Pre-flotation agitated leach with biosolvents to improve the separation of value metals in polymetallic substrates

The pre-flotation agitated leach process with biosolvents effectively solubilizes impurities and gangue from ore materials, improving the separation and recovery of value metals like nickel and copper by reducing waste and enhancing flotation efficiency.

WO2026236532A1PCT designated stage Publication Date: 2026-11-12ALLONNIA LLC
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
PCT/US2026/027157
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2025-05-07
Filing Date
2026-05-07
Publication Date
2026-11-12

AI Technical Summary

Technical Problem

Traditional flotation processes struggle with inefficient separation of value metals like nickel and copper, leading to loss of valuable metals in waste products and gangue trapping, which affects downstream processing and purification, necessitating improved methods for ore enrichment and separation.

Method used

A pre-flotation agitated leach process using biosolvents, such as organic acids derived from biobroths, selectively solubilizes impurities and gangue from ore materials, enhancing the separation efficiency of value metals by reducing the need for subsequent depressants and improving the recovery of metals like nickel, copper, and molybdenum.

Benefits of technology

The method enhances the separation and recovery of value metals by reducing the amount of valuable metals in tailings and improving the efficiency of flotation processes, allowing for better metal recovery and purification.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure US2026027157_12112026_PF_FP_ABST
    Figure US2026027157_12112026_PF_FP_ABST
Patent Text Reader

Abstract

A method for providing an ore substrate includes enriching a solid ore material via selective solubilization of an impurity component from the solid ore material with an extraction composition to produce an enriched ore material and a leachate; and separating the leachate from the enriched ore material. A method for improving a separation efficiency of a flotation process includes reducing an impurity content of a solid ore material with an extraction composition to form an enriched ore material and a leachate; separating the leachate from the enriched ore material; introducing the enriched ore material to a flotation apparatus; operating the flotation apparatus to produce a waste stream and one or more value streams; and recovering the value stream. The extraction composition includes an organic acid, can selectively solubilize an impurity from the solid ore material into the extraction composition, and retains at least one metal of value in the enriched ore material.
Need to check novelty before this filing date? Find Prior Art

Description

PATENT APPLICATION ATTORNEY DOCKET NO. 19148-013WO1 PRE-FLOTATION AGITATED LEACH WITH BIOSOLVENTS TO IMPROVE THE SEPARATION OF VALUE METALS IN POLYMETALLIC SUBSTRATES BACKGROUND

[0001] In the mining industry, there has been a general decline in ore grades over time.Decreasing ore quality requires more efficient operation or additional capital expenditure to meet production targets. This also presents an additional issue as further development of electrification technologies, such as battery economy and urbanization fuels, drives demand for relatively higher-grade ores of nickel, lithium, copper, rare earth metals, among others. Accordingly, there exists a need for methods for more sustainable mining practices to ensure production of high-grade ore.SUMMARY

[0002] This summary is provided to introduce a selection of concepts that are further described below in the detailed description. This summary is not intended to identify key or essential features of the claimed subject matter, nor is it intended to be used as an aid in limiting the scope of the claimed subject matter.

[0003] In one aspect, embodiments disclosed herein relate to a method for providing an ore substrate for a flotation process including enriching a solid ore material via selective solubilization of an impurity component from the solid ore material with an extraction composition to produce an enriched ore material and a leachate; and separating the leachate from the enriched ore material, thereby providing the ore substrate. The extraction composition includes at least one organic acid, is configured to selectively solubilize one or more impurities from the solid ore material into the extraction composition, and is configured to retain at least one metal of value in the enriched ore material.

[0004] In another aspect, embodiments herein a method for improving a separation efficiency of a flotation process including reducing an impurity content of a solid ore material with an extraction composition, thereby forming an enriched ore material and a leachate; separating the leachate from the enriched ore material; introducing the enrichedPATENT APPLICATION ATTORNEY DOCKET NO. 19148-013WO1ore material to a flotation apparatus; operating the flotation apparatus including a flotation mixture comprising the enriched ore material to produce a waste stream and a value stream; and recovering the value stream including a higher metal of value content as compared to a value stream obtained from a flotation process of the enriched ore material without treatment with the extraction composition. The extraction composition includes at least one organic acid; is configured to selectively transfer one or more impurities from the solid ore material into the extraction composition; and is configured to retain at least one metal of value in the enriched ore material.

[0005] Other aspects and advantages of the claimed subject matter will be apparent from the following description and the appended claims.BRIEF DESCRIPTION OF DRAWINGS

[0006] FIG. 1 is a block flow diagram of a method for providing an ore substrate for a flotation process in accordance with one or more embodiments.

[0007] FIG. 2 shows a simplified diagram of an extraction system in accordance with one or more embodiments.DETAILED DESCRIPTION

[0008] Traditional flotation processes that are designed to separate value metals, such as copper from nickel, copper from molybdenum, lead from zinc, among others, are imperfect where some of one value metal ends up in the same stream as the other value metals. When this happens, for example, the nickel in the copper concentrate eventually ends up as a waste product (e.g. in the tailings) and is lost rather than valorized. Additionally, during the flotation process a large amount of gangue remains trapped in the stream(s) including the value metal, which both impacts the flotation process and creates an issue in further downstream value metal processing and purification. As one of ordinary skill may appreciate, the term “gangue” as used herein refers to the material proximate to or in which ore is found having relatively little value as compared to the ore. A method in accordance with the present disclosure may include solubilization of select metals and / or impurities (e.g., non-metal components) from an ore material. In some embodiments, the selectivePATENT APPLICATION ATTORNEY DOCKET NO. 19148-013WO1solubilization of gangue and / or impurities from ore materials may support carbon sequestration.

[0009] During polymetallic separation in flotation processes for two or more metals, at least one of the value metals is floated, and at least one of the value metals is depressed. The challenge with conventional methods for this separation lies in that the flotation collector used for the bulk flotation floats some portion of both value metals (e.g., a metal for which depressing is desired as well as a floated metal of value). As such, during conventional operations, both value metals are passed to a separation stage, where a depressant that is specific to one of the value metals is necessarily added. The addition of the depressant is performed such that one of the two metals floats and one does not (i.e., is “depressed”). Advantageously, a biosolvent pre-treatment (e.g., a “pre-flotation” and / or an “in-between flotation leach”) in accordance with one or more embodiments, removes at least a portion of a flotation reagent (e.g., flotation collector) from a prior process such that the addition of the depressant in a subsequent separation stage (e.g., subsequent flotation process) is significantly reduced or not necessary. One or more embodiments herein may achieve the same, if not improved separation between metals of value with a biosolvent pre-treatment as described herein.

[0010] One or more embodiments herein are directed to the removal of gangue and / or impurity elements earlier in the ore enrichment process to enhance the separation and recovery efficiency between metals of value during a flotation process. Advantageously, one or more embodiments may allow for the improved separation and recovery of value metals during a flotation process. Non-limiting examples of value metals that can be separated and recovered include nickel and copper, copper and molybdenum, zinc and lead, or zinc and lead and copper, where one metal of value may be floated, and the remaining metal(s) of value is depressed during the flotation process. For example, one or more embodiments herein may allow for the improved separation and recovery of molybdenum, copper, and nickel as compared to traditional flotation processes without a pre-treatment.

[0011] Embodiments herein advantageously allow for less mass passing through to value metal upgrading and purification steps, such as flotation steps. The removal of gangue canPATENT APPLICATION ATTORNEY DOCKET NO. 19148-013WO1also reduce the amount of value metal(s) that is present in the resultant tailings stream produced from a flotation process. As used herein, the term “value metal” and “metal of value” refer to a metal that is used in a technological application, including but not limited to an electrification technology such as fuels electronic material applications, batteries, among others. A “value metal” and “metal of value” in accordance with one or more embodiments herein may refer to a metal selected from the group consisting of nickel (Ni), lithium (Li), copper (Cu), molybdenum (Mo), cobalt (Co), zinc (Zn), lead (Pb), rare earth metals, among others.

[0012] One or more embodiments of the present disclosure are directed to compositions, systems, and methods for enrichment of ore material. For example, in one or more embodiments, a method may include selectively removing one or more components (e.g., gangue and impurities) to improve ore grade prior to or during a flotation process. As one of ordinary skill may appreciate, the term “gangue” as used herein refers to the material proximate to or in which ore is found having relatively little value as compared to the ore material.

[0013] A method in accordance with the present disclosure may include solubilization of select metals and / or impurities (e.g., non-metal components) from an ore material. A method may include introducing solid ore material and a liquid extraction composition (e.g., a liquid biosolvent) to a container or system for an agitated leach. The selective solubilization of such embodiments is achieved while keeping a metal of value in the solid ore material, thereby enriching the metal of value in the enriched ore material.

[0014] As disclosed herein, selective solubilization of impurities and / or gangue from mining materials may be applied prior to flotation (i.e., “pre-flotation”) and / or in-between flotation steps (i.e. an “in-between leach”) to improve the selectivity of value metal separation during the concentration process. This solubilization is achieved while retaining most of the value metals in the solid ore material. This selective solubilization is achieved by contacting the extraction composition with the pre-flotation material or flotation concentrate in an agitated leaching tank under specific conditions that allow leaching of the impurities while retaining the value metals in solid form. Solids and liquids are thenPATENT APPLICATION ATTORNEY DOCKET NO. 19148-013WO1separated. Advantageously, the pre-flotation and / or in-between leach may remove (e.g., desorb, solubilize, and / or degrade) residual flotation reagents used in an upstream process and included in the solid ore material. As such, the surface chemistry of particles of the solid ore material may bealtered through this mechanism and / or other impurity removal such that a subsequent treatment (e.g., the subsequent flotation stage) including a subsequent component (e.g., a cleaner and / or scavenger) improves the performance of the subsequent flotation stage. Such an improvement may be relative to a subsequent flotation on an ore material that did not undergo a pre-flotation and / or in-between leach.

[0015] A leachate with solubilized gangue material can be separated from the enriched solids including the metal of value. In some embodiments, enriching the solids including the metals of value includes desorbing and / or degrading a flotation reagent present on the solid ore material. In such embodiments, the flotation reagent can include or is a flotation collector.

[0016] The impurities may be removed from the solution to regenerate an extraction composition (e.g., a biosolvent), which can be reused with untreated ore materials. In some embodiments, the selective solubilization of metals and / or cations from ore materials may support carbon sequestration. The solubilized metals may be stripped from the leachate liquid using one of several methods, and the biosolvent is re-used in subsequent agitated leaches. Post biosolvent leaching, the solids may be fed to a subsequent flotation process, where the flotation efficiency is altered as compared to a solid ore material that has not been treated.

[0017] Organic acids, such as citric acid and mixtures of organic acids including gluconic and oxalic acid, have been used to solubilize certain atoms from ore materials. Previously, gluconic and oxalic acid were often found to solubilize iron atoms and / or non-targeted atoms, which decreases the value of the ore material in further downstream processes. However, advantageously, one or more embodiments of the present disclosure unexpectedly show selective removal of a phosphorous (P) component, a potassium (K) component, a calcium (Ca) component, a sodium (Na) component, a chromium (Cr) component, a magnesium (Mg) component, an aluminum (Al) component, a silicon (Si)PATENT APPLICATION ATTORNEY DOCKET NO. 19148-013WO1component, a fluorine (F) component, an iron (Fe) component, a Pb component, a Zn component, and / or a Mo component, relative to a metal of value in the solid ore material, which significantly improves the separation efficiency in a flotation process.

[0018] As used herein, the term “organic acid” may include an individual organic acid and / or mixtures of organic acids that are produced by microbes (e.g., in a biobroth), or organic acids from other biological sources (e.g., in a plant produced biobroth), or organic acids that are synthetically made. The “organic acid” as used throughout this disclosure can include a mixture of an organic acid and the respective conjugate base.

[0019] As used herein, the terms “biosolvent” and “biobroth” refer to a solution including inorganic and / or organic acids and their respective conjugate bases, one or more biobroths, ionic liquids, or any combination thereof. The biosolvent of one or more embodiments may be either derived biologically or synthetically and may or may not include silicase and / or other enzymes. The term “biobroth” may refer to a solution produced and obtained from a natural and / or engineered organic acid-producing microbe, such as via a fermentation process, a natural and / or engineered organic acid-producing plant, or combinations thereof. The organic acid-producing microbe may produce an organic acid or a mixture of organic acids. The organic acid-producing microbe may produce one or more organic acids and one or more components, such as primary metabolites, secondary metabolites, antibodies, salts, ions, organelles, cellular components, extracellular components, biomolecules (e.g., polysaccharides, proteins, enzymes, amino acids, nucleic acids, lipids, carbohydrates, among others), or any combination thereof. The term “engineered microbe” may be a microbe that has been altered, such as with genetic engineering, for example, to modulate acid or other biobroth component production.

[0020] The terms “biosolvent” and “biobroth” may refer to a complex mixture of components derived from an organism, such as a broth obtained from a culture of a microbe, such as a fungus. The complex mixture can include inorganic and / or organic acids and their respective conjugate bases, ionic liquids, amino acids, cellular components derived from a microbe, extracellular components derived from a microbe, or any combination thereof. For example, the biobroth can include one or more enzymes, such asPATENT APPLICATION ATTORNEY DOCKET NO. 19148-013WO1silicase. The biobroth of one or more embodiments may be obtained from an Aspergillus spp. culture, such as a supernatant, a cell lysate, or combinations thereof. The natural and / or engineered microbe may include, but is not limited to, a microorganism of a genus selected from the group consisting of Aspergillus, Acetobacter, Bacillus, Propionibacterium, Corynebacterium, Rhizopus, Clostridium, Fusobacterium, Pseudomonas, Bifidobacterium, Saccharomyces, Enterobacter, Escherichia (e.g., Escherichia coli), and combinations thereof.

[0021] As used herein, the term “inorganic acid” may be an acid that is derived from an inorganic compound. The inorganic acid of one or more embodiments may include a protic acid.

[0022] As used herein, the term “gangue” refers to the impurity material that surrounds or is closely mixed with a wanted mineral in an ore deposit. Although termed “impurities” it is understood that value can be obtained from certain elements in the gangue, and that such elements are impurities with respect to the wanted material in the ore deposit.

[0023] As used herein, the term “flotation reagent” refers to a chemical that alters the surface of minerals (e.g., metallic minerals). For example, a flotation that hydrophobically alters the surface of particles during flotation may be a “flotation collector.” In another example, a flotation reagent that depresses particles during flotation may be a “depressant.” Non-limiting examples of a flotation reagent may include xanthates (e.g., potassium amyl xanthate (PAX), sodium isopropyl xanthate (SIPX), sodium ethyl xanthate (SEX)), dithiophosphates, dithiocarbamates, thionocarbamates, fatty acids, hydroxamates, frothers (such as methyl isobutyl carbinol (MIBC), polyglycols, pine oil, alcohols), depressants (such as carboxymethyl cellulose (CMC), dextrin, lime, cyanide, and sulfide-based depressants), activators (such as copper sulfate), pH modifiers as adsorbed to the solids of an ore material, any degradation products thereof, and any combinations thereof.

[0024] As used herein, the terms “load” or “leach” refers to the process of transferring one or more components from a first material to a second material. For example, the process of “loading” or “leaching” may include transferring one or more components from an ore material to an extraction composition in accordance with one or more embodiments.PATENT APPLICATION ATTORNEY DOCKET NO. 19148-013WO1

[0025] As used herein, the terms “strip” or “separate” refers to the removal of a first component (e.g., an impurity component, a biobroth, a biosolvent, an organic acid, etc.) from a second component (e.g., a mixture, solution, ore material, etc.).

[0026] As used herein, the terms “recycle” or “regenerate” refers to the recovery of a material (e.g., a component of an extraction composition, an extraction composition, or both such that the material may be reused in subsequent processes.

[0027] EXTRACTION COMPOSITION

[0028] In one aspect, embodiments herein relate to an extraction composition. In another aspect, embodiments herein relate to an extraction mixture including an extraction composition and an ore material. The extraction mixture may be a slurry including the extraction composition and the ore material. In one or more embodiments, the extraction composition includes one or more biobroths, one or more organic acids, or any combination thereof. In one or more embodiments, the extraction composition is a biosolvent or a biobroth. In one or more embodiments, the extraction composition includes at least one organic acid. As used herein, the term “extraction composition” may refer to solution including one or more components selected from the group consisting of biosolvents, biobroths, inorganic acids, and organic acids at selected concentrations and selected pH.

[0029] The extraction composition may be configured to selectively leach one or more components from an ore material. In one or more embodiments, the extraction composition is configured to remove one or more impurity components, which may include a residual flotation reagent (e.g., a flotation collector as previously described), gangue, one or more metals, and / or non-metallic atoms of value, from an ore material. In a non-limiting example, the extraction composition may be configured to extract one or more of a K component, a Mg component, an Al component, an Fe component, a Si component, a Mo component, a F component, a P component or any combination thereof from an ore material, such as an Fe ore material, a Cu ore material, a Li ore material, a Zn ore material, a Pb ore material, or a Ni ore material. In some embodiments, the extraction composition is configured to selectively extract one component with another component being solubilized to a lesser extent. For example, the extraction composition may be configuredPATENT APPLICATION ATTORNEY DOCKET NO. 19148-013WO1to selectively extract an Mg component with an Fe component being solubilized to a lesser extent from an ore material, such as a Ni-containing ore material or a Cu-containing ore material.

[0030] The extraction composition may include an aqueous solution. The aqueous solution includes water. The water may include, but is not limited to, Milli-Q water, distilled water, deionized water, tap water, fresh water from surface or subsurface sources, formation water, natural and synthetic brines, brackish water, natural and synthetic sea water, potable water, non-potable water, process water, other waters, and combinations thereof, that are suitable for use for treating a an ore material. As used herein, “Milli-Q water” is water purified using a Millipore Milli-Q laboratory water system. In one or more embodiments, the basic Milli-Q water meets ASTM Type I standards, having greater than 18.0 MegaOhms* centimeter (MQ*cm) resistivity at 25EC due to ions, less than 10 parts per billion (ppb) organics, less than 0.03 endotoxin per milliliter (EU / mL) of pyrogens, less than 1 particulate per mb (pariculate / mL), less than 10 ppb silica, and less than 1 bacterial colony forming unit per mL (cfu / mL).

[0031] In one or more embodiments, the water used can naturally contain contaminants, such as salts, ions, minerals, organics, and combinations thereof, as long as the contaminants do not interfere with extraction of target metal atoms and / or impurity components from an ore material. In one or more embodiments, one or more additives may be added to the extraction composition to enhance the selectivity for one or more components, efficiency for removing the one or more components, or combinations thereof.

[0032] In one or more embodiments, the aqueous solution includes a first organic acid, an optional additional organic acid, and an optional inorganic acid. The extraction composition may include one or more organic acids, one or more inorganic acids, one or more ionic liquids or mixtures thereof. The extraction composition may include at least two selected from organic acids, inorganic acids, or mixtures thereof. For example, the extraction composition may include a plurality of organic acids. The extraction composition may include three or more organic acids, four or more organic acids, five orPATENT APPLICATION ATTORNEY DOCKET NO. 19148-013WO1more organic acids, six or more organic acids, eight or more organic acids, or ten or more organic acids.

[0033] The extraction composition may include a first organic acid. The first organic acid may include, but is not limited to, an acid selected from the group consisting of gluconic acid, glutamic acid, oxalic acid, citric acid, malic acid, lactic acid, acetic acid, malic acid, tartaric acid, itaconic acid, hydroxypropionic acid, phthalic acid, tartaric acid, hexadecenoic acid, heptadecanoic acid, gallic acid, aspartic acid, succinic acid, oleic acid, tannic acid, palmitic acid, ascorbic acid, and combinations thereof. In some embodiments, when the first organic acid includes two or more organic acids, a main organic acid component may be present as compared to a minor organic acid component.

[0034] As a non-limiting example, the first organic acid may include oxalic acid as a main component and gluconic acid as a minor component. In one or more embodiments, the first organic acid includes gluconic acid as a main component and oxalic acid as a minor component. The first organic acid may include citric acid as a main component and malic acid as a minor component. The first organic acid may include malic acid as a main component and citric acid as a minor component. The first organic acid may be, but is not limited to, citric acid, malic acid, gluconic acid, or oxalic acid.

[0035] In some embodiments, the first organic acid, the optional additional organic acid(s), or both are synthetically produced, such as in a laboratory. In some embodiments, the first organic acid, the optional additional organic acid, or both are naturally occurring such that at least a portion of the aqueous solution may be or may be a biobroth and / or may be obtained and / or isolated from a biobroth. In one or more embodiments, the biosolvent includes purified (e.g., purified individual organic acids and / or purified mixtures of organic acids) or mixtures of unpurified organic acids. The biosolvent of one or more embodiments may be used with a single or mixtures of inorganic acids.

[0036] In one or more embodiments, the first organic acid is present in the aqueous solution in a concentration in a range between 0.01 M (Molar) to 4 M. For example, the concentration of the first organic acid may be in a range having a lower limit of any one of a non-zero value, 0.010 M, 0.015 M, 0.020 M, 0.025 M, 0.05 M, 0.075 M, 0.09 M, 0.10PATENT APPLICATION ATTORNEY DOCKET NO. 19148-013WO1M, 0.125 M, 0.150 M, 0.250 M, 0.5 M, 0.6 M, 0.8 M, 0.9 M, 1 M, 1.5 M, 2M, 2.5 M, 3M, 3.5 M, and 3.9 M and an upper limit of any one of 0.05 M, 0.075 M, 0.09 M, 0.10 M, 0.125 M, 0.150 M, 0.250 M, 0.5 M, 0.6 M, 0.7 M, 0.8 M, 0.9 M, 1.0 M, 1.1 M, 1.2 M, 1.5 M, 2 M, 2.5 M, 3 M, 3.5 M, 3.9 M, 3.95 M, and 4 M, where any lower limit can be paired with any mathematically compatible upper limit. As a non-limiting example, the concentration of the first organic acid may be present in a biosolvent at a concentration in a range from a non-zero value to 2.5 M, such as 0.05 M to 2.5 M.

[0037] The extraction composition may include one or more organic acids in a weight to volume percent (% (w / v)) in a range having a lower limit of any one of 0 % (w / v), 5 % (w / v), 10 % (w / v), 15 % (w / v), 20 % (w / v), 25 % (w / v), 30 % (w / v), 35 % (w / v), 40 % (w / v), 45 % (w / v), 50 % (w / v), 55 % (w / v), 60 % (w / v), 65 % (w / v), 70 % (w / v), and 75 % (w / v) and an upper limit of any one of 20 % (w / v), 25 % (w / v), 30 % (w / v), 35 % (w / v), 40 % (w / v), 45 % (w / v), 50 % (w / v), 55 % (w / v), 60 % (w / v), 65 % (w / v), 70 % (w / v), 75 % (w / v), 80 % (w / v), 85 % (w / v), 90% (w / v), 95 % (w / v), 98 % (w / v), 99 % (w / v), and 100 % (w / v), where any lower limit can be paired with any mathematically compatible upper limit.

[0038] The additional organic acid may include one or more organic acids, two or more organic acids, or a plurality of organic acids. In some embodiments, when the additional organic acid includes two or more organic acids, a main organic acid component may be present as compared to a minor organic acid component. The additional organic acid may include, but is not limited to, an acid selected from the group consisting of citric acid, malic acid, formic acid, lactic acid, acetic acid, itaconic acid, tartaric acid, hydroxypropionic acid, phthalic acid, tartaric acid, hexadecenoic acid, heptadecanoic acid, gallic acid, aspartic acid, succinic acid, oleic acid, tannic acid, palmitic acid, ascorbic acid, and combinations thereof.

[0039] In one or more embodiments, when the first organic acid is, or includes as a main component, oxalic acid, the additional organic acid comprises an acid selected from the group consisting of gluconic acid, oxalic acid, lactic acid, acetic acid, malic acid, citric acid hydroxypropionic acid, phthalic acid, tartaric acid, itaconic acid, hexadecenoic acid,PATENT APPLICATION ATTORNEY DOCKET NO. 19148-013WO1heptadecanoic acid, gallic acid, aspartic acid, succinic acid, oleic acid, tannic acid, palmitic acid, ascorbic acid, and combinations thereof. In a non-limiting example, when the first organic acid is, or includes as the main component, gluconic acid, the additional organic acid may include, but is not limited to, an acid selected from the group consisting of malic acid, oxalic acid, lactic acid, acetic acid, citric acid, hydroxypropionic acid, phthalic acid, tartaric acid, itaconic acid, hexadecenoic acid, heptadecanoic acid, ascorbic acid and combinations thereof. In one or more embodiments, when the first organic acid is, or includes as a main component, citric acid, the additional organic acid comprises an acid selected from the group consisting of gluconic acid, oxalic acid, lactic acid, acetic acid, malic acid, hydroxypropionic acid, phthalic acid, tartaric acid, itaconic acid, hexadecenoic acid, heptadecanoic acid, gallic acid, aspartic acid, succinic acid, oleic acid, tannic acid, palmitic acid, ascorbic acid and combinations thereof. In one or more embodiments, when the first organic acid is, or includes as a main component, malic acid, the additional organic acid comprises an acid selected from the group consisting of citric acid, gluconic acid, oxalic acid, lactic acid, acetic acid, malic acid, hydroxypropionic acid, phthalic acid, tartaric acid, itaconic acid, hexadecenoic acid, heptadecanoic acid, gallic acid, aspartic acid, succinic acid, oleic acid, tannic acid, palmitic acid, ascorbic acid and combinations thereof.

[0040] In one or more embodiments, the additional organic acid is present in the aqueous solution in a concentration in a range between 0 M to 3.0 M. For example, the concentration of the first organic acid may be in a range having a lower limit of any one of 0 M, a nonzero value, 0.005 M, 0.010 M, 0.015 M, 0.020 M, 0.025 M, 0.05 M, 0.075 M, 0.09 M, 0.10 M, 0.125 M, 0.150 M, 0.250 M, 0.5 M, 0.6 M, 0.8 M, and 0.9 M and an upper limit of any one of 0.05 M, 0.075 M, 0.09 M, 0.10 M, 0.125 M, 0.150 M, 0.250 M, 0.5 M, 0.6 M, 0.7 M, 0.8 M, 0.9 M, 1.0 M, 1.1 M, 1.5 M, 2.0 M, 2.1 M, 2.2 M, 2.5 M, 2.75 M, 2.9 M, and 3.0 M where any lower limit can be paired with any mathematically compatible upper limit.

[0041] In some embodiments, a ratio of the first organic acid to the additional organic acid is a concentration ratio in a range from 1 :0 to 1 : less than or equal to (<) 1. In one or more embodiments, the concentration ratio of the first organic acid to the additional organic acid is in a range having a lower limit of any one of 1:0, 1:0.05, 1:0.1, 1:0.2, 1:0.3, 1:0.4, 1:0.5,PATENT APPLICATION ATTORNEY DOCKET NO. 19148-013WO1and 1:0.75, and an upper limit of any one of 1:0.1, 1:0.2, 1:0.3, 1:0.4, 1:0.5, 1: 0.6, 1:0.7, 1:0.75, 1:0.8, 1:0.85, 1:0.9, 1:0.95, 1:0.99, and 1:1, where any lower limit can be paired with any mathematically compatible upper limit.

[0042] In one or more embodiments, the extraction composition includes an inorganic acid.The inorganic acid may include an acid selected from the group consisting of sulfuric acid, hydrochloric acid, nitric acid, phosphoric acid, and combinations thereof. The inorganic acid may be included in the aqueous fluid in an amount in a range from 0 M or a non-zero concentration to 3.0 M. For example, the concentration of the inorganic acid may be in a range having a lower limit of any one of 0 M, 0.005 M, 0.010 M, 0.015 M, 0.020 M, 0.025 M, 0.05 M, 0.075 M, 0.09 M, 0.10 M, 0.125 M, 0.150 M, 0.250 M, 0.5 M, 0.6 M, 0.8 M, and 0.9 M and an upper limit of any one of 0.05 M, 0.075 M, 0.09 M, 0.10 M, 0.125 M, 0.150 M, 0.250 M, 0.5 M, 0.6 M, 0.7 M, 0.8 M, 0.9 M, 1.0 M, 1.1 M, 1.5 M, 2.0 M, 2.1 M, 2.2 M, 2.5 M, 2.75 M, 2.9 M, and 3.0 M, where any lower limit can be paired with any mathematically compatible upper limit.

[0043] The extraction composition of one or more embodiments has a pH in a range from a non-zero value to 7. In some embodiments, the pH of the extraction composition is in a range having a lower limit of any one of a non-zero value, 0.05, 0.09, 0.10, 0.2, 0.25, 0.5, 0.75, 1, 1.2, 1.5, 1.7, 1.9, 2.0, 2.2, 2.5, 2.7, 2.9, 3.0, 3.2, 3.5, 3.7, 3.9, 4.0, 4.5, 5.0, and 6.0, and an upper limit of any one of 1, 1.2, 1.5, 1.7, 1.9, 2.0, 2.2, 2.5, 2.7, 2.9, 3.0, 3.2, 3.5, 3.7, 3.9, 4.0, 4.2, 4.5, 4.7, 5.0, 5.2, 5.5, 6.0, 6.5, and 7.0, where any lower limit can be paired with any mathematically compatible upper limit. As a non-limiting example, a pH of an extraction composition may be in a range of 0.09 to 5.5, such as from 0.1 to 5.0.

[0044] METHOD FOR PROVIDING AN ORE SUBSTRATE FOR A FLOTATION PROCESS

[0045] In another aspect, embodiments herein relate to a method for providing an ore substrate for a flotation process. The ore substrate may be derived from an ore material, such as ore tailings, ore concentrate, waste rock, ore, a solids stream from a flotation process (e.g., solids fed into or present within a flotation circuit, which may be obtained from the beginning, middle, and / or end of a flotation circuit), or any combination thereof.PATENT APPLICATION ATTORNEY DOCKET NO. 19148-013WO1For example, the ore substrate may be an enriched ore material. A method for providing an ore substrate may be method 100 as shown in FIG. 1. In block 102, the method may include enriching a solid ore material via selective solubilization of an impurity component from the solid ore material with an extraction composition to produce an enriched ore material and a leachate. Enriching the solid ore material may include desorbing and / or degrading a flotation reagent present on the solid ore material. In such embodiments, the flotation reagent can include or is a flotation collector.

[0046] The ore material may include an ore concentrate, slurry (e.g., a slurry of an ore concentrate, tailings, gangue, ore, waste rock, etc.), ore, gangue, ore tailings, waste rock, among other ore materials. The ore material may be a polymetallic mining substrate. The method may include obtaining the ore material. The ore material may be obtained from a mining process, a purification process, a flotation process, other treatment processes, or any combination thereof. For example, when the ore material is obtained from a flotation process, the method may include obtaining solids from a flotation apparatus as a solids stream. The ore material may be obtained directly from the flotation process without further processing such that the ore material includes an additive used during the treatment process. In one or more embodiments, a water content of the solids stream may be reduced (e.g., via filtration, decantation, centrifugation, among other water removal techniques) to provide the solid ore material. In such embodiments, the method can include thickening the solids to provide the solid ore material for enrichment.

[0047] The method may include leaching an impurity from the ore material to retain a metal of value in the ore material. In one or more embodiments, the method includes providing an extraction composition and an ore material. The method may include selectively solubilizing an impurity component including a flotation reagent, a degradation product of a flotation reagent, one or more minerals, salt, or any combination thereof having P, K, F, Fe, Cr, Na, Ca, Mg, Al, Si, and / or Mo from an ore material into an extraction composition to form a leachate and an enriched ore material.

[0048] The method may include preparing the extraction composition by obtaining the first organic acid and, optionally, the additional organic acid, the inorganic acid, orPATENT APPLICATION ATTORNEY DOCKET NO. 19148-013WO1combinations thereof. One or more organic acids of the extraction composition may be obtained via synthetic laboratory procedures. The first organic acid, the additional organic acid, the inorganic acid, or combinations thereof may be microbially produced, plant produced, or both such that the first organic acid, the additional organic acid, the inorganic acid, or combinations thereof may be collected from a microbe, a plant, or both (e.g., in the form of a biobroth). In some embodiments, the first organic acid, the additional organic acid, the inorganic acid, or combinations thereof is collected from a plant extract, a microbial cell lysate, a microbial supernatant, or combinations thereof. One or more organic acids of the extraction composition may be purified.

[0049] The method may include forming a mixture including an extraction composition and an ore material. The extraction composition and the ore material may be as previously described herein. An extraction composition, an ore material, or both may be introduced (or added) to an extraction unit of an extraction zone, such as an agitated leaching tank of an extraction system. In some embodiments, the extraction zone is a laboratory extraction unit that is a container capable of being manually agitated or stirred for the extraction process. The extraction unit may be a container capable of being automatically agitated or stirred for the extraction process, such as with a control system in electrical connection with the extraction unit. In some embodiments, the method includes providing an extraction system capable of performing one or more leaching processes. The extraction system may include one or more flow lines, valves, pumps, storage tanks, an extraction zone including an extraction unit (e.g., one or more agitated leaching tanks), among one or more additional units known to those skilled in the art for mineral leaching. One or more components of the extraction system may be an add-on component capable of being incorporated to one or more industrial mining processes, such as a flotation process, a tailings collection process, among other value metal separations processes.

[0050] In some embodiments, the extraction zone includes a plurality of leaching tanks positioned in parallel or in series. In one or more embodiments, one or more leaching tanks of the plurality of leaching tanks are in fluid communication with a subsequent leaching tank of the plurality of leaching tanks. In some embodiments, plurality of leaching tanksPATENT APPLICATION ATTORNEY DOCKET NO. 19148-013WO1are positioned in a cross- or counter-current design, in locked cycle leaching, or combinations thereof.

[0051] The ore material may be added to the extraction zone in an amount in a range from 5 to 70 wt% based on the total weight of the extraction mixture. The ore material may be added to the extraction unit in an amount in a range having a lower limit of any one of 5 wt%, 7.5 wt%, 8 wt%, 10 wt%, 15 wt%, 20 wt%, 25 wt%, 30 wt %, 40 wt%, 45 wt%, 48 wt%, and 50 wt % and an upper limit of any one of 15 wt%, 20 wt%, 25 wt%, 30 wt %, 40 wt%, 45 wt%, 48 wt%, 50 wt%, 52 wt%, 55 wt%, 57 wt%, 60 wt%, 62 wt%, 65 wt%, 68 wt%, and 70 wt%, where any lower limit can be paired with any mathematically compatible upper limit.

[0052] The extraction composition may be added to the extraction unit in an amount in a range from 30 to 95 wt% based on the total weight of the extraction mixture. The extraction composition may be added to the extraction unit in an amount in a range having a lower limit of any one of 30 wt%, 35 wt%, 38 wt%, 40 wt%, 42 wt%, 45 wt%, 47.5 wt%, 48 wt%, 50 wt%, 55 wt%, 60 wt%, 65 wt%, 70 wt %, 70 wt%, 75 wt%, 78 wt%, and 80 wt % and an upper limit of any one of 55 wt%, 60 wt%, 65 wt%, 70 wt %, 75 wt %, 80 wt%, 85 wt%, 88 wt%, 90 wt%, 91 wt%, 92 wt%, 93 wt%, 94 wt%, and 95 wt%, where any lower limit can be paired with any mathematically compatible upper limit.

[0053] The mixture of the extraction composition and the ore material may be agitated in the extraction zone for a select period of time and / or at a select temperature. The mixture may be heated while agitating to promote the selective removal of one or more components from the ore material. Agitating the extraction mixture in the extraction zone may form a leachate (or a “liquid mixture”) including the organic acid, the magnesium component, and, optionally, one or more additional components extracted from the ore material. The extraction mixture may be agitated in the extraction unit for a select period of time in a range having a lower limit of any one of 0.1 hour (h), 0.25 h, 0.5 h, 1 h, 2 h, 3, h, 4 h, 5 h, 6 h, 8 h, 10 h, 12 h, 14 h, 16 h, 18 h, and 20 h, and an upper limit of any one of 4 h, 5 h, 6 h, 7 h, 8 h, 10 h, 12 h, 14 h, 16 h, 18 h, 20 h, 22 h, 24 h, and 26 h, where any lower limit can be paired with mathematically compatible upper limit. The mixture may be heatedPATENT APPLICATION ATTORNEY DOCKET NO. 19148-013WO1(e.g., in the extraction unit) at a select temperature in a range from 5 °C, 10 °C, 15 °C, 20 °C, 25 °C, 27 °C, 28 °C, 29 °C, 30 °C, 35 °C, 40 °C, 45 °C, 50 °C, 60 °C, 70 °C, 80 °C, 90 °C, 95 °C, and 99 °C and an upper limit of any one of 35 °C, 40 °C, 45 °C, 50 °C, 55 °C, 60 °C, 65 °C, 70 °C, 75 °C, 80 °C, 90 °C, 95 °C, 99 °C, 100 °C, and 105 °C, where any lower limit can be paired with any mathematically compatible upper limit. In a non-limiting example, the method may include adjusting a temperature of the extraction zone to a temperature in a range from 10 to 100 °C and performing the extraction zone for a period of time in a range from 0.25 to 24 hours.

[0054] During the agitating step, one or more components may be selectively transferred from the ore material to the extraction composition, thereby forming an extraction mixture including an enriched ore material and a leachate. The leachate of one or more embodiments includes the extraction composition and one or more components removed from the ore material that may include one or more selected from a P component, a Ca component, a K component, a Na component, a Mg component, an Fe component, a Si component, an Al component, a Mo component, a F component, among other components (e.g., a lesser amount of a copper and / or lithium component). In some embodiments, the one or more components can include a Fe component, and / or a lithium component as relatively minor components compared to the P, K, Fe, Ca, Na, Mg, Al, Mo, Si, and / or F components. In such embodiments, the method of extraction is selective for the P, K, Fe, Ca, Na, Mg, Al, Mo, Si, and / or F components removal from the ore material. While a quantity of Fe may also be solubilized by the extraction composition, advantageously, the extraction composition selectively solubilizes other elements such that iron is solubilized to a lesser extent.

[0055] The one or more components may include an impurity in the form of a mineral, an oxide, a salt, or any combination thereof. The K component may include one or more of a K mineral, elemental K, a K oxide, a K salt having a K cation, or any other form of K. The Ca component may include one or more of a Ca mineral, elemental Ca, a Ca oxide, a Ca salt having a Ca cation, or any other form of Ca. The Na component may include one or more of a Na mineral, a Na oxide, a Na salt having a Na cation, or any other form of Na. The Mg component may include one or more of a Mg mineral, elemental Mg, a Mg oxide,PATENT APPLICATION ATTORNEY DOCKET NO. 19148-013WO1a Mg salt having a Mg cation, or any other form of Mg. The Cr component may include one or more of a Cr mineral, elemental Cr, a Cr oxide, a Cr salt having a Cr cation, or any other form of Cr. The Al component may include one or more of an Al mineral, elemental Al, an Al oxide, an Al salt having an Al cation, or any other form of Al. The Mo component may include one or more of a Mo mineral, elemental Mo, a Mo oxide, a Mo salt having a Mo cation, or any other form of Mo. The Si component may include one or more of a Si mineral, elemental Si, a Si oxide, a Si salt, or any other form of Si. The Fe component may include one or more of a Fe mineral, elemental Fe, a Fe oxide, a Fe salt having a Fe cation, or any other form of Fe. The F component may include one or more of a fluoride ion, diatomic fluorine, or any other form of F. The P component may include one or more of a P ion, phosphorous oxide, or any other form of P. A Cu component may include a Cu mineral, elemental Cu, a Cu oxide, a Cu salt having a Cu cation, or any other form of Cu. A lithium component may include a lithium mineral, elemental lithium, a lithium oxide, a lithium salt having a lithium cation, or any other form of lithium.

[0056] The enriched ore material may have a reduced concentration of one or more impurity components (e.g., one or more components described previously herein) as compared to the untreated ore material, such as a percent of the one or more impurity component concentration(s) in the untreated ore material. A treated solid ore material may include a reduced content of a flotation reagent as compared to an untreated solid material. The treatment of the solid ore material may include desorbing and / or degrading a flotation reagent present on the solid ore material. In such embodiments, the flotation reagent can include or is a flotation collector. The method of one or more embodiments may reduce the one or more impurity components in an enriched ore material as compared to an untreated ore material by a relative percent. The relative percent of an impurity component reduced in an enriched ore material as compared to an untreated ore material may be in a range having a lower limit of any one of a non-zero value, 1 %, 2 %, 5 %, 10 %, 15 %, 20 %, 25 %, 30 %, 35 %, 40 %, 45 %, 50 %, 55 %, 60 %, 65 %, 70 %, 75 %, 80 %, 85 %, and 90 %, and an upper limit of any one of 10 %, 20 %, 25 %, 30 %, 35 %, 40 %, 45 %, 50 %, 55 %, 60 %, 65 %, 70 %, 75 %, 80 %, 85 %, 90 %, 95 %, 98 %, 99 %, 99.5 %, 99.8 %, 99.9 %,PATENT APPLICATION ATTORNEY DOCKET NO. 19148-013WO1and 100 % where any lower limit can be paired with any mathematically compatible upper limit.

[0057] The method of one or more embodiments may reduce the one or more impurity components in an ore material to provide a total mass loss of the impurity component of about 1 wt% to about 100 wt%. The reduced one or more components content in an ore material may be reduced by an amount in a range having a lower limit of any one of 1 wt%, 2.5 wt%, 5 wt%, 10 wt%, 15 wt%, 20 wt%, 25 wt%, 30 wt%, 35 wt%, 40 wt%, 45 wt%, 50 wt%, 55 wt%, 60 wt%, 65 wt%, 70 wt%, and 75 wt% and an upper limit of any one of 20 wt%, 25 wt%, 30 wt%, 35 wt%, 40 wt%, 45 wt%, 50 wt%, 55 wt%, 60 wt%, 65 wt%, 70 wt%, 75 wt%, 80 wt%, 85 wt%, 90 wt%, 95 wt%, and 100 wt%, where any lower limit can be paired with any mathematically compatible upper limit.

[0058] In one or more embodiments, the untreated ore material has one or more impurity component content in a range from 0.01 wt% to 85 wt%. The enriched ore material may have a concentration of one or more impurity components in a range having a lower limit of any one of 0.01 wt%, 0.05 wt%, 0.1 wt%, 0.25 wt%, 0.5 wt%, 1.0 wt%, 1.5 wt%, 2.0 wt%, 5 wt%, 10 wt%, 15 wt%, 20 wt%, 25 wt%, 30 wt%, 35 wt%, 40 wt%, 45 wt%, 50 wt%, 55 wt%, and 60 wt% and an upper limit of any one of 2.0 wt%, 5 wt%, 10 wt%, 15 wt%, 20 wt%, 25 wt%, 30 wt%, 35 wt%, 40 wt%, 45 wt%, 50 wt%, 55 wt%, 60 wt%, 65 wt%, 70 wt%, 75 wt%, 80 wt%, and 85 wt%, where any lower limit can be paired with any mathematically compatible upper limit.

[0059] In embodiments where an impurity is found in an ore material in a relatively low amount (e.g., about 0.001 wt% to about 5 wt%) and reduces the overall financial value of the ore material such impurities may be referred to as penalty elements (or “penalty components”), which may be considered non-applicable for further processing. In embodiments described herein, all penalties are impurities but not all impurities are penalties. These penalty elements may render an ore material unsuitable for further use. Some non-limiting examples of penalty elements include one or more of Na, Cr, Ca, K, Mg, Mo, F, P, S, Si, As, Fe, among others. In embodiments in which penalty elements are present in a relatively low amounts in the ore material, the method may advantageouslyPATENT APPLICATION ATTORNEY DOCKET NO. 19148-013WO1remove one or more impurity components in a relative percentage of 20 % or more, 30 % more more, 40 % or more, 50% or more, 60 % or more, 70 % or more from the ore material. In embodiments where the ore material is or includes gangue, the method may advantageously increase the value of the ore material via removal of the penalty element while maintaining a relatively large percentage of gangue (e.g., 95 %).

[0060] In one or more embodiments, the untreated ore material has one or more impurity component content in a range from 0.001 wt% to 99.999 wt%. The enriched ore material may have a concentration of one or more impurity components in a range having a lower limit of any one of 0.001 wt%, 0.01 wt%, 0.05 wt%, 0.1 wt%, 0.25 wt%, 0.5 wt%, 1.0 wt%, 1.5 wt%, 2.0 wt%, 5 wt%, 10 wt%, 15 wt%, 20 wt%, 25 wt%, 30 wt%, 35 wt%, 40 wt%, 45 wt%, 50 wt%, 55 wt%, and 60 wt% and an upper limit of any one of 2.0 wt%, 5 wt%, 10 wt%, 15 wt%, 20 wt%, 25 wt%, 30 wt%, 35 wt%, 40 wt%, 45 wt%, 50 wt%, 55 wt%, 60 wt%, 65 wt%, 70 wt%, 75 wt%, 80 wt%, 85 wt%, 90 wt%, 92.5 wt%, 95 wt%, 97.5 wt%, 99 wt%, 99.5 wt%, 99.9 wt%, 99.99 wt%, and 99.999 wt%, where any lower limit can be paired with any mathematically compatible upper limit.

[0061] In some embodiments, the enriched ore material has a reduced one or more impurity component content as compared to the untreated ore material. In one or more embodiments, the enriched ore material has a reduced impurity component content in a range from 0 wt% to 100 wt%. The enriched ore material may have a concentration of one or more impurities in a range having a lower limit of any one of 0 wt%, 0.01 wt%, 0.05 wt%, 0.1 wt%, 0.25 wt%, 0.5 wt%, 1.0 wt%, 1.5 wt%, 2.0 wt%, 5 wt%, 10 wt%, 15 wt%, 20 wt%, 25 wt%, 30 wt%, 35 wt%, 40 wt%, 45 wt%, 50 wt%, 55 wt%, and 60 wt% and an upper limit of any one of 2.0 wt%, 5 wt%, 10 wt%, 15 wt%, 20 wt%, 25 wt%, 30 wt%, 35 wt%, 40 wt%, 45 wt%, 50 wt%, 55 wt%, 60 wt%, 65 wt%, 70 wt%, 75 wt%, 80 wt%, 85 wt%, 90 wt%, 92.5 wt%, 95 wt%, 96 wt%, 97 wt%, 98 wt%, 99 wt%, 99.95 wt%, 99.99, and 100 wt%, where any lower limit can be paired with any mathematically compatible upper limit. As a nonlimiting example, the reduced one or more impurity component concentration in the enriched ore material may be in a range from 0 to 95 wt%. In one or more embodiments, the amount of impurity components in an enriched ore material is less than 98 wt%, less than 95 wt%, less than 90 wt%, 85 wt%, less than 80 wt%, less than 75 wt%, less than 50PATENT APPLICATION ATTORNEY DOCKET NO. 19148-013WO1wt%, less than 25 wt%, or less than 10 wt%. In some embodiments, the ore material is upgraded by the selective removal of one or more of K, Ca, Na, Cr, Mg, Al, F, S, P, Si, Mo, while retaining metals of value in the solid ore material.

[0062] A method of one or more embodiments may include separating an enriched ore material from the leachate or vice versa as shown in block 104 of FIG. 1. In one or more embodiments, the leachate is removed to collect the leachate and the enriched ore material. The enriched ore material may be in the form of a solid such that the separation of the enriched ore material from the leachate can be performed by a method for separating solids from liquids known to those skilled in the art. In some embodiments, the separation includes decanting, , filtration, membrane filtration, gravity filtration, centrifugation, among others known to those skilled in the art. The separated enriched ore material may be washed and dried. In some embodiments, the separated treated ore is transferred for further processing.

[0063] The separation of the one or more components described previously, and if present, one or more additional metallic components from the leachate may be performed such that the extraction composition is regenerated. The leachate may be fed to a processing unit to regenerate the extraction composition. In some embodiments, separating the one or more components from the leachate includes extracting the one or more components from the leachate with one or more water treatment techniques. The extraction of the one or more components from the leachate may include performing one or more water treatment techniques selected from the group consisting of feeding the leachate through an ion exchange system, extracting the impurity component via solvent extraction, chromatography, filtration, nanofiltration, membrane filtration, osmotic separation (e.g., via reverse osmosis), using adsorption and / or absorption materials, precipitation including, but not limited to pH control and precipitation, precipitation via ion addition such as phosphate addition, sulfate addition, among other precipitation techniques known to those skilled in the art, and combinations thereof. The water treatment technique may include introducing the leachate to an ion exchange column, solvent extraction (e.g., biphasic solvent extraction), or both.PATENT APPLICATION ATTORNEY DOCKET NO. 19148-013WO1

[0064] The biosolvent, the biobroth, one or more components of the biosolvent and / or the biobroth (e.g., an organic acid), one or more metals of value, or combinations thereof may be separated from the leachate via feeding the leachate to a system configured to perform chromatography, filtration, nanofiltration, membrane filtration, osmotic separation (e.g. via reverse osmosis), using adsorption and / or absorption materials, solvent extraction, ion exchange chromatography, solvent extraction, simulated moving bed reactors (SMB), electrodeionization (EDI), centrifugation, precipitation including, but not limited to pH control and precipitation, precipitation via ion addition such as phosphate addition, sulfate addition, among other precipitation techniques known to those skilled in the art , decantation, and combinations thereof.

[0065] In one or more embodiments, one or more metals of value are removed from the leachate via the one or more water treatment techniques. In one or more embodiments, a value metal component is selectively removed from the leachate, the extraction mixture, or both. As a non-limiting example, the value metal component may be removed (e.g., via electrowinning or other extraction methods) and recovered for further processing of an enriched solid ore concentrate. In a non-limiting example, the extracted value metal component may be added to the enriched ore material recovered from the extraction mixture. Advantageously, one or more embodiment methods may allow for a reduced or minimal loss of value metal from a solid ore material even if relatively low amounts leach into the leachate.

[0066] In some embodiments, separating the extraction composition or one or more components of the extraction composition includes extracting the extraction composition or one or more components of the extraction composition from the extraction mixture, the leachate, or both. The extraction may be performed with one or more water treatments techniques selected from a group consisting of centrifugation, feeding the leachate through an ion exchange system, extracting the magnesium component via solvent extraction, chromatography, nanofiltration, filtration, membrane filtration, using adsorption and / or absorption materials, precipitation including, but not limited to pH control and precipitation, precipitation via ion addition such as phosphate addition, sulfate addition,PATENT APPLICATION ATTORNEY DOCKET NO. 19148-013WO1among other precipitation techniques known to those skilled in the art, and combinations thereof.

[0067] An organic acid component of the extraction composition, a biosolvent component of the extraction composition, a biobroth component of the extraction composition, or combinations thereof may be separated from the leachate and / or the extraction mixture and may subsequently be used to form a regenerated extraction composition. For example, at least a portion of an extraction composition may be separated from the extraction mixture, the leachate, or combinations thereof by precipitation including, but not limited to, pH control, precipitation via ion addition (e.g., cation addition such as via the addition of organic cations to the extracted solution), among other precipitation techniques known to those skilled in the art, chromatography, electrodeionization (EDI), ion exchange, or filtration. After this, the extracted portion may be recovered as a solid precipitate, in an aqueous solution, or both.

[0068] The regenerated extraction composition may be recovered and reused for subsequent extractions. For example, when the extracted portion is recovered as a solid precipitate, the precipitate may be redissolved to form the regenerated extraction composition. In some embodiments, the method includes repeating the extracting, such as with the regenerated extraction composition. In some embodiments, the regenerated extraction composition can be modified after recovery and prior to the repeating the extraction to add an organic acid, an inorganic acid or both, dilute the extraction composition, adjust a pH of the extraction composition (e.g., with a pH adjusting agent that does not interfere with the extraction process), or any combination thereof. The regenerated extraction composition may be transported (i.e., introduced) to the extraction zone, such that the regenerated extraction composition is recycled.

[0069] In one or more embodiments, the method includes altering the extraction composition to alter the selective solubilization of an impurity element. Altering the extraction composition may include selecting the first organic acid and / or a main component of the extraction composition based on the impurity to be removed. As a non-PATENT APPLICATION ATTORNEY DOCKET NO. 19148-013WO1limiting example, if F component solubilization is desired, then citric acid or lactic acid may be selected as a first organic acid or a main component.

[0070] The method may include altering the extraction composition based on the ore material composition. For example, altering the extraction composition may include selecting the first organic acid and / or a main component of the extraction composition based on the value metal in the solid ore material. A biobroth may be prepared to selectively retain the value metal in the ore material. In a non-limiting example, if the ore material is or includes Ni (e.g., as a nickel sulfide ore material), then lactic acid, tartaric acid, or combinations thereof may be selected as a first organic acid or a main component.

[0071] A simplified diagram of a non-limiting extraction process and recycling process may be as shown in FIG. 2. As shown in system 200 of FIG. 2 an ore material, an extraction composition, or both may be introduced to extraction zone 202 via feed line 201. A leachate may be introduced to component recovery zone 204 via input line 203 A. A treated metal ore material may be recovered from extraction zone 202 via output line 203B. The enriched ore material may be analyzed, such as weighed to determine a total mass difference from the untreated ore material. The component recovery zone 204 may include a component to selectively remove one or more of Na, Cr, Ca, K, P, Mg, Mo, Al, F, Si, Fe, and Cu, among other metal atoms (e.g., via line 205B) from the leachate such that the extraction composition is regenerated. In one or more embodiments, F may be removed from a Si- containing mineral or ore material.

[0072] One or more impurity components may be separated (or “stripped”) from the leachate along with one or more additional metal components (e.g., an Fe component, a Ni component, a Co component, among others) such that the extraction composition and a mixture of metallic components may be recovered. In one or more embodiments, each of the Na, Cr, Ca, K, P, Mg, Mo, Fe, Al, Si, and / or F components and, if present, one or more additional metallic components are recovered separately from the leachate as recovered components. In some embodiments, the recovered component has a purity in a range from 5% or greater, 10% or greater, 25% or greater, or 50% or greater. The recovered component may have a purity in a range from 5% to 100%. For example, the recovered componentPATENT APPLICATION ATTORNEY DOCKET NO. 19148-013WO1may have a purity in a range having a lower limit of any one of 1%, 5%, 7.5%, 10%, 15%, 20%, 25%, 30%, 35%, 40%, and 50%, and an upper limit of any one of 30%, 35%, 40%, 45%, 50%, 55%, 60%, 65%, 70%, 75%, 80%, 85%, 90%, 95%, 98%, 99%, 99.9%, 99.99%, and 100%, where any lower limit can be paired with any mathematically compatible upper limit.

[0073] The regenerated extraction composition may be fed to one or more extraction units of the extraction zone, such as via one or more flow lines (e.g., line 205A) in fluid communication with the metal atom recovery zone 204 and the extraction zone 202. In some embodiments, the regenerated extraction composition is transported to a storage tank to be used in a subsequent extraction process, for example. In some embodiments, it may be determined via analysis of the extraction composition, recovery efficiency of one or more metal atoms, or both, that the regenerated extraction composition requires additional components (e.g., one or more additional components of the extraction composition). The analysis may be performed with a method or system capable of measuring metal atoms in a solid sample (e.g., an ore material), a liquid sample (e.g., a leachate, a regenerated extraction composition), or both. Analysis of one or more embodiments may include determination of total mass loss of the untreated ore material, analysis of a sample (e.g., a leachate sample) with absorption spectroscopy, fluorescence spectroscopy, high performance liquid chromatography (HPLC), gas chromatography (GC), mass spectrometry (MS), Infrared Spectroscopy (IR), inductively coupled plasma - optical emission spectrometry (ICP-OES) of a solution, X-ray fluorescence (XRF) of a solid sample, X-ray Diffraction (XRD), Modal Mineralogy analysis (e.g., QEMSCAN® analysis), oxidation-reduction potential (ORP), pH, conductivity or combinations thereof.

[0074] A method of one or more embodiments may include providing a measurement system coupled to the extraction system to analyze one or more components of the extraction mixture, such as a regenerated extraction composition. The measurement system may include one or more components configured to perform the analytical methods including, but not limited to ICP-OES, absorption measurement, fluorescence measurements (e.g., excitation and / or emission), HPLC, IR, GC, MS, XRD, XRF, Modal Mineralogy (e.g., QEMSCAN®), ORP, pH, conductivity among others. The measurementPATENT APPLICATION ATTORNEY DOCKET NO. 19148-013WO1system may include various pumps, flow control components, a control system, among other components. The measurement system may be configured to collect a sample and analyze one or more components of the extraction mixture (e.g., a liquid sample of the extraction mixture) over set time intervals and time periods. In some embodiments, the analysis of a solid sample is performed at an off-site location after separation and collection from an extraction mixture.

[0075] In some embodiments, analysis of an extracted sample is carried out after each extraction in the extraction zone. Analysis of a regenerated extraction composition may be performed after processing through the metal atom recovery zone. In some embodiments, the extracted sample, the regenerated extraction solution, or both are continuously measured by one or more components of the extraction system. In some embodiments, the extraction system includes one or more sensors capable of collecting and / or transmitting data to a computer that may be a part of the extraction system or at an off-site location. In some embodiments, one or more parameters (e.g., recycled extraction composition makeup, temperature, pressure, residence time within the extraction zone, etc.) are adjusted based on the data collected from the analytical measurements.

[0076] In some embodiments, an extraction composition storage tank 206 can be present in system 200 such that one or more components of the extraction composition may be introduced to the regenerated extraction composition via line 207. For example, an extraction composition make-up may be introduced to the regenerated extraction composition to regenerate the concentration of the acid(s) in the extraction composition, to increase the concentration of the extraction composition, or to dilute the extraction composition. In such embodiments, the adjusting of the regenerated extraction composition via introduction of the make-up may maintain or increase the extraction efficiency of target metal component(s), enhance the selectivity of target metal component(s), or both.

[0077] Referring back to FIG. 1, a method 100 may include block 106 in which the enriched ore material is used as a substrate for a flotation process to produce a value stream including at least one metal of value. The enriched ore material may be introduced to a flotation apparatus, such as a flotation cell and / or a flotation circuit. An additive, such asPATENT APPLICATION ATTORNEY DOCKET NO. 19148-013WO1a flotation agent, a liquid, or both may be added to the enriched ore material to produce a flotation mixture in the flotation apparatus. A flotation collector may be added to the flotation process such that the flotation collector may be present or absent during the flotation process. Advantageously, the agitated leach pre-treatment in accordance with one or more embodiments may allow for a subsequent flotation process that does not require or significantly reduces the need for a flotation reagent (e.g., a depressant). The “significantly reduced” flotation reagent used in a subsequent flotation process may be used in an amount that is reduced by at least 1%, at least 5%, at least 10%, at least 15%, at least 20%, at least 25%, at least 30%, at least 35%, at least 40%, at least 45%, at least 50%, at least 55%, at least 60%, at least 65%, at least 70%, at least 75%, at least 80%, at least 85%, at least 90%, at least 95%, at least 99%, at least 99.9%, or 100% relative to a subsequent flotation process for which no pretreatment (e.g., a pre-flotation and / or inbetween) leach is performed.

[0078] Advantageously, a pre-flotation and / or in-between leach may remove (e.g., desorb, solubilize, and / or degrade) residual flotation reagents used in an upstream process and included in the solid ore material used for the leach. As such, the surface chemistry of particles of the solid ore materialmay be altered through this and / or other impurity removal such that a subsequent treatment (e.g., the subsequent flotation stage) including a subsequent component (e.g., a cleaner and / or scavenger) improves the performance of the subsequent flotation stage. Such an improvement may be considered relative to a subsequent flotation process of an ore material that did not undergo a pre-flotation and / or in-between leach.

[0079] In such embodiments, the flotation collector can be reduced or absent from the flotation process.

[0080] The flotation apparatus may be operated to separate the flotation mixture into a value stream and a waste stream. In one or more embodiments, when the value metal separation process is or includes a flotation process, at least one metal of value from the enriched ore may be floated, and one or more additional metal(s) of value present in the enriched ore is depressed during the flotation process. Flotation processes selectively floatPATENT APPLICATION ATTORNEY DOCKET NO. 19148-013WO1and depress certain minerals in the solid substrate, thereby separating the flotation mixture into the value and the waste stream. In one or more embodiments, the flotation process may produce a waste stream and value stream or two or more value streams. A stream that can be taken on to further processing of value products may refer to a “concentrate.” Another stream that goes to waste may be included in a “tailings” stream. The value stream of one or more embodiments may be a solids stream, such as a value metal concentrate.

[0081] The value stream may include at least 0.5 weight percent (wt. %) of a metal of value of the enriched ore material, at least 1 wt. % of a metal of value of the enriched ore material, at least 5 wt.% of a metal of value of the enriched ore material, at least 8 wt. % of a metal of value of the enriched ore material, at least 10 wt. % of a metal of value of the enriched ore material, at least 20 wt. % of a metal of value of the enriched ore material, at least 30 wt. % of a metal of value of the enriched ore material, at least 40 wt. % of a metal of value of the enriched ore material, at least 50 wt. % of a metal of value of the enriched ore material, at least 60 wt. % of a metal of value of the enriched ore material, at least 70 wt. % of a metal of value of the enriched ore material, at least 75 wt. % of a metal of value of the enriched ore material, at least 80 wt. % of a metal of value of the enriched ore material, at least 85 wt. % of a metal of value of the enriched ore material, at least 90 wt. % of a metal of value of the enriched ore material, at least 95 wt. % of a metal of value of the enriched ore material, or at least 98% of a metal of value of the enriched ore material.

[0082] In embodiments where at least two value streams are produced, the value streams may each include an enriched percentage of metal of value. The metal of value may be different in each of the two streams. A non-limiting example of two value streams obtained from a process may include a first stream that includes Cu (i.e., a Cu stream) and a second stream that includes Mo (i.e., a Mo stream). In another non-limiting example, two value streams obtained from a process may include a first stream that is a Cu stream and a second stream that includes tailings (i.e., a tailings stream).

[0083] Operating the flotation apparatus may include separating the value stream and the waste stream based on one or more parameters of the mixture, such as a difference in hydrophilicity of the components in the flotation mixture, by adjusting the water chemistryPATENT APPLICATION ATTORNEY DOCKET NO. 19148-013WO1(e.g., pH, ionic strength, among other properties) of the flotation mixture, and / or by adjusting ore particle size, among other properties that one of ordinary skill may understand can be adjusted to separate a value metal. The waste stream may include at least one impurity metal. When at least one impurity metal is included in the waste stream, the method may include collecting the waste stream and separating the at least one impurity metal from the waste stream. In some embodiments, the tailings in the waste stream can be recirculated to undergo a subsequent leaching process to produce an enriched ore material. In such embodiments, the subsequent leaching process may target the same or a different metal of value for ore material enrichment as compared to the prior leaching process.

[0084] In one or more embodiments, a process includes pretreating a solid ore material and / or a flotation concentrate with an extraction composition to remove at least a portion of a flotation collector present in the solid ore material and / or the flotation concentrate. In one or more embodiments, the pretreating comprises removing gangue from the solid ore material and / or the flotation concentrate with the extraction composition. The pretreating may produce a treated ore material and a leachate. A process of one or more embodiments may include one or more steps of a method (e.g., method 100 of FIG. 1) as described previously herein. The solid ore material and the extraction composition may be as described previously herein. The process may include subjecting the treated ore material to a flotation process for separating two or more value metals in the absence of a depressant or with a significantly reduced addition of the depressant to facilitate the separation of the two or more value metals.

[0085] In one or more embodiments, the pretreating of the solid ore material includes an agitated leach of the solid ore material and the extraction composition. The agitated leach may be performed at one or more conditions described previously herein. In some embodiments, the pretreatment includes enriching the solid ore material via selective solubilization of an impurity component from the solid ore material. At least a portion of the impurity component from the solid ore material is present in the leachate after the pretreatment. The impurity component may be as described previously.PATENT APPLICATION ATTORNEY DOCKET NO. 19148-013WO1

[0086] The treated ore material may be introduced into a flotation apparatus (e.g., a flotation cell and / or circuit). A flotation mixture including the treated ore material may be present in the flotation apparatus. One or more additives may be added to the flotation mixture. In one or more embodiments, a flotation collector is absent from the flotation mixture. In some embodiments, a flotation reagent (e.g., a flotation collector, a depressant, or both) is added to the flotation mixture. In some embodiments, a depressant is not necessary such that the depressant is absent from the flotation mixture. In one or more embodiments, a depressant added to the flotation process is relative to a subsequent flotation process for which no pretreatment (e.g., a pre-flotation and / or in-between) leach is performed.

[0087] A value stream may be recovered from the flotation process. The value stream may include a higher metal of value content as compared to a value stream obtained from a flotation process of the solid ore material without pre-treatment with the extraction composition. The flotation apparatus may be operated to produce a waste stream and a value stream from the flotation mixture. The value stream may be recovered. As described previously, the value stream may include a higher metal of value content as compared to a value stream obtained from a flotation process of the enriched ore material without treatment with the extraction composition.

[0088] In one or more embodiments, recovering the value stream includes recovering more than one value stream from the flotation process. For example, the process may include recovering a first value stream including a first metal of value; and recovering a second value stream including a second metal of value. The first value stream and the second value stream may each independently have a higher metal of value content relative to a flotation process performed without pre-treatment with the extraction composition.

[0089] The method of one or more embodiments may advantageously improve recovery of value metals from an ore material (e.g., an ore concentrate) as well as or better than traditional separation processes. The process of one or more embodiments may be cost- effective and can be adapted to equipment currently used in the mining industry. One or more embodiments of the present disclosure may advantageously improve the separationPATENT APPLICATION ATTORNEY DOCKET NO. 19148-013WO1efficiency of a flotation process as compared to traditional processes. Advantageously, altering the composition of the mining substrate (i.e., the ore material) pre-flotation or inbetween flotation steps through the use of an extraction composition, such as solutions that include biosolvents, leads to improved separation of value metals during the subsequent flotation process. For example, little to no value metal is dissolved during the leach to enrich the ore material, and the enriched solid mining substrate post-leach behaves differently in the flotation process as compared to an untreated mining substrate, where the enriched substrate demonstrates improved separation between at least two solids stream value metals that are separated in the process. Advantageously, one or more embodiments herein may reduce the cost of an overall separation process via flotation through the reduction and / or elimination of additives (e.g., a flotation reagent such as a depressant) in subsequent flotation steps. Additionally, one or more embodiments herein may improve safety conditions via the reduction and / or removal of a hazardous additive (e.g., a hazardous flotation reagent such as sodium hydrosulfide (NaSH)). One or more embodiments herein may improve value metal separation (e.g., between gangue and a metal of value and / or between two or more metals of value) from a flotation process by at least 1%, at least 5%, at least 8%, 10%, at least 20%, at least 30%, at least 40%, at least 50%, at least 60%, at least 70%, at least 80%, at least 90%, or at least 99% relative to a traditional flotation process.

[0090] EXAMPLES

[0091] The following examples are intended to demonstrate that multiple laboratory experiments were performed to highlight the selectivity for value metal separation from an enriched mining substrate after leaching with an extraction composition in accordance with one or more embodiments of the disclosure. These examples are not intended to limit the scope of the present disclosure.

[0092] Example 1 :

[0093] A nickel sulfide concentrate from in-between flotation steps was used as the substrate (Substrate 1) in this experiment. As the substrate was taken from in-between flotation steps, flotation chemicals are present on the substrate. In Condition 1 , 2 M LacticPATENT APPLICATION ATTORNEY DOCKET NO. 19148-013WO1acid was added to 20 wt% Substrate 1, and an agitated leach was run for 1 h at 70 °C. In Condition 2, 2 M Lactic acid was added to 20 wt% Substrate 1 and an agitated leach was run for 2 h at 70 °C. In Condition 3, 2 M Lactic acid was added to 20% wt Substrate 1, and an agitated leach was run for 3.5 h at 40 °C. In Condition 4, 2 M Tartaric acid was added to 20% wt Substrate 1, and an agitated leach was run for 2 h at 70 °C. In Condition 5, 2 M Tartaric acid was added to 40 °C Substrate 1, and an agitated leach was run for 4 h at 70 °C. Solids and liquids were separated following the experiment.

[0094] Post agitated leach and liquid / solid separation, the enriched solids were then run through flotation tests. In addition, an untreated Substrate 1 (Control) sample was also run through flotation tests using a Denver flow cell.

[0095] Flotation tests selectively float and depress certain minerals in the solid substrate, separating the solid substrate into two streams. The purpose of these flotation tests was to separate two value metals (Cu and Ni).

[0096] Table 1. Distribution of nickel and copper between the two solids material flotation streams. Distribution is calculated as a percentage, where 100% is the total Ni or Cu in the preflotation biosolvent treatment.Pre-flotation Post-Flotation% of total Ni % of total Cu Biosolvent Treatment StreamsUntreated Control Solid Stream 1 87 99 Untreated Control Solid Stream 2 13 1 Condition 1 Solid Stream 1 18 92 Condition 1 Solid Stream 2 82 8 Condition 2 Solid Stream 1 13 91 Condition 2 Solid Stream 2 87 9 Condition 3 Solid Stream 1 9 71 Condition 3 Solid Stream 2 91 29 Condition 4 Solid Stream 1 14 89 Condition 4 Solid Stream 2 86 11PATENT APPLICATION ATTORNEY DOCKET NO. 19148-013WO1Condition 5 Solid Stream 1 16 97 Condition 5 Solid Stream 2 84 3

[0097] For samples that had undergone the agitated leach treatments were determined to have better separation of the value metals Cu and Ni into their two respective streams. When Substrate 1 was not treated most of the Ni and Cu found in the substrate were present in solid stream 1. When the extraction compositions were used, most of the Cu was retained in stream 1, whereas the Ni went to stream 2.

[0098] Example 2:

[0099] Pre-flotation material from nickel sulfide substrate (Substrate 2) was used in this experiment. Substrate 2 underwent agitated leach tests under four different conditions. In Condition 1, 2 M Lactic acid was added to 20 wt% Substrate 2 and an agitated leach was run for 1 h at 70 °C. In Condition 2, 2 M Lactic acid was added to 20 wt% Substrate 2 and an agitated leach was run for 2 h at 70 °C. In Condition 3, 2M Lactic acid was added to 20 wt% Substrate 2 and an agitated leach was run for 2 h at 40 °C. In Condition 4, 2 M Lactic acid was added to 40 wt% substrate 2 and an agitated leach was run for 2 h at 70 °C. Solids and liquids were separated following the experiment.

[0100] Post agitated leach and liquid / solid separation, the solid samples were then run through flotation tests. In addition, an untreated Substrate 2 (Control) sample was also run through flotation tests using a Denver flow cell.

[0101] Table 2. Distribution of the nickel and copper in the flotation value versus the waste streams. For untreated material more of the Ni and Cu is lost to the waste stream (tailings). For the treated material a greater amount of the Ni and Cu is retained in the value stream.Pre-flotationBiosolventTreatement Post-Flotation Streams % of total Ni % of total Cu Untreated Value Stream 68.21 87.52 Untreated Waste Stream 31.79 12.48PATENT APPLICATION ATTORNEY DOCKET NO. 19148-013WO1Condition 1 Value Stream 92.72 93.37 Condition 1 Waste Stream 7.28 6.63 Condition 2 Value Stream 91.31 92.48 Condition 2 Waste Stream 8.69 7.52 Condition 3 Value Stream 92.47 94.34 Condition 3 Waste Stream 7.53 5.66 Condition 4 Value Stream 94.32 95.4 Condition 4 Waste Stream 5.68 4.6

[0102] As shown in Table 2, both metals of value were captured in the value stream when the substrate was treated with an extraction composition as compared to an untreated substrate.

[0103] Example 3 :

[0104] A nickel sulfide rougher feed from a different mining site as compared to Substrates 1 and 2 was used in this experiment as Substrate 3. Substrate 3 underwent agitated leach tests under two different conditions. In Condition 1, 1 M Lactic acid was added to 10 wt% Nickel sulfide rougher feed and an agitated leach was run for 6 hours at 70 °C. Solids and liquids were separated following the experiment. The agitated leaching treatment led to improvements in Nickel sulfide rougher feed grade, where impurities including Mg, Fe, K, and P were removed from the solids while retaining and upgrading the Ni and Cu in the solid form (Table 1).

[0105] Table 3. The enrichment ratio compares the % element in the treated solid materials of Conditions 1 and 2 to the starting solid feed material.Sample ID Fe2O3 % MgO % K2O % P2O5 % Ni % Cu% Sample A: Substrate3, Condition 1 0.9 0.86 0.88 0.57 1.12 1.17 Sample B: Substrate3, Condition 2 0.88 0.78 0.95 0.29 1.15 1.19PATENT APPLICATION ATTORNEY DOCKET NO. 19148-013WO1

[0106] The percentages in Table 3 were prepared by taking the percent element of either Condition 1 or 2 and dividing by the percent element in the untreated ore material.

[0107] Post agitated leach and liquid / solid separation, the solid samples (Sample 3A and Sample 3B) were then run through flotation tests. In addition, an untreated nickel sulfide rougher feed sample (Substrate 3 Control) was also run through flotation tests in a Denver flow cell for comparative purposes. Results are shown in Table 4

[0108] Table 4. Percentage of the solids going to the concentrates versus the tailings in the control untreated bulk rougher feed versus the biosolvent treated bulk rougher feed Substrate 3Sample ID (Control) Sample 3 A Sample 3B Concentrate wt % 47.3 54.4 56.6 Tailings wt % 52.7 45.6 43.4

[0109] It was determined that, for samples that had undergone the lactic acid leaching (Sample 3 A and Sample 3B), more of the solid material went to the concentrate versus the tailings streams compared to the control sample which had higher overall mass going to the tailings stream (Table 4).

[0110] In addition, the elemental composition of the concentrate versus the tailings streams differed between the untreated control Substrate 3 and the nickel sulfide rougher feed substrate that had undergone the agitated leaching in lactic acid prior to flotation, with improvements in the Ni grade of the concentrate feed. In other words, less of the Ni was lost to the tailings after the leaching treatment.

[0111] Table 5. Change in grade post flotation compared to the feed material (i.e. element % post flotation / element % flotation feed).Sample ID Substrate 3 (Control) Sample 3A Sample 3B Concentrate Ni% 1.35 1.71 1.67 Tailing Ni% 0.69 0.15 0.13PATENT APPLICATION ATTORNEY DOCKET NO. 19148-013WO1

[0112] As shown in Table 5, more of the value metal Ni goes to the concentrate stream versus the tailings stream with the biosolvent treated samples (Sample A and Sample B) compared to the control sample, which did not undergo any treatment prior to flotation.

[0113] Table 6. Substrate composition analysisSample ID Substrate 3 (Control) Sample 3A Sample 3B Concentrate SiO2% 0.93 0.85 0.860 Tailing SiO2% 1.06 1.18 1.180 Concentrate MgO% 0.94 0.84 0.840 Tailing MgO% 1.05 1.19 1.210 Concentrate AI2O3 % 0.91 0.78 0.8 Tailing AhO3% 1.08 1.26 1.26 Concentrate P20s% 1 0.9 0.82 Tailing P2O5 % 1 1.12 1.23 Concentrate MnO% 0.97 0.74 0.75 Tailing MnO% 1.03 1.31 1.32 Concentrate Na2O% 0.77 0.77 0.79 Tailing Na2O% 1.21 1.28 1.27 Concentrate CaO% 0.88 0.75 0.77 Tailing CaO% 1.11 1.3 1.3 Concentrate Cr2O3% 0.77 0.8 0.83 Tailing Cr2O3% 1.21 1.24 1.23 Concentrate Fe2O3% 1.08 1.33 1.33 Tailing Fe2O3% 0.93 0.6 0.57 Concentrate K2O% 0.99 0.9 0.9 Tailing K2O% 1.01 1.12 1.12

[0114] A larger proportion of impurities including gangue and penalty elements were determined to go into the tailings stream compared to the concentrate stream for SamplePATENT APPLICATION ATTORNEY DOCKET NO. 19148-013WO13A and Sample 3B that have been treated by biosolvents prior to flotation compared to Sample 3 (Control), which was not treated with a biosolvent prior to flotation. This change in grade post flotation compared to the feed material is shown in Table 5 above (e.g., as element % post flotation / element % flotation feed).

[0115] Example 4:

[0116] Select organic acids were added to collectors and incubated at temperature (60 °C) for 2 hours. Approximately 2.81 m (milliliters) of Lactic acid, and 7.19 mL of mine process water were placed in a 20 mL screw cap headspace vial and capped. The mixture was heated to 60 °C. Then, a known amount of each collector / promoter (individual solutions for each) were added to the solution such that the additive was present at 50 ppm (parts per million) concentration. The solution was capped and then equilibrated at 60 °C. Sampling occurred at two time intervals, first at 15 minutes and again at 120 minutes.

[0117] Semi- quantitation was accomplished using a toluene / hexadecane reference of known concentration added to the lactic acid / Mine Process Water mixture. The response factor from this known analyte was used to estimate the levels of volatile organic compounds in the sample headspace. Semi-quantitation for carbon dioxide (CO2) was achieved using the response of known atmospheric levels of CO2. The gas chromatography-mass spectroscopy (GC / MS) analysis was conducted on an Agilent 7890 gas chromatograph equipped with an Agilent 5975C mass selective detector. The system utilized a 60m Rtx-624 column for separations. The results shown in Table 7 demonstrate that representative organic acids degrade several typical collectors. This beneficial result of the agitated leach means that, in some multistage flotation processes, the flotation step(s) subsequent to the agitated leach will require reduced chemical usage to counteract the effect of residual collectors being present.

[0118] Table 7. Targeted GC / MS screening results for five different collectors used on ore substrates.Observed in Commercial CASAcid Hydrolysis Products Headspace Name Number(Yes / No)Plottec 304 2956-12-9 1 -pentanol NoPATENT APPLICATION ATTORNEY DOCKET NO. 19148-013WO12-propenethiol No carbonyl sulfide Yes, carbon carbon disulfide disulfide isopropanol No ethylamine No Aero® AF- 141-98-0 carbonyl sulfide3894 Yes, carbon hydrogen sulfidedioxide carbon dioxideisopropanol NoSPIX 140-93-2carbon disulfide Yesn-butanol No Aero® XD- carbonyl sulfide39142-36-45002 thiols No carbon dioxide25322-69-4 Polypropylene glycol Not applicable Aero®Yes, trace MX-2418 108-11-2 2-methyl-2-penteneamount

[0119] In the above detailed description of embodiments of the disclosure, numerous specific details are set forth in order to provide a more thorough understanding of the disclosure. However, it will be apparent to one of ordinary skill in the art that the disclosure may be practiced without these specific details. In other instances, well-known features have not been described in detail to avoid unnecessarily complicating the description.

[0120] In the above description, any component described with regard to FIGs. 1-2, in various embodiments disclosed herein, may be equivalent to one or more like-named components described with regard to any other embodiment and / or figure. For brevity, descriptions of these components will not be repeated with regard to each embodiment and / or figure. Thus, each and every embodiment of the components of each embodiment and / or figure is incorporated by reference and assumed to be optionally present within every other figure having one or more like-named components. Additionally, in accordance with various embodiments disclosed herein, any description of the components of a figure is to be interpreted as an optional embodiment which may be implemented in addition to, in conjunction with, or in place of the embodiments described with regard to a corresponding like-named component in any other embodiment and / or figure.PATENT APPLICATION ATTORNEY DOCKET NO. 19148-013WO1

[0121] Throughout the application, ordinal numbers (for example, first, second, third) may be used as an adjective for an element (that is, any noun in the application). The use of ordinal numbers does not imply or create a particular ordering of the elements or limit any element to being only a single element unless expressly disclosed, such as by the use of the terms “before,” “after,” “single,” and other such terminology. Rather, the use of ordinal numbers is to distinguish between the elements. By way of an example, a first element is distinct from a second element, and the first element may encompass more than one element and succeed (or precede) the second element in an ordering of elements.

[0122] It is to be understood that the singular forms “a,” “an,” and “the” include plural referents unless the context clearly dictates otherwise. Thus, for example, reference to “an organic acid” includes reference to one or more of such organic acids.

[0123] Terms such as “approximately” or “substantially” mean that the recited characteristic, parameter, or value need not be achieved exactly, but that deviations or variations, including, for example, tolerances, measurement error, measurement accuracy limitations, and other factors known to those of skill in the art, may occur in amounts that do not preclude the effect the characteristic was intended to provide.

[0124] It is to be understood that one or more of the steps shown in the flowcharts may be omitted, repeated, or performed in a different order than shown. Accordingly, the scope disclosed should not be considered limited to the specific arrangement of steps shown in the flowcharts.

[0125] Although multiple dependent claims are not introduced, it would be apparent to one of ordinary skill that the subject matter of the dependent claims of one or more embodiments may be combined with other dependent claims.

[0126] Although only a few example embodiments have been described in detail above, those skilled in the art will readily appreciate that many modifications are possible in the example embodiments without materially departing from this invention. Accordingly, all such modifications are intended to be included within the scope of this disclosure as defined in the following claims.

Claims

PATENT APPLICATION ATTORNEY DOCKET NO. 19148-013WO1 CLAIMSWhat is claimed:

1. A method for providing an ore substrate for a flotation process, the method comprising:enriching a solid ore material via selective solubilization of an impurity component from the solid ore material with an extraction composition to produce an enriched ore material and a leachate,wherein the extraction composition:comprises at least one organic acid, andis configured to selectively solubilize one or more impurities from the solid ore material into the extraction composition,is configured to retain at least one metal of value in the enriched ore material; andseparating the leachate from the enriched ore material, thereby providing the ore substrate.

2. The method of claim 1 , further comprising obtaining the solid ore material from a mining site, ore tailings, and / or a flotation process.

3. The method of claim 2, wherein obtaining the solid ore material comprises:obtaining solids from a flotation apparatus as a solids stream; andoptionally, reducing a water content of the solids stream to provide the solid ore material.

4. The method of claim 3, wherein reducing the water content comprises filtering the solids and / or thickening the solids to provide the solid ore material.

5. The method of any one of claims 2 to 4, wherein the solid ore material comprises ore tailings, an ore concentrate, waste rock, solids obtained from a flotation process, or any combination thereof.

6. The method of any one of the preceding claims, wherein the enriching comprises desorbing and / or degrading a flotation reagent present on the solid ore material.

7. The method of claim 6, wherein the flotation reagent is a flotation collector.PATENT APPLICATION ATTORNEY DOCKET NO. 19148-013WO18. The method of any one of the preceding claims, further comprising agitating a mixture of the solid ore material and the extraction composition.

9. The method of any one of the preceding claims, further comprising contacting the solid ore material with the extraction composition at a select temperature and a select period of time.

10. The method of claim 8, wherein the select temperature is a temperature in a range from 10 to 100 °C, and the select period of time is a value in a range from 15 minutes to 24 hours.

11. The method of any one of the preceding claims, further comprising preparing the extraction composition prior to treating the solid ore material.

12. The method of claim 11, wherein preparing the extraction composition comprises:based on a composition of the solid ore material, preparing a biobroth from a natural and / or engineered organic acid-producing microbe, a natural and / or engineered organic acid-producing plant, or combinations thereof; and / orbased on a composition of the solid ore material, preparing a solution comprising a first organic acid; an optional additional organic acid; and optionally an inorganic acid.

13. The method of any one of the preceding claims, further comprising:subjecting the enriched ore material to a flotation process to separate a metal of value from the enriched ore material; andseparating two or more metals of value from the enriched ore material in the flotation process to produce at least one value stream comprising the two or more metals of value and a waste stream comprising an impurity component,wherein a flotation collector is present or absent during the flotation process.

14. The method of any one of the preceding claims, further comprising stripping one or more impurity elements from the leachate via ion exchange, solvent extraction, nanofiltration, simulated moving bed reactors (SMB), electrodeionization (EDI), precipitation, centrifugation decantation, filtration, or combinations thereof.PATENT APPLICATION ATTORNEY DOCKET NO. 19148-013WO115. The method of any one of the preceding claims, wherein the extraction composition comprises a pH in a range from 0.1 to 7.

16. The method of any one of the preceding claims, wherein the extraction composition comprises the at least one organic acid at a concentration in a range from 0.05 M to 2.5 M.

17. A method for improving a separation efficiency of a flotation process, the method comprising:reducing an impurity content of a solid ore material with an extraction composition, thereby forming an enriched ore material and a leachate, wherein the extraction composition:comprises at least one organic acid,is configured to selectively transfer one or more impurities from the solid ore material into the extraction composition, andis configured to retain at least one metal of value in the enriched ore material; separating the leachate from the enriched ore material;introducing the enriched ore material to a flotation apparatus;operating the flotation apparatus including a flotation mixture comprising the enriched ore material to produce a waste stream and a value stream; andrecovering the value stream comprising a higher metal of value content as compared to a value stream obtained from a flotation process of the enriched ore material without treatment with the extraction composition.

18. The method of claim 17, wherein the value stream comprises at least 10% of a metal of value from the enriched ore material.

19. The method of claim 17 or claim 18, wherein operating the flotation apparatus comprises separating two or more metals of value from the enriched ore material into the value stream.

20. The method of any one of claims 17 to 19, wherein, when the waste stream comprises at least one impurity metal, the method further comprises separating at least one impurity metal from the waste stream.PATENT APPLICATION ATTORNEY DOCKET NO. 19148-013WO121. The method of any one of claims 17 to 20, wherein the extraction composition comprises a biobroth obtained from a natural and / or engineered organic acid-producing microbe, a natural and / or engineered organic acid-producing plant, or combinations thereof.

22. The method of any one of claims 17 to 21, wherein the extraction composition comprises an aqueous solution comprising:a first organic acid;an optional additional organic acid;optionally an inorganic acid; andoptionally a biobroth.

23. The method of claim 22, wherein a concentration ratio of the first organic acid to the additional acid is in a range from 1 : 0 to 1 : <1.

24. The method of claim 22 or claim 23, wherein the inorganic acid comprises an acid selected from the group consisting of sulfuric acid, hydrochloric acid, nitric acid, phosphoric acid, and combinations thereof.

25. The method of any one of claims 22 to 24, wherein the extraction composition is configured to selectively solubilize one or more components comprising a phosphorous (P) component, a potassium (K) component, a sodium (Na) component, a calcium (Ca), a chromium (Cr) component, a magnesium (Mg) component, an aluminum (Al) component, a silicon (Si) component, a fluorine (F) component, an iron (Fe) component, a lead (Pb) component, a zinc (Zn) component, a molybdenum (Mo) component, or any combination thereof from the solid ore material, and wherein the one or more components comprise one or more of an atom, a mineral, a salt of Mg, Na, Al, Si, F, Fe, Mo, Pb, P, K, Cr, Zn, or any combination thereof.

26. The method of any one of claims 22 to 25, wherein the at least one organic acid comprises an acid selected from the group consisting of gluconic acid, citric acid, oxalic acid, glutamic acid, formic acid, lactic acid, acetic acid, malic acid, hydroxypropionic acid, phthalic acid, tartaric acid, hexadecenoic acid, heptadecanoic acid, gallic acid, asparticPATENT APPLICATION ATTORNEY DOCKET NO. 19148-013WO1acid, succinic acid, oleic acid, tannic acid, palmitic acid, ascorbic acid, and combinations thereof.

27. The method of any one of claims 22 to 26, wherein the reducing the impurity content comprises desorbing and / or degrading a flotation reagent present on the solid ore material.

28. The method of claim 27, wherein the flotation reagent is a flotation collector.

29. The method of any one of claims 17 to 28, further comprising regenerating the extraction composition by stripping one or more impurity elements from the leachate via ion exchange, solvent extraction, nanofiltration, simulated moving bed reactors (SMB), electrodeionization (EDI), precipitation, decantation, filtration, or combinations thereof.

30. The method of any one of the preceding claims, wherein when at least two metals of value are present in the solid ore material, reducing the impurity component content in the solid ore material comprises retaining the at least two metals of value in the enriched ore material.

31. A process comprising:pretreating a solid ore material and / or a flotation concentrate with an extraction composition to remove at least a portion of a flotation collector present in the solid ore material and / or the flotation concentrate, thereby producing a treated ore material and a leachate, andsubjecting the treated ore material to a flotation process for separating two or more value metals in the absence of a depressant or with a significantly reduced addition of the depressant to facilitate the separation of the two or more value metals.

32. The process of claim 31, wherein the extraction composition:comprises at least one organic acid,is configured to selectively solubilize one or more impurities from the solid ore material into the extraction composition, andis configured to retain at least one metal of value in the treated ore material.PATENT APPLICATION ATTORNEY DOCKET NO. 19148-013WO133. The process of claim 31 or claim 32, wherein the pretreating comprises an agitated leach of the solid ore material and the extraction composition.

34. The process of any one of claims 31 to 33, wherein the pretreatment comprises enriching the solid ore material via selective solubilization of an impurity component from the solid ore material, wherein at least a portion of the impurity component from the solid ore material is present in the leachate.

35. The process of any one of claims 31 to 33, further comprising:introducing the treated ore material to a flotation apparatus;operating the flotation apparatus including a flotation mixture comprising the treated ore material to produce a waste stream and a value stream, wherein the depressant is absent from the flotation mixture; andrecovering the value stream comprising a higher metal of value content as compared to a value stream obtained from a flotation process of the treated ore material without treatment with the extraction composition.

36. The process of any one of claims 31 to 35, further comprising recovering a value stream from the flotation process comprising a higher metal of value content as compared to a value stream obtained from a flotation process of the solid ore material and / or the flotation concentrate without pre-treatment with the extraction composition.

37. The process of claim 36, wherein the recovering the value stream comprises:recovering a first value stream comprising a first metal of value; andrecovering a second value stream comprising a second metal of value,wherein the first value stream and the second value stream each independently have a higher metal of value content relative to a flotation process performed without pretreatment with the extraction composition.