Thermal print head and method for producing such a head
The thermal print head manufacturing process using laser ablation for both electrical tracks and identification zones addresses the high costs and environmental concerns of current methods, providing cost-effective and traceable thermal print heads with enhanced reliability and reduced environmental impact.
Patent Information
- Application Number
- PCT/EP2024/061170
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-05-16
- Filing Date
- 2024-04-24
- Publication Date
- 2024-11-21
AI Technical Summary
Current thermal print head manufacturing processes are costly, energy-intensive, and lack effective traceability due to the need for clean room facilities, aggressive chemicals, and complex photolithography, leading to high production costs and environmental concerns.
A thermal print head with a ceramic support and conductive layer, where the conductive layer forms both electrical tracks and an identification zone via laser ablation, allowing for unique identification and eliminating the need for clean rooms and aggressive chemicals, enabling simultaneous production of multiple heads with individual traceability.
This approach reduces production costs, simplifies the manufacturing process, enhances traceability, and allows for the use of alternative materials, such as silver, while minimizing environmental impact and operator risks.
Smart Images

Figure EP2024061170_21112024_PF_FP_ABST
Abstract
Description
Thermal print head and method of manufacturing such a head
[0001] The field of the invention is that of the design and manufacture of thermal printing devices.
[0002] More specifically, the invention relates in particular to a thermal print head and the method of manufacturing such a head.
[0003] Thermal printing involves heating dots on a heat-sensitive media.
[0004] To obtain fineness in printing the characters on the media, the dimension of the dots is of the order of 1 / 10mm on each side.
[0005] The dots are aligned on a print head and then the print heads are integrated into a printing device.
[0006] Generally, several print heads are manufactured on the same substrate, this substrate then being provided with pre-cut lines in order to separate the heads once manufactured.
[0007] Also, a print head includes a support, which is then a piece of the substrate, on which is deposited an electrically conductive layer on which the heating points are arranged.
[0008] More specifically, a print head comprises at least one ceramic support on which a conductive layer, for example gold, is deposited by screen printing and high-temperature firing (or also vacuum deposition).
[0009] Once the cooking is finished when the manufacturing is not carried out under vacuum, the conductive layer is then protected by a layer of resin.
[0010] The conductive layer is then photolithographed in order to obtain a pattern of electrical tracks allowing the electrical supply of a line of heating points on the one hand, and to connect the end of the tracks to integrated circuits controlling each of these heating points individually, on the other hand.
[0011] The heating points are thus electrically powered independently of each other via the electrical tracks. More precisely, each electrical track ends, under the line of heating points, with an electrode intended to be coupled to a heating point.
[0012] The photolithography process must be carried out in a high-cleanliness clean room (for example ISO class 5).
[0013] During the photolithography process, a photosensitive layer is deposited on the substrate, for example by ultrasonic vaporization, this photosensitive layer then being exposed to ultraviolet radiation with a mask obscuring the conductive areas to be preserved.
[0014] The assembly is then developed to remove the exposed resist, then etched, before the resist protecting the conductive areas is removed.
[0015] Other intermediate stages of resin cooking, washing and drying are inserted between the different manufacturing phases.
[0016] Because gold is difficult to oxidize, etching gold requires very aggressive acids.
[0017] However, such a manufacturing process has certain disadvantages.
[0018] First of all, the implementation of such a process requires the use of a very clean clean room (for example at least ISO class 5), i.e. a room free of dust, whose air is finely filtered, and potentially pressurized so that in the event of a leak, the air from the clean room escapes and the outside air (polluted compared to that of the clean room) cannot enter the clean room.
[0019] Such a clean room is therefore energy-intensive and costly to operate. This is explained in particular by the fact that the air renewal rate is proportional to the desired level of cleanliness, while maintaining constant humidity and temperature, but also by the fact of the numerous extractions of vapors and maintenance of the temperature of the chemical baths as well as their reprocessing, to which must finally be added the high consumption of high-purity water.
[0020] Then, as described previously, multiple printheads are usually manufactured simultaneously on the same substrate.
[0021] However, this hinders the traceability of the print heads once they are integrated into a printer. Indeed, each print head can be marked, for example, by laser. However, the marking is carried out on a rear portion of the support, that is to say the face opposite the one carrying the electrical tracks and the line of heating points.
[0022] Also, once the print head is assembled on its support in the printer, the print head marking is no longer accessible and traceability is lost.
[0023] Therefore, if a marketed head is defective, it can be difficult, even impossible, to know its traceability.
[0024] Furthermore, the use of chemistry (particularly very aggressive acids) for engraving heads requires compliance with environmental standards.
[0025] Therefore, a recycling process, which is usually expensive, must be planned, which further increases production costs. The wear of chemicals must be monitored regularly and manufacturing processes adapted accordingly to ensure consistent engraving quality.
[0026] In addition, the production line includes a plurality of manual and / or automated stations which require both significant space and qualified personnel.
[0027] Since the staff are human, the manufacturing process is therefore fallible compared to the use of robots, the latter being more reliable than a human operator for carrying out detailed tasks.
[0028] Finally, the choice of materials used for the production of the electrically conductive layer is limited by the process used.
[0029] Therefore, the materials chosen, especially gold, increase the cost of the print heads.
[0030] Changing the material then requires a readjustment of almost the entire manufacturing process, which is costly, or even impossible when the change of material is to be carried out for a small production run.
[0031] In the field of the invention, the patent document published under number JP 2021 030579 A is known. This document describes a thermal print head A1 which comprises a first substrate, likely to be ceramic, a protective layer, a conductive layer, a resistance layer, an insulation layer, an integrated driving circuit, a second substrate, ... The technique described in this document comprises, for each thermal print head, output pads which are terminals through which a current flows which actuates a heat-generating part. For control purposes, it is envisaged in this document that the output pads are accompanied by a mark, for example numeral, making it possible to identify a particular pad among others of a thermal print head.
[0032] The invention aims in particular to overcome the drawbacks of the prior art.
[0033] More specifically, the invention aims to provide a print head that is more reliable and less expensive than the prior art.
[0034] The invention also aims to provide a method for manufacturing such a print head which is simpler to implement, less expensive and less polluting than the methods of the prior art.
[0035] The invention further aims to provide such a method which makes it possible to improve the traceability of the manufactured print heads.
[0036] These objectives, as well as others which will appear subsequently, are achieved thanks to the invention which relates to a thermal print head integrating a ceramic support carrying at least one line of heating points making it possible to print characters or images on a strip of paper, each heating point being connected to an electrical track by means of electrodes terminating the electrical tracks, the support carrying an electrically conductive layer, from which the electrodes and the electrical tracks are formed, the electrically conductive layer defining an ablation surface of the conductive layer delimiting the electrodes and the electrical tracks, characterized in that the ablation surface also delimits, on the conductive layer, an identification zone of the print head, forming an identification code.
[0037] The presence of the identification zone provides unit traceability of the print head.
[0038] Indeed, in the case of a device comprising a plurality of heads, it is possible to identify a faulty head and know its origin.
[0039] This then makes it possible to trace it back to its production site, or even its production machine, to correct any manufacturing defect or failure of the manufacturing machine. The marking of the heads is then no longer just a correlation by batch, but an individual marking of each head that can include information on grouping into a manufacturing batch.
[0040] Furthermore, by being carried out directly on the ablation surface, the identification zone can be carried out simultaneously with the creation of the electrodes and electrical tracks. In other words, it is no longer necessary to turn each head over to carry out its identification marking, which reduces manufacturing time and, consequently, reduces production costs.
[0041] In addition, the position of the identification area on the conductive layer ensures continuous visibility of the printhead identification area.
[0042] Thus, during production, to detect and identify a faulty head, it is no longer necessary to mark the faulty head(s) with an additional ad hoc device which represents an additional cost and requires maintenance to ensure its operation.
[0043] It should be noted that the printhead identification area and its identification code (of the printhead) are not comparable to a series of marks used to identify components of a printhead, these series of marks being identical on all printheads of the same design.
[0044] According to an advantageous aspect, the identification zone is located in a central portion of the conductive layer.
[0045] The positioning of the identification zone in a central portion of the head, and therefore of the conductive layer, allows its continuous visibility to be maintained in order to facilitate its reading by an ad hoc tool.
[0046] Therefore, the side faces of the printing device are not likely to mask the identification zone for a reading sensor.
[0047] According to another advantageous aspect, the identification zone defines a two-dimensional bar code.
[0048] This type of two-dimensional barcode can be a quick response code, better known by its Anglo-Saxon name "QR code or Quick Response code", which offers the advantage of being easily and quickly created and used.
[0049] In fact, thanks to the rapid response code, an operator equipped with a portable computer device integrating a photo sensor and means of communication can identify the print head and know its origin.
[0050] Alternatively, this type of two-dimensional barcode can also be a vertical stripe barcode of different widths and spacings.
[0051] Furthermore, by using two-dimensional barcodes, traceability is improved and difficult to falsify since the manufacturer can integrate their manufacturer's signature.
[0052] According to another advantageous aspect, the identification code is unique for each print head.
[0053] Each print head therefore has a unique identification code, which further improves traceability.
[0054] The invention also relates to a method for manufacturing a thermal print head, comprising:- the deposition of an electrically conductive layer;- a step of ablation of the conductive layer carried out so as to form electrical tracks terminated by electrodes,- a step of depositing heating points connected to the electrical tracks via the electrodes, characterized in that the ablation step is carried out by a controlled laser device, the laser device being configured to also execute an identification zone defining an identification code of the print head, the laser device being further configured to modify the identification code for each print head.
[0055] Such a process offers many advantages.
[0056] First of all, implementing such a process does not require the use of a high-cleanliness room, i.e. a dust-free room with finely filtered air at a slight overpressure. In fact, a less controlled room, for example ISO class 7, can be used, limiting energy consumption and operating costs.
[0057] Then, thanks to the process, it is possible to manufacture several print heads simultaneously while providing each manufactured print head with a unique identification code.
[0058] Traceability is therefore increased since the different print heads can be identified independently of each other.
[0059] Therefore, individual identification of each head can be achieved without requiring the heads to be turned over to carry out their marking, which reduces the time and cost of manufacturing the print heads.
[0060] As a result, the marking can be visible in all circumstances, which guarantees long-term traceability unlike the prior art.
[0061] Then, the use of chemistry (very aggressive acids) is no longer necessary for etching the heads. Environmental standards are then less restrictive for the manufacture of print heads.
[0062] Therefore, there is no need for a special recycling process, which further reduces production costs.
[0063] Furthermore, the production line can be automated since it is not necessary to use qualified operators to limit the risks of production defects.
[0064] This makes the manufacturing process more reliable.
[0065] In addition, the choice of materials used for the production of the electrically conductive layer is wider thanks to the process used.
[0066] The gold in the conductive layer can then be replaced by another conductive material, such as silver for example.
[0067] This reduces the cost of the print head.
[0068] In addition, this process helps limit risks for operators working near the production line.
[0069] Indeed, since the use of harmful and / or toxic chemicals is no longer necessary, operators take fewer risks to their health.
[0070] Other characteristics and advantages of the invention will appear more clearly on reading the following description of a preferred embodiment of the invention, given by way of illustrative and non-limiting example, and the appended drawings described below.
[0071] This is a schematic front representation of a substrate comprising a plurality of print heads according to the invention.
[0072] This is a cross-sectional representation of a print head according to the invention.
[0073] This is a schematic front view representation of an ablated conductive layer of a print head according to the invention.
[0074] This is a schematic front view of a detail of the ablated conductive layer of a print head according to the invention.
[0075] Illustrates a substrate 100 comprising a plurality of thermal print heads 200 distributed in rows and columns.
[0076] Each print head 200 is intended to be integrated into a thermal printing device to enable thermal printing of characters on a heat-sensitive media.
[0077] According to the embodiment illustrated by the, the matrix 100 has ninety print heads 200 distributed in five columns of eighteen lines.
[0078] Of course, other sizes of substrates 100 can be provided depending on the size of the media on which the thermal printing is carried out.
[0079] With reference to the, a print head 200 according to the invention is now described.
[0080] As is particularly visible in the, the print head 200 integrates a ceramic support 210 carrying at least one line of heating points 215 making it possible to print characters or images on a medium, in particular a strip of paper. The heating points 215 take, for example, the form of heating resistors.
[0081] Each heating point 215 is connected to an electrical track 230.
[0082] More specifically, the support 210 carries an electrically conductive layer 240 (visible in FIGS. 3 and 4), from which electrodes 220 are formed which terminate the electrical tracks 230.
[0083] Still referring to the sectional view of the, these different elements are arranged as follows.
[0084] The ceramic support 210, which forms the previously mentioned substrate, is covered with a first vitrification layer 250.
[0085] The conductive layer 240, which forms the electrical tracks 230, as described below, is arranged on the first vitrification layer 250.
[0086] The conductive layer 240 is made of gold, or a gold alloy.
[0087] However, for cost reasons, gold could be replaced by silver or any other material already present on the market, thanks to the implementation of the manufacturing process described below.
[0088] The choice of material can, for example, be guided by its qualities of resistance to oxidation in air and its cost.
[0089] One or more areas of conductive material 260, for example silver, may be arranged to cover, at least partially, the conductive layer 240. These areas of conductive material then form reinforcement areas.
[0090] Finally, a second layer of vitrification 270 covers at least the heating points 215, this for their protection against abrasion due to the circulation of the media, that is to say the strip of paper on which the patterns are printed, against the print head 200.
[0091] As illustrated by the, the conductive layer 240 delimits the electrodes 220 and the electrical tracks 230.
[0092] The conductive layer 240 defines an ablation surface which is intended to be ablated to form the electrodes 220 and the electrical tracks 230.
[0093] For clarity, ablation involves removing a portion of the conductive layer 240.
[0094] Furthermore, the ablation surface also delimits, on the conductive layer, an identification zone 290 of the print head 200.
[0095] The identification zone 290 forms an identification code of the print head 200.
[0096] The identification code is then unique to each head.
[0097] The identification code advantageously takes the form of a two-dimensional bar code. For example, a two-dimensional bar code can be a quick response code or a bar code with vertical stripes of different widths and spacings.
[0098] As illustrated by Figures 3 and 4, the identification area 290 is located in a central portion 245 of the conductive layer 240.
[0099] The positioning of the identification zone 290 in the central portion 245 of the print head 200 makes it possible to maintain its continuous visibility. The identification zone 290 is also advantageously located as close as possible to the electrodes, and therefore to the heating points 215, to be more easily visible.
[0100] Therefore, side faces of a printing device in which the print head 200 is housed do not risk masking the identification zone for a reading sensor.
[0101] Obtaining a print head 200 as just described is done according to a manufacturing method comprising: - the deposition of the electrically conductive layer 240 on the ceramic support 210; - a step of ablation of the conductive layer 240, and - a deposition of the line of heating points 215 on the conductive layer.
[0102] The ablation of the conductive layer 240 is carried out so as to form at least the electrodes 220 and the electrical tracks 230.
[0103] As described above, each heating point 215 is connected to an electrical track 230 via the electrodes 220.
[0104] The ablation also makes it possible to produce the identification zone 290 of the print head 200.
[0105] As a reminder, the identification zone 290 allows the creation of a unique identification code for each print head 200 manufactured.
[0106] To enable this, the ablation step is carried out by a controlled laser device.
[0107]
[0108] The laser device is then configured to execute the identification zone 290 of the print head 200 simultaneously or sequentially with the production of the electrodes 220 and the electrical tracks 230.
[0109] The laser device is further configured to change the identification code at each print head 200.
[0110] This makes it possible to produce print heads 200, each having a unique identification code and, consequently, different from that of the other print heads 200.
[0111] The use of a laser device makes this unique identification of each print head 200 possible compared to the generally used technique which consists of using chemical solvents.
[0112] In fact, by ablation using a laser device, it is possible to change the identification code for each ablation, quickly and easily.
[0113] The generation of the identification code can be carried out automatically by a code generator or linear incrementation.
[0114] In the case of the use of chemical solvents, this unitary identification is not possible since the masks used during photolithography are common to each print head.
[0115] In other words, with a photolithography process, it would be necessary to have as many masks as there are print heads to be manufactured.
[0116] This would then lead to a significant increase in the manufacturing cost of print heads.
[0117] Furthermore, this would affect production throughput since it would be necessary to change the mask for each photolithography session, and to ensure that it is positioned correctly in order to obtain correct ablation.
[0118] The manufacturing process which has just been described therefore makes it possible to increase manufacturing rates while ensuring unitary identification of each print head 200 without recourse to photolithography tools such as masks.
[0119] In addition, this manufacturing process allows the production of 200 less expensive and less polluting print heads thanks to laser technology.
[0120] Another advantage of using the process is that making a new print head can be done simply and inexpensively.
[0121] To do this, simply modify the pattern to be reproduced by the controlled laser device in order to create the new geometry of the print head.
[0122] According to the prior art, each new head required the production of a dedicated mask, thus requiring a long production time and generating additional manufacturing costs.
[0123] Finally, this process allows studies to be carried out to validate new designs, while limiting costs.
[0124] In fact, it is enough to model the different designs to produce them quickly without having to create, for each design, specific tools which can turn out to be single-use, therefore polluting and expensive.
Claims
Thermal print head (200) incorporating a ceramic support (210) carrying at least one line of heating points (215) for printing characters or images on a paper strip, each heating point (215) being connected to an electrical track (230) via electrodes (220) terminating the electrical tracks (230), the support (210) carrying an electrically conductive layer (240), from which the electrodes (220) and the electrical tracks (230) are formed, the electrically conductive layer (240) defining an ablation surface of the conductive layer (240) delimiting the electrodes (220) and the electrical tracks (230), characterized in that the ablation surface also delimits, on the conductive layer (240), an identification zone (290) of the print head (200), forming an identification code. Print head (200) according to claim 1, characterized in that the identification zone (290) is located in a central portion of the conductive layer (240). Print head (200) according to any one of the preceding claims, characterized in that the identification zone (290) defines a two-dimensional bar code. Print head (200) according to any one of the preceding claims, characterized in that the identification code is unique for each print head (200). A method of manufacturing a thermal print head (200) according to any one of the preceding claims, comprising:- the deposition of an electrically conductive layer (240);- a step of ablation of the conductive layer (240) carried out so as to form electrical tracks (230) terminated by electrodes (220),- a step of depositing heating points (215) connected to the electrical tracks (230) via the electrodes (220), characterized in that the ablation step is carried out by a controlled laser device, the laser device being configured to also execute an identification zone (290) defining an identification code of the print head (200), the laser device being further configured to modify the identification code for each print head (200).
Citation Information
Patent Citations
Thermal head and thermal printer
CN110461615A
Driver IC for thermal printhead, and thermal printhead
CN112428696A
Thermal head and thermal printer
EP3608113A1
FR2110322A1
Thermal print head and manufacturing method of thermal print head
JP2019038184A