An aerosol generation system and heating medium using multicard coupling giant thermal effect

By employing a multi-card coupled giant thermal effect heating medium design in the aerosol generation system, and utilizing a composite structure of dielectric, magnetic, and conductive media, uniform heating and low-temperature excitation of the aerosol generation matrix are achieved. This solves the problems of uneven heating and temperature control in existing technologies, and improves heating efficiency and energy consumption management.

CN114617298BActive Publication Date: 2024-11-22HUBEI CHINA TOBACCO INDUSTRY CO LTD
View PDF 0 Cites 2 Cited by

Patent Information

Application Number
CN202210415674.2
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-04-20
Publication Date
2024-11-22
Estimated Expiration
2042-04-20

AI Technical Summary

Technical Problem

Existing resistance heating and electromagnetic induction heating methods are difficult to achieve uniform heating and temperature control of the aerosol generation matrix in aerosol generation systems, and no aerosol generation system utilizing the multi-calorie coupling giant heat effect has been found.

Method used

An aerosol generation system employing multi-card coupled giant thermal effect is developed. By designing a composite structure of dielectric, magnetic and conductive media in the heating medium, a giant thermal effect is generated through multi-field coupling, which reduces the thermal excitation temperature of the aerosol generation matrix. Furthermore, the uniformity of heating temperature and low power consumption are achieved through frequency matching of the alternating electromagnetic field.

Benefits of technology

Uniform heating and low-temperature activation of the aerosol generation matrix were achieved, improving heating efficiency and temperature control accuracy while reducing energy consumption.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114617298B_ABST
    Figure CN114617298B_ABST
Patent Text Reader

Abstract

The present invention provides an aerosol generating system and a heating medium utilizing the multicard coupling giant thermal effect, wherein the heating medium comprises a first heating medium suitable for an alternating electromagnetic field response frequency in the range of 0.3 MHz to 300 MHz, and a second heating medium in the range of 0.3 GHz to 30 GHz. The heating medium obtained by mesoscopically compounding the corresponding high dielectric loss, high hysteresis loss and high conductivity loss components meets the configuration requirements of the material for the multicard giant thermal effect generated by multi-field coupling, has a strong coupling effect and high heating efficiency. In the aerosol generating system, the heating medium is used as a heating particle blended with an aerosol matrix in an aerosol generating matrix, or as a foil-like film composite heating medium in an aerosol generating section as an auxiliary enhanced heating medium, and the heating medium is also used as a block heating medium of a heating chamber and a preheating shell particle coating heating medium to achieve a multi-source synergistic enhanced heating effect.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of tobacco, and in particular relates to an aerosol generating system and a heating medium utilizing a multi-card coupling giant thermal effect. Background Art

[0002] In heat-not-burn cigarettes, an aerosol generating system and method is formed by electrically heating an aerosol generating substrate for inhalation by the user. The most common method is to use the Joule heat generated by the current passing through the resistance heating element to heat the aerosol generating substrate. This type of method has formed many patents and many products and has become well-known in the field. The possible disadvantage of the resistance heating method is that it is difficult to achieve uniform heating of the aerosol generating substrate and accurate control of the heating temperature.

[0003] The electromagnetic induction heating systems and methods proposed later are typical of the series of Chinese patents applied for by Philip Morris, including application publication numbers: CN112739228A (heating assembly and method for inductively heating an aerosol-forming substrate, 2021-04-30); CN110461176A (receptor assembly for inductively heating an aerosol-forming substrate, 2019-11-15); CN112739227A (inductively heatable aerosol-generating article including an aerosol-forming substrate and a receptor assembly, 2021-04-30); CN111449293A, CN111109662A, CN111035072A (including Aerosol-forming articles of magnetic particles, 2020-07-28, 2020-05-08, 2020-04-21); CN112822950A (a sensor assembly for inductively heating an aerosol-forming substrate, 2021-05-18); CN112739229A (an inductive heating assembly for inductively heating an aerosol-forming substrate, 2021-04-30); CN112088577A (a sensor assembly for aerosol generation including a sensor tube, 2020-12-15); CN112739226A (an inductively heated aerosol-generating device including a sensor assembly, 2021-04-30); CN11238409 0A (Inductively heatable cartridge for aerosol generating system and aerosol generating system including an inductively heatable cartridge, 2021-02-19); CN112189901A (Aerosol generating article with internal receptor, 2021-01-08); CN112638186A (Inductively heatable aerosol generating article including aerosol-forming rod segments and method for manufacturing such aerosol-forming rod segments, 2021-04-09); CN112804899A (Aerosol generating device for inductively heating an aerosol-forming substrate, 2021-05-14); CN113597263A (Inductively heatable aerosol-forming rod and method for manufacturing such rod shaped device, 2021-11-02); CN110731125A (induction heating device, aerosol generating system including an induction heating device and operation method thereof, 2020-01-24); CN112218554A (electric heating component for heating aerosol-forming substrate, 2021-01-12); CN110891441A (aerosol generating device with a receptor layer, 2020-03-17); CN112931957A (receptor for aerosol generating device, aerosol generating device, 2021-06-11); CN110891443A (aerosol generating system with multiple receptors, 2020-03-17);CN110996696A (Aerosol generating device with induction heater and movable parts, 2020-04-10); CN111050582A (Heater for aerosol generating device with connector, 2020-04-21); CN110913712A (Aerosol generating device with reduced spacing inductor coil, 2020-03-24); CN111109658A (Electrically heated aerosol generating system, 2020-05-08); CN111031819A (Aerosol generating device with removable susceptor, 2020-04-17); CN109475194A (Susceptor assembly and aerosol generating article including the susceptor assembly, 2019-03-15), etc. ;

[0004] In the disclosed patents or patent applications related to electromagnetic heating systems and methods, there is no aerosol generating system utilizing the multi-card coupling giant thermal effect. Summary of the invention

[0005] In view of this, the purpose of the present invention is to provide an aerosol generating system and a heating medium utilizing the multi-card coupling giant thermal effect. The heating medium components of the system are designed to enhance dielectric loss, hysteresis loss, damping loss, resonance loss and conductivity loss. The material structure can realize multi-field coupling to produce the multi-card coupling giant thermal effect. The pore structure can increase the liquid phase saturated vapor pressure value and reduce the thermal excitation temperature of the aerosol generating matrix. The alternating electromagnetic field can meet the multi-field coupling drive matching requirements, be compatible with and balance the multi-card coupling response frequency, and achieve the purpose of uniform heating temperature and low power consumption.

[0006] The present invention provides an aerosol generating substrate, comprising a heating medium, wherein the heating medium comprises a first heating medium or a second heating medium;

[0007] The first heating medium includes a first dielectric medium, a first magnetic medium and a first conductive medium;

[0008] The first dielectric is selected from at least one of the following systems:

[0009] ①Perovskite structure system, including BaTiO3, and / or PbTiO3, and / or NaNbO3, and / or KNbO3, and / or BiFeO3; ②Tungsten bronze structure system, including lead metaniobate, and / or Sr 1-x Ba x Nb2O6; ③ Bismuth layered structure system, including SrBi2Ta2O9, and / or Bi4Ti3O 12 , and / or SrBi4Ti4O 15 ; ④ pyrochlore structure system, including Cd2Nb2O7, and / or Pb2Nb2O7;

[0010] The first magnetic medium is selected from at least one of the following ferrites:

[0011] Spinel ferrites, including MFe2O4, M=Mn, and / or Fe, and / or Ni, and / or Co, and / or Cu, and / or Mg, and / or Zn, and / or Li, and / or MnZn, and / or NiZn, and / or MgZn, and / or LiZn ferrites; and / or R3Fe5O 12 , R is a rare earth element, and the rare earth element is Y, and / or La, and / or Pr, and / or Nd, and / or Sm, and / or Eu, and / or Gd, and / or Tb, and / or Dy, and / or Ho, and / or Er, and / or Tm, and / or Yb, and / or Lu;

[0012] The first conductive medium is selected from at least one of the following components:

[0013] ZnO series, including doped Al (AZO), and / or doped In (IZO), and / or doped Ga (GZO); magnetic oxides, including CoO, and / or MnO, and / or Fe3O4, and / or NiO; and other semiconductor oxides, including Ga2O3, and / or In2O3, and / or InSnO (ITO);

[0014] The second heating medium includes a second dielectric medium, a second magnetic medium and a second conductive medium;

[0015] The second dielectric is selected from ①BaO-MgO-Ta2O5, and / or BaO-ZnO-Ta2O5, and / or BaO-MgO-Nb2O5, and / or BaO-ZnO-Nb2O5 system and their composite system; ②BaTi4O9, and / or BaTi9O 20 , (Zr, and / or Sn)TiO4-based systems; ③BaO-Ln2O3-TiO2, and / or CaO-Li2O-Ln2O3-TiO2 (Ln2O3 is a lanthanide rare earth oxide)-based systems; ④A5B4O 15 (A=Ba, and / or Sr, and / or Mg, and / or Zn, and / or Ca, B=Nb, and / or Ta), and / or AB2O6 (A=Ca, and / or Co, and / or Mn, and / or Ni, and / or Zn; B=Nb, and / or Ta); (Ba 1-x M x )ZnO5(M=Ca, and / or Sr, x=0~1.0),AgNb 1-x Ta xO3 (x = 0 ~ 1.0), and / or LnAlO3 (Ln = La, and / or Nd, and / or Sm), and / or Ta2O5-ZrO2, and / or ZnTiO3, and / or BiNbO4 series;

[0016] The second magnetic medium is selected from M-type hexagonal ferrite: BaM, and / or PbM, and / or SrM; X-type hexagonal ferrite, including Fe2X; W-type hexagonal ferrite, including Mg2W, and / or Mn2W, and / or Fe2W, and / or Co2W, and / or Ni2W, and / or Cu2W, and / or Zn2W; Y-type hexagonal ferrite, including Mg2Y, and / or Mn2Y, and / or Fe2Y, and / or Co2Y, and / or Ni2Y, and / or Cu2Y, and / or Zn2Y; Z-type hexagonal ferrite, including Mg2Z, and / or Mn2Z, and / or Fe2Z, and / or Co2Z, and / or Ni2Z, and / or Cu2Z, and / or Zn2Z;

[0017] The second conductive medium is selected from the ZnO series, including doped Al (AZO), and / or doped In (IZO), and / or doped Ga (GZO); magnetic oxides, including CoO, and / or MnO, and / or Fe3O4, and / or NiO; and other semiconductor oxides, including Ga2O3, and / or In2O3, and / or InSnO (ITO).

[0018] In the present invention, the first heating medium is formed into a core-shell type, or a heterojunction type, or a coating type, or a porous type or a membrane composite type through a mesoscopic scale compound of a physical and chemical method;

[0019] The core-shell type first heating medium includes an electric moment-magnetic moment coupling heating medium 1-H-1 of a core-shell type structure, an electric moment-conductivity coupling heating medium 1-H-2 of a core-shell type structure, or an electric moment-magnetic moment-conductivity coupling heating medium 1-H-3 of a core-shell type structure;

[0020] The specific method of forming the first heating medium having the core-shell type is a direct precipitation method, a coprecipitation method, an alcohol salt hydrolysis method, or a sol-gel method;

[0021] The first heating medium of the heterojunction structure includes an electric moment-magnetic moment coupling heating medium 1-Y-1 of the heterojunction structure, or an electric moment-conductivity coupling heating medium 1-Y-2 of the heterojunction structure, or an electric moment-magnetic moment-conductivity coupling heating medium 1-Y-3 of the heterojunction structure;

[0022] The specific method for forming the first heating medium having the heterojunction structure is a molten salt method, a high-temperature solid-phase reaction method, a mechanical alloying method, a precipitation method with controlled calcination temperature, an alcohol salt hydrolysis method, a hydrothermal method, or a sol (gel)-hydrothermal method;

[0023] The first heating medium of the encapsulated structure includes an electric moment-magnetic moment coupling heating medium 1-B-1 of the encapsulated structure or an electric moment-magnetic moment-conductivity coupling heating medium 1-B-2 of the encapsulated structure;

[0024] The specific method of forming the first heating medium having the coated structure is a mechanical fusion coating method, a mechanochemical effect method induced by a high-energy mill, a low-heat solid phase reaction method, or a sol-gel method;

[0025] The first heating medium with a porous structure is a porous structure electric moment-magnetic moment-conductance coupling heating medium 1-K, or a heating medium 1-D of a low excitation temperature aerosol generating matrix;

[0026] The first heating medium of the membrane composite structure is an electric moment-magnetic moment-conductivity coupling heating medium 1-M;

[0027] The second heating medium is formed into a core-shell type, a heterojunction type, a coating type, a porous type or a membrane composite type by mesoscopic compounding of physical and chemical methods;

[0028] The core-shell type second heating medium includes an electric moment-magnetic moment coupling heating medium 2-H-1 of a core-shell type structure, an electric moment-conductivity coupling heating medium 2-H-2 of a core-shell type structure, or an electric moment-magnetic moment-conductivity coupling heating medium 2-H-3 of a core-shell type structure;

[0029] The specific method of forming the second heating medium having the core-shell type is a direct precipitation method, a coprecipitation method, an alcohol salt hydrolysis method, or a sol-gel method;

[0030] The second heating medium of the heterojunction structure includes an electric moment-magnetic moment coupling heating medium 2-Y-1 of the heterojunction structure, or an electric moment-conductivity coupling heating medium 2-Y-2 of the heterojunction structure, or an electric moment-magnetic moment-conductivity coupling heating medium 2-Y-3 of the heterojunction structure;

[0031] The specific method for forming the second heating medium having the heterojunction structure is a molten salt method, a high-temperature solid-phase reaction method, a mechanical alloying method, a precipitation method with controlled calcination temperature, an alcohol salt hydrolysis method, a hydrothermal method, or a sol (gel)-hydrothermal method;

[0032] The second heating medium of the encapsulated structure includes an electric moment-magnetic moment coupling heating medium 2-B-1 of the encapsulated structure or an electric moment-magnetic moment-conductivity coupling heating medium 2-B-2 of the encapsulated structure;

[0033] The specific method of forming the second heating medium having the coated structure is a mechanical fusion coating method, a mechanical chemical effect method induced by a high-energy mill, a low-heat solid phase reaction method, or a sol-gel method;

[0034] The second heating medium with a porous structure is a porous electric moment-magnetic moment-conductance coupling heating medium 2-K, or a heating medium 2-D of a low excitation temperature aerosol generating matrix;

[0035] The second heating medium of the film composite structure is an electric moment-magnetic moment-conductivity coupling heating medium 2-M.

[0036] In the present invention, the electric moment-magnetic moment-conductivity coupling heating medium 1-K of the porous structure is prepared according to the following method:

[0037] The ultrafine particles of at least one component of the first dielectric, the first magnetic medium and the first conductive medium in the first heating medium are fully mixed with an inorganic binder, sodium silicate, or aluminum dihydrogen phosphate, or phosphoric acid-copper oxide, and a pore-forming agent, ultrafine carbon powder or starch, or ultrafine calcium carbonate, and then sintered, crushed and classified to obtain the porous structure of the electric moment-magnetic moment-conductivity coupled heating medium 1-K; or at least one component of the first dielectric, at least one component of the first magnetic medium system and at least one component of the first conductive medium are obtained by a polymer network gel method, or a soluble complex network gel is obtained by a metal complex gel method, and then dried, sintered, crushed and classified to obtain the porous structure of the electric moment-magnetic moment-conductivity coupled heating medium 1-K; or the first dielectric is treated by ions of at least one component of the first magnetic medium and ions of at least one component of the first conductive medium in a solution and a precipitant. The granular porous body is modified by precipitation method, so that a composite film layer of the first magnetic medium component and the first conductive medium component is formed on the inner surface of the pores, so as to obtain the electric moment-magnetic moment-conductivity coupling heating medium 1-K of the porous structure; or ultrafine particles of at least one component of the first dielectric and the first magnetic medium in the first heating medium are fully mixed with inorganic binder sodium silicate, or aluminum dihydrogen phosphate, or phosphoric acid-copper oxide, and pore-forming agent ultrafine carbon powder or starch, or ultrafine calcium carbonate, and then sintered, crushed and classified to obtain the electric moment-magnetic moment coupling heating medium of the porous structure, and then the pores of the electric moment-magnetic moment coupling heating medium of the porous structure are modified by chemical plating method, and the metal ions of at least one component of the first conductive medium system adsorbed in the plating solution in the pores are catalytically reduced to metal by the reducing agent in the plating solution and deposited on the inner surface of the pores to obtain the electric moment-magnetic moment-conductivity coupling heating medium 1-K of the porous structure;

[0038] The electric moment-magnetic moment-conductivity coupling heating medium of the porous structure has a pore size of 2 nm to 50 μm and a porosity of 70% to 95%.

[0039] The electric moment-magnetic moment-conductivity coupling heating medium 2-K of the porous structure is prepared according to the following method:

[0040] The ultrafine particles of at least one component of the second dielectric and the second magnetic medium and the second conductive medium system in the second heating medium are fully mixed with the inorganic binder sodium silicate, or aluminum dihydrogen phosphate, or phosphoric acid-copper oxide, and the pore-forming agent ultrafine carbon powder or starch, or ultrafine calcium carbonate, and then sintered, crushed and classified to obtain the porous structure of the electric moment-magnetic moment-conductivity coupled heating medium 2-K; or at least one component of the second dielectric, at least one component of the second magnetic medium and at least one component of the second conductive medium are subjected to a gel obtained by a polymer network gel method, or a soluble complex network gel obtained by a metal complex gel method, and then dried, sintered, crushed and classified to obtain the porous structure of the electric moment-magnetic moment-conductivity coupled heating medium 2-K; or the second dielectric particle porous body is modified by precipitation method using ions of at least one component of the second magnetic medium system and ions of at least one component of the second conductive medium system in the solution and a precipitant to form the second dielectric particle porous body on the inner surface of the pores. The composite film layer of the second magnetic medium component and the second conductive medium component is used to obtain the electric moment-magnetic moment-conductivity coupling heating medium 2-K of the porous structure; or the ultrafine particles of at least one component of the second dielectric and the second magnetic medium system in the second heating medium are fully mixed with the inorganic binder sodium silicate, or dihydrogen aluminum phosphate, or phosphoric acid-copper oxide, and the pore-forming agent ultrafine carbon powder or starch, or ultrafine calcium carbonate, and then sintered, crushed and classified to obtain the electric moment-magnetic moment coupling heating medium of the porous structure, and then The pores of the electric moment-magnetic moment coupled heating medium of the porous structure are modified by chemical plating, and the metal ions of at least one component of the second conductive medium adsorbed in the plating solution in the pores are catalytically reduced to metal by the reducing agent in the plating solution and deposited on the inner surface of the pores to obtain the electric moment-magnetic moment-conductivity coupled heating medium 2-K of the porous structure, wherein the pore size of the electric moment-magnetic moment-conductivity coupled heating medium 2-K of the porous structure is 2nm to 50μm, and the porosity is 70% to 95%;

[0041] In the present invention, the heating medium 1-D of the low excitation temperature aerosol generating substrate is prepared according to the following method:

[0042] From the electric moment-magnetic moment-conductivity coupling heating medium 1-K of the porous structure, a pore size range of 60nm to 50μm, a porosity range of 85% to 95%, and a specific heat capacity range of 0.1kJ·kg -1 ·K -1 Up to 0.6 kJ·kg -1 ·K -1 , thermal conductivity range is 0.035W·m-1 ·K -1 To 0.125W·m-1·K -1 The particles with the physical property parameters adsorb the liquid phase components of the aerosol generating medium, so that the liquid phase components are separated into small droplets entering the pores with a porosity of 85% to 95%, and the pore size range is 60nm to 50μm, so as to increase the saturated vapor pressure value of the liquid phase components of the aerosol generating medium, and obtain the heating medium of the low excitation temperature aerosol generating matrix, the excitation temperature is 160℃~200℃, and the particle size distribution range of the heating medium 1-D particles of the low excitation temperature aerosol generating matrix is ​​15μm to 500μm;

[0043] The heating medium 2-D of the low excitation temperature aerosol generating substrate is prepared according to the following method:

[0044] From the electric moment-magnetic moment-conductivity coupling heating medium 2-K of the porous structure, a pore size range of 60nm to 50μm, a porosity range of 85% to 95%, and a specific heat capacity range of 0.1kJ·kg -1 ·K -1 Up to 0.6 kJ·kg -1 ·K -1 , thermal conductivity range is 0.035W·m -1 ·K -1 To 0.125W·m-1·K -1 The particles with different physical property parameters adsorb the liquid phase components of the aerosol generating medium, so that the liquid phase components are separated into small droplets entering the pores with a porosity of 85% to 95%, and the pore size range is 60nm to 50μm, so as to increase the saturated vapor pressure value of the liquid phase components of the aerosol generating medium, and obtain the heating medium of the low excitation temperature aerosol generating matrix, the excitation temperature is 160℃~200℃, and the particle size distribution range of the 2-D particles of the heating medium of the low excitation temperature aerosol generating matrix is ​​15μm to 500μm.

[0045] In the present invention, the electric moment-magnetic moment-conductivity coupling heating medium 1-M is prepared according to the following method:

[0046] After fully mixing the ultrafine particles of at least one component of the first dielectric, the first magnetic medium and the first conductive medium system in the first heating medium with the binder sodium silicate, or aluminum dihydrogen phosphate, or phosphoric acid-copper oxide, a single-sided or double-sided film composite is performed on an aluminum sheet, a copper sheet or a stainless steel sheet by spraying or brushing to obtain the electric moment-magnetic moment-conductivity coupling heating medium 1-M of the film composite structure; or the particles of at least one component of the first dielectric, the first magnetic medium and the first conductive medium system in the first heating medium are deposited or sprayed on a single-sided or double-sided film composite on an aluminum sheet, a copper sheet or a stainless steel sheet by vapor deposition, flame vapor deposition or plasma spraying to prepare the electric moment-magnetic moment-conductivity coupling heating medium 1-M of the film composite structure;

[0047] The electric moment-magnetic moment-conductivity coupling heating medium 2-M is prepared according to the following method:

[0048] Ultrafine particles of at least one component of the second dielectric, second magnetic medium and second conductive medium system in the second heating medium are fully mixed with a binder of sodium silicate, or aluminum dihydrogen phosphate, or phosphoric acid-copper oxide, and then a single-sided or double-sided film composite is performed on an aluminum sheet, copper sheet or stainless steel sheet by spraying or brushing to obtain the electric moment-magnetic moment-conductivity coupled heating medium 2-M of the film composite structure; or particles of at least one component of the second dielectric, second magnetic medium and second conductive medium in the second heating medium are deposited or sprayed on a single-sided or double-sided film composite on an aluminum sheet, copper sheet or stainless steel sheet by vapor deposition, flame vapor deposition or plasma spraying to prepare the electric moment-magnetic moment-conductivity coupled heating medium 2-M of the film composite structure.

[0049] In the present invention, the aerosol generating substrate also includes an aerosol substrate;

[0050] The heating medium is directly blended with the aerosol matrix, or before the tobacco sheet in the aerosol matrix is ​​paper-made or rolled, the heating medium is mixed into the fiber slurry or paste, so that the tobacco sheet is evenly distributed with a mass ratio of 5 to 60% of the heating medium, and the particle size of the heating medium is 0.1 μm to 100 μm;

[0051] or a heating medium with a porous structure having a particle size of 15 μm to 100 μm, or a heating medium of a low excitation temperature aerosol generating matrix having a particle size of 15 μm to 100 μm, adsorbs the liquid phase component in the aerosol matrix, and then blends it with the heating medium and the aerosol matrix;

[0052] In the present invention, a foil-like film composite heating medium is also included;

[0053] The foil-like film composite heating medium is prepared by mixing the heating medium particles with a binder, carboxymethyl cellulose, or guar gum or tobacco extract, and then composite the aluminum foil or copper foil on one side or both sides with the film by a casting method or a spraying method, and then cutting the composite heating medium to have a size comparable to that of tobacco flakes, and a particle size distribution range of the heating medium particles is 15 μm to 100 μm; or the dielectric component and the precursor of the magnetic medium component are used to prepare the composite heating medium by chemical vapor deposition, gas phase pyrolysis, gas phase hydrolysis, gas phase combustion, or flame vapor deposition.

[0054] The present invention provides an aerosol generating system using a multi-card coupling giant thermal effect, comprising a heating structure, wherein the heating structure comprises a casing, and an air inlet hole is arranged on the casing;

[0055] A preheating shell is arranged inside the casing; the casing and the preheating shell have coaxial openings;

[0056] The opening of the preheating shell is connected to the filter segment; the preheating shell is provided with a preheating shell air inlet hole;

[0057] A plurality of pole plates are arranged inside the preheating housing; the plurality of pole plates form a heating chamber;

[0058] A heating chamber base is provided at the bottom of the heating chamber; a temperature control unit passes through the central hole of the heating chamber base, and a base disc air inlet hole is provided on the heating chamber base;

[0059] The upper end of the heating chamber is connected to the sealing ring and is nested in the opening of the preheating shell;

[0060] The interior of the electrode plate is an aerosol generating section; a metal particle layer filter medium is provided between the aerosol generating section and the filter tip section;

[0061] The aerosol generating section contains an aerosol generating matrix 1;

[0062] The electrode plate is connected to the heating drive unit via an electrode plate feeder;

[0063] The aerosol generating substrate 1 includes the first heating medium.

[0064] In the present invention, the electrode plate is a tubular electrode plate; the tubular electrode plate comprises a tubular insulating ceramic substrate, and a curved electrode 1 and a curved electrode 2 arranged on the inner surface of the tubular insulating ceramic substrate;

[0065] The curved surface electrodes 1 and the curved surface electrodes 2 are arranged in opposite sections; adjacent curved surface electrodes 1 and curved surface electrodes 2 are separated by insulating materials;

[0066] The number of the curved surface electrodes 1 and the number of the curved surface electrodes 2 are 2 to 5 respectively.

[0067] In the present invention, the electrode plate is a plurality of planar electrodes; the electrode plate includes a planar electrode plate 1 and a planar electrode plate 2 which are parallel and opposite to each other;

[0068] The distance between the planar electrode plate 1 and the planar electrode plate 2 is the diameter of the aerosol generating section.

[0069] In the present invention, a block of heating medium 1 is sandwiched between the two ends of the planar electrode plate 1 and the planar electrode plate 2;

[0070] A cylindrical hole is provided at the symmetric center of the two sandwiched block heating media 1, and the diameter of the cylindrical hole is the diameter of the aerosol generating section.

[0071] In the present invention, the thickness of the metal particle layer filter medium is 0.2 mm to 1.2 mm;

[0072] The metal particle layer filter is formed by pressing aluminum particles with a size of 0.5 to 1.5 mm.

[0073] In the present invention, the block heating medium 1 comprises first heating medium particles and an inorganic binder;

[0074] The inorganic binder is selected from one or more of sodium silicate, aluminum dihydrogen phosphate and phosphoric acid-copper oxide.

[0075] In the present invention, the air inlet hole of the base disc is a through hole with a diameter of 0.3 to 2 mm;

[0076] The number of the air inlet holes is 8 to 36.

[0077] In the present invention, the frequency of the alternating electromagnetic field used by the heating drive unit has a balanced compatible response frequency that meets the requirements of multi-card coupling and multi-field coupling driving of electric cards, magnetic cards and conductive cards. When the compatible response frequency range is from 0.3MHz to 300MHz, it is suitable for the first heating medium.

[0078] In the present invention, a first heating medium particle coating is provided on the inner surface of the preheating shell;

[0079] The first heating medium particle coating comprises a hexagonal boron carbon nitrogen ternary absorbing ceramic substrate and a coating coated on the substrate, wherein the coating comprises first heating medium particles and a film-forming agent; the film-forming agent is selected from sodium silicate sol, or aluminum dihydrogen phosphate sol, or aluminum hydroxide sol, or silica sol;

[0080] or the first heating medium particle coating comprises a metal substrate and a coating coated on the metal substrate, the coating comprising first heating medium particles and an inorganic binder;

[0081] The inorganic binder is selected from sodium silicate, aluminum dihydrogen phosphate, or phosphoric acid-copper oxide.

[0082] The present invention provides an aerosol generating system using a multi-card coupling giant thermal effect, comprising a heating structure, wherein the heating structure comprises a casing, and an air inlet hole is arranged on the casing;

[0083] A preheating shell is arranged inside the casing; the casing and the preheating shell have coaxial openings;

[0084] The opening of the preheating shell is connected to the filter segment; the preheating shell is provided with a preheating shell air inlet hole;

[0085] The preheating shell is provided with a metal shielding shell, a block heating medium 2 and an antenna embedded in the block heating medium 2; the metal shielding shell is wrapped around the outside of the block heating medium 2;

[0086] The metal shielding shell, the block heating medium 2 and the antenna embedded in the block heating medium 2 form a heating cavity;

[0087] The air inlet seat hole of the heating chamber is connected to the outside of the block heating medium 2 through 4 to 10 air inlet channels with a diameter of 0.5 to 2 mm;

[0088] The block heating medium 2 is a cube; a cylindrical hole is provided on the symmetry axis of the block heating medium 2, and an aerosol generating section is formed inside the hole; a wave-transmitting ceramic tube is nested inside the cylindrical hole, and the inner diameter of the wave-transmitting ceramic tube is the diameter of the aerosol generating section;

[0089] The upper end of the heating chamber is connected to the sealing ring and is nested in the opening of the preheating shell;

[0090] A metal particle layer filter medium is provided between the aerosol generating section and the filter tip section;

[0091] The aerosol generating section contains an aerosol generating matrix 2;

[0092] The antenna is connected to the heating drive unit via an antenna feeder foot;

[0093] The aerosol generating substrate 2 includes the second heating medium.

[0094] In the present invention, the wave-transmitting ceramic tube is selected from a quartz SiO2 ceramic tube, a high-alumina ceramic tube, or a Si3N4 ceramic tube.

[0095] The present invention further comprises a temperature control unit, which is laterally inserted into the inner surface of the wave-transmitting ceramic tube and is located 2 to 3 mm away from the free port of the aerosol generating section.

[0096] In the present invention, the block heating medium 2 includes second heating medium particles and an inorganic binder;

[0097] The inorganic binder is selected from sodium silicate, aluminum dihydrogen phosphate, or phosphoric acid-copper oxide.

[0098] In the present invention, a second heating medium particle coating is provided on the inner surface of the preheating shell;

[0099] The second heating medium particle coating comprises a hexagonal boron carbon nitrogen ternary absorbing ceramic substrate and a coating coated on the substrate, wherein the coating comprises second heating medium particles and a film-forming agent; the film-forming agent is selected from sodium silicate sol, or aluminum dihydrogen phosphate sol, or aluminum hydroxide sol, or silica sol;

[0100] or the second heating medium particle coating comprises a metal substrate and a coating coated on the metal substrate, the coating comprising second heating medium particles and an inorganic binder;

[0101] The inorganic binder is selected from sodium silicate, aluminum dihydrogen phosphate, or phosphoric acid-copper oxide.

[0102] In the present invention, the frequency of the alternating electromagnetic field used by the heating drive unit has a balanced compatible response frequency that meets the requirements of multi-card coupling of electric cards, magnetic cards and conductive cards for multi-field coupling driving. When the compatible response frequency range is from 0.3GHz to 30GHz, it is suitable for the second heating medium.

[0103] The aerosol generating system using the card-coupled giant heat effect provided by the present invention comprises: (1) in the dielectric component of the heating medium, measures are taken to strengthen the inherent electric moment orientation polarization, the thermal ion relaxation polarization and the ion displacement polarization, so as to optimize the utilization of the relaxation polarization loss and the resonance polarization loss, and obtain a high polarization loss dielectric; in the magnetic medium component of the heating medium, measures are taken to strengthen the hysteresis loss, the damping loss and the resonance loss, so as to obtain a high hysteresis loss magnetic medium; in the conductive medium component of the heating medium, measures are taken to increase the free electrons, ions and the doping defects and vacancies, so as to optimize the utilization of the conductivity loss of various carriers, and obtain a high conductivity loss conductive medium; (2) in the material structure of the heating medium, the dielectric, the magnetic medium and the conductive medium are compositely constructed by a physical and chemical method of multi-phase components to form a core-shell structure, or a heterojunction structure, or a coating structure, or a porous structure or a membrane composite structure, so as to realize the composite at the mesoscopic level, so as to facilitate the multi-field coupling to generate the multi-card-coupled giant heat effect. (3) In terms of lowering the thermal excitation temperature of the aerosol generating matrix, the porous structure of the heating medium adsorbs the liquid phase components of the aerosol generating medium, causing the liquid phase components to be differentiated into a large number of small droplets. (4) In the heating drive unit of the aerosol generating system, the frequency of the alternating electromagnetic field used is a balanced compatible response frequency that meets the requirements of multi-card coupling of electric cards, magnetic cards and conductive cards for multi-field coupling drive, and the compatible response frequency range is 0.3MHz to 30GHz. BRIEF DESCRIPTION OF THE DRAWINGS

[0104] Figure 1 An axial exemplary cross-sectional view of a first aerosol generating system form 01 of the aerosol generating system and method utilizing multicard coupling giant thermal effect;

[0105] Figure 2 An enlarged axial exemplary cross-sectional view of a heating structure A of the aerosol generating system of the first aerosol generating system form 01 of the aerosol generating system and method utilizing multi-card coupling giant thermal effect;

[0106] Figure 3 for Figure 2 Top view at section AA;

[0107] Figure 4 The first aerosol generating system form 01 of the aerosol generating system and method using multi-card coupling giant thermal effect, the heating structure A of the aerosol generating system, and an enlarged axial exemplary cross-sectional view of a foil-shaped film composite heating medium in the aerosol generating section;

[0108] Figure 5 for Figure 4 An exemplary top view at section AA of FIG.

[0109] Figure 6 The first aerosol generating system form 01 of the aerosol generating system and method using multicard coupling giant thermal effect is an exemplary expansion diagram of the curved surface electrode 1 and the curved surface electrode 2 of the tubular electrode plate in the heating structure A of the aerosol generating system along the circumferential direction;

[0110] Figure 7 An axial exemplary cross-sectional view of a second aerosol generating system form 02 of the aerosol generating system and method utilizing multi-card coupling giant thermal effect;

[0111] Figure 8 This is an enlarged exemplary top view of the CC section of the heating structure B of the aerosol generating system of the second aerosol generating system form 02 of the aerosol generating system and method utilizing the multi-card coupling giant thermal effect;

[0112] Fig. 9 An axial exemplary cross-sectional view of a third aerosol generating system form 03 of the aerosol generating system and method utilizing multicard coupling giant thermal effect;

[0113] Fig.10 The third aerosol generating system form 03 of the aerosol generating system and method using multi-card coupling giant thermal effect is an enlarged axial exemplary cross-sectional view of the heating structure C of the aerosol generating system;

[0114] Fig.11 This is a third aerosol generating system form 03 of the aerosol generating system and method utilizing multicard coupling giant thermal effect, and is an enlarged exemplary top view of the BB section of the heating structure C of the aerosol generating system;

[0115] Fig.12 This is a SEM image of the first heating medium of the core-shell structure in Example 1 of the present invention;

[0116] Fig.13 This is a SEM image of the first heating medium of the heterojunction structure in Example 2 of the present invention;

[0117] Fig.14 This is a SEM image of the second heating medium of the coated structure in Example 3 of the present invention;

[0118] Fig.15 This is a SEM image of the second heating medium of the coated structure in Example 4 of the present invention;

[0119] Fig.16 This is a SEM image of the first heating medium with a porous structure in Example 5 of the present invention;

[0120] Fig.17 This is a SEM image of the membrane composite structure coupled heating medium in Example 6 of the present invention;

[0121] Fig.18 This is a SEM image of the second heating medium of the coated structure in Example 7 of the present invention;

[0122] Fig.19 This is a SEM image of the second heating medium of the coated structure in Example 8 of the present invention;

[0123] Fig. 20 This is a SEM image of the second heating medium of the coated structure in Example 9 of the present invention;

[0124] Fig.21 This is a SEM image of the second heating medium of the coated structure in Example 10 of the present invention. DETAILED DESCRIPTION

[0125] The multi-card coupling giant heat effect described in the present invention refers to:

[0126] (1) Under the drive of external alternating electric field and alternating magnetic field, the thermal effect generated by the coupling of electric dipole formed by polarization and magnetic dipole formed by magnetization includes not only the electric moment thermal effect formed by the entropy of a single electric moment and the magnetic moment thermal effect formed by the entropy of a single magnetic moment, but also the electric moment and magnetic moment coupling thermal effect formed by the electric moment-magnetic moment coupling entropy.

[0127] (2) Driven by the external alternating electromagnetic field and the alternating electric field, the thermal effect generated by the coupling of the electric dipole formed by polarization and the carrier formed by polarization includes not only the moment thermal effect formed by the single moment entropy, the Joule thermal effect formed by the single lattice entropy and the electron entropy, but also the moment and conductivity coupling thermal effect formed by the moment-(lattice + electron) coupling entropy.

[0128] (3) Under the action of the external alternating electromagnetic field and its components, the alternating electric field and alternating magnetic field, the thermal effects produced by the coupling of electric dipoles and carriers formed by polarization and magnetic dipoles formed by magnetization include not only the electric moment thermal effect formed by a single electric moment entropy, the magnetic moment thermal effect formed by a single magnetic moment entropy, and the Joule thermal effect formed by a single lattice entropy and electron entropy, but also the electric moment and magnetic moment coupled thermal effect formed by the electric moment-magnetic moment coupling entropy, the electric moment and conductivity coupled thermal effect formed by the electric moment-(lattice + electron) coupling entropy, the magnetic moment and conductivity coupled thermal effect formed by the magnetic moment-(lattice + electron) coupling entropy, and the electric moment, magnetic moment and conductivity coupled thermal effect formed by the electric moment-magnetic moment-(lattice + electron) coupling entropy.

[0129] It should be pointed out that the multi-calorie effect is not simply the sum of the single-calorie effects, but also includes multiple correlated coupling terms formed by the cross-coupling between the single-calorie effects, making the heat release phenomenon more significant.

[0130] The following is the equation for the temperature change (ΔT) inside the material system based on the multi-card coupling effect, including the multiple related coupling terms formed by the cross-coupling between the single card effects:

[0131]

[0132] Where X i =M,P,ε,…; xi=H,E,σ,… The equation covers all the card effects, including the electro-cardial effect, the magnetic card effect, the conductive card effect, and the cross-coupled multi-card effect.

[0133] For the electric moment-magnetic moment coupled thermal effect, the above equation can be specifically expressed as follows:

[0134]

[0135] Where, the temperature rise of electrocaloric effect ΔT e and the temperature rise ΔT due to the magnetocaloric effect m The corresponding terms of , obviously, include not only the temperature rise term caused by the change of the polarization intensity to the electric field intensity and the temperature rise term caused by the change of the magnetization intensity to the magnetic field intensity, but also the temperature rise term caused by the cross-coupling effect of the change of the electric field intensity related to the dielectric and magnetic medium to the change of the magnetization intensity, and the change of the magnetic field intensity to the change of the polarization intensity. This is also the principle basis for the multi-card coupling giant heat effect described in the present invention.

[0136] The present invention adopts measures to strengthen the inherent electric moment orientation polarization, hot ion relaxation polarization and ion displacement polarization on the dielectric component of the heating medium, so as to optimize the utilization of relaxation polarization loss and resonance polarization loss and obtain a high polarization loss dielectric; adopts measures to strengthen the hysteresis loss, damping loss and resonance loss on the magnetic medium component of the heating medium, so as to obtain a high hysteresis loss magnetic medium; adopts measures such as increasing free electrons, ions and doping defects and vacancies on the conductive medium component of the heating medium, so as to optimize the utilization of the conductive loss of various carriers and obtain a high conductive loss conductive medium.

[0137] The present invention constructs the above dielectric, magnetic and conductive media by physical and chemical methods of multi-phase components to form a core-shell structure, a heterojunction structure, a coating structure, a porous structure and a membrane composite structure, and realizes the composite at the mesoscopic level, so as to facilitate multi-field coupling to produce multi-card giant heat effect:

[0138] ① Core-shell structure: Using ultrafine high hysteresis loss magnetic dielectric particles as cores, surface functionalization, and modification of high polarization loss dielectric materials by seed growth method, or using ultrafine high polarization loss dielectric particles as cores, surface functionalization, and modification of high hysteresis loss magnetic dielectric materials by seed growth method, to obtain a core-shell structure of electric moment-magnetic moment coupling heating medium; using ultrafine high polarization loss dielectric particles as cores, surface functionalization, and modification of high conductivity loss conductive dielectric materials by seed growth method, to obtain a core-shell structure of electric moment-conductivity coupling heating medium; using ultrafine high polarization loss dielectric particles as cores, surface functionalization, and modification of high hysteresis loss magnetic dielectric materials and high conductivity loss conductive dielectric materials by seed growth method, to obtain a core-shell structure of electric moment-magnetic moment-conductivity coupling heating medium. The core-shell structure can be prepared by direct precipitation method, co-precipitation method, or wet chemical method such as alcohol salt hydrolysis method or sol-gel method.

[0139] ② Heterojunction structure: High polarization loss dielectric particles and high hysteresis loss magnetic dielectric particles, due to different crystal structures and low lattice matching, are uniformly mixed in the contact interface region, and through epitaxial growth such as baking and melt precipitation, a heterojunction type electric moment-magnetic moment coupling heating medium is obtained; similarly, high polarization loss dielectric particles and high conductance loss conductive dielectric particles, are uniformly mixed in the contact interface region, and through epitaxial growth such as baking and melt precipitation, a heterojunction type electric moment-conductance coupling heating medium is obtained; high polarization loss dielectric particles, high hysteresis loss, high damping loss and resonance loss magnetic dielectric particles and high conductance loss conductive dielectric particles, are uniformly mixed in the contact interface region, and through epitaxial growth such as baking and melt precipitation, a heterojunction type electric moment-magnetic moment-conductance coupling heating medium is obtained. The heterojunction structure can be prepared by a molten salt method, a high-temperature solid-phase reaction method, a mechanical alloying method, a precipitation method with controlled calcination temperature, an alcohol salt hydrolysis method, a hydrothermal method, or a sol (gel)-hydrothermal method.

[0140] ③ Coating structure: Using high hysteresis loss magnetic medium as the mother particle, coating ultrafine high polarization loss dielectric sub-particles, and obtaining the electric moment-magnetic moment coupling heating medium of the coating structure; using high hysteresis loss magnetic medium as the mother particle, coating ultrafine high polarization loss dielectric sub-particles and ultrafine high conductivity loss conductive medium sub-particles, and obtaining the electric moment-magnetic moment-conductivity coupling heating medium of the coating structure. The coating structure can be prepared by mechanical methods, such as mechanical fusion coating equipment, through the mechanical chemical effect caused by mechanical forces such as shearing, friction, extrusion, and impact, to compound high polarization loss dielectric particles, high hysteresis loss magnetic medium particles, and high conductivity loss conductive medium particles. The coating structure can also be prepared by low-heat solid phase reaction method, or sol-gel method and other methods.

[0141] ④Porous structure: After fully mixing high hysteresis loss magnetic medium particles, high polarization loss dielectric particles, high conductivity loss conductive medium particles, inorganic binder sodium silicate, or aluminum dihydrogen phosphate, or phosphoric acid-copper oxide, and pore-forming agent, sintering is performed, and the porous sintered body is appropriately crushed and graded to obtain a porous structure of electric moment-magnetic moment-conductivity coupling heating medium. In addition, the porous structure can be prepared by polymer network gel method and metal complex gel method. The porous structure can also be modified by precipitation method of high polarization loss dielectric porous ceramics by using high hysteresis loss magnetic medium ions and high conductivity loss conductive medium ions in the solution through appropriate precipitants, so that a composite film layer of high hysteresis loss magnetic medium and high conductivity loss conductive medium is formed on the inner surface of the pores, and a porous structure of electric moment-magnetic moment-conductivity coupling heating medium is obtained. The porous structure can also use chemical plating to modify the pores of high polarization loss dielectric porous ceramics. The high conductivity loss dielectric metal ions adsorbed in the plating solution in the pores are catalytically reduced to metals by the reducing agent in the plating solution and deposited on the inner surface of the pores to obtain a porous structure of torque-conductivity coupled heating medium.

[0142] ⑤ Membrane composite structure: The binder sodium silicate, or aluminum dihydrogen phosphate, or phosphoric acid-copper oxide, and the composite high hysteresis loss magnetic medium particles and high polarization loss dielectric particles are used to form a single-sided or double-sided film composite on a metal sheet, such as aluminum foil, or copper foil, or copper sheet, or stainless steel sheet, by a casting method or a spraying method to obtain a membrane composite structure of electric moment-magnetic moment-conductivity coupling heating medium. The membrane composite structure can also be prepared by chemical vapor deposition, or gas phase pyrolysis, or gas phase hydrolysis, or gas phase combustion, or flame vapor deposition.

[0143] The present invention reduces the thermal excitation temperature of the aerosol generating matrix by adsorbing the liquid phase components of the aerosol generating medium through the heating medium of the porous structure, so that the liquid phase components are differentiated into a large number of small droplets. According to the Kelvin equation:

[0144]

[0145] Where p r ,p0 are the saturated vapor pressure values ​​of small droplets and plane liquids, σ,ρ,M are the surface tension, density and molar mass of the liquid, R,T are the gas constant and the absolute temperature of the gas, and r is the radius of the small droplet. Based on this, the saturated vapor pressure value of smaller droplets is higher than that of larger droplets, that is, the smaller the droplet size, the higher the saturated vapor pressure value and the faster the evaporation rate, and the low excitation temperature aerosol generation matrix is ​​obtained.

[0146] In a specific embodiment of the present invention, the aerosol generating matrix includes a heating medium; the heating medium is selected from first heating medium particles or second heating medium particles; the first heating medium particles include a first dielectric, a first magnetic medium and a first conductive medium; the second heating medium particles include a second dielectric, a second magnetic medium and a second conductive medium;

[0147] The present invention uses physical and chemical methods to perform mesoscopic composite construction on a first dielectric, a first magnetic medium, a first conductive medium, a second dielectric, a second magnetic medium and a second conductive medium to form a heating medium having one or more of a core-shell structure, a heterogeneous structure, a coating structure, a porous structure or a membrane composite structure that complies with multi-field coupling to generate a multi-card giant heat effect.

[0148] In the present invention, the first dielectric includes high moment orientation polarization loss and high thermal ion relaxation polarization loss components; the first dielectric includes one or more of a perovskite structure system, a tungsten bronze structure system, a bismuth layered structure system and a pyrochlore structure system; the perovskite structure system includes one or more of BaTiO3, PbTiO3, NaNbO3, KNbO3 and BiFeO3; the tungsten bronze structure system includes lead metaniobate and / or Sr 1-x Ba x Nb2O6 (x = 0 ~ 1.0); the bismuth layered structure system includes SrBi2Ta2O9, Bi4Ti3O 12 and SrBi4Ti4O 15 One or more of; the pyrochlore structure system includes Cd2Nb2O7 and / or Pb2Nb2O7.

[0149] In the present invention, the first magnetic medium is a component with high hysteresis loss, high damping loss, high domain wall resonance loss and high natural resonance loss, preferably spinel ferrite, and the spinel ferrite includes MFe2O4 (M=Mn, and / or Fe, and / or Ni, and / or Co, and / or Cu, and / or Mg, and / or Zn, and / or Li), and / or MnZn, and / or NiZn, and / or MgZn, and / or LiZn ferrite; and / or R3Fe5O 12 , R is a rare earth element (Y, and / or La, and / or Pr, and / or Nd, and / or Sm, and / or Eu, and / or Gd, and / or Tb, and / or Dy, and / or Ho, and / or Er, and / or Tm, and / or Yb, and / or Lu).

[0150] In the present invention, the second dielectric component is a component with high intrinsic moment orientation polarization loss, high thermal ion relaxation polarization loss and high resonance polarization loss; selected from ①BaO-MgO-Ta2O5, and / or BaO-ZnO-Ta2O5, and / or BaO-MgO-Nb2O5, and / or BaO-ZnO-Nb2O5 system and their composite system; ②BaTi4O9, and / or BaTi9O 20 , (Zr, and / or Sn)TiO4-based systems; ③BaO-Ln2O3-TiO2, and / or CaO-Li2O-Ln2O3-TiO2 (Ln2O3 is a lanthanide rare earth oxide)-based systems; ④A5B4O 15 (A=Ba, and / or Sr, and / or Mg, and / or Zn, and / or Ca, B=Nb, and / or Ta), and / or AB2O6 (A=Ca, and / or Co, and / or Mn, and / or Ni, and / or Zn; B=Nb, and / or Ta); (Ba 1- x M x )ZnO5(M=Ca, and / or Sr, x=0~1.0),AgNb 1-x Ta x O3 (x = 0 ~ 1.0), and / or LnAlO3 (Ln = La, and / or Nd, and / or Sm), and / or Ta2O5-ZrO2, and / or ZnTiO3, and / or BiNbO4 series.

[0151] In the present invention, the second magnetic medium is a component with high hysteresis loss, high damping loss, high domain wall resonance loss, high natural resonance loss, high size resonance loss and high spin wave resonance loss; the second magnetic medium is preferably selected from M-type hexagonal ferrite: BaM, and / or PbM, and / or SrM; X-type hexagonal ferrite, including Fe2X; W-type hexagonal ferrite, including Mg2W, and / or Mn2W, and / or Fe2W, and / or Co2W , and / or Ni2W, and / or Cu2W, and / or Zn2W; Y-type hexagonal ferrite including Mg2Y, and / or Mn2Y, and / or Fe2Y, and / or Co2Y, and / or Ni2Y, and / or Cu2Y, and / or Zn2Y; Z-type hexagonal ferrite including Mg2Z, and / or Mn2Z, and / or Fe2Z, and / or Co2Z, and / or Ni2Z, and / or Cu2Z, and / or Zn2Z.

[0152] The first conductive medium and / or the second conductive medium are multi-carrier high conductivity loss components that increase free electrons, ions, and doping defects and vacancies; the first conductive medium and / or the second conductive medium are selected from the ZnO series, including doped Al (AZO), and / or doped In (IZO), and / or doped Ga (GZO); magnetic oxides, including CoO, and / or MnO, and / or Fe3O4, and / or NiO; and other semiconductor oxides, including Ga2O3, and / or In2O3, and / or InSnO (ITO). The conductive medium can be a single component as one of the composite components of the heating medium, or it can be added separately or simultaneously in the dielectric component and the magnetic medium component.

[0153] In the present invention, the first heating medium with a core-shell structure has three structural forms. The first structural form is a core-shell structure electric moment-magnetic moment coupling heating medium 1-H-1, which uses ultrafine particles of the first magnetic medium as the core and modifies the first dielectric by a seed growth method, or uses ultrafine particles of the first dielectric as the core and modifies the first magnetic medium component by a seed growth method to obtain the core-shell structure electric moment-magnetic moment coupling heating medium 1-H-1; the second structural form is a core-shell structure electric moment-conductivity coupling heating medium 1-H-2, which uses ultrafine particles of the first dielectric as the core and modifies the first conductive medium by a seed growth method; the third structural form is a core-shell structure electric moment-magnetic moment-conductivity coupling heating medium 1-H-3, which uses ultrafine particles of the first dielectric as the core and modifies the first magnetic medium and the first conductive medium by a seed growth method;

[0154] The first heating medium having the core-shell structure is formed by mesoscopic-scale compounding through physical and chemical methods, and the specific preparation method is direct precipitation method, or coprecipitation method, or alcohol salt hydrolysis method, or sol-gel method.

[0155] In the present invention, the first heating medium with a heterojunction structure has three structural forms. The first structural form is an electric moment-magnetic moment coupled heating medium 1-Y-1 with a heterojunction structure, which is obtained by calcining, melting and precipitating the first dielectric and the first magnetic medium in a uniformly mixed state; the second structural form is an electric moment-conductivity coupled heating medium 1-Y-2 with a heterojunction structure, which is obtained by calcining, melting and precipitating the first dielectric and the first conductive medium in a uniformly mixed state; the third structural form is an electric moment-magnetic moment-conductivity coupled heating medium 1-Y-3 with a heterojunction structure, which is obtained by calcining, melting and precipitating the first dielectric, the first magnetic medium and the first conductive medium in a uniformly mixed state.

[0156] The first heating medium having the heterojunction structure is formed by mesoscopic-scale compounding through physical and chemical methods, and the specific preparation method is a molten salt method, or a high-temperature solid-phase reaction method, or a mechanical alloying method, and a precipitation method with controlled calcination temperature, or an alcohol salt hydrolysis method, or a hydrothermal method, or a sol (gel)-hydrothermal method.

[0157] In the present invention, the first heating medium with a coated structure has two structural forms. The first structural form is an electric moment-magnetic moment coupled heating medium 1-B-1 with a coated structure, which is obtained by taking the first magnetic medium as the mother particle and coating the ultrafine particles of the first dielectric; the second structural form is an electric moment-magnetic moment-conductivity coupled heating medium 1-B-2 with a coated structure, which is obtained by taking the first magnetic medium component as the mother particle and coating the ultrafine particles of the first dielectric and the ultrafine particles of the conductive medium.

[0158] The first heating medium having the coated structure is formed by mesoscopic-scale compounding through physical and chemical methods, and the specific preparation method is mechanical fusion coating method, or mechanical chemical effect method induced by high-energy mill, or low-heat solid phase reaction method, or sol-gel method.

[0159] In the present invention, the first heating medium having a porous structure is an electric moment-magnetic moment-conductivity coupling heating medium 1-K having a porous structure.

[0160] The first heating medium 1-K having a porous structure is formed by mesoscopic composite of physical and chemical methods, and the specific preparation method is: ultrafine particles of the first dielectric, ultrafine particles of the first magnetic medium, and ultrafine particles of the first conductive medium are fully mixed with inorganic binder sodium silicate, or aluminum dihydrogen phosphate, or phosphoric acid-copper oxide, and pore-forming agent ultrafine carbon powder or starch, or ultrafine calcium carbonate, and then sintered, crushed and classified to obtain;

[0161] or the ultrafine particles of the first dielectric, the ultrafine particles of the first magnetic medium and the ultrafine particles of the first conductive medium are subjected to a polymer network gel method using an N,N-methylenebisacrylamide network agent and ammonium sulfate to initiate a free radical polymerization reaction of acrylamide, and the obtained gel is dried, sintered, crushed and classified;

[0162] Or the precursor solution prepared from the first magnetic medium and the conductive medium is uniformly mixed with the ultrafine particles of the first dielectric, and a complexing agent is added to react with metal ions to form a complex, and the obtained soluble complex network gel is dried, sintered, crushed and classified;

[0163] or the porous body of the first dielectric is modified by a precipitation method using the ions of the first magnetic medium component and the ions of the conductive medium component in the solution and a precipitant, so that a composite film layer of the first magnetic medium component and the first conductive medium component is formed on the inner surface of the pores;

[0164] In the present invention, the pore size of the porous structured first heating medium 1-K is 2 nm to 50 μm, and the porosity is 70% to 95%.

[0165] The present invention preferably selects the electric moment-magnetic moment-conductivity coupling heating medium 1-K of the porous structure to obtain the heating medium 1-D of the low excitation temperature aerosol generating matrix. Specifically, the heating medium 1-D of the low excitation temperature aerosol generating matrix is ​​selected from the electric moment-magnetic moment-conductivity coupling heating medium 1-K of the porous structure, and the one that meets the principle conditions of the Kelvin equation is selected, and the pore size range is 60nm to 50μm, the porosity range is 85% to 95%, and the specific heat capacity range is 0.1kJ·kg -1 ·K -1 Up to 0.6 kJ·kg -1 ·K -1 , thermal conductivity range is 0.035W·m -1 ·K -1 Up to 0.125W·m -1 ·K -1 The particles with different physical property parameters adsorb the liquid phase components of the aerosol generating medium, so that the liquid phase components are separated into small droplets that enter the pores with a porosity of 85% to 95%, and the pore size range is 60nm to 50μm, so as to increase the saturated vapor pressure value of the liquid phase components of the aerosol generating medium, and obtain the heating medium of the low excitation temperature aerosol generating matrix, the excitation temperature is 160℃~200℃, and the particle size distribution range of the heating medium 1-D particles of the low excitation temperature aerosol generating matrix is ​​15μm to 500μm.

[0166] In the present invention, the first heating medium of the membrane composite structure is an electric moment-magnetic moment-conductivity coupling heating medium 1-M of the membrane composite structure, which is composited at a mesoscopic scale by a physical and chemical method; the specific preparation method for forming the electric moment-magnetic moment-conductivity coupling heating medium 1-M having the membrane composite structure is to fully mix the binder sodium silicate, or aluminum dihydrogen phosphate, or phosphoric acid-copper oxide, with the ultrafine particles of the first dielectric, the ultrafine particles of the first magnetic medium and the ultrafine particles of the first conductive medium, and then perform single-sided or double-sided film composite on the aluminum sheet, copper sheet or stainless steel sheet by spraying or brushing to obtain the electric moment-magnetic moment-conductivity coupling heating medium 1-M of the membrane composite structure; or adopt chemical vapor deposition, or gas phase pyrolysis, or gas phase hydrolysis, or gas phase combustion, or flame vapor deposition, or plasma spraying to prepare the electric moment-magnetic moment-conductivity coupling heating medium 1-M of the membrane composite structure.

[0167] In the present invention, the second heating medium with a core-shell structure has three structural forms. The first structural form is a core-shell structure electric moment-magnetic moment coupled heating medium 2-H-1, which is obtained by modifying the second dielectric by a seed growth method with ultrafine particles of the second magnetic medium as the core; or is obtained by modifying the second magnetic medium by a seed growth method with ultrafine particles of the second dielectric as the core; the second structural form is a core-shell structure electric moment-conductivity coupled heating medium 2-H-2, which is obtained by modifying the conductive medium component material by a seed growth method with ultrafine particles of the second dielectric as the core; the third structural form is a core-shell structure electric moment-magnetic moment-conductivity coupled heating medium 2-H-3, which is obtained by modifying the second magnetic medium component material and the conductive medium component material by a seed growth method with ultrafine particles of the second dielectric as the core.

[0168] The second heating medium having the core-shell structure is formed by mesoscopic-scale compounding through physical and chemical methods, and the specific preparation method is direct precipitation method, or coprecipitation method, or alcohol salt hydrolysis method or sol-gel method.

[0169] In the present invention, the second heating medium with a heterojunction structure has three structural forms. The first structural form is an electric moment-magnetic moment coupled heating medium 2-Y-1 with a heterojunction structure, which is obtained by calcining, melting and precipitating the second dielectric component particles and the second magnetic medium component particles in a uniformly mixed state; the second structural form is an electric moment-conductivity coupled heating medium 2-Y-2 with a heterojunction structure, which is obtained by calcining, melting and precipitating the second dielectric component particles and the second conductive medium component particles in a uniformly mixed state; the third structural form is an electric moment-magnetic moment-conductivity coupled heating medium 3-Y-3 with a heterojunction structure, which is obtained by calcining, melting and precipitating the second dielectric component particles, the second magnetic medium component particles and the second conductive medium component particles in a uniformly mixed state.

[0170] The second heating medium having a heterojunction structure is formed by mesoscopic-scale composite using physical and chemical methods. The specific preparation methods include molten salt method, high-temperature solid-phase reaction method, mechanical alloying method, precipitation method with controlled calcination temperature, alcohol salt hydrolysis method, hydrothermal method, or sol (gel)-hydrothermal method.

[0171] In the present invention, the second heating medium with a coating structure has two structural forms. The first structural form is an electric moment-magnetic moment coupling heating medium 2-B-1 with a coating structure, which is obtained by taking the second magnetic medium component as a mother particle and coating the ultrafine particles of the second dielectric component; the second structural form is an electric moment-magnetic moment-conductivity coupling heating medium 2-B-2 with a coating structure, which is obtained by taking the second magnetic medium component as a mother particle and coating the sub-ultrafine particles of the second dielectric component and the sub-ultrafine particles of the conductive medium component;

[0172] The second heating medium having the coating structure is formed by mesoscopic-scale compounding through physical and chemical methods, and the specific preparation method is mechanical fusion coating method, or mechanical chemical effect method induced by high-energy mill, or low-heat solid phase reaction method and sol-gel method.

[0173] In the present invention, the second heating medium with a porous structure is an electric moment-magnetic moment-conductivity coupling heating medium 2-K with a porous structure. The specific preparation method of the electric moment-magnetic moment-conductivity coupling heating medium 2-K is to form a porous structure through mesoscopic compounding by physical and chemical methods. The second dielectric component ultrafine particles, the second magnetic medium component ultrafine particles, and the conductive medium component ultrafine particles are fully mixed with an inorganic binder sodium silicate, or aluminum dihydrogen phosphate, or phosphoric acid-copper oxide, and a pore-forming agent ultrafine carbon powder or starch, or ultrafine calcium carbonate, and then sintered, crushed and classified to obtain the second heating medium; or the second dielectric component ultrafine particles, the second magnetic medium component ultrafine particles, and the conductive medium component ultrafine particles are mixed with an N,N-methylenebisacrylamide network agent and ammonium sulfate to initiate a propylene The polymer network gel method of amide free radical polymerization reaction is obtained by drying, sintering, crushing and grading the obtained gel; or the precursor solution prepared by the second magnetic medium component and the conductive medium component is uniformly mixed with the second dielectric component ultrafine particles, and a complexing agent is added to react with metal ions to form a complex, and the obtained soluble complex network gel is dried, sintered, crushed and graded to obtain it; or the porous body of the second dielectric component is modified by precipitation method using the ions of the second magnetic medium component and the ions of the conductive medium component and the precipitant in the solution, so that a composite film layer of the second magnetic medium component and the conductive medium component is formed on the inner surface of the pores to obtain it; the pore size of the porous structure is 2nm to 50μm, and the porosity is 70% to 95%.

[0174] In the present invention, the second heating medium with a porous structure can also be a heating medium 2-D of a low excitation temperature aerosol generating matrix. The heating medium 2-D of the low excitation temperature aerosol generating matrix is ​​selected from the electric moment-magnetic moment-conductance coupling heating medium 2-K of the porous structure, and the one that meets the principle conditions of the Kelvin equation is selected, and the pore size range is 60nm to 50μm, the porosity range is 85% to 95%, and the specific heat capacity range is 0.1kJ·kg -1 ·K -1 Up to 0.6 kJ·kg -1 ·K -1 , thermal conductivity range is 0.035W·m -1 ·K -1 Up to 0.125W·m -1 ·K -1The particles with different physical property parameters adsorb the liquid phase components of the aerosol generating medium, so that the liquid phase components are separated into small droplets entering the pores with a porosity of 85% to 95%, and the pore size range is 60nm to 50μm, so as to increase the saturated vapor pressure value of the liquid phase components of the aerosol generating medium, and obtain the heating medium of the low excitation temperature aerosol generating matrix, the excitation temperature is 160℃ to 200℃, and the particle size distribution range of the 2-D particles of the heating medium of the low excitation temperature aerosol generating matrix is ​​15μm to 500μm.

[0175] In the present invention, the second heating medium with a film composite structure is an electric moment-magnetic moment-conductivity coupling heating medium 2-M with a film composite structure. The specific preparation method of the electric moment-magnetic moment-conductivity coupling heating medium 2-M with the film composite structure formed by the mesoscopic scale composite method of the physical and chemical method is as follows: the binder sodium silicate, or aluminum dihydrogen phosphate, or phosphoric acid-copper oxide, and the second dielectric component ultrafine particles, the second magnetic medium component ultrafine particles and the conductive medium component ultrafine particles are fully mixed, and then the aluminum sheet, copper sheet or stainless steel sheet is subjected to single-sided or double-sided film composite by spraying or brushing to obtain the electric moment-magnetic moment-conductivity coupling heating medium 2-M with the film composite structure; or the electric moment-magnetic moment-conductivity coupling heating medium 2-M with the film composite structure is prepared by chemical vapor deposition, gas phase pyrolysis, gas phase hydrolysis, gas phase combustion, flame vapor deposition, or plasma spraying.

[0176] In the present invention, the particle size distribution range of the first dielectric component particles, or the first magnetic medium component particles, or the second dielectric component particles, or the second magnetic medium component particles, or the first conductive medium component particles is 20nm to 200μm. The particle size of the ultrafine particles of the first dielectric component, or the ultrafine particles of the first magnetic medium component, or the ultrafine particles of the second dielectric component, or the ultrafine particles of the second magnetic medium component, or the ultrafine particles of the second conductive medium component is 20nm to 10μm; the ultrafine particles meet the physical property requirements of the dense ultrafine particle aggregates to generate electromagnetic waves and heat.

[0177] In the present invention, the aerosol generating system heating structure includes three structures, aerosol generating system heating structure A, aerosol generating system heating structure B and aerosol generating system heating structure C;

[0178] The heating structure A of the aerosol generating system is composed of a heating chamber a, a preheating shell, an aerosol generating section, an aerosol generating matrix, a particle heating medium, an aerosol matrix, a foil-shaped film composite heating medium, a metal particle layer filter medium, a sealing ring, a temperature control unit, etc. The main structural relationship is: the heating chamber a composed of a tubular electrode is fixedly connected to the middle part of the preheating shell, the aerosol generating section is placed in the central axial hole tube of the heating chamber a, the aerosol generating section contains an aerosol generating matrix, and the aerosol generating matrix The material contains a particle heating medium and an aerosol matrix, and can also be mixed with a foil-shaped film composite heating medium with a size comparable to that of tobacco flakes. A metal particle layer filter medium is sandwiched between the aerosol generating section and the filter section. The upper end of the heating chamber a is connected to the sealing ring and is nested in the upper part of the preheating shell. The temperature control unit passes through the central hole of the heating chamber a base and is placed in the aerosol generating section 2 to 5 mm. The heating chamber a base disc is evenly distributed with 8 to 36 through holes with a diameter of 0.3 to 2 mm. The heating chamber a base is an insulating Al2O3 ceramic.

[0179] The heating structure B of the aerosol generating system is composed of a heating chamber b, a preheating shell, an aerosol generating section, an aerosol generating matrix, a particle heating medium, an aerosol matrix, a foil-shaped film composite heating medium, a metal particle layer filter medium, a sealing ring and a temperature control unit, etc. The main structural relationship is: the heating chamber b composed of a plane plate and a block heating medium 1 is fixedly connected to the middle part of the preheating shell, the aerosol generating section is placed in the central axial hole tube of the heating chamber b, the aerosol generating section contains an aerosol generating matrix, and the aerosol generating The raw matrix contains a particle heating medium and an aerosol matrix, and can also be mixed with a foil-like film composite heating medium of the same size as tobacco flakes. A metal particle layer filter medium is sandwiched between the aerosol generating section and the filter section. The upper end of the heating chamber b is connected to the sealing ring and nested in the upper part of the preheating shell. The temperature control unit passes through the central hole of the heating chamber b base and enters the aerosol generating section 2 to 5 mm. The heating chamber a base disc is evenly distributed with 8 to 36 through holes with a diameter of 0.3 to 2 mm. The heating chamber b base is an insulating Al2O3 ceramic. Block heating medium 1 is a type of block heating medium;

[0180] The heating structure C of the aerosol generating system is composed of a heating chamber c, a preheating shell, an aerosol generating section, an aerosol generating matrix, a particle heating medium, an aerosol matrix, a foil-like film composite heating medium, a metal particle layer filter medium, a wave-transmitting ceramic tube and a temperature control unit. The main structural relationship is: the heating chamber c composed of a cubic block heating medium 2 is fixedly connected to the middle part of the preheating shell, the aerosol generating section is placed in the central axial hole tube of the heating chamber c, the aerosol generating section contains an aerosol generating matrix, the aerosol generating matrix contains a particle heating medium and an aerosol matrix, and a foil-like film composite heating medium with a size equivalent to that of a tobacco sheet can also be added, a metal particle layer filter medium is sandwiched between the aerosol generating section and the filter section, a wave-transmitting ceramic sealing tube is nested in the central axis of the heating chamber c, the wave-transmitting ceramic tube material is quartz ceramic SiO2 or high alumina ceramic Al2O3 or Si3N4 ceramic, and the temperature control unit is arranged at the lower side wall of the bottom c of the heating chamber. The block heating medium 2 is a type of the block heating medium.

[0181] In the present invention, the heating chamber a is composed of a tubular electrode plate, which is composed of a curved electrode 1 and a curved electrode 2 composited on the inner surface of a tubular insulating ceramic substrate. The curved electrode 1 and the curved electrode 2 are arranged in pieces, and the curved electrode 1 and the curved electrode 2 are 2 to 5 pieces each. Preferably, the curved electrode 1 and the curved electrode 2 are 3 pieces, which are spaced and opposite. Adjacent curved electrodes 1 and 2 are separated by insulating Al2O3 ceramics, and can also be filled with insulating materials such as polyimide or aramid resin (polyisophthalamide). The curved electrode 1 and the curved electrode 2 are both made of copper or silver thin sheets. The length of the heating chamber a is equivalent to that of the aerosol generating section, and the diameter is well known in the art. The heating chamber a is used for heating when the frequency of the alternating electromagnetic field is in the range of 0.3MHz to 300MHz. The curved electrode 1 is a type of the electrode 1, and the curved electrode 2 is a type of the electrode 2.

[0182] The heating chamber b is composed of a planar electrode 1, a planar electrode 2 and a block heating medium 1. The planar electrode 1 and the planar electrode 2 are arranged in parallel with each other, and the spacing is the diameter value of the aerosol generating section. A block heating medium 1 is sandwiched between the two ends of the planar electrode 1 and the planar electrode 2. A cylindrical hole is arranged at the symmetric center of the two sandwiched block heating media 1, and the diameter is the diameter value of the aerosol generating section, and the length is the length value of the aerosol generating section. The heating chamber b is used for heating when the frequency of the alternating electromagnetic field is in the range of 0.3MHz to 300MHz. The planar electrode 1 is a type of the electrode 1, and the planar electrode 2 is a type of the electrode 2.

[0183] The heating chamber c is composed of a block heating medium 2, a metal shielding shell and an antenna (such as a PIFA planar inverted F antenna) embedded in the block heating medium 2. The block heating medium 2 is in a cubic shape, and a cylindrical hole is provided on the axis of symmetry. The hole depth is equal to the length of the aerosol generating section. A wave-transmitting ceramic tube is nested in the cylindrical hole, and the inner diameter of the wave-transmitting ceramic tube is equal to the diameter of the aerosol generating section. An antenna (such as a PIFA planar inverted F antenna) is embedded in the block heating medium 2 corresponding to the air inlet seat hole of the heating chamber c. The antenna feeder foot extends to the outside of the block heating medium 2. An air inlet hole connected to the cylindrical hole is provided at the axis of symmetry of the block heating medium 2 between the cylindrical hole and the antenna. The air inlet hole is connected to the outside of the block heating medium 2 through several small holes. The metal shielding shell encloses the block heating medium 2. The heating chamber c is used for heating when the frequency of the alternating electromagnetic field is in the range of 0.3GHz to 30GHz.

[0184] In the present invention, the preheating shell is composed of a metal shielding shell surrounding the heating chamber a, or surrounding the heating chamber b, or surrounding the heating chamber c, and having a certain gap with the outer wall of the metal shielding shell of the heating chamber a, or the heating chamber b, or the heating chamber c, and the gap is about 1.5 to 3 mm. The base material of the preheating shell is hexagonal boron carbon nitrogen ternary absorbing ceramic (h-BCN), and the inner wall of the preheating shell is coated with a particle coating of a heating medium, and the film-forming agent is sodium silicate sol, or dihydrogen aluminum phosphate sol, or aluminum hydroxide sol, or silica sol, and is sintered and solidified at a high temperature of more than 800°C.

[0185] The room temperature airflow flows through the gap space from the air inlet hole to be preheated, and then is introduced into the heating chamber a, or the heating chamber b, or the heating chamber c; the preheating shell is made of the electric moment-magnetic moment-conductivity coupling heating medium 1-M material of the membrane composite structure, and is used to surround the heating chamber a or the heating chamber b; the preheating shell is made of the electric moment-magnetic moment-conductivity coupling heating medium 2-M material of the membrane composite structure, and is used to surround the heating chamber c.

[0186] In the present invention, the aerosol generating section contains an aerosol generating matrix and a metal particle layer filter medium, or further contains a foil-shaped film composite heating medium cut to the size of a tobacco sheet, and has a cigarette-shaped appearance and a size known in the art. The mixing mass ratio of the foil-shaped film composite heating medium is 3 to 30%. Specifically, the aerosol generating section 1 is composed of an aerosol generating matrix 1 and a metal particle layer filter medium or contains the foil-shaped film composite heating medium 1-M, forming a structure that can be connected to the cigarette filter section, one end is connected to the filter section, and the other end is a free end, and the metal particle layer filter medium is between the connection interface of the filter section and the aerosol generating section 1; the aerosol generating section 2 is composed of an aerosol generating matrix 2 and a metal particle layer filter medium or contains the foil-shaped film composite heating medium 2-M, forming a structure that can be connected to the cigarette filter section, one end is connected to the filter section, and the other end is a free end, and the metal particle layer filter medium is between the connection interface of the filter section and the aerosol generating section 2.

[0187] One end of the aerosol generating matrix is ​​a free end, and the other end is connected to the filter segment, and the metal particle layer filter medium is between the connection interfaces. The filter segment can be a common filter well known in the art, or a new filter with special cooling, adsorption and filtering functions.

[0188] The aerosol generating matrix is ​​composed of a particle heating medium and an aerosol matrix. The particle heating medium is directly blended with the aerosol matrix, or the particle heating medium is mixed into a fiber slurry or paste before the tobacco sheet in the aerosol matrix is ​​paper-made or rolled, so that the tobacco sheet is evenly distributed with a particle heating medium of 5 to 60% by mass, or the particle heating medium with a porous structure or the low excitation temperature aerosol generating matrix adsorbs the liquid phase component in the aerosol matrix and then blends with the particle heating medium and the aerosol matrix. The liquid phase component in the aerosol matrix is ​​well known in the art; except for the liquid phase component, the other components of the aerosol matrix are composed of various monomer substrates and substrate carriers well known in the art.

[0189] In a specific embodiment, the aerosol generating substrate 1 is composed of the first heating medium particles and the aerosol substrate, the first heating medium particles are directly blended with the aerosol substrate, and the particle size distribution range of the first heating medium particles is 15 μm to 500 μm; or before the tobacco sheet in the aerosol substrate is papered or rolled, the first heating medium particles are mixed into the fiber slurry or paste, so that the tobacco sheet is uniformly distributed with the first heating medium particles having a mass ratio of 5% to 60%, and the particle size distribution range of the first heating medium particles is 0.1 μm to 100 μm; or The electric moment-magnetic moment-conductivity coupled heating medium 1-K particles with a porous structure adsorb the liquid phase components in the aerosol matrix and then blend with other aerosol matrices. The particle size distribution range of the electric moment-magnetic moment-conductivity coupled heating medium 1-K particles with a porous structure is 15μm to 500μm; or the heating medium 1-D particles of the low excitation temperature aerosol generating matrix are adsorbed with the liquid phase components in the aerosol matrix and then blended with other aerosol matrices. The particle size distribution range of the heating medium 1-D particles of the low excitation temperature aerosol generating matrix is ​​15μm to 500μm. The aerosol generating substrate 2 is composed of the second heating medium particles and the aerosol substrate. The second heating medium particles are directly blended with the aerosol substrate, and the particle size distribution range of the second heating medium particles is 15 μm to 500 μm; or before the tobacco sheet in the aerosol substrate is papered or rolled, the second heating medium particles are mixed into the fiber slurry or paste, so that the tobacco sheet is uniformly distributed with the second heating medium particles with a mass ratio of 5% to 60%, and the particle size distribution range of the second heating medium particles is 0.1 μm to 100 μm; or the multi- The electric moment-magnetic moment-conductivity coupling heating medium 2-K with a porous structure adsorbs the liquid phase components in the aerosol matrix and then blends with other aerosol matrices. The particle size distribution range of the electric moment-magnetic moment-conductivity coupling heating medium 2-K particles with a porous structure is 15μm to 500μm; or the heating medium 2-D of the low excitation temperature aerosol generating matrix adsorbs the liquid phase components in the aerosol matrix and then blends with other aerosol matrices. The particle size distribution range of the heating medium 2-D particles of the low excitation temperature aerosol generating matrix is ​​15μm to 500μm.

[0190] The particle heating medium is compositely constructed by a multi-component physical and chemical method using the high polarization loss dielectric, high hysteresis loss magnetic medium and high conductivity loss conductive medium, and has one of the structures selected from the group consisting of a core-shell structure, a heterojunction structure, a coating structure and a porous structure, or particles of a mixture of multiple structures thereof, and has a particle size distribution range of 0.1 μm to 500 μm, wherein the particle size distribution range of the particle heating medium directly blended with the aerosol matrix is ​​15 μm to 500 μm; the particle size distribution range of the particle heating medium added to the tobacco sheet papermaking slurry or roller-pressed paste is 0.1 μm to 100 μm.

[0191] The block heating medium is compositely constructed by a multi-component physical and chemical method using the high polarization loss dielectric, high hysteresis loss magnetic medium and high conductivity loss conductive medium, and has one of the structures selected from the group consisting of a core-shell structure, a heterojunction structure, a coating structure and a porous structure, or a plurality of structural particles thereof are mixed with an inorganic binder such as sodium silicate, or aluminum dihydrogen phosphate, or phosphoric acid-copper oxide, and then formed by pressing and low-temperature calcination. In a specific case, the block heating medium 1 is formed by mixing the first heating medium with an inorganic binder such as sodium silicate, or aluminum dihydrogen phosphate, or phosphoric acid-copper oxide, and then pressing and low-temperature calcination; the block heating medium 2 is formed by mixing the second heating medium with an inorganic binder such as sodium silicate, or aluminum dihydrogen phosphate, or phosphoric acid-copper oxide, and then pressing and low-temperature calcination.

[0192] The foil-like film composite heating medium is composited by a multi-component physical and chemical method using the high polarization loss dielectric, high hysteresis loss magnetic medium and high conductance loss conductive medium, and has one of a core-shell structure, a heterojunction structure, a coated structure and a porous structure, or mixed particles of multiple structures thereof. The foil-like film composite is prepared by a casting method or a spraying method, or other preparation methods such as chemical vapor deposition, gas phase pyrolysis, gas phase hydrolysis, gas phase combustion and flame vapor deposition, to form a single-sided or double-sided film on aluminum foil or copper foil, and then cut to obtain a size comparable to that of tobacco flakes.

[0193] The metal particle layer filter medium is formed by pressing aluminum particles with a size of 0.5 to 1 mm and a thickness of about 0.5 to 2 mm.

[0194] The present invention provides an aerosol generating system using a multi-card coupling giant thermal effect, comprising a heating structure, wherein the heating structure comprises a casing, and an air inlet hole is arranged on the casing;

[0195] A preheating shell is arranged inside the casing; the casing and the preheating shell have coaxial openings;

[0196] The opening of the preheating shell is connected to the filter segment; the preheating shell is provided with a preheating shell air inlet hole;

[0197] A plurality of pole plates are arranged inside the preheating housing; the plurality of pole plates form a heating chamber;

[0198] A heating chamber base is provided at the bottom of the heating chamber; a temperature control unit passes through the central hole of the heating chamber base, and a base disc air inlet hole is provided on the heating chamber base;

[0199] The upper end of the heating chamber is connected to the sealing ring and is nested in the opening of the preheating shell;

[0200] The interior of the electrode plate is an aerosol generating section; a metal particle layer filter medium is provided between the aerosol generating section and the filter tip section;

[0201] The aerosol generating section contains an aerosol generating matrix 1;

[0202] The electrode plate is connected to the heating drive unit via an electrode plate feeder;

[0203] The aerosol generating substrate 1 includes the first heating medium.

[0204] The present invention also provides an aerosol generating system using the multi-card coupling giant thermal effect, comprising a heating structure, wherein the heating structure comprises a casing, and the casing is provided with a casing air inlet hole;

[0205] A preheating shell is arranged inside the casing; the casing and the preheating shell have coaxial openings;

[0206] The opening of the preheating shell is connected to the filter segment; the preheating shell is provided with a preheating shell air inlet hole;

[0207] The preheating shell is provided with a metal shielding shell, a block heating medium 2 and an antenna embedded in the block heating medium 2; the metal shielding shell is wrapped around the outside of the block heating medium 2;

[0208] The metal shielding shell, the block heating medium 2 and the antenna embedded in the block heating medium 2 form a heating cavity;

[0209] The air inlet seat hole of the heating chamber is connected to the outside of the block heating medium 2 through 4 to 10 air inlet channels with a diameter of 0.5 to 2 mm;

[0210] The block heating medium 2 is a cube; a cylindrical hole is provided on the symmetry axis of the block heating medium 2, and an aerosol generating section is formed inside the hole; a wave-transmitting ceramic tube is nested inside the cylindrical hole, and the inner diameter of the wave-transmitting ceramic tube is the diameter of the aerosol generating section;

[0211] The upper end of the heating chamber is connected to the sealing ring and is nested in the opening of the preheating shell;

[0212] A metal particle layer filter medium is provided between the aerosol generating section and the filter tip section;

[0213] The aerosol generating section contains an aerosol generating matrix 2;

[0214] The antenna is connected to the heating drive unit via an antenna feeder foot;

[0215] The aerosol generating substrate 2 includes the second heating medium.

[0216] In the present invention, the aerosol generating system has three forms, namely the first aerosol generating system form, the second aerosol generating system form and the third aerosol generating system form, which respectively have an aerosol generating system heating structure A, an aerosol generating system heating structure B and an aerosol generating system heating structure C, wherein:

[0217] The first aerosol generation system is mainly composed of an aerosol generation section, an aerosol generation matrix, a metal particle layer filter, or a foil-shaped film composite heating medium, a heating chamber a, a tubular electrode plate, a curved electrode 1 and a curved electrode 2, a tubular insulating ceramic substrate, a heating chamber a base, a temperature control unit, a preheating shell, a heating drive unit and a casing, wherein the heating drive unit is composed of a power amplifier and control, an alternating electromagnetic field generator and a battery, and the alternating voltage provided by the power amplifier and the control unit is connected to the curved electrode 1 and the curved electrode 2 respectively through a feeder;

[0218] The second aerosol generation system is mainly composed of an aerosol generation section, an aerosol generation matrix, a metal particle layer filter, or a foil-shaped film composite heating medium, a heating chamber b, a planar electrode 1 and a planar electrode 2, a block heating medium 1, a heating chamber b base, a temperature control unit, a preheating shell, a heating drive unit and a casing, wherein the heating drive unit is composed of a power amplifier and control, an alternating electromagnetic field generator and a battery, and the alternating voltage provided by the power amplifier and the control unit is connected to the planar electrode 1 and the planar electrode 2 respectively through a feeder;

[0219] The third type of aerosol generating system is mainly composed of an aerosol generating section, an aerosol generating matrix, a metal particle layer filter, or a foil-like membrane composite heating medium, as well as a heating chamber c, a block heating medium 2, a wave-transparent ceramic tube, an antenna embedded in the block heating medium 2, an antenna feeder base, a PCB circuit board, a temperature control unit, a metal shielding shell, a preheating shell, a heating drive unit and a casing, wherein the heating drive unit is composed of a power amplifier and control, an alternating electromagnetic field generating source and a battery.

[0220] In the heating drive units of the three aerosol generating system forms, the alternating electromagnetic field frequency range used is 0.3MHz~30GHz; among them, the frequency range used by the first aerosol generating system form and the second aerosol generating system form is 0.3MHz~300MHz, which can meet the matching requirements of multi-card coupling of electric card, magnetic card and conductive card for multi-field coupling drive, and has a frequency range that is compatible and balanced with the multi-card coupling response frequency, that is, within this frequency range, the dielectric component can enhance the relaxation polarization loss of the inherent electric moment orientation polarization and the thermal ion relaxation polarization; the magnetic medium component can increase the hysteresis loss and damping loss and the domain wall resonance and natural resonance in the resonance loss; the conductive medium component can increase the conductivity loss of carriers such as free electrons and ions and the absorption loss of dense ultrafine particle aggregates. The frequency range adopted by the third type of aerosol generation system is 0.3GHz to 30GHz, which can meet the matching requirements of multi-card coupling of electric cards, magnetic cards and conductive cards for multi-field coupling drive, and has a frequency range that is compatible and balanced with the multi-card coupling response frequency, that is, within this frequency range, the dielectric component can enhance the relaxation polarization loss of inherent electric moment orientation polarization and thermal ion relaxation polarization, as well as the resonant polarization loss of ion displacement polarization; the magnetic medium component can increase the hysteresis loss and damping loss, as well as the domain wall resonance, natural resonance, size resonance, and spin wave resonance in the resonance loss; the conductive medium component can increase the conductivity loss of carriers such as free electrons and ions and the absorption loss of dense ultrafine particle aggregates.

[0221] In order to explain in detail the aerosol system using multicard coupling giant thermal effect of the present invention, please refer to the following content for details. :

[0222] See also Figure 1 to Figure 6 The invention relates to a first aerosol system form (01) of an aerosol system and method that mainly utilizes the multi-card coupling giant thermal effect. The materials and unit structures involved include: an aerosol generating section 1 (011), a preheating shell (012), a heating chamber a (013), a plate feeder (014), a power amplifier and control (015), an alternating electromagnetic field generator (016), a battery (017), a housing (018), and a metal particle layer filter medium (0111) (in order to prevent the radiation leakage of electromagnetic waves), an aerosol generating matrix 1 (0112), first heating medium particles (0113), a foil-shaped film composite The invention comprises a combined heating medium 1 (0114), an air inlet of a preheating shell (0121), an air inlet of a casing (0181), a substrate of a preheating shell (0122), a first heating medium particle coating (0123), a sealing ring (0131), a tubular electrode plate (0132), a base of a heating chamber a (0133), a temperature control unit (0134), an air inlet of a base disc (0135), a curved electrode 1 (01321) and a curved electrode 2 (01322), a gap insulating material (01323), a feeder connection position (01324) of the curved electrode 2 and a curved electrode 1 (01325).

[0223] The present invention Figure 1 The first aerosol generating system form (01) of the aerosol generating system and method utilizing multi-card coupling giant thermal effect is shown, and Figure 2 Shown with Figure 3 The aerosol generating system heating structure A at the AA section shown, and Figure 4 Shown with Figure 5 The aerosol generating section 1 at the AA section shown contains a foil-like film composite heating medium 1, and Figure 6 The curved surface electrode 1 and the curved surface electrode 2 of the tubular electrode shown, the specific method for preparing the first heating medium particles (0113), the foil-shaped film composite heating medium 1 (0114) and the aerosol generating matrix 1 (0112) used, and the preparation basis and method of the curved surface electrode 1 (01321) and the curved surface electrode 2 (01322) of the tubular electrode (0132), and the first heating medium particle coating (0123), and the steps include:

[0224] In the first aerosol generating system form (01) of the aerosol generating system and method utilizing the multicard coupling giant thermal effect, the alternating electromagnetic field frequency range adopted by the heating drive unit is 0.3MHz to 300MHz, and the design principle for being compatible with and balancing the multicard coupling frequency response interval is: for dielectric components, enhancing the relaxation polarization loss of the inherent electric moment orientation polarization and the thermal ion relaxation polarization; for magnetic medium components, increasing the hysteresis loss and damping loss and domain wall resonance loss; for conductive medium components, increasing the conductivity loss of carriers such as free electrons and ions and the wave absorption loss of densely packed ultrafine particle aggregates. The heating medium particles suitable for the first aerosol generating system form (01) are referred to as the first heating medium particles in the present invention.

[0225] In the present invention, the design method of the first heating medium particles is: to perform physical and chemical composite construction of multi-phase components of dielectric, magnetic and conductive media, the heating medium adopts one or more structures of core-shell structure, heterojunction structure, coating structure, porous structure and membrane composite structure, so that each structure composites the dielectric, magnetic and conductive media at the mesoscopic level.

[0226] Step I-1 , the preparation of the first heating medium particles (0113) used in the first aerosol generating system form (01) of the aerosol generating system and method using multicard coupling giant thermal effect:

[0227] (1) The components of the dielectric include components that can enhance the intrinsic electric moment orientation polarization and thermionic relaxation polarization and lead to high relaxation polarization loss, and the components include: ① a perovskite structure system, including BaTiO3, and / or PbTiO3, and / or NaNbO3, and / or KNbO3, and / or BiFeO3; ② a tungsten bronze structure system, including lead metaniobate, and / or Sr 1- x Ba x Nb2O6; ③ Bismuth layered structure system, including SrBi2Ta2O9, and / or Bi4Ti3O 12 , and / or SrBi4Ti4O 15 ; ④ Pyrochlore structure system, including Cd2Nb2O7, and / or Pb2Nb2O7.

[0228] (2) The components of the magnetic medium include components that increase hysteresis loss, damping loss and domain wall resonance loss, and increase the absorption loss of dense ultrafine particle aggregates, and the components include: spinel ferrites, including MFe2O4 (M=Mn, and / or Fe, and / or Ni, and / or Co, and / or Cu, and / or Mg, and / or Zn, and / or Li), and / or MnZn, and / or NiZn, and / or MgZn, and / or LiZn ferrites; and / or R3Fe5O 12 , R is a rare earth element (Y, and / or La, and / or Pr, and / or Nd, and / or Sm, and / or Eu, and / or Gd, and / or Tb, and / or Dy, and / or Ho, and / or Er, and / or Tm, and / or Yb, and / or Lu)

[0229] (3) The components of the conductive medium include components that increase free electrons, ions, and doping defects and vacancies. The conductive medium can be a separate component as one of the composite components of the heating medium, or it can be added separately or simultaneously in the dielectric component and the magnetic medium component. The conductive medium components include: ZnO series, including doped Al (AZO), and / or doped In (IZO), and / or doped Ga (GZO); magnetic oxides, including CoO, and / or MnO, and / or Fe3O4, and / or NiO; and other semiconductor oxides, including Ga2O3, and / or In2O3, and / or InSnO (ITO).

[0230] (4) The present invention performs a physical and chemical composite construction of the dielectric, magnetic and conductive media using multi-phase components:

[0231] First, the component particles that increase the hysteresis loss, damping loss and domain wall resonance loss and increase the absorption loss of dense ultrafine particle aggregates as the core, or the component particles that enhance the inherent electric moment orientation polarization and thermal ion relaxation polarization to cause high relaxation polarization loss as the core, are modified on the surface of the core particles by direct precipitation method, coprecipitation method, alcohol salt hydrolysis method or sol-gel method using a precipitant, using the component ions that enhance the inherent electric moment orientation polarization and thermal ion relaxation polarization to cause high relaxation polarization loss, or the component ions that increase the hysteresis loss, damping loss and domain wall resonance loss and increase the absorption loss of dense ultrafine particle aggregates, or the component ions that increase free electrons, ions and doping defects and vacancies and other carriers as the ultrafine, and after calcination, a core-shell structure electric moment-magnetic moment coupling heating medium, or a core-shell structure electric moment-conductivity coupling heating medium is obtained;

[0232] Secondly, by means of a molten salt method, a high-temperature solid-phase reaction method or a mechanical alloying method, the ultrafine component particles that can lead to high relaxation polarization loss by enhancing the inherent electric moment orientation polarization and thermionic relaxation polarization are uniformly mixed with the ultrafine component particles that increase the hysteresis loss, damping loss and domain wall resonance loss, and increase the absorption loss of dense ultrafine particle aggregates; or the ultrafine component particles that can lead to high relaxation polarization loss by enhancing the inherent electric moment orientation polarization and thermionic relaxation polarization are uniformly mixed with the ultrafine component particles that increase carriers such as free electrons, ions, doping defects and vacancies; or the ultrafine component particles that increase the hysteresis loss are uniformly mixed with the ultrafine component particles that increase the hysteresis loss. , damping loss and domain wall resonance loss, and simultaneously increase the absorption loss of dense ultrafine particle aggregates, and the ultrafine particles that increase the hysteresis loss, damping loss and domain wall resonance loss, and simultaneously increase the absorption loss of dense ultrafine particle aggregates are uniformly mixed with the ultrafine particles that increase free electrons, ions and doping defects and vacancies and other carriers, and are melted and precipitated in the heterogeneous contact interface region by roasting to obtain the electric moment-magnetic moment coupling heating medium of the heterojunction structure; or obtain the electric moment-conductivity coupling heating medium of the heterojunction structure; or obtain the electric moment-magnetic moment-conductivity coupling heating medium of the heterojunction structure. It is also possible to obtain the electric moment-magnetic moment coupling heating medium of the heterojunction structure by epitaxial growth in the heterogeneous contact interface region by controlling the calcination temperature, or the alcohol salt hydrolysis method, or the hydrothermal method, or the sol (gel)-hydrothermal method, etc.; or obtain the electric moment-magnetic moment-conductivity coupling heating medium of the heterojunction structure; or obtain the electric moment-magnetic moment-conductivity coupling heating medium of the heterojunction structure;

[0233] Thirdly, the components that increase the hysteresis loss, damping loss and domain wall resonance loss as well as the absorbing loss of densely packed ultrafine particle aggregates are used as mother particles, and the component particles that can lead to high relaxation polarization loss by enhancing the inherent electric moment orientation polarization and thermal ion relaxation polarization are coated on the mother particles; or the components that increase the hysteresis loss, damping loss and domain wall resonance loss as well as the absorbing loss of densely packed ultrafine particle aggregates are used as mother particles, and the component particles that can lead to high relaxation polarization loss by enhancing the inherent electric moment orientation polarization and thermal ion relaxation polarization are coated on the component particles that increase free electrons, ions, doping defects and vacancies and other carriers are coated on the ultrafine; and the electric moment-magnetic moment-conductivity coupling heating medium of the coated structure is obtained through the mechanochemical effect caused by mechanical forces such as shear, friction, extrusion and impact of mechanical fusion coating equipment. For ultrafine particles that are slightly soluble in water or contain water of crystallization, which increase the hysteresis loss, damping loss and domain wall resonance loss, and at the same time increase the absorption loss of dense ultrafine particle aggregates, and ultrafine particles that enhance the inherent electric moment orientation polarization and thermal ion relaxation polarization and can lead to high relaxation polarization loss, they can be fully mixed and ground by a low-heat solid-phase reaction method to form a cold melt layer on the surface of the particles, and the precipitated ions diffuse with each other in the cold melt layer. As the grinding process continues, new cold melt layers are continuously formed on the surface of the particles. The cold melt layer on the surface of each particle is equivalent to a micro-reaction zone, and the generated products nucleate and grow to obtain an electric moment-magnetic moment-conductivity coupled heating medium with a coated structure. It is also possible to obtain a colloid particle dispersion system formed by the components that increase the hysteresis loss, damping loss and domain wall resonance loss of the ultrafine particles that can undergo polycondensation reaction, and increase the absorption loss of the dense ultrafine particle aggregates, and the components that enhance the inherent electric moment orientation polarization and thermal ion relaxation polarization to cause high relaxation polarization loss, through the further aggregation and bonding of the sol-gel condensation reaction to form a three-dimensional network structure, and then through low-temperature heat treatment digestion and high-temperature sintering to obtain an electric moment-magnetic moment-conductivity coupling heating medium with a coating structure;

[0234] Fourthly, the component particles that increase the hysteresis loss, damping loss and domain wall resonance loss as well as the absorption loss of dense ultrafine particle aggregates, the component particles that enhance the inherent electric moment orientation polarization and thermal ion relaxation polarization to cause high relaxation polarization loss, the component particles that increase free electrons, ions, doping defects and vacancies and other carriers, the inorganic binder sodium silicate, or aluminum dihydrogen phosphate, or phosphoric acid-copper oxide, and the pore-forming agent ultrafine carbon powder or starch, or ultrafine calcium carbonate are fully mixed, and then sintered, crushed and graded to obtain a porous structured electric moment-magnetic moment-conductivity coupled heating medium. The water-soluble ultrafine particles that increase hysteresis loss, damping loss and domain wall resonance loss, and at the same time increase the absorption loss of dense ultrafine particle aggregates, the ultrafine particles that enhance the inherent electric moment orientation polarization and thermal ion relaxation polarization to cause high relaxation polarization loss, and the ultrafine particles that increase free electrons, ions, doping defects, vacancies and other carriers can also be sintered by the polymer network gel method, using acrylamide free radical polymerization reaction and a network agent to connect the polymer chains into a network to obtain a gel. Or for the ultrafine component particles that are insoluble in alcohol and increase the hysteresis loss, damping loss and domain wall resonance loss, and at the same time increase the absorption loss of dense ultrafine particle aggregates, the ultrafine component particles that enhance the inherent electric moment orientation polarization and thermal ion relaxation polarization to cause high relaxation polarization loss, and the ultrafine component particles that increase free electrons, ions, doping defects and vacancies and other carriers, a metal complex gel method can be used, in which a complexing agent is added to the metal inorganic salt precursor solution to react with the metal ions to form a soluble complex or a network gel formed by a complex salt, and then sintering is performed to obtain a porous structure of electric moment-magnetic moment-conductivity coupled heating medium. It is also possible to modify the high polarization loss dielectric porous ceramic by precipitation method by using the ultrafine component ions in the solution that increase the hysteresis loss, damping loss and domain wall resonance loss, and increase the absorption loss of the dense ultrafine particle aggregates, and the ultrafine component ions that increase free electrons, ions, doping defects and vacancies, etc., so that the inner surface of the pores forms a composite film layer of the component that increases the hysteresis loss, damping loss and domain wall resonance loss, and increases the absorption loss of the dense ultrafine particle aggregates, and the component that increases free electrons, ions, doping defects and vacancies, etc., to obtain a porous structure of electric moment-magnetic moment-conductivity coupling heating medium. In addition, the pores of the high polarization loss dielectric porous ceramic can be modified by chemical plating, and the component metal ions that increase free electrons, ions, doping defects and vacancies, etc., which are adsorbed in the plating solution in the pores, are catalytically reduced to metals by the reducing agent in the plating solution, and are deposited on the inner surface of the pores to obtain a porous structure of electric moment-conductivity coupling heating medium;

[0235] Fifth, the electric moment-conductivity coupling heating medium particles with a core-shell structure obtained by the first physical and chemical method, or the electric moment-magnetic moment coupling heating medium particles with a heterojunction structure obtained by the second physical and chemical method, or the electric moment-conductivity coupling heating medium particles with a porous structure obtained by the fourth physical and chemical method are mixed with an inorganic binder such as sodium silicate, or aluminum dihydrogen phosphate, or phosphoric acid-copper oxide, and then a single-sided or double-sided film is composited on an aluminum sheet, a copper sheet, or a stainless steel sheet by spraying or brushing to obtain an electric moment-magnetic moment-conductivity coupling heating medium with a membrane composite structure. The components that increase hysteresis loss, damping loss and domain wall resonance loss, and increase the absorption loss of densely packed ultrafine particle aggregates, and the components that enhance inherent electric moment orientation polarization and thermal ion relaxation polarization to cause high relaxation polarization loss can also be composited on one or both sides of an aluminum sheet, a copper sheet or a stainless steel sheet by chemical vapor deposition, gas phase pyrolysis, gas phase hydrolysis, phase combustion, flame vapor deposition or plasma spraying to obtain an electric moment-magnetic moment-conductivity coupled heating medium with a membrane composite structure.

[0236] The first heating medium particles (0113) used in the first step are processed by a pulverizing method and / or a synthesis method to a particle size distribution range of 0.1μm to 500μm, wherein the particle size distribution range of the particle heating medium directly blended with the aerosol matrix is ​​15μm to 500μm; the particle size distribution range of the particle heating medium added to the tobacco sheet papermaking slurry or rolled paste is 0.1μm to 100μm.

[0237] Step I-2, Preparation of the foil-like film composite heating medium 1 (0114) used in the first aerosol generating system form (01) of the aerosol generating system and method using multicard coupling giant thermal effect:

[0238] The ultrafine particles of the first heating medium prepared in step I-1 are mixed with carboxymethyl cellulose, guar gum or tobacco extract, and then a single-sided or double-sided film is composited on an aluminum foil or copper foil by a casting method or a spraying method, and then the film is cut to obtain a size comparable to that of tobacco flakes, and the particle size distribution range of the first heating medium particles is 15μm to 100μm; the foil-like film composite heating medium 1, or a precursor of a first dielectric component and a first magnetic medium component is prepared by a chemical vapor deposition method, a gas phase pyrolysis method, a gas phase hydrolysis method, a gas phase combustion method, or a flame vapor deposition method, and a single-sided or double-sided film is composited on an aluminum foil or copper foil, and then the film is cut to obtain a size comparable to that of tobacco flakes.

[0239] Step I-3,Preparation of the aerosol generating substrate 1 (0112) used in the first aerosol generating system form (01) of the aerosol generating system and method using multicard coupling giant thermal effect:

[0240] The first heating medium particles (0113) prepared in step I-1 are directly blended with the aerosol matrix, and the particle size distribution range of the first heating medium particles is 15 μm to 500 μm. Alternatively, before the tobacco sheet in the aerosol matrix is ​​paper-made or rolled, the first heating medium particles (0113) prepared in step I-1 are mixed into the fiber slurry or paste, so that the tobacco sheet is uniformly distributed with 5 to 60% by mass of the first heating medium particles (0113) prepared in step I-1, and the particle size distribution range of the first heating medium particles is 0. 1μm to 100μm; or the electric moment-magnetic moment-conductivity coupled heating medium particles of the porous structure adsorb the liquid phase components in the aerosol matrix and then blend with other aerosol matrices, and the particle size distribution range of the electric moment-magnetic moment-conductivity coupled heating medium particles of the porous structure is 15μm to 500μm; or the heating medium particles of the low excitation temperature aerosol generating matrix adsorb the liquid phase components in the aerosol matrix and then blend with other aerosol matrices, and the particle size distribution range of the heating medium particles of the low excitation temperature aerosol generating matrix is ​​15μm to 500μm. The foil-like film composite heating medium 1 (0114) can also be added to the aerosol generating matrix 1 (0112), and the mixing mass ratio is 3 to 30%.

[0241] Step I-4, Preparation of the curved electrode 1 (01321) and the curved electrode 2 (01322) of the tubular electrode plate (0132) used in the first aerosol generation system form (01) of the aerosol generation system and method using multicard coupling giant thermal effect:

[0242] The tubular electrode plate (0132) is composed of the curved electrode 1 (01321) and the curved electrode 2 (01322) compounded on the inner surface of the tubular insulating ceramic substrate. The curved electrode 1 and the curved electrode 2 are divided into pieces and are opposed to each other. The curved electrode 1 and the curved electrode 2 are each 2 to 5 pieces. Preferably, the curved electrode 1 and the curved electrode 2 are each 3 pieces, which are opposed to each other at intervals. The adjacent curved electrodes 1 and curved electrodes 2 are separated by a gap insulating material (01323). The gap insulating material can be a tubular insulating ceramic substrate material, or a polyimide or aramid resin (polyisophthalamide). The ceramic substrate material is Al2O3 ceramic, the gap between the curved electrode 1 and the curved electrode 2 is 0.5-2mm, preferably, the gap between the curved electrode 1 and the curved electrode 2 is 1mm, the curved electrode 1 and the curved electrode 2 are made of copper or silver, the height of the curved electrode 1 and the curved electrode 2 is equivalent to the aerosol generating section, the diameter of the tubular electrode plate is the diameter value of the aerosol generating section, and a feeder connection position (01324) and (01325) are provided at the lower end of each curved electrode 1 and the curved electrode 2 corresponding to the tubular electrode plate (0132), which is connected to the heating drive unit of the aerosol generating system through the feeder.

[0243] Step I - 5 , the preparation of the first heating medium particle coating (0123) involved in the first aerosol generating system form (01) of the aerosol generating system and method using multicard coupling giant thermal effect:

[0244] The substrate of the first heating medium particle coating (0123) is hexagonal boron carbon nitrogen ternary absorbing ceramic (h-BCN), the first heating medium particles are fully mixed with a film-forming agent sodium silicate sol, or aluminum dihydrogen phosphate sol, or aluminum hydroxide sol, or silica sol, coated to form a film, and sintered and solidified at a high temperature above 800°C to form the first heating medium particle coating (0123). The first heating medium particle coating (0123) can also be based on a metal material, such as aluminum, or a copper or stainless steel sheet, coated with the particle heating medium (0112) prepared in the first step and an inorganic binder sodium silicate, or aluminum dihydrogen phosphate, or a phosphoric acid-copper oxide mixed slurry, and heat treated at 300°C to 450°C to form the preheating shell coating (0123). It can also be obtained by chemical vapor deposition, gas phase pyrolysis, gas phase hydrolysis, gas phase combustion, flame vapor deposition, or plasma spraying, by deposition and heating on aluminum, copper or stainless steel sheets.

[0245] Step I-6The metal particle layer filter medium (0111) is formed by pressing aluminum particles with a size of 0.5 to 1.5 mm and a thickness of about 0.2 to 1.2 mm; the sealing ring (0131) is made of silicone rubber; the heating chamber a base disc (0133) is made of insulating Al2O3 ceramic material. There are 8 to 36 through holes with a diameter of 0.3 to 2 mm evenly distributed on the disc; the temperature control unit (0134) passes through the central hole of the heating chamber a base and enters the aerosol generating section (011) 2 to 5 mm.

[0246] The present invention Figure 7 and Figure 8 The second aerosol generating system form (02) of the aerosol generating system and method utilizing the multicard coupling giant thermal effect, the materials and unit structures involved include: an aerosol generating section 1 (021), a preheating shell (022), a heating chamber b (023), a plate feeder (024), a power amplifier and control (025), an alternating electromagnetic field generator (026), a battery (027), a housing (028), and a metal particle layer filter (0211), an aerosol generating matrix 1 (0212), first heating medium particles (0213), a preheating shell air inlet (0221), a preheating shell substrate (0222), a first heating medium particle coating (0223), a sealing ring (0231), a planar plate (0232), a heating chamber b base (0233), a temperature control unit (0234), a block heating medium 1 (0235), a planar electrode 1 (02321) and a planar electrode 2 (02322).

[0247] The present invention Figure 7 The second aerosol generating system form (02) of the aerosol generating system and method utilizing multi-card coupling giant thermal effect, and Figure 8 The specific method for preparing the first heating medium particles (0213), the block heating medium 1 (0235), and the aerosol generating matrix 1 (0212) involved in the heating structure B of the aerosol generating system at the CC section shown, as well as the preparation basis and method of the planar electrode 1 (02321) and the planar electrode 2 (02322) and the first heating medium particle coating (0223), and the steps include:

[0248] In the second aerosol generating system form (02) of the aerosol generating system and method utilizing the multicard coupling giant thermal effect, the alternating electromagnetic field frequency range adopted by the heating drive unit is 0.3MHz to 300MHz, and the design principle for being compatible with and balancing the multicard coupling frequency response range is: for dielectric components, enhancing the relaxation polarization loss of the inherent electric moment orientation polarization and the thermal ion relaxation polarization; for magnetic medium components, increasing the hysteresis loss and damping loss and domain wall resonance loss; for conductive medium components, increasing the conductivity loss of carriers such as free electrons and ions and the absorption loss of densely packed ultrafine particle aggregates.

[0249] Step II-1 The preparation of the first heating medium particles (0213) in the second aerosol generating system is consistent with the preparation of the first heating medium particles (0113) used in the first aerosol generating system (01), and will not be repeated here.

[0250] The first heating medium particles (0213) prepared in step II-1 are processed by a pulverizing method and / or a synthesis method to have a particle size distribution range of 0.1μm to 500μm, wherein the particle size distribution range of the particle heating medium directly blended with the aerosol matrix is ​​15μm to 500μm; the particle size distribution range of the particle heating medium incorporated into the tobacco sheet papermaking slurry or rolled paste is 0.1μm to 100μm.

[0251] Step II-2 The block heating medium 1 (0235) used in the second aerosol generating system form (02) of the aerosol generating system and method utilizing the multicard coupling giant thermal effect is formed by mixing the first heating medium particles (0213) prepared in step II-2 with an inorganic binder such as sodium silicate, or dihydrogen aluminum phosphate, or phosphoric acid-copper oxide, through pressing and low-temperature calcination.

[0252] Step II-3The first heating medium particles (0213) prepared in step II-1 are directly blended with the aerosol matrix, and the particle size distribution range of the first heating medium particles is 15 μm to 500 μm. Alternatively, before the tobacco sheet in the aerosol matrix is ​​paper-made or rolled, the first heating medium particles (0213) prepared in the first step are mixed into the fiber slurry or paste, so that the tobacco sheet is uniformly distributed with 5 to 60% by mass of the first heating medium particles (0213) prepared in step II-1, and the particle size distribution range of the first heating medium particles is 0. 1μm to 100μm; or the electric moment-magnetic moment-conductivity coupled heating medium particles of the porous structure adsorb the liquid phase components in the aerosol matrix and then blend with other aerosol matrices, and the particle size distribution range of the electric moment-magnetic moment-conductivity coupled heating medium particles of the porous structure is 15μm to 500μm; or the heating medium particles of the low excitation temperature aerosol generating matrix adsorb the liquid phase components in the aerosol matrix and then blend with other aerosol matrices, and the particle size distribution range of the heating medium particles of the low excitation temperature aerosol generating matrix is ​​15μm to 500μm. The foil-like film composite heating medium 1 (0214) can also be added to the aerosol generating matrix 1 (0212), and the mixing mass ratio is 3 to 30%.

[0253] Step II-4 , the preparation of the planar electrode 1 (02321) and the planar electrode 2 (02322) of the planar plate (0232) used in the second aerosol generating system form (02) of the aerosol generating system and method using multicard coupling giant thermal effect:

[0254] The planar electrode (0232) is formed by compounding the planar electrode 1 (02321) and the planar electrode 2 (02322) on the surface of a planar insulating ceramic substrate. The planar electrode 1 and the planar electrode 2 are made of copper or silver, and the insulating ceramic substrate material is Al2O3 ceramic.

[0255] Step II-5 , the preparation of the (0223) involved in the second aerosol generating system form (02) of the aerosol generating system and method using multicard coupling giant thermal effect:

[0256] The substrate of the first heating medium particle coating (0223) is hexagonal boron carbon nitrogen ternary absorbing ceramic (h-BCN), the first heating medium particles are fully mixed with a film-forming agent sodium silicate sol, or aluminum dihydrogen phosphate sol, or aluminum hydroxide sol, or silica sol, coated to form a film, and sintered and solidified at a high temperature above 800°C to form the first heating medium particle coating (0223). The first heating medium particle coating (0223) can also be based on a metal material, such as aluminum, or a copper or stainless steel sheet, coated with the particle heating medium (0212) prepared in the first step and an inorganic binder sodium silicate, or aluminum dihydrogen phosphate, or a phosphoric acid-copper oxide mixed slurry, and subjected to a heat treatment at 300°C to 450°C to form the preheating shell coating (0223). It can also be obtained by chemical vapor deposition, or gas phase pyrolysis, or gas phase hydrolysis, or gas phase combustion, or flame vapor deposition, or plasma spraying, or plasma spraying, by deposition and heating on aluminum, or copper or stainless steel sheets.

[0257] Step II-6 The metal particle layer filter medium (0211) is pressed from aluminum particles with a size of 0.5 to 1 mm and a thickness of about 0.5 to 2 mm; the sealing ring (0231) is made of silicone rubber; the heating chamber b base disc (0233) is made of insulating Al2O3 ceramic material; the temperature control unit (0234) passes through the central hole of the heating chamber b base and enters the aerosol generating section (021) 2 to 5 mm.

[0258] The present invention Fig. 9 , Fig.10 and Fig.11 The third aerosol generating system form (03) of the aerosol generating system and method using the multi-card coupling giant thermal effect, the materials and unit structures involved include: an aerosol generating section 2 (031), a preheating shell (032), a heating chamber c (033), a PCB circuit board control (034), an alternating electromagnetic field generating source (035), a battery (036), a housing (037), and an aerosol generating matrix 2 (0312), second heating medium particles (0313), a preheating shell Air inlet (0321), preheating shell (0322), second heating medium particle coating (0323), metal particle layer filter (0331), block heating medium 2 (0332), temperature control unit (0333), heating chamber c air inlet channel (0334), heating chamber c air inlet seat hole (0335), antenna (0336), antenna feeder base (0337) and heating chamber c metal shielding shell (0338), wave-transmitting ceramic tube (0339), casing air inlet (0371).

[0259] The present invention Fig. 9The third aerosol generating system form (03) of the aerosol generating system and method utilizing multicard coupling giant thermal effect is shown, Fig.10 and Fig.11 The specific method for preparing the second heating medium particles (0313), the block heating medium 2 (0332), and the aerosol generating matrix 2 (0312) involved in the heating structure C of the aerosol generating system at the CC section shown, as well as the preparation basis and method of the second heating medium particle coating (0323), and the steps include:

[0260] In the third aerosol generation system form (03) of the aerosol generation system and method utilizing the multicard coupling giant thermal effect, the alternating electromagnetic field frequency range adopted by the heating drive unit is 0.3 GHz to 30 GHz, and the design principle for being compatible with and balancing the multicard coupling frequency response range is: for dielectric components, the relaxation polarization loss of the inherent electric moment orientation polarization and the thermal ion relaxation polarization and the resonant polarization loss of the ion displacement polarization are enhanced; for magnetic medium components, the hysteresis loss and damping loss and the domain wall resonance, natural resonance, size resonance, and spin wave resonance in the resonance loss are increased; for conductive medium components, the conductivity loss of carriers such as free electrons and ions and the absorption loss of densely packed ultrafine particle aggregates are increased.

[0261] Step III-1 The preparation of the second heating medium particles (0313) used in the third aerosol generating system form (03) of the aerosol generating system and method utilizing the multicard coupling giant thermal effect is consistent with the preparation of the first heating medium particles (0113) used in the first aerosol generating system form (01), and will not be repeated here.

[0262] The second heating medium particles (0313) are processed by a pulverization method and / or a synthesis method to have a particle size distribution range of 0.1μm to 500μm, wherein the particle size distribution range of the particle heating medium directly blended with the aerosol matrix is ​​15μm to 500μm; the particle size distribution range of the particle heating medium added to the tobacco sheet papermaking slurry or rolled paste is 0.1μm to 100μm.

[0263] Step III-2In the third aerosol generating system form (03), the block heating medium 2 (0332) involved is formed by mixing the second heating medium particles (0313) prepared in step III-1 with an inorganic binder such as sodium silicate, or dihydrogen aluminum phosphate, or phosphoric acid-copper oxide, through pressing and low-temperature calcination. The antenna (0336) adopts a PIFA planar inverted F antenna. Before roasting, the antenna (0336) is embedded in the block heating medium 2 corresponding to the bottom of the heating chamber c air inlet seat hole (0335) and pressed into shape. The antenna feeder base (0337) extends to the outside of the block heating medium 2 (0332). The heating chamber c air inlet seat hole (0335) is connected to the outside of the block heating medium 2 (0332) through 4 to 10 heating chamber c air inlet channels (0334) with a diameter of 0.5 to 2 mm. The heating chamber c metal shielding shell (0338) encloses the block heating medium 2 therein, and the heating chamber c metal shielding shell (0338) is made of aluminum, copper or stainless steel.

[0264] In the third aerosol generating system form (03), a foil-like film composite heating medium 2 can also be added to the aerosol generating matrix 2. After the second heating medium particles are mixed with a binder such as carboxymethyl cellulose, guar gum or tobacco extract, the aluminum foil or copper foil is composited on one side or both sides by a casting method or a spraying method, and then cut to obtain a size equivalent to that of tobacco flakes. The foil-like film composite heating medium 2 can be prepared by using the second dielectric component and the precursor of the second magnetic medium component through chemical vapor deposition, gas phase pyrolysis, gas phase hydrolysis, gas phase combustion, or flame vapor deposition.

[0265] Step III-3 , the preparation of the aerosol generating substrate 2 (0312) used in the third aerosol generating system form (03):

[0266] The second heating medium particles (0313) prepared in step III-1 are directly blended with the aerosol matrix, and the particle size distribution range of the second heating medium particles is 15μm to 500μm. The second heating medium particles (0313) prepared in step III-1 can also be mixed into the fiber slurry or paste before the tobacco sheets in the aerosol matrix are papered or rolled, so that the second heating medium particles (0313) prepared in step III-1 are evenly distributed in the tobacco sheets at a mass ratio of 5 to 60%, and the particle size distribution range of the second heating medium particles is 0.1μm to 100μm. The foil-like film composite heating medium 2 (0314) can also be added to the aerosol generating matrix 2 (0312) with a mixing mass ratio of 3 to 30%.

[0267] The second heating medium particles (0313) may also be heating medium particles of a low excitation temperature aerosol generating matrix. The heating medium particles of the low excitation temperature aerosol generating matrix are selected from the second heating medium particles (0313) prepared in step III-1, and are selected to meet the principle conditions of the Kelvin equation, with a pore size range of 60nm to 50μm, a porosity range of 85% to 95%, and a specific heat capacity range of 0.1kJ·kg -1 ·K -1 Up to 0.6 kJ·kg -1 ·K -1 , thermal conductivity range is 0.035W·m -1 ·K -1 Up to 0.125W·m -1 ·K -1 The particles with different physical property parameters adsorb the liquid phase components of the aerosol generating medium, so that the liquid phase components are separated into small droplets entering the pores with a porosity of 85% to 95%, and the pore size distribution range is 60nm to 50μm, so as to increase the saturated vapor pressure value of the liquid phase components of the aerosol generating medium, and obtain the heating medium of the low excitation temperature aerosol generating matrix, the excitation temperature is 160℃ to 200℃, and the heating medium particles of the low excitation temperature aerosol generating matrix are blended with other aerosol matrices, and the particle size distribution range of the heating medium particles of the low excitation temperature aerosol generating matrix is ​​15μm to 500μm.

[0268] Step III-4 , the preparation of the second heating medium particle coating (0323) used in the third aerosol generating system form (03):

[0269] The substrate of the second heating medium particle coating (0323) is hexagonal boron carbon nitrogen ternary absorbing ceramic (h-BCN), and the second heating medium particles are fully mixed with a film-forming agent, sodium silicate sol, or aluminum dihydrogen phosphate sol, or aluminum hydroxide sol, or silica sol, and coated to form a film, and sintered and solidified at a high temperature above 800°C to form the second heating medium particle coating (0323). The second heating medium particle coating (0323) can also be based on a metal material, such as aluminum, or a copper or stainless steel sheet, coated with the particle heating medium (0313) prepared in the first step and an inorganic binder, sodium silicate, or aluminum dihydrogen phosphate, or a phosphoric acid-copper oxide mixed slurry, and subjected to a heat treatment at 300°C to 450°C to form the preheating shell coating (0323). It can also be obtained by chemical vapor deposition, gas phase pyrolysis, gas phase hydrolysis, gas phase combustion, flame vapor deposition, or plasma spraying, by deposition and heating on aluminum, copper or stainless steel sheets.

[0270] Step III-5,The metal particle layer filter medium (0331) is formed by pressing aluminum particles with a size of 0.5 to 1.5 mm and a thickness of about 0.2 to 1.2 mm; the wave-transmitting ceramic tube (0339) is made of quartz ceramic SiO2 or high alumina ceramic Al2O3 or Si3N4 ceramic material; the temperature control unit (0333) is laterally inserted into the inner surface of the wave-transmitting ceramic tube (0339) at a distance of 2 to 3 mm from the free port of the aerosol generating section (031).

[0271] In order to further illustrate the present invention, an aerosol generating system and a heating medium utilizing multi-card coupling giant thermal effect provided by the present invention are described in detail below in conjunction with embodiments, but they should not be construed as limiting the scope of protection of the present invention.

[0272] Example 1

[0273] The first aerosol generating system form (01) of the aerosol generating system using multicard coupling giant thermal effect and the first heating medium (0113) of the present invention are used to prepare:

[0274] 1-i) The first heating medium includes a first dielectric, a first magnetic medium and a first conductive medium, and the system is composed of:

[0275] The first magnetic medium component is Fe3O4; the first conductive medium component is ZnO. The first heating medium of the Fe3O4@ZnO core-shell structure is prepared by direct precipitation method, and the specific steps are:

[0276] Step 1: Add 500 ml of zinc acetate dihydrate and 50 g of ascorbic acid granules into a stirred reactor, and add deionized water;

[0277] Step 2: After the raw material particles in step 1 are completely dissolved, 40g of Fe3O4 raw material particles are added to the solution, and stirred at high speed. After the particles are evenly dispersed to form a mixed suspension, 200ml of hexamethylenetetramine (HMTA) precipitant is added to the mixed suspension, and stirring is continued at high speed. The Fe3O4 particle size is between 500nm and 1μm;

[0278] Step 3: Heat the stirred reactor, slowly raise the temperature to 90°C and maintain it for 3 hours, and maintain the speed at 800 rpm;

[0279] Step 4: After the reaction product Fe3O4@ZnO was centrifuged at a speed of 7500rpm for 2min, it was washed with 500ml of deionized water and 500ml of anhydrous ethanol respectively, and then dried in a constant temperature drying oven at 80°C for 12h to prepare a core-shell structure powder product with Fe3O4 as the core and ZnO as the shell, wherein the thickness of the ZnO shell was between 100nm and 300nm;

[0280] Step 5: 30g of Fe3O4@ZnO core-shell structure powder product is compacted into a green body, placed in a high-temperature furnace, sintered at 1000°C for 3h, cooled, crushed and classified to a particle size distribution range of 0.1μm to 500μm, and the first heating medium (0113) of the core-shell structure is obtained. Fig.12 .

[0281] 1-ii) Preparation of other heating media based on the first heating medium (0113)

[0282] (1) The first heating medium is classified to a particle size distribution range of 1 μm to 200 μm, mixed with sodium silicate sol to form a slurry, the sodium silicate sol is added in an amount of 35 wt %, sprayed on a 0.8 mm thick copper sheet, and subjected to a heat treatment at 420° C. to form a first heating medium particle coating (0123);

[0283] (2) The first heating medium is classified to a particle size distribution range of 15 μm to 100 μm, mixed with a carboxymethyl cellulose solution to form a slurry, the carboxymethyl cellulose solution is added in an amount of 40 wt %, and is double-sided sprayed on an aluminum foil, and dried at 80° C. to form a foil-shaped film composite heating medium 1 (0114);

[0284] (3) The first heating medium is classified into a particle size distribution range of 0.1 μm to 100 μm, and is used as a particulate heating medium for mixing tobacco sheet papermaking slurry into the aerosol generating matrix 1 (0112), wherein the first heating medium is mixed with a mass proportion of 30%.

[0285] 1-iii) The first aerosol generating system form (01) of the aerosol generating system utilizing multi-card coupling giant thermal effect is related to the following structure:

[0286] (1) Preparation of the curved electrode 1 (01321) and the curved electrode 2 (01322) of the tubular electrode plate (0132) used in the first aerosol generation system form (01) of the aerosol generation system and method using multicard coupling giant thermal effect:

[0287] The tubular electrode plate (0132) is composed of the curved surface electrode 1 (01321) and the curved surface electrode 2 (01322) compounded on the inner surface of the tubular insulating ceramic substrate. The curved surface electrode 1 and the curved surface electrode 2 are divided into pieces and are opposite to each other. The curved surface electrode 1 and the curved surface electrode 2 each have 3 pieces and are opposite to each other at intervals. The adjacent curved surface electrodes 1 and curved surface electrodes 2 are separated by a gap insulating material (01323). The gap insulating material is polyimide or aramid resin (polyisophthalamide). The insulating ceramic The base material is Al2O3 ceramic, the gap between the curved electrode 1 and the curved electrode 2 is 1mm, the curved electrode 1 and the curved electrode 2 are made of 1mm copper sheets, the height of the curved electrode 1 and the curved electrode 2 is 14mm, the diameter of the tubular electrode plate is 7.5mm, and feeder connection positions (01324) and (01325) are provided at the lower end of each curved electrode 1 and the curved electrode 2 corresponding to the tubular electrode plate (0132), and are connected to the heating drive unit of the aerosol generating system through the feeder;

[0288] (2) The metal particle layer filter medium (0111) is pressed from aluminum particles with a size of 1 mm and a thickness of about 0.6 mm; the sealing ring (0131) is made of silicone rubber; the heating chamber a base disc (0133) is made of insulating Al2O3 ceramic material. There are 12 through holes with a diameter of 0.6 mm evenly distributed on the disc; the temperature control unit (0134) passes through the central hole of the heating chamber a base and enters the aerosol generating section (011) 3 mm;

[0289] (3) The aerosol generating section is mainly composed of an aerosol generating matrix 1 (0112) and a foil-like film composite heating medium 1 (0114), wherein the content of the aerosol generating matrix 1 is 92wt%, and the content of the foil-like film composite heating medium 1 is 8wt%; the aerosol generating matrix 1 is composed of an incorporated first heating medium and an aerosol matrix containing tobacco flakes, wherein the aerosol matrix is ​​composed of natural tobacco, or artificial homogenized tobacco plant materials such as reconstituted tobacco shreds and tobacco flakes, and tobacco extracts, flavors, and liquid phase aerosols such as polyols or polyol esters. The first heating medium can be blended with the aerosol matrix, or can be added as a particle filler during the papermaking process of the tobacco flakes contained in the aerosol matrix to form the aerosol generating matrix 1, and the mass ratio of the first heating medium contained in the aerosol generating matrix 1 is 20%. The tobacco flakes are mainly composed of tobacco dust, tobacco leaves and tobacco stem fibers, with carboxymethyl cellulose or natural adhesives such as pectin and gum and other additives added. The composition of common tobacco flakes is well known in the art.

[0290] Aerosol matrix component mass ratio: tobacco sheet 45%, first heating medium 20%, tobacco extract 15%, glycerol 17%, carboxymethyl cellulose 2%, tobacco flavoring agent 1%;

[0291] (4) The first aerosol generating system type (01) of the aerosol generating system utilizing the multicard coupling giant thermal effect takes about 20 seconds to heat the aerosol generating section from 30°C to 250°C when driven by an alternating electromagnetic field with a frequency of 27.12 MHz.

[0292] Example 2

[0293] The second aerosol generating system form (02) of the aerosol generating system using multicard coupling giant thermal effect of the present invention and the first heating medium (0213) are used to prepare:

[0294] 2-i) The first heating medium includes a first dielectric, a first magnetic medium and a first conductive medium, and the system is composed of:

[0295] The first dielectric component is Bi and Te; the first magnetic medium component is La and Mn; and the first conductive medium is Mn. Bi2Te3@Mn is prepared by mechanical alloying method. 15 Bi 34 Te 51 @La 15 Bi 34 Te 51 The first heating medium of the heterojunction structure comprises the following specific steps:

[0296] Step 1: High purity elements Bi, Te and pure La, Mn are respectively calculated according to the atomic percentage Bi2Te3, Mn 15 Bi 34 Te 51 and La 15 Bi 34 Te 51 The ingredients are added to a batch ball mill;

[0297] Step 2: The vacuum degree of the ball mill is pumped to 10 -3 Pa then introduced high-purity argon gas, the ball-to-material ratio was 15:1, and the rotation speed was 150r / min;

[0298] Step 3: Through long-term intense impact and collision between raw material particles and grinding balls, the particles are repeatedly cold welded and broken. During the long ball milling time, atoms can diffuse in the system to obtain a uniform heterojunction structure heating medium. 15 Bi 34 Te 51 and La 15 Bi 34 Te 51 The mass ratio is 4.5:3:2.5, and the particle size is between 15μm and 100μm;

[0299] Step 4: 20g Bi2Te3, 50g Mn 15 Bi 34 Te 51 and 30g La 15 Bi 34 Te 51 The constructed heterojunction powder is made into a round green body, placed in a high temperature furnace, sintered at 800°C for 5 hours, crushed and classified to a particle size distribution range of 0.1 μm to 500 μm, and the first heating medium (0213) of the heterojunction structure is obtained. Fig.13 .

[0300] 2-ii) Preparation of other heating media based on the first heating medium (0213)

[0301] (1) The first heating medium is classified to a particle size distribution range of 1 μm to 200 μm, mixed with aluminum dihydrogen phosphate sol to form a slurry, the aluminum dihydrogen phosphate sol is added in an amount of 40 wt%, and coated on the inner wall of the substrate (0222) of the preheating shell, which is hexagonal boron carbon nitrogen ternary absorbing ceramic (h-BCN), and cured at a high temperature of 820° C. to form the first heating medium particle coating (0223);

[0302] (2) Add 8 wt % of aluminum dihydrogen phosphate sol to the first heating medium (with a particle size distribution range of 0.1 μm to 500 μm), mix well, press into shape, and cure at 820° C. to form the block heating medium 1 (0235);

[0303] (3) classifying the first heating medium to a particle size distribution range of 15 μm to 500 μm, and using it as a particulate heating medium directly blended with the aerosol matrix in the aerosol generating matrix 1 (0212);

[0304] (4) The first heating medium is classified to a particle size distribution range of 0.1 μm to 100 μm, and is evenly mixed with aluminum dihydrogen phosphate sol and starch dextrin in a mass ratio of: first heating medium: aluminum dihydrogen phosphate sol: starch dextrin = 9:0.4:0.6, and lightly pressed into a green body, sintered at 1000°C, and crushed and classified to obtain porous particles with a particle size distribution range of 15 μm to 500 μm, a pore size of 8 nm to 35 μm, and a porosity of 78% to 90%; after adsorbing the liquid phase component in the aerosol matrix, the liquid absorption mass ratio is approximately: porous particles: liquid phase group = 1:1.2, and heating medium particles of a low excitation temperature aerosol generating matrix are obtained.

[0305] 2-iii) The second aerosol generating system form (02) of the aerosol generating system utilizing multi-card coupling giant thermal effect is related to the structure:

[0306] (1) Preparation of the planar electrode 1 (02321) and the planar electrode 2 (02322) of the planar plate (0232) used in the second aerosol generating system form (02) of the aerosol generating system and method using multicard coupling giant thermal effect:

[0307] The planar electrode (0232) is formed by compounding the planar electrode 1 (02321) and the planar electrode 2 (02322) on the surface of a planar insulating ceramic substrate, which are parallel and opposite to each other with a spacing of 7.5 mm, which is the diameter value of the aerosol generating section. A block heating medium 1 (0235) is sandwiched at each end of the planar electrode 1 and the planar electrode 2. A cylindrical hole is provided at the symmetric center of the two sandwiched block heating media 1, and the diameter is also 7.5 mm, which is the diameter value of the aerosol generating section, and the length is about 14 mm, which is the length value of the aerosol generating section. The material of the planar electrode 1 and the planar electrode 2 is a copper sheet with a thickness of 0.5 mm, and the insulating ceramic substrate material is Al2O3 ceramic. The planar electrode 1 and the planar electrode 2 are connected to the heating drive unit of the aerosol generating system through a feeder.

[0308] (2) The metal particle layer filter medium (0211) is pressed from aluminum particles with a size of 1 mm and a thickness of about 0.6 mm; the sealing ring (0231) is made of silicone rubber; the heating chamber b base disc (0233) is made of insulating Al2O3 ceramic material; the temperature control unit (0234) passes through the central hole of the heating chamber b base and enters the aerosol generating section (021) 3 mm.

[0309] (3) The aerosol generating substrate 1 is mainly composed of a mixture of an aerosol substrate, the first heating medium and the heating medium of the low excitation temperature aerosol generating substrate, wherein the aerosol substrate is 50 wt% (the component composition is the same as in Example 1), the first heating medium is 20 wt%, and the heating medium of the low excitation temperature aerosol generating substrate is 30 wt%;

[0310] (4) The second aerosol generating system form (02) of the aerosol generating system and method utilizing the multicard coupling giant thermal effect takes about 17 seconds to heat the aerosol generating section from 30°C to 250°C when driven by an alternating electromagnetic field with a frequency of 40.68 MHz.

[0311] Example 3

[0312] The third aerosol generating system form (03) of the aerosol generating system and method using the multicard coupling giant thermal effect of the present invention and the second heating medium (0313) are prepared:

[0313] 3-i) The second heating medium includes a second dielectric medium, a second magnetic medium and a second conductive medium, and the system is composed of:

[0314] The second dielectric is a BaO-MgO-Ta2O5 system; the second magnetic medium is a Co2Z (Z-type hexagonal ferrite) system; the second conductive medium is CoO and Fe2O3. The second heating medium of the BaO-MgO-Ta2O5 / Co2Z coated structure is prepared by a solid phase method, and the specific steps are:

[0315] Step 1: Mix 200g BaCO3 particles, 40g MgO particles, and 440g Ta2O5 particles, and react them at a high temperature of 1200°C for 24h to obtain BaO-MgO-Ta2O5 particles.

[0316] Step 2: Mix 178g BaCO3 particles, 48g Co3O4 particles, and 550g Fe2O3 particles, and react them at a high temperature of 1280℃ for 6h to obtain Ba3Co2Fe 23 O 41 (Co2Z) particles.

[0317] Step 3: Mix 30 g of BaO-MgO-Ta2O5 particles with 45 g of Co2Z particles, and react them at a high temperature of 1100°C for 24 hours to obtain BaTiO3 / NiZnFe composite particles.

[0318] Step 5: 30g of BaO-MgO-Ta2O5 / Co2Z composite structure coupled heating medium is made into a circular blank, placed in a high temperature furnace, sintered at 1200°C for 6h, crushed and classified to a particle size distribution range of 0.1μm to 500μm, and the second heating medium (0313) of the coated structure is obtained, see Fig.14 .

[0319] 3-ii) Preparation of other heating media based on the second heating medium (0313):

[0320] (1) The second heating medium is classified to a particle size distribution range of 1 μm to 200 μm, mixed with aluminum hydroxide sol to form a slurry, the aluminum hydroxide sol is added in an amount of 36 wt %, and coated on the inner wall of the substrate (0322) of the preheating shell, which is hexagonal boron carbon nitrogen ternary absorbing ceramic (h-BCN), and cured at a high temperature of 900° C. to form the second heating medium particle coating (0323);

[0321] (2) Add 10 wt % of aluminum dihydrogen phosphate sol to the second heating medium (with a particle size distribution range of 0.1 μm to 500 μm), mix well, press into shape, and calcine at 820° C. to form the block heating medium 2 (0332);

[0322] (3) The second heating medium is classified into a particle size distribution range of 0.1 μm to 100 μm, and is used as a particulate heating medium for mixing tobacco flake fiber paste into the aerosol generating matrix 2 (0312), wherein the second heating medium is mixed with a mass proportion of 30%.

[0323] 3-iii) The third aerosol generating system form (03) of the aerosol generating system utilizing multi-card coupling giant thermal effect is related to the following structure:

[0324] (1) The preheating shell (032) is provided with a metal shielding shell (0338), a block heating medium 2 (0332) and an antenna (0336) embedded in the block heating medium 2, wherein the antenna is a PIFA planar inverted F antenna; the metal shielding shell is wrapped around the outside of the block heating medium 2, and the metal shielding shell is a stainless steel sheet with a thickness of 0.2 mm;

[0325] The metal shielding shell, the block heating medium 2 and the antenna embedded in the block heating medium 2 form a heating chamber, and the air inlet seat hole of the heating chamber is connected to the outside of the block heating medium 2 through 6 air inlet channels with a diameter of 0.6 mm;

[0326] (2) The block heating medium 2 is a cube; a cylindrical hole is provided on the symmetry axis of the block heating medium 2, and an aerosol generating section is formed inside the hole; a wave-transmitting ceramic tube is nested in the cylindrical hole, and the inner diameter of the wave-transmitting ceramic tube is 7.4 mm, which is the diameter of the aerosol generating section, and the depth is 14 mm, and the material is high-alumina Al2O3 wave-transmitting ceramic; the temperature control unit is horizontally placed on the inner surface of the wave-transmitting ceramic tube, and the position is 2 mm away from the free port of the aerosol generating section;

[0327] (3) The aerosol generating matrix 2 is mainly composed of an aerosol matrix and second heating medium particles mixed into a tobacco sheet fiber paste, wherein the second heating medium particles have a particle size distribution range of 0.1 μm to 100 μm, an addition amount of 30 wt%, and the remaining 70 wt% is an aerosol matrix (the component composition is the same as in Example 1);

[0328] (4) The third aerosol generating system form (03) of the aerosol generating system and method utilizing the multicard coupling giant thermal effect, when driven by an alternating electromagnetic field with a frequency of 2.45 GHz, takes about 13 seconds to heat the aerosol generating section from 30°C to 250°C.

[0329] Example 4

[0330] The sol-gel method is used to prepare the second heating medium of the coating structure, comprising the following steps:

[0331] Step 1: Add 50g Fe3O4 raw material particles into a reactor filled with 300ml ethylene glycol and stir at high speed to disperse. The Fe3O4 particles have a size between 100nm and 500nm;

[0332] Step 2: Add deionized water and 25% ammonia water, add 10 liters of 25% ammonia water per kilogram of Fe3O4, then add 0.5 liters of tetraethyl orthosilicate, and stir at a constant speed for 10 hours;

[0333] Step 3: After the reaction, the obtained particles were separated by an electromagnet and washed several times with 500 ml of ethanol and 500 ml of deionized water;

[0334] Step 4: Finally, dry at 60°C for 12 hours to prepare a coated structure coupling heating medium with Fe3O4 as the mother particle and SiO2 as the daughter particle.

[0335] Step 5: 30g of Fe3O4@SiO2 coated structure heating medium is made into a circular blank, placed in a high temperature furnace, and sintered at 900℃ for 5h. Fig.15 The finished product is obtained after crushing and classification, and is used as the second heating medium of the coated structure with a response frequency ranging from 0.3 GHz to 30 GHz.

[0336] Step 6: In the third aerosol generating system form (03) of the aerosol generating system and method using multicard coupling giant thermal effect at a frequency of 2.45 GHz, the sample in step 5 is heated from 30°C to 250°C, which takes about 19 seconds.

[0337] Example 5

[0338] The method of preparing a porous structure first heating medium by a polymer network gel method comprises the following steps:

[0339] Step 1: prepare 1 mol / L triammine citrate solution, add 500 ml of tetrabutyl titanate to 300 ml of triammine citrate in a ratio of n(triammine citrate):n(Ti)=1:1 and stir, then add 50 g of ferric nitrate to the mixed solution in a ratio of n(Fe):n(Ti)=0; 0.5%; 1.0%; 1.5% and 2.0%, and adjust the pH value to 8.5 with aqueous ammonia;

[0340] Step 2: After fully mixing, add 30g of organic monomer N-hydroxymethyl acrylamide, 6g of cross-linking agent N,N′-methylenebisacrylamide, 1g of initiator ammonium persulfate and 1g of catalyst tetramethylethylenediamine to each liter of the solution, stir evenly, and form a polymer network gel after 5 to 15 minutes;

[0341] Step 3: Dry the polymer network gel in an oven at 80°C for 48 hours;

[0342] Step 4: 300 g of dry gel is placed in a calcining furnace and calcined at a certain temperature for 2 hours to obtain an iron-doped TiO2 porous structure coupled heating medium, wherein the pore size is between 100 and 500 nanometers.

[0343] Step 5: 30g of the iron-doped TiO2 porous structure is coupled with a heating medium to form a circular blank, which is placed in a high-temperature furnace and sintered at 800°C for 5h to obtain a finished product. Fig.16 , as the first heating medium of the porous structure with a frequency ranging from 0.3 MHz to 300 MHz.

[0344] Step 6: In the first aerosol generating system form (01) of the aerosol generating system and method using multicard coupling giant thermal effect at a frequency of 13.56 MHz, the sample in step 5 is heated from 30°C to 250°C, which takes about 21 seconds.

[0345] Example 6

[0346] The chemical vapor deposition method is used to prepare a first heating medium of a film composite structure, comprising the following steps:

[0347] Step 1: Select aluminum foil of a certain size as the base material, use alcohol and acetone to ultrasonically remove stains on the surface of the aluminum foil, and then use pickling liquid to remove the surface oxide layer;

[0348] Step 2: 100g Nd 13.5 (FeZrCo) 80.5 B6 magnetic powder and 150g Fe(CO)3 were placed in a reactor and sealed in an evaporator respectively, and the evaporated Fe(CO)3 was mixed with argon gas and passed into the reactor for chemical vapor deposition. The reactor was continuously vibrated to ensure the uniformity of coating.

[0349] Step 3: After the reaction is completed, cool to room temperature to obtain Nd 13.5 (FeZrCo) 80.5 B6-Fe(CO)3 membrane composite structure coupled heating medium, see Fig.17 The thickness of the composite film is between 100 μm and 500 μm, and it serves as the first heating medium of the film composite structure with a frequency ranging from 0.3 MHz to 300 MHz.

[0350] Step 4: In the second aerosol generating system form (02) of the aerosol generating system and method using multicard coupling giant thermal effect at a frequency of 27.12 MHz, the sample in step 3 is heated from 30°C to 250°C, which takes about 16 seconds.

[0351] Example 7

[0352] The solid phase method is used to prepare the second heating medium of the coated structure, comprising the following steps:

[0353] Step 1: Mix 200 g of BaCO3 particles and 80 g of TiO2 particles in a molar ratio of 1:1, and react at a high temperature of 1500°C for 24 hours to obtain BaTiO3 particles.

[0354] Step 2: Mix 22g NiO particles, 57g ZnO particles, and 160g Fe2O3 particles, and react them at 1250℃ for 4h to obtain Ni 0.3 Zn 0.7 Fe2O4 particles.

[0355] Step 3: Mix 10g BaTiO3 particles with 20g Ni 0.3 Zn 0.7 After mixing the Fe2O4 particles, the mixture was reacted at 1150℃ for 5h to obtain BaTiO3 / Ni 0.3 Zn 0.7 Fe2O4 composite particles.

[0356] Step 4: 30g BaTiO3 / Ni 0.3 Zn 0.7 The Fe2O4 composite structure is coupled with a heating medium to form a circular blank, which is placed in a high-temperature furnace and sintered at 1100°C for 5 hours. Fig.18 The finished product is obtained after crushing and classification, and is used as the second heating medium of the sheathed structure with a frequency ranging from 0.3 GHz to 30 GHz.

[0357] Step 5: In the third aerosol generating system form (03) of the aerosol generating system and method using multicard coupling giant thermal effect at a frequency of 2.45 GHz, the sample in step 5 is heated from 30°C to 250°C, which takes about 18 seconds.

[0358] Example 8

[0359] The high-temperature solid phase method and the sol-gel method are used to prepare the second heating medium of the coated structure, which includes the following steps:

[0360] Step 1: Mix 140 g of K2CO3 particles with 265 g of Nb2O5 particles, and react them at a high temperature of 1200°C for 14 hours to obtain KNbO3 particles.

[0361] Step 2: Use 50g of ferric nitrate, 30g of manganese nitrate, and 25g of zinc nitrate as source materials, 500ml of citric acid as a chelating agent, and 300ml of ethylene glycol as a thickener, adjust the pH value to >13.0 with ammonia water, reflux the mixed solution at 70°C, and evaporate at 90°C to obtain a sol, and then dry to obtain a dry gel, which is then calcined to obtain a sol-gel Mn 0.5 Zn 0.5 Fe2O4 powder;

[0362] Step 3: Mix 10g KNbO3 particles with 25g Mn 0.5 Zn 0.5 After mixing the Fe2O4 particles, the mixture was reacted at 1150℃ for 5h to obtain KNbO3 / Mn 0.5 Zn 0.5 Fe2O4 composite particles.

[0363] Step 4: 30g KNbO3 / Mn 0.5 Zn 0.5 The Fe2O4 composite structure is coupled with a heating medium to form a circular blank, which is placed in a high-temperature furnace and sintered at 1100°C for 5 hours. Fig.19 The finished product is obtained after crushing and classification, and is used as the second heating medium of the sheathed structure with a frequency ranging from 0.3 GHz to 30 GHz.

[0364] Step 5: In the third aerosol generating system form (03) of the aerosol generating system and method using multicard coupling giant thermal effect at a frequency of 2.45 GHz, the sample in step 5 is heated from 30°C to 250°C, which takes about 20 seconds.

[0365] Example 9

[0366] The solid phase method is used to prepare the second heating medium of the coated structure, comprising the following steps:

[0367] Step 1: Mix 200g BaCO3 particles, 40g MgO particles, and 440g Ta2O5 particles, and react them at a high temperature of 1200°C for 24h to obtain BaO-MgO-Ta2O5 particles.

[0368] Step 2: Mix 50 g of BaO-MgO-Ta2O5 particles with 30 g of NiO particles, and react them at a high temperature of 900°C for 10 hours to obtain BaO-MgO-Ta2O5 / NiO composite particles.

[0369] Step 3: 25g BaO-MgO-Ta2O5 / NiO composite structure is coupled with a heating medium to form a circular blank, which is placed in a high-temperature furnace and sintered at 1100℃ for 5h. Fig. 20The finished product is obtained after crushing and classification, and is used as the second heating medium of the sheathed structure with a frequency ranging from 0.3 GHz to 30 GHz.

[0370] Step 4: In the third aerosol generating system form (03) of the aerosol generating system and method using multicard coupling giant thermal effect at a frequency of 2.45 GHz, the sample in step 4 is heated from 30°C to 250°C, which takes about 18 seconds.

[0371] Example 10

[0372] The solid phase method is used to prepare the second heating medium of the coated structure, comprising the following steps:

[0373] Step 1: Mix 178g BaCO3 particles, 48g Co3O4 particles, and 550g Fe2O3 particles, and react them at a high temperature of 1280℃ for 6h to obtain Ba3Co2Fe 23 O 41 (Co2Z) particles.

[0374] Step 2: Mix 50g Co2Z particles and 30g ZnO particles, and react them at a high temperature of 1100°C for 14h to obtain Co2Z / ZnO particles.

[0375] Step 3: 30g Co2Z / ZnO composite structure is coupled with heating medium to form a circular blank, placed in a high temperature furnace, and sintered at 1100℃ for 5h. Fig.21 The finished product is obtained after crushing and classification, and is used as the second heating medium of the sheathed structure with a frequency ranging from 0.3 GHz to 30 GHz.

[0376] Step 4: In the third aerosol generating system form (03) of the aerosol generating system and method using multicard coupling giant thermal effect at a frequency of 2.45 GHz, the sample in step 4 is heated from 30°C to 250°C, which takes about 17 seconds.

[0377] As can be seen from the above embodiments, the aerosol generating system utilizing the card-coupled giant thermal effect provided by the present invention comprises the following steps: (1) in the dielectric component of the heating medium, measures are taken to strengthen the inherent electric moment orientation polarization, thermal ion relaxation polarization and ion displacement polarization, so as to optimize the utilization of relaxation polarization loss and resonance polarization loss, and obtain a high polarization loss dielectric; in the magnetic medium component of the heating medium, measures are taken to strengthen the hysteresis loss, damping loss and resonance loss, and obtain a high hysteresis loss magnetic medium; in the conductive medium component of the heating medium, measures are taken to increase free electrons, ions and doping defects and vacancies, so as to optimize the utilization of the conductivity loss of various carriers, and obtain a high conductivity loss conductive medium; (2) in the material structure of the heating medium, the dielectric, magnetic medium and conductive medium are compositely constructed by a physical and chemical method of multi-phase components to form a core-shell structure, a heterojunction structure, a coating structure, a porous structure and a membrane composite structure, so as to realize the composite at the mesoscopic level, so as to facilitate multi-field coupling to generate a multi-card-coupled giant thermal effect. (3) In terms of lowering the thermal excitation temperature of the aerosol generating matrix, the porous structure of the heating medium adsorbs the liquid phase components of the aerosol generating medium, causing the liquid phase components to be differentiated into a large number of small droplets. (4) In the heating drive unit of the aerosol generating system, the frequency of the alternating electromagnetic field used is a balanced compatible response frequency that meets the requirements of multi-card coupling of electric cards, magnetic cards and conductive cards for multi-field coupling drive, and the compatible response frequency range is 0.3MHz to 30GHz.

[0378] The above is only a preferred embodiment of the present invention. It should be pointed out that for ordinary technicians in this technical field, several improvements and modifications can be made without departing from the principle of the present invention. These improvements and modifications should also be regarded as the scope of protection of the present invention.

Claims

1. An aerosol generating substrate, comprising a heating medium, wherein the heating medium comprises a first heating medium or a second heating medium; The first heating medium includes a first dielectric medium, a first magnetic medium and a first conductive medium; The first dielectric is selected from at least one of the following systems: ①Perovskite structure system, including BaTiO 3 , and / or PbTiO 3 , and / or NaNbO 3 , and / or KNbO 3 , and / or BiFeO 3 ;② Tungsten bronze structure system, including lead metaniobate, and / or Sr 1-x Ba x Nb 2 O 6 ;③ Bismuth layered structure system, including SrBi 2 Ta 2 O 9 , and / or Bi 4 Ti 3 O 12 , and / or SrBi 4 Ti 4 O 15 ④ Pyrochlore structure system, including Cd 2 Nb 2 O 7 , and / or Pb 2 Nb 2 O 7 ; The first magnetic medium is selected from at least one of the following ferrites: Spinel ferrites, including MFe 2 O 4 , M=Mn, and / or Fe, and / or Ni, and / or Co, and / or Cu, and / or Mg, and / or Zn, and / or Li, and / or MnZn, and / or NiZn, and / or MgZn, and / or LiZn ferrite; and / or R 3 Fe 5 O 12 , R is a rare earth element, and the rare earth element is Y, and / or La, and / or Pr, and / or Nd, and / or Sm, and / or Eu, and / or Gd, and / or Tb, and / or Dy, and / or Ho, and / or Er, and / or Tm, and / or Yb, and / or Lu; The first conductive medium is selected from at least one of the following components: ZnO series, including Al-doped (AZO), and / or In-doped (IZO), and / or Ga-doped (GZO); magnetic oxides, including CoO, and / or MnO, and / or Fe 3 O 4 , and / or NiO; and other semiconductor oxides, including Ga 2 O 3 , and / or In 2 O 3 , and / or InSnO (ITO); The second heating medium includes a second dielectric medium, a second magnetic medium and a second conductive medium; The second dielectric is selected from ①BaO-MgO-Ta 2 O 5 , and / or BaO-ZnO-Ta 2 O 5 , and / or BaO-MgO-Nb 2 O 5 , and / or BaO-ZnO-Nb 2 O 5 systems and their composite systems; ②BaTi 4 O 9 , and / or BaTi 9 O 20 , (Zr, and / or Sn)TiO 4 Based on the system; ③BaO-Ln 2 O 3 -TiO 2 , and / or CaO-Li 2 O-Ln 2 O 3 -TiO 2 (Ln 2 O 3 4A 5 B 4 O 15 (A=Ba, and / or Sr, and / or Mg, and / or Zn, and / or Ca, B=Nb, and / or Ta), and / or AB 2 O 6 (A=Ca, and / or Co, and / or Mn, and / or Ni, and / or Zn; B=Nb, and / or Ta); (Ba 1-x M x )ZnO 5 (M=Ca, and / or Sr, x=0~1.0), AgNb 1-x Ta x O 3 (x=0~1.0), and / or LnAlO 3 (Ln=La, and / or Nd, and / or Sm), and / or Ta 2 O 5 -ZrO 2 , and / or ZnTiO 3 , and / or BiNbO 4 series; The second magnetic medium is selected from M-type hexagonal ferrite: BaM, and / or PbM, and / or SrM; X-type hexagonal ferrite, including Fe 2 X; W type hexagonal ferrite, including Mg 2 W, and / or Mn 2 W, and / or Fe 2 W, and / or Co 2 W, and / or Ni 2 W, and / or Cu 2 W, and / or Zn 2 W; Y-type hexagonal ferrite, including Mg 2 Y, and / or Mn 2 Y, and / or Fe 2 Y, and / or Co 2 Y, and / or Ni 2 Y, and / or Cu 2 Y, and / or Zn 2 Y; Z type hexagonal ferrite, including Mg 2 Z, and / or Mn 2 Z, and / or Fe 2 Z, and / or Co 2 Z, and / or Ni 2 Z, and / or Cu 2 Z, and / or Zn 2 Z; The second conductive medium is selected from the ZnO series, including Al-doped (AZO), and / or In-doped (IZO), and / or Ga-doped (GZO); magnetic oxides, including CoO, and / or MnO, and / or Fe 3 O 4 , and / or NiO; and other semiconductor oxides, including Ga 2 O 3 , and / or In 2 O 3 , and / or InSnO (ITO).

2. The heating medium of the aerosol generating substrate according to claim 1, It is characterized in that The first heating medium is formed into a core-shell type, a heterojunction type, a coating type, a porous type or a membrane composite type by mesoscopic compounding of physical and chemical methods; The core-shell type first heating medium includes an electric moment-magnetic moment coupling heating medium 1-H-1 of a core-shell type structure, an electric moment-conductivity coupling heating medium 1-H-2 of a core-shell type structure, or an electric moment-magnetic moment-conductivity coupling heating medium 1-H-3 of a core-shell type structure; The specific method of forming the first heating medium having the core-shell type is a direct precipitation method, a coprecipitation method, an alcohol salt hydrolysis method, or a sol-gel method; The first heating medium of the heterojunction structure includes an electric moment-magnetic moment coupling heating medium 1-Y-1 of the heterojunction structure, or an electric moment-conductivity coupling heating medium 1-Y-2 of the heterojunction structure, or an electric moment-magnetic moment-conductivity coupling heating medium 1-Y-3 of the heterojunction structure; The specific method for forming the first heating medium having the heterojunction structure is a molten salt method, a high-temperature solid-phase reaction method, a mechanical alloying method, a precipitation method with controlled calcination temperature, an alcohol salt hydrolysis method, a hydrothermal method, or a sol (gel)-hydrothermal method; The first heating medium of the encapsulated structure includes an electric moment-magnetic moment coupling heating medium 1-B-1 of the encapsulated structure or an electric moment-magnetic moment-conductivity coupling heating medium 1-B-2 of the encapsulated structure; The specific method of forming the first heating medium having the coated structure is a mechanical fusion coating method, a mechanochemical effect method induced by a high-energy mill, a low-heat solid phase reaction method, or a sol-gel method; The first heating medium with a porous structure is a porous structure electric moment-magnetic moment-conductance coupling heating medium 1-K, or a heating medium 1-D of a low excitation temperature aerosol generating matrix; The first heating medium of the membrane composite structure is an electric moment-magnetic moment-conductivity coupling heating medium 1-M; The second heating medium is formed into a core-shell type, a heterojunction type, a coating type, a porous type or a membrane composite type by mesoscopic compounding of physical and chemical methods; The core-shell type second heating medium includes an electric moment-magnetic moment coupling heating medium 2-H-1 of a core-shell type structure, an electric moment-conductivity coupling heating medium 2-H-2 of a core-shell type structure, or an electric moment-magnetic moment-conductivity coupling heating medium 2-H-3 of a core-shell type structure; The specific method of forming the second heating medium having the core-shell type is a direct precipitation method, a coprecipitation method, an alcohol salt hydrolysis method, or a sol-gel method; The second heating medium of the heterojunction structure includes an electric moment-magnetic moment coupling heating medium 2-Y-1 of the heterojunction structure, or an electric moment-conductivity coupling heating medium 2-Y-2 of the heterojunction structure, or an electric moment-magnetic moment-conductivity coupling heating medium 2-Y-3 of the heterojunction structure; The specific method for forming the second heating medium having the heterojunction structure is a molten salt method, a high-temperature solid-phase reaction method, a mechanical alloying method, a precipitation method with controlled calcination temperature, an alcohol salt hydrolysis method, a hydrothermal method, or a sol (gel)-hydrothermal method; The second heating medium of the encapsulated structure includes an electric moment-magnetic moment coupling heating medium 2-B-1 of the encapsulated structure or an electric moment-magnetic moment-conductivity coupling heating medium 2-B-2 of the encapsulated structure; The specific method of forming the second heating medium having the coated structure is a mechanical fusion coating method, a mechanical chemical effect method induced by a high-energy mill, a low-heat solid phase reaction method, or a sol-gel method; The second heating medium with a porous structure is a porous electric moment-magnetic moment-conductance coupling heating medium 2-K, or a heating medium 2-D of a low excitation temperature aerosol generating matrix; The second heating medium of the film composite structure is an electric moment-magnetic moment-conductivity coupling heating medium 2-M.

3. The heating medium according to claim 2, It is characterized in that The electric moment-magnetic moment-conductivity coupling heating medium 1-K of the porous structure is prepared according to the following method: The ultrafine particles of at least one component of the first dielectric, the first magnetic medium and the first conductive medium in the first heating medium are fully mixed with an inorganic binder, sodium silicate, or aluminum dihydrogen phosphate, or phosphoric acid-copper oxide, and a pore-forming agent, ultrafine carbon powder or starch, or ultrafine calcium carbonate, and then sintered, crushed and classified to obtain the porous structure of the electric moment-magnetic moment-conductivity coupled heating medium 1-K; or at least one component of the first dielectric, at least one component of the first magnetic medium system and at least one component of the first conductive medium are obtained by a polymer network gel method, or a soluble complex network gel is obtained by a metal complex gel method, and then dried, sintered, crushed and classified to obtain the porous structure of the electric moment-magnetic moment-conductivity coupled heating medium 1-K; or the first dielectric is treated by ions of at least one component of the first magnetic medium and ions of at least one component of the first conductive medium in a solution and a precipitant. The granular porous body is modified by precipitation method, so that a composite film layer of the first magnetic medium component and the first conductive medium component is formed on the inner surface of the pores, so as to obtain the electric moment-magnetic moment-conductivity coupling heating medium 1-K of the porous structure; or ultrafine particles of at least one component of the first dielectric and the first magnetic medium in the first heating medium are fully mixed with inorganic binder sodium silicate, or aluminum dihydrogen phosphate, or phosphoric acid-copper oxide, and pore-forming agent ultrafine carbon powder or starch, or ultrafine calcium carbonate, and then sintered, crushed and classified to obtain the electric moment-magnetic moment coupling heating medium of the porous structure, and then the pores of the electric moment-magnetic moment coupling heating medium of the porous structure are modified by chemical plating method, and the metal ions of at least one component of the first conductive medium system adsorbed in the plating solution in the pores are catalytically reduced to metal by the reducing agent in the plating solution and deposited on the inner surface of the pores to obtain the electric moment-magnetic moment-conductivity coupling heating medium 1-K of the porous structure; The electric moment-magnetic moment-conductivity coupling heating medium of the porous structure has a pore size of 2 nm to 50 μm and a porosity of 70% to 95%; The electric moment-magnetic moment-conductivity coupling heating medium 2-K of the porous structure is prepared according to the following method: The ultrafine particles of at least one component of the second dielectric, the second magnetic medium and the second conductive medium system in the second heating medium are fully mixed with the inorganic binder sodium silicate, or aluminum dihydrogen phosphate, or phosphoric acid-copper oxide, and the pore-forming agent ultrafine carbon powder or starch, or ultrafine calcium carbonate, and then sintered, crushed and classified to obtain the electric moment-magnetic moment-conductivity coupling heating medium 2-K of the porous structure; or the gel obtained by the polymer network gel method or the soluble complex network gel obtained by the metal complex gel method of at least one component in the second dielectric, at least one component in the second magnetic medium and at least one component in the second conductive medium is dried, sintered, crushed and classified to obtain the electric moment-magnetic moment-conductivity coupling heating medium 2-K of the porous structure; or modifying the second dielectric particle porous body by precipitation method through ions of at least one component of the second magnetic medium system and ions of at least one component of the second conductive medium system in the solution and a precipitant, so that a composite film layer of the second magnetic medium component and the second conductive medium component is formed on the inner surface of the pores, thereby obtaining the electric moment-magnetic moment-conductivity coupled heating medium 2-K of the porous structure; or ultrafine particles of at least one component of the second dielectric and the second magnetic medium system in the second heating medium are mixed with an inorganic binder of sodium silicate, or dihydrogen aluminum phosphate, or phosphoric acid-copper oxide, and a pore-forming agent of ultrafine carbon powder or starch, or ultrafine carbon After the acid and calcium are fully mixed, sintering, crushing and classification are carried out to obtain the electric moment-magnetic moment coupled heating medium of the porous structure, and then the pores of the electric moment-magnetic moment coupled heating medium of the porous structure are modified by chemical plating, and the metal ions of at least one component of the second conductive medium adsorbed in the plating solution in the pores are catalytically reduced to metal by the reducing agent in the plating solution and deposited on the inner surface of the pores to obtain the electric moment-magnetic moment-conductivity coupled heating medium 2-K of the porous structure. The pore size of the electric moment-magnetic moment-conductivity coupled heating medium 2-K of the porous structure is 2nm to 50μm, and the porosity is 70% to 95%.

4. The heating medium according to claim 3, It is characterized in that The heating medium 1-D of the low excitation temperature aerosol generating substrate is prepared according to the following method: From the electric moment-magnetic moment-conductivity coupling heating medium 1-K of the porous structure, a pore size range of 60nm to 50μm, a porosity range of 85% to 95%, and a specific heat capacity range of 0.1kJ·kg -1 ·K -1 Up to 0.6 kJ·kg -1 ·K -1 , thermal conductivity range is 0.035W·m -1 ·K -1 To 0.125W·m-1·K -1 The particles with the physical property parameters adsorb the liquid phase components of the aerosol generating medium, so that the liquid phase components are separated into small droplets entering the pores with a porosity of 85% to 95%, and the pore size range is 60nm to 50μm, so as to increase the saturated vapor pressure value of the liquid phase components of the aerosol generating medium, and obtain the heating medium of the low excitation temperature aerosol generating matrix, the excitation temperature is 160℃~200℃, and the particle size distribution range of the heating medium 1-D particles of the low excitation temperature aerosol generating matrix is ​​15μm to 500μm; The heating medium 2-D of the low excitation temperature aerosol generating substrate is prepared according to the following method: From the electric moment-magnetic moment-conductivity coupling heating medium 2-K of the porous structure, select the pores The diameter ranges from 60nm to 50μm, the porosity ranges from 85% to 95%, and the specific heat capacity ranges from 0.1kJ·kg -1 ·K -1 Up to 0.6 kJ·kg -1 ·K -1 , thermal conductivity range is 0.035W·m -1 ·K -1 To 0.125W·m-1·K -1 The particles with different physical property parameters adsorb the liquid phase components of the aerosol generating medium, so that the liquid phase components are separated into small droplets entering the pores with a porosity of 85% to 95%, and the pore size range is 60nm to 50μm, so as to increase the saturated vapor pressure value of the liquid phase components of the aerosol generating medium, and obtain the heating medium of the low excitation temperature aerosol generating matrix, the excitation temperature is 160℃~200℃, and the particle size distribution range of the 2-D particles of the heating medium of the low excitation temperature aerosol generating matrix is ​​15μm to 500μm.

5. The heating medium according to claim 2, It is characterized in that The electric moment-magnetic moment-conductivity coupling heating medium 1-M is prepared according to the following method: After fully mixing the ultrafine particles of at least one component of the first dielectric, the first magnetic medium and the first conductive medium system in the first heating medium with the binder sodium silicate, or aluminum dihydrogen phosphate, or phosphoric acid-copper oxide, a single-sided or double-sided film composite is performed on an aluminum sheet, a copper sheet or a stainless steel sheet by spraying or brushing to obtain the electric moment-magnetic moment-conductivity coupling heating medium 1-M of the film composite structure; or the particles of at least one component of the first dielectric, the first magnetic medium and the first conductive medium system in the first heating medium are deposited or sprayed on a single-sided or double-sided film composite on an aluminum sheet, a copper sheet or a stainless steel sheet by vapor deposition, flame vapor deposition or plasma spraying to prepare the electric moment-magnetic moment-conductivity coupling heating medium 1-M of the film composite structure; The electric moment-magnetic moment-conductivity coupling heating medium 2-M is prepared according to the following method: Ultrafine particles of at least one component of the second dielectric, second magnetic medium and second conductive medium system in the second heating medium are fully mixed with a binder of sodium silicate, or aluminum dihydrogen phosphate, or phosphoric acid-copper oxide, and then a single-sided or double-sided film composite is performed on an aluminum sheet, copper sheet or stainless steel sheet by spraying or brushing to obtain the electric moment-magnetic moment-conductivity coupled heating medium 2-M of the film composite structure; or particles of at least one component of the second dielectric, second magnetic medium and second conductive medium in the second heating medium are deposited or sprayed on a single-sided or double-sided film composite on an aluminum sheet, copper sheet or stainless steel sheet by vapor deposition, flame vapor deposition or plasma spraying to prepare the electric moment-magnetic moment-conductivity coupled heating medium 2-M of the film composite structure.

6. The heating medium according to claim 4, It is characterized in that The aerosol generating substrate also includes an aerosol substrate; The heating medium is directly blended with the aerosol matrix, or before the tobacco sheet in the aerosol matrix is ​​paper-made or rolled, the heating medium is mixed into the fiber slurry or paste, so that the tobacco sheet is evenly distributed with a mass ratio of 5 to 60% of the heating medium, and the particle size of the heating medium is 0.1 μm to 100 μm; Or a heating medium with a porous structure and a particle size of 15 μm to 100 μm, or a heating medium of a low excitation temperature aerosol generating matrix with a particle size of 15 μm to 100 μm is adsorbed with the liquid phase component in the aerosol matrix and then blended with the heating medium and the aerosol matrix.

7. The heating medium according to claim 1, It is characterized in that Also included are foil-like film composite heating media; The foil-like film composite heating medium is prepared by mixing the heating medium particles with a binder, carboxymethyl cellulose, or guar gum or tobacco extract, and then composite the aluminum foil or copper foil on one side or both sides with the film by a casting method or a spraying method, and then cutting the composite heating medium to have a size comparable to that of tobacco flakes, and a particle size distribution range of the heating medium particles is 15 μm to 100 μm; or the dielectric component and the precursor of the magnetic medium component are used to prepare the composite heating medium by chemical vapor deposition, gas phase pyrolysis, gas phase hydrolysis, gas phase combustion, or flame vapor deposition.

8. An aerosol generation system using multi-card coupling giant thermal effect, It is characterized in that It comprises a heating structure, the heating structure comprises a casing, and the casing is provided with a casing air inlet hole; A preheating housing is arranged in the casing; The casing and the preheating shell are coaxially opened; The opening of the preheating shell is connected to the filter segment; the preheating shell is provided with a preheating shell air inlet hole; A plurality of pole plates are arranged inside the preheating housing; the plurality of pole plates form a heating chamber; A heating chamber base is provided at the bottom of the heating chamber; a temperature control unit passes through the central hole of the heating chamber base, and a base disc air inlet hole is provided on the heating chamber base; The upper end of the heating chamber is connected to the sealing ring and is nested in the opening of the preheating shell; The interior of the electrode plate is an aerosol generating section; a metal particle layer filter medium is provided between the aerosol generating section and the filter tip section; The aerosol generating section contains an aerosol generating matrix 1; The electrode plate is connected to the heating drive unit via an electrode plate feeder; The aerosol generating substrate 1 comprises the first heating medium described in claim 1.

9. The heating structure according to claim 8, It is characterized in that The electrode plate is a tubular electrode plate; the tubular electrode plate comprises a tubular insulating ceramic substrate, and a curved electrode 1 and a curved electrode 2 arranged on the inner surface of the tubular insulating ceramic substrate; The curved surface electrodes 1 and the curved surface electrodes 2 are arranged in opposite sections; adjacent curved surface electrodes 1 and curved surface electrodes 2 are separated by insulating materials; The number of the curved surface electrodes 1 and the number of the curved surface electrodes 2 are 2 to 5 respectively.

10. The heating structure according to claim 8, It is characterized in that The electrode plate is a plurality of planar electrodes; the electrode plate comprises a planar electrode plate 1 and a planar electrode plate 2 which are parallel and opposite to each other; The distance between the planar electrode plate 1 and the planar electrode plate 2 is the diameter of the aerosol generating section.

11. The heating structure according to claim 10, It is characterized in that A block of heating medium 1 is sandwiched between two ends of each pair of the planar electrode plate 1 and the planar electrode plate 2; A cylindrical hole is provided at the symmetric center of the two sandwiched block heating media 1, and the diameter of the cylindrical hole is the diameter of the aerosol generating section.

12. The heating structure according to claim 8, It is characterized in that The thickness of the metal particle layer filter medium is 0.2 mm to 1.2 mm; The metal particle layer filter is formed by pressing aluminum particles with a size of 0.5 to 1.5 mm.

13. The heating structure according to claim 11, It is characterized in that The block heating medium 1 includes first heating medium particles and an inorganic binder; The inorganic binder is selected from one or more of sodium silicate, aluminum dihydrogen phosphate and phosphoric acid-copper oxide.

14. The heating structure according to claim 8, It is characterized in that The air inlet hole of the base disc is a through hole with a diameter of 0.3 to 2 mm; The number of the air inlet holes is 8 to 36.

15. The heating structure according to claim 8, It is characterized in that The frequency of the alternating electromagnetic field used by the heating drive unit has a balanced compatible response frequency that meets the requirements of multi-card coupling of electric cards, magnetic cards and conductive cards for multi-field coupling driving. When the compatible response frequency range is from 0.3MHz to 300MHz, it is suitable for the first heating medium.

16. The heating structure according to claim 8, It is characterized in that The inner surface of the preheating shell is provided with a first heating medium particle coating; The first heating medium particle coating comprises a hexagonal boron carbon nitrogen ternary absorbing ceramic substrate and a coating coated on the substrate, wherein the coating comprises first heating medium particles and a film-forming agent; the film-forming agent is selected from sodium silicate sol, or aluminum dihydrogen phosphate sol, or aluminum hydroxide sol, or silica sol; or the first heating medium particle coating comprises a metal substrate and a coating coated on the metal substrate, the coating comprising first heating medium particles and an inorganic binder; The inorganic binder is selected from sodium silicate, aluminum dihydrogen phosphate, or phosphoric acid-copper oxide.

17. An aerosol generation system using multi-card coupling giant thermal effect, It is characterized in that It comprises a heating structure, the heating structure comprises a casing, and the casing is provided with a casing air inlet hole; A preheating housing is arranged in the casing; The casing and the preheating shell are coaxially opened; The opening of the preheating shell is connected to the filter segment; the preheating shell is provided with a preheating shell air inlet hole; The preheating shell is provided with a metal shielding shell, a block heating medium 2 and an antenna embedded in the block heating medium 2; the metal shielding shell is wrapped around the outside of the block heating medium 2; The metal shielding shell, the block heating medium 2 and the antenna embedded in the block heating medium 2 form a heating cavity; The air inlet seat hole of the heating chamber is connected to the outside of the block heating medium 2 through 4 to 10 air inlet channels with a diameter of 0.5 to 2 mm; The block heating medium 2 is a cube; a cylindrical hole is provided on the symmetry axis of the block heating medium 2, and an aerosol generating section is formed inside the hole; a wave-transmitting ceramic tube is nested inside the cylindrical hole, and the inner diameter of the wave-transmitting ceramic tube is the diameter of the aerosol generating section; The upper end of the heating chamber is connected to the sealing ring and is nested in the opening of the preheating shell; A metal particle layer filter medium is provided between the aerosol generating section and the filter tip section; The aerosol generating section contains an aerosol generating matrix 2; The antenna is connected to the heating drive unit via an antenna feeder foot; The aerosol generating substrate 2 comprises the second heating medium described in claim 1.

18. The heating structure according to claim 17, It is characterized in that The wave-transmitting ceramic tube is selected from quartz SiO 2 Ceramic tube, or high alumina ceramic tube, or Si 3 N 4 Ceramic tube.

19. The heating structure according to claim 17, It is characterized in that It also includes a temperature control unit, which is laterally placed on the inner surface of the wave-transmitting ceramic tube at a distance of 2 to 3 mm from the free port of the aerosol generating section.

20. The heating structure according to claim 17, It is characterized in that The block heating medium 2 includes second heating medium particles and an inorganic binder; The inorganic binder is selected from sodium silicate, aluminum dihydrogen phosphate, or phosphoric acid-copper oxide.

21. The heating structure according to claim 17, It is characterized in that A second heating medium particle coating is provided on the inner surface of the preheating shell; The second heating medium particle coating comprises a hexagonal boron carbon nitrogen ternary absorbing ceramic substrate and a coating coated on the substrate, wherein the coating comprises second heating medium particles and a film-forming agent; the film-forming agent is selected from sodium silicate sol, or aluminum dihydrogen phosphate sol, or aluminum hydroxide sol, or silica sol; or the second heating medium particle coating comprises a metal substrate and a coating coated on the metal substrate, the coating comprising second heating medium particles and an inorganic binder; The inorganic binder is selected from sodium silicate, aluminum dihydrogen phosphate, or phosphoric acid-copper oxide.

22. The heating structure according to claim 17, It is characterized in that The heating drive unit uses the frequency of the alternating electromagnetic field, and has a balanced compatible response frequency that meets the requirements of multi-card coupling of electric cards, magnetic cards and conductive cards for multi-field coupling driving. When the compatible response frequency range is in the range of 0.3 GHz to 30 GHz, it is suitable for the second heating medium.

Citation Information

Cited By

  • Aerosol generating system using multi-caloric coupling giant caloric effect, and heating medium

    EP4497337A1

  • Aerosol generating system using multi-caloric coupling giant caloric effect, and heating medium

    WO2023202081A1