High-reflection monocrystalline silicon alkali polishing additive, alkali polishing liquid, preparation method and application
By using highly reflective single-crystal silicon alkaline-polishing additives, including silicone ether-based protective agents and lithium-containing compound polishing agents in alkali sprinklers, the problem of poor polishing effect of alkali sprinklers is solved, high selective corrosion is achieved, and the improvement of The reflectivity of single crystal silicon wafers and the conversion efficiency of solar cells.
Patent Information
- Application Number
- CN202411396525.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-10-09
- Publication Date
- 2024-11-08
- Estimated Expiration
- 2044-10-09
AI Technical Summary
The existing alkali sprinkler has poor polishing effect on the surface of single crystal silicon wafers, resulting in low reflectivity and affecting the conversion efficiency of solar cells.
Highly reflective single-crystal silicon alkali-polishing additives, including silicone ether-based protective agents, lithium-containing compound polishing agents, surfactants and corrosion inhibitors, can achieve high selective corrosion and improve the surface of the silicon wafer by forming a protective film and uniform polishing agent distribution. Roughness and reflectivity.
It significantly improves the polishing effect of single crystal silicon wafers, protects the surface of the silicon wafer, extends the service life of alkali sprinklers, and enhances the conversion efficiency of solar cells.
Smart Images

Figure CN118909552A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to an alkali polishing technology, and in particular to a high-reflection single-crystal silicon alkali polishing additive, an alkali polishing liquid, and a preparation method and use thereof. Background Art
[0002] With the continuous development of solar cell technology, the surface quality and performance requirements of monocrystalline silicon wafers are increasing. Alkali polishing of monocrystalline silicon wafers is one of the key steps in the manufacturing process of solar cells, which directly affects the surface flatness, reflectivity and conversion efficiency of the final cell. The purpose of the alkali polishing process is to remove defects and contaminants on the surface of the silicon wafer so that the surface of the silicon wafer reaches a certain flatness and micro-roughness, which is conducive to the production of cells and electron migration. The alkali polishing process usually uses sodium hydroxide or potassium hydroxide as the processing liquid to control the roughness of different silicon wafers. In the alkali polishing process, due to the polarity and concentration of the reactants, non-uniform corrosion often occurs. At this time, it is necessary to add some chemical additives to make the reaction liquid evenly distributed on the surface of the silicon wafer, so as to obtain a uniform surface roughness.
[0003] During the alkaline polishing process, additives can form a certain dispersion system, control the viscosity and surface tension of the reaction liquid, and reduce surface defects and non-uniform corrosion. In addition, additives can also form a protective film to protect the surface of the silicon wafer from excessive corrosion, thereby achieving precise control of the surface roughness of the silicon wafer. Another function of the alkaline polishing additive is to improve the interaction between the reaction liquid and the surface of the silicon wafer, so that the desired microstructure is formed on the surface of the silicon wafer. By adjusting the concentration and pH of substances such as sodium hydroxide or potassium hydroxide, the purpose of adjusting the reaction speed on the surface of the silicon wafer is achieved, thereby improving the conversion efficiency of the silicon wafer. Therefore, the research and development of high-reflectivity single-crystal silicon alkaline polishing additives is of great significance for improving the performance of solar cells. Summary of the invention
[0004] The purpose of the present invention is to propose a high-reflectivity single-crystal silicon alkali polishing additive to address the problem that the polishing effect of the current alkali polishing solution needs to be improved. Adding the alkali polishing additive to the alkali polishing solution can improve the polishing effect of the silicon wafer, achieve highly selective corrosion, and ultimately obtain a single-crystal silicon wafer with a highly reflective back-polished surface, thereby improving the conversion efficiency of the solar cell.
[0005] To achieve the above object, the technical solution adopted by the present invention is: a high-reflection single-crystal silicon alkali polishing additive, comprising the following components in parts by weight: 1-2 parts of protective agent; 1-5 parts of polishing agent; Surfactant 0.1-1 part; Corrosion inhibitor 0.5-2 parts; 60-80 parts of deionized water; The protective agent is a silicon ether compound; The polishing agent is a lithium-containing compound.
[0006] Furthermore, the protective agent is one or more of tert-butyldimethylsilyl glycidyl ether, tert-butyldimethylallylsilyl ether and 1,3-bis(aminopropyl)tetramethyldisiloxane.
[0007] Furthermore, the protective agent is preferably tert-butyldimethylsilyl glycidyl ether.
[0008] Furthermore, the protective agent is 1.5-2 parts.
[0009] The protective agent in the high-reflective single-crystal silicon alkaline polishing additive of the present invention is a silicon ether compound, the silyl group contained in which can chemically react with the hydroxyl group (-OH) or other active groups on the silicon surface to form a protective film on the surface of the silicon wafer, thereby reducing damage to the silicon wafer surface during the polishing process and protecting the PN junction on the front side of the silicon wafer from being destroyed.
[0010] Furthermore, the polishing agent is one or more of lithium methacrylate, lithium hexafluorophosphate and isopropylmagnesium chloride-lithium chloride.
[0011] Furthermore, the polishing agent is preferably lithium methacrylate.
[0012] Furthermore, the polishing agent is 3-5 parts.
[0013] The polishing agent in the high-reflection single-crystal silicon alkali polishing additive of the present invention relies on the isotropy of lattice atoms to polish the textured pyramid flat, and at the same time removes the back and surrounding borosilicate glass in the boron diffusion. At the same time, the protective agent and the polishing agent work synergistically. On the one hand, the silyl ether compound reacts with the lithium compound to generate silanol (Si-OH) or silane (Si-H), which can form silicon oxygen bonds with silicon atoms on the surface of the silicon wafer, thereby enhancing the hydrophilicity and wettability of the silicon wafer surface. On the other hand, due to the presence of the protective film, the polishing agent can polish the surface of the silicon wafer more evenly and smoothly, which helps to improve the polishing efficiency and quality.
[0014] Furthermore, the surfactant is one or more of dodecyl glucoside, decyl glucoside, glucopyranoside and o-nitrophenyl-β-D-galactopyranoside.
[0015] Furthermore, the surfactant is preferably glucopyranoside.
[0016] Furthermore, the surfactant is 0.1-0.5 parts.
[0017] The surfactant in the high-reflective single-crystal silicon alkali polishing additive of the present invention can reduce the contact angle between the polishing liquid and the silicon wafer surface, making it easier for the polishing liquid to penetrate into the microstructure of the silicon wafer surface, thereby more effectively removing surface defects and pollutants and making the entire surface more uniform.
[0018] Furthermore, the corrosion inhibitor is one or more of polyglutamic acid, polylysine, m-hydroxybenzoic acid and p-hydroxybenzoic acid.
[0019] Furthermore, the corrosion inhibitor is preferably polyglutamic acid.
[0020] Furthermore, the corrosion inhibitor is 0.5-1 part.
[0021] The corrosion inhibitor in the high-reflection single-crystal silicon alkali polishing additive of the present invention can control the reaction rate in the alkali polishing process, reduce the amount of alkali used in the reaction process, and extend the service life of the alkali polishing solution.
[0022] Another object of the present invention is to disclose a method for preparing a highly reflective single-crystal silicon alkali polishing additive, comprising the following steps: At room temperature, a protective agent, a polishing agent, a surfactant and a corrosion inhibitor are added to deionized water in sequence, and the mixture is stirred until completely dissolved and then stirred for 1-2 hours to obtain a high-reflectivity single-crystal silicon alkali polishing additive.
[0023] Another object of the present invention is to disclose the use of a high-reflective single-crystal silicon alkali polishing additive in the field of alkali polishing liquid.
[0024] Another object of the present invention is to disclose an alkali polishing solution, comprising the highly reflective single crystal silicon alkali polishing additive, alkali and deionized water.
[0025] Furthermore, the mass ratio of the high-reflection single-crystal silicon alkali polishing additive, alkali and deionized water in the alkali polishing solution is 0.3-1:0.75-1.5:100.
[0026] Furthermore, the mass ratio of the high-reflective single-crystal silicon alkali polishing additive, alkali and deionized water in the alkali polishing solution is preferably 0.3-0.5:0.75-1:100.
[0027] Furthermore, the mass ratio of the high-reflective single-crystal silicon alkali polishing additive, alkali and deionized water in the alkali polishing solution is more preferably 0.3:1:100.
[0028] Furthermore, the alkali is sodium hydroxide and / or potassium hydroxide.
[0029] Another object of the present invention is to disclose a method for preparing an alkali polishing solution, comprising the following steps: adding a high-reflection single-crystal silicon alkali polishing additive and an alkali into deionized water and stirring and mixing them uniformly to prepare the alkali polishing solution.
[0030] Furthermore, the temperature of the deionized water is 60-65°C.
[0031] Furthermore, the temperature of the deionized water is preferably 62°C.
[0032] Another object of the present invention is to disclose the use of an alkaline polishing liquid in the field of silicon wafer polishing.
[0033] Further, the method of polishing a silicon wafer using the alkaline polishing solution is as follows: S1: Use pre-cleaning liquid to pre-clean the silicon wafer before polishing; S2: Soak the pre-cleaned silicon wafer in deionized water for 80-120 seconds, take it out and polish it in an alkaline polishing solution, the polishing time is 190 seconds-240 seconds, and the polishing temperature is 60°C-65°C.
[0034] Furthermore, the pre-cleaning solution in S1 includes alkali, hydrogen peroxide and deionized water.
[0035] Furthermore, the mass ratio of alkali, hydrogen peroxide and deionized water in the pre-cleaning solution in S1 is 0.2-0.5:0.3-1.5:100.
[0036] Furthermore, the mass ratio of alkali, hydrogen peroxide and deionized water in the pre-cleaning solution is preferably 0.2:0.5:100.
[0037] Furthermore, the base in S1 is sodium hydroxide and / or potassium hydroxide.
[0038] Furthermore, the pre-cleaning time in S1 is 110s-250s, and the pre-cleaning temperature is 60°C-63°C.
[0039] Furthermore, the pre-cleaning time in S1 is preferably 190 seconds, and the pre-cleaning temperature is preferably 61°C.
[0040] Further, in S2, the pre-cleaned silicon wafer is immersed in deionized water for 100 seconds.
[0041] Furthermore, the polishing time in S2 is preferably 200 s, and the polishing temperature is preferably 62°C.
[0042] The high-reflective single-crystal silicon alkali polishing additive, alkali polishing solution, preparation method and use of the present invention have the following advantages compared with the prior art: 1) The protective agent in the high-reflection single-crystal silicon alkaline polishing additive of the present invention is a silane ether compound, in which the silyl group contained can react chemically with the hydroxyl group (-OH) or other active groups on the silicon surface to form a protective film on the surface of the silicon wafer, thereby reducing the damage to the silicon wafer surface during the polishing process and protecting the PN junction on the front of the silicon wafer from being destroyed; the polishing agent relies on the isotropy of the lattice atoms to polish the velvet pyramid flat, and at the same time removes the back and surrounding borosilicate glass in the boron diffusion. At the same time, the protective agent and the polishing agent work synergistically. On the one hand, the silane ether compound reacts with the lithium compound to form silanol (Si-OH) or silane (Si-H), which can form silicon oxygen bonds with the silicon atoms on the surface of the silicon wafer, thereby enhancing the hydrophilicity and wettability of the silicon wafer surface. On the other hand, due to the presence of the protective film, the polishing agent can polish the surface of the silicon wafer more evenly and smoothly, which helps to improve the polishing efficiency and quality.
[0043] 2) The surfactant in the high-reflective single-crystal silicon alkali polishing additive of the present invention can reduce the contact angle between the alkali polishing liquid and the surface of the silicon wafer, making it easier for the alkali polishing liquid to penetrate into the microstructure of the silicon wafer surface, thereby more effectively removing surface defects and pollutants and making the entire surface more uniform.
[0044] 3) The corrosion inhibitor in the high-reflective single-crystal silicon alkali polishing additive of the present invention can control the reaction rate during the alkali polishing process, reduce the amount of alkali used during the reaction process, and extend the service life of the alkali polishing solution.
[0045] 4) Alkali polishing liquid with high-reflection single-crystal silicon alkaline polishing additives can improve the polishing effect of silicon wafers and achieve highly selective corrosion, that is, protect the silicon oxide coating on the front side of the silicon wafer after boron diffusion from being corroded, and corrode the back side to form a tower base, and finally obtain a single-crystal silicon wafer with a highly reflective back-polished surface, thereby improving the conversion efficiency of solar cells. BRIEF DESCRIPTION OF THE DRAWINGS
[0046] Figure 1 This is a dark field optical microscope image magnified 500 times after polishing the back side using the alkali polishing solution of Example 7; Figure 2 This is a picture of the front side after alkali polishing using the alkali polishing solution of Example 7, magnified 500 times by a dark field optical microscope; Figure 3 This is a dark field optical microscope photo magnified 500 times of the back surface after alkali polishing using the alkali polishing solution of Comparative Example 4; Figure 4 This is a dark field optical microscope photo magnified 500 times of the front side after alkali polishing using the alkali polishing solution of Comparative Example 4. DETAILED DESCRIPTION
[0047] The present invention is further described below with reference to the examples. The description of the technical features described below is based on representative embodiments and specific examples of the present invention, but the present invention is not limited to these embodiments and specific examples. It should be noted that: Unless otherwise stated, the units used in this specification are all international standard units, and the numerical values and numerical ranges appearing in the present invention should be understood to include the inevitable systematic errors in industrial production.
[0048] In this specification, the numerical range expressed using "a numerical value A to a numerical value B" means a range including the endpoints numerical values A and B.
[0049] In this specification, the numerical range expressed using "above" or "below" means a numerical range including the number.
[0050] In this specification, the word "may" includes both performing a certain process and not performing a certain process.
[0051] In this specification, the use of "optional" or "optional" indicates that certain substances, components, execution steps, application conditions and other factors are used or not used.
[0052] In this specification, when "normal temperature" or "room temperature" is used, the temperature may be 15-25°C.
[0053] In this manual, the reagents or instruments used without indicating the manufacturer are all conventional products that can be obtained through commercial purchase.
[0054] Examples 1-6 Examples 1-6 disclose a variety of highly reflective single crystal silicon alkali polishing additives, the components and mass ratios of which are shown in Table 1. The preparation method is as follows: at room temperature, deionized water is first added to a container, and then a protective agent, a polishing agent, a surfactant and a corrosion inhibitor are added in sequence, and stirred until completely dissolved and then stirred for another 2 hours to obtain a highly reflective single crystal silicon alkali polishing additive.
[0055] Table 1 Components and mass ratios of high reflective single crystal silicon alkali polishing additives of Examples 1-6
[0056] Comparative Examples 1-3 Comparative Examples 1-3 disclose a variety of alkali polishing additives, whose components and mass ratios are shown in Table 2, and whose preparation methods are the same as those of Example 1.
[0057] Table 2 Components and mass ratios of alkali polishing additives in comparative examples 1-3
[0058] Examples 7-12 Examples 7-12 disclose a variety of alkali polishing solutions, which respectively include the alkali polishing additives described in Examples 1-6, sodium hydroxide and deionized water, and the mass ratio of the alkali polishing additives, sodium hydroxide and deionized water is 0.3:1:100.
[0059] The preparation method of the alkali polishing solution is as follows: adding a high-reflection single-crystal silicon alkali polishing additive and sodium hydroxide into 62° C. deionized water and stirring and mixing them uniformly to prepare the alkali polishing solution.
[0060] Comparative Examples 4-6 Comparative Examples 4-6 disclose a variety of alkali polishing solutions, including the alkali polishing additives, sodium hydroxide and deionized water described in Comparative Examples 1-3, wherein the mass ratio of the alkali polishing additives, sodium hydroxide and deionized water is 0.3:1:100. The preparation method of the alkali polishing solution is the same as that of Example 7.
[0061] The various properties of the alkali polishing liquids of Examples 7-12 and Comparative Examples 4-6 were tested below.
[0062] Preparation of pre-cleaning solution: sodium hydroxide and hydrogen peroxide are added into deionized water at 61° C. and stirred to mix evenly to prepare a pre-cleaning solution, wherein the mass ratio of sodium hydroxide, hydrogen peroxide and deionized water is 0.2:0.5:100.
[0063] The back side of the single crystal silicon was polished using the alkaline polishing solutions of Examples 7-12 and Comparative Examples 4-6, respectively. The method for polishing the back side of the single crystal silicon is as follows: first, the single crystal silicon wafer after boron expansion is placed in a 61°C pre-cleaning solution, react for 190 seconds, take out the silicon wafer and soak it in deionized water for 100 seconds, take it out and put the pre-cleaned single crystal silicon wafer in the alkaline polishing solution, polish for 200 seconds at 62°C, take out the silicon wafer and immediately rinse it with deionized water for 20 seconds, then rinse it with ethanol for 10 seconds and put it in a 50°C oven for drying.
[0064] Performance Testing: Average reflectivity test: Use a film thickness meter to measure the absolute reflectivity, and then integrate the obtained data to obtain the weighted average reflectivity.
[0065] Tower base size test: Use an optical microscope in dark field mode to measure the distance between the two long sides of the tower base.
[0066] The performance test data of the alkali polishing liquid of Examples 7-12 and Comparative Examples 4-6 are shown in Table 3: Table 3 Performance test data
[0067] From the data in Table 3, it can be seen that when polishing with the alkaline polishing solution of Examples 7-12 (the alkaline polishing solution containing the high-reflectivity single crystal silicon alkaline polishing additive of Examples 1-6, respectively), the tower base size of the silicon wafers obtained in Examples 7-12 meets the requirements and has better integrity, achieving a higher reflectivity; while the tower base size of the silicon wafers obtained with the alkaline polishing solution of Comparative Examples 4-6 (the alkaline polishing solution containing the alkaline polishing additive of Comparative Examples 1-3, respectively) is smaller, the integrity is poor, and the reflectivity is low, which will lead to poor subsequent battery performance.
[0068] Example 7 Alkaline polishing solution was used to polish the back side of the silicon wafer tower base (see Figure 1 ) is compared with the silicon wafer back tower base obtained by using the alkaline polishing solution of Comparative Example 4 (see Figure 3 ) is more uniform and complete, and the front side velvet surface of the silicon wafer obtained by polishing with alkaline polishing solution in Example 7 (see Figure 2 ) is compared with the front velvet surface of the silicon wafer obtained by using the alkaline polishing solution of Comparative Example 4 (see Figure 4 ) has better protection, that is, the front silicon oxide film is not corroded, and the alkaline polishing liquid in Example 7 achieves protection of the front velvet surface.
[0069] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit it. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or replace some or all of the technical features therein with equivalents. However, these modifications or replacements do not cause the essence of the corresponding technical solutions to deviate from the scope of the technical solutions of the embodiments of the present invention.
Claims
1. A highly reflective single crystal silicon alkali polishing additive, characterized in that: The composition comprises the following components in parts by weight: 1-2 parts of protective agent; 1-5 parts of polishing agent; Surfactant 0.1-1 part; Corrosion inhibitor 0.5-2 parts; 60-80 parts of deionized water; The protective agent is a silicon ether compound; The polishing agent is a lithium-containing compound.
2. The high-reflection single-crystal silicon alkali polishing additive according to claim 1, characterized in that: The protective agent is one or more of tert-butyldimethylsilyl glycidyl ether, tert-butyldimethylallylsilyl ether and 1,3-bis(aminopropyl)tetramethyldisiloxane; And / or, the polishing agent is one or more of lithium methacrylate, lithium hexafluorophosphate and isopropyl magnesium chloride-lithium chloride; and / or, the surfactant is one or more of dodecyl glucoside, decyl glucoside, glucopyranoside and o-nitrophenyl-β-D-galactopyranoside; And / or, the corrosion inhibitor is one or more of polyglutamic acid, polylysine, m-hydroxybenzoic acid and p-hydroxybenzoic acid.
3. A method for preparing the highly reflective single-crystal silicon alkali polishing additive according to claim 1 or 2, characterized in that: The following steps are involved: At room temperature, a protective agent, a polishing agent, a surfactant and a corrosion inhibitor are added to deionized water in sequence, and the mixture is stirred until completely dissolved and then stirred for 1-2 hours to obtain a high-reflectivity single-crystal silicon alkali polishing additive.
4. Use of the high-reflection single-crystal silicon alkali polishing additive according to claim 1 or 2 in the field of alkali polishing liquid.
5. An alkali polishing solution, characterized in that It comprises the high-reflective single-crystal silicon alkali polishing additive as described in claim 1 or 2, alkali and deionized water.
6. The alkali polishing solution according to claim 5, characterized in that: The mass ratio of the high-reflection single-crystal silicon alkali polishing additive, alkali and deionized water in the alkali polishing solution is 0.3-1:0.75-1.5:
100.
7. The alkali polishing solution according to claim 5, characterized in that: The alkali is sodium hydroxide and / or potassium hydroxide.
8. A method for preparing the alkali polishing solution according to claim 5, characterized in that: The method comprises the following steps: adding a high-reflection single-crystal silicon alkali polishing additive and alkali into deionized water, stirring and mixing the mixture evenly to prepare an alkali polishing solution.
9. Use of the alkaline polishing solution according to any one of claims 5 to 7 in the field of silicon wafer polishing.
10. The use according to claim 9, characterized in that: The method for polishing a silicon wafer using the alkaline polishing solution is as follows: S1: Use pre-cleaning liquid to pre-clean the silicon wafer before polishing; S2: Soak the pre-cleaned silicon wafer in deionized water, take it out and polish it in an alkaline polishing solution, the polishing time is 190s-240s, and the polishing temperature is 60°C-65°C.
Citation Information
Patent Citations
Composition and method for chemical mechanical polishing of polycrystalline silicon
CN114341287A
Monocrystalline silicon alkali polishing additive and alkali polishing method
CN115948123A
Polish composition FOR CHEMICAL-MECHANICAL POLISHING OF CRYSTALS
DD287843A7
Colloidal silica for polishing
JP2003226865A
Aqueous dispersing element for chemical mechanical polishing
JP2004335897A
Cited By
Small tower footing alkali polishing additive suitable for high back contact of TOPCon battery and use method of small tower footing alkali polishing additive
CN119144238A
A high back contact small tower base alkali throwing additive for topcon cells and method of use thereof
CN119144238B
Preparation method and use method of original silicon wafer alkali polishing additive
CN119800520A