Apparatus and method for smelting nickel alloy with suspension roaster-electric furnace

Through the suspension roasting furnace-electric furnace smelting nickel alloy device and method, the problems of high investment and environmental pollution in the smelting process of laterite nickel ore are solved, efficient selective reduction of nickel and high-grade production of nickel alloys are achieved, and environmental protection and energy costs are reduced. .

WO2024239502A1PCT designated stage expired Publication Date: 2024-11-28SHANGHAI MILESTONE TECH CO LTD

Patent Information

Application Number
PCT/CN2023/120557
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-05-25
Filing Date
2023-09-22
Publication Date
2024-11-28

AI Technical Summary

Technical Problem

The existing laterite nickel ore smelting process has problems such as high investment costs, environmental pollution, high energy consumption and low production efficiency. In particular, the rotary kiln connection smelting process is unfriendly to the environment and has low metal conversion rate.

Method used

The equipment and methods for smelting nickel alloys using suspended roasting furnace-electric furnace, including feeding system, magnetized roasting system, discharge system and electric furnace system, and the production of nickel alloys is carried out through cyclone preheater, suspended roasting main furnace, reaction chamber and electric furnace. , cyclone preheating, multiple partitions in the reaction chamber are designed and precisely controlled reaction time, reducing agent allocation ratio and temperature to achieve selective reduction and enrichment of nickel.

Benefits of technology

The efficient selective reduction of nickel is achieved, and the nickel metallization rate reaches more than 90%, which reduces the impact of oxidation atmosphere, reduces the demand for waste gas treatment, improves production efficiency and the grade of nickel alloys, and reduces environmental protection and energy costs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN2023120557_28112024_PF_FP_ABST
    Figure CN2023120557_28112024_PF_FP_ABST
Patent Text Reader

Abstract

The present invention provides an apparatus and method for smelting a nickel alloy with a suspension roaster-electric furnace. The apparatus comprises a feeding system, a magnetizing roasting system, a discharging system, and an electric furnace system connected in sequence. The magnetizing roasting system comprises a cyclone preheater, a main suspension roaster, a cyclone separator, and a reaction chamber. A discharging port of the feeding system is connected to a feeding port of the cyclone preheater; a discharging port of the cyclone preheater is connected to an air inlet in a lower end of the main suspension roaster; a gas outlet of the cyclone preheater is connected to a feeding port of a cyclone dust remover; a discharging port of the cyclone dust remover is connected to a feeding port in an upper end of the main suspension roaster; a discharging port of the main suspension roaster is connected to a feeding port of the reaction chamber; a discharging port of the reaction chamber is connected to the electric furnace system by means of the discharging system; a gas outlet of the cyclone dust remover is connected to a dust collection system, and the dust collection system is connected to a system power source. The present invention is a production process of producing the nickel alloy with the suspension roaster-electric furnace.
Need to check novelty before this filing date? Find Prior Art

Description

Device and method for smelting nickel alloy using suspension roaster-electric furnace Technical Field

[0001] The present invention belongs to the technical field of laterite nickel ore smelting, and in particular relates to a device and method for smelting nickel alloy using a suspension roaster-electric furnace. Background Art

[0002] Laterite nickel ore is a mineral formed in tropical and subtropical regions by the weathering of nickel-bearing ultramafic rocks. To date, laterite nickel ore cannot be enriched using beneficiation methods, requiring only smelting of the raw ore, resulting in high investment and operating costs. The smelting of laterite nickel ore can be categorized into two methods: hydrometallurgy and pyrometallurgy.

[0003] Pyrometallurgical processes include blast furnace smelting and submerged arc furnace smelting. Both processes can achieve high nickel recoveries exceeding 90%. Blast furnace smelting, which includes shaft furnaces and blast furnaces, is difficult to control the reducing atmosphere during the smelting process. The shaft furnace process was first used to smelt laterite nickel ore as early as 1875. Due to high energy consumption, high pollution, and low product quality, it was eliminated globally in 1985. Due to its low investment, several Chinese factories revived this process between 2006 and 2010, using imported laterite nickel ore to produce low-nickel ferronickel to meet the huge market demand. However, increasingly stringent environmental protection requirements and energy-saving regulations have accelerated the process's elimination. Blast furnaces are primarily used to smelt pig iron. Due to their high production capacity, comprehensive supporting facilities, and low environmental impact, they have been adapted for smelting nickel-iron alloys. The rotary kiln smelting process (RKEF) can produce ferronickel with a higher nickel content, with nickel content exceeding 10%, making it an excellent raw material for stainless steel production. The rotary kiln smelting process (RKEF) is considered a mature pyrometallurgical smelting process. Existing laterite nickel ore smelting is primarily based on the RKEF process. However, the RKEF process has high requirements for the quality of the laterite ore and reducing agent, is environmentally unfriendly, and requires additional exhaust gas treatment equipment, increasing production costs. Furthermore, the RKEF process has low metal conversion rates for rotary kiln materials, requires high coal consumption, consumes a lot of electricity, and has low production efficiency.

[0004] Summary of the Invention

[0005] The technical task of the present invention is to address the deficiencies of the above existing technologies and to provide a device and method for smelting nickel alloy using a suspension roaster-electric furnace, which is a production process for producing nickel alloy using a suspension roaster-electric furnace.

[0006] The technical solution adopted by the present invention to solve its technical problems is: a device for smelting nickel alloy using a suspension roasting furnace-electric furnace, comprising a feeding system, a magnetized roasting system, a discharging system, and an electric furnace system connected in sequence; the magnetized roasting system comprises a cyclone preheater, a suspension roasting main furnace, a cyclone separator, and a reaction chamber; the discharge port of the feeding system is connected to the inlet of the cyclone preheater, the discharge port of the cyclone preheater is connected to the air inlet at the lower end of the suspension roasting main furnace, the gas outlet of the cyclone preheater is connected to the inlet of the cyclone dust collector, and the discharge port of the cyclone dust collector is connected to the inlet of the upper end of the suspension roasting main furnace; the discharge port of the suspension roasting main furnace is connected to the inlet of the reaction chamber, and the discharge port of the reaction chamber is connected to the electric furnace system through the discharge system; the gas outlet of the cyclone dust collector is connected to the dust collection system, and the dust collection system is connected to the system power source.

[0007] Furthermore, the reaction chamber is provided with a plurality of partitions, which divide the reaction chamber into a plurality of reaction chambers; different air chambers are provided at the bottom of each reaction chamber for blowing gas into the reaction chamber to fluidize the material in the reaction chamber, and the air chambers are connected to the gas supply system respectively; the reaction chamber feed port is provided at the top of the first reaction chamber, and the side wall of the partition is connected to the side wall of the reaction chamber, and the plurality of partitions make the material flow from the feed port to the discharge port according to a serpentine trajectory.

[0008] Furthermore, three partitions are provided in the reaction chamber, dividing the reaction chamber into four reaction chambers, namely loosening chamber I, fluidizing chamber I, loosening chamber II, and fluidizing chamber II; the upper part of the first partition is connected to the top of the reaction chamber, the lower part of the second partition is connected to the bottom of the reaction chamber, and the upper part of the third partition is not directly connected to the top of the reaction chamber, and an opening is provided between the third partition and the top of the reaction chamber, and a baffle is provided on the top of the reaction chamber in front of the opening.

[0009] Furthermore, the lower part of the second baffle is connected to the bottom of the reaction chamber, and the distance between the upper part and the top of the reaction chamber is x; the upper part of the third baffle is not directly connected to the top of the reaction chamber, and an opening with a height of y is provided between the upper part and the top of the reaction chamber; the height of the baffle is h, where y<x<h.

[0010] Furthermore, a metal sintered mesh is provided on the top of each air chamber, or a wind cap is provided on the top of each air chamber, and a tuyere is provided on the side of the wind cap; the gas in the air chamber enters the reaction chamber through the metal sintered mesh or the wind cap.

[0011] Furthermore, the feeding system includes a belt conveyor and an EM1 vertical mill connected in sequence; the magnetization roasting system also includes a batching machine I, and the discharge port of the batching machine I is connected to the reaction chamber; the discharge system includes an air lock valve; the electric furnace system includes an electric furnace and a batching machine II, and the discharge port of the batching machine II is connected to the electric furnace; the dust collection system includes a bag dust collector; the system power source includes a Roots blower; the smoke outlet of the bag dust collector is connected to the Roots blower, and the air outlet of the Roots blower is connected to the chimney.

[0012] Furthermore, the exhaust port of the electric furnace is connected to the suspension roasting main furnace; the exhaust port at the upper end of the suspension roasting main furnace is connected to the air inlet of the EM type vertical mill.

[0013] A method for smelting nickel alloy using the above device comprises the following steps:

[0014] Step 1: Grind the laterite nickel ore raw material and remove water to obtain laterite nickel ore powder, and send the laterite nickel ore powder to the suspension roasting system;

[0015] Step 2: The laterite nickel ore powder is preheated in a cyclone preheater and then enters the main furnace of the suspension roasting furnace for heating;

[0016] Step 3: The ore powder heated in the suspension roasting main furnace enters the reaction chamber and reacts with the reducing agent to obtain pre-reduced material;

[0017] Step 4: The pre-reduced material is introduced into an electric furnace to react and obtain a nickel alloy.

[0018] Furthermore, in step 1, the Fe / Ni mass content ratio in the laterite nickel ore is ≤9.

[0019] Furthermore, in step 1, the particle size of the mineral powder is less than or equal to 1.5 mm, and the moisture content is less than 10 wt%.

[0020] Furthermore, in step 2, the temperature of the cyclone preheater is 240°C-270°C, and the ore powder is heated to 650°C-700°C in the main furnace of the suspension roasting furnace.

[0021] Furthermore, in step 2, a burner is provided at the bottom of the main furnace of the suspension roasting furnace, which is a natural gas burner or a pulverized coal injection burner.

[0022] Furthermore, in step 3, the temperature in the reaction chamber is 700-900° C., and the reaction time is 1-3 hours.

[0023] Furthermore, in step 3, the reducing agent is a reducing gas or coal-based elemental carbon; if the reducing agent is coal-based elemental carbon, the ore powder is mixed with the reducing agent added by the batching machine in the front pipe of the reaction chamber, and then enters the reaction chamber, wherein the amount of coal-based elemental carbon added is 10%-15% of the mass of the ore powder; if reducing gas is used as the reducing agent, the reducing gas is directly introduced from the bottom of the reaction chamber into contact with the ore powder, and the reducing gas is hydrogen and / or carbon monoxide, specifically 30m3 of hydrogen is added per ton of laterite nickel ore. 3 (0.2MPa) + carbon monoxide 12m 3 (0.2MPa), the ore powder is stirred by the reducing gas and fully contacted.

[0024] Furthermore, in step 3, if the reducing agent is coal-based elemental carbon, nitrogen is blown into the bottom of the reaction chamber for material fluidization; if the reducing agent is reducing gas, nitrogen + reducing gas are blown into the bottom of the reaction chamber for material fluidization and reduction; the gas flow rate of different chambers is controlled by the gas supply system.

[0025] Furthermore, in step 4, the pre-reduced material is mixed with the flux material added by the batching machine in the front end pipe of the electric furnace.

[0026] Furthermore, the composition of the nickel alloy in step 4 is controlled by blending the laterite nickel ore and / or adding the required alloy raw materials into the electric furnace.

[0027] Furthermore, in step 4, the temperature in the electric furnace is at least 1450°C.

[0028] Compared with the prior art, the present invention has the following beneficial effects:

[0029] The suspension roasting furnace in this invention is the primary stage for achieving the selective reduction and enrichment of nickel. Before the mineral enters the suspension roasting reaction chamber, a dedicated batching machine is used to mix an appropriate amount of reducing agent (coal-based elemental carbon) with the laterite nickel ore, or a reducing gas is directly introduced into the reaction chamber to react with the laterite nickel ore. The reducing agent completely penetrates the surface of the dry mineral particles or the mineral phase lattice in the reaction chamber, and a reaction temperature of 700°C to 900°C is selected. By precisely controlling the reaction time in the reaction chamber for 1-3 hours, the nickel metallization rate in the laterite nickel ore reaches over 90%, and some iron oxides are reduced.

[0030] The present invention smelts nickel alloys, and selectively reduces nickel by accurately controlling the amount of reducing agent. Some iron oxides are not reduced. Under the high temperature conditions in the furnace, reasonable changes in the raw material composition will weaken the oxidizing atmosphere, which is beneficial to nickel reduction. If the Fe / Ni ratio is too high (the ratio is less than 9), the difficulty of selective reduction of nickel increases. For pre-reduced laterite ore, laterite ores of various grades and components can be used in combination to adjust the appropriate Fe / Ni ratio before entering the melting to complete the enrichment of nickel, so as to obtain a higher grade nickel alloy after melting. The present invention fully controls the reaction conditions of the suspension roasting reaction chamber, focusing on achieving accurate control of the reaction time, reducing agent addition ratio and temperature range of the suspension roasting reaction chamber. The ore powder discharged from the suspension roasting furnace reaction chamber is directly added to the melting by re-batch (a certain amount of flux can be added if slag making is required) to directly produce nickel alloy. BRIEF DESCRIPTION OF THE DRAWINGS

[0031] FIG1 is a schematic diagram of the structure of a suspension roasting furnace-circuit device for smelting nickel alloy;

[0032] FIG2 is a schematic diagram of the reaction chamber structure;

[0033] Among them: 1. Belt conveyor; 2. EM vertical mill grinding system; 3. Cyclone preheater; 4. Suspension roasting main furnace; 5. Reaction chamber; 6. Melting furnace; 7. Air supply system; 8. Air lock valve; 9. Batching machine I; 10. Batching machine II; 11. Cyclone dust collector; 12. Bag dust collector; 13. Roots blower; 14. Chimney; 5-1. Reaction chamber inlet; 5-2. Reaction chamber outlet; 5-3. Partition; 5-4. Baffle; 5-5. Metal sintered mesh. DETAILED DESCRIPTION

[0034] In order to make the purpose, technical solutions and advantages of the present invention more clearly understood, the present invention is further described in detail below in conjunction with the embodiments. It should be understood that the specific embodiments described herein are only used to explain the present invention and are not intended to limit the present invention.

[0035] Example 1

[0036] As shown in Figure 1, a device for smelting nickel alloy using a suspension roasting furnace-circuit smelting circuit includes a feeding system, a magnetized roasting system, a discharging system, an electric furnace system, a dust collection system, and a system power source; the feeding system includes a belt conveyor 1 and an EMI vertical mill 2; the magnetized roasting system includes a cyclone preheater 3, a suspension roasting main furnace 4, a cyclone separator 11, a reaction chamber 5, and an air supply system 7; the discharging system includes an air lock valve 8; the electric furnace system includes a melting furnace 6; the dust collection system includes a bag dust collector 12; and the system power source includes a Roots blower 13.

[0037] The belt conveyor 1 responsible for transporting laterite ore is connected to the feeding port of the EM type vertical mill 2 which receives the raw ore and crushes it. The mill discharge port is connected to the feeding port of the cyclone preheater 3 with a stainless steel pipe. The cyclone preheater 3 discharge port is connected to the air inlet (material) at the lower end of the suspension roasting main furnace 4 with a stainless steel pipe. The gas outlet of the cyclone preheater 3 is connected to the feeding port of the cyclone dust collector 11. The cyclone dust collector 11 discharge port is connected to the feeding port at the upper end of the suspension roasting main furnace 4 with a stainless steel pipe. The exhaust port at the upper end of the suspension roasting main furnace is connected to the air inlet of the EM type vertical mill 2 with a stainless steel pipe (to utilize the flue gas heat). A burner is provided at the bottom of the suspension roasting furnace main furnace, which is a natural gas burner or a pulverized coal injection burner. The discharge port of furnace 4 is connected to the feed port of reaction chamber 5 with a stainless steel pipe, the gas supply system 7 is connected to the bottom of reaction chamber 5 through a stainless steel pipe, the discharge port of reaction chamber 5 is connected to the air lock valve 8 using a white steel pipe, the discharge port of batching machine I9 is ​​connected to the reaction chamber 5 using a white steel pipe, the air lock valve 8 is connected to the feed port of melting furnace 6 using a stainless steel pipe, the batching machine II10 is connected to the feed port of melting furnace 6 using a stainless steel pipe, and the exhaust port of melting furnace 6 is connected to the suspension roasting main furnace 4; the gas outlet of cyclone dust collector 11 is connected to bag dust collector 12 through a stainless steel pipe, the flue gas outlet of bag dust collector 12 is connected to Roots blower 13, and the air outlet of Roots blower 13 is connected to chimney 14 with a pipe.

[0038] As shown in FIG2 , the reaction chamber is provided with three partitions 5-3, which divide the reaction chamber into four reaction chambers, namely loosening chamber I, fluidizing chamber I, loosening chamber II, and fluidizing chamber II; the side walls of the partitions are connected to the side walls of the reaction chamber, wherein the upper part of the first partition is connected to the top of the reaction chamber, and the lower part is 200 mm away from the bottom of the reaction chamber; the lower part of the second partition is connected to the bottom of the reaction chamber, and the upper part is 200 mm away from the top of the reaction chamber; the upper part of the third partition is not directly connected to the top of the reaction chamber, and an opening with a height of 80 mm is provided between the upper part and the top of the reaction chamber, and the lower part is 200 mm away from the bottom of the reaction chamber; a baffle 5-4 is provided on the top of the reaction chamber in front of the opening, and the height of the baffle is 216 mm. Different air chambers are provided at the bottom of each reaction chamber, and the air chambers are respectively connected to the gas supply system; the reaction chamber feed port 5-1 is provided at the top of the first reaction chamber, and the three partitions allow the material to flow from the feed port 5-1 to the discharge port 5-2 in a serpentine trajectory. In this embodiment, part of the gas flows along a serpentine trajectory with the material, and part of the gas flows above the reaction chamber. Therefore, the third upper portion is not directly connected to the top of the reaction chamber, but an opening is left. At the same time, in order to prevent the material from directly entering the next reaction chamber from the opening, a baffle is provided in front of the opening.

[0039] A metal sintered mesh 5-5 is provided on the upper portion of each gas chamber, and the gas in the gas chamber enters the reaction chamber through the metal sintered mesh or the air hood.

[0040] Example 2

[0041] The method for smelting nickel alloy based on the device described in Example 1 includes the following steps:

[0042] Step 1: Use a belt conveyor to deliver the raw materials to the suspension roasting system, grind the laterite nickel ore (Fe / Ni mass ratio <9) into a 1.5mm ore powder with a moisture content of less than 10wt% in the EM type vertical mill of the grinding system;

[0043] Step 2: The ore powder is preheated in a cyclone preheater and then enters the main furnace of the suspension roasting furnace for heating. The preheater temperature is 240°C, and the ore powder is heated to 650°C in the main furnace. The bottom of the main furnace uses hot flue gas from the electric furnace and the reaction chamber.

[0044] Step 3: The ore powder heated in the roasting main furnace enters the reaction chamber and reacts with the reducing agent to obtain pre-reduced material; the reducing agent is reducing gas, and nitrogen + reducing gas is blown into the gas chamber at the bottom of the reaction chamber for material fluidization and reduction. 30m3 of hydrogen is added per ton of laterite nickel ore. 3 (0.2MPa) + carbon monoxide 12m 3 (0.2MPa), the ore is stirred by the reducing gas to fully contact; the discharge port of the reaction chamber is provided with a gas lock valve to control the reaction chamber in an oxygen-free reducing atmosphere, and the mixture in the reaction chamber is reacted at 700℃ for 1 hour;

[0045] Step 4: The pre-reduced material is mixed with the flux material added by the batching machine in the front pipe of the melting furnace, and then enters the melting furnace to obtain nickel alloy at 1450℃-1550℃.

[0046] Example 3

[0047] The method for smelting nickel alloy based on the device described in Example 1 includes the following steps:

[0048] Step 1: Grind laterite nickel ore (Fe / Ni mass ratio <9) into -1.5 mm ore powder in an EM type vertical mill of a crushing and grinding system using a belt conveyor and a moisture content of less than 10 wt%;

[0049] Step 2: The ore powder is preheated in a cyclone preheater and then enters the main furnace of the suspension roasting furnace for heating. The preheater temperature is 270°C. The ore powder is heated to 700°C in the main furnace. The bottom of the main furnace uses hot flue gas from the electric furnace and the reaction chamber.

[0050] Step 3: The ore powder heated in the main furnace of the suspension roasting furnace is mixed with the reducing agent added by the batching machine in the pipeline at the front end of the reaction chamber, and then enters the reaction chamber, where it reacts with the reducing agent to obtain a pre-reduced material; nitrogen is blown into the air chamber at the bottom of the reaction chamber to fluidize the material. The reducing agent is coal-based elemental carbon, which accounts for 15% of the mass of the ore powder; a gas lock valve is installed at the discharge port of the reaction chamber to control the reaction chamber under anaerobic reducing conditions. The mixture in the reaction chamber reacts at 900°C for 2-3 hours;

[0051] Step 4: The pre-reduced material is mixed with the flux material added by the batching machine in the front pipe of the melting furnace, and then enters the melting furnace to obtain nickel alloy at 1450℃-1550℃.

[0052] In Examples 1 and 2, the nickel metallization rate in the laterite nickel ore reaches over 90%. In the embodiments of the present invention, a reducing agent (coal-based elemental carbon) can be added to the pre-reduced ore powder through a front-end pipeline or a reducing gas (H2, CO; H2+CO) can be introduced into the bottom of the reaction chamber to obtain a nickel alloy after smelting.

[0053] The above technical solution illustrates the technical idea of ​​the present invention and cannot be used to limit the protection scope of the present invention. Any changes and modifications made to the above technical solution based on the technical essence of the present invention without departing from the content of the technical solution of the present invention shall fall within the protection scope of the technical solution of the present invention.

Claims

1. A device for smelting nickel alloy using a suspension roasting furnace-electric furnace, characterized in that: It comprises a feeding system, a magnetized roasting system, a discharging system and an electric furnace system which are connected in sequence; the magnetized roasting system comprises a cyclone preheater, a suspension roasting main furnace, a cyclone separator and a reaction chamber; the discharging port of the feeding system is connected to the feeding port of the cyclone preheater, the discharging port of the cyclone preheater is connected to the air inlet at the lower end of the suspension roasting main furnace, the gas outlet of the cyclone preheater is connected to the feeding port of the cyclone dust collector, the discharging port of the cyclone dust collector is connected to the feeding port at the upper end of the suspension roasting main furnace; the discharging port of the suspension roasting main furnace is connected to the feeding port of the reaction chamber, the discharging port of the reaction chamber is connected to the electric furnace system through the discharging system; the gas outlet of the cyclone dust collector is connected to the dust collecting system, and the dust collecting system is connected to the system power source.

2. The device for smelting nickel alloy using a suspension roasting furnace-electric furnace according to claim 1, characterized in that: The reaction chamber is provided with a plurality of partitions, which divide the reaction chamber into a plurality of reaction chambers; a different gas chamber is provided at the bottom of each reaction chamber for blowing gas into the reaction chamber to fluidize the material in the reaction chamber, and the gas chambers are connected to the gas supply system respectively; the reaction chamber feed port is arranged at the top of the first reaction chamber, and the side wall of the partition is connected to the side wall of the reaction chamber, and the plurality of partitions enable the material to flow from the feed port to the discharge port along a serpentine trajectory.

3. The device for smelting nickel alloy using a suspension roasting furnace-electric furnace according to claim 1, characterized in that: Three partitions are arranged in the reaction chamber, dividing the reaction chamber into four reaction chambers, wherein the upper part of the first partition is connected to the top of the reaction chamber, the lower part of the second partition is connected to the bottom of the reaction chamber, the upper part of the third partition is not directly connected to the top of the reaction chamber, an opening is arranged between the third partition and the top of the reaction chamber, and a baffle is arranged on the top of the reaction chamber in front of the opening.

4. The device for smelting nickel alloy using a suspension roasting furnace-electric furnace according to claim 1, characterized in that: The feeding system comprises a belt conveyor and an EM1 vertical mill connected in sequence; the magnetization roasting system also comprises a batching machine I, and the discharge port of the batching machine I is connected to the reaction chamber; the discharge system comprises an air lock valve; the electric furnace system comprises an electric furnace and a batching machine II, and the discharge port of the batching machine II is connected to the electric furnace; the dust collection system comprises a bag filter; the power source of the system comprises a Roots blower; the smoke outlet of the bag filter is connected to the Roots blower, and the air outlet of the Roots blower is connected to the chimney; The exhaust port of the electric furnace is connected to the main suspension roasting furnace; the exhaust port at the upper end of the main suspension roasting furnace is connected to the air inlet of the EM type vertical mill.

5. A method for smelting nickel alloy based on the device according to any one of claims 1 to 4, characterized in that: The steps include: Step 1: Grind the laterite nickel ore raw material to remove water to obtain laterite nickel ore powder, and send the laterite nickel ore powder to a suspension roasting system; Step 2: The laterite nickel ore powder is preheated by a cyclone preheater and then enters the main furnace of the suspension roasting furnace for heating; Step 3: The ore powder heated in the suspension roasting main furnace enters the reaction chamber and reacts with the reducing agent to obtain a pre-reduced material; Step 4: introducing the pre-reduced material into an electric furnace to react therein to obtain a nickel alloy.

6. The method for smelting nickel alloy according to claim 5, characterized in that: In the step 1, the Fe / Ni mass content ratio in the laterite nickel ore is ≤9; the particle size of the ore powder is less than or equal to 1.5 mm, and the moisture content is less than 10 wt%.

7. The method for smelting nickel alloy according to claim 5, characterized in that: In step 2, the temperature of the cyclone preheater is 240°C-270°C, and the ore powder is heated to 650°C-700°C in the main furnace of the suspension roasting furnace; in step 4, the temperature in the electric furnace is at least 1450°C.

8. The method for smelting nickel alloy according to claim 5, characterized in that: In step 3, the temperature in the reaction chamber is 700-900° C., and the reaction time is 1-3 hours.

9. The method for smelting nickel alloy according to claim 5, characterized in that: The reducing agent is reducing gas or coal-based elemental carbon; if the reducing agent is coal-based elemental carbon, the mineral powder is mixed with the reducing agent added by the batching machine in the front pipe of the reaction chamber, and then enters the reaction chamber, wherein the amount of coal-based elemental carbon added is 10%-15% of the mass of the mineral powder; if reducing gas is used as the reducing agent, the reducing gas is hydrogen and / or carbon monoxide, and the reducing gas is directly introduced from the bottom of the reaction chamber to mix and contact with the mineral powder.

10. The method for smelting nickel alloy according to claim 5, characterized in that: The composition of the nickel alloy in step 4 is controlled by blending the laterite nickel ore and / or adding the required alloy raw materials into the electric furnace.

Citation Information

Patent Citations

  • Method and device for preparing nickel iron roasted ore by utilizing lateritic nickel ore

    CN103468930A

  • Laterite-nickel ore suspension roasting-smelting comprehensive utilization system

    CN116004976A

  • Device and method for smelting nickel alloy by using suspension roaster-electric furnace

    CN116732320A

  • Multi-stage suspension magnetizing roasting-magnetic separation system device and method for refractory iron ore

    US20180361395A1

Cited By

  • System for preparing sulfuric acid through retreatment of industrial byproduct ardealite and acid preparation process