above, a structural unit (a2) containing a lactone-containing cyclic group, and a structural unit (a8) derived from a compound represented by general formula (a8-1) described below.

[0214] Structural Unit (a1): The explanation for the structural unit (a1) is the same as that given above in relation to the component (P).

[0215] The structural unit (a1) contained in the component (A1) may be of one type, or may be of two or more types. As the structural unit (a1), a structural unit represented by the above formula (a1-1) or a structural unit represented by the above formula (a1-3) is more preferred, as these tend to further improve the properties (sensitivity, shape, etc.) in lithography using electron beams or EUV. Among these, an acid-dissociable group (Ra 1 , Rax 01 ) are preferably acid-dissociable groups represented by the above general formula (a1-r2-1), (a1-r2-3), (a1-r2-4) or (a1-r-4), respectively, and among these, it is particularly preferable to select those which are cyclic groups.

[0216] The proportion of the structural unit (a1) in the component (A1), based on the total (100 mol%) of all structural units constituting the component (A1), is preferably 5 to 80 mol%, more preferably 10 to 75 mol%, even more preferably 30 to 70 mol%, and particularly preferably 40 to 70 mol%. By ensuring that the proportion of the structural unit (a1) is at least the lower limit of the above-mentioned preferred range, lithography properties such as sensitivity, resolution, and roughness improvement are improved. On the other hand, by ensuring that the proportion is at most the upper limit of the above-mentioned preferred range, a balance with other structural units can be achieved, resulting in various favorable lithography properties.

[0217] Structural Unit (a10): The explanation for the structural unit (a10) is the same as that given above in relation to the component (G).

[0218] The structural unit (a10) contained in the component (A1) may be one type, or two or more types. The component (A1) may or may not contain the structural unit (a10), but preferably contains the structural unit (a10). When the component (A1) contains the structural unit (a10), the proportion of the structural unit (a10) in the component (A1) is preferably 20 to 80 mol%, more preferably 25 to 70 mol%, even more preferably 30 to 60 mol%, and particularly preferably 30 to 50 mol%, relative to the total (100 mol%) of all structural units constituting the component (A1). By ensuring that the proportion of the structural unit (a10) is at or above the lower limit, sensitivity is likely to be further improved. On the other hand, by ensuring that the proportion is at or below the upper limit, it is easier to achieve a balance with other structural units.

[0219] Structural Unit (a2): The component (A1) may include a structural unit (a2) that includes a lactone-containing cyclic group (provided that this does not fall under the category of the structural unit (a1)).

[0220] A "lactone-containing cyclic group" refers to a cyclic group that contains a ring (lactone ring) that contains -O-C(=O)- within its ring skeleton. The lactone ring is counted as the first ring, and when there is only a lactone ring, it is called a monocyclic group, and when there is also another ring structure, it is called a polycyclic group regardless of the structure. The lactone-containing cyclic group may be a monocyclic group or a polycyclic group. There are no particular restrictions on the lactone-containing cyclic group in the structural unit (a2), and any group can be used. Specific examples include groups represented by the following general formulae (a2-r-1) to (a2-r-7).

[0221] [In the formula, Ra' 21 are each independently a hydrogen atom, an alkyl group, an alkoxy group, a halogen atom, a halogenated alkyl group, a hydroxyl group, —COOR″, —OC(═O)R″, a hydroxyalkyl group, or a cyano group; R″ is a hydrogen atom, an alkyl group, or a lactone-containing cyclic group; A″ is an alkylene group having 1 to 5 carbon atoms which may contain an oxygen atom (—O—) or a sulfur atom (—S—), an oxygen atom, or a sulfur atom; n′ is an integer of 0 to 2, and m′ is 0 or 1. * represents a bond (the same applies hereinafter).

[0222] In the general formulas (a2-r-1) to (a2-r-7), Ra' 21 The alkyl group in Ra' is preferably an alkyl group having 1 to 6 carbon atoms. The alkyl group is preferably linear or branched. Specific examples include a methyl group, an ethyl group, a propyl group, an isopropyl group, an n-butyl group, an isobutyl group, a tert-butyl group, a pentyl group, an isopentyl group, a neopentyl group, and a hexyl group. Of these, a methyl group or an ethyl group is preferred, and a methyl group is particularly preferred. Ra' 21 The alkoxy group in the formula (1) is preferably an alkoxy group having 1 to 6 carbon atoms. The alkoxy group is preferably linear or branched. Specifically, 21 Examples of the alkyl groups include those mentioned as examples of the alkyl group in the above formula and an oxygen atom (—O—). 21 The halogen atom in Ra' is preferably a fluorine atom.21 As the halogenated alkyl group in the formula Ra′, 21 Examples of the halogenated alkyl group include groups in which some or all of the hydrogen atoms of the alkyl group have been substituted with the halogen atoms. As the halogenated alkyl group, a fluorinated alkyl group is preferred, and a perfluoroalkyl group is particularly preferred.

[0223] Ra' 21 In -COOR" and -OC(=O)R" in the formula (I), R" is either a hydrogen atom, an alkyl group, or a lactone-containing cyclic group. The alkyl group for R" may be linear, branched, or cyclic, and preferably has 1 to 15 carbon atoms. When R" is a linear or branched alkyl group, it preferably has 1 to 10 carbon atoms, more preferably has 1 to 5 carbon atoms, and is particularly preferably a methyl group or an ethyl group. When R" is a cyclic alkyl group, it preferably has 3 to 15 carbon atoms, more preferably has 4 to 12 carbon atoms, and most preferably has 5 to 10 carbon atoms. Specific examples include groups in which one or more hydrogen atoms have been removed from a monocycloalkane which may or may not be substituted with a fluorine atom or a fluorinated alkyl group; and groups in which one or more hydrogen atoms have been removed from a polycycloalkane such as a bicycloalkane, tricycloalkane, or tetracycloalkane. More specifically, groups in which one or more hydrogen atoms have been removed from a monocycloalkane such as cyclopentane or cyclohexane; 2,6 ] decane, tetracyclododecane, and other polycycloalkanes in which one or more hydrogen atoms have been removed. Examples of the lactone-containing cyclic group in R" include the same groups as those represented by the general formulae (a2-r-1) to (a2-r-7). Ra' 21 The hydroxyalkyl group in the formula (Ra') preferably has 1 to 6 carbon atoms. 21 and a group in which at least one hydrogen atom of the alkyl group is substituted with a hydroxyl group.

[0224] Ra' 21Among the above, each of the groups is preferably independently a hydrogen atom or a cyano group.

[0225] In the general formulae (a2-r-2), (a2-r-3), and (a2-r-5), the alkylene group having 1 to 5 carbon atoms for A" is preferably a linear or branched alkylene group, and examples thereof include a methylene group, an ethylene group, an n-propylene group, and an isopropylene group. When the alkylene group contains an oxygen atom or a sulfur atom, specific examples thereof include groups in which -O- or -S- is present at the terminal or between carbon atoms of the alkylene group, such as -O-CH 2 -, -CH 2 -O-CH 2 -, -S-CH 2 -, -CH 2 -S-CH 2 A" is preferably an alkylene group having 1 to 5 carbon atoms or -O-, more preferably an alkylene group having 1 to 5 carbon atoms, and most preferably a methylene group.

[0226] Of the structural units (a2), structural units derived from acrylate esters in which the hydrogen atom bonded to the α-position carbon atom may be substituted with a substituent are particularly preferred.

[0227] The structural unit (a2) contained in the component (A1) may be of one type, or may contain two or more types. The component (A1) may or may not contain the structural unit (a2). When the component (A1) contains the structural unit (a2), the proportion of the structural unit (a2) is preferably 1 to 20 mol %, more preferably 1 to 15 mol %, and even more preferably 1 to 10 mol %, relative to the total (100 mol %) of all structural units constituting the component (A1). When the proportion of the structural unit (a2) is at least the preferred lower limit, the effects achieved by including the structural unit (a2) can be fully obtained due to the aforementioned effects. When the proportion is at or below the upper limit, a balance with the other structural units can be achieved, resulting in various favorable lithography properties.

[0228] Structural Unit (a8): The structural unit (a8) is a structural unit derived from a compound represented by the following general formula (a8-1).

[0229] [In the formula, W 2 is a polymerizable group-containing group. x2 is a single bond or (n ax2 +1)valent linking group. x2 and W 2 may form a condensed ring. 1 is a fluorinated alkyl group having 1 to 12 carbon atoms. 2 R is a hydrogen atom or an organic group having 1 to 12 carbon atoms which may have a fluorine atom. 2 and Ya x2 may be bonded to each other to form a ring structure. ax2 is an integer from 1 to 3.

[0230] W 2 The "polymerizable group" in the polymerizable group-containing group is a group that enables a compound having a polymerizable group to be polymerized by radical polymerization or the like, and refers to a group that contains a multiple bond between carbon atoms, such as an ethylenic double bond.

[0231] The polymerizable group-containing group may be a group composed of only a polymerizable group, or may be a group composed of a polymerizable group and a group other than the polymerizable group. Examples of the group other than the polymerizable group include a divalent hydrocarbon group which may have a substituent, and a divalent linking group containing a hetero atom. Examples of the polymerizable group-containing group include a group represented by the chemical formula: C(R X11 ) (R X12 ) = C(R X13 ) -Ya x0 In this chemical formula, R X11 , R X12 and R X13 are each a hydrogen atom, an alkyl group having 1 to 5 carbon atoms, or a halogenated alkyl group having 1 to 5 carbon atoms, and Ya x0 is a single bond or a divalent linking group.

[0232] Ya x2 and W 2 The fused ring formed by 2 The polymerizable group at the site and Ya x2 and a fused ring formed by W 2 Other groups than the polymerizable group at the Yax2 and a fused ring formed by x2 and W 2 The fused ring formed by these may have a substituent.

[0233] The structural unit (a8) contained in the component (A1) may be of one type, or may contain two or more types. The component (A1) may or may not contain the structural unit (a8). The proportion of the structural unit (a8) in the component (A1) is preferably 0 to 50 mol %, and more preferably 0 to 30 mol %, relative to the total (100 mol %) of all structural units constituting the component (A1).

[0234] The resist composition may contain one type of component (A1), or two or more types of components may be used in combination.

[0235] Examples of the component (A1) include polymeric compounds that contain a repeating structure of the structural unit (a1) and the structural unit (a10); and polymeric compounds that contain a repeating structure of the structural unit (a1), the structural unit (a10), and the structural unit (a2).

[0236] The component (A1) can be produced by dissolving the monomers that derive the respective structural units in a polymerization solvent, and then adding a radical polymerization initiator such as azobisisobutyronitrile (AIBN) or dimethyl azobisisobutyrate (e.g., V-601) to the solution, followed by polymerization.

[0237] Regarding the component (A2): The resist composition of this embodiment may also use, as the component (A), a base component (A2) (hereafter referred to as "component (A2)") that does not fall under the category of the component (A1) and whose solubility in a developer changes under the action of acid. There are no particular limitations on the component (A2), and it may be arbitrarily selected from the many base components conventionally known for use in chemically amplified resist compositions. The component (A2) may be a polymeric compound or a low molecular weight compound, and may be used either alone or in combination of two or more types.

[0238] <Acid Generator Component (B)> The component (B) is not particularly limited, and any of those that have been proposed as acid generators for chemically amplified resist compositions can be used. Examples of such acid generators include onium salt-based acid generators such as iodonium salts and sulfonium salts; oxime sulfonate-based acid generators; diazomethane-based acid generators such as bisalkyl- or bisarylsulfonyldiazomethanes and poly(bissulfonyl)diazomethanes; nitrobenzyl sulfonate-based acid generators; iminosulfonate-based acid generators; and disulfone-based acid generators.

[0239] The amount of component (B) in the resist composition, relative to 100 parts by mass of component (A), is preferably 0 to 30 parts by mass, more preferably 0 to 20 parts by mass, even more preferably 0 to 10 parts by mass, and particularly preferably 0 to 8 parts by mass. By ensuring that the amount of component (B) falls within this preferred range, a homogeneous solution is more likely to be obtained when the respective components of the resist composition are dissolved in an organic solvent, and the storage stability of the resist composition is favorable.

[0240] <<Base Component (D)>> The component (D) acts as a quencher (acid diffusion controller) that traps acid generated in the resist composition upon exposure. Examples of the component (D) include a photodegradable base (D1) (hereinafter referred to as “component (D1)”) that decomposes upon exposure and loses its acid diffusion control properties, and a nitrogen-containing organic compound (D2) (hereinafter referred to as “component (D2)”) that does not fall under the category of component (D1).

[0241] Regarding the Component (D1): The component (D1) is not particularly limited as long as it is decomposed by exposure to light and loses its acid diffusion controllability, and examples thereof include compounds represented by any of the following general formulas (d1-1) to (d1-3):

[0242] [In the formula, Rd 1 ~Rd 4 represents a cyclic group which may have a substituent, a chain alkyl group which may have a substituent, or a chain alkenyl group which may have a substituent. 2In the above, no fluorine atom is bonded to the carbon atom adjacent to the S atom. 1 is a single bond or a divalent linking group; m is an integer of 1 or more; M m+ are each independently an m-valent organic cation.

[0243] M m+ The organic cation in the formula (I) is preferably a sulfonium cation or an iodonium cation.

[0244] The component (D1) may be any one of the above components (d1-1) to (d1-3), or a combination of two or more of them. When the resist composition contains the component (D1), the amount of the component (D1) within the resist composition is preferably 0.5 to 15 parts by mass, more preferably 1 to 12 parts by mass, and even more preferably 2 to 10 parts by mass, relative to 100 parts by mass of the component (A).

[0245] Regarding the component (D2), the component (D2) is not particularly limited as long as it acts as an acid diffusion controller and does not fall under the category of the component (D1), and any known component may be used. Among these, aliphatic amines are preferred, and among these, secondary aliphatic amines and tertiary aliphatic amines are particularly preferred.

[0246] The component (D2) may be used singly, or in combination of two or more types. When the resist composition contains the component (D2), the amount of the component (D2) within the resist composition is typically within a range from 0.01 to 5 parts by mass per 100 parts by mass of the component (A). By ensuring that the amount is within this range, the resist pattern shape and stability over time during storage can be improved.

[0247] <<At least one compound (E) selected from the group consisting of organic carboxylic acids, phosphorus oxo acids, and derivatives thereof>> The resist composition may contain at least one compound (E) (hereinafter referred to as "component (E)") selected from the group consisting of organic carboxylic acids, phosphorus oxo acids, and derivatives thereof as an optional component for the purposes of preventing sensitivity degradation and improving resist pattern shape and post-exposure stability. Specific examples of organic carboxylic acids include acetic acid, malonic acid, citric acid, malic acid, succinic acid, benzoic acid, and salicylic acid, with salicylic acid being preferred. Examples of phosphorus oxo acids include phosphoric acid, phosphonic acid, and phosphinic acid, with phosphonic acid being particularly preferred.

[0248] In the resist composition of this embodiment, the component (E) may be used either as a single type, or as a combination of two or more types. When the resist composition contains the component (E), the amount of the component (E) relative to 100 parts by mass of the component (A) is preferably 0.01 to 5 parts by mass, and more preferably 0.05 to 3 parts by mass.

[0249] <Fluorine Additive Component (F)> The component (F) is used to impart water repellency to the resist film, and when used as a resin separate from the component (A), it can improve lithography properties. Examples of the component (F) that can be used include the fluorine-containing polymeric compounds described in JP-A Nos. 2010-002870, 2010-032994, 2010-277043, 2011-13569, and 2011-128226.

[0250] The weight-average molecular weight (Mw) of component (F) (based on polystyrene standards measured by gel permeation chromatography) is preferably 1,000 to 50,000, more preferably 5,000 to 40,000, and most preferably 10,000 to 30,000. When the Mw is below the upper limit of this range, the component has sufficient solubility in a resist solvent for use as a resist, while when the Mw is above the lower limit of this range, the resulting resist film has good water repellency. The dispersity (Mw / Mn) of component (F) is preferably 1.0 to 5.0, more preferably 1.0 to 3.0, and most preferably 1.0 to 2.5.

[0251] The component (F) may be used singly, or in combination of two or more different compounds. When the resist composition contains the component (F), the amount of the component (F) relative to 100 parts by mass of the component (A) is preferably 0.5 to 10 parts by mass, and more preferably 1 to 10 parts by mass.

[0252] <Organic Solvent Component (S)> The component (S) may be used alone or as a mixed solvent of two or more kinds. Among them, propylene glycol monomethyl ether acetate (PGMEA), propylene glycol monomethyl ether (PGME), γ-butyrolactone, ethyl lactate (EL), and cyclohexanone are preferred.

[0253] A preferred component (S) is a mixed solvent of PGMEA and a polar solvent. The blending ratio (mass ratio) can be determined appropriately taking into account the compatibility of PGMEA with the polar solvent. A preferred component (S) is a mixed solvent of at least one selected from PGMEA and EL with γ-butyrolactone. In this case, the mass ratio of the former to the latter is preferably 70:30 to 95:5. The amount of component (S) used is not particularly limited and is set appropriately depending on the coating film thickness and at a concentration that allows application to a substrate or the like. The component (S) is generally used so that the solids concentration of the resist composition is within the range of 0.1 to 20% by mass, preferably 0.2 to 15% by mass.

[0254] The surface modification layer-forming composition of this embodiment contains component (P) in addition to component (G). This allows for the formation of a surface modification layer on a support using the surface modification layer-forming composition of this embodiment, and then forming a resist film on the surface modification layer. This improves the adhesion of the resist film to the support. Furthermore, the generation of residues during the formation of a resist pattern by exposure and development of the resist film can be suppressed. The reason for this effect is presumed to be as follows: By baking during the formation of the surface modification layer on the support, the epoxy group in the structural unit (g0) of component (G) undergoes ring-opening and crosslinks with the support. Meanwhile, when a resist film is formed on the surface modification layer, the affinity between the structural unit (p0) in component (P) and the resist film causes the resist film to adsorb to the surface modification layer. It is believed that these synergistic effects enhance the adhesion of the resist film to the support and reduce residues after the formation of the resist pattern.

[0255] (Method of forming a resist pattern) A method of forming a resist pattern according to a second aspect of the present invention includes the steps of: (i) forming a surface modification layer on a support using the composition for forming a surface modification layer according to the first aspect; (ii) forming a resist film on the surface modification layer formed on the support using a resist composition; (iii) exposing the resist film; and (iv) developing the exposed resist film to form a resist pattern.

[0256] <Step (i)> The support may be the same as that described in the first embodiment. The method for forming a surface modification layer on a support using a surface modification layer-forming composition is not particularly limited, and a conventionally known method may be used. For example, the surface modification layer can be formed by applying the surface modification layer-forming composition to a support using a conventionally known method such as a spinner, and then performing a baking treatment to volatilize the organic solvent.

[0257] The baking temperature in the baking treatment can be 80 to 400°C, preferably 100 to 300°C, more preferably 160 to 300°C, even more preferably 190 to 300°C, and particularly preferably 190 to 250°C. By setting the baking temperature within the above preferred range, it is possible to sufficiently improve the adhesion of the resist film to the support. The baking time can be 30 seconds to 10 minutes, preferably 50 seconds to 10 minutes, and more preferably 60 seconds to 10 minutes. By setting the baking time within the above preferred range, it is possible to sufficiently improve the adhesion of the resist film to the support.

[0258] The thickness of the surface modification layer is 1 to 5 nm, preferably 2 to 4 nm. By setting the thickness of the surface modification layer within this range, the effect of improving the adhesion of the resist film to the support can be sufficiently obtained. Furthermore, residues after forming the resist pattern can be reduced.

[0259] <Step (ii)> The resist composition may be the same as that described in the first embodiment. The method for forming a resist film on the surface modification layer using the resist composition is not particularly limited, and a conventionally known method may be used. For example, the resist composition is applied to the surface modification layer by a conventionally known method using a spinner or the like. Next, a bake (post-applied bake (PAB)) treatment is performed at a temperature of, for example, 80 to 150°C for 60 seconds to 10 minutes to form a resist film.

[0260] The thickness of the resist film can be 10 to 300 nm, preferably 15 to 200 nm, more preferably 20 to 100 nm, and even more preferably 20 to 50 nm. By setting the thickness of the resist film within this range, a resist pattern can be formed with high resolution and sufficient resistance to etching can be obtained.

[0261] <Step (iii)> The resist film can be exposed by a conventionally known method. For example, the resist film is selectively exposed using an exposure device such as an electron beam lithography device or an ArF lithography device, either through a mask (mask pattern) on which a predetermined pattern has been formed, or by direct irradiation with an electron beam without using a mask pattern. Thereafter, the resist film is baked (post-exposure bake (PEB)) for 60 seconds to 10 minutes at a temperature of 80 to 150°C.

[0262] The wavelength used for exposure is not particularly limited, and may be an ArF excimer laser, a KrF excimer laser, or a F 2 Radiation such as excimer laser, EUV (extreme ultraviolet), VUV (vacuum ultraviolet), EB (electron beam), X-ray, or soft X-ray can be used.

[0263] The exposure method for the resist film may be a normal exposure (dry exposure) performed in an inert gas such as air or nitrogen, or may be liquid immersion exposure (liquid immersion lithography). Liquid immersion exposure is an exposure method in which the space between the resist film and the lowest lens of the exposure apparatus is filled in advance with a solvent (immersion medium) having a refractive index greater than that of air, and exposure (immersion exposure) is performed in this state. The liquid immersion medium is preferably a solvent having a refractive index greater than that of air and smaller than that of the resist film to be exposed, and examples thereof include water, a fluorine-based inert liquid, a silicon-based solvent, and a hydrocarbon-based solvent. Water is preferably used as the liquid immersion medium.

[0264] <Step (iv)> The development treatment of the resist film after exposure can be carried out by a conventionally known method. In the case of an alkali development process, the development treatment is carried out using an alkali developer, and in the case of a solvent development process, the development treatment is carried out using a developer containing an organic solvent (organic developer). The development treatment is preferably carried out using alkali development.

[0265] An example of an alkaline developer used in the development treatment in the alkaline development process is a 0.1 to 10% by mass aqueous solution of tetramethylammonium hydroxide (TMAH). The organic solvent contained in the organic developer used in the development treatment in the solvent development process may be any organic solvent that can dissolve component (A) (component (A) before exposure), and can be appropriately selected from known organic solvents. Specific examples include polar solvents such as ketone solvents, ester solvents, alcohol solvents, nitrile solvents, amide solvents, and ether solvents, as well as hydrocarbon solvents.

[0266] The development process can be carried out by a known development method, such as a method of immersing the support in a developer for a certain period of time (dip method), a method of piling up the developer on the surface of the support by surface tension and leaving it standing for a certain period of time (puddle method), a method of spraying the developer onto the surface of the support (spray method), or a method of continuously applying the developer while scanning a developer application nozzle at a constant speed onto a support rotating at a constant speed (dynamic dispense method).

[0267] After the development treatment, a rinse treatment is preferably carried out. In the case of an alkaline development process, the rinse treatment is preferably a water rinse using pure water, and in the case of a solvent development process, a rinse solution containing an organic solvent is preferably used. In the case of a solvent development process, after the development treatment or rinse treatment, a treatment may be carried out to remove the developer or rinse solution adhering to the pattern using a supercritical fluid. After the development treatment or rinse treatment, drying is carried out. Furthermore, in some cases, a bake treatment (post-bake) may be carried out after the development treatment.

[0268] The rinse treatment (cleaning treatment) using a rinse solution can be carried out by a known rinse method, such as a method of continuously applying the rinse solution onto a support rotating at a constant speed (spin coating method), a method of immersing the support in the rinse solution for a certain period of time (dipping method), or a method of spraying the rinse solution onto the surface of the support (spray method).

[0269] According to the resist pattern forming method of the present embodiment described above, a surface modification layer is formed on a support using the surface modification layer forming composition according to the first aspect, and a resist film is formed on the surface modification layer, thereby improving the adhesion of the resist film to the support. Therefore, even when a fine pattern is formed, pattern collapse of the resist pattern can be suppressed. Furthermore, the generation of residues during resist pattern formation can be suppressed.

[0270] The surface modification layer-forming composition of the above-described embodiment and the various materials used in the resist pattern formation method of the above-described embodiment (e.g., resist composition, resist solvent, developer, rinse, etc.) preferably do not contain impurities such as metals, halogen-containing metal salts, acids, alkalis, and components containing sulfur or phosphorus atoms. Here, examples of impurities containing metal atoms include Na, K, Ca, Fe, Cu, Mn, Mg, Al, Cr, Ni, Zn, Ag, Sn, Pb, Li, or salts thereof. The content of impurities contained in these materials is preferably 200 ppb or less, more preferably 1 ppb or less, even more preferably 100 ppt (parts per trillion) or less, particularly preferably 10 ppt or less, and most preferably substantially absent (below the detection limit of the measuring device).

[0271] The present invention will be described in more detail below with reference to examples, but the present invention is not limited to these examples.

[0272] <Preparation of Composition for Forming Surface Modification Layer> Each composition for forming a surface modification layer of each example was prepared by mixing and dissolving the components shown in Tables 1 to 3. The resin component was dissolved in 2-heptanone and diluted with propylene glycol monomethyl ether acetate to prepare a solution with a solids concentration of 1,300 ppm (0.13% by mass).

[0273]

[0274]

[0275]

[0276] In Tables 1 to 3, the abbreviations have the following meanings: (G)-1: A polymer compound represented by the following formula (G-1). The weight average molecular weight (Mw) calculated in terms of standard polystyrene as determined by GPC measurement was 7,000, and the molecular weight dispersity (Mw / Mn) was 2.80. 13 The copolymer composition ratio (the proportion (molar ratio) of each structural unit in the structural formula) determined by C-NMR was l / m = 40 / 60. (G)-2: A polymer compound represented by the following formula (G-2). The weight average molecular weight (Mw) calculated in terms of standard polystyrene determined by GPC measurement was 7,000, and the molecular weight dispersity (Mw / Mn) was 2.80. 13 The copolymer composition ratio (the proportion (molar ratio) of each structural unit in the structural formula) determined by C-NMR was l / m = 80 / 20. (G)-3: A polymer compound represented by the following formula (G-3). The weight average molecular weight (Mw) calculated in terms of standard polystyrene determined by GPC measurement was 7,000, and the molecular weight dispersity (Mw / Mn) was 2.80. 13 The copolymer composition ratio (proportion (molar ratio) of each structural unit in the structural formula) determined by C-NMR was l / m / n=40 / 40 / 20.

[0277]

[0278] (P)-1: A polymer compound represented by the following formula (P-1): The weight average molecular weight (Mw) calculated in terms of standard polystyrene as determined by GPC measurement was 240,000, and the molecular weight dispersity (Mw / Mn) was 2.50. 13 The copolymer composition ratio (proportion (molar ratio) of each structural unit in the structural formula) determined by C-NMR was l / m / n / o = 35 / 40 / 15 / 10. (P)-2: Polymer compound represented by the following formula (P-2). The weight average molecular weight (Mw) calculated in terms of standard polystyrene determined by GPC measurement was 240,000, and the molecular weight dispersity (Mw / Mn) was 2.50. 13 The copolymer composition ratio (proportion (molar ratio) of each structural unit in the structural formula) determined by C-NMR was l / m / n / o = 35 / 40 / 15 / 10. (P)-3: Polymer compound represented by the following formula (P-3). The weight average molecular weight (Mw) calculated in terms of standard polystyrene determined by GPC measurement was 240,000, and the molecular weight dispersity (Mw / Mn) was 2.50. 13The copolymer composition ratio (proportion (molar ratio) of each structural unit in the structural formula) determined by C-NMR was l / m / n / o = 35 / 40 / 15 / 10. (P)-4: Polymer compound represented by the following formula (P-4). The weight average molecular weight (Mw) calculated in terms of standard polystyrene determined by GPC measurement was 240,000, and the molecular weight dispersity (Mw / Mn) was 2.50. 13 The copolymer composition ratio (proportion (molar ratio) of each structural unit in the structural formula) determined by C-NMR was l / m / n / o = 35 / 40 / 15 / 10. (P)-5: Polymer compound represented by the following formula (P-5). The weight average molecular weight (Mw) calculated in terms of standard polystyrene determined by GPC measurement was 240,000, and the molecular weight dispersity (Mw / Mn) was 2.50. 13 The copolymer composition ratio (proportion (molar ratio) of each structural unit in the structural formula) determined by C-NMR was l / m / n / o = 35 / 40 / 15 / 10. (P)-6: Polymer compound represented by the following formula (P-6). The weight average molecular weight (Mw) calculated in terms of standard polystyrene determined by GPC measurement was 240,000, and the molecular weight dispersity (Mw / Mn) was 2.50. 13 The copolymer composition ratio (proportion (molar ratio) of each structural unit in the structural formula) determined by C-NMR was l / m / n / o = 35 / 40 / 15 / 10. (P)-7: Polymer compound represented by the following formula (P-7). The weight average molecular weight (Mw) calculated in terms of standard polystyrene determined by GPC measurement was 240,000, and the molecular weight dispersity (Mw / Mn) was 2.50. 13 The copolymer composition ratio (proportion (molar ratio) of each structural unit in the structural formula) determined by C-NMR was l / m / n / o = 35 / 40 / 15 / 10. (P)-8: Polymer compound represented by the following formula (P-8). The weight average molecular weight (Mw) calculated in terms of standard polystyrene determined by GPC measurement was 240,000, and the molecular weight dispersity (Mw / Mn) was 2.50. 13 The copolymer composition ratio (proportion (molar ratio) of each structural unit in the structural formula) determined by C-NMR was l / m / n / o = 35 / 40 / 15 / 10. (P)-9: Polymer compound represented by the following formula (P-9). The weight average molecular weight (Mw) calculated in terms of standard polystyrene determined by GPC measurement was 240,000, and the molecular weight dispersity (Mw / Mn) was 2.50. 13The copolymer composition ratio (proportion (molar ratio) of each structural unit in the structural formula) determined by C-NMR was l / m / n / o = 35 / 40 / 15 / 10. (P)-10: Polymer compound represented by the following formula (P-10). The weight average molecular weight (Mw) calculated in terms of standard polystyrene determined by GPC measurement was 240,000, and the molecular weight dispersity (Mw / Mn) was 2.50. 13 The copolymer composition ratio (proportion (molar ratio) of each structural unit in the structural formula) determined by C-NMR was l / m / n / o = 35 / 40 / 15 / 10. (P)-11: Polymer compound represented by the following formula (P-11). The weight average molecular weight (Mw) calculated in terms of standard polystyrene determined by GPC measurement was 240,000, and the molecular weight dispersity (Mw / Mn) was 2.50. 13 The copolymer composition ratio (proportion (molar ratio) of each structural unit in the structural formula) determined by C-NMR was l / m / n / o = 35 / 40 / 15 / 10. (P)-12: A polymer compound represented by the following formula (P-12). The weight average molecular weight (Mw) calculated in terms of standard polystyrene determined by GPC measurement was 240,000, and the molecular weight dispersity (Mw / Mn) was 2.50. 13 The copolymer composition ratio (proportion (molar ratio) of each structural unit in the structural formula) determined by C-NMR was l / m / n / o = 35 / 40 / 15 / 10. (P)-13: Polymer compound represented by the following formula (P-13). The weight average molecular weight (Mw) calculated in terms of standard polystyrene determined by GPC measurement was 240,000, and the molecular weight dispersity (Mw / Mn) was 2.50. 13 The copolymer composition ratio (proportion (molar ratio) of each structural unit in the structural formula) determined by C-NMR was l / m / n / o = 35 / 40 / 15 / 10. (P)-14: Polymer compound represented by the following formula (P-2). The weight average molecular weight (Mw) calculated in terms of standard polystyrene determined by GPC measurement was 240,000, and the molecular weight dispersity (Mw / Mn) was 2.50. 13 The copolymer composition ratio (proportion (molar ratio) of each structural unit in the structural formula) determined by C-NMR was l / m / n = 55 / 35 / 10. (P)-15: A polymer compound represented by the following formula (P-15). The weight average molecular weight (Mw) calculated in terms of standard polystyrene determined by GPC measurement was 240,000, and the molecular weight dispersity (Mw / Mn) was 2.50. 13The copolymer composition ratio (proportion (molar ratio) of each structural unit in the structural formula) determined by C-NMR was l / m / n=55 / 35 / 10.

[0279]

[0280]

[0281]

[0282]

[0283]

[0284]

[0285] <Formation of Resist Pattern> (Examples 1 to 29, Comparative Examples 1 to 3) The surface modification layer-forming compositions shown in Tables 4 to 6 were applied to silicon substrates and glass substrates using a spinner, and the resulting compositions were baked on a hot plate as shown in Tables 4 to 6 to form surface modification layers with a thickness of 3 nm. Next, a positive EB resist (OEBR-CAP1000AE, manufactured by Tokyo Ohka Kogyo Co., Ltd.) was applied to the surface modification layer using a spinner, and baked at 100°C for 60 seconds on silicon substrates and 10 minutes on glass substrates to form a 30 nm thick resist film. Next, the resist film was subjected to exposure to light using a JEOL JBX-9300FS electron beam lithography system (manufactured by JEOL Ltd.) at an acceleration voltage of 100 kV, resulting in a 1:1 line and space pattern (hereinafter referred to as "LS pattern") with a target size of 20 nm, 25 nm, or 30 nm line width. Thereafter, a post-exposure bake (PEB) treatment was performed at 80°C for 60 seconds for the silicon substrate and for 10 minutes for the glass substrate. Subsequently, alkaline development was performed for 30 seconds at 23°C using a 2.38% by mass tetramethylammonium hydroxide (TMAH) aqueous solution "NMD-3" (trade name, manufactured by Tokyo Ohka Kogyo Co., Ltd.). This was followed by a water rinse for 15 seconds using pure water. As a result, a 1:1 LS pattern with a line width of 30 nm, 25 nm, or 20 nm was formed.

[0286] [Evaluation of LS Pattern Shape] The shape of the LS pattern formed by the above <Formation of Resist Pattern> was observed using a critical dimension SEM (scanning electron microscope, accelerating voltage 800 V, product name: SU-8000, manufactured by Hitachi High-Technologies Corporation). There was no difference in the evaluation results between the case where a silicon substrate was used and the case where a glass substrate was used.

[0287] (Evaluation Method) The 1:1 LS pattern shapes with line widths of 30 nm, 25 nm, and 20 nm were evaluated according to the following evaluation criteria. The results are shown in Tables 4 to 6 under "30 nm LS," "25 nm LS," and "20 nm LS," respectively. The "Evaluation" in Tables 4 to 6 shows the overall evaluation. <Evaluation Criteria> A: No residue, and sufficient resist adhesion effect (no pattern collapse). B: Some residue, and sufficient adhesion effect (no pattern collapse). C: Some residue, and adhesion effect (partial pattern collapse). D: Much residue, or no adhesion effect (no pattern formed).

[0288]

[0289]

[0290]

[0291] From the results shown in Tables 4 to 6, it was confirmed that in Examples 1 to 29, which used compositions (M1)-1 to (M1)-21 for forming a surface modification layer, there was little or no residue after resist pattern formation, and the adhesion of the resist film to the substrate was also good, regardless of the LS pattern. Generally, finer 20 nm LS patterns are more likely to leave residue than 30 nm LS patterns, making it difficult to achieve effective adhesion. In Examples 1 to 29, even with 20 nm LS patterns, there was little residue and effective adhesion was achieved. On the other hand, in Comparative Examples 1 to 3, which used compositions (M2)-1 to (M2)-3 for forming a surface modification layer, the adhesion of the resist film to the substrate was poor, making it impossible to form a pattern, or even if a resist pattern was formed, a large amount of residue was generated. It was also confirmed that the (P) component preferably contains a structural unit (a1) containing an acid-decomposable group whose polarity increases under the action of acid, and preferably contains two or more structural units (p0) represented by general formula (p0-1). It was confirmed that the baking temperature when forming the surface modification layer is preferably 190° C. or higher.

[0292] Although the preferred embodiments of the present invention have been described above, the present invention is not limited to these embodiments. Addition, omission, substitution, and other modifications of the configuration are possible within the scope of the spirit of the present invention. The present invention is not limited by the above description, but is limited only by the scope of the appended claims.

Claims

1. A composition for forming a surface modification layer for forming a surface modification layer provided between a support and a resist film, comprising: a resin component (G) having a structural unit (g0) represented by the following general formula (g0-1); and a resin component (P) having a structural unit (p0) represented by the following general formula (p0-1). [In the formula, R represents a hydrogen atom, an alkyl group having 1 to 5 carbon atoms, or a halogenated alkyl group having 1 to 5 carbon atoms; 0 represents a divalent linking group; Rg 0 represents an epoxy group-containing group. [In the formula, R represents a hydrogen atom, an alkyl group having 1 to 5 carbon atoms, or a halogenated alkyl group having 1 to 5 carbon atoms; 0 represents a divalent linking group; Rp 0 represents a chain hydrocarbon group having 2 to 20 carbon atoms which may have a substituent.

2. Rg in the general formula (g0-1) 0 The composition for forming a surface modification layer according to claim 1, wherein is a group represented by the following general formula (rg-1) or an alicyclic epoxy group. [In the formula, Rg 01 ~Rg 03 each independently represents a hydrogen atom or an alkyl group. * represents a bond.

3. A composition for forming a surface modification layer according to claim 1 or 2, wherein the resin component (P) contains a structural unit (a1) that contains an acid-decomposable group whose polarity increases due to the action of an acid.

4. The composition for forming a surface modification layer according to claim 1 or 2, wherein the resin component (P) has two or more types of structural units (p0).

5. A composition for forming a surface modification layer according to claim 1 or 2, wherein the content of the resin component (P) is 5 to 50 parts by mass per 100 parts by mass of the total mass of the resin component (G) and the resin component (P).

6. A method for forming a resist pattern, comprising: a step (i) of forming a surface modification layer on a support using a composition for forming a surface modification layer according to claim 1 or 2; a step (ii) of forming a resist film on the surface modification layer formed on the support using a resist composition; a step (iii) of exposing the resist film; and a step (iv) of developing the exposed resist film to form a resist pattern.

7. The method for forming a resist pattern according to claim 6, wherein the film thickness of the surface modification layer is 1 to 5 nm.

Citation Information

Patent Citations

  • Resist composition for liquid immersion lithography, resist pattern forming method, and fluorine-containing polymer compound

    JP2010002870A

  • Resist composition for immersion exposure, method of forming resist pattern using the same, and fluorine-containing compound

    JP2010032994A

  • Positive resist composition and method of forming resist pattern

    JP2010277043A

  • Positive type resist composition, method of forming resist pattern using the same, and fluorine-contained high molecular compound

    JP2011013569A

  • Positive resist composition and resist pattern forming method

    JP2011128226A