Non-stick glass container and manufacturing method therefor

By forming silicon nitride and dielectric layers on the surface of the glass container, combined with magnetron sputtering technology, the environmental and health hazards of Teflon coating are solved, and a non-stick and easy-to-clean glass container is achieved, with high hardness , wear resistance and corrosion resistance.

WO2024244208A1PCT designated stage expired Publication Date: 2024-12-05SHENZHEN TINNO WIRELESS TECH +1
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
PCT/CN2023/118507
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-09-07
Filing Date
2023-09-13
Publication Date
2024-12-05

AI Technical Summary

Technical Problem

Existing Teflon coatings contain PFAS substances that are harmful to human health and the environment and lack effective alternatives to achieve non-stick and easy-to-clean glass containers.

Method used

A silicon nitride layer is used and a glass substrate is formed on its surface, which may include a zirconium, chromium or titanium dielectric layer, and a graphite-mixed silicon nitride composite layer is formed through magnetron sputtering technology to achieve a non-stick effect.

Benefits of technology

It achieves non-stick, easy to clean, high hardness, high wear resistance, high corrosion resistance, high temperature resistance and organic chemical coating performance, while avoiding the use of PFAS.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN2023118507_05122024_PF_FP_ABST
    Figure CN2023118507_05122024_PF_FP_ABST
Patent Text Reader

Abstract

The present invention relates to the technical field of non-stick coatings, and in particular to a non-stick glass container and a manufacturing method therefor. The non-stick glass container comprises a base material made of a glass material, and a silicon nitride layer provided on the base material, wherein the silicon nitride layer is configured to be in contact with a food material. A dielectric layer is further provided between the base material and the silicon nitride layer. According to the non-stick glass container of the present application, the base material made of the glass material is used, and then the dielectric layer or the dielectric layer and the silicon nitride layer are formed on the surface; the silicon nitride layer is stable in molecular structure, non-toxic and harmless, such that Teflon-related products can be replaced in the field of non-stick glass containers, the non-stick performance can be met, and substances containing PFAS are not used; and the non-stick glass container has the characteristics of high hardness, high wear resistance, high corrosion resistance, high-temperature resistance, easiness in cleaning, no discoloration, no organic chemical coating, lasting non-stick performance and the like.
Need to check novelty before this filing date? Find Prior Art

Description

Non-stick glass container and preparation method thereof Technical Field

[0001] The present invention relates to the technical field of non-stick coatings, and in particular to a non-stick glass container and a preparation method thereof. Background Art

[0002] Currently, the industry uses Teflon-coated non-stick pans and heated glass storage boxes and glasses, which have been greatly promoted in the global market in the past few decades. The high temperature resistance, corrosion resistance, and high efficiency of Teflon coatings have made Teflon non-stick pans enter thousands of households, with a market size of over one trillion. However, further research has found that the presence of PFAS (perfluoroalkyl substances) will cause harm to human health and the environment. The chemical composition of PFAS prevents it from being degraded in the environment for a long time. Although this characteristic makes PFAS have a high application value, it also causes them to cause long-term harm to the natural environment and the human body, including the possibility of causing cancer. Several states in the United States have introduced bans on PFAS, and Europe is about to introduce relevant regulations. The use of coatings that can replace Teflon has become an industry trend. So far, there has been no better solution to this problem that can meet the performance of non-stick pans while not using substances containing PFAS. Contents of the invention

[0003] In view of the above shortcomings of the prior art, an object of the present invention is to provide a non-stick glass container and a preparation method thereof, so as to prevent food from sticking to the container and facilitate cleaning.

[0004] To achieve the above-mentioned and other related objectives, a first aspect of an embodiment of the present application provides a non-stick glass container, comprising:

[0005] a substrate made of glass; and

[0006] a silicon nitride layer disposed on the substrate;

[0007] The silicon nitride layer is configured to be in contact with a food material.

[0008] In one embodiment of the present application, the non-stick glass container further includes a zirconium dielectric layer disposed between the substrate and the silicon nitride layer.

[0009] In one embodiment of the present application, the non-stick glass container further includes a chromium dielectric layer disposed between the substrate and the silicon nitride layer.

[0010] In one embodiment of the present application, the non-stick glass container further includes a titanium dielectric layer disposed between the substrate and the silicon nitride layer.

[0011] In an embodiment of the present application, a thickness of the zirconium dielectric layer is 0.01 um to 2 um.

[0012] In an embodiment of the present application, a thickness of the chromium dielectric layer is 0.01 um to 2 um.

[0013] In an embodiment of the present application, a thickness of the titanium dielectric layer is 0.01 um to 2 um.

[0014] In an embodiment of the present application, a thickness of the silicon nitride layer is 0.01 um to 8 um.

[0015] In one embodiment of the present application, a composite layer of the silicon nitride layer and graphite is formed on a surface of the substrate by magnetron sputtering.

[0016] A second aspect of the present invention provides a method for preparing a non-stick glass container, the method comprising:

[0017] providing a substrate made of a glass material; and

[0018] A silicon nitride layer is formed on a surface of the substrate by magnetron sputtering.

[0019] In an embodiment of the present application, a thickness of the silicon nitride layer is 0.01 um to 8 um.

[0020] In one embodiment of the present application, the substrate is detachably mounted on a holding frame in a magnetron sputtering furnace. When the silicon nitride layer is formed by magnetron sputtering, the holding frame remains stationary.

[0021] In one embodiment of the present application, the substrate is detachably mounted on a holding frame in a magnetron sputtering furnace, and the holding frame is rotated when the silicon nitride layer is formed by magnetron sputtering.

[0022] A third aspect of the present invention provides a method for preparing a non-stick glass container, the method comprising:

[0023] Providing a substrate made of a glass material;

[0024] forming a dielectric layer on a surface of the substrate by magnetron sputtering; and

[0025] A silicon nitride layer is formed on a surface of the dielectric layer by magnetron sputtering.

[0026] In an embodiment of the present application, the dielectric layer is a zirconium dielectric layer.

[0027] In an embodiment of the present application, a thickness of the zirconium dielectric layer is 0.01 um to 2 um.

[0028] In an embodiment of the present application, the dielectric layer is a chromium dielectric layer.

[0029] In an embodiment of the present application, a thickness of the chromium dielectric layer is 0.01 um to 2 um.

[0030] In one embodiment of the present application, the dielectric layer is a titanium dielectric layer.

[0031] In an embodiment of the present application, a thickness of the titanium dielectric layer is 0.01 um to 2 um.

[0032] In an embodiment of the present application, a thickness of the silicon nitride layer is 0.01 um to 8 um.

[0033] In one embodiment of the present application, the silicon nitride layer is mixed with graphite to form a composite layer disposed on the surface of the dielectric layer, wherein the ratio of silicon nitride is 95wt% to 85wt% and the ratio of graphite is 5wt% to 15wt%.

[0034] In one embodiment of the present application, the substrate is detachably mounted on a holding frame in a magnetron sputtering furnace. When the dielectric layer and the silicon nitride layer are formed by magnetron sputtering, the holding frame remains stationary.

[0035] In one embodiment of the present application, the substrate is detachably mounted on a holding frame in a magnetron sputtering furnace, and the holding frame rotates when the dielectric layer and the silicon nitride layer are formed by magnetron sputtering.

[0036] As described above, the non-stick glass container and preparation method provided in the embodiments of the present application use a glass material as a substrate, and then form a dielectric layer or a dielectric layer and a silicon nitride layer on the surface. The silicon nitride layer has a stable molecular structure and is non-toxic and harmless. It can replace Teflon-related products in the field of non-stick glass containers. It can not only meet the non-stick performance but also does not use substances containing PFAS. It has the characteristics of high hardness, high wear resistance, high corrosion resistance, high temperature resistance, easy cleaning, no discoloration, no organic chemical coating, and long-lasting non-stick. BRIEF DESCRIPTION OF THE DRAWINGS

[0037] In order to more clearly illustrate the technical solutions in the embodiments of the present application, the following briefly introduces the drawings required for use in the description of the embodiments. Obviously, the drawings described below are only some embodiments of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without any creative work.

[0038] FIG1 is a schematic cross-sectional view of a partial structure of a first embodiment of the non-stick glass container of the present application;

[0039] FIG2 is a schematic cross-sectional view of a partial structure of a second embodiment of the non-stick glass container of the present application;

[0040] FIG2-1 is a schematic cross-sectional view of a partial structure of a third embodiment of the non-stick glass container of the present application;

[0041] FIG3 is a schematic flow chart of a first embodiment of a method for preparing a non-stick glass container according to the present invention;

[0042] FIG3-1 is a schematic flow chart of a third embodiment of a method for preparing a non-stick glass container according to the present application;

[0043] FIG4 is a schematic flow chart of a second embodiment of a method for preparing a non-stick glass container according to the present invention;

[0044] FIG4-1 is a schematic flow chart of a third embodiment of a method for preparing a non-stick glass container according to the present application;

[0045] FIG5 is a schematic structural diagram of a magnetron sputtering furnace used in the preparation method according to an embodiment of the present application, wherein the holding frame is stationary; and

[0046] FIG6 is a schematic structural diagram of a magnetron sputtering furnace used in the preparation method in an embodiment of the present application, wherein the holding frame rotates.

[0047] The numbers in the figure represent: 100, non-stick glass container; 110, substrate; 120, dielectric layer; 130, silicon nitride layer; 200, magnetron sputtering furnace; 210, holding rack; 220, target material; S100, method for preparing non-stick glass container; S101~S102, steps; S200, method for preparing non-stick glass container; S201~S203, steps. DETAILED DESCRIPTION

[0048] The following will be combined with the drawings in the embodiments of this application to clearly and completely describe the technical solutions in the embodiments of this application. Obviously, the embodiments described are part of the embodiments of this application, not all of them. Based on the embodiments in this application, all other embodiments obtained by ordinary technicians in this field without making creative efforts are within the scope of protection of this application.

[0049] It should be noted that the structures, proportions, sizes, etc. illustrated in the drawings of this specification are only used to match the contents disclosed in the specification for people familiar with this technology to understand and read, and are not used to limit the limiting conditions for the implementation of the present invention. Therefore, they have no substantial technical significance. Any modification of the structure, change in the proportional relationship or adjustment of the size should still fall within the scope of the technical content disclosed by the present invention without affecting the efficacy and purpose that can be achieved by the present invention. At the same time, terms such as "upper", "lower", "left", "right", "middle", "first", "second", etc. quoted in this specification are only for the convenience of description and are not used to limit the scope of the implementation of the present invention. Changes or adjustments in their relative relationships should also be regarded as the scope of the implementation of the present invention without substantially changing the technical content.

[0050] The embodiment of the present application first provides a non-stick glass container, which can be a glass food storage box, a glass cup, etc., which is not specifically limited here. The present application uses a glass cup as an example for illustration.

[0051] Please refer to Figure 1, which is a schematic cross-sectional view of a partial structure of a first embodiment of a non-stick glass container of the present invention. In this embodiment, the non-stick glass container 100 includes a substrate 110 and a silicon nitride (Si3N4) layer 130. The substrate 110 of the non-stick glass container 100 of the present invention is made of glass. In some embodiments, the silicon nitride layer 130 is disposed on the substrate 110 and is configured to contact a food. In some embodiments, the silicon nitride layer has a thickness of 0.01 μm to 8 μm.

[0052] Please refer to Figure 2, which is a schematic cross-sectional view of a partial structure of a second embodiment of the non-stick glass container of the present application. In this embodiment, the non-stick glass container 100 includes a substrate 110, a dielectric layer 120, and a silicon nitride layer 130. In some embodiments, the dielectric layer 120 is a zirconium dielectric layer with a thickness of 0.01 to 2 μm. In other embodiments, the dielectric layer 120 is a chromium dielectric layer with a thickness of 0.01 to 2 μm. In other embodiments, the dielectric layer 120 is a titanium dielectric layer with a thickness of 0.01 to 2 μm. In some embodiments, the silicon nitride layer has a thickness of 0.01 to 8 μm.

[0053] As described above, the non-stick glass container provided in the embodiment of the present application adopts a glass material as a substrate, and then forms a dielectric layer or a dielectric layer and a silicon nitride layer on the surface. The silicon nitride layer has a stable molecular structure and is non-toxic and harmless. It can replace Teflon-related products in the field of non-stick glass containers. It can not only meet the non-stick performance but also does not use substances containing PFAS. It has the characteristics of high hardness, high wear resistance, high corrosion resistance, high temperature resistance, easy cleaning, no discoloration, no organic chemical coating, and long-lasting non-stick.

[0054] Please refer to Figure 2-1, which is a schematic cross-sectional view of the partial structure of the third embodiment of the non-stick glass container of the present application. In order to increase hardness and wear resistance, the silicon nitride layer 130 is mixed with graphite to form a composite layer 130a disposed on the surface of the dielectric layer, wherein the ratio of silicon nitride is 95wt% to 85wt% and the ratio of graphite is 5wt% to 15wt%.

[0055] In addition, the embodiment of the present application further provides a method S100 for preparing a non-stick glass container. Please refer to FIG3 , which is a flow chart of the first embodiment of the method for preparing a non-stick glass container of the present application. The preparation method S100 includes but is not limited to the following steps.

[0056] In step S101, a substrate 110 is provided. The substrate 110 is made of glass. The shape of the substrate 110 can be any pot or any food storage box, and is not specifically limited here.

[0057] In step S102 , a silicon nitride layer 130 is formed on a surface of the substrate 110 by magnetron sputtering.

[0058] In step S102, a silicon nitride layer 130 may be formed on a surface of the substrate 110 using a magnetron sputtering furnace 200 and a target (silicon nitride) 220. Referring to FIG5 , FIG5 is a schematic diagram of the structure of a magnetron sputtering furnace used in the preparation method according to an embodiment of the present application, wherein the substrate 110 is detachably mounted on a holder 210 within the magnetron sputtering furnace 200. When the silicon nitride layer 130 is formed by magnetron sputtering, the holder 210 remains stationary. Alternatively, referring to FIG6 , FIG6 is a schematic diagram of the structure of a magnetron sputtering furnace used in the preparation method according to an embodiment of the present application, wherein the substrate 110 is detachably mounted on a holder 210 within the magnetron sputtering furnace 200. When the silicon nitride layer 130 is formed by magnetron sputtering, the holder 210 rotates so that the silicon nitride layer 130 is uniformly formed on the surface of the substrate 110.

[0059] The following will introduce a specific embodiment of the first embodiment of the method S100 for preparing a non-stick glass container as shown in FIG. 3 .

[0060] For example, substrate 110 is made of glass. The glass substrate 110 is first mechanically polished, then sandblasted and blown with compressed air to remove any dust from the surface. The substrate is then placed in a magnetron sputtering furnace 200. Thin film deposition is performed using a magnetron sputtering target (e.g., silicon nitride) (i.e., target material 220) in the magnetron sputtering furnace 200. After the film reaches a thickness of 0.01 to 8 μm, the substrate is removed, completing the thin film deposition. Specific data is shown in the table below.

[0061]

[0062] 3-1 , in order to increase hardness and wear resistance, a step S102a is used to mix the silicon nitride layer 130 with graphite to form a composite layer 130a, wherein the ratio of silicon nitride is 95wt% to 85wt% and the ratio of graphite is 5wt% to 15wt%.

[0063] In addition, the embodiment of the present application further provides a method S200 for preparing a non-stick glass container. Please refer to FIG4 , which is a flow chart of a second embodiment of the method for preparing a non-stick glass container of the present application. The preparation method S200 includes but is not limited to the following steps.

[0064] In step S201, a substrate 110 is provided. The substrate 110 is made of glass. The shape of the substrate 110 can be any pot or any food storage box, and is not specifically limited here.

[0065] In step S202 , a dielectric layer 120 is formed on a surface of the substrate 110 by magnetron sputtering.

[0066] In step S202, a magnetron sputtering furnace 200 and a target material (zirconium (Zr), chromium (Cr), or titanium (Ti)) may be used to form a dielectric layer 120 on a surface of the substrate 110. Step S202 is similar to the aforementioned step S102, with the only difference being the target material. The following description uses step S102 as an example, and the dielectric layer 102 is not labeled or exposed in Figures 5 and 6. The dielectric layer 120 may be a zirconium dielectric layer (target material is zirconium), a chromium dielectric layer (target material is chromium), or a titanium dielectric layer (target material is titanium). Please refer to Figure 5, which is a schematic diagram of the structure of the magnetron sputtering furnace used in the preparation method of the embodiment of the present application. The substrate 110 is detachably mounted on a holder 210 within the magnetron sputtering furnace 200. The holder 210 remains stationary while the dielectric layer 120 is formed by magnetron sputtering (not shown in Figure 5, but refer to Figure 2). Alternatively, please refer to Figure 6, which is a structural schematic diagram of the magnetron sputtering furnace used in the preparation method in an embodiment of the present application, wherein the substrate 110 is detachably arranged on a holding frame 210 in a magnetron sputtering furnace 200. When the dielectric layer 120 (not shown in Figure 6, refer to Figure 2) is formed by magnetron sputtering, the holding frame 210 is rotated so that the dielectric layer 120 (not shown in Figure 6, refer to Figure 2) is evenly formed on the surface of the substrate 110.

[0067] In step S203 , a silicon nitride layer 130 is formed on a surface of the dielectric layer 120 by magnetron sputtering.

[0068] In step S203, a silicon nitride layer 130 may be formed on a surface of the dielectric layer 120 using a magnetron sputtering furnace 200 and a target material 220 (silicon nitride). Referring to FIG5 , FIG5 is a schematic diagram of the structure of a magnetron sputtering furnace used in the preparation method according to an embodiment of the present application. In the magnetron sputtering furnace 200, a substrate 110 including the dielectric layer 120 (not shown in FIG5 , but refer to FIG2 ) is detachably mounted on a holder 210. The holder 210 remains stationary during the formation of the silicon nitride layer 130 by magnetron sputtering. Alternatively, please refer to Figure 6, which is a schematic diagram of the structure of a magnetron sputtering furnace used in the preparation method according to an embodiment of the present application. Here, a substrate 110 including a dielectric layer 120 (not shown in Figure 6, refer to Figure 2) is detachably mounted on a holder 210 within a magnetron sputtering furnace 200. During the formation of the silicon nitride layer 130 by magnetron sputtering, the holder 210 rotates to ensure that the silicon nitride layer 130 is evenly formed on the surface of the dielectric layer 120. A pump system is also provided for vacuuming.

[0069] The following will introduce a specific embodiment of the first embodiment of the method S200 for preparing a non-stick glass container shown in FIG. 4 .

[0070] For example, substrate 110 is made of glass. The glass substrate 110 is first mechanically polished, then sandblasted and blown with compressed air to remove surface dust. The substrate is then placed in a magnetron sputtering furnace 200. Thin film deposition is performed using an arc target (e.g., zirconium, chromium, or titanium) and a magnetron sputtering target 220 (e.g., silicon) in the magnetron sputtering furnace 200. After the film reaches a thickness of 0.01 to 8 μm, the substrate is removed, completing the film deposition process. Specific data is shown in the table below.

[0071]

[0072] In addition, please refer to FIG. 4-1 . In order to increase hardness and wear resistance, a step S203 a is used to mix the silicon nitride layer 130 with graphite to form a composite layer 130 a disposed on the surface of the dielectric layer, wherein the ratio of silicon nitride is 95 wt % to 85 wt % and the ratio of graphite is 5 wt % to 15 wt %.

[0073] According to experiments, after the above processing, the surface covering material (dielectric layer and silicon nitride layer) of the non-stick glass container has the properties of high hardness, high wear resistance, high corrosion resistance, high temperature resistance, easy cleaning, no discoloration, no organic chemical coating, and long-lasting non-stick.

[0074] The preparation method in the embodiment of the present application adopts a glass material as a substrate, and then forms a dielectric layer or a dielectric layer and a silicon nitride layer on the surface. The silicon nitride layer has a stable molecular structure and is non-toxic and harmless. It can replace Teflon-related products in the field of non-stick glass containers. It can not only meet the non-stick performance but also does not use substances containing PFAS. It has the characteristics of high hardness, high wear resistance, high corrosion resistance, high temperature resistance, easy cleaning, no discoloration, no organic chemical coating, and long-lasting non-stick.

[0075] The above-described embodiments are only used to illustrate the technical solutions of the present application, rather than to limit them. Although the present application has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or make equivalent replacements for some of the technical features therein. These modifications or replacements do not deviate from the essence of the corresponding technical solutions from the spirit and scope of the technical solutions of the embodiments of the present application, and should all be included in the scope of protection of the present application. All equivalent modifications or changes made by those with ordinary knowledge in the relevant technical field without departing from the spirit and technical ideas disclosed by the present invention should still be covered by the claims of the present invention.

Claims

1. A non-stick glass container, It is characterized in that include: A substrate made of a glass material; as well as a silicon nitride layer disposed on the substrate; The silicon nitride layer is configured to contact with a food material.

2. A non-stick glass container according to claim 1, It is characterized in that The non-stick glass container further comprises a zirconium dielectric layer disposed between the substrate and the silicon nitride layer.

3. A non-stick glass container according to claim 1, It is characterized in that The non-stick glass container further comprises a chromium dielectric layer disposed between the substrate and the silicon nitride layer.

4. The non-stick glass container according to claim 1, It is characterized in that The non-stick glass container further comprises a titanium dielectric layer disposed between the substrate and the silicon nitride layer.

5. A non-stick glass container according to claim 2, It is characterized in that The zirconium dielectric layer has a thickness of 0.01 um to 2 um.

6. A non-stick glass container according to claim 3, It is characterized in that The thickness of the chromium dielectric layer is 0.01um to 2um.

7. A non-stick glass container according to claim 4, It is characterized in that The thickness of the titanium dielectric layer is 0.01 um to 2 um.

8. The non-stick glass container according to claim 1, It is characterized in that The silicon nitride layer has a thickness of 0.01 um to 8 um.

9. The non-stick glass container according to claim 1, It is characterized in that The silicon nitride layer is mixed with graphite to form a composite layer, wherein the ratio of the silicon nitride layer is 95wt% to 85wt% and the ratio of the graphite is 5wt% to 15wt%.

10. A method for preparing a non-stick glass container, It is characterized in that The preparation method comprises: Providing a substrate made of a glass material; and A silicon nitride layer is formed on a surface of the substrate by magnetron sputtering.

11. A method for preparing a non-stick glass container according to claim 10, It is characterized in that The silicon nitride layer has a thickness of 0.01 um to 8 um.

12. The method for preparing a non-stick glass container according to claim 10, It is characterized in that The substrate is detachably arranged on a holding frame in a magnetron sputtering furnace. When the silicon nitride layer is formed by magnetron sputtering, the holding frame remains stationary.

13. The method for preparing a non-stick glass container according to claim 10, It is characterized in that The substrate is detachably arranged on a holding frame in a magnetron sputtering furnace. When the silicon nitride layer is formed by magnetron sputtering, the holding frame is rotated.

14. A method for preparing a non-stick glass container, It is characterized in that The preparation method comprises: Providing a substrate made of a glass material; forming a dielectric layer on a surface of the substrate by magnetron sputtering; and A silicon nitride layer is formed on a surface of the dielectric layer by magnetron sputtering.

15. A method for preparing a non-stick glass container according to claim 14, It is characterized in that The dielectric layer is a zirconium dielectric layer, and a thickness of the zirconium dielectric layer is 0.01 um to 2 um.

16. The method for preparing a non-stick glass container according to claim 14, It is characterized in that The dielectric layer is a chromium dielectric layer, and a thickness of the chromium dielectric layer is 0.01 um to 2 um.

17. The method for preparing a non-stick glass container according to claim 14, It is characterized in that The dielectric layer is a titanium dielectric layer, and a thickness of the titanium dielectric layer is 0.01 um to 2 um.

18. The method for preparing a non-stick glass container according to claim 14, It is characterized in that The silicon nitride layer has a thickness of 0.01 um to 8 um.

19. The method for preparing a non-stick glass container according to claim 14, It is characterized in that The substrate is detachably arranged on a holding frame in a magnetron sputtering furnace. When the dielectric layer and the silicon nitride layer are formed by magnetron sputtering, the holding frame remains stationary.

20. The method for preparing a non-stick glass container according to claim 14, It is characterized in that The substrate is detachably arranged on a holding frame in a magnetron sputtering furnace, and the holding frame is rotated when the dielectric layer is formed by magnetron sputtering and the silicon nitride layer is formed by magnetron sputtering.

21. A method for preparing non-stick glass according to claim 14, It is characterized in that The preparation method comprises: Providing a substrate made of a glass material; forming a dielectric layer on a surface of the substrate by magnetron sputtering; and A composite layer of the silicon nitride layer and a graphite mixture is formed on a surface of the dielectric layer by magnetron sputtering.

Citation Information

Patent Citations

  • Plain copper foodware and metal articles with durable and tarnish free multilayer ceramic coating and method of making

    CN102378830A

  • Cooking device hacing a cooking surface comprising a non-oxide or at least partially non-oxide ceramic non-stick coating, and kitchen item or electrical cooking appliance comprising such a cooking device

    CN104768435A

  • Iron-shovel-resistant non-sticking cooker and manufacturing method thereof

    CN109984618A

  • Cooker with pure inorganic non-stick coating and manufacturing method thereof

    CN115474829A

  • Nonstick Utensil and Manufacturing Method Thereof

    US20200229635A1