Semiconductor device and MRAM

By using alloy metal layers composed of multiple metals in semiconductor devices, the problem of MRAM degradation after high-temperature annealing is solved, the perpendicular magnetic anisotropy and synchronous antiferromagnetic coupling strength are improved, and the high-temperature data retention ability of the device is ensured and reliability.

WO2024244997A1PCT designated stage expired Publication Date: 2024-12-05ZHEJIANG HIKSTOR TECHOGY CO LTD
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
PCT/CN2024/093748
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-05-31
Filing Date
2024-05-16
Publication Date
2024-12-05

AI Technical Summary

Technical Problem

After high-temperature annealing of existing MRAM, the perpendicular magnetic anisotropy and synchronous antiferromagnetic coupling strength performance will seriously degrade, resulting in poor device reliability.

Method used

Design of semiconductor devices using an alloy metal layer composed of a variety of metals. The metal layer of the second pinning layer is located between the first pinning layer and the isolation layer. The metal layer material includes transition metal and alkaline earth metal to ensure vertical after high temperature annealing. Magnetic anisotropy and stability of synchronous antiferromagnetic coupling strength.

Benefits of technology

It improves the data retention capability and reliability of semiconductor devices after high-temperature annealing, avoids the performance degradation problems caused by a single metal layer, and ensures the high-temperature data retention capability and performance stability of the device.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN2024093748_05122024_PF_FP_ABST
    Figure CN2024093748_05122024_PF_FP_ABST
Patent Text Reader

Abstract

A semiconductor device and an MRAM. The semiconductor device comprises a seed layer, a first pin layer and a second pin layer, wherein the first pin layer is located on the surface of the seed layer; and the second pin layer is located on the side of the first pin layer that is away from the seed layer, and the second pin layer comprises a metal layer and an isolation layer which are arranged in a stacked manner, the metal layer being located on the surface of the isolation layer that is close to the first pin layer, and the metal layer is made of an alloy formed by a plurality of metals. The second pin layer comprises the metal layer, and the metal layer is made of an alloy formed by a plurality of metals, and therefore the metal layer has a relatively good thermal stability, such that it is ensured that a device has relatively good vertical magnetic anisotropy and synchronous anti-ferromagnetic coupling strength after the metal layer is subjected to high-temperature annealing, thereby preventing the problem in the prior art of the performance deteriorating after high-temperature annealing due to the second pin layer being made of a single metal, and solving the problem in the prior art of the performance of an MRAM deteriorating after high-temperature annealing, thus ensuring the relatively good performance of a semiconductor device.
Need to check novelty before this filing date? Find Prior Art

Description

Semiconductor devices and MRAM Technical Field

[0001] The present disclosure relates to the field of semiconductor memory, and in particular to a semiconductor device and an MRAM. Background Art

[0002] Currently, the MTJ (Magnetic Tunnel Junction) structure, the main structure of MRAM (Magnetoresistive Random Access Memory), will experience severe degradation in properties such as perpendicular magnetic anisotropy and synchronous antiferromagnetic coupling strength after high-temperature annealing, resulting in poor reliability of MRAM devices.

[0003] Summary of the Invention

[0004] The main purpose of the present disclosure is to provide a semiconductor device and an MRAM to solve the problem in the prior art that the performance of the MRAM deteriorates after high-temperature annealing.

[0005] In order to achieve the above-mentioned purpose, according to one aspect of the present disclosure, a semiconductor device is provided, which includes a seed layer, a first pinning layer and a second pinning layer, wherein the first pinning layer is located on the surface of the seed layer; the second pinning layer is located on the side of the first pinning layer away from the seed layer, the second pinning layer includes a stacked metal layer and an isolation layer, the metal layer is located on the surface of the isolation layer close to the first pinning layer, and the metal layer includes an alloy composed of multiple metals.

[0006] Optionally, the material of the metal layer includes a first metal and a second metal, wherein the first metal includes a transition metal; and the second metal includes a transition metal and / or an alkaline earth metal.

[0007] Optionally, the first metal includes one of Co, Fe, CoFe and CoFeB, and the second metal includes at least one of Hf, Zr, Ta, Mo, W, Cr, Ti, Rh, Nb and Mg.

[0008] Optionally, the second metal accounts for 5%-50% of the metal layer.

[0009] Optionally, the semiconductor device further includes a coupling layer, wherein the coupling layer is located between the first pinning layer and the second pinning layer, and the coupling layer is in contact with the first pinning layer and the metal layer respectively.

[0010] Optionally, the material of the coupling layer includes Ir.

[0011] Optionally, the semiconductor device further includes a reference layer, a first tunneling layer, a free layer, a second tunneling layer and a covering layer, wherein the reference layer is located on a surface of the second pinning layer away from the first pinning layer, and the reference layer is in contact with the isolation layer; the first tunneling layer is located on a surface of the reference layer away from the second pinning layer; the free layer is located on a surface of the first tunneling layer away from the reference layer; the second tunneling layer is located on a surface of the free layer away from the first tunneling layer; and the covering layer is located on a surface of the second tunneling layer away from the free layer.

[0012] Optionally, the material of the isolation layer includes at least one of Ta, W and Mo.

[0013] Optionally, the thickness of the metal layer is in the range of 3 angstroms to 15 angstroms.

[0014] According to another aspect of the present disclosure, an MRAM is provided, comprising any one of the semiconductor devices described above.

[0015] Using the technical solution of the present disclosure, the semiconductor device includes a seed layer, a first pinning layer, and a second pinning layer, wherein the first pinning layer is located on the surface of the seed layer; the second pinning layer is located on a side of the first pinning layer away from the seed layer; the second pinning layer includes a stacked metal layer and an isolation layer, the metal layer is located on the surface of the isolation layer near the first pinning layer, and the metal layer includes an alloy composed of multiple metals. Compared to the problem of poor performance of MRAM in the prior art after high-temperature annealing, the semiconductor device of the present disclosure, because the second pinning layer includes the metal layer and the metal layer is an alloy composed of multiple metals, has higher thermal stability, ensuring that the perpendicular magnetic anisotropy and synchronous antiferromagnetic coupling strength of the device are better after high-temperature annealing. This avoids the problem of poor performance of MRAM in the prior art due to the relatively single metal in the second pinning layer, solves the problem of poor performance of MRAM in the prior art after high-temperature annealing, and ensures better performance of the semiconductor device. BRIEF DESCRIPTION OF THE DRAWINGS

[0016] The accompanying drawings, which constitute part of the present disclosure, are intended to provide a further understanding of the present disclosure. The exemplary embodiments of the present disclosure and their descriptions are intended to explain the present disclosure and do not constitute an improper limitation of the present disclosure. In the accompanying drawings:

[0017] FIG1 is a schematic structural diagram of a semiconductor device according to an embodiment of the present disclosure;

[0018] FIG2 is a schematic diagram showing a performance test of an MRAM device after high-temperature annealing in the prior art;

[0019] FIG3 is a schematic diagram showing a performance test of a semiconductor device after high-temperature annealing according to an embodiment of the present disclosure.

[0020] The above drawings include the following reference numerals: 10, seed layer; 20, first pinned layer; 30, second pinned layer; 40, coupling layer; 50, reference layer; 60, first tunneling layer; 70, free layer; 80, second tunneling layer; 90, covering layer; 301, metal layer; 302, isolation layer. DETAILED DESCRIPTION

[0021] It should be noted that the following detailed descriptions are illustrative and intended to provide further explanation of the present disclosure. Unless otherwise specified, all technical and scientific terms used herein have the same meaning as commonly understood by those skilled in the art to which the present disclosure belongs.

[0022] It should be noted that the terms used herein are only for describing specific embodiments and are not intended to limit the exemplary embodiments according to the present disclosure. As used herein, unless the context clearly indicates otherwise, the singular form is intended to include the plural form. In addition, it should be understood that when the terms "comprise" and / or "include" are used in this specification, they indicate the presence of features, steps, operations, devices, components and / or combinations thereof.

[0023] It should be understood that when an element (such as a layer, film, region, or substrate) is described as being "on" another element, the element may be directly on the other element or intervening elements may be present. Moreover, in the specification and claims, when it is described that an element is "connected to" another element, the element may be "directly connected to" the other element or "connected to" the other element through a third element.

[0024] As introduced in the background technology, the prior art MRAM has the problem of poor performance after high-temperature annealing. To solve the above problem, embodiments of the present disclosure provide a semiconductor device and an MRAM.

[0025] The technical solutions in the embodiments of the present disclosure will be described clearly and completely below with reference to the accompanying drawings in the embodiments of the present disclosure.

[0026] According to an embodiment of the present disclosure, a semiconductor device is provided, as shown in Figure 1, the semiconductor device includes a seed layer 10, a first pinning layer 20 and a second pinning layer 30, wherein the first pinning layer 20 is located on the surface of the seed layer 10; the second pinning layer 30 is located on the side of the first pinning layer 20 away from the seed layer 10, and the second pinning layer 30 includes a stacked metal layer 301 and an isolation layer 302, the metal layer 301 is located on the surface of the isolation layer 302 close to the first pinning layer 20, and the metal layer 301 includes an alloy composed of multiple metals.

[0027] The semiconductor device includes a seed layer, a first pinning layer, and a second pinning layer, wherein the first pinning layer is located on a surface of the seed layer; the second pinning layer is located on a side of the first pinning layer away from the seed layer; the second pinning layer includes a stacked metal layer and an isolation layer, the metal layer is located on a surface of the isolation layer near the first pinning layer, and the metal layer includes an alloy composed of multiple metals. Compared to the problem of poor performance of MRAM in the prior art after high-temperature annealing, the semiconductor device disclosed herein, because the second pinning layer includes the metal layer and the metal layer is an alloy composed of multiple metals, has higher thermal stability, ensuring that the perpendicular magnetic anisotropy and synchronous antiferromagnetic coupling strength of the device are better after high-temperature annealing. This avoids the problem of poor performance after high-temperature annealing in the prior art due to the relatively single metal in the second pinning layer, solves the problem of poor performance of MRAM in the prior art after high-temperature annealing, and ensures better performance of the semiconductor device.

[0028] In addition, the semiconductor device disclosed herein has a better data retention capability after high-temperature annealing because the metal layer of the second pinning layer includes an alloy composed of multiple metals, thereby ensuring better reliability of the semiconductor device.

[0029] In the prior art, the material of the metal layer is generally selected as Co. As shown in Figures 2 and 3, Figure 2 shows a performance test diagram of the synchronous antiferromagnetic coupling strength of a semiconductor device in the prior art after high-temperature annealing, and Figure 3 shows a performance test diagram of the synchronous antiferromagnetic coupling strength of a semiconductor device in the present disclosure after high-temperature annealing. The high-temperature annealing is performed at 400°C for 1H. The synchronous antiferromagnetic coupling strength is represented by AP1 (the first pinning layer) and AP2 (the second pinning layer). As can be seen from Figures 2 and 3, the high-temperature data retention capability in Figure 2 is relatively weak, resulting in poor reliability of the semiconductor device in the prior art. The data in Figure 3 shows a step-by-step increase, that is, the high-temperature data retention capability in Figure 3 is relatively strong, with BEOL (Back End Of Line) compatibility after 400°C, enhanced data retention capability at high temperatures, and ensured good reliability of the semiconductor device in the present disclosure.

[0030] Perpendicular magnetic anisotropy is a magnetic anisotropy with a preferred orientation along a certain direction, caused by factors such as interface and lattice distortion. This magnetic anisotropy is crucial for memory function. Synchronous antiferromagnetic coupling refers to the strength of the exchange interaction between two adjacent antiferromagnetic layers. When two adjacent antiferromagnetic layers are synchronized, their spin orientations are complementary—one spin points up, the other points down. This generates an exchange interaction known as synchronous antiferromagnetic coupling. Therefore, properties such as perpendicular magnetic anisotropy and synchronous antiferromagnetic coupling strength are crucial for determining memory function.

[0031] To further ensure the excellent performance of the semiconductor device, the metal layer comprises a first metal and a second metal, wherein the first metal comprises a transition metal, and the second metal comprises a transition metal and / or an alkaline earth metal. Because the metal layer comprises the first metal and the second metal, and because the first metal comprises the transition metal and the second metal comprises the transition metal and / or the alkaline earth metal, the metal layer is a structural layer composed of multiple metals. This further ensures the metal layer has high thermal stability, resulting in excellent perpendicular magnetic anisotropy and synchronous antiferromagnetic coupling strength of the device after high-temperature annealing. This avoids the problem in the prior art of poor performance after high-temperature annealing due to the relatively simple metal content of the second pinned layer, solves the problem of poor performance of MRAM after high-temperature annealing in the prior art, and further ensures the excellent performance of the semiconductor device.

[0032] In this implementation, transition metals offer advantages such as good electronic conductivity, high stability, and controllable oxidation states. Alkaline earth metals offer advantages such as long-term data retention and low power consumption. Specifically, these alkaline earth metals can provide lower resistivity and better retention time, while also reducing power consumption and increasing lifespan.

[0033] Specifically, the first metal in the metal layer includes a transition metal, and the second metal includes a transition metal and / or an alkaline earth metal. In order to obtain the semiconductor device with superior performance, the specific material selection of the first metal and the second metal can be determined based on experiments, that is, after determining the material and thickness and other parameters of other structural layers in the semiconductor device, the first metal and the second metal of different materials can be prepared to obtain the semiconductor devices of different materials. By performing performance tests on the semiconductors corresponding to the metal layers of different materials, mainly including perpendicular magnetic anisotropy and synchronous antiferromagnetic coupling strength, the material of the metal layer with the best performance is determined as the preferred material. Therefore, the materials of the first metal and the second metal can be determined based on actual conditions.

[0034] To further ensure the superior performance of the semiconductor device, the first metal includes one of Co, Fe, CoFe, and CoFeB, and the second metal includes at least one of Hf, Zr, Ta, Mo, W, Cr, Ti, Rh, Nb, and Mg. The inclusion of the second metal in Hf, Zr, Ta, Mo, W, Cr, Ti, Rh, Nb, and Mg provides the second metal with high thermal stability, ensuring high-temperature diffusion isolation. This ensures that, after high-temperature annealing, the metal layer does not degrade the semiconductor device's perpendicular magnetic anisotropy and synchronous antiferromagnetic coupling properties. This ensures superior high-temperature data retention, avoids the prior art issue of poor performance after high-temperature annealing due to the relatively simple metal content of the second pinned layer, and addresses the prior art issue of poor performance of MRAMs after high-temperature annealing. This further ensures the superior reliability and performance of the semiconductor device.

[0035] Specifically, Mg is an alkaline earth metal, and Hf, Zr, Ta, Mo, W, Cr, Ti, Rh, and Nb are transition metals. The second metal materials Hf, Zr, Ta, Mo, W, Cr, Ti, Rh, Nb, and Mg all have extremely high thermal stability, ensuring that the second metal has a high-temperature diffusion isolation function. This ensures that the semiconductor device's properties, such as perpendicular magnetic anisotropy and synchronous antiferromagnetic coupling strength, do not degrade after high-temperature annealing, further ensuring the excellent performance of the semiconductor device.

[0036] In addition, the alkaline earth metal in the above-mentioned second metal is not limited to Mg. Semiconductor devices corresponding to alkaline earth metals of different materials can be prepared according to actual conditions, and performance tests can be performed on multiple of the above-mentioned semiconductor devices to obtain the material of the above-mentioned second metal with the best performance.

[0037] In the above implementation process, the metal layer includes one of CoZr, CoFeCr, CoFeBHf, and FeW. When the metal layer is made of CoZr, the first metal is Co and the second metal is Zr. When the metal layer is made of CoFeCr, the first metal is CoFe and the second metal is Cr. When the metal layer is made of CoFeBHf, the first metal is CoFeB and the second metal is Hf. When the metal layer is made of FeW, the first metal is Fe and the second metal is W.

[0038] Of course, the specific materials of the first metal and the second metal in the metal layer are not limited to the four mentioned above. According to actual experimental tests, when the first metal includes one of Co, Fe, CoFe and CoFeB, and the second metal includes at least one of Hf, Zr, Ta, Mo, W, Cr, Ti, Rh, Nb and Mg, the metal layers can be freely matched with a variety of materials, and the performance of the semiconductor devices with different material combinations can be tested to select the material with the best performance as the optimal material ratio of the semiconductor device.

[0039] In a specific implementation process, the proportion of the second metal in the metal layer is in a range of 5% to 50%. Specifically, the proportion of the second metal in the metal layer can be determined based on actual detection results.

[0040] Of course, the proportion of the second metal in the metal layer is not limited to 5%-50%. According to the thickness and material of other layers of the semiconductor device, the metal layers with multiple proportions can be provided, and then the vertical magnetic anisotropy and synchronous antiferromagnetic coupling and other properties of the metal layers with multiple proportions can be tested. Finally, the proportion of the second metal with better performance is determined as the final proportion, that is, the proportion range of the second metal in the metal layer can be determined according to actual conditions.

[0041] In a specific embodiment, as shown in FIG1 , the semiconductor device further includes a coupling layer 40. The coupling layer 40 is located between the first pinned layer 20 and the second pinned layer 30, and the coupling layer 40 is in contact with the first pinned layer 20 and the metal layer 301. Because the semiconductor device further includes the coupling layer, the coupling layer can achieve antiferromagnetic coupling between the first pinned layer and the second pinned layer, further ensuring better performance of the semiconductor device.

[0042] In the above implementation, the coupling layer can be formed by PVD (Physical Vapor Deposition), although other fabrication methods are also possible. Furthermore, the isolation layer and other layer structures can also be formed by PVD or other methods. During the PVD process, an inert or rare gas, such as argon (Ar), helium (He), krypton (Kr), or xenon (Xe), is ionized into a plasma in a sputtering chamber while the chamber is maintained in a vacuum state. Furthermore, the PVD processing chamber also contains at least one sputtering target, the material of which is determined based on the material of the structure to be fabricated, and a substrate is positioned so as to face the substantially flat surface of the sputtering target. The sputtering target is connected to a power source, such that the sputtering target is electrically driven or self-establishes as a cathode in a circuit connected to the power source, through the plasma to a ground, such as a grounded portion of the sputtering chamber. The substrate is positioned on a susceptor or other structure within the sputtering chamber. The susceptor or other structure can be at a floating potential, connected to ground, or biased to form an anode in the cathode target, through the plasma to the anode or ground circuit. The positively ionized portion of the inert gas atoms in the sputtering chamber is electrically attracted to the negatively biased target, causing the plasma ions to bombard the target, causing the atoms in the target to be ejected and deposited on the substrate to form a thin film of the target material on the substrate.

[0043] Specifically, the seed layer is mainly used to ensure that the quality of the first pinned layer is good. The material of the seed layer includes platinum (Pt) or ruthenium (Ru). By reducing or eliminating the lattice mismatch between the subsequent structures such as the first pinned layer and the substrate, the seed layer can be used to improve the adhesion and seeding effect of the subsequently deposited layers. Subsequently, the first pinned layer is formed on the surface of the seed layer by sputtering. Here, the first pinned layer includes a cobalt (Co) layer, and then sputtering is performed to form the coupling layer on the surface of the first pinned layer away from the seed layer. The coupling layer can be formed by iridium (Ir) sputtered from its target material. Then, the second pinned layer is formed on the surface of the coupling layer away from the first pinned layer by sputtering. Since the coupling layer is located between the first pinned layer and the second pinned layer, when the semiconductor device is exposed to a magnetic field, the surface atoms of the first pinned layer and the second pinned layer are aligned with the surface atoms of the coupling layer, thereby pinning the orientation of the first pinned layer and the second pinned layer. The first pinned layer and the second pinned layer each exhibit similar magnetic moments, and the coupling layer maintains antiparallel alignment of the magnetic moments of the first pinned layer and the second pinned layer.

[0044] In a specific implementation, the coupling layer includes Ir. Ir has excellent magnetic and electrical properties. Furthermore, since Ir is located between the first pinned layer and the second pinned layer, it enables spin transfer between the first and second pinned layers, further ensuring good performance of the semiconductor device.

[0045] In the above implementation process, in MRAM, Ir is selected as the material for the above coupling layer, mainly because Ir has good magnetic and electrical properties. Ir can form a strong exchange coupling with ferromagnets and has high resistivity and low magnetic leakage characteristics, which are very important for achieving high-density storage. By placing Ir between the above-mentioned first pinning layer and the above-mentioned second pinning layer, spin transfer between the two can be achieved, and an effective exchange bias field can be generated. In addition, the use of Ir in MRAM also has the advantages of improving reading speed, reducing power consumption and increasing stability. In short, Ir plays a vital role as a coupling layer in MRAM. It not only affects basic parameters such as memory capacity and stability, but also directly determines whether the entire system can meet application requirements such as high speed and low power consumption.

[0046] Of course, the material of the coupling layer is not limited to Ir, and other materials with the same performance may also be selected, which is determined according to actual conditions.

[0047] In a specific embodiment, as shown in FIG1 , the semiconductor device further includes a reference layer 50, a first tunneling layer 60, a free layer 70, a second tunneling layer 80, and a capping layer 90. The reference layer 50 is located on a surface of the second pinned layer 30 away from the first pinned layer 20, and the reference layer 50 contacts the isolation layer 302. The first tunneling layer 60 is located on a surface of the reference layer 50 away from the second pinned layer 30. The free layer 70 is located on a surface of the first tunneling layer 60 away from the reference layer 50. The second tunneling layer 80 is located on a surface of the free layer 70 away from the first tunneling layer 60. The capping layer 90 is located on a surface of the second tunneling layer 80 away from the free layer 70. Because the semiconductor device further includes the reference layer, the first tunneling layer, the free layer, the second tunneling layer, and the capping layer, the semiconductor device can implement magnetic tunnel junction storage and read functions.

[0048] In this implementation, the reference layer is a magnetic material with a constant magnetization and stable polarity. By interacting with the free layer, it generates a magnetoresistance effect and determines the rotation direction of electrons in the free layer. The free layer is a thin, flexible magnetic material that can change its magnetization state when an external magnetic field is applied. When current passes through the magnetic tunnel junction, it causes forward or reverse rotational motion within the free region, thereby enabling data storage and readout. The first and second tunnel layers are primarily composed of metal oxides, forming an insulating dielectric. By adjusting the thickness and material properties of the first and second tunnel layers, the energy required for electrons to cross the insulating interface between the two ferromagnetic materials can be controlled. By significantly increasing the difference in device impedance ratios, the readout sensitivity of the semiconductor device can be improved. In summary, the reference layer, free layer, first tunnel layer, and second tunnel layer work together to achieve the memory's data storage, readout, and transmission functions.

[0049] In addition, the above-mentioned covering layer is mainly used to include the above-mentioned second tunneling layer and other layers, so as to prevent other layers in the above-mentioned semiconductor device from being damaged, thereby further ensuring the good performance of the above-mentioned semiconductor device.

[0050] In a specific implementation process, the material of the isolation layer includes at least one of Ta, W and Mo. The isolation layer can be one of Ta, W or Mo. The isolation layer is used to isolate the metal layer and the free layer, further ensuring good performance of the semiconductor device.

[0051] In the above implementation process, the thickness of the above isolation layer ranges from 2 angstroms to 4 angstroms.

[0052] In a specific embodiment, the thickness of the metal layer is in the range of 3 angstroms to 15 angstroms.

[0053] In addition, the thickness range of the metal layer is not limited to 3 angstroms to 15 angstroms, and can be 2.5 angstroms, 15.5 angstroms, 16 angstroms, etc., which is determined based on test results.

[0054] The following are several main implementations of the semiconductor device, but the implementations of the present disclosure are not limited thereto.

[0055] In embodiment 1, the semiconductor device comprises a stacked seed layer, a first pinned layer, a coupling layer, a second pinned layer (including the metal layer and the isolation layer), a reference layer, a first tunneling layer, a free layer, a second tunneling layer, and a capping layer. The metal layer is made of the first metal and the second metal, wherein the first metal comprises Co, the second metal comprises Zr, the coupling layer comprises Ir, and the isolation layer comprises at least one of Ta, W, and Mo.

[0056] Example 2: The difference between Example 2 and Example 1 is that the first metal in Example 2 includes CoFe, and the second metal in Example 2 includes Cr;

[0057] Example 3: The difference between Example 3 and Example 1 is that the first metal in Example 3 includes CoFeB, and the second metal in Example 3 includes Hf;

[0058] Example 4: The difference between Example 4 and Example 1 is that the first metal in Example 4 includes Fe, and the second metal in Example 4 includes W.

[0059] The embodiments of the present disclosure further provide an MRAM, which includes any one of the above-mentioned semiconductor devices.

[0060] The MRAM includes any of the aforementioned semiconductor devices. Compared to the prior art MRAM that suffers from performance degradation after high-temperature annealing, the MRAM disclosed herein, because the second pinned layer in the semiconductor device includes the metal layer, and because the metal layer is an alloy composed of multiple metals, has high thermal stability. This ensures that after high-temperature annealing, the device exhibits good perpendicular magnetic anisotropy and synchronous antiferromagnetic coupling strength. This avoids the prior art problem of performance degradation after high-temperature annealing due to the relatively single metal in the second pinned layer, thereby resolving the prior art MRAM performance degradation after high-temperature annealing and ensuring good performance of the semiconductor device.

[0061] In the above-mentioned implementation process, the above-mentioned semiconductor device is mainly an MTJ stack structure in MRAM. By setting at least one of the above-mentioned second metals Hf, Zr, Ta, Mo, W, Cr, Ti, Rh, Nb and Mg in the above-mentioned metal layer of the above-mentioned MTJ stack structure, and because Hf, Zr, Ta, Mo, W, Cr, Ti, Rh, Nb and Mg have good thermal stability, the above-mentioned metal layer has a high-temperature diffusion isolation function. Therefore, during the high-temperature annealing process of the above-mentioned MTJ stack structure, since the above-mentioned metal layer has the high-temperature diffusion isolation function, the perpendicular magnetic anisotropy and synchronous antiferromagnetic coupling strength of the above-mentioned MTJ stack structure will not be degraded, thereby avoiding the problem in the prior art that the performance deteriorates after high-temperature annealing due to the relatively single metal in the second pinned layer, solving the problem of the prior art that the performance of MRAM deteriorates after high-temperature annealing, and further ensuring the better performance of the above-mentioned MRAM.

[0062] In addition, the first metal in the metal layer of the MRAM includes one of Co, Fe, CoFe, and CoFeB, so that the metal layer is a metal alloy composed of the first metal and the second metal. Since the metal alloy has high thermal stability, the perpendicular magnetic anisotropy and synchronous antiferromagnetic coupling strength of the device are ensured to be good after high-temperature annealing of the metal layer, further ensuring good performance of the MRAM.

[0063] In the above embodiments of the present disclosure, the description of each embodiment has its own focus. For parts that are not described in detail in a certain embodiment, reference can be made to the relevant descriptions of other embodiments.

[0064] From the above description, it can be seen that the above embodiments of the present disclosure achieve the following technical effects:

[0065] 1) The semiconductor device disclosed herein includes a seed layer, a first pinning layer, and a second pinning layer, wherein the first pinning layer is located on the surface of the seed layer; the second pinning layer is located on a side of the first pinning layer away from the seed layer; the second pinning layer includes a stacked metal layer and an isolation layer, the metal layer is located on the surface of the isolation layer near the first pinning layer, and the metal layer includes an alloy composed of multiple metals. Compared to the problem of poor performance of MRAM in the prior art after high-temperature annealing, the semiconductor device disclosed herein, because the second pinning layer includes the metal layer and the metal layer is an alloy composed of multiple metals, has higher thermal stability, ensuring that after high-temperature annealing, the perpendicular magnetic anisotropy and synchronous antiferromagnetic coupling strength of the device are better. This avoids the problem of poor performance after high-temperature annealing in the prior art due to the relatively single metal in the second pinning layer, solves the problem of poor performance of MRAM in the prior art after high-temperature annealing, and ensures better performance of the semiconductor device.

[0066] 2) The MRAM disclosed herein includes any of the aforementioned semiconductor devices. Compared to the prior art MRAM, which suffers from performance degradation after high-temperature annealing, the MRAM disclosed herein, because the second pinned layer in the semiconductor device includes the metal layer, and because the metal layer is an alloy composed of multiple metals, has high thermal stability. This ensures that after high-temperature annealing, the device exhibits good perpendicular magnetic anisotropy and synchronous antiferromagnetic coupling strength. This avoids the prior art problem of performance degradation after high-temperature annealing due to the relatively single metal in the second pinned layer, thereby resolving the prior art MRAM performance degradation after high-temperature annealing and ensuring good performance of the semiconductor device.

[0067] The foregoing description is merely a preferred embodiment of the present disclosure and is not intended to limit the present disclosure. Those skilled in the art will readily appreciate that various modifications and variations are possible. Any modifications, equivalent substitutions, or improvements made within the spirit and principles of the present disclosure shall be included within the scope of protection of the present disclosure.

Claims

1. A semiconductor device, comprising: Seed layer; A first pinning layer, located on a surface of the seed layer; The second pinning layer is located on a side of the first pinning layer away from the seed layer. The second pinning layer includes a stacked metal layer and an isolation layer. The metal layer is located on a surface of the isolation layer close to the first pinning layer. The metal layer includes an alloy composed of multiple metals.

2. The semiconductor device according to claim 1, wherein The material of the metal layer includes: a first metal, the first metal comprising a transition metal; The second metal comprises a transition metal and / or an alkaline earth metal.

3. The semiconductor device according to claim 2, wherein: The first metal includes one of Co, Fe, CoFe and CoFeB, and the second metal includes at least one of Hf, Zr, Ta, Mo, W, Cr, Ti, Rh, Nb and Mg.

4. The semiconductor device according to claim 2, wherein: The second metal accounts for 5%-50% of the metal layer.

5. The semiconductor device according to claim 1, wherein The semiconductor device further comprises: The coupling layer is located between the first pinning layer and the second pinning layer, and the coupling layer is in contact with the first pinning layer and the metal layer respectively.

6. The semiconductor device according to claim 5, wherein: The material of the coupling layer includes Ir.

7. The semiconductor device according to claim 1, wherein The semiconductor device further comprises: A reference layer, located on a surface of the second pinned layer away from the first pinned layer, the reference layer being in contact with the isolation layer; a first tunneling layer, located on a surface of the reference layer away from the second pinning layer; A free layer, located on a surface of the first tunneling layer away from the reference layer; A second tunneling layer, located on a surface of the free layer away from the first tunneling layer; The capping layer is located on a surface of the second tunneling layer away from the free layer.

8. The semiconductor device according to any one of claims 1 to 7, wherein: The material of the isolation layer includes at least one of Ta, W and Mo.

9. The semiconductor device according to any one of claims 1 to 7, wherein: The thickness of the metal layer is in the range of 3 angstroms to 15 angstroms.

10. An MRAM, wherein: A semiconductor device comprising any one of claims 1 to 9.

Citation Information

Patent Citations

  • Etching method of double magnetic tunnel junctions

    CN105374936A

  • Magnetic tunnel junctions with tunable high perpendicular magnetic anisotropy

    CN111868946A

  • Method for controlling pinning layer domain structure to realize polymorphic storage in giant / tunneling magnetoresistance structure and polymorphic memory

    CN113314166A

  • Optimization method of fixed layer in MTJ structure

    CN114665007A

  • Magnetic tunnel junction for MRAM applications

    US20130043471A1