Method of manufacturing a catalyst-coated ion-conducting membrane

WO2024246487A1PCT designated stage expired Publication Date: 2024-12-05JOHNSON MATTHEY HYDROGEN TECH LTD
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
PCT/GB2024/051310
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-05-26
Filing Date
2024-05-21
Publication Date
2024-12-05

Smart Images

  • Figure GB2024051310_05122024_PF_FP_ABST
    Figure GB2024051310_05122024_PF_FP_ABST
Patent Text Reader

Abstract

A method of manufacturing a catalyst-coated ion-conducting membrane is provided. The method comprises the step of spray-coating a first catalyst layer with a dispersion of an ion- conducting polymer to form a first ion-conducting polymer layer and then depositing one or more additional layers of ion-conducting polymer on the first ion-conducting polymer layer.
Need to check novelty before this filing date? Find Prior Art

Description

[0001]METHOD OF MANUFACTURING A CATALYST-COATED ION-CONDUCTING MEMBRANE Field of the Invention This invention relates to a method of manufacturing a catalyst-coated ion-conducting membrane. In particular, this invention relates to a method of manufacturing a catalyst-coated ion-conducting membrane for an electrochemical device, such as a fuel cell or an electrolyser. This invention also relates to associated methods of manufacturing a membrane-electrode assembly. Background Catalyst-coated ion-conducting membranes (CCMs) may be employed within electrochemical devices, such as electrolysers, fuel cells, electrochemical hydrogen pumps, and devices for the electrochemical reduction of carbon dioxide. Such CCMs comprise a solid polymeric ion- conducting membrane, such as a proton exchange membrane (PEM) or an anion exchange membrane (AEM), with an anode catalyst layer and / or a cathode catalyst layer applied to a face of the membrane, the anode catalyst layer and the cathode catalyst layer being applied to opposite faces of the membrane. For water electrolyser applications, hydrogen evolution reaction (HER) catalysts are used in such cathode catalyst layers, for example HER catalysts comprising platinum, such as platinum on a carbon support. Oxygen evolution reaction (OER) catalysts are utilised in electrolyser anode catalyst layers. For PEM water electrolyser applications, suitable OER catalysts comprise iridium and / or ruthenium, for example oxides of iridium, or oxides containing both iridium and ruthenium. For AEM water electrolyser applications, non-platinum group metal OER catalysts may also be used, such as alloys and oxides of nickel, cobalt, iron, and copper. For fuel cell applications, oxygen reduction reaction (ORR) catalysts are used in cathode catalyst layers and hydrogen oxidation reaction (HOR) catalysts are utilised in anode catalyst layers. For PEM fuel cell applications, suitable cathode and anode catalyst materials comprise a platinum group metal or an alloy of a platinum group metal with one or more other metals, for example platinum, or an alloy of platinum with one or more other metals, typically provided on a carbon support. Other electrochemical devices may also incorporate CCMs, with the catalyst layers being selected according to the desired electrochemistry. For example, for electrochemical hydrogen pump applications, CCMs may be provided with a first catalyst layer incorporating a hydrogen oxidation reaction (HOR) catalyst (such as a platinum catalyst) on one face of the ion-conducting membrane, and a second catalyst layer incorporating a hydrogen evolution reaction (HER) catalyst (such as a platinum catalyst) on the opposite face of the ion- conducting membrane. Separate seal material layers, typically formed from non-ion conducting polymers, may be positioned around the edge region of a CCM, for example on exposed surfaces of the ion- conducting membrane where no electrocatalyst is present (but will also often overlap on to the edge of the electrocatalyst layer) to provide a seal to prevent escape of reactant and product gases, to reinforce and strengthen the edge of the CCM and provide a suitable surface for supporting subsequent components such as sub-gaskets or elastomeric gaskets. An adhesive layer may be present on one or both surfaces of the seal material layer. Such an arrangement is known as a membrane-seal assembly. CCMs may be incorporated into a membrane electrode assembly (MEA), which is essentially composed of five layers. The central layer is the ion-conducting membrane. On either side of the ion-conducting membrane there is an electrocatalyst layer, containing an electrocatalyst designed for the specific electrolytic reaction. Finally, adjacent to each electrocatalyst layer there is a gas diffusion layer or a porous transport layer, depending on the final MEA application and stack configuration. Such layers allow the reactants to reach the electrocatalyst layer and the products to leave. It is known to form CCMs by sequential deposition of layers. EP2774203B1 describes method comprising the steps of a) preparing a first catalyst layer on a supporting substrate; b) coating the first catalyst layer with an ionomer dispersion to form an ionomer membrane in contact with the first catalyst layer; and c) applying a second catalyst layer on top of the ionomer membrane. In the Examples, a roll of Pt-alloy cathode electrode on a carrier substrate is coupled and made to adhere to a still wet ionomer impregnated ePTFE film. There are significant manufacturing efficiency advantages associated with sequential deposition of layers to form CCMs (such processes may be known as additive layer manufacturing). However, formation of an ion-conducting membrane on the surface of a catalyst layer provides technical challenges. For example, it has been found that coating a dispersion of an ion-conducting polymer (for example by slot dye coating) onto a catalyst layer can lead to both the solvent and the ion-conducting polymer (used to form the membrane) penetrating the catalyst layer. This can lead to the formation of bubbles and / or blisters in the catalyst layer which can affect CCM performance. This can be a significant issue in particular during large scale manufacture with tight quality control standards. There remains a need to further enhance and develop methods for the production of catalyst- coated ion-conducting membranes, in particular methods which enable sequential deposition of CCM components whilst maintaining technical performance. Summary of the invention The present inventors have identified an enhanced approach for the production of catalyst- coated ion-conducting membranes that addresses some of the manufacturing concerns previously described. In a first aspect of the invention, there is provided a method of manufacturing a catalyst-coated ion-conducting membrane, the method comprising the steps of: (a) providing a first catalyst layer on a support substrate; (b) forming an ion-conducting membrane in contact with the first catalyst layer by a process comprising the steps of: (i) spray-coating the first catalyst layer with a dispersion of an ion-conducting polymer to form a first ion-conducting polymer layer; and (ii) depositing one or more additional layers of ion-conducting polymer on the first ion-conducting polymer layer; (c) heat-treating the ion-conducting membrane; (d) optionally, after step (b) or after step (c), applying a second catalyst layer to the opposite face of the ion-conducting membrane to the first catalyst layer. The use of a spray coating step prior to further deposition of ion-conducting polymer to form an ion-conducting membrane offers a reduction in the ingress of membrane ion-conducting polymer and / or solvent into the catalyst layer and therefore offers a reduction in the presence of bubbles and / or blisters in the catalyst layers and an improvement in layer quality. The process improvements also provide benefits for the production of membrane-electrode assemblies. Therefore, in a second aspect of the invention there is provided a method of manufacturing a membrane-electrode assembly, the method comprising the steps of: (i) providing a catalyst-coated ion-conducting membrane manufactured using the method according to the first aspect, the catalyst-coated ion-conducting membrane comprising a first face and a second face; and (ii) applying a gas diffusion layer and / or a porous transport layer onto the first face and / or the second face of the catalyst-coated ion-conducting membrane. In a third aspect of the invention there is provided a catalyst-coated ion-conducting membrane obtained, or obtainable by, the method of the first aspect. Brief description of the Figures Figure 1 shows a schematic representation of a support substrate provides with patches of a first catalyst later. Figure 2 shows a schematic representation of an example of a method of manufacturing a catalyst-coated ion-conducting membrane. Detailed Description Preferred and / or optional features of the invention will now be set out. Any of the preferred and / or optional features of any aspect may be combined, either singly or in combination, with any other preferred and / or optional features of any aspect of the invention unless the context demands otherwise. The invention provides a method of manufacturing a catalyst-coated ion-conducting membrane. Typically, the catalyst-coated ion-conducting membrane is a catalyst-coated proton exchange membrane or a catalyst-coated anion exchange membrane. The catalyst- coated ion-conducting membrane is suitable for an electrochemical device, such as a fuel cell an electrolyser, an electrochemical hydrogen pump, or a device for the electrochemical reduction of carbon dioxide, and in particular a proton exchange membrane fuel cell or electrolyser or an anion exchange membrane fuel cell or electrolyser. As used herein the term “catalyst-coated ion-conducting membrane” refers to an ion- conducting membrane with a first face and a second face, and which has a first catalyst layer on the first face and, optionally, a second catalyst layer on the second opposite face. The method comprises step (a) providing a first catalyst layer on a support substrate. The support substrate provides support for the catalyst-coated ion-conducting membrane during manufacture and, if not immediately removed, can provide support and strength during any subsequent storage and / or transportation. The material from which the support substrate is made should provide the required support, be able to withstand the process conditions involved in producing the catalyst-coated ion-conducting membrane and be able to be easily removed without damage to the catalyst-coated ion-conducting membrane. Examples of materials suitable for use as a support substrate include a fluoropolymer, such as polytetrafluoroethylene (PTFE), ethylene tetrafluoroethylene (ETFE), perfluoroalkoxy polymer (PFA), fluorinated ethylene propylene (FEP – a copolymer of hexafluoropropylene and tetrafluoroethylene), and polyolefins, such as biaxially oriented polypropylene (BOPP). Other examples include laminates, multi-layer extrusions and coated films / foils capable of retaining their mechanical strength / integrity at elevated temperatures, for example temperatures up to 200 °C. Examples include laminates of: poly(ethylene-co-tetrafluoroethylene) and polyethylene naphthalate (PEN); polymethylpentene (PMP) and PEN; polyperfluoroalkoxy (PFA) and polyethylene terephthalate (PET) and polyimide (PI). The laminates can have two or more layers, for example ETFE-PEN-ETFE, PMP-PEN-PMP, PFA-PET-PFA, PEN-PFA, FEP-PI-FEP, PFA-PI-PFA and PTFE-PI-PTFE. The layers may be bonded using an adhesive, such as acrylic or polyurethane. The first catalyst layer is provided on a first face of the support substrate. The first catalyst layer may cover substantially the entire first face of the support substrate, or it may be preferred that the first catalyst layer may be provided in at least one region of the first face of the support substrate with the first catalyst layer being absent on other regions of the first face of the support substrate. In such cases it will be understood that the dimensions of the one or more regions coated with a first catalyst layer will depend on the configuration of the electrochemical device into which the formed catalyst-coated ion-conducting membrane is designed to be incorporated. Typically, the region(s) coated with the first catalyst layer corresponds to the active catalyst area of the formed catalyst-coated ion-conducting membrane. Suitably, such regions are in the shape of a quadrilateral, such as a rectangle or a square, or may be, for example an oval or circle. It may be preferred that the regions coated with a first catalyst layer do not extend to the edges of the support substrate. It will be understood by the skilled person that the present method may be used to prepare a single catalyst-coated ion-conducting membrane, in which case a single region (or patch) of catalyst layer may be provided on the support substrate, or may be used to manufacture multiple catalyst-coated ion-conducting membranes, for example using a roll-to-roll process. In such cases, multiple regions (or patches) of catalyst layer may be provided on the support substrate. Preferably, the first catalyst layer is provided in the form of discrete patches on the support substrate. By discrete patches it is meant that the first catalyst layer is present on the first face of the support substrate in two or more regions which are not connected to each other. The provision of the first catalyst layer as discrete patches offers advantages associated with a reduction in the amount of catalyst material used in the manufacturing process and avoids the provision of catalyst layers in areas of the catalyst coated membrane that are not required to be electrochemically active. The catalyst layer is suitably for an electrode (e.g. anode or cathode) of a fuel cell or an electrolyser. The first catalyst layer comprises a catalyst. The catalyst is suitably an electrocatalyst. The catalyst layer can comprise a conductive support, wherein the catalyst is supported on the conductive support. The catalyst can be a finely divided unsupported metal powder, or may, for example, be a supported catalyst wherein small metal nanoparticles are dispersed on an electrically conducting particulate support, such as a carbon support. The catalyst metal is suitably selected from: (i) the platinum group metals (i.e. platinum, palladium, rhodium, ruthenium, iridium, and osmium), (ii) gold or silver, (iii) a base metal (e.g. nickel, cobalt, or copper), or (iv) an alloy or mixture comprising one or more of these metals or their oxides. If the catalyst is a supported catalyst, the loading of metal particles on the (e.g. carbon) support material is suitably in the range of and including 10 to 90 wt%, preferably in the range of and including 15 to 75 wt% of the total weight of resulting electrocatalyst. It may be preferred that the catalyst metal in the first catalyst layer is platinum, which may be alloyed with other precious metals or base metals. It may be further preferred that the catalyst in the first catalyst layer is platinum on a carbon support. It may be further preferred that the catalyst metal in the first catalyst layer is iridium, for example that the first catalyst layer comprises iridium oxide (IrOx). The first catalyst layer may comprise more than one catalyst, for example an iridium catalyst and a platinum catalyst, such as iridium (or iridium oxide) and platinum. The catalyst layer typically comprises additional components, such as an ion-conducting polymer, to improve ionic conductivity within the layer. Preferably, the first catalyst layer is electronically conducting. Typically, the first catalyst layer has a thickness in the range of and including 2 to 20 ^m, such as in the range of and including 2 to 10 ^m. The first catalyst layer may be prepared using, for example, coating methods such as a slot- die (slot, extrusion) coating process, inkjet printing, gravure printing, curtain coating, or a spray coating process. Suitably, step (a) can further comprise the sub-steps of: (i) depositing a first catalyst dispersion on the support substrate; and (ii) drying the first catalyst dispersion to form the first catalyst layer. Typically, the catalyst dispersion comprises the catalyst material and an ion-conducting polymer dispersed in a solvent, such as water, a polar solvent (other than water), or a mixture of water and a polar solvent (other than water). The polar solvent can be a polar protic solvent. Preferably, the polar solvent is an alcohol, more preferably a C1-4alcohol, such as be methanol, ethanol, propan-1-ol or propan-2-ol. The first catalyst dispersion can be dried at a temperature in the range of and including 50-100 °C, preferably in the range of and including 60-80 °C. The method comprises step (b) forming an ion-conducting membrane in contact with the first catalyst layer. This membrane acts as the polymer electrolyte in the manufactured catalyst- coated ion-conducting membrane. It will be understood by the skilled person that the membrane is formed in contact with opposite face of the first catalyst layer to the face of the first catalyst layer in contact with the support substrate. The ion-conducting membrane is formed by a process comprising a first step of spray-coating the first catalyst layer with a dispersion of an ion-conducting polymer to form a first ion- conducting polymer layer. The first ion-conducting polymer layer is formed on and in direct contact with the first catalyst layer. In this step a dispersion of the ion-conducting polymer in one or more solvents is sprayed onto the first catalyst layer to form a coating. Preferably, the coating completely covers (or encapsulates) the first catalyst layer. Typically, the first ion-conducting polymer layer is formed by moving the first catalyst layer through a static spray coater. It may be preferred to use an ultrasonic spray coater. The use of an ultrasonic spray coater offers advantages with respect to coating uniformity and layer thickness control. The dispersion of ion-conducting polymer used for spray coating comprises the ion-conducting polymer dispersed in a solvent, or a mixture of solvents. Advantageously, the solvent (or mixture of solvents) is selected such that rapid solvent evaporation may be achieved after spray coating. It may be preferred that the solvent (or each solvent in a mixture of solvents) has a boiling point at 1 bar of pressure in the range of and including 60 to 110 °C. It may be preferred that the solvent is water, a polar solvent (other than water), or a mixture of water and a polar solvent (other than water). The polar solvent can be a polar protic solvent. Preferably, the polar solvent is an alcohol, more preferably a C1-4 alcohol, such as methanol, ethanol, or propan-1-ol. It may be preferred that the solvent is a mixture of water and a C1-4 alcohol (such as methanol, ethanol, or propan-1-ol). Typically, the dispersion of ion-conducting polymer used for spray coating comprises ion- conducting polymer in an amount in the range of and including 5 to 25 wt% based on the total weight of components in the dispersion. It will be understood that the amount of ion-conducting polymer in the dispersion can readily be varied to adjust the viscosity of the dispersion to facilitate spray coating. In the case that the catalyst-coated ion-conducting membrane comprises a PEM, the ion- conducting polymer is a proton-conducting polymer, such as an ion-conducting polymer which comprises sulfonic acid groups. The ion-conducting polymer preferably comprises a perfluorinated sulfonic acid (PFSA) ionomer, a partially-fluorinated sulfonic acid ionomer, a non-fluorinated sulfonic acid ionomer (such as a non-fluorinated hydrocarbon sulfonic acid ionomer, or mixtures thereof. The ion-conducting polymer may comprise a blend of proton- conducting polymers. Examples of suitable proton-conducting polymers include perfluorosulphonic acid ionomers (e.g. Nafion® (Chemours), Aciplex® (Asahi Kasei), AquivionTM (Solvay Speciality Polymers), Flemion® (Asahi Glass Co.), or ionomers based on a sulphonated hydrocarbon such as those available from FuMA-Tech GmbH as the fumapem® P, E or K series of products, JSR Corporation, Toyobo Corporation, and others. In the case that the catalyst-coated ion-conducting membrane comprises an AEM, the ion- conducting polymer is an anion-conducting polymer, such as a hydroxy-conducting polymer, for example ion-conducting polymers comprising quaternary ammonium functional groups. Suitable ion-conducting polymers include Fumion FAA-3 (Fumatech), Aemion ionomers (Ionomr), and PiperION ionomers (Versogen). Advantageously, solvent is evaporated from the first ion-conducting polymer layer prior to further deposition of ion-conducting polymer. This helps to avoid solvent and ion-conducting polymer ingress into the first catalyst layer. Evaporation may be achieved by heating the first ion-conducting polymer layer, for example by passing the layer through an oven. Preferably, the first catalyst layer is heated prior to spray coating. Such heating may be achieved, for example by passing the first catalyst layer on the support substrate through an oven prior to spray coating. Pre-heating the first catalyst layer facilitates rapid solvent evaporation and therefore offers a reduction in the time available for solvents to permeate into the first catalyst layer. The temperature of pre-heating will be selected depending on the choice of solvent (s) used in the spray coating step, but would typically be in the range of 60 to 110 °C. The rapid evaporation of solvent is also aided by controlling the thickness of the formed first ion-conducting polymer layer after spray coating and solvent removal. It may be preferred that the thickness of the first ion-conducting polymer layer is less than 8 µm, such as in the range of and including 1 to 8 µm. It may be preferred that the thickness of the first ion- conducting polymer layer is less than 5 µm, such as in the range of and including 1 to 5 µm. The thickness of the first ion-conducting polymer layer may be determined by, for example, analysis of a scanning electron microscope (SEM) image of a cross section of the first ion- conducting polymer layer on the support substrate at 0% relative humidity. Following spray coating, the process comprises depositing one or more additional layers of ion-conducting polymer on the first ion-conducting polymer layer. Preferably, the one or more additional layers are formed by a method comprising the steps of (i) depositing a dispersion of ion-conducting polymer; and (ii) drying the ion-conducting polymer dispersion to form part of the ion-conducting membrane. It will be understood by the skilled person that the dispersion is a dispersion of the ion-conducting polymer in a solvent (such as a mixture of water and a C1-4 alcohol (such as methanol, ethanol, or propan-1-ol)), and the drying step is used to remove solvent to form the membrane layer. The ion-conducting polymer(s) used to form the one or more additional layers is typically the same as the ion-conducting polymer used for the spray coating step. The ion-conducting polymer used to form the one or more additional layers may however be different from the ion- conducting polymer used for the spray coating step. The ion-conducting polymer used to form the one or more additional layers may suitably be selected from the ion-conducting polymers described hereinbefore in relation to the spray coating step. The ion-conducting polymer used to form the one or more additional layers is typically deposited as a dispersion in a solvent as previously described hereinbefore in relation to the spray coating step. It will be understood by the skilled person that the amount of ion- conducting polymer in the dispersion and the choice and ratio of solvents may be readily adjusted to achieve the desired dispersion properties for the chosen deposition method, for example dispersion viscosity. Suitably, the ion-conducting polymer is provided as a dispersion in a mixture of mixture of water and a C1-4alcohol (such as methanol, ethanol, or propan-1-ol) with amount of ion-conducting polymer in the range of and including 5-80 wt.% based on the total weight of components of the dispersion, preferably 10-50 wt.%, or more preferably 15-30 wt.% Preferably, the one or more additional layers are not deposited by a spray-coating process. The use of spray coating for deposition of additional layers limits the layer thickness that can be achieved and does not enable polymer reinforcements to be readily introduced during membrane manufacture. The one or more additional layers are preferably deposited by slot-die coating, knife-coating, bar coating, inkjet printing, gravure printing, or a curtain coating process. Preferably, the one or more additional layers are deposited by slot-die coating. The ion-conducting polymer dispersion may be dried at a temperature, for example, in the range of and including 50 °C to 100 °C, such as in the range of and including 60 °C to 80 °C. It may be preferred that step (b) (ii) comprises depositing a plurality of ion-conducting polymer layers. For example, step (b) (ii) may comprise the steps of (i) depositing an ion-conducting polymer dispersion onto the first ion-conducting polymer layer to form a first additional ion- conducting polymer layer; (ii) optionally drying the first additional ion-conducting polymer layer; (iii) depositing one or more additional ion-conducting polymer layers onto the first additional ion-conducting polymer layer. The subsequent additional ion-conducting polymer layers may be formed from the same composition as the first additional ion-conducting polymer layer or may have a different composition. It may be preferred that each ion-conducting polymer layer is dried (or partially dried) before the next layer is deposited. It may be preferred that the deposition of at least one additional ion-conducting polymer layer includes the incorporation of a polymer reinforcement, such as a polymer reinforcement comprising expanded polytetrafluoroethylene (ePTFE) or polybenzimidazole (PBI). Once dried, the first ion-conducting polymer layer and the one or more additional layers together form the ion-conducting membrane. The ion-conducting membrane is suitably ion- conducting and electrically insulating. The ion-conducting membrane layer can be for (part of) the electrolyte of an electrochemical device, such as fuel cell or electrolyser. The ion-conducting membrane may comprise one or more additives for example a radical scavenger (such as ceria), and / or a recombination catalyst. Such additives may be introduced by inclusion in one of the dispersions used for the formation of an ion-conducting polymer layer. Suitable radical scavengers are known to those in the art and include metal oxides, such as cerium oxides, manganese oxides, titanium oxides, beryllium oxides, bismuth oxides, tantalum oxides, niobium oxides, hafnium oxides, vanadium oxides and lanthanum oxides, suitably cerium oxides, manganese oxides or titanium oxides, preferably cerium dioxide (ceria). A recombination catalyst catalyses the reaction of H2and O2to form H2O. Suitable recombination catalysts can comprise a metal (such as platinum) which may be supported, for example on carbon. Typically, the ion-conducting membrane has a thickness at 0% relative humidity of at least about 5 µm. It may be preferred that the reinforced ion-conducting membrane has a thickness of at least about 8 µm, at least about 9 µm or at least about 10 µm. Typically, the thickness of the reinforced ion-conducting membrane at 0% relative humidity is less than or equal to about 200 µm, such as less than or equal to 150 µm, less than or equal to 100 µm, less than or equal to 50 µm, less than or equal to 30 µm, less than or equal to 25 µm, or less than or equal to 20 µm. The thickness of the membrane may be determined by analysis of a scanning electron microscope (SEM) image of a cross section of the membrane. It may be preferred that the membrane has a thickness at 0% relative humidity in the range of and including 8 µm to 200 µm, or 10 to 100 µm. The process comprises the step of (c) heat-treating the ion-conducting membrane. Heat treatment of the ion-conducting membrane improves the mechanical strength and dissolution resistance of the membrane and can increase the adhesion of the first and second (if present) catalyst layers to the membrane. Typically, the heat treatment is carried out a temperature in the range of and including 110 to 250 °C, such as 140 to 220 °C, or in the range of and including 150 to 180 °C. The process comprises the optional step of (d) applying a second catalyst layer on the surface of the ion-conducting membrane. It will be understood by the skilled person that the second catalyst layer is applied to the opposite face of the ion-conducting membrane from the first catalyst layer such that, once the second catalyst layer is applied, the ion-conducting membrane is positioned between, and typically in direct contact with, the first and the second catalyst layers. Components of the second catalyst layer and methods of application of the second catalyst layer are as described hereinbefore for the first catalyst layer. The second catalyst layer may also be applied using a transfer process onto the surface of the membrane, for example using a decal, such as by hot pressing. Typically, the first catalyst layer and the second catalyst layer comprise different catalyst materials. The catalyst materials are chosen depending on the required functionality (e.g. water electrolysis) and operating conditions (e.g. acidic or alkaline) of the formed catalyst-coated ion-conducting membrane. The application of the second catalyst layer may occur after any one of step (b) or step (c). It may be further preferred that the second catalyst layer is applied after step (c). Applying the second catalyst layer on the surface of the membrane after heat treatment offers advantages associated with reduced membrane swelling and solvent uptake during the application process. Preferably, the second catalyst layer is applied to regions of the ion-conducting membrane which correspond to the regions of the ion-conducting membrane with the first catalyst layer applied to the opposite face. Preferably, the regions of the second catalyst layer are centrally positioned over the regions of the first catalyst layer (but on the opposite face of the ion- conducting membrane). Preferably, the ion-conducting membrane formation in step (b) is carried out by roll-to-roll processing. More preferably, the spray coating step (b) (i) and the deposition of a first additional ion-conducting polymer layer in step (b) (ii) are carried out in a single pass (i.e. during a single unrolling and re-rolling process). Additionally, it may be further preferred that the steps of applying the first catalyst layer on the support substrate and / or heat treating the ion-conducting membrane in step (c) and / or applying the second catalyst layer in step (d) are carried out by roll-to-roll processes. Optionally, the process comprises the step of removing the support substrate from the catalyst-coated ion-conducting membrane. Optionally, the process comprises the step of applying a seal material to the first face and / or the second face of the catalyst-coated ion-conducting membrane. Typically, the seal material is applied after the removal of the catalyst-coated ion-conducting membrane from the support substrate, but the seal material may also be applied to one face of the catalyst-coated ion- conducting membrane after heat-treatment of the membrane (subsequent to step (c)) or after application of the second catalyst layer (subsequent to step (d)) and prior to removal from the support substrate. The catalyst-coated ion-conducting membrane manufactured using the hereinbefore described method can also be used in the manufacture of a membrane-electrode assembly. In order to form a membrane-electrode assembly a gas diffusion layer (GDL) and / or a porous transport layer (PTL) is applied onto at least one of the first and second faces of the catalyst- coated ion-conducting membrane (with or without prior application of a seal material). The choice of GDL and / or PTL will depend on the nature and configuration of the electrochemical device. Such materials are well known to the skilled person, for example gas diffusion layers are suitably based on conventional gas diffusion substrates. Typical substrates include non-woven papers or webs comprising a network of carbon fibres and a thermoset resin binder (e.g. the TGP-H series of carbon fibre paper available from Toray Industries Inc., Japan or the H2315 series available from Freudenberg FCCT KG, Germany, or the Sigracet® series available from SGL Technologies GmbH, Germany or AvCarb® series from Ballard Power Systems Inc., or woven carbon cloths. The carbon paper, web or cloth may be provided with a further treatment prior to being incorporated into a MEA either to make it more wettable (hydrophilic) or more wet-proofed (hydrophobic). The nature of any treatments will depend on the type of electrochemical device and the operating conditions that will be used. The substrate can be made more wettable by incorporation of materials such as amorphous carbon blacks via impregnation from liquid suspensions, or can be made more hydrophobic by impregnating the pore structure of the substrate with a colloidal suspension of a polymer such as PTFE or polyfluoroethylenepropylene (FEP), followed by drying and heating above the melting point of the polymer. For applications such as the PEMFC, a microporous layer may also be applied to the gas diffusion substrate on the face that will contact the electrocatalyst layer. The microporous layer typically comprises a mixture of a carbon black and a polymer such as polytetrafluoroethylene (PTFE). Porous transport layers are suitably based on conventional porous transport substrates, such as a titanium mesh for PEM electrolysis. Figures 1 and 2 depict exemplary methods of the present invention. The dimensions (e.g. thickness) of each layer are not drawn to scale for the sake of clarity. It will be clear to the skilled person that although the process described below is with reference to the manufacture to a continuous roll of multiple catalyst-coated ion-conducting membrane components, the basic process could be applied to the individual manufacture of a catalyst- coated ion-conducting membrane component. Figure 1 shows a plan view of a section of a support substrate (1) provided with patches of the first catalyst layer (2). Figure 2 shows a schematic of a process of forming a catalyst-coated ion-conducting membrane viewed as a cross section along line a-a indicated on Figure 1. In step (i) the support substrate (1) is provided with patches of the first catalyst layer (2). In step (ii), a thin first layer of ion-conducting polymer (3) is deposited onto the first catalyst layer (2) via spray- coating. In step (iii) a further layer of ion-conducting polymer (4) is deposited onto the first ion- conducting polymer layer (3), for example by slot-dye coating to form an ion-conducting membrane. In step (iv) patches of a second catalyst layer (5) are applied to the opposite face of the ion-conducting membrane to the first catalyst layer (2). In step (v), the ion-conducting membrane is heat treated. The product of stage (v) is the catalyst-coated ion-conducting membrane on the support substrate (1). The product may be further processed, for example though removal of the support substrate, cutting the coated membrane to form individual CCMs, the application of seals, etc. It will be understood that the first catalyst layer (2) may be provided as patches as shown in Figures 1 and 2 or may, for example, be provided in other configurations, such as provided over substantially all of the surface of the support substrate (1), or as a central continuous strip in the longitudinal direction of the support substrate (1). The first ion-conducting polymer layer formed by spray coating may be provided as a continuous layer over substantially all of the surface of the first catalyst layer (2) and any regions of the surface of the support substrate (1) where the first catalyst layer (2) is absent or may, for example, only be provided in regions where the first catalyst layer (2) is present. The process shown in Figure 2 provides for a single additional layer of ion-conducting polymer (4) on the first ion-conducting polymer layer, but it will be understood that the ion-conducting membrane may be formed from multiple additional layers applied via a series of passes through a coating machine, such as a slot dye coater, for example, there may be 2, 3, 4, 5, or more additional layers of ion-conducting polymer. One or more polymer reinforcements may be incorporated into the membrane (not shown in Figure 2), for example by introducing an ePTFE web during the deposition of an additional ion-conducting polymer layer. As alternatives to the process shown in Figure 2, the ion-conducting membrane may be heat treated prior to the application of the second catalyst layer (5), or no second catalyst layer (5) may be provided (for example for applications where the catalyst-coated membrane is used together with a catalyst coated substrate).

Claims

Claims 1. A method of manufacturing a catalyst-coated ion-conducting membrane, the method comprising the steps of: (a) providing a first catalyst layer on a support substrate; (b) forming an ion-conducting membrane in contact with the first catalyst layer by a process comprising the steps of: (i) spray-coating the first catalyst layer with a dispersion of an ion-conducting polymer to form a first ion-conducting polymer layer; and (ii) depositing one or more additional layers of ion-conducting polymer on the first ion-conducting polymer layer; (c) heat-treating the ion-conducting membrane; (d) optionally, after step (b) or after step (c), applying a second catalyst layer to the opposite face of the ion-conducting membrane to the first catalyst layer.

2. A method according to claim 1, wherein the first catalyst layer is heated to an elevated temperature prior to spray-coating.

3. A method according to claim 1 or claim 2, wherein the first ion-conducting polymer layer has a thickness less than 5 µm, such as in the range of and including 1 to 5 µm.

4. A method according to any one of the preceding claims, wherein the first catalyst layer is provided in the form of discrete patches on the support substrate.

5. A method according to any one any one of the preceding claims, wherein the one or more additional layers of ion-conducting polymer are formed by a method comprising the steps of (i) depositing a dispersion of ion-conducting polymer in a solvent; and (ii) drying the ion-conducting polymer dispersion to form the additional layer.

6. A method according to any one of the preceding claims, wherein the deposition of the one or more additional layers in step (b) (ii) is carried out by slot dye coating, knife coating, bar coating, inkjet printing or gravure printing.

7. A method according to any one of the preceding claims, wherein the spray coating is ultrasonic spray coating.

8. A method according to any one of the preceding claims, wherein the ion- conducting polymer is a proton-conducting polymer or a hydroxide-conducting polymer.

9. A method according to any one of the preceding claims, wherein steps (b) (i) and (b) (ii) are carried out as a roll-to-roll process.

10. A method according to claim 9, wherein step (b) (i) and the first deposition of ion-conducting polymer in step (b) (ii) and are carried out during a single roll-to-roll pass.

11. A method according to any one of the preceding claims, wherein the method comprises the additional step of removing the support substrate.

12. A method according to any one of the preceding claims, wherein the method comprises the additional step of applying a seal material to a first face and / or a second face of the catalyst-coated ion-conducting membrane.

13. A method according to any one of the preceding claims, wherein step (a) comprises the sub-steps of (i) depositing a first catalyst dispersion onto the support substrate; and (ii) drying the first catalyst dispersion to form the first catalyst layer.

14. A method according to any one of the preceding claims wherein the deposition of one of more additional layers of ion-conducting polymer in step (b) (ii) includes the incorporation of one or more polymeric reinforcements.

15. A method according to any one of the preceding claims, wherein heat-treating the ion-conducting membrane in step (c) comprises heating to a temperature in the range of and including 110 to 250 °C, such as 140 to 220 °C, or preferably 150 to 180 °C.

16. A method according to any one of the preceding claims, wherein applying a second catalyst layer on the surface of the ion-conducting membrane in step (d) comprises the sub-steps of (i) depositing a second catalyst dispersion on the surface of the ion- conducting membrane; and (ii) drying the second catalyst dispersion to form the second catalyst layer.

17. A method of manufacturing a membrane electrode assembly, the method comprising the steps of: (i) providing a catalyst-coated ion-conducting membrane manufactured using the method according to any of claims 1 to 16, the catalyst-coated ion-conducting membrane comprising a first face and a second face; and (ii) applying a gas diffusion layer and / or a porous transport layer onto at least one of the first or the second faces of the catalyst-coated ion-conducting membrane.

Citation Information

Patent Citations

  • Method for the preparation of catalyst-coated membranes

    EP2774203B1

  • Membrane electrode assembly with adhesive layer between membrane and electrode, method for preparing the same, and fuel cell comprising the same

    KR1020180002089A

  • Display device

    KR102546988B1

  • Method of manufacturing an integrated water vapor transfer device and fuel cell-II

    US10680266B2

  • Method of making fuel cell components including a catalyst layer and a plurality of ionomer overcoat layers

    US20070213203A1