Cavity filter system-in-package module, electronic product, and preparation method
By using substrate grooves and solder resist design in the cavity filter system-level packaging module, combined with selective plastic packing, the problems of insufficient filter bottom filling and insufficient reliability in traditional modules are solved, and the more High module reliability and efficiency.
Patent Information
- Application Number
- PCT/CN2024/095366
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-05-25
- Filing Date
- 2024-05-25
- Publication Date
- 2024-11-28
AI Technical Summary
In traditional diversity receiving modules, the filter chips are insufficiently filled due to the influence of coating, which is prone to device short circuits, and the reliability of non-filter chips is insufficient.
The system-level packaging module design of the cavity filter is used. By setting grooves on the substrate and flip the chip, a solder resist layer is formed to surround the chip, and the plastic packaging material is used to selectively fill it to ensure that the bottom of the filter is formed into a cavity and non-filter. The chip bottom is well filled to avoid short circuits and improve reliability.
The effective cavity formation at the bottom of the filter and the good filling of the non-filter chip are achieved, which avoids device short circuits and improves the reliability and efficiency of the module.
Smart Images

Figure CN2024095366_28112024_PF_FP_ABST
Abstract
Description
Cavity filter system-level packaging module, electronic product and preparation method Technical Field
[0001] The present invention relates to a cavity filter system-level packaging module, an electronic product comprising the cavity filter system-level packaging module, and a method for preparing the cavity filter system-level packaging module, belonging to the field of semiconductor packaging technology. Background Art
[0002] In wireless networks, when data needs to be transmitted, user devices (UEs) must constantly monitor the physical downlink control channel (PDC), sending and receiving data based on instructions sent by the network. This results in high UE power consumption and data transmission latency. Therefore, the 3GPP protocol introduced the discontinuous reception (DRX) energy-saving strategy in LTE systems, defined within the physical layer media access control (MAC). Consequently, the RF front end for 5G includes a diversity receive path, essentially a receive path that assists the main receiver in signal reception.
[0003] Traditional diversity receiver modules contain multiple filter chips, typically insulated with plastic encapsulation compound to create a cavity at the filter bottom. However, due to the film, the bottoms of other chips and components within the module cannot be properly filled, which can easily lead to solder shorts. Furthermore, the reliability of non-filter chips and components cannot be guaranteed due to insufficient plastic encapsulation compound.
[0004] Summary of the Invention
[0005] The primary technical problem to be solved by the present invention is to provide a cavity filter system-level packaging module.
[0006] Another technical problem to be solved by the present invention is to provide a method for preparing a cavity filter system-level packaging module.
[0007] Another technical problem to be solved by the present invention is to provide an electronic product including a cavity filter system-level packaging module.
[0008] In order to achieve the above technical objectives, the present invention adopts the following technical solutions:
[0009] According to a first aspect of an embodiment of the present invention, there is provided a cavity filter system-level packaging module, comprising a substrate, a first flip chip, a second flip chip device, a film layer, and a plastic packaging material;
[0010] The substrate is provided with a groove, the groove extending from the upper surface of the substrate toward the inside of the substrate to the layer where the second pattern layer is located or below;
[0011] The first flip chip is mounted or welded in the groove;
[0012] The second flip-chip device is mounted or soldered on the upper surface of the substrate;
[0013] A solder resist layer is disposed around the first flip chip and the second flip chip device;
[0014] The first flip chip forms a continuous film layer with the surface of the solder resist layer; the second flip chip is disconnected from the film layer on the surface of the solder resist layer.
[0015] Preferably, a gap is formed between the solder resist layer and the first flip chip, and the gap is smaller than a size of a filler in the plastic packaging material.
[0016] Preferably, a distance is formed between the second flip-chip device and the solder resist layer, and the distance is greater than the gap.
[0017] Preferably, the distance is adjusted according to the height of the bumps of the second flip-chip device, the size of the openings of the solder resist layer, and the thickness of the solder resist layer.
[0018] Preferably, the distance is greater than 20 μm.
[0019] Preferably, the cavity filter system-level packaging module further includes a colloid filling the gap.
[0020] According to a second aspect of an embodiment of the present invention, a method for preparing a cavity filter system-in-package module is provided, comprising the following steps:
[0021] S11: preparing a substrate having a groove, wherein the groove extends from the upper surface of the substrate toward the inside of the substrate to a layer where the second pattern layer is located or below;
[0022] S12: preparing a first flip chip and a second flip chip device;
[0023] S13: Connecting the bump of the first flip chip to the second conductive circuit in the groove to fix the first flip chip in the groove;
[0024] S14: soldering the second flip-chip device to the second solder pad;
[0025] S15: forming a solder resist layer on the upper surface of the substrate, wherein the solder resist layer surrounds the first flip chip and the second flip chip;
[0026] S16: Covering the solder mask layer, the first flip chip, and the second flip chip device with a film layer through a laminating process;
[0027] S17: forming a plastic sealing material on the film layer by using a plastic sealing process.
[0028] According to a third aspect of an embodiment of the present invention, a method for preparing a cavity filter system-level packaging module is provided, comprising the following steps:
[0029] S21: preparing a substrate having a groove, wherein the groove extends from the upper surface of the substrate toward the inside of the substrate to a layer where the second pattern layer is located or below;
[0030] S22: preparing a first flip chip and a second flip chip device;
[0031] S23: Connecting the bump of the first flip chip to the second conductive circuit in the groove to fix the first flip chip in the groove;
[0032] S24: soldering the second flip-chip device to the second solder pad;
[0033] S25: forming a solder resist layer on the upper surface of the substrate, wherein the solder resist layer surrounds the first flip chip and the second flip chip;
[0034] S26: forming a colloid between the first flip chip and the solder resist layer surrounding the first flip chip by using a dispensing process;
[0035] S27: forming a plastic sealing material by using a plastic sealing process.
[0036] Wherein, in the step S27, the film layer is broken by utilizing the pressure of the molding material.
[0037] According to a fourth aspect of the embodiments of the present invention, an electronic product is provided, comprising the aforementioned cavity filter system-in-package module.
[0038] Compared with the existing technology, the present invention has the following technical effects: the filter chip is soldered in a sunken cavity formed by the substrate solder mask layer and polypropylene (PP), and the non-filter chip and passive components are normally soldered on the surface layer pad of the substrate, and then selectively filled with plastic packaging material, which can ensure that a cavity can be formed at the bottom of the filter in the module, and the bottom of the non-filter chip and passive component can be well filled, avoiding solder joints and improving the reliability of the module. BRIEF DESCRIPTION OF THE DRAWINGS
[0039] FIG1 is a schematic structural diagram of a cavity filter system-in-package module in a first embodiment of the present invention;
[0040] 2A(a) to 2A(I) are schematic diagrams illustrating a process for preparing a substrate of a cavity filter system-in-package module according to a second embodiment of the present invention;
[0041] 2B(a) to 2B(m) are schematic diagrams illustrating a process for preparing a substrate of a cavity filter system-in-package module according to a second embodiment of the present invention;
[0042] FIG2C is a schematic diagram of a lamination process in a method for preparing a cavity filter system-in-package module according to a second embodiment of the present invention;
[0043] FIG2D is a schematic diagram of the plastic encapsulation process in the method for preparing a cavity filter system-level packaging module according to the second embodiment of the present invention;
[0044] FIG2E is a schematic top view of the substrate before lamination in FIG2C , after removing the first flip chip and the second flip chip;
[0045] 3A is a schematic diagram of a dispensing process in a method for preparing a cavity filter system-level packaging module according to a third embodiment of the present invention;
[0046] FIG. 3B is a schematic diagram of a plastic encapsulation process in a method for preparing a cavity filter system-level packaging module according to a third embodiment of the present invention. DETAILED DESCRIPTION
[0047] The technical content of the present invention is described in detail below with reference to the accompanying drawings and specific embodiments.
[0048] First embodiment:
[0049] As shown in Figure 1, the cavity filter system-level packaging module provided by the first embodiment of the present invention includes a substrate 1, a first flip chip 2, a second flip device 3, a film layer 6 and a plastic packaging material 7. Among them, the first flip chip 2 and the second flip device 3 are both flip chips, that is, the bumps of the chip are connected to the substrate, carrier, and circuit board with the bottom facing down. Among them, the first flip chip 2 is a cavity filter chip, such as a surface acoustic wave (SAW) filter or a bulk acoustic wave (BAW) filter chip, but this does not constitute a limitation of the present invention. Moreover, the second flip device can be a flip chip or a mounted component, and the flip chip is used as an example for explanation.
[0050] Here, substrate 1 can be any organic or inorganic substrate, such as a carrier with multiple wiring layers, a circuit board, a ceramic substrate, or an FR-4 epoxy fiberglass cloth substrate. In this embodiment, a polypropylene (PP) substrate is used as an example. A PP substrate, also known as a prepreg, typically consists of fiberglass cloth (glass fabric), resin, dicyandiamide (dicyandiamide), an accelerator, a solvent, and an additive.
[0051] In this embodiment, a three-layer substrate is used as an example for description, but those skilled in the art will appreciate that the present invention can be implemented with a substrate having three or more layers.
[0052] The substrate 1 includes a first layer pattern 101, a second layer pattern 102, a second pad 12, and a barrier layer 4. The substrate may further include a third layer pattern 103, the number of which is not limited and only needs to be greater than two layers. The first layer pattern 101 and the second pad 12 are formed on the upper surface 100 of the substrate 1 in the same process by processes such as electroplating or etching. In other words, a plurality of second pads 12 are formed with copper in an area without grooves on the front side 100 of the substrate 1 for connecting the second flip-chip device 3. The first flip chip 2 and the second flip-chip device 3 are soldered to the upper surface 100 of the substrate 1. A barrier layer 4 is formed on the upper surface 100 around the periphery of the first flip chip 2 and the second flip-chip device 3.
[0053] Furthermore, substrate 1 includes a groove 111. Groove 111 extends from solder resist layer 4 into the substrate, extending to the surface where second-layer pattern 102 is located. That is, the bottom surface of groove 111 (i.e., the surface within the substrate) is coplanar with second-layer pattern 102 (ignoring the thickness of the metal in the second-layer pattern). In other words, the depth of groove 111 is equal to the distance between first-layer pattern 101 and second-layer pattern 102. A copper second conductive trace 11 is formed on the bottom surface of groove 111 for connecting to first flip-chip 2.
[0054] The first flip chip 2 includes a chip body 21 and bumps 22. The chip body 21 has a lower surface 211 and a side surface 212. The bumps 22 are formed on the lower surface 211 of the chip body 21. The bumps 22 can be copper pillars, solder balls, etc.
[0055] The first flip chip 2 is mounted in the groove 111 so that the lower surface 211 of the chip body 21 is lower than the upper surface of the solder resist layer 4 of the substrate 1. Furthermore, the distance between the lower surface 211 and the solder resist layer 4 satisfies the following condition: the distance between the side surface 212 of the chip body 1 and the solder resist layer 4 is small enough so that large-sized filler particles contained in the molding compound cannot flow between the solder resist layer 4 and the side surface 212. As a result, the large-sized filler particles block the gap 9 between the solder resist layer 4 and the side surface 212, thereby blocking the molding compound outside the groove 111.
[0056] In this embodiment, the second conductive circuit 11 in the groove is a portion of the second layer pattern 102 , and is the second layer pattern 102 exposed in the groove.
[0057] To ensure that the distance between the solder resist layer 4 and the lower surface 211 meets the aforementioned conditions, the size of the bump 22 must match the depth of the groove 111 so that the lower surface 211 is lower than the surface of the solder resist layer 4, making it difficult for the plastic encapsulation material to flow through the gap 9.
[0058] The film layer 6 is made of a conventional thermoplastic material and is coated on the upper surfaces of the solder mask layer 4, the first flip chip 2, and the second flip chip 3 using a conventional vacuum coating process. A continuous film layer 6 is formed between the chip body 21 of the first flip chip 2 and the solder mask layer 4 surrounding the chip body 21, and the film layer 6 covers (or blocks) the gap 9, so that the plastic encapsulation material 7 cannot enter the gap 9 and cannot enter the cavity 111. By designing the film layer 6 to match the gap 9, it is ensured that the film layer 6 can seal the gap without entering the gap (let alone flowing through the gap into the cavity); it is also ensured that the film layer 6 covering the first flip chip and the solder mask layer 4 surrounding the first flip chip can withstand molding and will not be broken by the plastic encapsulation material.
[0059] However, there is no continuous film layer 6 between the second flip-chip device 3 and the solder mask 4 surrounding it. As shown in Figure 1, the film layer between the second flip-chip device 3 and the solder mask 4 nearby is broken. By designing the distance between the second flip-chip device 3 and the solder mask 4 nearby, or by changing the film layer thickness or material, the present invention can simultaneously achieve that the film layer 6 covering the first flip-chip and the solder mask 4 surrounding it remains intact, while the film layer 6 covering the second flip-chip and the solder mask 4 surrounding it is broken or partially broken.
[0060] Second embodiment:
[0061] As shown in FIG. 2A and FIG. 2B , a second embodiment of the present invention provides a method for preparing a cavity filter system-level packaging module, comprising the following steps:
[0062] S11: preparing a substrate 1 having a groove 111 , wherein the groove 111 extends from the solder resist layer 4 of the substrate 1 toward the inside of the substrate to the layer where the second layer pattern 102 is located or below.
[0063] As shown in FIG. 2A(a) to FIG. 2A(I), the substrate 1 has a groove 111 sunken into the second layer pattern 102 (in this embodiment, the second conductive line is used as an example for description), or the layer where the third layer pattern is located.
[0064] In this embodiment, the groove 111 is formed by electroplating copper on the inner substrate and then etching away the copper block. Specifically, as shown in FIG2A(a), a second conductive circuit (second layer pattern 102) made of copper is formed on the inner layer substrate (e.g., PP material); a film is then applied and exposed and developed (as shown in FIG2A(b) and FIG2A(c)) to expose the conductive circuit; a copper pillar is formed on the exposed second conductive circuit by a plating process, etc. (as shown in FIG2A(d)); a film stripping process is used to remove the residual film (as shown in FIG2A(e)); a resin film is then laminated (as shown in FIG2A(f)), and a thinning process is used to expose the copper pillar (as shown in FIG2A(g)); then a film is applied again and exposed and developed (as shown in FIG2A(h) and FIG2A(i)) to expose the copper pillar located at the groove position (groove position copper pillar); an etching process is then used (as shown in FIG2A(j)) to remove the exposed groove position copper pillar, thereby exposing the second conductive circuit in the groove below the groove position copper pillar, that is, exposing the second conductive circuit (i.e., second layer pattern 102) in the groove. The film is then stripped (as shown in FIG. 2A(k) ), and finally a first conductive circuit (ie, a first layer pattern 101 ) is formed on the resin film.
[0065] As shown in Figures 2B(a) and 2B(b), the substrate 1 has a recess 111 extending downward to the second layer pattern 102. This recess is formed by pre-pressing a copper block onto the inner layer substrate and then etching away the copper block. As shown in Figure 2B(a), a copper second conductive circuit (second layer pattern 102) is formed on the inner layer substrate (e.g., PP material). A film is then applied and exposed and developed (as shown in Figures 2B(b) and 2B(c)), exposing the second conductive circuit (102B) while leaving the second conductive circuit (102A) within the recess unexposed. Copper pillars are formed on the exposed second conductive circuit (102B) using an electroplating process (as shown in Figure 2B(d)). The remaining film is removed using a stripping process (as shown in Figure 2B(e)), exposing the entire second conductive circuit (including 102A and 102B). Afterwards, a prefabricated copper block is attached to the second conductive circuit (102A) in the groove (as shown in FIG. 2B(f)), and then a resin film is pressed (as shown in FIG. 2B(g)). The copper block is exposed by a thinning process (as shown in FIG. 2B(h)). The film is then attached and exposed and developed to expose the copper block located at the groove position (the groove position copper block) (as shown in FIG. 2B(i) and FIG. 2B(g)). The exposed groove position copper block is then removed by an etching process to expose the second conductive circuit (102A) in the groove below the groove position copper block, that is, to expose the second layer pattern 102 in the groove (as shown in FIG. 2B(k)). The film is then stripped, and finally a first copper layer (i.e., the first layer pattern 101) is formed on the resin film.
[0066] S12: Prepare a first flip chip 2 and a second flip chip device 3.
[0067] This is a routine step and will not be described in detail here.
[0068] S13 : Connecting the bump 22 of the first flip chip 2 to the second conductive trace 11 in the groove, and fixing the first flip chip 2 in the groove 111 .
[0069] As shown in FIG3 , the first flip chip 2 is fixed to the second layer of the substrate, not to the upper surface of the substrate, because the groove 111 is coplanar with the second layer pattern 102. However, the lower surface 211 of the first flip chip 2 is higher than the upper surface of the substrate (i.e., the two are not in contact).
[0070] S14 : soldering the second flip-chip device 3 to the second solder pad 12 .
[0071] As shown in FIG. 2C , since the second pad 12 is coplanar with the first layer pattern 101 , the second flip-chip device 3 is fixed on the upper surface of the substrate.
[0072] S15 : forming a solder resist layer 4 on the upper surface of the substrate 1 , wherein the solder resist layer 4 surrounds the first flip chip 2 and the second flip chip 3 .
[0073] As shown in Figures 2C and 2E , the solder resist layer 4 surrounds the projection areas of the first flip chip 2 and the second flip chip 3 on the substrate 1. Figure 2E is a schematic top view of the substrate with the first flip chip and the second flip chip removed, clearly showing that the solder resist layer 4 is outside the projection areas of the first flip chip and the second flip chip, that is, the solder resist layer 4 does not extend below the lower surface of the first flip chip.
[0074] As shown in FIG2C , a gap 9 is formed between the side surface 212 of the first flip chip and the solder resist layer 4. The size of the gap 9 (the horizontal dimension) meets the aforementioned conditions so that the gap 9 can be blocked by a large filler, thereby blocking the molding material outside the groove 111 and protecting the first flip chip 2 from contamination by the molding material.
[0075] At the same time, in the horizontal direction, the distance S between the solder resist layer 4 and the second flip-chip device 3 is greater than the size L of the gap 9, for example, S≧1.2~5L. The distance S between the second flip-chip device and the substrate can be adjusted according to the height of the bumps of the second flip-chip device, the size of the window of the solder resist layer, and the thickness of the solder resist layer. For example, the size L of the gap 9 should be controlled to be less than 15um; the distance S needs to be controlled to be above 15um. Preferably, the distance S reaches 20um, or even above 30um, to ensure that the film layer 6 can be broken during the plastic encapsulation process. Preferably, the gap L is less than or equal to the filler size to ensure that the filler does not enter the gap 9.
[0076] It is understandable that step S15 can be designed after step S12 and before step S13, that is, the solder resist layer is applied first and then the first flip chip 2 and the second flip chip 3 are fixed.
[0077] S16: Covering the solder resist layer 4, the first flip chip 2, and the second flip chip 3 with a film layer 6 through a laminating process (as shown in FIG. 2C ).
[0078] Since the gap 9 is very small and can provide sufficient support for the film layer 6, the gap 9 can be covered by the film layer 6, so that the plastic packaging material cannot enter the gap.
[0079] S17: forming a plastic sealing material 7 on the film layer 6 by using a plastic sealing process.
[0080] As shown in Figure 2D, due to the pressure caused by the molding material, the film layer 6 surrounding the second flip-chip device 3 is broken during the molding process; the film layer 6 surrounding the first flip-chip 2 remains continuous and unbroken even after being broken during the molding process. This is because the distance S between the solder resist layer 4 and the second flip-chip device 3 is greater than the size L of the gap 9 between the solder resist layer 4 and the first flip-chip 2. The larger the distance S, the longer the length of the film layer 6 not supported by the solder resist layer 4 (in a suspended state). Even under the same molding pressure, the support force exerted by the film layer 6 between the solder resist layer 4 and the second flip-chip device 3 is less than the support force exerted by the film layer 6 between the solder resist layer 4 and the first flip-chip 2. Therefore, the film layer 6 between the solder resist layer 4 and the second flip-chip device 3 is more likely to break under pressure.
[0081] Therefore, in this step, the film layer 6 shown in FIG2D is obtained, which is continuous around the first flip chip 2 and broken around the second flip chip 3. Furthermore, the molding material enters between the second flip chip 3 and the upper surface 100 of the substrate 1; however, it does not enter the groove 111 below the first flip chip.
[0082] More preferably, even if the film layer 6 surrounding the first flip chip 2 is broken, the gap 9 is small enough so that the filler is blocked in the gap 9 and the plastic material cannot enter the groove 111 .
[0083] Third embodiment:
[0084] Different from the second embodiment, this embodiment provides a method for preparing a cavity filter system-level packaging module, which adopts a dispensing process, as shown in FIG3A and FIG3B , and specifically includes the following steps:
[0085] S21: preparing a substrate 1 having a groove 111, wherein the groove 111 extends from the upper surface of the substrate 1 toward the inside of the substrate to the layer where the second layer pattern 102 is located or below;
[0086] S22: preparing a first flip chip 2 and a second flip chip 3;
[0087] S23 : Connecting the bump 22 of the first flip chip 2 to the second conductive trace 11 in the groove, and fixing the first flip chip 2 in the groove 111 .
[0088] S24 : soldering the second flip-chip device 3 to the second solder pad 12 .
[0089] S25: forming a solder resist layer 4 on the upper surface of the substrate 1, the solder resist layer 4 surrounding the first flip chip 2 and the second flip chip 3;
[0090] S26 : forming a glue 5 between the first flip chip 2 and the solder resist layer 4 surrounding the first flip chip 2 by using a glue dispensing process.
[0091] As shown in FIG3A , a dispensing process is used to allow part of the colloid to enter the gap 9 and form a colloid 5 , thereby achieving a seal between the first flip chip 2 and the solder mask layer 4 surrounding the first flip chip 2 , preventing the molding material from flowing into the groove.
[0092] S27: forming a plastic packaging material 7 by using a plastic packaging process.
[0093] As shown in FIG. 3B , since the first flip chip 2 and the surrounding solder resist layer 4 are sealed by the colloid 5 , the molding material cannot pass through the gap and enter the groove below the first flip chip 2 during the molding process.
[0094] There is no seal between the second flip-chip device 3 and the surrounding solder resist layer 4 , so the plastic encapsulation material can directly enter between the second flip-chip device 3 and the upper surface of the substrate.
[0095] The filler particles in the molding material 7 are too large to enter and fill the gap 9, and are thus isolated from the first flip chip 2; a sufficient distance S is maintained between the second flip chip 3 and other passive components and the substrate so that the molding material 7 can be filled to the bottom.
[0096] Fourth embodiment:
[0097] Different from the first embodiment, in this embodiment, a solder resist layer is formed first, and then the first flip chip 2 and the second flip chip 3 are placed; moreover, no lamination or glue dispensing is required, and only a sufficiently small gap 9 is used to prevent the plastic packaging material from entering the bottom of the first flip chip.
[0098] S31: preparing a substrate 1 having a groove 111, wherein the groove 111 extends from the upper surface of the substrate 1 to the inside of the substrate until the second layer pattern 102 is located or below, and forming a solder resist layer;
[0099] S32: preparing a first flip chip 2 and a second flip chip 3;
[0100] S33: Connecting the bump 22 of the first flip chip 2 to the second conductive line 11 in the groove, fixing the first flip chip 2 in the groove 111, so that the solder resist layer 4 surrounds the first flip chip 2 and forms a gap 9, wherein the size L of the gap 9 is smaller than the size of the filler in the molding material;
[0101] S34: soldering the second flip-chip device 3 to the second pad 12, so that the solder resist layer 4 surrounds the second flip-chip device 3 and forms a distance S, and S>L;
[0102] S35: adopting a plastic packaging process to form a plastic packaging material 7 using the plastic packaging material containing the filler.
[0103] Fifth embodiment:
[0104] A fifth embodiment of the present invention further provides an electronic product comprising the cavity filter system-in-package module, which may be a wireless communication device, a wearable electronic device, or an electric vehicle.
[0105] It should be noted that the above embodiments are merely examples, and the technical solutions of the various embodiments may be combined and are all within the scope of protection of the present invention.
[0106] In summary, the cavity filter system-level packaging module provided by the embodiment of the present invention can ensure that a cavity can be formed at the bottom of the filter in the module by soldering the filter chip in the sunken cavity formed by the substrate solder mask layer and the prepreg, and the non-filter chip and passive components are normally soldered to the surface layer pads of the substrate, and then selectively filled with plastic encapsulation material. This can avoid solder bridging and improve the reliability of the cavity filter system-level packaging module. Moreover, due to the simple process in the preparation method, the cost is low.
[0107] The above describes in detail the cavity filter system-in-package module, electronic product, and preparation method provided by the present invention. For those skilled in the art, any obvious modification without departing from the essence of the present invention would constitute an infringement of the patent rights of the present invention and would result in corresponding legal liability.
Claims
1. A cavity filter system-level packaging module, comprising a substrate, a first flip chip, a second flip chip device, a film layer and a plastic sealing material, characterized in that: The substrate is provided with a groove, and the groove extends from the upper surface of the substrate to the inside of the substrate until it reaches or below the layer where the second pattern layer is located; The first flip chip is mounted or welded in the groove; The second flip-chip device is mounted or welded on the upper surface of the substrate; A solder resist layer is disposed around the first flip chip and the second flip device; The first flip chip forms a continuous film layer with the surface of the solder resist layer; the second flip chip is disconnected from the film layer on the surface of the solder resist layer.
2. The cavity filter system-in-package module according to claim 1, wherein: A gap is formed between the solder resist layer and the first flip chip, and the gap is smaller than the size of the filler in the plastic packaging material.
3. The cavity filter system-in-package module according to claim 2, wherein: A distance is formed between the second flip-chip device and the solder resist layer, and the distance is greater than the gap.
4. The cavity filter system-in-package module according to any one of claims 1 to 3, characterized in that: The distance is adjusted according to the height of the bump of the second flip-chip device, the size of the window of the solder resist layer, and the thickness of the solder resist layer.
5. The cavity filter system-in-package module according to claim 4, wherein: The distance is greater than 30 um.
6. The cavity filter system-level packaging module according to claim 1 or 2, characterized in that Also included is a colloid that fills the gap.
7. A method for preparing a cavity filter system-level packaging module, characterized in that The following steps are involved: S11: preparing a substrate having a groove, wherein the groove extends from the upper surface of the substrate toward the inside of the substrate until the second layer pattern is located at or below the layer; S12: preparing a first flip chip and a second flip chip; S13: connecting the bump of the first flip chip to the second conductive circuit in the groove, and fixing the first flip chip in the groove; S14: soldering the second flip-chip device to the second solder pad; S15: forming a solder resist layer on the upper surface of the substrate, wherein the solder resist layer surrounds the first flip chip and the second flip chip; S16: Covering a film layer on the solder mask layer, the first flip chip, and the second flip chip device through a laminating process; S17: forming a plastic sealing material on the film layer by using a plastic sealing process.
8. The method for preparing a cavity filter system-in-package module according to claim 7, wherein: In the step S17, the film layer is broken by using the pressure of the molding material.
9. A method for preparing a cavity filter system-level packaging module, characterized in that The following steps are involved: S21: preparing a substrate having a groove, wherein the groove extends from the upper surface of the substrate toward the inside of the substrate until the second layer pattern is located at or below the layer; S22: preparing a first flip chip and a second flip chip; S23: connecting the bump of the first flip chip to the second conductive circuit in the groove, and fixing the first flip chip in the groove; S24: soldering the second flip-chip device to the second solder pad; S25: forming a solder resist layer on the upper surface of the substrate, wherein the solder resist layer surrounds the first flip chip and the second flip chip; S26: forming a colloid between the first flip chip and the solder resist layer surrounding the first flip chip by using a dispensing process; S27: forming a plastic sealing material by using a plastic sealing process.
10. A method for preparing a cavity filter system-level packaging module, characterized in that The following steps are involved: S31: preparing a substrate having a groove, wherein the groove extends from the upper surface of the substrate to the inside of the substrate until the second layer pattern is located or below, and forming a solder resist layer; S32: preparing a first flip chip and a second flip chip; S33: Connecting the bump of the first flip chip to the second conductive line in the groove, fixing the first flip chip in the groove, making the solder resist layer surround the first flip chip and form a gap, The size L of the gap is smaller than the size of the filler in the plastic packaging material; S34: soldering the second flip-chip device to the second solder pad, so that the solder resist layer surrounds the second flip-chip device and forms a distance S, and S>L; S35: adopting a plastic encapsulation process to form a plastic encapsulation material using the plastic encapsulation material having the filler.
11. An electronic product, characterized in that It comprises the cavity filter system-level packaging module as described in any one of claims 1 to 6.
Citation Information
Patent Citations
Integrated circuit package body, manufacturing method therefor and packaging substrate adopted thereby
CN106067457A
Module chip packaging structure and circuit board
CN113794461A
Module structure of cavity chip device and packaging method
CN115020400A
Surface acoustic wave filter packaging structure and packaging method thereof
CN115189668A
Cavity filter system-level packaging module, electronic product and preparation method
CN116799456A