Method for producing pyromellitic acid by liquid phase oxidation of durenyl
Through the liquid phase oxidation method of homotetratoluene, a two-stage reaction was adopted and the catalyst composition and reaction conditions were optimized, which solved the problems of large catalyst dosage and low product yield, and achieved efficient production of chlorophenol.
Patent Information
- Application Number
- CN202110446554.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2021-04-25
- Publication Date
- 2024-11-29
- Estimated Expiration
- 2041-04-25
AI Technical Summary
The existing production methods for phenylatinic acid have large catalyst usage and low product yield.
The liquid phase oxidation method of homotetratoluene is adopted, and a two-stage reaction is carried out: in the first stage, in the presence of catalyst and solvent, the oxidant and homotetratoluene undergo liquid phase oxidation reaction, the reaction temperature gradually increases and maintains, and the second stage, the bromine-containing compounds and Pure water, the oxidation reaction continues to produce phenylene tetracarboxylic acid. The catalyst used in this process contains Co salt, Mn salt and bromine-containing compound, preferably Zr salt and rare earth salt, the reaction temperature and pressure are between 150°C and 230°C, and the reaction time is adjustable.
The yield of phenylatic acid is significantly improved, the amount of catalyst is reduced, and the purity and yield of the product are improved.
Smart Images

Figure BDA0003036719670000041 
Figure BDA0003036719670000141 
Figure BDA0003036719670000151
Abstract
Description
Technical Field
[0001] The invention relates to a method for producing pyromellitic acid by liquid-phase oxidation of durenyl. Background Art
[0002] Pyromellitic acid (PMA) is an important chemical raw material. It can be further dehydrated to generate pyromellitic dianhydride (PMDA). The use of PMDA is constantly expanding. It can react with 4,4-diaminobiphenyl ether to synthesize polyimide (PI). Polyimide is a new synthetic material that is resistant to high temperature, low temperature, radiation, impact, and has excellent electrical and mechanical properties. It has important uses in the aerospace industry, atomic energy industry, and electromechanical industry that cannot be replaced by other engineering plastics. With the continuous expansion of the market use of polyimide, the demand for pyromellitic dianhydride as the main raw material for synthesizing polyimide is also increasing day by day; at the same time, PMA can also undergo dehydration condensation with different alcohols and phenols, and can be used as shrinkage agents with different properties.
[0003] There are currently two main production methods for PMA. One uses gas-phase oxidation to directly generate PMDA, using vanadium dioxide as the main catalyst and oxidizing at 450-500°C. The advantage of this oxidation is that PMDA can be produced in one step, but the purity is not high. In addition, the yield of PMDA is low. The current industrial yield is below 45wt%, and a large part of it is deeply oxidized to CO2. The other method uses liquid-phase oxidation, which is the same as the MC process, using Co / Mn / Br / Zr as the catalyst system, oxidizing at 150-250°C, 1.0-3.0Mpa, and then crystallizing, separating, activated carbon adsorption and other purification processes to obtain PMA. Japanese patent JP2014152143 (Method for preparing pyromellitic acid) uses two-step oxidation to produce pyromellitic acid: first, Co / Mn / Br is used as a catalyst, oxygen is introduced at a temperature of 150°C and a pressure of 3.6MPa for reaction for 30 minutes, then Co / Mn / Br catalyst is added, and pure water is added to continue the reaction for 60 minutes until the temperature reaches 230°C, and then the reaction is continued at 230°C for another 30 minutes; the entire reaction consumes 1.1% Br and 3000ppm Co / Mn. The PMA yield is about 75%. U.S. Patent US5041633 (Process for the Production of an Aromatic Polycarboxylic Acid) also uses a two-step method, using Co / Mn / Br / Zr as a catalyst system, and the materials and catalysts are added semi-continuously, the Br dosage is 1.5wt%, and the PMA yield is up to 84%. Summary of the invention
[0004] The technical problem to be solved by the present invention is the problem of large catalyst dosage and low product yield in the prior art, and a new method for producing pyromellitic acid by liquid phase oxidation of durenyl is provided, which has the characteristics of small catalyst dosage and high product yield.
[0005] In order to solve the above technical problems, the technical solution adopted by the present invention is as follows:
[0006] The method for producing pyromellitic acid by liquid phase oxidation of durenyl comprises:
[0007] First stage reaction
[0008] The method comprises the following steps: in the presence of a catalyst and a solvent, an oxidant and durene are subjected to a liquid phase oxidation reaction to obtain an intermediate product mixture; the reaction temperature change of the first stage reaction sequentially comprises: a reaction temperature rising process of gradually raising the temperature from T11 to T12, and a reaction temperature maintaining process of maintaining T13, wherein T11 is 100 to 120° C., and T12 and T13 are independently 160 to 180° C.;
[0009] The catalyst contains Co salt, Mn salt and bromine-containing compound 1;
[0010] Second stage reaction
[0011] The above intermediate product mixture is used as a raw material, a mixture of bromine-containing compound 2 and pure water is added, and the oxidation reaction with the oxidant is continued to obtain the product containing pyromellitic acid, and the reaction temperature T2 is 180-230°C.
[0012] In the prior art, the first stage reaction either continues to increase the temperature or directly maintains the temperature at a certain reaction temperature. However, the present invention significantly improves the PMA yield by first undergoing a temperature increase reaction stage and a reaction temperature maintenance stage in the first stage reaction.
[0013] As a non-limiting example, T11 may be, but is not limited to, 111° C., 112° C., 113° C., 114° C., 115° C., 116° C., 117° C., 118° C., 119° C., and the like.
[0014] As a non-limiting example, T12 can be but is not limited to 161°C, 162°C, 163°C, 164°C, 165°C, 166°C, 167°C, 168°C, 169°C, 170°C, 171°C, 172°C, 173°C, 174°C, 175°C, 176°C, 177°C, 178°C, 179°C, etc.
[0015] As a non-limiting example, T13 can be but is not limited to 161°C, 162°C, 163°C, 164°C, 165°C, 166°C, 167°C, 168°C, 169°C, 170°C, 171°C, 172°C, 173°C, 174°C, 175°C, 176°C, 177°C, 178°C, 179°C, etc.
[0016] As a non-limiting example, T2 may be, but is not limited to, 185°C, 190°C, 195°C, 200°C, 205°C, 210°C, 215°C, 220°C, 225°C, and the like.
[0017] In the above technical solution, preferably the catalyst comprises Zr salt and / or rare earth salt.
[0018] In the above technical solution, preferably the solvent includes acetic acid and / or water.
[0019] In the above technical solution, the oxidant is preferably a gas containing oxygen, preferably air.
[0020] In the above technical scheme, the heating rate from T11 to T12 is preferably 1 to 3°C / min, for example but not limited to a heating rate of 1.1, 1.2, 1.3, 1.4, 1.5, 1.6, 1.7, 1.8, 1.9, 2.0, 2.1, 2.2, 2.3, 2.4, 2.5, 2.6, 2.7, 2.8, 2.9 and the like.
[0021] In the above technical scheme, it is preferred that the reaction pressure in the reaction temperature heating process gradually increasing from T11 to T12 in the first stage reaction, the reaction temperature maintaining process maintaining T13 in the first stage reaction, and the second stage reaction process are independently 1.0 to 5.0 MPa, for example but not limited to 1.5 MPa, 2.0 MPa, 2.5 MPa, 3.0 MPa, 3.5 MPa, 4.0 MPa, 4.5 MPa, etc.
[0022] In the above technical scheme, it is preferred that the reaction temperature maintenance process of maintaining T13 in the first stage reaction lasts for 10 to 40 minutes, for example but not limited to 12 minutes, 14 minutes, 16 minutes, 18 minutes, 20 minutes, 22 minutes, 24 minutes, 26 minutes, 28 minutes, 30 minutes, 32 minutes, 34 minutes, 36 minutes, 38 minutes, 39 minutes and the like.
[0023] In the above technical solution, the reaction time of the second stage reaction is preferably 10 to 60 minutes, for example but not limited to 15, 20, 25, 30, 35, 40, 45, 50, 55, etc.
[0024] In the above technical solution, it is preferred that the bromine-containing compound 1 and the bromine-containing compound 2 are independently selected from at least one of the substance group consisting of hydrogen bromide and tetrabromoethane.
[0025] In the above technical solution, it is preferred that the bromine content in the mixture of bromide and pure water in the second stage is 0.5-2.5wt%, for example but not limited to 0.6wt%, 0.7wt%, 0.8wt%, 0.9wt%, 1.0wt%, 1.1wt%, 1.2wt%, 1.3wt%, 1.4wt%, 1.5wt%, 1.6wt%, 1.7wt%, 1.8wt%, 1.9wt%, 2.0wt%, 2.1wt%, 2.2wt%, 2.3wt%, 2.4wt% and the like.
[0026] In the above technical scheme, the bromine-containing compound 2 is preferably 0.01 to 1.0 times the mass of tetramethylbenzene, for example but not limited to 0.015 times, 0.02 times, 0.025 times, 0.03 times, 0.035 times, 0.04 times, 0.045 times, 0.05 times, 0.055 times, 0.06 times, 0.065 times, 0.07 times, 0.075 times, 0.08 times, 0.085 times, 0.09 times, 0.095 times, etc.
[0027] In the above technical solution, the catalyst preferably comprises:
[0028] The Co salt, calculated as Co, is 300 to 1000 parts by weight (for example, but not limited to, 350 parts by weight, 400 parts by weight, 450 parts by weight, 500 parts by weight, 550 parts by weight, 600 parts by weight, 650 parts by weight, 700 parts by weight, 750 parts by weight, 800 parts by weight, 850 parts by weight, 900 parts by weight, 950 parts by weight);
[0029] The Mn salt is 200 to 800 parts by weight (for example, but not limited to, 250 parts by weight, 300 parts by weight, 350 parts by weight, 400 parts by weight, 450 parts by weight, 500 parts by weight, 550 parts by weight, 600 parts by weight, 650 parts by weight, 700 parts by weight, 750 parts by weight, etc.) calculated as Mn;
[0030] The bromine-containing compound 1, calculated as Br, is 100 to 1000 parts by weight (for example, but not limited to 150 parts by weight, 200 parts by weight, 250 parts by weight, 300 parts by weight, 350 parts by weight, 400 parts by weight, 450 parts by weight, 500 parts by weight, 550 parts by weight, 600 parts by weight, 650 parts by weight, 700 parts by weight, 750 parts by weight, 800 parts by weight, 850 parts by weight, 900 parts by weight, 950 parts by weight, etc.).
[0031] In the above technical scheme, the catalyst preferably includes a Zr salt; more preferably, the Zr salt is 2 to 50 parts by weight (for example, but not limited to 4 parts by weight, 6 parts by weight, 8 parts by weight, 10 parts by weight, 15 parts by weight, 20 parts by weight, 25 parts by weight, 30 parts by weight, 35 parts by weight, 40 parts by weight, 45 parts by weight, etc.) calculated as Zr.
[0032] In the above technical scheme, the catalyst preferably includes a rare earth salt; more preferably, the rare earth salt is 2 to 50 parts by weight (for example, but not limited to 4 parts by weight, 6 parts by weight, 8 parts by weight, 10 parts by weight, 15 parts by weight, 20 parts by weight, 25 parts by weight, 30 parts by weight, 35 parts by weight, 40 parts by weight, 45 parts by weight, etc.) calculated as rare earth elements.
[0033] In the above technical solution, preferably the Co salt is cobalt acetate.
[0034] In the above technical solution, preferably the Mn salt is manganese acetate.
[0035] In the above technical solution, preferably the Zr salt is zirconium acetate.
[0036] In the above technical solution, preferably, the rare earth salt includes at least one selected from the group consisting of cerium acetate, lanthanum acetate, neodymium acetate and samarium acetate.
[0037] In the above technical solution, it is preferred that the bromine-containing compound 1 and the bromine-containing compound 2 are independently bromine-containing compounds that are easily soluble in water and / or acetic acid.
[0038] In the above-mentioned first technical solution, the synthetic oxidant is preferably air, and the air velocity (the ratio of the gas volume flow rate to the volume of the liquid raw material mixture) is 2 to 5 h -1 For example, but not limited to, the air velocity is 2.5h -1 , 3.0h -1 , 3.5h -1 , 4.0h -1 , 4.5h -1 etc.
[0039] For the products of the embodiments of the present invention and the comparative examples, the samples to be analyzed were first completely dissolved in dimethyl sulfoxide and analyzed by high performance liquid chromatography (HPLC).
[0040] Co, Mn, Zr and Ce in the product are analyzed by ICP.
[0041]
[0042] The present invention will be further described below by way of examples. DETAILED DESCRIPTION
[0043] [Example 1]
[0044] The reaction was carried out in a 1000 ml titanium autoclave equipped with a magnetic stirrer, a gas delivery pipe, an in-autoclave cooling bypass pipe, a reflux condenser, a thermocouple, and a bursting disc. The stirring speed was 400 rpm and the reaction was heated by circulating hot oil. The reaction steps are as follows:
[0045] 1) durene, acetic acid, cobalt acetate tetrahydrate, manganese acetate tetrahydrate, zirconium acetate, cerium acetate and hydrogen bromide are uniformly mixed to obtain a liquid raw material mixture, wherein the liquid raw material mixture contains 100 g of durene, 300 g of acetic acid, 500 ppmw of cobalt, 250 ppmw of manganese, 10 ppmw of Zr, 10 ppmw of Ce and 600 ppmw of bromine, and the liquid raw material mixture is added into an autoclave and sealed.
[0046] 2) Add 3.0MPa nitrogen and conduct an airtight test for 30 minutes. The test is qualified if the pressure drop is no more than 0.1MPa within 30 minutes.
[0047] 3) Add nitrogen, the air velocity is 6h -1 (Space velocity is the ratio of the volume of nitrogen to the volume of the liquid raw material mixture) and start the stirrer at a stirring rate of 400 rpm, raise the temperature to 110°C, and maintain the pressure at 2.0 MPa.
[0048] 4) Switch with air at 110℃, pressure of 2.0MPa, air volume velocity of 6h -1 (space velocity is the ratio of the volume flow rate of air to the volume of the liquid raw material mixture), the temperature was raised to 170°C at a heating rate of 2°C / min, and then the temperature was maintained at 170°C for 30 minutes to complete the first stage reaction.
[0049] 5) After the first stage is completed, the temperature is raised to 210°C in 10 minutes. At the same time, a 2.0 wt% aqueous solution of hydrogen bromide is added to the reactor at a flow rate of 10 g / min over 10 minutes. The reactor pressure is 2.0 MPa and the air volume space velocity is 6 h -1 (space velocity is the ratio of the volume flow rate of air to the volume of the liquid raw material mixture), continue the reaction at 210°C for 20 minutes, switch to nitrogen again after the temperature reaction is good, cool to room temperature, depressurize the reactor to normal pressure, add dimethyl sulfoxide to completely dissolve the oxidation product, and analyze the product by high performance liquid chromatography.
[0050] For ease of comparison, the main experimental conditions and experimental results are summarized in Table 1.
[0051] [Example 2]
[0052] The reaction was carried out in a 1000 ml titanium autoclave equipped with a magnetic stirrer, a gas delivery pipe, an in-autoclave cooling bypass pipe, a reflux condenser, a thermocouple, and a bursting disc. The stirring speed was 400 rpm and the reaction was heated by circulating hot oil. The reaction steps are as follows:
[0053] 1) durene, acetic acid, cobalt acetate tetrahydrate, manganese acetate tetrahydrate, zirconium acetate, cerium acetate and hydrogen bromide are uniformly mixed to obtain a liquid raw material mixture, wherein the liquid raw material mixture contains 100 g of durene, 300 g of acetic acid, 500 ppmw of cobalt, 250 ppmw of manganese, 10 ppmw of Zr, 10 ppmw of Ce and 600 ppmw of bromine, and the liquid raw material mixture is added into an autoclave and sealed.
[0054] 2) Add 3.0MPa nitrogen and conduct an airtight test for 30 minutes. The test is qualified if the pressure drop is no more than 0.1MPa within 30 minutes.
[0055] 3) Add nitrogen, the air velocity is 6h -1 (Space velocity is the ratio of the volume of nitrogen to the volume of the liquid raw material mixture) and start the stirrer at a stirring rate of 400 rpm, raise the temperature to 100°C, and maintain the pressure at 2.0 MPa.
[0056] 4) Switch to air at 100℃, pressure 2.0MPa, air volume velocity 6h -1 (space velocity is the ratio of the volume flow rate of air to the volume of the liquid raw material mixture), the temperature was raised to 170°C at a heating rate of 2°C / min, and then the temperature was maintained at 170°C for 30 minutes to complete the first stage reaction.
[0057] 5) After the first stage is completed, the temperature is raised to 210°C in 10 minutes. At the same time, a 2.0 wt% aqueous solution of hydrogen bromide is added to the reactor at a flow rate of 10 g / min over 10 minutes. The reactor pressure is 2.0 MPa and the air volume space velocity is 6 h -1 (space velocity is the ratio of the volume flow rate of air to the volume of the liquid raw material mixture), continue the reaction at 210°C for 20 minutes, switch to nitrogen again after the temperature reaction is good, cool to room temperature, depressurize the reactor to normal pressure, add dimethyl sulfoxide to completely dissolve the oxidation product, and analyze the product by high performance liquid chromatography.
[0058] For ease of comparison, the main experimental conditions and experimental results are summarized in Table 1.
[0059] [Example 3]
[0060] The reaction was carried out in a 1000 ml titanium autoclave equipped with a magnetic stirrer, a gas delivery pipe, an in-autoclave cooling bypass pipe, a reflux condenser, a thermocouple, and a bursting disc. The stirring speed was 400 rpm and the reaction was heated by circulating hot oil. The reaction steps are as follows:
[0061] 1) durene, acetic acid, cobalt acetate tetrahydrate, manganese acetate tetrahydrate, zirconium acetate, cerium acetate and hydrogen bromide are uniformly mixed to obtain a liquid raw material mixture, wherein the liquid raw material mixture contains 100 g of durene, 300 g of acetic acid, 500 ppmw of cobalt, 250 ppmw of manganese, 10 ppmw of Zr, 10 ppmw of Ce and 600 ppmw of bromine, and the liquid raw material mixture is added into an autoclave and sealed.
[0062] 2) Add 3.0MPa nitrogen and conduct an airtight test for 30 minutes. The test is qualified if the pressure drop is no more than 0.1MPa within 30 minutes.
[0063] 3) Add nitrogen, the air velocity is 6h -1 (Space velocity is the ratio of the volume of nitrogen to the volume of the liquid raw material mixture) and start the stirrer at a stirring rate of 400 rpm, raise the temperature to 120°C, and maintain the pressure at 2.0 MPa.
[0064] 4) Switch with air at 120℃, pressure of 2.0MPa, air volume velocity of 6h -1 (space velocity is the ratio of the volume flow rate of air to the volume of the liquid raw material mixture), the temperature was raised to 170°C at a heating rate of 2°C / min, and then the temperature was maintained at 170°C for 30 minutes to complete the first stage reaction.
[0065] 5) After the first stage is completed, the temperature is raised to 210°C in 10 minutes. At the same time, a 2.0 wt% aqueous solution of hydrogen bromide is added to the reactor at a flow rate of 10 g / min over 10 minutes. The reactor pressure is 2.0 MPa and the air volume space velocity is 6 h -1 (space velocity is the ratio of the volume flow rate of air to the volume of the liquid raw material mixture), continue the reaction at 210°C for 20 minutes, switch to nitrogen again after the temperature reaction is good, cool to room temperature, depressurize the reactor to normal pressure, add dimethyl sulfoxide to completely dissolve the oxidation product, and analyze the product by high performance liquid chromatography.
[0066] For ease of comparison, the main experimental conditions and experimental results are summarized in Table 1.
[0067] [Example 4]
[0068] The reaction was carried out in a 1000 ml titanium autoclave equipped with a magnetic stirrer, a gas delivery pipe, an in-autoclave cooling bypass pipe, a reflux condenser, a thermocouple, and a bursting disc. The stirring speed was 400 rpm and the reaction was heated by circulating hot oil. The reaction steps are as follows:
[0069] 1) durene, acetic acid, cobalt acetate tetrahydrate, manganese acetate tetrahydrate, zirconium acetate, cerium acetate and hydrogen bromide are uniformly mixed to obtain a liquid raw material mixture, wherein the liquid raw material mixture contains 100 g of durene, 300 g of acetic acid, 500 ppmw of cobalt, 250 ppmw of manganese, 10 ppmw of Zr, 10 ppmw of Ce and 600 ppmw of bromine, and the liquid raw material mixture is added into an autoclave and sealed.
[0070] 2) Add 3.0MPa nitrogen and conduct an airtight test for 30 minutes. The test is qualified if the pressure drop is no more than 0.1MPa within 30 minutes.
[0071] 3) Add nitrogen, the air velocity is 6h -1 (Space velocity is the ratio of the volume of nitrogen to the volume of the liquid raw material mixture) and start the stirrer at a stirring rate of 400 rpm, raise the temperature to 110°C, and maintain the pressure at 2.0 MPa.
[0072] 4) Switch with air at 110℃, pressure of 2.0MPa, air volume velocity of 6h -1 (space velocity is the ratio of the volume flow rate of air to the volume of the liquid raw material mixture), the temperature was raised to 160°C at a heating rate of 2°C / min, and then the temperature was maintained at 160°C for 30 minutes to complete the first stage reaction.
[0073] 5) After the first stage is completed, the temperature is raised to 210°C in 10 minutes. At the same time, a 2.0 wt% aqueous solution of hydrogen bromide is added to the reactor at a flow rate of 10 g / min over 10 minutes. The reactor pressure is 2.0 MPa and the air volume space velocity is 6 h -1 (space velocity is the ratio of the volume flow rate of air to the volume of the liquid raw material mixture), continue the reaction at 210°C for 20 minutes, switch to nitrogen again after the temperature reaction is good, cool to room temperature, depressurize the reactor to normal pressure, add dimethyl sulfoxide to completely dissolve the oxidation product, and analyze the product by high performance liquid chromatography.
[0074] For ease of comparison, the main experimental conditions and experimental results are summarized in Table 1.
[0075] [Example 5]
[0076] The reaction was carried out in a 1000 ml titanium autoclave equipped with a magnetic stirrer, a gas delivery pipe, an in-autoclave cooling bypass pipe, a reflux condenser, a thermocouple, and a bursting disc. The stirring speed was 400 rpm and the reaction was heated by circulating hot oil. The reaction steps are as follows:
[0077] 1) durene, acetic acid, cobalt acetate tetrahydrate, manganese acetate tetrahydrate, zirconium acetate, cerium acetate and hydrogen bromide are uniformly mixed to obtain a liquid raw material mixture, wherein the liquid raw material mixture contains 100 g of durene, 300 g of acetic acid, 500 ppmw of cobalt, 250 ppmw of manganese, 10 ppmw of Zr, 10 ppmw of Ce and 600 ppmw of bromine, and the liquid raw material mixture is added into an autoclave and sealed.
[0078] 2) Add 3.0MPa nitrogen and conduct an airtight test for 30 minutes. The test is qualified if the pressure drop is no more than 0.1MPa within 30 minutes.
[0079] 3) Add nitrogen, the air velocity is 6h -1 (Space velocity is the ratio of the volume of nitrogen to the volume of the liquid raw material mixture) and start the stirrer at a stirring rate of 400 rpm, raise the temperature to 110°C, and maintain the pressure at 2.0 MPa.
[0080] 4) Switch with air at 110℃, pressure of 2.0MPa, air volume velocity of 6h -1 (space velocity is the ratio of the volume flow rate of air to the volume of the liquid raw material mixture), the temperature was raised to 175°C at a heating rate of 2°C / min, and then the temperature was maintained at 175°C for 30 minutes to complete the first stage reaction.
[0081] 5) After the first stage is completed, the temperature is raised to 210°C in 10 minutes. At the same time, a 2.0 wt% aqueous solution of hydrogen bromide is added to the reactor at a flow rate of 10 g / min over 10 minutes. The reactor pressure is 2.0 MPa and the air volume space velocity is 6 h -1 (space velocity is the ratio of the volume flow rate of air to the volume of the liquid raw material mixture), continue the reaction at 210°C for 20 minutes, switch to nitrogen again after the temperature reaction is good, cool to room temperature, depressurize the reactor to normal pressure, add dimethyl sulfoxide to completely dissolve the oxidation product, and analyze the product by high performance liquid chromatography.
[0082] For ease of comparison, the main experimental conditions and experimental results are summarized in Table 1.
[0083] [Example 6]
[0084] The reaction was carried out in a 1000 ml titanium autoclave equipped with a magnetic stirrer, a gas delivery pipe, an in-autoclave cooling bypass pipe, a reflux condenser, a thermocouple, and a bursting disc. The stirring speed was 400 rpm and the reaction was heated by circulating hot oil. The reaction steps are as follows:
[0085] 1) durene, acetic acid, cobalt acetate tetrahydrate, manganese acetate tetrahydrate, zirconium acetate, cerium acetate and hydrogen bromide are uniformly mixed to obtain a liquid raw material mixture, wherein the liquid raw material mixture contains 100 g of durene, 300 g of acetic acid, 500 ppmw of cobalt, 250 ppmw of manganese, 10 ppmw of Zr, 10 ppmw of Ce and 600 ppmw of bromine, and the liquid raw material mixture is added into an autoclave and sealed.
[0086] 2) Add 3.0MPa nitrogen and conduct an airtight test for 30 minutes. The test is qualified if the pressure drop is no more than 0.1MPa within 30 minutes.
[0087] 3) Add nitrogen, the air velocity is 6h -1 (Space velocity is the ratio of the volume of nitrogen to the volume of the liquid raw material mixture) and start the stirrer at a stirring rate of 400 rpm, raise the temperature to 110°C, and maintain the pressure at 2.0 MPa.
[0088] 4) Switch with air at 110℃, pressure of 2.0MPa, air volume velocity of 6h -1 (space velocity is the ratio of the volume flow rate of air to the volume of the liquid raw material mixture), the temperature is raised to 180°C at a heating rate of 2°C / min, and then the temperature is maintained at 180°C for 30 minutes to complete the first stage reaction.
[0089] 5) After the first stage is completed, the temperature is raised to 210°C in 10 minutes. At the same time, a 2.0 wt% aqueous solution of hydrogen bromide is added to the reactor at a flow rate of 10 g / min over 10 minutes. The reactor pressure is 2.0 MPa and the air volume space velocity is 6 h -1 (space velocity is the ratio of the volume flow rate of air to the volume of the liquid raw material mixture), continue the reaction at 210°C for 20 minutes, switch to nitrogen again after the temperature reaction is good, cool to room temperature, depressurize the reactor to normal pressure, add dimethyl sulfoxide to completely dissolve the oxidation product, and analyze the product by high performance liquid chromatography.
[0090] For ease of comparison, the main experimental conditions and experimental results are summarized in Table 1.
[0091] [Example 7]
[0092] The reaction was carried out in a 1000 ml titanium autoclave equipped with a magnetic stirrer, a gas delivery pipe, an in-autoclave cooling bypass pipe, a reflux condenser, a thermocouple, and a bursting disc. The stirring speed was 400 rpm and the reaction was heated by circulating hot oil. The reaction steps are as follows:
[0093] 1) durene, acetic acid, cobalt acetate tetrahydrate, manganese acetate tetrahydrate, zirconium acetate, cerium acetate and hydrogen bromide are uniformly mixed to obtain a liquid raw material mixture, wherein the liquid raw material mixture contains 100 g of durene, 300 g of acetic acid, 500 ppmw of cobalt, 250 ppmw of manganese, 10 ppmw of Zr, 10 ppmw of Ce and 600 ppmw of bromine, and the liquid raw material mixture is added into an autoclave and sealed.
[0094] 2) Add 3.0MPa nitrogen and conduct an airtight test for 30 minutes. The test is qualified if the pressure drop is no more than 0.1MPa within 30 minutes.
[0095] 3) Add nitrogen, the air velocity is 6h -1 (Space velocity is the ratio of the volume of nitrogen to the volume of the liquid raw material mixture) and start the stirrer at a stirring rate of 400 rpm, raise the temperature to 110°C, and maintain the pressure at 2.0 MPa.
[0096] 4) Switch with air at 110℃, pressure of 2.0MPa, air volume velocity of 6h -1 (space velocity is the ratio of the volume flow rate of air to the volume of the liquid raw material mixture), the temperature was raised to 170°C at a heating rate of 2°C / min, and then the temperature was maintained at 170°C for 30 minutes to complete the first stage reaction.
[0097] 5) After the first stage is completed, the temperature is raised to 210°C in 10 minutes. At the same time, a 1.0 wt% aqueous solution of hydrogen bromide is added to the reactor at a flow rate of 10 g / min over 10 minutes. The reactor pressure is 2.0 MPa and the air volume space velocity is 6 h -1 (space velocity is the ratio of the volume flow rate of air to the volume of the liquid raw material mixture), continue the reaction at 210°C for 20 minutes, switch to nitrogen again after the temperature reaction is good, cool to room temperature, depressurize the reactor to normal pressure, add dimethyl sulfoxide to completely dissolve the oxidation product, and analyze the product by high performance liquid chromatography.
[0098] For ease of comparison, the main experimental conditions and experimental results are summarized in Table 1.
[0099] [Example 8]
[0100] The reaction was carried out in a 1000 ml titanium autoclave equipped with a magnetic stirrer, a gas delivery pipe, an in-autoclave cooling bypass pipe, a reflux condenser, a thermocouple, and a bursting disc. The stirring speed was 400 rpm and the reaction was heated by circulating hot oil. The reaction steps are as follows:
[0101] 1) durene, acetic acid, cobalt acetate tetrahydrate, manganese acetate tetrahydrate, zirconium acetate, cerium acetate and hydrogen bromide are uniformly mixed to obtain a liquid raw material mixture, wherein the liquid raw material mixture contains 100 g of durene, 300 g of acetic acid, 500 ppmw of cobalt, 250 ppmw of manganese, 10 ppmw of Zr, 10 ppmw of Ce and 600 ppmw of bromine, and the liquid raw material mixture is added into an autoclave and sealed.
[0102] 2) Add 3.0MPa nitrogen and conduct an airtight test for 30 minutes. The test is qualified if the pressure drop is no more than 0.1MPa within 30 minutes.
[0103] 3) Add nitrogen, the air velocity is 6h -1 (Space velocity is the ratio of the volume of nitrogen to the volume of the liquid raw material mixture) and start the stirrer at a stirring rate of 400 rpm, raise the temperature to 110°C, and maintain the pressure at 2.0 MPa.
[0104] 4) Switch with air at 110℃, pressure of 2.0MPa, air volume velocity of 6h -1 (space velocity is the ratio of the volume flow rate of air to the volume of the liquid raw material mixture), the temperature was raised to 170°C at a heating rate of 2°C / min, and then the temperature was maintained at 170°C for 30 minutes to complete the first stage reaction.
[0105] 5) After the first stage is completed, the temperature is raised to 220°C in 10 minutes. At the same time, a 2.0 wt% aqueous solution of hydrogen bromide is added to the reactor at a flow rate of 10 g / min over 10 minutes. The reactor pressure is 2.0 MPa and the air volume space velocity is 6 h -1 (space velocity is the ratio of the volume flow rate of air to the volume of the liquid raw material mixture), continue the reaction at 220°C for 20 minutes, switch to nitrogen again after the temperature reaction is good, cool to room temperature, depressurize the reactor to normal pressure, add dimethyl sulfoxide to completely dissolve the oxidation product, and analyze the product by high performance liquid chromatography.
[0106] For ease of comparison, the main experimental conditions and experimental results are summarized in Table 1.
[0107] [Example 9]
[0108] The reaction was carried out in a 1000 ml titanium autoclave equipped with a magnetic stirrer, a gas delivery pipe, an in-autoclave cooling bypass pipe, a reflux condenser, a thermocouple, and a bursting disc. The stirring speed was 400 rpm and the reaction was heated by circulating hot oil. The reaction steps are as follows:
[0109] 1) durene, acetic acid, cobalt acetate tetrahydrate, manganese acetate tetrahydrate, zirconium acetate, cerium acetate and hydrogen bromide are uniformly mixed to obtain a liquid raw material mixture, wherein the liquid raw material mixture contains 100 g of durene, 300 g of acetic acid, 500 ppmw of cobalt, 250 ppmw of manganese, 10 ppmw of Zr, 10 ppmw of Ce and 600 ppmw of bromine, and the liquid raw material mixture is added into an autoclave and sealed.
[0110] 2) Add 3.0MPa nitrogen and conduct an airtight test for 30 minutes. The test is qualified if the pressure drop is no more than 0.1MPa within 30 minutes.
[0111] 3) Add nitrogen, the air velocity is 6h -1 (Space velocity is the ratio of the volume of nitrogen to the volume of the liquid raw material mixture) and start the stirrer at a stirring rate of 400 rpm, raise the temperature to 110°C, and maintain the pressure at 2.0 MPa.
[0112] 4) Switch with air at 110℃, pressure of 2.0MPa, air volume velocity of 6h -1 (space velocity is the ratio of the volume flow rate of air to the volume of the liquid raw material mixture), the temperature was raised to 170°C at a heating rate of 2°C / min, and then the temperature was maintained at 170°C for 30 minutes to complete the first stage reaction.
[0113] 5) After the first stage is completed, the temperature is raised to 230°C in 10 minutes. At the same time, a 2.0 wt% aqueous solution of hydrogen bromide is added to the reactor at a flow rate of 10 g / min over 10 minutes. The reactor pressure is 2.0 MPa and the air volume space velocity is 6 h -1 (space velocity is the ratio of the volume flow rate of air to the volume of the liquid raw material mixture), continue the reaction at 230°C for 20 minutes, switch to nitrogen again after the temperature reaction is good, cool to room temperature, depressurize the reactor to normal pressure, add dimethyl sulfoxide to completely dissolve the oxidation product, and analyze the product by high performance liquid chromatography.
[0114] For ease of comparison, the main experimental conditions and experimental results are summarized in Table 1.
[0115] [Example 10]
[0116] The reaction was carried out in a 1000 ml titanium autoclave equipped with a magnetic stirrer, a gas delivery pipe, an in-autoclave cooling bypass pipe, a reflux condenser, a thermocouple, and a bursting disc. The stirring speed was 400 rpm and the reaction was heated by circulating hot oil. The reaction steps are as follows:
[0117] 1) durene, acetic acid, cobalt acetate tetrahydrate, manganese acetate tetrahydrate, zirconium acetate, cerium acetate and hydrogen bromide are uniformly mixed to obtain a liquid raw material mixture, wherein the liquid raw material mixture contains 100 g of durene, 300 g of acetic acid, 500 ppmw of cobalt, 250 ppmw of manganese, 10 ppmw of Zr, 10 ppmw of Ce and 600 ppmw of bromine, and the liquid raw material mixture is added into an autoclave and sealed.
[0118] 2) Add 3.0MPa nitrogen and conduct an airtight test for 30 minutes. The test is qualified if the pressure drop is no more than 0.1MPa within 30 minutes.
[0119] 3) Add nitrogen, the air velocity is 6h -1 (Space velocity is the ratio of the volume of nitrogen to the volume of the liquid raw material mixture) and start the stirrer at a stirring rate of 400 rpm, raise the temperature to 110°C, and maintain the pressure at 2.0 MPa.
[0120] 4) Switch with air at 110℃, pressure of 2.0MPa, air volume velocity of 6h -1 (space velocity is the ratio of the volume flow rate of air to the volume of the liquid raw material mixture), the temperature was raised to 170°C at a heating rate of 2°C / min, and then the temperature was maintained at 170°C for 30 minutes to complete the first stage reaction.
[0121] 5) After the first stage is completed, the temperature is raised to 230°C in 10 minutes. At the same time, a 1.0 wt% aqueous solution of hydrogen bromide is added to the reactor at a flow rate of 10 g / min over 10 minutes. The reactor pressure is 2.0 MPa and the air volume space velocity is 6 h -1 (space velocity is the ratio of the volume flow rate of air to the volume of the liquid raw material mixture), continue the reaction at 230°C for 20 minutes, switch to nitrogen again after the temperature reaction is good, cool to room temperature, depressurize the reactor to normal pressure, add dimethyl sulfoxide to completely dissolve the oxidation product, and analyze the product by high performance liquid chromatography.
[0122] For ease of comparison, the main experimental conditions and experimental results are summarized in Table 1.
[0123] [Comparative Example 1]
[0124] The reaction was carried out in a 1000 ml titanium autoclave equipped with a magnetic stirrer, a gas delivery pipe, an in-autoclave cooling bypass pipe, a reflux condenser, a thermocouple, and a bursting disc. The stirring speed was 400 rpm and the reaction was heated by circulating hot oil. The reaction steps are as follows:
[0125] 1) durene, acetic acid, cobalt acetate tetrahydrate, manganese acetate tetrahydrate, zirconium acetate, cerium acetate and hydrogen bromide are uniformly mixed to obtain a liquid raw material mixture, wherein the liquid raw material mixture contains 100 g of durene, 300 g of acetic acid, 500 ppmw of cobalt, 250 ppmw of manganese, 10 ppmw of Zr, 10 ppmw of Ce and 600 ppmw of bromine, and the liquid raw material mixture is added into an autoclave and sealed.
[0126] 2) Add 3.0MPa nitrogen and conduct an airtight test for 30 minutes. The test is qualified if the pressure drop is no more than 0.1MPa within 30 minutes.
[0127] 3) Add nitrogen, the volume space velocity is 6h -1 (Space velocity is the ratio of nitrogen volume flow rate to the volume of liquid raw material mixture) and start the stirrer at a stirring rate of 400 rpm, raise the temperature to 110°C, and maintain the pressure at 2.0 MPa.
[0128] 4) Switch to air at 110℃, pressure 2.0MPa, air velocity 6h -1 (space velocity is the ratio of air volume flow rate to the volume of liquid raw material mixture), and the temperature is raised to 170°C at a heating rate of 1°C / min to complete the first stage reaction.
[0129] 5) After the first stage is completed, the temperature is raised to 210°C in 10 minutes. At the same time, a 2.0 wt% aqueous solution of hydrogen bromide is added to the reactor at a flow rate of 10 g / min over 10 minutes. The reactor pressure is 2.0 MPa and the air volume space velocity is 6 h -1 (space velocity is the ratio of the volume flow rate of air to the volume of the liquid raw material mixture), continue the reaction at 210°C for 20 minutes, switch to nitrogen again after the temperature reaction is good, cool to room temperature, depressurize the reactor to normal pressure, add dimethyl sulfoxide to completely dissolve the oxidation product, and analyze the product by high performance liquid chromatography.
[0130] For ease of comparison, the main experimental conditions and experimental results are summarized in Table 1.
[0131] [Comparative Example 2]
[0132] The reaction was carried out in a 1000 ml titanium autoclave equipped with a magnetic stirrer, a gas delivery pipe, an in-autoclave cooling bypass pipe, a reflux condenser, a thermocouple, and a bursting disc. The stirring speed was 400 rpm and the reaction was heated by circulating hot oil. The reaction steps are as follows:
[0133] 1) durene, acetic acid, cobalt acetate tetrahydrate, manganese acetate tetrahydrate, zirconium acetate, cerium acetate and hydrogen bromide are uniformly mixed to obtain a liquid raw material mixture, wherein the liquid raw material mixture contains 100 g of durene, 300 g of acetic acid, 500 ppmw of cobalt, 250 ppmw of manganese, 10 ppmw of Zr, 10 ppmw of Ce and 600 ppmw of bromine, and the liquid raw material mixture is added into an autoclave and sealed.
[0134] 2) Add 3.0MPa nitrogen and conduct an airtight test for 30 minutes. The test is qualified if the pressure drop is no more than 0.1MPa within 30 minutes.
[0135] 3) Add nitrogen, the air velocity is 6h -1 (Space velocity is the ratio of nitrogen volume flow rate to the volume of liquid raw material mixture) and start the stirrer at a stirring rate of 400 rpm, raise the temperature to 170°C, and maintain the pressure at 2.0 MPa.
[0136] 4) Switch to air at 170℃, pressure 2.0MPa, air velocity 6h -1 (Space velocity is the ratio of air volume flow rate to the volume of liquid raw material mixture), react for 60 minutes to complete the first stage reaction.
[0137] 5) After the first stage is completed, the temperature is raised to 210°C in 10 minutes. At the same time, a 2.0 wt% aqueous solution of hydrogen bromide is added to the reactor at a flow rate of 10 g / min over 10 minutes. The reactor pressure is 2.0 MPa and the air volume space velocity is 6 h -1 (space velocity is the ratio of the volume flow rate of air to the volume of the liquid raw material mixture), continue the reaction at 210°C for 20 minutes, switch to nitrogen again after the temperature reaction is good, cool to room temperature, depressurize the reactor to normal pressure, add dimethyl sulfoxide to completely dissolve the oxidation product, and analyze the product by high performance liquid chromatography.
[0138] For ease of comparison, the main experimental conditions and experimental results are summarized in Table 1.
[0139] It should be noted that the embodiments described above are only used to explain the present invention and do not constitute any limitation to the present invention. The present invention has been described with reference to typical embodiments, but it should be understood that the words used therein are descriptive and explanatory words, rather than restrictive words. The present invention may be modified as specified within the scope of the claims of the present invention, and the present invention may be revised without departing from the scope and spirit of the present invention. Although the present invention described therein relates to specific methods, materials and embodiments, it does not mean that the present invention is limited to the specific examples disclosed therein, on the contrary, the present invention can be extended to all other methods and applications with the same functions.
[0140] Table 1 (to be continued)
[0141]
[0142] Table 1 (continued)
[0143]
Claims
1. A method for producing pyromellitic acid by liquid phase oxidation of durenyl, comprising: First stage reaction The method comprises the following steps: in the presence of a catalyst and a solvent, an oxidant and durene are subjected to a liquid phase oxidation reaction to obtain an intermediate product mixture; the reaction temperature change of the first stage reaction sequentially comprises: a reaction temperature rising process from T11 to T12, and a reaction temperature maintaining process of maintaining T13, wherein T11 is 100-120° C., and T12 and T13 are independently 160-180° C.; the reaction temperature maintaining process of maintaining T13 in the first stage reaction lasts for 10-40 minutes; The catalyst contains Co salt, Mn salt, bromine-containing compound 1, Zr salt and rare earth salt; Second stage reaction The intermediate product mixture is used as a raw material, a mixture of bromine-containing compound 2 and pure water is added, and an oxidation reaction with an oxidant is continued to obtain pyromellitic acid. The reaction temperature T2 is 180-230°C, and the reaction time of the second stage reaction is 10-60 minutes.
2. The method according to claim 1, characterized in that The solvent includes acetic acid and / or water.
3. The method according to claim 1, characterized in that The oxidant is a gas containing oxygen.
4. The method according to claim 1, characterized in that The oxidant is air.
5. The method according to claim 1, characterized in that The heating rate from T11 to T12 is 1~3℃ / min.
6. The method according to claim 1, characterized in that In the first stage reaction, during the temperature increase process from T11 to T12, during the first stage reaction, during the temperature maintenance process of maintaining T13, and during the second stage reaction, the reaction pressure is independently 1.0 to 5.0 MPa.
7. The method according to claim 1, characterized in that The bromine-containing compound 1 and the bromine-containing compound 2 are independently selected from at least one of the substance group consisting of hydrogen bromide and tetrabromoethane.
8. The method according to claim 1, characterized in that The bromine content in the mixture of the bromine-containing compound 2 and pure water in the second stage is 0.5-2.5wt%; and / or the bromine-containing compound 2 is 0.01-1.0 times the mass of durene.
9. The method according to claim 1, characterized in that The catalyst comprises: Co salt, calculated as Co, is 300 to 1000 parts by weight; The Mn salt is 200 to 800 parts by weight, calculated as Mn; The bromine-containing compound 1 is 100 to 1000 parts by weight in terms of Br.
10. The method according to claim 1, characterized in that The catalyst comprises: Zr salt, calculated as Zr, in an amount of 2 to 50 parts by weight.
11. The method according to claim 1, characterized in that The catalyst comprises: the rare earth salt is calculated as rare earth element and is 2 to 50 parts by weight.
Citation Information
Patent Citations
Process for producing pyromellitic acid
JP2014152143A
Process for the production of an aromatic polycarboxylic acid
US5041633A
Process for producing aromatic polycarboxylic acid
US20110071314A1
Process for the production of aromatic polycarboxylic acids
US4719311A