Device for producing an inorganic non-metal melt, having a cooled upper furnace

The upper furnace with metallic coolant lines and refractory fillers addresses corrosion and maintenance challenges in lithium-containing material production, ensuring high-purity melts and extended service life with reduced heat loss.

WO2026234122A1PCT designated stage Publication Date: 2026-11-12SCHOTT AG
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
PCT/EP2026/063149
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2025-05-09
Filing Date
2026-05-06
Publication Date
2026-11-12

AI Technical Summary

Technical Problem

Conventional melting processes for producing lithium-containing materials with garnet-like structures and lithium-containing glasses are hindered by corrosion issues, leading to contamination and high costs, while existing upper furnaces have limited service life and require frequent disassembly for maintenance.

Method used

An upper furnace design with metallic coolant lines and refractory fillers, allowing for active cooling and self-supporting structure, preventing direct contact between condensate and furnace components, thus reducing corrosion and enabling quick access without disassembly.

Benefits of technology

The solution provides a longer service life, reduces contamination, and ensures high-purity melt production by minimizing contact between condensate and furnace materials, while allowing easy maintenance and reduced heat loss.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure EP2026063149_12112026_PF_FP_ABST
    Figure EP2026063149_12112026_PF_FP_ABST
Patent Text Reader

Abstract

The invention relates to a device for producing or guiding an inorganic non-metal melt, comprising at least one melt container (1), a unit (4) for heating a batch (3) so as to obtain a melt (5) and / or for heating the melt (5), a unit (7) for removing the melt (5), and an upper furnace (600) comprising a ceiling (65) and side walls (66), wherein the upper furnace (600) is situated above the melt container (1) when the device (100) is used as intended, at least the side walls (66) comprise cooled regions, and the cooled regions of the side walls (66) comprise metal lines (62, 63, 64) for a coolant.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] SCHOTT AG

[0002] P06274 WO

[0003] Device for producing an inorganic non-metallic melt with a cooled upper furnace

[0004] The present invention relates generally to a device for producing an inorganic, non-metallic material in a melting process. In particular, the present invention relates to a device for producing an inorganic, non-metallic melt with an upper furnace.

[0005] State of the art

[0006] The increased use of electrical energy as part of the energy transition, for example in electromobility, has led to a greater need for materials that can be used in energy storage systems. These materials can include, for example, inorganic non-metallic materials that can be used as solid-state ion conductors or as electrode materials.

[0007] Suitable materials for such applications, such as lithium-containing materials with a garnet-like structure and / or lithium-containing glasses, exhibit a number of special characteristics that make their production difficult. For example, lithium-containing sulfide glasses are known to have high ionic conductivity, but cannot be melted using conventional melting methods and are very susceptible to corrosion.Other inorganic non-metallic materials, such as those suitable as solid-state ion conductors, for example, lithium-containing crystalline materials with a garnet-like structure (e.g., lithium lanthanum zirconate, or LLZO for lithium lanthanum zirconate oxide), or with a so-called NASICON structure (NASICON for "sodium superion conductor," e.g., lithium aluminum titanium phosphate, or LATP for short), or cathode material for lithium-ion batteries made of lithium nickel manganese cobalt oxide (Li-NMC), are less susceptible to corrosion, but they strongly attack common crucible materials in known melting processes. For example, a melt of an "LLZO"-like material strongly corrodes a precious metal like platinum, which is frequently used in high-temperature applications, leading to contamination of the resulting material with metallic particles.This is important for the resulting electrical properties of such a molten material, since a solid-state ion conductor in a solid-state battery should simultaneously be insulating against electron conduction. Metallic impurities in the solid-state ion conductor are therefore undesirable. Regardless, severe corrosion of the refractory materials used in a melting process, such as platinum or other precious metals commonly used in melting vessels, or even other ceramic refractory materials, is generally undesirable, as it is associated with considerable costs and is therefore not economically viable.Although the above explanations were given as examples with regard to crystallizing materials, they naturally also apply to non-crystalline materials, such as glasses, which are also highly corrosive to common crucible or tank materials, for example due to a high fluorine content in the melt.

[0008] In conventional processes, the relevant materials cannot be produced via melting processes, or not in an economically viable way. However, it has been found that some of these materials can be produced in so-called "skull" crucibles or using appropriate melting methods. These devices feature cooled components or components with cooled sidewalls, where a thin layer of the material to be melted forms in solidified form on the cooled sidewalls. As a result, the molten material itself forms the outermost sidewall of the component at these points—that is, the part of the sidewall that is in contact with the aggressive melt. Thus, the aggressive or corrosive melt is not in contact with the component itself, but only with the corresponding solid, which is in equilibrium with the melt.With the appropriate devices or processes, it is therefore possible to melt materials that cannot be produced in conventional melting processes due to the high corrosion resistance of the melts.

[0009] Such skull crucibles, i.e., melting vessels with cooled walls, are described, for example, in US 2006 / 291528 A1, US 6817212 B1, US 2005 / 005646 A1, JP 2016 / 051701 A, US 2005 / 083989 A1, and DE 102 02449 A1. These patents concern general designs for such melting vessels, particularly with regard to the production of glasses and / or glass-ceramics in such melting vessels. A melting process for an LLZO material is described, for example, in US 2016 / 329598 A1.

[0010] To minimize heat loss, devices with crucibles often feature upper furnaces. The upper furnace is positioned above the crucible, thus separating a hot chamber from the surrounding environment, allowing, for example, the addition of the melt mixture to the crucible. The upper furnace is constructed from refractory materials. Furthermore, dust and gas particles, which typically occur during melting and loading, can be easily removed and extracted via the upper furnace.

[0011] The upper furnace can thus be made from a single, monolithic casting, for example from SiO2-based refractory ceramics such as so-called...

[0012] "Quartzal" is used in this process. Due to its one-piece construction, the upper furnace can be completely lifted off the crucible and removed without prior disassembly. However, a disadvantage is that the selection of suitable refractory materials for the production of one-piece upper furnaces using a casting process is limited.

[0013] Another disadvantage of upper furnaces made of refractory material lies in the low thermal shock resistance of many refractory materials. This can mean that these materials, or the corresponding components, have to be replaced after each firing cycle. With a one-piece upper furnace, the entire upper furnace therefore has to be replaced, resulting in a correspondingly short service life.

[0014] Therefore, alternative designs envision the upper furnace being constructed as a brick component. This allows individual components to be replaced as needed. However, a brick furnace cannot be removed from the crucible in one piece, meaning that, for example, the upper furnace must be dismantled and then rebuilt every time the melt is changed.

[0015] Particularly in the production of aggressive melts, it must also be ensured that the components condensed on the upper furnace do not attack it, thus preventing the introduction of particles and / or foreign material into the melt or a reduction in the service life of the upper furnace. Objective of the invention

[0016] The invention is therefore based on the objective of providing an upper furnace that has a longer service life, exhibits a very low tendency to contamination and allows quick and uncomplicated access to the crucible.

[0017] Description of the invention

[0018] The problem is already solved by the subject matter of the independent claims. Advantageous elaborations and further developments can be found in the dependent claims, the description, and the drawings of the disclosure.

[0019] Within the scope of this disclosure, the following definitions apply:

[0020] For the purposes of this disclosure, an upper furnace is understood to be an atmospheric and thermal confining space above the melt, which is designed as part of the melting vessel and serves as the point of access for burners, batch feed, and sensors. The unit consisting of the melting vessel and the upper furnace is also referred to as a melting assembly or assembly for the purposes of this disclosure.

[0021] An inorganic non-metallic material is understood to be a material that exists inorganically and exhibits no metallic bonding or metal bonding. The inorganic non-metallic material of the disclosure may, for example, exist in a crystalline state, be amorphous (which includes X-ray amorphous), or contain both crystalline and amorphous components, i.e., be partially crystalline. A partially crystalline inorganic non-metallic material may also be referred to as a glass-ceramic; an amorphous, especially X-ray amorphous, material as a glass; and a completely crystalline material as a ceramic.

[0022] Even if the inorganic non-metallic material of the disclosure is non-metallic in the sense that it in particular does not exhibit any electronic conductivity (i.e., conductivity with electrons as the charge carriers) or preferably exhibits such conductivity at a maximum of 10 S / cm in the case of LLZO or at 10 2In the case of NMC, where S / cm is low, it is possible and may even be preferred that the material acts as a solid-state ion conductor or at least has some ion conductivity.

[0023] The disclosure relates to an apparatus for producing an inorganic non-metallic material in a melting process. The apparatus comprises at least a melting vessel, a device for heating the mixture to obtain a melt and / or for heating the melt, a device for removing the melt, and an upper furnace comprising a roof and side walls. During intended use of the apparatus, for example, during its operation in a melting process, the upper furnace is arranged above the melting vessel. It is provided that at least the side walls include areas with metallic coolant lines. The upper furnace thus contains at least one metallic component. In particular, the upper furnace is not formed entirely of refractory materials.

[0024] Similar to a crucible, a solid layer forms on the cooled side walls of the upper furnace from the condensate of the melt. This condensate can have the same composition as the melt, or it can contain only individual elements or components of the melt. The solid layer thus formed ensures that further condensate, which returns to the melt, does not come into contact with the material of the cooled side walls. This protects the side walls of the upper furnace from corrosive attack by components of the melt. As a result, materials can also be used for the upper furnace that would not have sufficiently high corrosion resistance in direct contact with the melt. Furthermore, by preventing direct contact between the condensate and the side walls of the upper furnace, it is ensured that no particulate matter or other contaminants are released.Material from components of the upper furnace is introduced into the melt. This enables the production of melts with particularly high purity.

[0025] The side walls feature active cooling, at least in certain areas, whereby the coolant dissipates heat from the walls. The temperature of the cooled side walls, or the cooled sections thereof, is therefore lower than the temperature of the hot chamber formed by the upper furnace. This cooling allows the use of materials whose operating temperature is below that of the hot chamber. Thus, the material selection is not limited to refractory materials. The active cooling also makes it possible to use metallic materials in the upper furnace. The upper furnace therefore incorporates metallic coolant lines.

[0026] Cooling the side walls also significantly reduces temperature fluctuations. This means the side wall materials are exposed to less temperature variation during operation. As a result, materials with a comparatively low resistance to thermal shock can be used for the upper furnace's side walls without necessarily having a negative impact on the furnace's service life.

[0027] To ensure efficient heat dissipation, one embodiment provides that the coolant lines comprise or consist of a material exhibiting a thermal conductivity (ΔG) at 20 °C in the range of 5 W / m K to 500 W / m K, preferably in the range of 5 W / m K to 50 W / m K, and particularly preferably in the range of 5 W / m K to 20 W / m K. The use of stainless steel, copper, aluminum, and / or their alloys has proven particularly advantageous. In addition to their good thermal conductivity, these materials possess high mechanical stability. Furthermore, they are readily available and machinable.

[0028] According to one embodiment, the coolant lines are designed to carry a liquid, or preferably aqueous, coolant. The coolant can, for example, comprise high-temperature-stable oils, siloxanes, or water. This makes it easy to cool the upper furnace and / or integrate it into existing coolant circuits.

[0029] Preferably, the upper furnace is designed as a self-supporting or cantilevered structure, with the coolant lines forming the supporting structure. The coolant lines then form a support structure that defines and supports the upper furnace. To ensure sufficient stability of the structure, the weight and / or surface area of ​​the upper furnace are appropriately matched. For the purposes of this disclosure, "self-supporting" or "cantilevered" means that the upper furnace does not require any separate support elements. Instead, the upper furnace is supported by its own coolant lines. The side walls of the upper furnace are designed such that the entire upper furnace is movable without the need to dismantle individual components or parts. Thus, the upper furnace can be completely lifted without having to dismantle it.This allows the upper furnace to be removed from the assembly. This is particularly advantageous when changing the melt in the melting vessel.

[0030] The upper furnace comprises side walls and a roof, the roof defining the upper boundary of the hot chamber. Preferably, both the side walls and the roof of the upper furnace comprise cooled side walls. The upper furnace is open at the bottom and therefore has no bottom. The upper furnace is positioned above the melting vessel such that the lower opening faces the melting vessel and is preferably in contact with it.

[0031] A further development provides that the side walls of the upper furnace are essentially formed by the coolant lines. The coolant lines are preferably designed as cooling fins and spaced apart from one another, particularly running parallel to each other along a longitudinal axis L of the upper furnace. Analogous to a crucible, the condensate solidifies upon cooling into a solid crust, which forms a closed surface. This requires sufficient cooling of the side walls and a limited distance between adjacent cooling fins. Preferably, the distance d between two adjacent cooling fins is in the range of 5 cm to 40 cm, where d represents the mean (or "average") distance between two adjacent cooling fins, provided that the distance between two adjacent cooling fins is not constant.For example, if the distance between two adjacent cooling fins is 10 cm at the narrowest point and 20 cm at the widest, the average distance d would be 15 cm. In this further development, the upper furnace is particularly resistant to temperature changes when the crucible is switched on and off. It is therefore low-maintenance and has a long service life. Furthermore, the formation of a solid crust on the entire inner surface of the upper furnace prevents foreign material from entering the melt. Components such as the loading machine or a camera can be inserted into the upper furnace through one or more lateral openings. Upper furnaces with a conical shape have proven particularly advantageous. In this design, the upper furnace has a larger cross-sectional area in the lower, open section than at the top. The upper furnace can also be dome-shaped.Preferably, the upper furnace can also be removed from the melting vessel without damage and placed back on the melting vessel.

[0032] A further development therefore provides that, in addition to the metallic coolant lines, the side walls comprise non-metallic, temperature-resistant fillers, which are preferably arranged between the metallic coolant lines. The non-metallic fillers are not actively cooled and are therefore preferably made of a refractory material, which may be selected from the following group:

[0033] - Refractory ceramics based on SiO2, such as so-called "Quarzal", - Refractory ceramics based on corundum, such as mullite, - Refractory ceramics based on a material with at least 90% AlO3, - Refractory ceramics based on a material with at least 90% ZrO2, - Refractory ceramics based on boron nitrite, and

[0034] - Zirconium silicate.

[0035] The filler material preferably comprises or is composed of modules arranged between the coolant lines. The modules can be designed, in particular, as plates or bricks and made of the aforementioned material. The filler material can be in contact with the coolant lines, at least partially, and preferably, especially when comprising modules, can be detachably connected to the coolant lines. The filler modules can, for example, be designed such that they are inserted into the spaces between the coolant lines and held there in a form-fitting manner. It is conceivable, for instance, that the modules are essentially wedge-shaped and have beveled sides. Their wedge shape or beveled sides allow the modules to be held in position particularly reliably.Furthermore, this design allows the filler modules to remain movable relative to each other and to the coolant lines ("to have play"), thus preventing cracks in the upper furnace that could otherwise occur due to thermal expansion of the upper furnace. The filler preferably comprises at least one ceiling module that forms the ceiling of the upper furnace. Particularly preferably, the filler comprises two ceiling modules, each forming half of the upper furnace ceiling and which can be joined together to form the complete ceiling. In this embodiment, each of the two ceiling modules comprises half of a ceiling opening, so that when the two ceiling modules are joined, an opening is created in the ceiling.

[0036] The material of the filler arranged between the metallic cooling lines can also be described by its thermal conductivity. In particular, materials with a thermal conductivity of less than 10 W / m K, preferably less than 5 W / m K, and especially less than 2.5 W / m K are considered suitable fillers. The thermal conductivity of the material should also be at least 0.5 W / m K.

[0037] In principle, the non-metallic fillers of the side walls can be made of materials that are also present in the melt, because these do not result in undesirable contamination in the event of corrosion. In this embodiment, the metallic coolant lines form a framework that constitutes the supporting structure of the upper furnace. The areas of the side walls between the coolant lines are filled with the temperature-resistant filler.

[0038] Preferably, the filler material is connected to the coolant lines. Furthermore, it can be provided that the upper furnace, consisting of the filler material and coolant lines, can be removed from the melting vessel and reattached to it without damage.

[0039] The areas of the upper furnace formed by the temperature-resistant filler material do not have coolant lines. Instead, the filler areas are arranged between the coolant lines. In this embodiment, a solid layer does not form on the entire surface of the upper furnace's side walls. Thus, the surface of the areas formed by the refractory filler material is at least partially in contact with the condensates that form during the melting process. Depending on the process conditions under which the device is operated, as well as the refractory filler materials used, this can lead to corrosion of the corresponding components or modules. One embodiment therefore provides that the non-metallic components, i.e., the temperature-resistant filler material, are detachably connected to the metallic coolant lines.This allows for the easy replacement of individual non-metallic components or modules without the need to disassemble the entire upper furnace. Preferably, the non-metallic fillers are connected to the metallic coolant lines via screw connections, clamp connections, or similar mechanical connections.

[0040] It can also be provided that the filler occupies a proportion of the total internal surface area of ​​the upper furnace ranging from 10% to 99%. It is also conceivable that the filler occupies a proportion of the total internal surface area of ​​the upper furnace ranging from 40% to 99%, preferably from 70% to 99%, and particularly preferably from 80% to 99%. One embodiment provides that the non-metallic modules of the filler have a maximum area of ​​1,600 cm². 2and / or have a maximum weight of 30 kg. This allows the non-metallic modules to be moved manually without tools. This ensures, in particular, the self-supporting nature of the upper furnace.

[0041] In a preferred embodiment, the upper furnace is characterized by reduced heat loss compared to conventional solutions and, in particular, compared to an upper furnace constructed solely of directly cooled components. For example, the upper furnace may exhibit a heat loss per unit area that is at least 20% lower than that of an upper furnace made entirely of directly cooled components. Preferably, the reduction in heat loss per unit area can be at least 50%, and in particular, the reduction in heat loss compared to an upper furnace made entirely of directly cooled components can be up to 90%.

[0042] According to one embodiment, the side walls and / or the roof of the upper furnace each have at least one opening. Preferably, the upper furnace has at least one opening in the roof. The cross-sectional area of ​​the upper opening in the roof is many times smaller than the cross-sectional area of ​​the roof; thus, apart from the upper opening(s), the upper furnace is closed at the top. Alternatively or in addition to the upper opening in the roof of the upper furnace, the side walls of the upper furnace can have one or more lateral openings.

[0043] The openings in the side walls and / or the ceiling can, for example, accommodate a feed device for adding the mixture into the hot chamber. Other devices, such as devices for observing the melt surface or tools for manipulating the melt, like a tool for homogenizing the melt (e.g., a plunger or stirrer), can also be introduced into the hot chamber in this way. Furthermore, samples can be taken and the equipment maintained through openings in the side walls and / or the ceiling of the upper furnace. The tool for manipulating the melt can, for example, be attached to a suspension system that is designed to be movable both vertically and longitudinally.

[0044] A further development provides that the device has at least one burner. The burner can be, in particular, a conventional gas burner or an oxyfuel burner. A preferred embodiment provides for the use of a hydrogen burner. This reduces CO2 emissions, leading to a reduction in the CO2 footprint.

[0045] According to one embodiment, the melting vessel is designed as a crucible, and heat is supplied by a high-frequency heater (HF heater). However, this requires that the mixture has a sufficiently high conductivity. Therefore, an additional heat source, such as a burner, may be necessary to initiate the melting process of a cold melting vessel or a cold mixture. One embodiment provides that at least one burner is inserted into the upper furnace through a suitable opening, preferably the upper opening in the furnace roof. The burner is ignited and heats the unit, the upper furnace, and the mixture until the conductivity of the mixture is high enough for the HF heater's field to couple into the melt and supply the energy. The burner can then be removed from the upper furnace through the upper opening. The burner is suspended vertically within the device.The distance of the burner to the melt can thus be changed, and the burner can be inserted into or removed from the upper furnace.

[0046] Another embodiment provides that the melting vessel is designed as a conventional melting vessel. Here, the burner(s) can function as a permanent heating element and remain in the upper furnace during the melting process. The invention will be described in more detail below with reference to the figures and without limitation thereto. Identical reference numerals denote identical or similar elements.

[0047] They show:

[0048] Fig. 1 shows the schematic structure of the device according to one embodiment,

[0049] Fig. 2 shows the schematic structure of a water-cooled upper furnace according to one embodiment and

[0050] Fig. 3 shows the schematic structure of a water-cooled upper furnace comprising refractory materials according to a further embodiment.

[0051] Fig. 1 shows the schematic structure of a device 100 for producing or guiding an inorganic, non-metallic melt according to one embodiment. The device 100 comprises a melting vessel 1, which in the illustrated embodiment is designed as a crucible. The melting vessel therefore includes cooled side walls. The melt 5 in the melting vessel is heated by a high-frequency (HF) heating device 4. The heating device 4 therefore includes, in addition to a high-frequency source 41, a coil 42, which is arranged around the melting vessel 1. The melt 5 can be removed from the melting vessel 1 by a melt removal device 7, the melt removal device being arranged at the bottom of the melting vessel 1.

[0052] The device 100 comprises a device for supplying a mixture 2, with which a mixture 3 can be transferred from the mixture reservoir 21 to the melting vessel 1 via the mixture feed 22. To enable the continuous supply of the mixture 3 to the device 2 and to allow the melt extraction device 7 to enable continuous extraction of the melt 5 from the melting vessel 1, the inorganic, non-metallic melt 5 can be fed and / or melted in a continuous process using the device 100. The upper furnace 600 is another component of the device 100 and is arranged above the melting vessel 1. The upper furnace 600 is largely closed at the top and open at the bottom. The opening of the upper furnace 600 is positioned above the melting vessel 1 in such a way as to create a closed hot chamber 90.The hot chamber 90 is separated from the surroundings of the device 100 by the upper furnace 600. In the embodiment shown in Fig. 1, the side wall 66 of the upper furnace 600 has a lateral opening 67 through which the mixture feed 22 is led into the interior of the hot chamber 90.

[0053] The ceiling 65 of the upper furnace 600 is essentially closed, but contains an upper opening 61. This opening is designed to allow the insertion of a tool for manipulating the molten metal, such as a burner 70, into the hot chamber 90. The burner 70 is suspended vertically by means of the support 71 and, in the illustrated embodiment, is required to start the cold melting vessel 1. In the embodiment shown in Fig. 1, conventional gas burners, hydrogen burners, or oxyfuel burners can be used.

[0054] When the cold melting vessel 1 is started, the mixture 3 is already placed in the melting vessel 1. The burner 70 is ignited and heats the melting vessel 1, the mixture, and the hot chamber 90 until the conductivity of the mixture is high enough for the field of the high-frequency heater 4 to couple into the melt 5 and provide the energy input. The burner 70 can then be pulled out of the hot chamber 90 and the upper furnace 600 by means of the vertically movable suspension 71 through the upper opening 61. The burner 70 is then located outside the upper furnace 600 and can be removed as needed. However, embodiments are also possible in which the burner 70 remains in the hot chamber 90 or in the upper furnace 600 even after the cold melting vessel 1 has been started. This is particularly advantageous if the melting vessel 1 is designed as a conventional melting vessel rather than a crucible.Here, the burner 70 preferably remains for permanent heating in the upper furnace 600.

[0055] The side walls 66 of the upper furnace 600 include coolant lines (not shown) and are at least partially actively cooled. The upper furnace 600 is self-supporting and can be lifted off the melting vessel 1, particularly when assembled. Therefore, no disassembly of individual components is necessary to lift the upper furnace 600 from the melting vessel.

[0056] Figure 2 schematically depicts an embodiment of an upper furnace 600, in which the upper furnace 600 is constructed from metallic coolant lines 62, 63, 64. A coolant, preferably water, is circulated through the coolant lines 62, 63, 64, also referred to as cooling fins. A layer of condensate from elements of the melt forms on the surface of the coolant lines 62, 63, 64. The individual coolant lines 62, 63, 64 have a maximum distance of 40 cm from each other. This allows the formation of a continuous solid layer even in the areas 68 between the cooling fins 62, 63, 64. In this embodiment, the side walls 66 are thus formed by the cooling fins 62, 63, 64 and the solid layer. Due to the cooling and the associated formation of the solid layer, the condensate of the melt does not come into contact with the materials of the cooling fins 62, 63, 64.Furthermore, the cooling fins 62, 63, 64 exhibit relatively low and constant temperatures due to continuous cooling.

[0057] Furthermore, the upper furnace 600 is resistant to temperature changes during the switching on and off of the crucible and is therefore low-maintenance and has a long service life. This means that the coolant lines 62, 63, 64 are not limited to materials exhibiting high temperature stability, high thermal shock resistance, and high corrosion resistance. However, the coolant lines should preferably be corrosion-resistant, as the thermal conductivity of the refractory material is relatively low. Therefore, metals such as aluminum, stainless steel, or corresponding alloys are preferably used as materials for the coolant lines 62, 63, 64. This has the advantage that these materials are dimensionally stable, readily available, and machinable.

[0058] The solid layer also ensures that no foreign material is introduced into the melt. The embodiment shown in Fig. 2 is therefore particularly suitable for the production or handling of melts with high purity levels.

[0059] In the embodiment shown in Fig. 2, the ceiling 65 of the upper furnace 600 is also formed by coolant lines and the solid layer deposited on it and in the spaces between, wherein the upper furnace 600 has an upper opening 61 in the ceiling 65 through which components could be introduced into the hot room.

[0060] The upper furnace 600 is cooled across the entire surface of its side walls and a large portion of its roof. This results in cooling losses from the upper furnace 600 within the apparatus. Therefore, when designing a suitable upper furnace 600, the heat balance must be carefully considered so that the cooling losses of the upper furnace 600 are compensated for by the heat input into the melting pot 1; otherwise, problems may arise during coupling.

[0061] Fig. 3 therefore shows an alternative embodiment of a top furnace 600. Here, the coolant lines 62, 63, 64 form a support frame 69. Temperature-resistant fillers 80 made of refractory material are arranged at intervals 68 between the individual coolant lines 62, 63, 64. In this embodiment, the top furnace 600 is thus formed from a combination of a metallic, cooled support frame 69 comprising the coolant lines 62, 63, 64 and individual fillers made of refractory materials, for example, refractory bricks, connected to the support frame 69. The support frame 69 carries all the components of the top furnace 600. This allows it to be lifted from the melting vessel 1 without having to dismantle the refractory components of the filler material (80).

[0062] In the embodiment shown in Fig. 3, the upper furnace 600 is conically shaped. Here, the upper furnace 600 has a larger cross-sectional area in its lower region than in the region of the ceiling 65.

[0063] The support frame 69 is designed to ensure adequate cooling of the metal parts. By using materials such as aluminum or stainless steel, the support frame 69 can be shaped as desired. This allows for the use of suitable geometries for the components of the filler material 80.

[0064] The components made of refractory materials for the filling material 80 are arranged in the support frame 69 in such a way that a secure hold is ensured even under load during operation. In the embodiment shown in Fig. 3, the components of the filling material 80 are connected to the support frame 69 via detachable connections, preferably screwed together. This allows the individual components of the filling material 80 to be changed quickly and easily for simple maintenance and / or replacement.

[0065] In the embodiment shown in Fig. 3, essentially only the surfaces of the coolant lines 62, 63, 64 and the support frame 66 are covered with a solid layer. Thus, the surfaces of the filling material 80 facing into the hot chamber can come into contact with the condensate of the melt during operation. Therefore, refractory materials are selected for the filling material 80 that exhibit the highest possible corrosion resistance to the condensate and / or at least do not introduce any critical contaminants into the melt.

[0066] The combination shown in Fig. 3 of a cooled support frame 69 with refractory material 80 inserted or connected therein offers the advantage over a top furnace in which the side walls are completely formed and thus cooled by coolant lines that the energy loss in the device is significantly reduced by the cooled top furnace. The combination of refractory materials with a self-supporting support frame 69 and the possibility of replacing individual components of the refractory material 80 without requiring complete disassembly of the top furnace 600 nevertheless makes the furnace 600 easy to maintain.

[0067] Although the present invention has been described with reference to preferred embodiments, it is not limited to these and can be modified in many ways. Reference numerals

[0068] 1 melting vessel

[0069] 2 Device for feeding a mixture

[0070] 3 Mixture

[0071] 4 Heating device

[0072] 5 Melt

[0073] 7 Device for extracting the melt

[0074] 21 Mixed reservoir

[0075] 22 Mixture feed

[0076] 41 High-frequency source

[0077] 42 coil

[0078] 61 upper opening

[0079] 62, 63, 64 Coolant lines

[0080] 65 Ceiling of the upper furnace

[0081] 66 Wall of the upper furnace

[0082] 67 side opening

[0083] 68 Space between the coolant lines 69 Support frame

[0084] 70 burners

[0085] 71 vertically movable suspension

[0086] 80 Filler

[0087] 90 Hot room

[0088] 100 Device for producing or guiding a melt 600 Upper furnace

[0089] L Longitudinal direction of the upper furnace

Claims

Patent claims 1. Device (100) for producing or guiding an inorganic non-metallic melt, comprising at least - a melting vessel (1) - a device (4) for heating a mixture (3) to obtain a melt (5) and / or for heating the melt (5), - a device (7) for extracting the melt (5) and - a top furnace (600) comprising a ceiling (65) and side walls (66), wherein the upper furnace (600) is arranged above the melting vessel (1) when the device (100) is used as intended, wherein at least the side walls (66) comprise cooled areas and wherein the cooled areas of the side walls (66) comprise metallic coolant lines (62, 63, 64).

2. Device (100) according to claim 1, characterized in that the metallic coolant lines (62, 63, 64) comprise a material with a thermal conductivity A at 20 °C in a range of 5 W / m K to 500 W / m K, preferably in a range of 5 W / m K to 50 W / m K, and particularly preferably in a range of 5 W / m K to 20 W / m K and / or that the coolant lines (62, 63, 64) contain stainless steel, copper, aluminium and / or alloys of the aforementioned materials.

3. Device (100) according to one of the preceding claims, characterized in that the side walls (66) of the upper furnace (600) are formed at least partially by the coolant lines (62, 63, 64).

4. Device (100) according to one of the preceding claims, characterized in that the upper furnace (100) is designed to be self-supporting by comprising a support structure (69), wherein the support structure (69) is formed by the coolant lines (62, 63, 64).

5. Device (100) according to the preceding claim, characterized in that the upper furnace (600) can be removed from the melting vessel (1) and placed back onto the melting vessel (1) without damage.

6. Device (100) according to any one of the preceding claims, characterized in that the coolant lines (62, 63, 64) are arranged spaced apart from one another, wherein each pair of adjacent coolant lines (62, 63, 64) preferably has a mean distance d from one another, which is in a range of 5 cm to 40 cm.

7. Device (100) according to one of the preceding claims, characterized in that the side walls (66) of the upper furnace (600) have a non-metallic temperature-resistant filler (80) arranged between the coolant lines (62, 63, 64).

8. Device (100) according to claim 7, characterized in that the filler (80) comprises non-metallic components, wherein the non-metallic components of the filler (80) are preferably made of a refractory material, and wherein the refractory material is in particular selected from the group comprising: - Refractory ceramics based on SiÜ2 - Refractory ceramics based on corundum - Refractory ceramics based on a material with at least 90% Al₂O₃ - Refractory ceramics based on a material with at least 90% ZrÜ₂ - Refractory ceramics based on boron nitrite - Zircon silicate.

9. Device (100) according to one of claims 7 or 8, characterized in that the filler (80) has contact with the coolant lines (62, 63, 64) at least sectionally, wherein the filler (80) is preferably positively connected and preferably detachably connected to the coolant lines (62, 63, 64).

10. Device (100) according to any one of claims 7 to 9, characterized in that the filler (80) occupies a proportion of the total inner surface of the upper furnace (600) that is in the range of 10% to 99%, wherein the filler (80) preferably occupies a proportion of the total inner surface of the upper furnace (600) that is in the range of 40% to 99%, particularly preferably in the range of 70% to 99%, and especially in the range of 80% to 99%.

11. Device (100) according to claim 10, characterized in that the filler (80) has a total maximum inner surface area of ​​1,600 cm². 2 and / or has a maximum weight of 30 kg.

12. Device according to one of the preceding claims, characterized in that the ceiling (65) of the upper furnace (600) has at least one upper opening (61) and / or that the side walls (66) of the upper furnace (600) have at least one lateral opening (67).

13. Device (100) according to claim 12, characterized in that the device (100) has at least one burner (70) arranged on a suspension (71), wherein the suspension (71) of the burner (70) is vertically movable along a longitudinal axis (L) and wherein the suspension (71) is designed to insert the burner (70) through the upper opening (61) into the upper furnace (600) and / or to remove it from the upper furnace (600).

14. Device (100) according to one of the preceding claims, characterized in that the melting vessel (1) has cooled walls and is designed as a skull crucible.