Novel low-temperature-resistant fluorite collecting agent and preparation method thereof

By adding low-temperature resistant additives and other auxiliary agents to the fluorite collector, the preparation process is optimized, and the problem of insufficient capture capacity of oleic acid in low-temperature environment is solved, and a more efficient fluorite harvesting effect and purity are achieved. Reduced flotation costs.

CN118904549AInactive Publication Date: 2024-11-08HENAN PROVINCIAL ROCK & MINERAL TESTING CENT
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411274631.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-12
Publication Date
2024-11-08
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

During the existing fluorite flotation process, oleic acid, as a collector, exhibits insufficient capture capacity, large consumption, poor low temperature resistance and weak foaming properties in low temperature environments, resulting in winter flotation costs in northern regions. Increase.

Method used

Using a new low-temperature fluorite collector, including oleic acid, deionized water or purified water, low-temperature aid, synergist, stabilizer and foaming agent, multiple flotation tests in the preparation method, The steps of stirring, filtration, high-temperature fractionation, freezing crystallization and low-temperature separation are optimized to optimize the ratio and component reaction of oleic acid to additives, and improve the low-temperature resistance and purity of the collector.

Benefits of technology

It significantly improves the capture effect of fluorite collector in low temperature environments, avoids heating operations, saves energy, and improves the capture capacity and purity by enhancing bubbles and stability, reducing flotation costs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118904549A_ABST
    Figure CN118904549A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of fluorite collecting agents, in particular to a novel low-temperature-resistant fluorite collecting agent and a preparation method thereof.The novel low-temperature-resistant fluorite collecting agent comprises 30%-50% of oleic acid, 5%-50% of deionized water or purified water, 5%-50% of low-temperature-resistant auxiliaries, 5%-20% of synergist, 5%-20% of stabilizer and 5%-20% of foaming agent; the proportion of the low-temperature-resistant auxiliary agent is 10%-20%. The low-temperature-resistant fluorite collecting agent has the advantages that the low-temperature-resistant additive is added on the basis of the fluorite collecting agent, and the low-temperature-resistant capability of the fluorite collecting agent can be greatly enhanced through the low-temperature-resistant additive, so that the fluorite collecting agent can well collect minerals in a low-temperature environment; the fluorite collecting agent has the beneficial effects that the fluorite collecting agent is good in collecting effect in the low-temperature environment, the situation that ore pulp is heated is avoided, energy is saved, foaming of the fluorite collecting agent in the low-temperature environment is enhanced through the foaming agent, and the agent stability of the fluorite collecting agent in the low-temperature environment is enhanced through the stabilizing agent.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of fluorite collectors, in particular to a novel low-temperature resistant fluorite collector and a preparation method thereof. Background Art

[0002] Fluorite is a strategic non-metallic mineral resource with a wide range of uses. It can be used in metallurgy, chemistry, refrigeration and building materials industries. my country is one of the countries with the richest fluorite resources in the world, but with the rapid exploitation and consumption of resources, single fluorite is rapidly depleted, and the mining of semi-raw fluorite mines is becoming more and more important. However, the grade of such fluorite mines is generally low, and the grade of fluorite in the raw ore is generally only 18-35%. Therefore, the difficulty of fluorite mining is gradually increasing.

[0003] The flotation process of fluorite mostly uses oleic acid as a collector, soda ash as a regulator, and water glass as an inhibitor. When the flotation process is carried out at room temperature (about 25°C), the collection performance of oleic acid can meet the flotation requirements. However, when the ambient temperature is lower than 20°C, using oleic acid as a collector will expose great problems, such as insufficient collection capacity, large consumption, poor low temperature resistance and weak foaming due to factors such as poor water solubility and dispersibility. Especially in the winter in northern regions, the temperature is relatively low, and the temperature of the flotation pulp after grinding is generally lower than 15°C. The situation will only improve when the flotation pulp is heated to about 20°C. The heating operation will inevitably cause a large amount of energy consumption, which will greatly increase the flotation cost. Therefore, a new low-temperature resistant fluorite collector and a preparation method thereof are needed to solve the above problems. Summary of the invention

[0004] In view of the deficiencies in the prior art, the present invention provides a novel low-temperature resistant fluorite collector and a preparation method thereof, which has the advantages of low-temperature resistance and the like, and solves the problems existing in the prior art.

[0005] To achieve the above-mentioned purpose, the present invention provides the following technical scheme: a novel low-temperature resistant fluorite collector, comprising oleic acid, deionized water or purified water, a low-temperature resistant auxiliary agent, a synergist, a stabilizer and a foaming agent, wherein the proportion of the oleic acid is 30%-50%, the proportion of the deionized water or purified water is 5%-50%, the proportion of the low-temperature resistant auxiliary agent is 10%-20%, the proportion of the synergist is 5%-15%, the proportion of the stabilizer is 4%-7%, and the proportion of the foaming agent is 1%-3%.

[0006] Preferably, the low temperature resistant additive is ethylene glycol or ethylene glycol ethyl ether.

[0007] Preferably, the synergist is sodium dodecylbenzene sulfonate.

[0008] Preferably, the stabilizer is ethylene oxide-propylene oxide copolymer.

[0009] A method for preparing a novel low-temperature resistant fluorite collector comprises the following steps: 1) Choose different oils to prepare different types of oleic acid; 2) Through two flotation tests, different types of oleic acid were compared and screened, and several oleic acids with good flotation test results were selected; 3) Mix the selected oleic acids with deionized water or purified water in a certain proportion, heat to 40-50°C, and stir until completely dissolved to obtain a basic solution; 4) Slowly add the low-temperature resistant additive to several basic solutions respectively, and continue stirring to make the low-temperature resistant additive and the basic solution evenly mixed; 5) Add synergist and stabilizer to the several basic solutions after adding low temperature resistant additives, and heat the solution to 60-70°C, maintain stirring speed, and react for 2-3 hours to ensure that each component is fully reacted and evenly dispersed to obtain several mixed solutions; 6) Add the foaming agent to the mixed solutions respectively, and continue the stirring operation at a constant stirring speed to make the foaming agent and the mixed solutions evenly mixed; 7) Cooling the several mixed solutions after mixing with the foaming agent to room temperature respectively, and filtering to remove impurities in the mixed solutions; 8) Perform high-temperature fractionation operation on the several mixed solutions after filtration; 9) Perform freezing crystallization operations on the several mixed solutions after high-temperature distillation; 10) The several solutions after freezing and crystallization are subjected to low temperature separation operation respectively, thereby obtaining several fluorite collectors; 11) Several fluorite collectors were subjected to flotation tests again and screened to obtain the best low-temperature resistant fluorite collector.

[0010] The temperature of the high temperature fractionation in step 8 is 350°C-360°C.

[0011] The temperature of the freezing crystallization in step 9 is 8°C-10°C, and the temperature of the low-temperature separation in step 10 is 5°C-7°C.

[0012] Compared with the prior art, the present invention provides a novel low-temperature resistant fluorite collector and a preparation method thereof, which has the following beneficial effects: 1. The novel low-temperature resistant fluorite collector and its preparation method are characterized by adding a low-temperature resistant auxiliary agent to the fluorite collector. The low-temperature resistant auxiliary agent can greatly enhance the low-temperature resistance of the fluorite collector, so that the fluorite collector can better capture minerals in a low-temperature environment, and the fluorite collector has a better collection effect in a low-temperature environment, avoiding the situation of heating the ore pulp, saving energy, and enhancing the foaming of the fluorite collector in a low-temperature environment through a foaming agent, and enhancing the agent stability of the fluorite collector in a low-temperature environment through a stabilizer. The synergist can adjust the chemical characteristics of the fluorite collector, such as foaming ability and surface tension, thereby improving the adsorption ability and stability of the collector on the fluorite surface, thereby better improving the collection ability of the fluorite collector.

[0013] 2. The novel low-temperature-resistant fluorite collector and its preparation method can understand the capture capabilities of different oleic acids by preparing and comparing a variety of oleic acids, and after mixing oleic acid with deionized water or purified water, add a low-temperature-resistant auxiliary agent, a synergist, a stabilizer and a foaming agent and perform a stirring operation to make the mixing between the materials more uniform, and perform filtering, high-temperature fractionation, freeze crystallization and low-temperature separation operations on the mixed solution to remove impurities in the fluorite collector, so that the purity of the fluorite collector is higher, and further the collection effect of the fluorite collector is better. BRIEF DESCRIPTION OF THE DRAWINGS

[0014] Figure 1 It is a schematic diagram of the process of the preparation method of the present invention. DETAILED DESCRIPTION

[0015] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0016] See also Figure 1 A new type of low-temperature resistant fluorite collector includes oleic acid, deionized water or purified water, a low-temperature resistant auxiliary agent, a synergist, a stabilizer and a foaming agent. The proportion of oleic acid is 30%-50%, the proportion of deionized water or purified water is 5%-50%, the proportion of low-temperature resistant auxiliary agent is 10%-20%, the proportion of synergist is 5%-15%, the proportion of stabilizer is 4%-7%, and the proportion of foaming agent is 1%-3%.

[0017] Preferably, the low temperature resistant additive is one of ethylene glycol or ethylene glycol ether, and ethylene glycol is an organic solvent with low freezing point and high boiling point, and has good solubility and stability. Adding an appropriate amount of ethylene glycol to the fluorite collector can effectively reduce the freezing point of the fluorite collector and improve its fluidity at low temperatures. The low temperature resistant additive can enable the fluorite collector to maintain effective flotation performance at a lower temperature without heating the slurry, thereby saving energy and reducing environmental pollution.

[0018] Preferably, the synergist is sodium dodecylbenzene sulfonate. The synergist can adjust the chemical characteristics of the fluorite collector, such as foaming ability and surface tension, thereby improving the adsorption capacity and stability of the collector on the fluorite surface. The synergist can also promote the conversion of the fluorite collector from single-layer adsorption to multi-layer adsorption on the fluorite surface, increase the adsorption amount, and strengthen the adsorption effect at low temperatures. The synergist can improve the recovery rate.

[0019] Preferably, the stabilizer is an ethylene oxide-propylene oxide copolymer, and the stabilizer can be selected from inorganic salt compounds such as sodium chloride and sodium sulfate. The stabilizer can enhance the stability of the collector in the slurry and prevent it from failing or decomposing due to physical or chemical factors, thereby ensuring the continuity and stability of the flotation process. The stabilizer can adjust the physical and chemical conditions such as the pH value and ionic strength of the slurry to create a more favorable environment for the adsorption of the collector on the fluorite surface.

[0020] A method for preparing a novel low-temperature resistant fluorite collector comprises the following steps: 1) Choose different oils to prepare different types of oleic acid; There are 24 types of oils used, including vegetable oils (such as soybean oil, rapeseed oil, olive oil, etc.), animal fats (such as lard, tallow, etc.) and some industrial-grade oils; 2) Through two flotation tests, different types of oleic acid were compared and screened, and several oleic acids with good flotation test results were selected; In the process of flotation test of oleic acid, oleic acid is adsorbed on the surface of minerals through physical and chemical effects to form a hydrophobic film, so that mineral particles can adhere to bubbles and rise to the water surface with bubbles, so as to achieve separation from gangue minerals. The flotation test of oleic acid includes four steps. Step 1 is to select representative mineral samples, and obtain slurry that meets flotation requirements after pretreatment steps such as crushing and grinding. Step 2 is to prepare flotation reagents such as oleic acid and other collectors, frothers, and regulators according to a certain proportion. Step 3 is to add the slurry to the flotation machine, adjust the parameters such as slurry concentration and pH value, and then add the flotation reagent. Under the action of stirring and aeration, the mineral particles are fully contacted with the bubbles and attached to the bubbles. Subsequently, the bubbles carry the mineral particles and rise to the water surface to form a foam layer. The foam layer is scraped out and collected by a scraping device. Step 4 is to filter and dry the collected foam layer to obtain the final flotation product, and then select several oleic acids with a large content of mineral particles in the flotation product by comparing and screening multiple flotation products. 3) Mix the selected oleic acids with deionized water or purified water in a certain proportion, heat to 40-50°C, and stir until completely dissolved to obtain a basic solution; By using deionized water or purified water as a solvent, the purity and stability after mixing with oleic acid can be improved; 4) Slowly add the low-temperature resistant additive to several basic solutions respectively, and continue stirring to make the low-temperature resistant additive and the basic solution evenly mixed; 5) Add synergist and stabilizer to the several basic solutions after adding low temperature resistant additives, and heat the solution to 60-70°C, maintain stirring speed, and react for 2-3 hours to ensure that each component is fully reacted and evenly dispersed to obtain several mixed solutions; 6) Add the foaming agent to the mixed solutions respectively, and continue the stirring operation at a constant stirring speed to make the foaming agent and the mixed solutions evenly mixed; 7) Cooling the several mixed solutions after mixing with the foaming agent to room temperature respectively, and filtering to remove impurities in the mixed solutions; Before adding the foaming agent, ensure that other conditions of the mixed solution (such as pH value, concentration, stirring intensity, etc.) have been adjusted to an appropriate range so that the foaming agent can fully exert its effect. At the same time, it should be added gradually and stirred fully during the addition process to avoid the situation where the local concentration of the foaming agent is too high or too low; 8) Perform high-temperature fractionation operation on the several mixed solutions after filtration; It is used to purify raw materials such as oleic acid and remove impurities through high-temperature fractionation; 9) Perform freezing crystallization operations on the several mixed solutions after high-temperature distillation; Freeze crystallization is an important step for further purification of raw materials such as oleic acid, and affects the physical and chemical properties of the product by controlling the temperature. The oleic acid fraction obtained by high-temperature distillation is cooled at low temperatures so that the high-melting point fatty acids therein first form crystals and precipitate, thereby removing high-melting point impurities. 10) The several solutions after freezing and crystallization are subjected to low temperature separation operation respectively, thereby obtaining several fluorite collectors; The low-temperature separation operation further crystallizes or solidifies the low-freezing-point oleic acid of the oleic acid species and removes impurities with low freezing points; 11) Conduct flotation tests on several fluorite collectors again and screen them to obtain the best low-temperature resistant fluorite collector; When screening, filtration or centrifugation can be used.

[0021] The temperature of the freezing crystallization in step 9 is 8°C-10°C, and the temperature of the low-temperature separation in step 10 is 5°C-7°C.

[0022] The temperature of freezing crystallization in step 9 is 8°C-10°C, and the temperature of low-temperature separation in step 10 is 5°C-7°C. In summary, the new low-temperature resistant fluorite collector and its preparation method, by adding a low-temperature resistant auxiliary agent to the fluorite collector, can greatly enhance the low-temperature resistance of the fluorite collector through the low-temperature resistant auxiliary agent, so that the fluorite collector can better capture minerals in a low-temperature environment, so that the fluorite collector has a better collection effect in a low-temperature environment, avoids the situation of heating the ore pulp, saves energy, and enhances the foaming of the fluorite collector in a low-temperature environment through a foaming agent, and enhances the stability of the fluorite collector in a low-temperature environment through a stabilizer. The synergist can adjust the chemical characteristics of the fluorite collector, such as the foaming ability. and surface tension, thereby improving the adsorption capacity and stability of the collector on the fluorite surface, thereby being able to better improve the collection capacity of the fluorite collector, by preparing a variety of oleic acids and comparing them, the collection capacity of different oleic acids can be understood, and after the oleic acid is mixed with deionized water or purified water, a low-temperature resistant auxiliary agent, a synergist, a stabilizer and a foaming agent are added and stirred to make the mixing between the materials more uniform, and the mixed solution is filtered, high-temperature fractionated, frozen crystallized and low-temperature separated to remove impurities in the fluorite collector, so that the purity of the fluorite collector is higher, and further the collection effect of the fluorite collector is better.

[0023] It should be noted that, in this article, relational terms such as first and second, etc. are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprise" or any other variants thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or device. In the absence of further restrictions, the elements defined by the statement "comprise one" do not exclude the existence of other identical elements in the process, method, article or device including the elements.

[0024] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.

Claims

1. A novel low-temperature resistant fluorite collector, characterized in that: The invention comprises oleic acid, deionized water or purified water, a low-temperature resistant auxiliary agent, a synergist, a stabilizer and a foaming agent, wherein the proportion of the oleic acid is 30%-50%, the proportion of the deionized water or purified water is 5%-50%, the proportion of the low-temperature resistant auxiliary agent is 10%-20%, the proportion of the synergist is 5%-15%, the proportion of the stabilizer is 4%-7%, and the proportion of the foaming agent is 1%-3%.

2. A novel low-temperature resistant fluorite collector according to claim 1, characterized in that: The low temperature resistant auxiliary agent is one of ethylene glycol or ethylene glycol ethyl ether.

3. A novel low-temperature resistant fluorite collector according to claim 2, characterized in that: The synergist is sodium dodecylbenzene sulfonate.

4. A novel low-temperature resistant fluorite collector according to claim 3, characterized in that: The stabilizer is ethylene oxide-propylene oxide copolymer.

5. A method for preparing a novel low-temperature resistant fluorite collector, applied to a novel low-temperature resistant fluorite collector according to any one of claims 1 to 4, characterized in that: The following steps are included: 1) Choose different oils to prepare different types of oleic acid; 2) Through two flotation tests, different types of oleic acid were compared and screened, and several oleic acids with good flotation test results were selected; 3) Mix the selected oleic acids with deionized water or purified water in a certain proportion, heat to 40-50°C, and stir until completely dissolved to obtain a basic solution; 4) Slowly add the low-temperature resistant additive to several basic solutions respectively, and continue stirring to make the low-temperature resistant additive and the basic solution evenly mixed; 5) Add synergist and stabilizer to the several basic solutions after adding low temperature resistant additives, and heat the solution to 60-70°C, maintain stirring speed, and react for 2-3 hours to ensure that each component is fully reacted and evenly dispersed to obtain several mixed solutions; 6) Add the foaming agent to the mixed solutions respectively, and continue the stirring operation at a constant stirring speed to make the foaming agent and the mixed solutions evenly mixed; 7) Cooling the several mixed solutions after mixing with the foaming agent to room temperature respectively, and filtering to remove impurities in the mixed solutions; 8) Perform high-temperature fractionation operation on the several mixed solutions after filtration; 9) Perform freezing crystallization operations on the several mixed solutions after high-temperature distillation; 10) The several solutions after freezing and crystallization are subjected to low temperature separation operation respectively, thereby obtaining several fluorite collectors; 11) Several fluorite collectors were subjected to flotation tests again and screened to obtain the best low-temperature resistant fluorite collector.

6. The method for preparing a novel low-temperature resistant fluorite collector according to claim 5, characterized in that: The temperature of the high temperature fractionation in step 8 is 350°C-360°C.

7. The method for preparing a novel low-temperature resistant fluorite collector according to claim 6, characterized in that: The temperature of the freezing crystallization in step 9 is 8°C-10°C, and the temperature of the low-temperature separation in step 10 is 5°C-7°C.