A high-quality pentaerythritol oleate and its preparation method and application

By combining pentaerythritol oleate with graphene oxide, graphene-modified pentaerythritol oleate is formed, which solves the problems of insufficient low-temperature fluidity and anti-wear and friction-reducing properties, and realizes the application of efficient and environmentally friendly lubricants.

CN118165777BActive Publication Date: 2024-11-15CANGZHOU ZHONGKE GREASE CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410290921.X
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-03-14
Publication Date
2024-11-15
Estimated Expiration
2044-03-14

AI Technical Summary

Technical Problem

Existing pentaerythritol oleate has poor low-temperature fluidity and insufficient anti-wear and friction-reducing properties, resulting in high lubricant costs and potential environmental pollution.

Method used

After esterification with pentaerythritol, graphene oxide and triethylamine are added to form graphene-modified pentaerythritol oleate, which improves fluidity and lubricity through hydrogen bonding and double bond structure.

Benefits of technology

It significantly improves the low-temperature fluidity and anti-wear and friction-reducing properties of pentaerythritol oleate, reduces lubricant costs and environmental pollution, and has excellent flame retardant properties.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118165777B_ABST
    Figure CN118165777B_ABST
Patent Text Reader

Abstract

The present invention relates to the technical field of preparation of chemical products, and in particular to a high-quality pentaerythritol oleate and a preparation method and application thereof. After pentaerythritol and oleic acid are mixed in a molar ratio of 1:3, a catalyst and a solvent are added to carry out an esterification reaction to obtain pentaerythritol trioleate; graphene oxide and a promoter triethylamine are added to the obtained pentaerythritol trioleate to obtain graphene-modified pentaerythritol oleate; the graphene-modified pentaerythritol oleate is cooled to room temperature, washed with water, the organic layer is vacuum-desolventized, and dried to obtain the final product. The present invention adopts the above-mentioned high-quality pentaerythritol oleate and a preparation method and application thereof, solves the problems of poor low-temperature fluidity and anti-wear and anti-friction performance of pentaerythritol oleate in the prior art, and greatly reduces the cost of preparing lubricating oil.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of preparation of chemical products, and in particular to high-quality pentaerythritol oleate and a preparation method and application thereof. Background Art

[0002] Pentaerythritol oleate has excellent lubrication performance, good flame retardancy, low volatility, biodegradation rate greater than 90%, and pour point -32°C. High-quality products can be used as base oil for synthetic ester-type flame-resistant hydraulic oil and base oil for aviation engine lubricants.

[0003] Low-temperature fluidity is an important property of lubricating oil, which is expressed by pour point. Pour point refers to the lowest temperature at which a cooled sample of oil can flow under specified test conditions. Oils with high pour points are not suitable for use in cold areas. However, pentaerythritol oleate in the prior art has the problem of poor low-temperature fluidity, and its anti-wear and friction-reducing properties need to be improved. When pentaerythritol oleate is used in lubricating oil, a large amount of additives to increase lubricity need to be added, which greatly increases the cost of the lubricating oil. In addition, the added additives often contain pollutants such as sulfur, phosphorus, chlorine, and metal salts, etc. These additives are easy to decompose and cause environmental pollution. Summary of the invention

[0004] The purpose of the present invention is to provide a high-quality pentaerythritol oleate and a preparation method and application thereof, so as to solve the problems of poor low-temperature fluidity and anti-wear and anti-friction performance of pentaerythritol oleate in the prior art and greatly reduce the cost of preparing lubricating oil.

[0005] To achieve the above object, the present invention provides a method for preparing high-quality pentaerythritol oleate, comprising the following steps:

[0006] S1: mixing pentaerythritol and oleic acid in a molar ratio of 1:3, adding a catalyst and a solvent, and performing an esterification reaction to obtain pentaerythritol trioleate;

[0007] S2 adding graphene oxide and a promoter, triethylamine, to the pentaerythritol trioleate obtained in S1 to obtain graphene-modified pentaerythritol trioleate;

[0008] S3: Cooling the graphene-modified pentaerythritol oleate to room temperature, washing with water, removing the solvent from the organic layer in vacuo, and drying to obtain the final product, i.e., high-quality pentaerythritol oleate.

[0009] Preferably, in S1, the catalyst is p-toluenesulfonic acid and the solvent is petroleum ether.

[0010] Preferably, the amount of the catalyst in S1 is 6-8‰ of the mass of pentaerythritol.

[0011] Preferably, the reaction temperature of the S1 esterification reaction is 100-160° C., and the reaction time is 3-8 hours.

[0012] Preferably, the reaction temperature of S2 is 70-110° C., and the reaction time is 2-6 hours.

[0013] Preferably, the mass ratio of pentaerythritol trioleate, graphene oxide and promoter triethylamine in S2 is 5:1:5.

[0014] A method for preparing high-quality pentaerythritol oleate to obtain graphene-modified pentaerythritol oleate.

[0015] The invention discloses an application of graphene-modified pentaerythritol oleate, which is applied to fire-resistant hydraulic oil or engine lubricating oil.

[0016] Mechanism of the present invention:

[0017] Pentaerythritol trioleate contains three long carbon chain oleic acid groups to ensure high viscosity, high viscosity index and high biodegradability. The hydroxyl groups in pentaerythritol trioleate form a large number of hydrogen bonds with the oxygen-containing groups of graphene oxide, so that pentaerythritol trioleate is tightly combined with graphene oxide. Graphene oxide contains a large number of double bond structures, which increases the number of double bonds per unit mass of pentaerythritol oleate, thereby reducing the pour point and improving the low-temperature fluidity of pentaerythritol oleate. In addition, graphene itself has excellent lubricity, which further improves the anti-wear and friction-reducing properties of pentaerythritol trioleate, and is green and pollution-free.

[0018] Beneficial effects of the present invention:

[0019] (1) The synthesis method of the present invention does not use highly toxic and highly corrosive raw materials and toxic and harmful organic solvents, and has the advantages of high safety and environmental protection.

[0020] (2) The graphene-modified pentaerythritol oleate prepared by the present invention has good low-temperature fluidity and good anti-wear and friction-reducing properties. When used in lubricating oil, it can greatly reduce the use of lubricating additives, greatly reduce the cost of lubricating oil, and reduce pollution to the environment.

[0021] (3) The graphene-modified pentaerythritol oleate prepared by the invention also has excellent flame retardant properties. Graphene forms a dense carbon layer during the combustion process, thereby inhibiting the penetration of oxygen and the conduction of heat. Therefore, when it is applied to fire-resistant hydraulic oil, the flame retardant properties of the fire-resistant hydraulic oil can be significantly improved.

[0022] The technical solution of the present invention is further described in detail below through the accompanying drawings and embodiments. BRIEF DESCRIPTION OF THE DRAWINGS

[0023] Figure 1The present invention is a flow chart of a method for preparing high-quality pentaerythritol oleate. DETAILED DESCRIPTION

[0024] The present invention is further described below in conjunction with the accompanying drawings and embodiments. Unless otherwise defined, the technical terms or scientific terms used in the present invention should be the common meanings understood by people with ordinary skills in the field to which the present invention belongs. The above-mentioned features or features mentioned in the specific examples mentioned in the present invention can be combined arbitrarily, and these specific embodiments are only used to illustrate the present invention and are not used to limit the scope of the present invention.

[0025] Example 1

[0026] Figure 1 The flowchart of the method for preparing high-quality pentaerythritol oleate of the present invention is shown in the figure. The present invention provides a method for preparing high-quality pentaerythritol oleate, which comprises the following steps:

[0027] S1: After pentaerythritol and oleic acid are mixed in a molar ratio of 1:3, p-toluenesulfonic acid and petroleum ether are added, and the amount of p-toluenesulfonic acid added is 6% of the mass of pentaerythritol, and then an esterification reaction is carried out at a temperature of 100° C. After reacting for 8 hours, pentaerythritol trioleate is obtained;

[0028] S2: adding graphene oxide and promoter triethylamine to the pentaerythritol trioleate obtained in S1, wherein the mass ratio of pentaerythritol trioleate, graphene oxide and promoter triethylamine is 5:1:5, and then reacting at a temperature of 70° C. for 6 hours to obtain graphene-modified pentaerythritol oleate;

[0029] S3: Cooling the graphene-modified pentaerythritol oleate to room temperature, washing with water, removing the solvent from the organic layer in vacuo, and drying to obtain the final product, i.e., high-quality pentaerythritol oleate.

[0030] Example 2

[0031] The present invention provides a method for preparing high-quality pentaerythritol oleate, comprising the following steps:

[0032] S1: After pentaerythritol and oleic acid are mixed in a molar ratio of 1:3, p-toluenesulfonic acid and petroleum ether are added, and the amount of p-toluenesulfonic acid added is 7% of the mass of pentaerythritol, and then an esterification reaction is carried out at a temperature of 100° C. After reacting for 8 hours, pentaerythritol trioleate is obtained;

[0033] S2: adding graphene oxide and promoter triethylamine to the pentaerythritol trioleate obtained in S1, wherein the mass ratio of pentaerythritol trioleate, graphene oxide and promoter triethylamine is 5:1:5, and then reacting at a temperature of 70° C. for 6 hours to obtain graphene-modified pentaerythritol oleate;

[0034] S3: Cooling the graphene-modified pentaerythritol oleate to room temperature, washing with water, removing the solvent from the organic layer in vacuo, and drying to obtain the final product, i.e., high-quality pentaerythritol oleate.

[0035] Example 3

[0036] The present invention provides a method for preparing high-quality pentaerythritol oleate, comprising the following steps:

[0037] S1: After pentaerythritol and oleic acid are mixed in a molar ratio of 1:3, p-toluenesulfonic acid and petroleum ether are added, and the amount of p-toluenesulfonic acid added is 8% of the mass of pentaerythritol, and then an esterification reaction is carried out at a temperature of 100° C. After reacting for 8 hours, pentaerythritol trioleate is obtained;

[0038] S2: adding graphene oxide and promoter triethylamine to the pentaerythritol trioleate obtained in S1, wherein the mass ratio of pentaerythritol trioleate, graphene oxide and promoter triethylamine is 5:1:5, and then reacting at a temperature of 70° C. for 2 hours to obtain graphene-modified pentaerythritol oleate;

[0039] S3: Cooling the graphene-modified pentaerythritol oleate to room temperature, washing with water, removing the solvent from the organic layer in vacuo, and drying to obtain the final product, i.e., high-quality pentaerythritol oleate.

[0040] Example 4

[0041] The present invention provides a method for preparing high-quality pentaerythritol oleate, comprising the following steps:

[0042] S1: After pentaerythritol and oleic acid are mixed in a molar ratio of 1:3, p-toluenesulfonic acid and petroleum ether are added, and the amount of p-toluenesulfonic acid added is 6% of the mass of pentaerythritol, and then an esterification reaction is carried out at a temperature of 110° C. After reacting for 7 hours, pentaerythritol trioleate is obtained;

[0043] S2: adding graphene oxide and promoter triethylamine to the pentaerythritol trioleate obtained in S1, wherein the mass ratio of pentaerythritol trioleate, graphene oxide and promoter triethylamine is 5:1:5, and then reacting at a temperature of 80° C. for 5 hours to obtain graphene-modified pentaerythritol oleate;

[0044] S3: Cooling the graphene-modified pentaerythritol oleate to room temperature, washing with water, removing the solvent from the organic layer in vacuo, and drying to obtain the final product, i.e., high-quality pentaerythritol oleate.

[0045] Example 5

[0046] The present invention provides a method for preparing high-quality pentaerythritol oleate, comprising the following steps:

[0047] S1: After pentaerythritol and oleic acid are mixed in a molar ratio of 1:3, p-toluenesulfonic acid and petroleum ether are added, and the amount of p-toluenesulfonic acid added is 6% of the mass of pentaerythritol, and then an esterification reaction is carried out at a temperature of 120° C. After reacting for 6 hours, pentaerythritol trioleate is obtained;

[0048] S2: adding graphene oxide and promoter triethylamine to the pentaerythritol trioleate obtained in S1, wherein the mass ratio of pentaerythritol trioleate, graphene oxide and promoter triethylamine is 5:1:5, and then reacting at a temperature of 90° C. for 4 hours to obtain graphene-modified pentaerythritol oleate;

[0049] S3: Cooling the graphene-modified pentaerythritol oleate to room temperature, washing with water, removing the solvent from the organic layer in vacuo, and drying to obtain the final product, i.e., high-quality pentaerythritol oleate.

[0050] Example 6

[0051] The present invention provides a method for preparing high-quality pentaerythritol oleate, comprising the following steps:

[0052] S1: pentaerythritol and oleic acid are mixed in a molar ratio of 1:3, p-toluenesulfonic acid and petroleum ether are added, and the amount of p-toluenesulfonic acid added is 6% of the mass of pentaerythritol, and then an esterification reaction is carried out at a temperature of 140° C. After reacting for 4 hours, pentaerythritol trioleate is obtained;

[0053] S2: adding graphene oxide and promoter triethylamine to the pentaerythritol trioleate obtained in S1, wherein the mass ratio of pentaerythritol trioleate, graphene oxide and promoter triethylamine is 5:1:5, and then reacting at a temperature of 100° C. for 4 hours to obtain graphene-modified pentaerythritol oleate;

[0054] S3: Cooling the graphene-modified pentaerythritol oleate to room temperature, washing with water, removing the solvent from the organic layer in vacuo, and drying to obtain the final product, i.e., high-quality pentaerythritol oleate.

[0055] Example 7

[0056] The present invention provides a method for preparing high-quality pentaerythritol oleate, comprising the following steps:

[0057] S1: After pentaerythritol and oleic acid are mixed in a molar ratio of 1:3, p-toluenesulfonic acid and petroleum ether are added, and the amount of p-toluenesulfonic acid added is 6% of the mass of pentaerythritol, and then an esterification reaction is carried out at a temperature of 160° C. After reacting for 3 hours, pentaerythritol trioleate is obtained;

[0058] S2: adding graphene oxide and promoter triethylamine to the pentaerythritol trioleate obtained in S1, wherein the mass ratio of pentaerythritol trioleate, graphene oxide and promoter triethylamine is 5:1:5, and then reacting at a temperature of 110° C. for 2 hours to obtain graphene-modified pentaerythritol oleate;

[0059] S3: Cooling the graphene-modified pentaerythritol oleate to room temperature, washing with water, removing the solvent from the organic layer in vacuo, and drying to obtain the final product, i.e., high-quality pentaerythritol oleate.

[0060] Comparative Example 1

[0061] A method for preparing pentaerythritol tetraoleate comprises the following steps:

[0062] S1: After pentaerythritol and oleic acid are mixed in a molar ratio of 1:4, p-toluenesulfonic acid and petroleum ether are added, and the amount of p-toluenesulfonic acid added is 6% of the mass of pentaerythritol. Then, an esterification reaction is carried out at a temperature of 160° C. After reacting for 3 hours, pentaerythritol tetraoleate is obtained.

[0063] The pentaerythritol oleate prepared in Examples 1-7 and Comparative Example 1 was tested for CCS@-35 low temperature apparent viscosity and pour point using ASTM D5293 and ASTM D97 respectively, and its friction coefficient was tested using SRV-IV friction and wear tester. The tribological test conditions were load 50N, frequency 50Hz, temperature 50℃, and time 30min. The results are shown in Table 1.

[0064] Table 1 Test data of pentaerythritol oleate obtained in Examples 1-7 and Comparative Example 1

[0065]

[0066]

[0067] It can be seen from Table 1 that the graphene-modified pentaerythritol oleate prepared in the present invention has a lower pour point, good fluidity at low temperatures, and also has good anti-wear and friction-reducing properties.

[0068] Finally, it should be noted that the above embodiments are only used to illustrate the technical solution of the present invention rather than to limit it. Although the present invention has been described in detail with reference to the preferred embodiments, those skilled in the art should understand that they can still modify or replace the technical solution of the present invention with equivalents, and these modifications or equivalent replacements cannot cause the modified technical solution to deviate from the spirit and scope of the technical solution of the present invention.

Claims

1. A method for preparing high-quality pentaerythritol oleate, characterized in that: The following steps are included: S1: mixing pentaerythritol and oleic acid in a molar ratio of 1:3, adding a catalyst and a solvent, and performing an esterification reaction to obtain pentaerythritol trioleate; S2: adding graphene oxide and promoter triethylamine to the pentaerythritol trioleate obtained in S1 to obtain graphene-modified pentaerythritol oleate; the mass ratio of pentaerythritol trioleate, graphene oxide and promoter triethylamine is 5:1:5; S3: Cooling the graphene-modified pentaerythritol oleate to room temperature, washing with water, removing the solvent from the organic layer in vacuo, and drying to obtain the final product, i.e., high-quality pentaerythritol oleate.

2. The method for preparing high-quality pentaerythritol oleate according to claim 1, characterized in that: In S1, the catalyst is p-toluenesulfonic acid and the solvent is petroleum ether.

3. The method for preparing high-quality pentaerythritol oleate according to claim 1, characterized in that: The amount of catalyst used in S1 is 6-8‰ of the mass of pentaerythritol.

4. The method for preparing high-quality pentaerythritol oleate according to claim 1, characterized in that: The reaction temperature of the S1 esterification reaction is 100 to 160° C., and the reaction time is 3 to 8 hours.

5. The method for preparing high-quality pentaerythritol oleate according to claim 1, characterized in that: The reaction temperature of S2 is 70 to 110° C., and the reaction time is 2 to 6 hours.

6. A graphene-modified pentaerythritol oleate obtained by the method for preparing high-quality pentaerythritol oleate according to any one of claims 1 to 5.

7. An application of a graphene-modified pentaerythritol oleate as claimed in claim 6, characterized in that: Used in fire-resistant hydraulic oils or engine lubricants.