Welding machine
The welding device addresses the challenge of defect detection in lithium secondary battery electrode tabs by using ultrasonic vibrations and a vision sensor to inspect holes in the metal materials, ensuring reliable welding and easy maintenance.
Patent Information
- Application Number
- PCT/KR2023/018393
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-05-09
- Filing Date
- 2023-11-15
- Publication Date
- 2024-11-14
AI Technical Summary
Current welding technologies for electrode tabs in lithium secondary batteries lack efficient methods for quickly and accurately detecting welding defects, making maintenance and repair challenging.
A welding device equipped with a detection unit that creates holes in the metal materials using ultrasonic vibrations and a vision sensor to inspect these holes for defect detection, featuring a horn with protrusions and an anvil with a cutting blade for easy maintenance and repair.
Enables quick and accurate detection of welding defects, ensuring reliable welding and facilitating easy maintenance and repair by forming holes in the metal materials for quality assessment.
Smart Images

Figure KR2023018393_14112024_PF_FP_ABST
Abstract
Description
welding equipment
[0001] The present invention relates to a welding device.
[0002] This application claims priority to Korean Patent Application No. 10-2023-0059969, filed May 9, 2023, the entire disclosure of which is incorporated herein by reference.
[0003] As demand for portable electronic products such as laptops, video cameras, and mobile phones rapidly increases and the commercialization of robots and electric vehicles becomes more widespread, research into high-performance secondary batteries capable of repeated charging and discharging is actively underway.
[0004] Currently commercialized secondary batteries include nickel-cadmium batteries, nickel-hydrogen batteries, nickel-zinc batteries, and lithium secondary batteries. Among these, lithium secondary batteries are receiving attention for their advantages of being able to charge and discharge freely, having a very low self-discharge rate, and having a high energy density, as they have almost no memory effect compared to nickel-based secondary batteries.
[0005] In general, lithium secondary batteries can be classified into can-type secondary batteries in which the electrode assembly is built into a metal can and pouch-type secondary batteries in which the electrode assembly is built into a pouch of an aluminum laminate sheet, depending on the shape of the outer packaging material.
[0006] Additionally, electrode tabs provided in multiple electrode assemblies may be joined by welding. After the multiple electrode tabs are welded, they may be connected to the electrode leads by welding.
[0007] At this time, multiple electrode tabs can be joined through a two-step welding process. The multiple electrode tabs can be initially joined through ultrasonic welding. Subsequently, the multiple electrode tabs can be secondarily joined through laser welding. When multiple electrode tabs are joined through ultrasonic welding, it is necessary to quickly and accurately detect welding defects.
[0008] The present invention aims to solve the above-mentioned problems and other problems.
[0009] In particular, one object of the present invention may be to provide a welding device including a detection unit capable of quickly and accurately detecting a welding defect.
[0010] Another object of the present invention may be to provide a welding device that is easy to maintain and repair.
[0011] In order to achieve the above object, a welding device according to one embodiment of the present invention is a device for welding a plurality of metal materials, which may include: an anvil on which the plurality of metal materials are placed; a horn positioned on the anvil and including a plurality of protrusions protruding toward the anvil; and a processor for vibrating the horn so as to create holes penetrating the plurality of metal materials.
[0012] Additionally, the welding device may be configured to further include a vision sensor that detects the hole.
[0013] Additionally, the processor can vibrate the plurality of protrusions to draw a circular trajectory.
[0014] In addition, the plurality of protrusions may include: a welding protrusion that welds the plurality of metal materials; and a first penetrating protrusion that creates a hole that penetrates the plurality of metal materials.
[0015] Additionally, the protrusion length of the first penetration projection may be configured to be longer than the protrusion length of the welding projection.
[0016] Additionally, the anvil may include a receiving portion facing the first through-hole.
[0017] Additionally, the anvil may be configured to further include a cutting blade formed around the receiving portion.
[0018] Additionally, the anvil may be configured such that at least a portion of the plurality of metal materials is accommodated in the receiving portion.
[0019] Additionally, the cutting blade may be configured to be replaceable.
[0020] Additionally, the anvil may include a second through-hole protrusion protruding toward the horn and facing the first through-hole protrusion.
[0021] Additionally, the horn may further include a groove formed around the first through-hole.
[0022] Additionally, the horn may be configured to form a protrusion around the hole of the plurality of metal materials.
[0023] Additionally, the second through-hole protrusion may be configured to be replaceable.
[0024] In addition, a battery cell according to one aspect of the present invention includes a plurality of metal materials welded by a welding device according to the present invention.
[0025] According to at least one of the embodiments of the present invention, welding defects can be detected quickly and accurately.
[0026] According to at least one embodiment of the present invention, holes can be formed in a plurality of metal materials to detect welding defects.
[0027] According to at least one of the embodiments of the present invention, a welding device including a detection unit capable of quickly and accurately detecting a welding defect can be provided.
[0028] According to at least one of the embodiments of the present invention, a welding device that is easy to maintain and repair can be provided.
[0029] The following drawings attached to this specification illustrate preferred embodiments of the present invention, and together with the detailed description of the invention described below, serve to further understand the technical idea of the present invention, and therefore, the present invention should not be interpreted as being limited to matters described in such drawings.
[0030] Figure 1 is a drawing showing an example of a battery cell.
[0031] Fig. 2 is a drawing showing a part of a cross-sectional configuration along the cutting line A-A' of Fig. 1.
[0032] Figure 3 is a drawing showing a welding device according to one embodiment of the present invention.
[0033] FIG. 4 is a drawing showing an example of a welding device's horn transmitting vibration according to one embodiment of the present invention.
[0034] FIGS. 5 and 6 are drawings showing a process of forming holes in a plurality of metal materials by a welding device according to one embodiment of the present invention.
[0035] Figure 7 is a drawing showing welding being performed by a welding device according to one embodiment of the present invention.
[0036] Figure 8 is a drawing showing a welding device according to another embodiment of the present invention.
[0037] FIG. 9 is a drawing showing a welding device according to another embodiment of the present invention.
[0038] FIG. 10 is a drawing showing an example of inspecting welding quality using a welding device according to one embodiment of the present invention.
[0039] Fig. 11 is a drawing showing a welding device according to another embodiment of the present invention.
[0040] Fig. 12 is a drawing showing a welding device according to another embodiment of the present invention.
[0041] FIG. 13 is a drawing showing welding being performed by a welding device according to another embodiment of the present invention.
[0042] Fig. 14 is a drawing showing a welding device according to another embodiment of the present invention.
[0043] FIG. 15 is a view looking at a first through-hole of a welding device according to another embodiment of the present invention.
[0044] FIG. 16 is a drawing showing a welding device according to another embodiment of the present invention.
[0045] FIG. 17 is a drawing showing an example of inspecting welding quality by a welding device according to another embodiment of the present invention.
[0046] Hereinafter, preferred embodiments of the present invention will be described in detail with reference to the attached drawings. Prior to this, it should be noted that the terms and words used in this specification and claims should not be construed as limited to their conventional or dictionary meanings. Based on the principle that the inventor can appropriately define the concepts of terms to best explain his or her invention, they should be interpreted in a way that aligns with the technical spirit of the present invention.
[0047] Accordingly, the embodiments described in this specification and the configurations illustrated in the drawings are only the most preferred embodiments of the present invention and do not represent all of the technical ideas of the present invention, and it should be understood that there may be various equivalents and modified examples that can replace them at the time of filing this application.
[0048] FIG. 1 is a drawing showing an example of a battery cell (600). FIG. 2 is a drawing showing a part of a cross-sectional configuration taken along the line A-A' of FIG. 1. FIG. 3 is a drawing showing a welding device according to an embodiment of the present invention. Referring to FIGS. 1 to 3, a welding device according to an embodiment of the present invention may include an anvil (100), a horn (200), and a processor (not shown). The battery cell (600) may refer to a secondary battery. And, the battery cell (600) may be a pouch-type secondary battery. The battery cell (600) may include a plurality of electrode assemblies (630). The electrode assemblies (630) may be configured such that an electrode active material is coated on an electrode current collector metal. A portion of the electrode current collector may extend to form an electrode tab (610). The electrode tab (610) may be provided on each electrode assembly (630). A plurality of electrode tabs (610) can be joined by welding. And, the plurality of electrode tabs (610) can be joined to electrode leads (620). The battery cell (600) can be configured to include an electrode assembly (630), electrode tabs (610), and a case (640) that surrounds the electrode leads (620). The case (640) can be configured to surround at least a portion of the electrode leads (620). The electrode tabs (610) can be referred to as a metal foil (610) or a metal material (610). The electrode tabs (610) can be joined by laser welding after ultrasonic welding.
[0049] The welding device may be configured to weld a plurality of metal materials (610). The plurality of metal materials (610) may be a plurality of electrode tabs (610) that are placed in an overlapping manner or a plurality of stacked electrode tabs (610). The welding device may ultrasonically weld the plurality of electrode tabs (610).
[0050] The anvil (100) may be configured to accommodate a plurality of metal materials (610). For example, the anvil (100) may be configured to have a wide surface on its upper portion, and to allow the metal materials to be settled on this wide surface. Furthermore, the anvil (100) may be configured to stably support the plurality of metal materials (610) even while welding is in progress.
[0051] The horn (200) may be positioned on the anvil (100). The horn (200) may be configured to include a plurality of protrusions (220, 230) protruding toward the anvil (100). The plurality of protrusions (220, 230) may contact a plurality of metal materials (610) to transmit ultrasonic vibrations.
[0052] The processor may be configured to operate and control the welding device. The processor may vibrate the horn (200) to create a hole (611) penetrating a plurality of metal materials (610).
[0053] According to this configuration of the present invention, the welding device can weld a plurality of metal materials (610) and simultaneously create holes penetrating the plurality of metal materials (610). Accordingly, a user or a processor can confirm whether the plurality of metal materials (610) have been properly welded by confirming that holes penetrating the plurality of metal materials (610) have been formed. For example, if holes penetrating the plurality of metal materials (610) are not confirmed, it can be determined that the welding of the plurality of metal materials (610) has not been successfully performed.
[0054] According to this configuration of the present invention, a user or a processor can clearly and easily determine whether welding of a plurality of metal materials (610) is successful.
[0055] FIG. 4 is a drawing showing an example of a horn (200) of a welding device according to an embodiment of the present invention transmitting vibration. Referring to FIGS. 3 and 4, the welding device according to an embodiment of the present invention may be configured such that a plurality of protrusions (220, 230) vibrate while drawing a circular trajectory. In particular, in FIG. 4, one protrusion (230) is illustrated as vibrating in a circular manner, but another protrusion (220) may also vibrate in a circular trajectory in the same manner. In addition, the circular vibration of these protrusions (220, 230) may be controlled by a processor.
[0056] Conventional welding devices are configured to form straight welding lines. However, according to this configuration of the present invention, the plurality of welding protrusions (220, 230) are configured to trace a circular trajectory, thereby reducing the number of welding spots or indentations compared to straight welding lines. This allows for a wider spacing between the plurality of protrusions (220, 230), and increases the degree of freedom in changing the shape of each protrusion (220, 230).
[0057] FIGS. 5 and 6 are drawings showing a process of forming holes in a plurality of metal materials (610) by a welding device according to an embodiment of the present invention. Referring to FIGS. 3 to 6, the plurality of protrusions (220, 230) of the welding device according to an embodiment of the present invention may be configured to include a welding protrusion (220) that welds a plurality of metal materials (610) and a first penetrating protrusion (230) that creates holes (611) that penetrate the plurality of metal materials (610).
[0058] When ultrasonic vibration is generated from the horn (200), the welding projection (220) can weld a plurality of metal materials (610). At the same time, the first penetrating projection (230) can form a hole (611) that penetrates the plurality of metal materials (610). The welding projection (220) and the first penetrating projection (230) can each be configured with at least one or more. In addition, the first penetrating projection (230) can be positioned adjacent to the welding projection (220).
[0059] According to this configuration of the present invention, since welding and hole creation are performed simultaneously, the reliability of determining whether welding is successful based on whether a hole is formed or the size of the hole formed can be improved.
[0060] Referring to FIGS. 3 to 6, the protrusion length (h2) of the first penetration projection (230) of the welding device according to one embodiment of the present invention may be configured to be longer than the protrusion length (h1) of the welding projection (220).
[0061] The body (210) of the horn (200) may be positioned to face the anvil (100). And, the welding projection (200) and the first through-hole projection (230) may be formed on the body (210) of the horn (200). The body (210) of the horn (200) may have one side facing the anvil (100), and the one side may have a flat shape. The body (210) of the horn (200) and the anvil (100) may be configured to maintain a constant distance while welding is in progress. While welding is in progress, the welding projection (220) and the first through-hole projection (230) may come into contact with a plurality of metal materials (610).
[0062] According to this configuration of the present invention, while welding is in progress, the first through-hole protrusion (230) can press the plurality of metal materials (610) downward. Due to the first through-hole protrusion (230), at least a portion of the plurality of metal materials (610) can be pushed downward. Alternatively, due to the first through-hole protrusion (230), a hole (611) penetrating the plurality of metal materials (610) can be formed.
[0063] Referring to FIGS. 3 to 6, the anvil (100) of the welding device according to one embodiment of the present invention may be configured to include a receiving portion (111) facing the first through-hole (230).
[0064] The receiving portion (111) may be formed on the upper surface of the body (110) of the anvil (100). As welding progresses, the distance between the receiving portion (111) and the first through-hole protrusion (230) may become shorter. During welding, at least a portion of the plurality of metal materials (610) pushed by the first through-hole protrusion (230) may be configured to be received in the receiving portion (111).
[0065] According to this configuration of the present invention, while welding is in progress, the receiving portion (111) can easily form a hole (611) by receiving at least a portion of a plurality of metal materials (610).
[0066] Referring to FIGS. 3 to 6, the anvil (100) of the welding device according to one embodiment of the present invention may be configured to further include a cutting blade (120) formed around the receiving portion (111).
[0067] The cutting blade (120) may be formed inwardly along the periphery of the receiving portion (111). The cutting blade (120) may cut at least a portion of the plurality of metal materials (610). Referring to FIGS. 5 and 6, while welding is in progress, at least a portion of the plurality of metal materials (610) may be pushed downward by the first penetrating protrusion (230). At this time, the pushed portion (612) may be cut by the cutting blade (120). As the first penetrating protrusion (230) vibrates while drawing a circular trajectory, a cutting line may be formed along the circular trajectory. As a result, at least a portion of the plurality of metal materials (610) may be separated into a circular chip (612) shape, and a circular hole (611) penetrating the plurality of metal materials (610) may be formed. A portion separated from a plurality of metal materials (610) may be referred to as a chip (612) or a piece (612).
[0068] According to this configuration of the present invention, at least a portion of the plurality of metal materials (610) can be cut while welding is in progress. This makes it easy to determine whether welding is successful, and the reliability of the determination can be improved.
[0069] FIG. 7 is a drawing showing welding performed by a welding device according to an embodiment of the present invention. Referring to FIG. 7, the anvil (100) of the welding device according to an embodiment of the present invention may be configured such that at least a portion of a plurality of metal materials (610) are accommodated in a receiving portion (111). The receiving portion (111) may be formed at a position facing the first through-protrusion (230). A portion of the plurality of metal materials (610) pushed out by the first through-protrusion (230) may be configured to be accommodated in the receiving portion (111). In addition, the chips (612) cut by the cutting blade (120) may fall downward due to gravity and be accommodated in the receiving portion (111).
[0070] According to this configuration of the present invention, chips (612) generated during welding can be separated from other components of the welding device by being accommodated in the receiving portion (111). As a result, welding defects or errors caused by chips (612) can be prevented.
[0071] FIG. 8 is a drawing illustrating a welding device according to another embodiment of the present invention. Referring to FIG. 8, the welding device according to one embodiment of the present invention may be configured to further include a weight measuring unit (400). The weight measuring unit (400) may be configured to be positioned in the receiving unit (111) of the anvil (100). The processor may be configured to detect the weight measured by the weight measuring unit (400). For example, the weight measuring unit (400) may be a scale (400).
[0072] According to this configuration of the present invention, the chip (612) generated during welding can be placed on the scale (400). Accordingly, the weight measuring unit (400) can detect the weight of the chip (612). Accordingly, while welding is performed multiple times, the processor can detect that the chip (612) is generated or added by detecting an increase in the weight measured by the weight measuring unit (400).
[0073] In addition, according to this configuration of the present invention, the processor can detect that a welding defect has occurred when it detects that there is no change in the weight of the scale while welding is performed multiple times.
[0074] Fig. 9 is a drawing showing a welding device according to another embodiment of the present invention. Referring to Fig. 9, the welding device according to one embodiment of the present invention may be configured to further include a suction device (500). The receiving portion (111) of the anvil (100) may be formed to penetrate the body (110). In addition, the suction device (500) may be configured to be connected or communicated with one end of the receiving portion (111). Chips (612) generated during welding may be suctioned into the suction device (500) through the receiving portion (110).
[0075] According to this configuration of the present invention, chips (612) generated during welding can be separated from other components of the welding device by being sucked in by the suction device (500). In addition, since the chips (612) do not accumulate inside the receiving portion (111), there is an advantage in that the inside of the receiving portion (111) does not need to be emptied.
[0076] FIG. 10 is a drawing showing an example of inspecting welding quality by a welding device according to an embodiment of the present invention. Referring to FIG. 10, the welding device according to an embodiment of the present invention may be configured to further include a vision sensor (300) that detects a hole (611). The vision sensor (300) can detect a hole (611) formed in a plurality of metal materials (610) by a first penetrating protrusion (230). The vision sensor (300) can detect whether the hole (611) is formed to penetrate. The processor can determine that the welding is defective when the hole (611) does not penetrate the plurality of metal materials (610), as shown in (a) of FIG. 10. In addition, the processor can determine that the welding is successful when the hole (611) penetrates the plurality of metal materials (610), as shown in (b) of FIG.
[0077] According to this configuration of the present invention, the success or failure of welding can be quickly and accurately determined.
[0078] Fig. 11 is a drawing showing a welding device according to another embodiment of the present invention. Referring to Fig. 11, the cutting blade (120a) of the welding device according to another embodiment of the present invention may be configured to be replaceable. The cutting blade (120a) may be detachably coupled or fastened to the receiving portion (111) of the anvil (100). The cutting blade (120a) may be configured to have an internal space. Chips (612) generated during welding may be accommodated or captured in the internal space formed by the cutting blade (120a).
[0079] According to this configuration of the present invention, the durability of the welding device can be improved. The cutting blade (120a) may wear out more quickly than other components of the welding device. If the cutting blade (120a) wears out, chip (612) formation may not occur smoothly, and the reliability of determining whether welding is successful may decrease. However, since the cutting blade (120a) is replaceable, maintenance of the welding device can be facilitated.
[0080] Fig. 12 is a drawing showing a welding device according to another embodiment of the present invention. Fig. 13 is a drawing showing welding being performed by the welding device illustrated in Fig. 12. Fig. 14 is a drawing showing a welding device according to another embodiment of the present invention. Referring to Figs. 12 to 14, the anvil (100) of the welding device according to one embodiment of the present invention may be configured to include a second through-hole (130) protruding toward the horn (200) and facing the first through-hole (230).
[0081] As welding progresses, the plurality of metal materials (610) positioned between the first through-hole protrusion (230) and the second through-hole protrusion (130) may be pushed out to the periphery. And, as the first through-hole protrusion (230) and the second through-hole protrusion (130) come into contact or meet, a hole (611) penetrating the plurality of metal materials (610) may be formed. At this time, the pushed out portion of the plurality of metal materials (610) may move to the periphery of the first through-hole protrusion (230).
[0082] According to this configuration of the present invention, a hole (611) penetrating a plurality of metal materials (610) can be formed. In addition, even if a hole (611) penetrating a plurality of metal materials (610) is formed, a chip (612) may not be generated.
[0083] FIG. 15 is a view looking at the first through-hole (230) of a welding device according to another embodiment of the present invention. Referring to FIGS. 12 to 15, the horn (200) of the welding device according to one embodiment of the present invention may be configured to further include a groove (211) formed around the first through-hole (230). The groove (211) may be formed in the body (210) of the horn (200). The groove (211) may be formed in an upward direction. The groove (211) may be formed around the circumference of the first through-hole (230) or adjacent to the first through-hole (230). In addition, the groove (211) may extend along the circumference of the first through-hole (230). The groove (211) may be formed in a circular shape surrounding the first through-hole (230).
[0084] According to this configuration of the present invention, the portions of the plurality of metal materials (610) pushed out by the first through-protrusion (230) and the second through-protrusion (130) can move along the surface of the first through-protrusion (230) and be accommodated in the groove (211). By being accommodated in the groove (211), the plurality of metal materials (610) can be separated from other components of the welding device. As a result, welding defects or errors caused by the pushed out plurality of metal materials (610) can be prevented.
[0085] Referring to FIGS. 12 to 15, the horn (200) of the welding device according to one embodiment of the present invention may be configured to form a protrusion (613) around a hole (611) of a plurality of metal materials (610). A portion of the plurality of metal materials (610) pushed out by the first through-hole (230) and the second through-hole (130) may be accommodated in the groove (211). As a result, a protrusion (613) may be formed along the perimeter of the hole (611) penetrating the plurality of metal materials (610). That is, the groove (211) may form the protrusion (613).
[0086] According to this configuration of the present invention, the processor can determine whether welding is successful by detecting the protrusion (613). By detecting the hole (611) penetrating a plurality of metal materials (610) and the protrusion (613), the processor can increase the accuracy of determining the welding quality.
[0087] Referring to FIGS. 12 to 15, the horn (200) of the welding device according to one embodiment of the present invention may be configured to further include a stopper (212). The stopper (212) may be formed on the body (210) and may be formed to protrude downward from the body (210). The stopper (212) may be formed along the periphery of the groove (211). The stopper (212) may extend to surround the groove (211). The stopper (212) may be formed in a circular shape that surrounds the groove (211) or the first through-hole (230).
[0088] According to this configuration of the present invention, the portion of the plurality of metal materials (610) pushed out by the first through-protrusion (230) and the second through-protrusion (130) can move along the surface of the first through-protrusion (230) and be accommodated in the groove (211). The stopper (212) can limit the plurality of metal materials (610) from spreading widely. In addition, the stopper (212) can guide the plurality of metal materials (610) to be stably accommodated in the groove (211). By being accommodated in the groove (211), the plurality of metal materials (610) can be separated from other components of the welding device. As a result, welding defects or errors caused by the pushed out plurality of metal materials (610) can be prevented.
[0089] Fig. 16 is a drawing showing a welding device according to another embodiment of the present invention. Referring to Fig. 16, the second through-hole protrusion (130a) of the welding device according to another embodiment of the present invention may be configured to be replaceable. The second through-hole protrusion (130a) may be detachably coupled or fastened to the receiving portion (111) of the anvil (100).
[0090] According to this configuration of the present invention, the durability of the welding device can be improved. The second through-hole projection (130a) may wear out more quickly than other components of the welding device due to contact or friction with the first through-hole projection (230). If the second through-hole projection (130a) wears out, the hole (611) may not be formed smoothly, and the reliability of determining whether welding is successful may decrease. However, since the second through-hole projection (130a) is replaceable, maintenance of the welding device can be facilitated.
[0091] FIG. 17 is a drawing showing an example of inspecting welding quality by a welding device according to another embodiment of the present invention. Referring to FIG. 17, the welding device according to one embodiment of the present invention may be configured to further include a vision sensor (300) that detects a hole (611). The vision sensor (300) can detect a hole (611) formed in a plurality of metal materials (610) by a first through-hole protrusion (230) and a second through-hole protrusion (130). The vision sensor (300) can detect whether the hole (611) is formed to penetrate. The processor can determine that the welding is defective when the hole (611) does not penetrate the plurality of metal materials (610), as shown in (a) of FIG. 17. In addition, the processor can determine that the welding is successful when the hole (611) penetrates the plurality of metal materials (610), as shown in (b) of FIG.
[0092] According to this configuration of the present invention, the success or failure of welding can be quickly and accurately determined.
[0093] A battery cell (600) according to one aspect of the present invention may include a plurality of metal materials (610) welded by the welding device of the present invention. Specifically, the plurality of metal materials (610) welded by the welding device of the present invention may be a plurality of electrode tabs (610).
[0094] Meanwhile, although terms indicating directions such as up, down, left, right, front, and back are used in this specification, it is obvious to those skilled in the art that these terms are only for convenience of explanation and may vary depending on the location of the target object or the location of the observer.
[0095] As described above, although the present invention has been described by limited embodiments and drawings, the present invention is not limited thereto, and it is obvious that various modifications and variations are possible within the scope of the technical idea of the present invention and the equivalent scope of the patent claims to be described below by a person having ordinary skill in the art to which the present invention pertains.
Claims
1. In a device for welding multiple metal materials, An anvil on which the above plurality of metal materials are placed; a horn positioned above the anvil and including a plurality of protrusions protruding toward the anvil; and A welding device comprising a processor for vibrating the horn so as to create a hole penetrating the plurality of metal materials.
2. In paragraph 1, A welding device further comprising a vision sensor for detecting the above hole.
3. In paragraph 1, The above processor, A welding device that vibrates the above-mentioned plurality of protrusions so that they draw a circular trajectory.
4. In paragraph 1, The above multiple protrusions are: A welding projection for welding the above plurality of metal materials; and, A welding device comprising a first penetrating projection that creates a hole penetrating the plurality of metal materials.
5. In paragraph 4, The protrusion length of the first through-hole protrusion is A welding device configured to be longer than the protrusion length of the above welding protrusion.
6. In paragraph 4, The above envil, A welding device including a receiving portion facing the first through-hole projection.
7. In paragraph 6, The above envil, A welding device further comprising a cutting blade formed around the above-described receiving portion.
8. In paragraph 6, The above envil, A welding device configured such that at least a portion of the plurality of metal materials is accommodated in the accommodation portion.
9. In paragraph 6, The above cutting blade, A welding device configured to be replaceable.
10. In paragraph 4, The above envil, A welding device comprising a second through-hole projection protruding toward the soul and facing the first through-hole projection.
11. In paragraph 10, The above soul, A welding device further comprising a groove formed around the first through-hole.
12. In paragraph 10, The above soul, A welding device configured to form a protrusion around a hole of the plurality of metal materials.
13. In paragraph 10, The above second penetrating projection is, A welding device configured to be replaceable.
14. A battery cell comprising a plurality of metal materials welded by a welding device according to any one of claims 1 to 13.
Citation Information
Patent Citations
Welding machine
KR1020240162850A
Method and jig for bump formation
JP1994069213A
Method for deciding normal / defective condition of welding and welding equipment
JP2007237201A
Ultrasonic machining device
JP2022059121A
Device for the ultrasonic sealing and separation of a pipe section
KR1020040104496A