A method for aqueous lanthanide and / or actinide extraction separation based on carboxyl-substituted o-phenanthroline imide ligands
By designing carboxyl-containing o-phenanthroline imide ligands, the problem of poor separation effect of water-soluble lanthanum-actinium separation ligands under high acidity was solved, achieving efficient separation of lanthanum-actinium and actinium-actinium, which has good prospects for industrial application.
Patent Information
- Application Number
- CN202310303581.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2023-03-27
- Publication Date
- 2026-06-23
- Estimated Expiration
- 2043-03-27
Smart Images

Figure CN116271974B_ABST
Abstract
Description
Technical Field
[0001] This invention relates to a method for the extraction and separation of lanthanide and / or actinide ions, belonging to the technical fields of nuclear fuel cycle and waste liquid treatment, rare earth element extraction, separation and purification. Background Technology
[0002] Nuclear energy is an important clean energy source, and its development is crucial for my country's energy conservation, emission reduction, and optimization of its energy structure. However, while the rapidly developing nuclear power industry brings economic benefits, the large accumulation and safe disposal of spent fuel from nuclear reactions has become a major issue that cannot be avoided in my country and even worldwide. In my country, as of 2020, the cumulative amount of spent fuel from the nuclear power industry had reached over 7,000 tons, and with the rapid development of my country's nuclear power industry, this figure is expected to exceed 14,000 tons by 2025. The main component of spent fuel is unreacted U (approximately 95%), along with 1% Pu and minor actinides (MAs, 0.1%) and other fission products; although minor actinides account for only 0.1% of spent fuel, they contribute a significant proportion of long-term radioactivity.
[0003] To reduce the radiation hazards of spent fuel, shorten the time it takes for radioactive nuclear waste to reach environmentally safe levels, and effectively reduce its geological storage costs, the "partitioning and transmutation" (P&T) strategy has been proposed since the last century. This strategy involves separating actinides and long-lived fission products from high-level radioactive waste to create targets, which are then converted into short-lived or stable nuclides through irradiation in a transmutation device. As the current dominant nuclear fuel recycling strategy, P&T can effectively reduce the radioactive hazards of long-lived minor actinides. However, its effectiveness is closely related to the separation of relevant elements, especially the separation of trivalent minor actinides (Am, Cm) and lanthanides (lanthanides have a large neutron absorption cross-section, thus reducing transmutation efficiency).
[0004] Separating trivalent actinides and lanthanides (hereinafter referred to as trivalent lanthanum-actinium separation) is extremely difficult because they have very similar physicochemical properties. Currently, there are two main ligand design approaches: 1) Designing lipophilic ligands with ion-selective and specific separation capabilities. This involves comprehensively considering factors such as the type of coordinating atoms (N, O, S, P, etc., single or combinations thereof), ligand skeleton rigidity, ligand coordination vacancy size, ligand solubility, and chemical and radiation resistance during molecular design. Forward extractants for the organic phase are then designed and synthesized to extract and separate lanthanum-actinium ions from highly acidic ionic mixtures. 2) Designing water-soluble ligands with ion-selective and specific separation capabilities. Industrially mature non-selective lipophilic ligands (such as TODGA) are selected for the organic phase, while selective aqueous masking agents are designed and synthesized to achieve the extraction and separation of lanthanum-actinium ions. The second design approach can effectively reduce the use of toxic organic phases and diluents in liquid-liquid extraction, thus having greater application prospects. However, since the ligand design needs to further consider the water / acid solubility of the molecule on the basis of the requirements of the first ligand design, it is more challenging in molecular design, and the practical systems studied and reported are very limited.
[0005] Currently, the main water-soluble ligands studied in the literature are N- (or N, O)-containing heterocyclic aromatic ligands substituted with sulfonic acid groups (Solvent Extr. Ion Exch. 2012, 30, 433-444; Chem. Sci. 2015, 6, 4812-4821; Inorg. Chem. 2021, 60, 357-365). However, the introduction of sulfonic acid groups requires harsh synthesis conditions (requiring large amounts of fuming sulfuric acid) and the presence of sulfur atoms in the sulfonic acid base itself can cause secondary pollution (not in accordance with the CHON principle). In 2016, Macerata et al. reported the hydroxyl-modified triazole-pyridine derivative molecule PyTri. At an acidity of 0.25 M HNO3 and an organic phase of 0.2 M TODGA (soluble in kerosene containing 5% n-octanol), PyTri can achieve back-extraction of almost all minor actinides, with a separation factor reaching 144 (J. Am. Chem. Soc. 2016, 138, 7232-7235). Although PyTri can achieve good separation of lanthanum and actinides, it lacks intra-actinide differentiation capability (separation of Am and Cm). Based on this, Webling (Inorg. Chem. 2022, 61, 17719-17729) and Edwards (Chem. Commun. 2017, 53, 5001-5004) reported the synthesis of hydroxyl-modified triazole-bipyridine and o-phenanthroline molecules (EtOH-BPTD and BTrzPhen), respectively. The change in the number of coordination sites and the introduction of pre-organized structures further improved the intra-system segregation ability of the ligands (SF of BTrzPhen). Cm / Am(2.5). Compared to lipophilic ligands, research on water-soluble ligands is still in its early stages: reported ligand structures are relatively simple (sulfonic acid groups or hydroxyl derivatives), lacking the construction of structure-property relationships. Ligand synthesis often requires stringent conditions or reagents (e.g., fuming sulfuric acid is needed for sulfonic acid group introduction; hydroxyl groups are mostly introduced through click chemistry reactions of azides). Meanwhile, most water-soluble ligands are currently suitable for acidities below 1 M. With increasing acidity, the shift in coordination equilibrium and protonation of the ligands lead to a rapid decrease in separation efficiency. Summary of the Invention
[0006] This invention addresses the key technical and scientific problems of poor acid resistance of lanthanum-actinium separation ligands and the limited variety and insufficient development of water-soluble lanthanum-actinium separation ligands. It proposes a class of carboxyl-containing o-phenanthroline imide ligands capable of achieving efficient separation between and within lanthanum-actinium systems under high acidity. The evolution of each system during solution complexation was determined using UV-Vis absorption, high-resolution mass spectrometry, and NMR titration experiments. The mechanism of efficient ligand separation was investigated using infrared spectroscopy and single-crystal analysis, and the single-crystal structure elucidated the reason for high acidity tolerance. The ligands designed in this invention are characterized by simple structure, ease of large-scale preparation, acid resistance, and good separation effect.
[0007] The main technical solutions adopted in this invention are:
[0008] This invention addresses the main problems of water-soluble lanthanum-actinium separation ligands, including their simple structures, demanding synthetic conditions, limited available functional groups, lack of structure-activity relationship-guided molecular design, and poor acid tolerance of existing ligands. For the first time, a class of carboxyl-containing o-phenanthroline imide ligands is proposed and revealed, capable of effectively separating lanthanum-actinium and actinium-actinium under high acidity. Compared with reported ligand types in the literature, the new ligands are characterized by easy synthesis and purification, high acid tolerance, and the ability to simultaneously separate lanthanum-actinium and actinium-actinium, as discussed in detail below:
[0009] The general formula of the ligand molecule is as follows:
[0010]
[0011] Where n = 1, 3, 5.
[0012] The ligands contain both an ONNO tetradentate o-phenanthroline coordination cavity and soluble side chains with carboxyl-terminal groups of varying alkyl lengths. Taking a C4 side chain with n=3 as an example: the ligand has poor solubility in water, but solubility increases with increasing acidity. In HNO3 solutions above 1.25 M, the maximum solubility of the ligand can reach 5 mM, meeting the requirements for extraction experiments. Ligand solubility can be further adjusted and optimized by modifying the alkyl chain; for example, the solubility of a C2 side chain ligand in a 1.25 M HNO3 solution can reach 15 mM. Alkyl chain length is detrimental to the solubility of the ligand in acid.
[0013] Carboxyl-substituted o-phenanthroline imide ligands, represented by formula (1), act as aqueous masking agents, working in conjunction with the organic phase of a non-selective extractant to extract and separate trivalent lanthanides and / or actinides from high-acidity solutions. The ligands exhibit excellent extraction kinetics; the solution complexation system study shows a dominant 1:1 system, and the single-crystal structure of the complex is a dual-center metal-dual-ligand structure—the first such crystal configuration observed in lanthanum-actinide separation. This structure ensures the ligands' excellent extraction performance and acidity tolerance.
[0014] The trivalent lanthanide ions described in this invention include one or more combinations of La(III), Ce(III), Pr(III), Nd(III), Pm(III), Sm(III), Eu(III), Gd(III), Tb(III), Dy(III), Ho(III), Er(III), Tm(III), Yb(III), Lu(III), Y(III), and Sc(III);
[0015] The trivalent actinide ions of the present invention include one or more combinations of Ac(III), Th(III), Pa(III), U(III), Np(III), Pu(III), Am(III), Cm(III), Bk(III), Cf(III), Es(III), Fm(III), Md(III), No(III) and Lr(III);
[0016] Preferably, the trivalent lanthanide ions include one or more combinations of La(III), Nd(III), Eu(III) and Lu(III);
[0017] Preferably, the trivalent actinide ions include Am(III) and / or Cm(III);
[0018] More preferably, the trivalent actinide ion includes Am(III) and / or Cm(III); the trivalent lanthanide ion is Eu(III);
[0019] Preferably, the alkyl chain lengths in the ligand structure (1) are C2, C4 and C6, respectively;
[0020] Further preferred are the extraction and separation performance of ligands (1) containing C4 chain length;
[0021] Preferably, the organic phase extractant is one or a combination of several types of aromatic / aliphatic phospholipid ligands, aromatic / aliphatic imide ligands, and aromatic / aliphatic sulfur-containing ligands;
[0022] Further preferably, the organic phase extractant is 0.05M 2,2′-oxydi(N,N-dioctylacetamide), TODGA;
[0023] Preferably, the organic phase diluent is one or a mixture of several of the following: aromatics (3-nitrotrifluorotoluene, nitrobenzene, chlorobenzene, di / trichlorobenzene, etc.), alkanes (kerosene, n-hexane, etc.) and heteroatom-containing diluents (chlorinated / fluorinated solvents, cyclic ketones, etc.);
[0024] A further preferred option is n-dodecane as the organic phase diluent;
[0025] Preferably, the acidic solution is a nitric acid solution with a concentration of 1-5M. In the treatment of high-level radioactive waste in the nuclear industry, the solutions are often strong acid solutions (>3M). The ligand described in this invention has poor solubility at low acidity, but excellent solubility and extraction performance at high acidity. However, the extraction performance decreases when the acidity is too high.
[0026] Preferably, the acidic solution is a nitric acid solution with a concentration of 1-3M;
[0027] Preferably, the aqueous phase of the extraction process is an acid solution of different concentrations containing 1-5 mM ligands, and NaNO3 is added to control the total nitrate content at 3 M.
[0028] To supplement the above conditions, for example, 1.5M NaNO3 needs to be added to 1.5M HNO3; NaNO3 does not need to be added to 3M HNO3; further preferred, the optimal extraction performance conditions are 1.5M HNO3 and 1.5M NaNO3.
[0029] The preferred extraction time is 1s-0.5h. Due to the pre-organized cavitation configuration of the ligand (1) skeleton, the extraction kinetics are faster, and the extraction process quickly reaches equilibrium. Under other conditions described in this invention, the extraction time is fixed at 0.5h to ensure sufficient equilibrium between the oil and water phases.
[0030] The extraction methods described in this invention are all carried out at room temperature, specifically 25±1℃. At this temperature, the extraction effect is good, and the extraction process requires no heating or cooling, thus consuming no other energy.
[0031] In the extraction experiments described in this invention, the volume ratio of the oil and water phases is 1:1.
[0032] Compared with the prior art, the present invention has the following advantages:
[0033] The ligands used in this invention are simple in structure, easy to synthesize and purify, and readily mass-produced without requiring complex operations or toxic reagents, thus possessing excellent industrial potential. The ligands exhibit excellent separation selectivity for Am(III), with Eu(III) / Am(III) and Cm(III) / Am(III) separation factors reaching 120 and 4.4, respectively, in a 1.5M HNO3 solution (containing 1.5M NaNO3). Solution complexation behavior studies show that the extraction system mainly generates a 1:1 complex system, and the single-crystal structure indicates that ligand (1) and Eu(III) can form a unique dimer coordination mode, which may explain the ligand's high acid tolerance and high selectivity. Combining these characteristics, the ligand structure and extraction method involved in this invention not only have significant academic value but also strong practicality. Attached Figure Description
[0034] Figure 1 The proton NMR spectrum of the C2-substituted ligand (1) prepared for Example 1.
[0035] Figure 2 The proton NMR spectrum of C4-substituted ligand (1) prepared for Example 2.
[0036] Figure 3 The proton NMR spectrum of C6-substituted ligand (1) prepared for Example 3.
[0037] Figure 4 The partition ratio and separation coefficient of Eu(III) and Am(III) extracted under different nitric acid concentrations are given.
[0038] Figure 5 The partition ratio and separation coefficient of Cm(III) and Am(III) extracted with nitric acid at a concentration of 1.5 M are given.
[0039] Figure 6 It is a single crystal structure of a dimer formed by ligand (1) and Eu(III). Detailed Implementation Plan
[0040] The specific implementation schemes described in this invention are merely illustrative examples used to illustrate the invention's purpose, technical solutions, and advantages. These examples are for explanation only and are not intended to limit the invention. Any modifications or equivalent substitutions made based on this invention, that do not fundamentally depart from its essential content and technical characteristics, should be included within the scope of protection of this invention.
[0041] Example 1:
[0042] Synthesis of C2-modified ligand (1): 11.5 g (25 mM) of bis(2,5-dioxopyrrolino-1-yl) ester of 2,9-benzodicarboxylic acid was dissolved in 100 ml of DMSO. 4.7 g of glycine (62.5 mM, 2.5 equivalents) and 0.5 ml of triethylamine were added sequentially as catalysts. The mixture was stirred at room temperature for 12 hours, and water was added to precipitate the product. The product was collected by filtration and dried under vacuum to give 7.1 g of white crystalline product (yield 75%). 1 H NMR(600MHz,DMSO-d6)δ12.80(s,broad,2H),9.63(t,J=5.9Hz,2H),8.77(d,J=8 .2Hz,2H),8.47(d,J=8.2Hz,2H),8.21(s,2H),4.15(d,J=12Hz,4H),2.50(m,2H).
[0043] Example 2:
[0044] Synthesis of C4-modified ligand (1): 11.5 g (25 mM) of bis(2,5-dioxopyrrolino-1-yl) ester of 2,9-benzodicarboxylic acid was dissolved in 100 ml of DMSO. 6.4 g of 4-aminobutyric acid (62.5 mM, 2.5 equivalents) and 0.5 ml of triethylamine were added sequentially as catalysts. The mixture was stirred at room temperature for 12 hours, and then water was added to precipitate the product. The product was collected by filtration and dried under vacuum to give 9.3 g of white crystalline product (yield 85%). 1 H NMR(600MHz,DMSO-d6)δ12.08(s,broad,2H),9.44(t,J=5.9Hz,2H),8.73(d,J=8.2Hz,2H),8.45( d,J=8.2Hz,2H),8.18(s,2H),3.50(q,J=6.7Hz,4H),2.38(t,J=7.2Hz,4H),1.92(p,J=7.1Hz,4H).
[0045] Example 3:
[0046] Synthesis of C6-modified ligand (1): 11.5 g (25 mM) of bis(2,5-dioxopyrrolino-1-yl) 2,9-benzodicarboxylic acid was dissolved in 100 ml of DMSO. 8.2 g of 6-aminobutyric acid (62.5 mM, 2.5 equivalents) and 0.5 ml of triethylamine were added sequentially as catalysts. The mixture was stirred at room temperature for 12 hours, and then water was added to precipitate the product. The product was collected by filtration and dried under vacuum to give 11 g of white crystalline product (yield 89%). 1HNMR(600MHz,DMSO-d6)δ11.97(s,broad,2H),9.41(t,J=5.9Hz,2H),8.73(d,J=8.2Hz,2H),8.45(d,J =8.2Hz,2H),8.18(s,2H),3.45(m,4H),2.23(t,J=7.2Hz,4H),1.67(m,4H),1.57(m,4H),1.40(m,4H).
[0047] Example 4:
[0048] Preparation of the organic phase: A 0.05 M TODGA solution in n-dodecane was prepared as the organic phase;
[0049] Preparation of the aqueous phase: The ligand molecules from Example 2 were prepared into a 5 mM nitric acid solution with nitric acid concentrations of 1, 1.5, 2.0, 2.5, and 3.0 M. NaNO3 was added to the solution to maintain the total nitrate ion concentration at 3 M. Subsequently, an equal amount of a tracer-containing radionuclide was added to the solution. 241 Am(III) and 152,154 Eu(III);
[0050] Determination of partition ratio and separation coefficient of Eu(III) and Am(III) extracted under different nitric acid concentrations: 0.5 mL of each extract containing... 241 Am(III) and 152,154 An aqueous solution of Eu(III) with 5 mM ligand in HNO3 / NaNO3 (3 M total nitrate concentration) was used as the aqueous phase, and an equal volume of n-dodecane solution containing 0.05 M TODGA was used as the organic phase. The two phases were mixed and shaken thoroughly for 30 minutes in a homogenizer. The mixture was then centrifuged at 3000 rpm for 2 minutes. 100 mL of the aqueous phase solution was placed in a scintillation flask, and the concentrations of the aqueous phase before and after extraction were analyzed. 241 Am(III) and 152,154 The emission count of Eu(III) was used to calculate the extraction partition ratio D (the ratio of organic phase ion concentration to aqueous phase ion concentration at equilibrium) and the separation factor SF (SF0) after conversion to ion concentration. Eu(III) / Am(III) D Eu(III) / D Am(III) );
[0051] Example 5:
[0052] Preparation of the organic phase: A 0.05 M TODGA solution in n-dodecane was prepared as the organic phase;
[0053] Preparation of the aqueous phase: The ligand molecules from Example 2 were prepared into a 5 mM nitric acid solution with nitric acid concentrations of 1, 1.5, 2.0, 2.5, and 3.0 M. NaNO3 was added to the solution to maintain the total nitrate ion concentration at 3 M. Subsequently, an equal amount of a tracer-containing radionuclide was added to the solution. 241 Am(III) and 244 Cm(III);
[0054] Determination of the partition ratio and separation coefficient of Cm(III) and Am(III) extracted with nitric acid at a concentration of 1.5 M: 0.5 mL of each extract containing... 241 Am(III) and 152,154 An aqueous solution of Eu(III) with 5 mM ligands in HNO3 / NaNO3 (1.5 M / 1.5 M) was used as the aqueous phase, and an equal volume of n-dodecane solution containing 0.05 M TODGA was used as the organic phase. The two phases were mixed and shaken thoroughly for 30 minutes in a homogenizer. The mixture was then centrifuged at 3000 rpm for 2 minutes. 100 mL of the aqueous phase was placed in a scintillation flask, and the concentrations of the aqueous phase before and after extraction were analyzed. 241 Am(III) and 244 The emission count of Cm(III) was used to calculate the extraction partition ratio D (the ratio of organic phase ion concentration to aqueous phase ion concentration at equilibrium) and the separation factor SF (SF0) after conversion to ion concentration. Cm(III) / Am(III) D Cm(III) / D Am(III) );
[0055] The interaction mechanism between ligand (1) and Eu(III) was determined: The binding mode between the carboxyl-containing ligand and Eu(III) ions involved in this invention was determined by single-crystal structure analysis. Equimolar amounts of ligand (1) and Eu(NO3)36H2O were dissolved in methanol. Isopropanol was slowly added to the solution, and the system was allowed to stand for 2 days. Block crystals were collected, and the crystals exhibited the characteristic red fluorescence of Eu(III) under ultraviolet light. The single-crystal structure was then analyzed.
Claims
1. A carboxyl-substituted o-phenanthroline imide water-soluble ligand for the extraction and separation of lanthanides and actinides or actinides and actinides in aqueous phase, characterized in that, Using a carboxyl-substituted o-phenanthroline imide water-soluble ligand as shown in formula (1) as an aqueous phase masking agent, in conjunction with the alkyl amide-containing non-selective organic phase extractant TODGA, Eu(III) and Am(III) are extracted and separated from 1.5-3 M HNO3, or Cm(III) and Am(III) are extracted and separated from 1.5 M HNO3. Formula (1) is shown below: ; Where n = 1, n = 3, or n = 5.
2. The carboxyl-substituted o-phenanthroline imide water-soluble ligand according to claim 1 is used for the extraction and separation of lanthanides and actinides or actinides and actinides in aqueous phase, characterized in that, The organic phase diluent is n-dodecane.
3. The carboxyl-substituted o-phenanthroline imide water-soluble ligand according to claim 1 is used for the extraction and separation of lanthanides and actinides or actinides and actinides in aqueous phase, characterized in that, The concentration of the carboxyl-substituted o-phenanthroline imide water-soluble ligand was 5 mM, and the volume ratio of the aqueous phase to the organic phase was 1.