Display substrate, display panel and display device
By designing a pixel-defined layer of gradient fluorine concentration and retaining wall structure on the display substrate, the problems of overflow and uneven film formation after ink droplets in the OLED display panel are solved, and a more uniform film formation of the light emitting layer is achieved.
Patent Information
- Application Number
- CN202411003225.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-24
- Publication Date
- 2024-11-12
AI Technical Summary
When preparing the light emitting layer of the OLED display panel by inkjet printing, there are problems of overflow color mixing and uneven film formation after ink droplets are sprayed into the pixel opening.
A display substrate is designed with a pixel-defined layer containing a material with a gradient fluorine concentration and a retaining wall structure, by adjusting the fluorine concentration and retaining wall thickness, ensuring that ink droplets flow evenly within the pixel opening and avoid overflowing to adjacent openings.
It effectively avoids the problems of ink droplet overflow and color mixing, improves the film formation uniformity of the light emitting layer, and improves the display effect of the display panel.
Smart Images

Figure CN118946198A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the field of display technology, and in particular to a display substrate, a display panel and a display device. Background Art
[0002] Organic light-emitting diode (OLED) display panels are a new generation of light-emitting display technology after liquid crystal display panels. They have the advantages of wide viewing angle, high contrast, bright colors, and flexible display. They have been widely used in various mobile phones, laptops, and wearable devices. When the light-emitting layer in the OLED display panel is prepared by inkjet printing, a pixel defining layer needs to be made on the array substrate / base in advance. The pixel defining layer defines multiple pixel openings so that the ink droplets of the light-emitting layer can be accurately sprayed into the specified pixel openings.
[0003] However, in the related art, after the ink droplets of the light-emitting layer are sprayed into the designated pixel openings, there are problems of overflow, color mixing and uneven film formation. Summary of the invention
[0004] The embodiments of the present application provide a display substrate, a display panel and a display device, which can solve the problems of overflow color mixing and uneven film formation after ink droplets of the light-emitting layer are sprayed into designated pixel openings in the related art.
[0005] According to a first aspect of an embodiment of the present application, a display substrate is provided, comprising a substrate, and a pixel defining layer disposed on one side of the substrate, wherein the pixel defining layer comprises a plurality of pixel defining structures, and a plurality of pixel openings defined by the pixel defining structures;
[0006] The material of the pixel defining structure includes fluorine element, and the side surface of the pixel defining structure facing the pixel opening has a gradual fluorine concentration along a direction perpendicular to the plane where the substrate is located, and in the side surface of the pixel defining structure, the fluorine concentration at one end close to the substrate is less than the fluorine concentration at one end away from the substrate.
[0007] In some embodiments, in the side surface of the pixel defining structure, a ratio of a fluorine concentration at an end close to the substrate to a fluorine concentration at an end far from the substrate is 0 to 0.3.
[0008] In some embodiments, the pixel defining layer further includes a plurality of first retaining walls, at least one of the pixel openings is provided with the first retaining wall, the first retaining wall divides the pixel opening into a first sub-opening and a second sub-opening, and in a direction perpendicular to the plane where the substrate is located, the thickness of the pixel defining structure is a first thickness, the thickness of the first retaining wall is a second thickness, and the second thickness is less than the first thickness; or / and
[0009] The pixel defining layer also includes a plurality of second retaining walls, wherein the second retaining wall is disposed in at least one of the pixel openings, and the side of the second retaining wall away from the pixel opening is connected to the pixel defining structure, and the side of the second retaining wall close to the pixel opening faces the pixel opening, and in a direction perpendicular to the plane where the substrate is located, the thickness of the second retaining wall is a third thickness, and the third thickness is less than the first thickness.
[0010] In some embodiments, when the first retaining wall is provided in at least one of the pixel openings, in the extension direction of the first retaining wall, the first retaining wall includes a first sub-retaining wall portion and a second sub-retaining wall portion located on at least one side of the first sub-retaining wall portion, the first sub-retaining wall portion is connected to the second sub-retaining wall portion, and in the direction perpendicular to the plane where the substrate is located, the thickness of the first sub-retaining wall portion is different from the thickness of the second sub-retaining wall portion.
[0011] In some embodiments, in the extension direction of the first retaining wall, the first retaining wall includes the first sub-retaining wall portion and two second sub-retaining wall portions located on both sides of the first sub-retaining wall portion, and the thickness of the first sub-retaining wall portion is greater than the thickness of the second sub-retaining wall portion.
[0012] In some embodiments, the thickness in a direction perpendicular to the plane where the base is located gradually decreases from the first sub-retaining wall portion toward the second sub-retaining wall portion.
[0013] In some embodiments, the thickness of the first sub-retaining wall portion is greater than the thickness of the second sub-retaining wall portion;
[0014] The first retaining wall includes a first sub-membrane layer and a second sub-membrane layer arranged on a side of the first sub-membrane layer away from the substrate. The first sub-retaining wall portion is composed of the first sub-membrane layer and the second sub-membrane layer, and the second sub-retaining wall portion is composed of the first sub-membrane layer.
[0015] In some embodiments, the first sub-layer is an inorganic material, and the second sub-layer is an organic material.
[0016] In some embodiments, when the first barrier wall is disposed in at least one of the pixel openings, the first sub-opening and the second sub-opening have different areas.
[0017] In some embodiments, when the first barrier wall is disposed in at least one of the pixel openings, at least one of the following conditions is satisfied:
[0018] The width of the pixel defining structure is greater than the width of the first retaining wall;
[0019] The first retaining wall is arranged away from the center point of the pixel opening;
[0020] A difference in area between the first sub-opening and the second sub-opening is greater than or equal to 10%.
[0021] In some embodiments, when the first barrier wall is disposed in at least one of the pixel openings, a width of an end of the at least one of the first barrier walls away from the substrate is greater than a width of an end of the first barrier wall close to the substrate; or / and
[0022] The width of at least one end of the pixel definition structure away from the substrate is greater than the width of the end of the pixel definition structure close to the substrate.
[0023] In some embodiments, when the first barrier wall is disposed in at least one of the pixel openings, the display substrate further comprises a first electrode layer disposed between the base and the pixel defining layer, the first electrode layer comprises a plurality of first electrodes arranged in an array, and the pixel opening exposes the corresponding first electrode;
[0024] The first electrode includes a first sub-electrode, a second sub-electrode and a spacer, the first sub-electrode and the second sub-electrode are arranged on both sides of the spacer to be spaced apart, and within the pixel opening, the orthographic projection of the first blocking wall on the substrate covers the orthographic projection of the spacer on the substrate.
[0025] In some embodiments, when the second retaining wall is provided in at least one of the pixel openings, in at least one of the pixel openings, the second retaining wall is attached to the pixel defining structure to form a first opening, and the orthographic projection of the first opening on the substrate is located within the orthographic projection of the pixel opening on the substrate.
[0026] In some embodiments, when the second retaining wall is provided in at least one of the pixel openings, the edge of the second retaining wall away from the nearest pixel defining structure has a first climbing portion, and the slope angle of the first climbing portion is 40 to 50 degrees, and the slope angle is the angle between the tangent of the first climbing portion and the plane parallel to the substrate.
[0027] In some embodiments, the pixel defining layer includes a plurality of the first retaining walls and a plurality of the second retaining walls, and the display substrate satisfies at least one of the following conditions:
[0028] The pixel defining structure, the first retaining wall and the second retaining wall are connected to form a continuous structure;
[0029] The third thickness is less than or equal to the second thickness.
[0030] In some embodiments, at least one of the following conditions is met:
[0031] In the case where the first barrier wall is disposed in at least one of the pixel openings, a ratio of the first thickness to the second thickness is greater than or equal to 3 and less than or equal to 6;
[0032] In the case where the second barrier wall is disposed in at least one of the pixel openings, a ratio of the second thickness to the third thickness is greater than or equal to 1 and less than or equal to 1.5.
[0033] In some embodiments, at least one of the following conditions is met:
[0034] In the case where the first retaining wall is disposed in at least one of the pixel openings, the pixel defining structure is made of a liquid-repellent material, and the first retaining wall is made of a liquid-philic material;
[0035] In the case where the second retaining wall is disposed in at least one of the pixel openings, the pixel defining structure is made of a liquid-repellent material, and the second retaining wall is made of a liquid-repellent material.
[0036] According to a second aspect of the embodiments of the present application, a display panel is provided, comprising a substrate, and a pixel defining layer disposed on one side of the substrate, wherein the pixel defining layer comprises a plurality of pixel defining structures, and a plurality of pixel openings defined by the pixel defining structures;
[0037] The pixel defining layer further comprises a plurality of first retaining walls, at least one of the pixel openings is provided with the first retaining wall, the first retaining wall divides the pixel opening into a first sub-opening and a second sub-opening, in a direction perpendicular to the plane where the substrate is located, the thickness of the pixel defining structure is a first thickness, the thickness of the first retaining wall is a second thickness, and the second thickness is less than the first thickness;
[0038] The first sub-opening and the second sub-opening have different areas.
[0039] According to a third aspect of the embodiments of the present application, a display panel is provided, comprising any one of the display substrates described above.
[0040] According to a fourth aspect of the embodiments of the present application, a display device is provided, comprising the display panel described above, or the display device comprises any one of the display substrates described above.
[0041] In some embodiments of the present application, the side surface of the pixel defining structure facing the pixel opening has a gradual fluorine concentration along a direction perpendicular to the plane where the substrate is located, and in the side surface of the pixel defining structure, the fluorine concentration at one end close to the substrate is less than the fluorine concentration at one end away from the substrate, that is, the fluorine concentration gradually increases from the first end to the second end, the fluorine concentration at the first end is smaller, the first end has smaller liquid repellency, and the fluorine concentration at the second end is larger, the second end has larger liquid repellency, and the first end can be used to avoid poor wetting (De-Weeting) of ink droplets of the light-emitting layer at the edge of the pixel defining structure, for example, to avoid the shrinkage of some sub-film layers of the light-emitting layer, etc., thereby improving the problem of uneven film formation of the light-emitting layer of the display panel; at the same time, the fluorine concentration of the second surface is the same or similar to the fluorine concentration of the second end, and the liquid repellency of the second end and the second surface (the surface of the pixel defining structure away from the substrate) can ensure that the ink droplets flow in the corresponding pixel opening (flow between the pixel defining structures surrounding the corresponding pixel opening), thereby avoiding the ink droplets from crossing the pixel defining structure and entering the adjacent pixel opening, thereby avoiding the problem of color mixing. Therefore, in some embodiments of the present application, the color mixing problem can be improved and the uneven film formation of the light-emitting layer of the display panel can be improved. BRIEF DESCRIPTION OF THE DRAWINGS
[0042] Figure 1 A schematic diagram of a process in which ink droplets of a light-emitting layer are sprayed into a pixel opening in a related technology provided in an embodiment of the present application;
[0043] Figure 2 A schematic top view of a first partial structure of a display substrate provided in an embodiment of the present application;
[0044] Figure 3 A schematic top view of a second partial structure of a display substrate provided in an embodiment of the present application;
[0045] Figure 4 A schematic top view of a third partial structure of a display substrate provided in an embodiment of the present application;
[0046] Figure 5 A schematic top view of a fourth partial structure of a display substrate provided in an embodiment of the present application;
[0047] Figure 6 A schematic top view of a fifth partial structure of a display substrate provided in an embodiment of the present application;
[0048] Figure 7 A schematic top view of a sixth partial structure of a display substrate provided in an embodiment of the present application;
[0049] Figure 8 A schematic top view of a seventh partial structure of a display substrate provided in an embodiment of the present application;
[0050] Fig. 9 A cross-sectional schematic diagram of a first partial structure of a display substrate provided in an embodiment of the present application;
[0051] Fig.10 A cross-sectional schematic diagram of a second partial structure of a display substrate provided in an embodiment of the present application;
[0052] Fig.11 A schematic cross-sectional view of a third partial structure of a display substrate provided in an embodiment of the present application;
[0053] Fig.12 A schematic cross-sectional view of a fourth partial structure of a display substrate provided in an embodiment of the present application;
[0054] Fig.13 A schematic cross-sectional view of a fifth partial structure of a display substrate provided in an embodiment of the present application;
[0055] Fig.14 A schematic cross-sectional view of a sixth partial structure of a display substrate provided in an embodiment of the present application;
[0056] Fig.15 A schematic cross-sectional view of a seventh partial structure of a display substrate provided in an embodiment of the present application;
[0057] Fig.16 A schematic cross-sectional view of an eighth partial structure of a display substrate provided in an embodiment of the present application;
[0058] Fig.17 A schematic top view of an eighth partial structure of a display substrate provided in an embodiment of the present application;
[0059] Fig.18 A schematic cross-sectional view of a ninth partial structure of a display substrate provided in an embodiment of the present application;
[0060] Fig.19 A schematic top view of a ninth partial structure of a display substrate provided in an embodiment of the present application;
[0061] Fig. 20 A schematic top view of a tenth partial structure of a display substrate provided in an embodiment of the present application;
[0062] Fig.21 A schematic cross-sectional view of a tenth partial structure of a display substrate provided in an embodiment of the present application;
[0063] Fig. 22 A schematic cross-sectional view of an eleventh partial structure of a display substrate provided in an embodiment of the present application;
[0064] Fig.23 A schematic cross-sectional view of a twelfth partial structure of a display substrate provided in an embodiment of the present application;
[0065] Fig.24 A schematic cross-sectional view of a thirteenth partial structure of a display substrate provided in an embodiment of the present application;
[0066] Fig.25 A schematic top view of an eleventh partial structure of a display substrate provided in an embodiment of the present application;
[0067] Fig.26 A schematic top view of a twelfth partial structure of a display substrate provided in an embodiment of the present application;
[0068] Fig. 27 This is a schematic top view of a thirteenth local structure of a display substrate provided in an embodiment of the present application. DETAILED DESCRIPTION
[0069] In order to better understand the technical solutions provided by the embodiments of this specification, the technical solutions of the embodiments of this specification are described in detail below through the accompanying drawings and specific embodiments. It should be understood that the embodiments of this specification and the specific features in the embodiments are detailed descriptions of the technical solutions of the embodiments of this specification, rather than limitations on the technical solutions of this specification. In the absence of conflict, the embodiments of this specification and the technical features in the embodiments can be combined with each other.
[0070] In this article, relational terms such as first and second, etc. are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply that there is any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprise" or any other variants thereof are intended to cover non-exclusive inclusion, so that the process, method, article or equipment including a series of elements includes not only those elements, but also includes other elements not explicitly listed, or also includes elements inherent to such process, method, article or equipment. In the absence of more restrictions, the elements limited by the statement "comprise one..." do not exclude the existence of other identical elements in the process, method, article or equipment including the elements. The term "more than two" includes two or more than two situations.
[0071] like Figure 1 As shown, Figure 1A schematic diagram of the process of ink droplets of the light-emitting layer being sprayed into the pixel opening SP in a related technology provided in an embodiment of the present application, when the light-emitting layer in the OLED display panel is prepared by inkjet printing (the light-emitting layer includes at least one of the film layers such as the light-emitting material layer EML, the hole transport layer HTL, the hole injection layer HIL, the electron injection layer EIL, the electron transport layer ETL, the hole blocking layer HBL and the electron blocking layer EBL, but not limited thereto), it is necessary to pre-make a pixel defining layer De on the substrate 11 or the array substrate, the pixel defining layer De includes a plurality of pixel defining structures D1, and the pixel defining structure D1 defines a plurality of pixel openings SP, so that the ink droplets M01 of the light-emitting layer are accurately sprayed into the specified pixel openings SP, however, in the related technology, there is a problem that the ink droplets M01 of the light-emitting layer overflow to the adjacent sub-pixels after being sprayed into the specified pixel openings SP, and the problem of uneven film formation. For example, the inventor found that the ink droplets M01 crossed the pixel defining structure D1 and entered the adjacent pixel openings SP, causing color mixing. For example, the inventors found that the width of the pixel defining structure D1 is large and the number is large. The pixel defining structure D1 occupies a large area, which reduces the area of the pixel opening SP. The volume of the ink droplets required for one pixel opening SP is small, which makes the allowable volume error of the ink droplets small, reduces the uniformity of film formation between different pixel openings, and makes the light-emitting layer of the display panel unevenly formed. For example, the inventors found that when the pixel opening SP has a pixel defining structure D1 in the long side direction and a pixel defining structure D1 in the short side direction (in the extension direction of the pixel defining structure, the length of the pixel defining structure in the long side direction is greater than the length of the pixel defining structure in the short side direction), the diffusion distance of the ink droplets of the light-emitting layer in the long side and short side directions is different, so that there is also a problem of uneven film formation in the same pixel opening SP. At the same time, the surface energy of the anode at the edge of the pixel defining structure D1 is less than the surface energy at the center of the pixel opening SP, and the ink droplets MO1 of the light-emitting layer have a poor wetting (De-Weeting) phenomenon at the edge of the pixel defining structure D1, which also makes the light-emitting layer of the display panel unevenly formed.
[0072] In view of this, the embodiments of the present application provide a display substrate, a display panel and a display device, which can solve or improve at least one problem existing in the above-mentioned related technologies.
[0073] Some embodiments of the present application provide a display substrate, comprising a substrate, and a pixel defining layer disposed on one side of the substrate, wherein the pixel defining layer comprises a plurality of pixel defining structures, and a plurality of pixel openings defined by the pixel defining structures;
[0074] The material of the pixel defining structure includes fluorine element, and the side surface of the pixel defining structure facing the pixel opening has a gradual fluorine concentration along a direction perpendicular to the plane where the substrate is located, and in the side surface of the pixel defining structure, the fluorine concentration at one end close to the substrate is less than the fluorine concentration at one end away from the substrate.
[0075] Some embodiments of the present application provide a display substrate, comprising a substrate, and a pixel defining layer disposed on one side of the substrate, wherein the pixel defining layer comprises a plurality of pixel defining structures, and a plurality of pixel openings defined by the pixel defining structures;
[0076] The pixel defining layer further comprises a plurality of first retaining walls, at least one of the pixel openings is provided with the first retaining wall, the first retaining wall divides the pixel opening into a first sub-opening and a second sub-opening, in a direction perpendicular to the plane where the substrate is located, the thickness of the pixel defining structure is a first thickness, the thickness of the first retaining wall is a second thickness, and the second thickness is less than the first thickness;
[0077] The first sub-opening and the second sub-opening have different areas.
[0078] The present application also provides a display panel, which includes any one of the above-mentioned display substrates.
[0079] The present application also provides a display device, which includes any one of the above-mentioned display substrates and / or display panels.
[0080] Different embodiments are described in detail below, and the implementation features in different embodiments can be combined with each other.
[0081] See also Figures 2 to 9 , Figure 2 A schematic top view of a first partial structure of a display substrate provided in an embodiment of the present application; Figure 3 A schematic top view of a second partial structure of a display substrate provided in an embodiment of the present application; Figure 4 A schematic top view of a third partial structure of a display substrate provided in an embodiment of the present application; Figure 5 A schematic top view of a fourth partial structure of a display substrate provided in an embodiment of the present application; Figure 6 A schematic top view of a fifth partial structure of a display substrate provided in an embodiment of the present application; Figure 7 A schematic top view of a sixth partial structure of a display substrate provided in an embodiment of the present application; Figure 8 A schematic top view of a seventh local structure of a display substrate provided in an embodiment of the present application. Figure 2 and Figure 3 Similar, but different: Figure 2 Schematic diagram of a display substrate of a transparent display panel, Figure 3 Schematic diagram of a display substrate of a non-transparent display panel, Figure 3 The pixel openings of sub-pixels of different colors (pixel openings of different colors) in the display substrate are also marked.
[0082] See also Figures 9 to 14 , Fig. 9 A cross-sectional schematic diagram of a first partial structure of a display substrate provided in an embodiment of the present application; Fig.10 A cross-sectional schematic diagram of a second partial structure of a display substrate provided in an embodiment of the present application; Fig.11 A schematic cross-sectional view of a third partial structure of a display substrate provided in an embodiment of the present application; Fig.12 A schematic cross-sectional view of a fourth partial structure of a display substrate provided in an embodiment of the present application; Fig.13 A schematic cross-sectional view of a fifth partial structure of a display substrate provided in an embodiment of the present application; Fig.14 A schematic cross-sectional view of a sixth partial structure of a display substrate provided in an embodiment of the present application; Fig.15 A schematic cross-sectional view of a seventh partial structure of a display substrate provided in an embodiment of the present application; Fig.16 A cross-sectional schematic diagram of an eighth partial structure of a display substrate provided in an embodiment of the present application. Fig. 9 , Fig.11 , Fig.12 , Fig.13 , Fig.14 for Figure 2 The cross-sectional schematic diagram along the direction of the first dotted line CC is a cross-sectional schematic diagram along the extension direction of the first retaining wall D2; Fig.10 , Fig.15 and Fig.16 for Figure 2 The cross-sectional schematic diagram along the second dotted line DD is a cross-sectional schematic diagram perpendicular to the extending direction of the first retaining wall D2.
[0083] See also Fig.17 and Fig.18 , Fig.17 A schematic top view of an eighth partial structure of a display substrate provided in an embodiment of the present application; Fig.18 A schematic cross-sectional view of a ninth partial structure of a display substrate provided in an embodiment of the present application. Fig.18 for Fig.17 The cross-sectional schematic diagram along the second dotted line DD is a cross-sectional schematic diagram perpendicular to the extending direction of the first retaining wall D2. Fig.17 Schematic diagram of the relationship between the orthographic projection of the first electrode on the substrate and the orthographic projection of the first retaining wall D2 on the substrate.
[0084] See also Figures 19 to 24 , Fig.19 A schematic top view of a ninth partial structure of a display substrate provided in an embodiment of the present application; Fig. 20 A schematic top view of a tenth local structure of a display substrate provided in an embodiment of the present application. Fig.21 A schematic cross-sectional view of a tenth partial structure of a display substrate provided in an embodiment of the present application; Fig. 22 A schematic cross-sectional view of an eleventh partial structure of a display substrate provided in an embodiment of the present application; Fig.23 A schematic cross-sectional view of a twelfth partial structure of a display substrate provided in an embodiment of the present application; Fig.24 This is a cross-sectional schematic diagram of the thirteenth local structure of a display substrate provided in an embodiment of the present application. Fig.21 for Fig.19 The cross-sectional schematic diagram along the third dotted line EE is a cross-sectional schematic diagram along a direction perpendicular to the side surface of the pixel defining structure (the pixel defining structure D1 extends around the pixel opening SP); Fig. 22 , Fig.23 for Fig. 20 The cross-sectional schematic diagram along the direction of the first dotted line CC is a cross-sectional schematic diagram along the extension direction of the first retaining wall D2; Fig.24 for Fig. 20 The cross-sectional schematic diagram along the second dotted line DD is a cross-sectional schematic diagram perpendicular to the extending direction of the first retaining wall D2.
[0085] The present application provides a display substrate 1000, which includes a substrate 11 and a pixel defining layer De arranged on one side of the substrate 11, wherein the pixel defining layer De includes a plurality of pixel defining structures D1 and a plurality of pixel openings SP defined by the pixel defining structures D1; wherein the material of the pixel defining structures D1 includes a fluorine element, and a side surface of the pixel defining structure D1 facing the pixel opening SP has a gradual fluorine concentration along a direction perpendicular to a plane where the substrate 11 is located, and in the side surface of the pixel defining structure D1, the fluorine concentration at one end close to the substrate 11 is less than the fluorine concentration at the end away from the substrate 11.
[0086] For example, the substrate 11 may be glass or a flexible substrate 11 , and the flexible substrate 11 may be polyimide, which is not limited here.
[0087] For example, the film structure of the display substrate 1000 may include: a substrate 11, a driving circuit layer disposed on one side of the substrate 11, a first electrode layer disposed on a side of the driving circuit layer away from the substrate, and a pixel defining layer De disposed on a side of the first electrode layer away from the substrate. The first electrode layer includes a plurality of first electrodes AN arranged in an array, and the pixel defining layer De includes a plurality of pixel defining structures D1 and a plurality of pixel openings SP, wherein the pixel openings SP expose the corresponding first electrodes AN.
[0088] For example, in some embodiments, the display substrate 1000 may include a plurality of light-emitting devices, and the light-emitting devices include: a first electrode AN disposed on one side of a substrate 11, a light-emitting layer disposed on a side of the first electrode AN away from the substrate 11, and a second electrode disposed on a side of the light-emitting layer away from the substrate 11. One of the first electrode AN and the second electrode is an anode, and the other is a cathode. In the present application, the first electrode AN is an anode and the second electrode is a cathode.
[0089] For example, in some embodiments, the driving circuit layer may include a plurality of pixel driving circuits, the first electrode AN is electrically connected to a corresponding pixel driving circuit, and the pixel driving circuit is used to drive the light-emitting device to emit light.
[0090] For example, Fig.10 As shown, the side surface of the pixel defining structure D1 facing the pixel opening SP is the first surface D11, the end of the side surface of the pixel defining structure D1 close to the substrate 11 is the first end D111 (that is, the end of the first surface D11 close to the substrate 11 is the first end D111), and the end of the side surface of the pixel defining structure D1 away from the substrate 11 is the second end D112 (that is, the end of the first surface D11 away from the substrate 11 is the second end D112), and along the direction perpendicular to the plane where the substrate 11 is located (along the thickness direction of the pixel defining structure D1), the fluorine concentration from the first end D111 to the second end D112 gradually increases.
[0091] For example, Fig.10 As shown, the surface of the pixel defining structure D1 away from the substrate 11 (the top surface of the pixel defining structure D1 ) is the second surface D12 , and the fluorine concentration of the second surface D12 is the same as or similar to the fluorine concentration of the second end D112 .
[0092] For example, Fig.10 As shown, the fluorine concentration at the second end D112 is relatively large, so that the second end D112 and the second surface D12 are more liquid-phobic, which can ensure that the ink droplet M01 flows within the corresponding pixel opening SP (flows between the pixel defining structures D1 surrounding the corresponding pixel opening SP), avoiding the ink droplet M01 from crossing the pixel defining structure D1 and entering the adjacent pixel opening SP, thereby avoiding the color mixing problem.
[0093] For example, Fig.10 As shown, the fluorine concentration at the first end D111 is relatively small, so that the first end D111 is less liquid-phobic, thereby avoiding poor wetting (De-Weeting) of the ink droplets MO1 of the light-emitting layer at the edge of the pixel-defining structure D1, for example, avoiding the shrinkage of sub-film layers such as the hole injection layer HIL of the light-emitting layer, thereby improving the problem of uneven film formation of the light-emitting layer of the display panel.
[0094] For example, in some embodiments, along the direction perpendicular to the plane of the substrate 11, the surface energy from the first end D111 to the second end D112 gradually decreases, so that the liquid repellency from the first end D111 to the second end D112 gradually increases. On the one hand, the second end D112 and the second surface D12 have greater liquid repellency, which can prevent the ink droplet M01 from crossing the pixel defining structure D1 and entering the adjacent pixel opening SP, thereby avoiding the color mixing problem; on the other hand, the first end D111 has less liquid repellency, thereby preventing the ink droplet MO1 of the light-emitting layer from having poor wetting (De-Weeting) at the edge of the pixel defining structure D1, for example, preventing the sub-film layers such as the hole injection layer HIL of the light-emitting layer from shrinking, thereby improving the problem of uneven film formation of the light-emitting layer of the display panel.
[0095] In some embodiments of the present application, Fig.10 As shown, the side surface of the pixel defining structure D1 facing the pixel opening SP has a gradually changing fluorine concentration along a direction perpendicular to the plane where the substrate 11 is located, and in the side surface of the pixel defining structure D1, the fluorine concentration at one end close to the substrate 11 is less than the fluorine concentration at one end away from the substrate 11, that is, the fluorine concentration from the first end D111 to the second end D112 gradually increases, the fluorine concentration at the first end D111 is smaller, the liquid repellency of the first end D111 is smaller, the fluorine concentration at the second end D112 is larger, and the liquid repellency of the second end D112 is larger, and the ink droplet MO1 of the light-emitting layer can be prevented from being deposited on the pixel defining structure D1 by the first end D111. 1 has poor wetting (De-Weeting), for example, avoiding the shrinkage of some sub-film layers of the light-emitting layer, etc., improving the problem of uneven film formation of the light-emitting layer of the display panel; at the same time, the fluorine concentration of the second surface D12 is the same or similar to the fluorine concentration of the second end D112, and the liquid repellency of the second end D112 and the second surface D12 can ensure that the ink droplet M01 flows in the corresponding pixel opening SP (flows between the pixel defining structure D1 surrounding the corresponding pixel opening SP), avoiding the ink droplet M01 from crossing the pixel defining structure D1 and entering the adjacent pixel opening SP, avoiding the color mixing problem. Therefore, in some embodiments of the present application, it has the effect of improving the color mixing problem and improving the uneven film formation of the light-emitting layer of the display panel.
[0096] In some embodiments, in the side surface of the pixel defining structure D1 , a ratio of a fluorine concentration at an end close to the substrate 11 to a fluorine concentration at an end far from the substrate 11 is 0 to 0.3.
[0097] For example, Fig.10As shown, after verification by the inventor's design, the ratio of the fluorine concentration at the first end D111 to that at the second end D112 ranges from 0 to 0.3. For example, the ratio of the fluorine concentration at the first end D111 to that at the second end D112 is any one of 0, 0.05, 0.1, 0.15, 0.2, 0.25 and 0.3, which can simultaneously have a better effect of improving the color mixing problem and better improving the uneven film formation of the light-emitting layer of the display panel.
[0098] By way of example, in some embodiments, the ratio of the fluorine concentration at the first end D111 to the fluorine concentration at the second end D112 ranges from 0 to 0.1 (for example, the ratio of the fluorine concentration at the first end D111 to the fluorine concentration at the second end D112 can be any value of 0, 0.02, 0.05, 0.08 and 0.1), and in the direction perpendicular to the plane of the substrate 11, the thickness of the portion of the pixel defining structure D1 at (or corresponding to) the first end D111 is less than or equal to 0.1 micrometers (for example, the thickness of the portion of the pixel defining structure D1 corresponding to the first end D111 is any value of 0.02 micrometers, 0.05 micrometers, 0.08 micrometers and 0.1 micrometers).
[0099] By way of example, in some embodiments, on the side surface of the pixel defining structure D1, the contact angle between the first end D111 and the ink droplet M01 of the light-emitting layer is less than or equal to 10 degrees, so that the first end D111 is less liquid-phobic to the ink droplet M01 of the light-emitting layer. At this time, in a direction perpendicular to the plane of the substrate 11, the thickness of the portion of the pixel defining structure D1 at (or corresponding to) the first end D111 is 10% to 50% (h1×10% to h1×50%) of the first thickness h1.
[0100] By way of example, in some embodiments, in the side surface of the pixel defining structure D1, the contact angle between the second end D112 and the ink droplet M01 of the light-emitting layer is greater than or equal to 40 degrees, so that the second end D112 is more lyophobic to the ink droplet M01 of the light-emitting layer. At this time, in the direction perpendicular to the plane of the substrate 11, the thickness of the portion of the pixel defining structure D1 at (or corresponding to) the second end D112 is 60% to 80% of the first thickness h1 (h1×60% to h1×80%).
[0101] For example, in some embodiments, the mass percentage of fluorine element at the first end D111 is 0 to 2%, for example, the mass percentage of fluorine element at the first end D111 is any value among 0%, 0.5%, 1%, 1.5% and 2%. In some embodiments, the mass percentage of fluorine element at the second end D112 is 5 to 20%, for example, the mass percentage of fluorine element at the second end D112 is any value among 5%, 8%, 10%, 12%, 15%, 18% and 20%.
[0102] In some embodiments, the display substrate 1000 includes a base 11 and a pixel defining layer De disposed on one side of the base 11 , the pixel defining layer De includes a plurality of pixel defining structures D1 and a plurality of pixel openings SP defined by the pixel defining structures D1 . Among them, the pixel defining layer De also includes a plurality of first retaining walls D2, at least one pixel opening SP is provided with a first retaining wall D2, the first retaining wall D2 divides the pixel opening SP into a first sub-opening SP01 and a second sub-opening SP02, and in a direction perpendicular to the plane where the substrate 11 is located, the thickness of the pixel defining structure D1 is a first thickness h1, the thickness of the first retaining wall D2 is a second thickness h2, and the second thickness h2 is less than the first thickness h1; or / and, the pixel defining layer De also includes a plurality of second retaining walls D3, at least one pixel opening SP is provided with a second retaining wall D3, and the side of the second retaining wall D3 away from the pixel opening SP is connected to the pixel defining structure D1, and the side of the second retaining wall D3 close to the pixel opening SP faces the pixel opening SP, and in a direction perpendicular to the plane where the substrate 11 is located, the thickness of the second retaining wall D3 is a third thickness h3, and the third thickness h3 is less than the first thickness h1.
[0103] For example, Fig.10 As shown, combined with Fig.18 In a direction perpendicular to the plane where the substrate 11 is located, the thickness of the pixel defining structure D1 is a first thickness h1, and the thickness of the first retaining wall D1 is a second thickness h2, and the second thickness h2 is less than the first thickness h1, so that in a direction perpendicular to the plane where the substrate 11 is located, the distance from the surface of the first retaining wall D2 away from the substrate 11 to the substrate 11 (or the first electrode AN) is less than the distance from the surface of the pixel defining structure D1 away from the substrate 11 to the substrate 11 (or the first electrode AN).
[0104] For example, in some embodiments, the structure of the display substrate 1000 may include a substrate 11, a plurality of first electrodes AN arranged in an array, and a pixel defining layer De disposed on a side of the first electrode AN away from the substrate 11; in a direction perpendicular to the plane where the substrate 11 is located, the thickness of the pixel defining structure D1 refers to the thickness of the pixel defining structure D1 on the first electrode AN, and the thickness of the first retaining wall D1 refers to the thickness of the first retaining wall D1 on the first electrode AN. For example, Fig.24 As shown, combined with Fig.18 In a direction perpendicular to the plane where the substrate 11 is located, the thickness of the second retaining wall D3 is a third thickness h3, and the third thickness h3 is less than the first thickness h1, so that in a direction perpendicular to the plane where the substrate 11 is located, the distance from the surface of the second retaining wall D3 away from the substrate 11 to the substrate 11 (or the first electrode AN) is less than the distance from the surface of the pixel defining structure D1 away from the substrate 11 to the substrate 11 (or the first electrode AN).
[0105] By way of example, in some embodiments, the structure of the display substrate 1000 may include a substrate 11, a plurality of first electrodes AN arranged in an array, and a pixel defining layer De disposed on a side of the first electrode AN away from the substrate 11; in a direction perpendicular to the plane where the substrate 11 is located, the thickness of the pixel defining structure D1 refers to the thickness of the pixel defining structure D1 on the first electrode AN, and the thickness of the second retaining wall D3 refers to the thickness of the second retaining wall D3 on the first electrode AN.
[0106] Wherein, in some embodiments, Figures 2 to 18 As shown, the pixel defining layer De further includes a plurality of first retaining walls D2, and the pixel defining layer De does not include a second retaining wall D3. However, in some other embodiments, the pixel defining layer De may further include a second retaining wall D3.
[0107] For example, in the region of the plurality of pixel openings SP defined by the pixel defining structure D1 , the first barrier wall D2 is used to divide the pixel openings into at least a first sub-opening SP01 and a second sub-opening SP02 .
[0108] For example, one or more first blocking walls D2 may be disposed in one pixel opening SP. The embodiment of the present application takes one first blocking wall D2 disposed in one pixel opening SP as an example, but is not limited thereto.
[0109] For example, Fig.10 As shown, in some embodiments, ink droplets of at least part of the film layer of the light-emitting layer are only set in one pixel opening SP, and are not diffused / flowed in adjacent pixel openings SP at the same time. The pixel defining structure D1 has the function of blocking the ink droplets from flowing between adjacent pixel openings SP, so the first thickness h1 is set to be larger. Ink droplets of at least part of the film layer of the light-emitting layer are sprayed into one of the first sub-opening SP01 and the second sub-opening SP02, and the ink droplets flow or diffuse into the other (or, ink droplets of at least part of the film layer of the light-emitting layer are sprayed into the first sub-opening SP01 and the second sub-opening SP02 at the same time, and the ink droplets flow between the first sub-opening SP01 and the second sub-opening SP02), so the second thickness h2 is set to be smaller. In order to make the ink droplets be confined in the pixel opening SP, and to make the ink droplets flow or diffuse between the first sub-opening SP01 and the second sub-opening SP02 of the same pixel opening SP, the second thickness h2 is set to be smaller than the first thickness h1.
[0110] For example, in some embodiments, one first barrier wall D2 is disposed in a pixel opening SP; in some other embodiments, two or more first barrier walls D2 may be disposed in a pixel opening SP.
[0111] For example, in the related art, the ink droplet M01 passes over the pixel defining structure D1 and enters the adjacent pixel opening SP, causing color mixing. In some embodiments of the present application, by setting the pixel defining structure D1 to be a liquid-repellent material, it is possible to ensure that the ink droplet M01 flows in the corresponding pixel opening SP (flows between the pixel defining structures D1 surrounding the corresponding pixel opening SP), thereby preventing the ink droplet M01 from passing over the pixel defining structure D1 and entering the adjacent pixel opening SP, thereby avoiding the color mixing problem.
[0112] For example, in some embodiments, for example Fig. 9 Example compared to Figure 1 For example, a first blocking wall D2 is used to replace the pixel limiting structure D1 originally set in the position, and the first sub-opening SP01 and the second sub-opening SP02 replace the two pixel openings in the related technology. The area of the pixel opening SP is increased, and the volume of the ink droplet required for one pixel opening SP is increased, so that the allowable volume error of the ink droplet is increased, the film formation uniformity between different pixel openings is improved, and the light-emitting layer of the display panel is formed more uniformly.
[0113] For example, in some embodiments, some sub-pixels need to be provided with maintenance sub-pixels (spare sub-pixels), for example, Figure 2 In comparison, in the related art, an area with four pixel openings SP of the same area requires eight pixel openings (four of which belong to maintenance sub-pixels). In the embodiment of the present application, a first barrier wall D2 is set between the normally displayed sub-pixels and the maintenance sub-pixels, so that the area of the pixel opening SP is twice that of the related art. The area of the pixel opening SP is increased, and the volume of the ink droplet required for one pixel opening SP is increased, which increases the allowable volume error of the ink droplet, thereby improving the film formation uniformity between different pixel openings and making the film formation of the light-emitting layer of the display panel more uniform.
[0114] For example, with the embodiment of the present application Figure 2In comparison, in the related art, for example, in a transparent display panel, the display panel includes a plurality of pixel areas PX and a plurality of transparent areas TR, one pixel area PX corresponds to at least one or two transparent areas TR (for example, the transparent area TR is arranged on one side or both sides of the pixel area PX), and one pixel area PX includes eight pixel openings, that is, eight pixel openings need to be set to correspond to one or two transparent areas TR (or other numbers). The related technology has at least the following disadvantages: 1) The area of the pixel opening is small, and the accuracy of the inkjet / printer needs to be improved, which will cause color bleeding and uneven printing; 2) During the printing process, the number of nozzles increases and the nozzle allocation time increases, resulting in an increase in printing process time; 3) The design of eight pixel openings (in a pixel unit, four normally displayed sub-pixels and four repair sub-pixels are set, and two sub-pixels of the same color are set. Before repair, the four normally displayed sub-pixels and the four repair sub-pixels are displayed normally. Compared with printing in columns, it is helpful to repair defects such as dark spots on the display panel. For example, when two sub-pixels of the same color are both dark spot defects, the defective sub-pixel can be found through repair, so that the defective sub-pixel is converted into a dark spot, and the other sub-pixel of the same color is displayed normally, and the color that can be displayed in the pixel unit is maintained) does not meet the printing requirements of some mass-produced printers, requires printing in rows, has a long printing cycle, and has many product defects (such as Mura). In some embodiments of the present application, two pixel openings of the same color in the related art are connected into one pixel opening SP through the first barrier wall D2, and two pixel openings of the same color in the related art are divided into a first sub-opening SP01 and a second sub-opening SP02 through the first barrier wall D2. In one pixel opening, or in the first sub-opening SP01 and the second sub-opening SP02, only one ink droplet needs to be sprayed / printed. Some embodiments of the present application have at least the following effects: 1) The accuracy of the inkjet / printer needs to be reduced, which improves the situation of color cross-talk and uneven printing; 2) The number of nozzles (Nozzles) is reduced during the printing process, and the nozzle allocation time is reduced, so that the printing process time is reduced; 3) The design of four pixel openings is more in line with the printing requirements of some mass-produced printers, and the printing cycle is reduced, which reduces the occurrence of product defects (such as Mura).
[0115] Wherein, in some embodiments, Fig.19 and Fig.21 As shown, the pixel defining layer De further includes a plurality of second retaining walls D3, and the pixel defining layer De does not include the first retaining wall D2. However, in some other embodiments, the pixel defining layer De may further include the first retaining wall D2.
[0116] For example, the side of the second blocking wall D3 away from the pixel opening SP is connected to the pixel defining structure D1, and the side of the second blocking wall D3 close to the pixel opening SP is toward the pixel opening SP, that is, the pixel defining structure D1 extends around the corresponding pixel opening SP, and the extension direction of the second blocking wall D3 is the same as the extension direction of the pixel defining structure D1.
[0117] For example, the side of the second blocking wall D3 away from the pixel opening SP is connected to the pixel defining structure D1, and the side of the second blocking wall D3 close to the pixel opening SP faces the pixel opening SP, that is, the side of the pixel defining structure D1 close to the pixel opening SP is connected to the side of the second blocking wall D3 away from the pixel opening SP, and the pixel defining structure D1 and the second blocking wall D3 form a step-like structure.
[0118] For example, compare Fig.21 and Fig.10 In some implementations, the fluorine concentration of the first end D111 is too low, resulting in poor liquid repellency of the first end D111 (for example, the fluorine concentration of the first end D111 is not easy to control, resulting in poor liquid repellency of the first end D111). For example, when the thickness of the light-emitting layer is thick and the volume of the ink droplets is large, the ink droplets or the light-emitting layer are prone to excessive climbing on the pixel-defining structure D1 due to the large first thickness h1 of the pixel-defining structure D1. In some embodiments of the present application, by setting the second retaining wall D3, the ink droplets or the light-emitting layer will not have a large climbing on the second retaining wall D3 due to the small third thickness h3 of the second retaining wall D3, thereby improving the film formation uniformity of the light-emitting layer. Further, when the second retaining wall D3 is made of a liquid-repellent material, the side surface of the second retaining wall D3 and the surface away from the substrate 11 are also liquid-repellent surfaces, thereby reducing the fluidity of the ink droplets on the surface of the second retaining wall D3 away from the substrate 11, thereby reducing or avoiding the climbing of the ink droplets on the pixel-defining structure D1 and the second retaining wall D3.
[0119] For example, in some embodiments of the present application, by simultaneously setting the pixel defining structure D1 and the second retaining wall D3 as liquid-repellent materials, on the one hand, it is possible to prevent ink droplets from overflowing into adjacent pixels SP after exceeding the pixel opening SP, thereby increasing the floating amount of ink droplets and avoiding color mixing problems; on the other hand, it is possible to improve uneven film formation problems such as climbing caused by uneven fluorine concentrations at various locations from the first end D111 to the second end D112 (for example, uneven film formation caused by uneven fluorine concentrations at different locations at the same height on the first surface D11 in a direction perpendicular to the plane where the substrate 11 is located); on the third hand, it reduces the fluidity of ink droplets on the surface of the second retaining wall D3 away from the substrate 11, thereby simultaneously reducing or avoiding the climbing of ink droplets on the pixel defining structure D1 and the second retaining wall D3. Therefore, by simultaneously setting the pixel defining structure D1 and the second retaining wall D3 as liquid-repellent materials, the uniformity of film formation of the light-emitting layer of the display panel is improved from multiple aspects.
[0120] Wherein, in some embodiments, Fig. 20 , Fig. 22 , Fig.23 and Fig.24 As shown, the pixel defining layer De further includes a plurality of first retaining walls D2 and a plurality of second retaining walls D3.
[0121] For example, the pixel defining layer De includes a pixel defining structure D1, a first retaining wall D2 and a second retaining wall D3, and the display substrate 1000 has the effects of the pixel defining structure D1, the first retaining wall D2 and the second retaining wall D3, for example, the film formation uniformity of the display substrate 1000 can be better improved.
[0122] In some embodiments of the present application, by setting the pixel defining structure D1 to a liquid-phobic material, it can be ensured that the ink droplet M01 flows within the corresponding pixel opening SP (flows between the pixel defining structures D1 surrounding the corresponding pixel opening SP), thereby preventing the ink droplet M01 from crossing the pixel defining structure D1 and entering the adjacent pixel opening SP, thereby avoiding the color mixing problem.
[0123] In some embodiments of the present application, by setting a first retaining wall D2, the second thickness h2 of the first retaining wall D2 is less than the first thickness h1 of the pixel defining structure D1, and the first retaining wall D2 replaces the pixel defining structure D1 originally set in the position, and the first sub-opening SP01 and the second sub-opening SP02 replace the two pixel openings of the related art, the area of the pixel opening SP is increased, and the volume of the ink droplets required for one pixel opening SP is increased, so that the volume error of the ink droplets is increased, the film formation uniformity between different pixel openings is improved, and the film formation of the light-emitting layer of the display panel is more uniform. In addition, the ink droplets are allowed to land randomly in a pixel opening, and then they can be fully mixed and evenly mixed. The larger pixel opening area increases the landing range of the ink droplets, improves the allowable landing accuracy of the ink droplets, reduces the risk of cross-color, reduces the accuracy requirements of the printer, and improves printing efficiency.
[0124] In some embodiments of the present application, by setting the first baffle D2, compared with the related art, the number of pixel openings required for inkjet printing is at least halved, the landing range of ink droplets is increased, the accuracy requirements of the printer are reduced, the printing efficiency of ink droplets is improved, and at the same time, color bleeding and other poor drying of ink droplets are reduced, thereby improving the display quality.
[0125] In some embodiments of the present application, in some implementation situations, the fluorine concentration at the first end D111 is too small, resulting in poor liquid repellency of the first end D111 (for example, the fluorine concentration at the first end D111 is not easy to control, resulting in poor liquid repellency of the first end D111). For example, when the thickness of the light-emitting layer is thicker and the volume of the ink droplets is larger, since the first thickness h1 of the pixel defining structure D1 is larger, the ink droplets or the light-emitting layer are prone to excessive climbing on the pixel defining structure D1. In some embodiments of the present application, by setting a second retaining wall D3, since the third thickness h3 of the second retaining wall D3 is smaller, the ink droplets or the light-emitting layer will not have a large climb on the second retaining wall D3 (the height of the side surface that can climb in the second retaining wall D3 is smaller), thereby improving the film formation uniformity of the light-emitting layer. Furthermore, when the second retaining wall D3 is made of a lyophobic material, since the side surface of the second retaining wall D3 and the surface away from the substrate 11 are also lyophobic surfaces, the fluidity of the ink droplets on the surface of the second retaining wall D3 away from the substrate 11 is reduced, thereby reducing or avoiding the climbing of the ink droplets on the pixel defining structure D1 and the second retaining wall D3.
[0126] In some embodiments of the present application, by simultaneously setting the pixel defining structure D1 and the second retaining wall D3 as liquid-repellent materials, on the one hand, it is possible to prevent ink droplets from overflowing into adjacent pixels SP after exceeding the pixel opening SP, thereby increasing the floating amount of ink droplets and avoiding color mixing problems; on the other hand, it is possible to improve uneven film formation problems such as climbing caused by uneven fluorine concentrations at various locations from the first end D111 to the second end D112 (for example, uneven film formation caused by uneven fluorine concentrations at different locations at the same height on the first surface D11 in a direction perpendicular to the plane where the substrate 11 is located); on the third hand, it reduces the fluidity of ink droplets on the surface of the second retaining wall D3 away from the substrate 11, thereby simultaneously reducing or avoiding the climbing of ink droplets on the pixel defining structure D1 and the second retaining wall D3. Therefore, by simultaneously setting the pixel defining structure D1 and the second retaining wall D3 as liquid-repellent materials, the uniformity of film formation of the light-emitting layer of the display panel is improved from multiple aspects.
[0127] In some embodiments of the present application, by simultaneously providing the pixel defining structure D1, the first retaining wall D2 and the second retaining wall D3, the display substrate 1000 simultaneously has the effects of the pixel defining structure D1, the first retaining wall D2 and the second retaining wall D3, for example, the film formation uniformity of the display substrate 1000 can be better improved.
[0128] In some embodiments, Figures 11 to 14As shown, in the case where a first retaining wall D2 is provided in at least one pixel opening SP, in the extension direction of the first retaining wall D2, the first retaining wall D2 includes a first sub-retaining wall portion D21 and a second sub-retaining wall portion D22 located on at least one side of the first sub-retaining wall portion D21, the first sub-retaining wall portion D21 is connected to the second sub-retaining wall portion D22, and in the direction perpendicular to the plane where the substrate 11 is located, the thickness of the first sub-retaining wall portion D21 is different from the thickness of the second sub-retaining wall portion D22.
[0129] For example, in a direction perpendicular to the plane where the substrate 11 is located, the thickness of the first sub-blocking wall portion D21 is different from the thickness of the second sub-blocking wall portion D22, that is, the distance from the surface of the first sub-blocking wall portion D21 away from the substrate 11 to the substrate 11 (or the first electrode AN) is different from the distance from the surface of the second sub-blocking wall portion D22 away from the substrate 11 to the substrate 11 (or the first electrode AN).
[0130] For example, when ink droplets of the light-emitting layer are sprayed into the pixel opening SP, for example, ink droplets of the light-emitting layer are sprayed into the first sub-opening SP01 or the second sub-opening SP02, setting the thickness of the first sub-blocking wall portion D21 to be different from the thickness of the second sub-blocking wall portion D22 can increase the diffusion / flow speed of the ink droplets at the second sub-blocking wall portion D22, so that the ink droplets are evenly diffused in the first sub-opening SP01 and the second sub-opening SP02, thereby improving the uniformity of film formation.
[0131] In some embodiments, Figures 11 to 14 As shown, in the extension direction of the first retaining wall D2, the first retaining wall D2 includes a first sub-retaining wall portion D21 and two second sub-retaining wall portions D22 located on both sides of the first sub-retaining wall portion D21, and the thickness of the first sub-retaining wall portion D21 is greater than the thickness of the second sub-retaining wall portion D22.
[0132] For example, Fig.11 As shown, in the extension direction of the first retaining wall D2, the first sub-retaining wall portion D21 occupies at least the middle portion (central portion) of the first retaining wall D2, and the two second sub-retaining wall portions D22 are on both sides of the first sub-retaining wall portion D21 (for example, the second sub-retaining wall portion D22 are the two end portions of the first retaining wall D2, for example, the second sub-retaining wall portion D22 contacts the pixel defining structure D1), that is, compared with the thickness of the first sub-retaining wall portion D21 being equal to the thickness of the second sub-retaining wall portion D22 (the closer to the edge of the pixel opening SP, the slower the diffusion speed of the ink of the light-emitting layer), when the thickness of the second sub-retaining wall portion D22 is less than the thickness of the first sub-retaining wall portion D21, the speed at which the ink droplets of the light-emitting layer diffuse / flow between the first sub-opening SP01 and the second sub-opening SP02 through the space on one side of the second sub-retaining wall portion D22 away from the substrate 11 is accelerated, so that the uniformity of the light-emitting layer between the edge portion and the middle portion (central portion) of the pixel opening SP is better.
[0133] In some embodiments, Fig.14 As shown, in the direction perpendicular to the plane where the base 11 is located, the thickness of the first sub-retaining wall portion D21 gradually decreases toward the second sub-retaining wall portion D22.
[0134] For example, in the extension direction of the first retaining wall D2 and in the direction in which the first sub-retaining wall portion D21 points to the pixel defining structure D1, the thickness of the first retaining wall D2 in the direction perpendicular to the plane where the substrate 11 is located gradually decreases.
[0135] For example, in the extension direction of the first retaining wall D2, the first sub-retaining wall portion D21 occupies the middle portion (center portion) of the first retaining wall D2, and the two second sub-retaining wall portions D22 are on both sides of the first sub-retaining wall portion D21 (for example, the second sub-retaining wall portion D22 are the two end portions of the first retaining wall D2, for example, the second sub-retaining wall portion D22 contacts the pixel defining structure D1), and the thickness of the first retaining wall D2 gradually decreases from the middle portion to the edge portion, which further adjusts the diffusion / flow speed of the ink droplets of the light-emitting layer at different portions, so that the uniformity of the light-emitting layer between various portions such as the edge portion of the pixel opening SP and the middle portion (center portion) is better.
[0136] In some embodiments, Fig.13 , Fig.14 As shown, the thickness of the first sub-retaining wall portion D21 is greater than the thickness of the second sub-retaining wall portion D22; the first retaining wall D2 includes a first sub-membrane layer 131, and a second sub-membrane layer 132 arranged on the side of the first sub-membrane layer 131 away from the substrate 11, the first sub-retaining wall portion D21 is composed of the first sub-membrane layer 131 and the second sub-membrane layer 132, and the second sub-retaining wall portion D22 is composed of the first sub-membrane layer 131.
[0137] For example, the first sub-membrane layer 131 and the second sub-membrane layer 132 are stacked in sequence on one side of the substrate 11, and the first sub-retaining wall portion D21 is formed by the first sub-membrane layer 131 and the second sub-retaining wall portion D22 is formed by the first sub-membrane layer 131, that is, the first sub-retaining wall portion D21 of the required thickness and the second sub-retaining wall portion D22 of the required thickness can be better formed by different layers of material membrane layers.
[0138] In some embodiments, Fig.13 , Fig.14 As shown, the first sub-film layer 131 is an inorganic material, and the second sub-film layer 132 is an organic material.
[0139] For example, the first sub-membrane layer 131 is an inorganic material, the second sub-retaining wall portion D22 is composed of the first sub-membrane layer 131, the second sub-membrane layer 132 is an organic material, and the first sub-retaining wall portion D21 is composed of the first sub-membrane layer 131 and the second sub-retaining wall portion D22, so that a suitable thickness difference is generated between the first sub-retaining wall portion D21 and the second sub-retaining wall portion D22.
[0140] For example, the film thickness of the inorganic material can be made relatively thin, for example, the film thickness of the inorganic material is 50 nanometers to 2000 nanometers, and the film thickness of the organic material is generally at least 300 nanometers. However, the organic material process has flow properties and a certain flattening effect. The second sub-film layer 132 located at the edge adopts a thinner inorganic material layer, which can better improve the flow distribution of ink droplets during ink droplet printing. The first sub-blocking wall portion D21 located in the middle adopts a thicker organic material layer (and the first sub-film layer 131), which is beneficial to the flatness of the first sub-blocking wall portion D21 away from the surface of the substrate 11 (making the flow speed of ink droplets in the middle part of the pixel opening SP consistent, which can better ensure the uniformity of film formation of the light-emitting layer in the middle part of the pixel opening SP). The drying process reduces the flow of ink droplets, thereby better improving the uniformity of the light-emitting layer near the middle part and the edge part of the first blocking wall D2.
[0141] In some embodiments, Figure 6 , Figure 7 As shown, in the case where the first barrier wall D2 is disposed in at least one pixel opening SP, the areas of the first sub-opening SP01 and the second sub-opening SP02 are different.
[0142] For example, the areas of the first sub-opening SP01 and the second sub-opening SP02 are different, and the ink droplets of the light-emitting layer can be sprayed into the larger one of the first sub-opening SP01 and the second sub-opening SP02 to avoid the ink droplets of the light-emitting layer from being sprayed onto the first baffle wall D2 and splashing of the ink droplets of the light-emitting layer, thereby preventing the ink droplets of the light-emitting layer from splashing outside the corresponding pixel opening SP, thereby improving the film formation uniformity of the light-emitting layer.
[0143] In some embodiments, Figure 6 , Figure 7 , Fig.10 As shown, in the case where a first barrier wall D2 is provided in at least one pixel opening SP, at least one of the following conditions is satisfied: the width of the pixel defining structure D1 is greater than the width of the first barrier wall D2; the first barrier wall D2 is provided away from the center point of the pixel opening SP; the area difference between the first sub-opening SP01 and the second sub-opening SP02 is greater than or equal to 10%.
[0144] For example, Fig.10As shown, the width of the pixel defining structure D1 means: in the extension direction perpendicular to the pixel defining structure D1, the width of the pixel defining structure D1 is the first width W1. The width of the first retaining wall D2 means: in the extension direction perpendicular to the first retaining wall D2, the width of the first retaining wall D2 is the second width W2.
[0145] For example, Fig.10 As shown, the first width W1 is greater than the second width W2, which can reduce the area occupied by the first blocking wall D2 in the pixel opening SP, help to increase the area of the pixel opening SP, increase the volume of the ink droplets in the light-emitting layer, and reduce the requirements for the accuracy of the ink droplet volume, thereby improving the uniformity of the film layer between different pixel openings SP.
[0146] For example, Figure 6 and Figure 7 As shown, the first baffle wall D2 is set to avoid the center point SPZ of the pixel opening SP, that is, the first baffle wall D2 does not overlap with the center point SPZ of the pixel opening SP; the ink droplets of the light-emitting layer can be sprayed at the center point SPZ or near the center point SPZ, so that the ink droplets in the pixel opening are evenly diffused or flowed to the surroundings, thereby improving the uniformity of film formation; at the same time, the first baffle wall D2 avoids the center point SPZ of the pixel opening SP, which can prevent the ink droplets of the light-emitting layer from being sprayed on the first baffle wall D2, and prevent the ink droplets of the light-emitting layer from splashing, thereby preventing the ink droplets of the light-emitting layer from splashing outside the corresponding pixel opening SP, thereby improving the uniformity of film formation of the light-emitting layer.
[0147] For example, Figure 6 and Figure 7 As shown, the area difference between the first sub-opening SP01 and the second sub-opening SP02 is greater than or equal to 10%, and the ink droplets are sprayed into the one with a larger area. The ink droplets flow to the other through the space on the surface of the first baffle wall D1 away from the substrate 11, so that the ink droplets can form a more uniform film in the first sub-opening SP01 and the second sub-opening SP02.
[0148] For example, Figure 2 and Figure 3 As shown, combined Figure 6 and Figure 7 The pixel defining structure D1 surrounding the pixel opening SP includes a first sub-pixel defining structure extending along a first direction Y, and a second sub-pixel defining structure extending along a second direction X, the first direction Y intersects with the second direction X, the length of the first sub-pixel defining structure is greater than the length of the second sub-pixel defining structure, and the first retaining wall D2 extends along the second direction, so that the first sub-opening SP01 and the second sub-opening SP02 of different areas can be better arranged, and the farthest distance of ink droplet diffusion / flow is reduced, so that the ink droplets can form a film more evenly in the first sub-opening SP01 and the second sub-opening SP02.
[0149] In some embodiments, Fig.15 , Fig.16 As shown, in the case where a first barrier wall D2 is provided in at least one pixel opening SP, the width of an end of the at least one first barrier wall D2 away from the substrate 11 is greater than the width of an end of the first barrier wall D2 close to the substrate 11; or / and, the width of an end of the at least one pixel defining structure D1 away from the substrate 11 is greater than the width of an end of the pixel defining structure D1 close to the substrate 11.
[0150] For example, in some embodiments, Fig.15 As shown, the width of the end of the first retaining wall D2 away from the substrate 11 is greater than the width of the end of the first retaining wall D2 close to the substrate 11, for example, the cross section of the first retaining wall D2 is in an inverted trapezoid. With this arrangement, when the thickness of the light-emitting layer is large and the volume of the ink droplets is large, the climbing of the ink droplets on the first retaining wall D2 can be reduced, so that the ink droplets can be more evenly filmed in the first sub-opening SP01 and the second sub-opening SP02. With this arrangement, the inverted trapezoidal first retaining wall D2 increases the resistance between the ink droplets and the first retaining wall D2 when the ink droplets flow during the drying process, increases the resistance of the ink droplets climbing to the first retaining wall D2, and can reduce the degree of the ink droplets flowing at the first retaining wall D2 during the drying process, thereby improving poor drying.
[0151] For example, in some other embodiments, Fig.16 As shown, the width of the end of the pixel defining structure D1 away from the substrate 11 is greater than the width of the end of the pixel defining structure D1 close to the substrate 11, for example, the cross section of the pixel defining structure D1 is an inverted trapezoid. Through this arrangement, when the thickness of the light-emitting layer is large and the volume of the ink droplets is large, the climbing of the ink droplets on the pixel defining structure D1 can be reduced, so that the ink droplets can be more evenly filmed at the edge of the pixel opening SP. Through this arrangement, the cross section of the pixel defining structure D1 is an inverted trapezoid. The inverted trapezoidal pixel defining structure D1 increases the resistance between the ink droplets and the pixel defining structure D1 when the ink droplets flow during the drying process, and increases the resistance of the ink droplets climbing toward the pixel defining structure D1, which can reduce the degree of the ink droplets flowing at the pixel defining structure D1 during the drying process, thereby improving poor drying. Furthermore, when the pixel defining structure D1 is a liquid-repellent material, the climbing of the ink droplets on the pixel defining structure D1 can be better avoided from both the structural and material properties of the pixel defining structure D1.
[0152] For example, in some other embodiments, please combine Fig.15 and Fig.16, the display substrate 1000 simultaneously satisfies: the width of at least one end of the first retaining wall D2 away from the substrate 11 is greater than the width of the end of the first retaining wall D2 close to the substrate 11; the width of at least one end of the pixel defining structure D1 away from the substrate 11 is greater than the width of the end of the pixel defining structure D1 close to the substrate 11.
[0153] In some embodiments, Fig.17 and Fig.18 As shown, in the case where a first retaining wall D2 is provided in at least one pixel opening SP, the display substrate 1000 further includes a first electrode layer provided between the substrate 11 and the pixel defining layer De, the first electrode layer includes a plurality of first electrodes AN arranged in an array, and the pixel opening SP exposes the corresponding first electrode AN; the first electrode AN includes a first sub-electrode AN01, a second sub-electrode AN02 and a spacer AN12X, the first sub-electrode AN01 and the second sub-electrode AN02 are provided on both sides of the spacer AN12X to be spaced apart, and in the pixel opening SP, the orthographic projection of the first retaining wall D2 on the substrate 11 covers the orthographic projection of the spacer AN12X on the substrate 11 ( Fig.17 The mark in the middle indicates the edge of the orthographic projection of the first retaining wall D2 on the base 11).
[0154] For example, Fig.17 and Fig.18 As shown, the first sub-pixel opening SP01 exposes the first sub-electrode AN01 , and the second sub-pixel opening SP02 exposes the second sub-electrode AN02 .
[0155] For example, in some embodiments, the first sub-electrode AN01 and the second sub-electrode AN02 are electrically connected to the same thin film transistor or pixel driving circuit, and the first sub-electrode AN01 and the second sub-electrode AN02 are driven or supplied with electrical signals by the same pixel driving circuit, which can facilitate the maintenance of the display substrate 1000. For example, the first sub-electrode AN01 fails and becomes a bright spot, and the first sub-electrode AN01 is transformed into a dark spot that is not easily observed through a maintenance process.
[0156] For example, in some embodiments, the first sub-electrode AN01 is a pixel electrode of a normal display sub-pixel, and the second sub-electrode AN02 is a pixel electrode of a maintenance sub-pixel (spare sub-pixel), but is not limited thereto.
[0157] For example, the manufacturing method of some embodiments of the present application may include: S100, forming an array substrate with a driving circuit on one side of the substrate 11 by a patterning process such as exposure; S200, forming a first electrode layer on the array substrate, the first electrode layer including a plurality of first electrodes AN arranged in an array, the first electrode AN including a first sub-electrode AN01, a second sub-electrode AN02 and a spacer AN12X, the first sub-electrode AN01 and the second sub-electrode AN02 are arranged on both sides of the spacer AN12X to be spaced apart; S300, forming an image on the side of the first electrode layer away from the substrate The pixel defining structure D1 of the pixel defining layer De is made of a liquid-repellent material, and the pixel defining structure D1 defines a plurality of pixel openings SP, and the pixel openings SP expose the corresponding first electrodes AN; S400, a first retaining wall D2 of the pixel defining layer De is formed on the side of the first electrode layer away from the substrate, and the first retaining wall D2 is made of a liquid-philic material, and the first retaining wall D2 divides the pixel opening SP into a first sub-opening SP01 and a second sub-opening SP02; S500, printing / jetting ink droplets to form a light-emitting layer; S600, forming a second electrode on the side of the light-emitting layer away from the substrate 11. The order of step S300 and step S400 can be reversed.
[0158] It should be noted that, in some other embodiments, the first sub-electrode AN01 and the second sub-electrode AN02 are directly connected via a connecting electrode, and the connecting electrode is arranged in the same layer as the first sub-electrode AN01 and the second sub-electrode AN02 and is made of the same material, so that sub-pixels can also be repaired. For example, in a pixel unit, two sub-pixels of the same color are arranged, and the two sub-pixels are displayed normally before repair. When two sub-pixels of the same color have dark spot defects, the defective sub-pixel can be found through repair, and the connecting electrode is cut off through a laser process, so that the defective sub-pixel is converted into a dark spot, and the other sub-pixel of the same color is displayed normally, and the color that can be displayed in the pixel unit is maintained.
[0159] It should be noted that in the above embodiment, the material of the light-emitting layer of the sub-pixel of the same color is set in a pixel opening SP as an example, that is, the material of the light-emitting layer of the sub-pixel of the same color is set in the first sub-opening SP01 and the second sub-opening SP02 as an example (for example, the light-emitting material layer EML of the same color is set in the first sub-opening SP01 and the second sub-opening SP02). For example, the material of the red light-emitting layer is set in the first sub-opening SP01 and the second sub-opening SP02 of a pixel opening SP.
[0160] It should be noted that the pixel definition structure D1 includes a long side and a short side. Figure 2 and Figure 3 FIG. 4 shows that the first retaining wall D2 extends parallel to the short side, which can improve the fluidity of the ink droplets between the first sub-opening SP01 and the second sub-opening SP02. Figure 4 FIG. 2 shows that the first retaining wall D2 extends parallel to the long side. Figure 5 FIG. 4 shows that the first barrier wall D2 extends between two diagonal corners of the pixel opening SP. In a pixel region PX, the extension directions of the first barrier walls D2 in different pixel openings SP may intersect. Figure 6 FIG. 4 shows that the first barrier wall D2 extends between two diagonal corners of the pixel opening SP. In a pixel region PX, the extension directions of the first barrier walls D2 in different pixel openings SP are parallel.
[0161] It should be noted that Figure 2 and Figure 3 , it is illustrated that the plurality of pixel openings SP of the display substrate 1000 may include a first color pixel opening SP1, a second color pixel opening SP2, a third color pixel opening SP3, and a fourth color pixel opening SP4. In some examples, the first color pixel opening SP1, the second color pixel opening SP2, the third color pixel opening SP3, and the fourth color pixel opening SP4 may be an opening of a red sub-pixel, an opening of a green sub-pixel, an opening of a green sub-pixel, and an opening of a blue sub-pixel, respectively, but not limited thereto. The first color pixel opening SP1, the second color pixel opening SP2, the third color pixel opening SP3, and the fourth color pixel opening SP4 each include a first sub-opening SP01 and a second sub-opening SP02, respectively.
[0162] It should be noted that compared with Figure 3 , Figure 2 It is also shown that the display panel includes a plurality of transparent regions TR, and the display substrate 1000 is used for a transparent display panel. Therefore, various embodiments of the present application can be used for a non-transparent display panel or a transparent display panel.
[0163] It should be noted that in a transparent display panel, a transparent area TR or a transparent sub-pixel needs to be set. The transparent area TR or the transparent sub-pixel further occupies the area of the pixel opening SP, thereby reducing the area of the pixel opening SP. Through any display substrate in the present application, in a transparent display panel, the effect of improving the uniformity of film formation of the light-emitting layer is particularly prominent.
[0164] It should be noted that in Figure 2 In the embodiment, a transparent region TR is located at one side of the pixel region PX, and another transparent region TR is located at the other side of the pixel region PX. The pixel region PX includes a first color pixel opening SP1, a second color pixel opening SP2, a third color pixel opening SP3, and a fourth color pixel opening SP4.
[0165] It should be noted that compared with Figure 2 , Figure 7 The display substrate does not include a fourth color pixel opening. Figure 7Among them, the first-color pixel opening SP1, the second-color pixel opening SP2, the third-color pixel opening SP3, and the transparent region TR are arranged in a "field" character array. However, the arrangement of the pixel openings SP in the display substrate is not limited to this.
[0166] It should be noted that, compared with Figure 7 , Figure 8 in which the first-color pixel opening SP1, the second-color pixel opening SP2, the third-color pixel opening SP3, and the transparent region TR are arranged in the same direction.
[0167] It should be noted that Figure 7 and Figure 8 schematically show that the display substrate includes the first-color pixel opening SP1, the second-color pixel opening SP2, and the third-color pixel opening SP3. The first-color pixel opening SP1, the second-color pixel opening SP2, and the third-color pixel opening SP3 can be the openings of red sub-pixels, green sub-pixels, and blue sub-pixels respectively, but are not limited to this.
[0168] It should be noted that in some embodiments, the pixel opening SP is divided into a first sub-opening SP01 and a second sub-opening SP02. The materials of the light-emitting layers in the first sub-opening SP01 and the second sub-opening SP02 are of the same color, or the first sub-opening SP01 and the second sub-opening SP02 are pixel openings of the same color.
[0169] It should be noted that in some embodiments, the pixel opening SP is divided into a first sub-opening SP01 and a second sub-opening SP02. The first sub-opening SP01 and the second sub-opening SP02 of a pixel opening SP are the same sub-pixel.
[0170] It should be noted that Figures 2 to 8 in which it is exemplified that both ends of the first barrier D2 are in contact with the pixel defining structure D1, but are not limited to this.
[0171] Please refer to Figure 25 to Figure 27 , Fig.25 which is a top view schematic diagram of the eleventh partial structure of a display substrate provided by an embodiment of the present application; Fig.26 which is a top view schematic diagram of the twelfth partial structure of a display substrate provided by an embodiment of the present application; Fig. 27 which is a top view schematic diagram of the thirteenth partial structure of a display substrate provided by an embodiment of the present application.
[0172] In Figure 25 to Figure 27In the pixel region PX, there are a first color pixel opening SP1, a second color pixel opening SP2, a third color pixel opening SP3, and a fourth color pixel opening SP4. The first color pixel opening SP1 and the second color pixel opening SP2 are arranged along a third direction W. The third color pixel opening SP3 and the fourth color pixel opening SP4 are arranged along the third direction W. The first color pixel opening SP1 and the third color pixel opening SP3 are arranged along a fourth direction V. The second color pixel opening SP2 and the fourth color pixel opening SP4 are arranged along the fourth direction V. The third direction W intersects with the fourth direction V (for example, the third direction W is perpendicular to the fourth direction V). The first color pixel opening SP1, the second color pixel opening SP2, the third color pixel opening SP3, and the fourth color pixel opening SP4 are arranged in a "field" shape.
[0173] In Fig.25 In it, the first barrier D2 disposed in the first color pixel opening SP1 has the same extending direction as the first barrier D2 disposed in the second color pixel opening SP2. The first barrier D2 in the first color pixel opening SP1 connects a vertex of its pixel opening SP. The first barrier D2 in the second color pixel opening SP2 connects a vertex of its pixel opening. The extending direction of the first barrier D2 disposed in the first color pixel opening SP1 overlaps with the extending direction of the first barrier D2 disposed in the second color pixel opening SP2. The first barrier D2 disposed in the third color pixel opening SP3 has the same extending direction as the first barrier D2 disposed in the fourth color pixel opening SP4. The first barrier D2 in the third color pixel opening SP3 connects a vertex of its pixel opening. The first barrier D2 in the fourth color pixel opening SP2 connects a vertex of its pixel opening. The extending direction of the first barrier D2 disposed in the third color pixel opening SP3 overlaps with the extending direction of the first barrier D2 disposed in the fourth color pixel opening SP4. The extending direction of the first barrier D2 disposed in the first color pixel opening SP1 is parallel to the extending direction of the first barrier D2 disposed in the third color pixel opening SP3.
[0174] In Fig.26In the embodiment, the first barrier wall D2 disposed in the first color pixel opening SP1 has the same extension direction as the first barrier wall D2 disposed in the third color pixel opening SP3, the first barrier wall D2 disposed in the first color pixel opening SP1 connects to a vertex of its pixel opening, the first barrier wall D2 disposed in the third color pixel opening SP3 connects to a vertex of its pixel opening, and the extension direction of the first barrier wall D2 disposed in the first color pixel opening SP1 overlaps with the extension direction of the first barrier wall D2 disposed in the third color pixel opening SP3. The first barrier wall D2 disposed in the second color pixel opening SP2 has the same extension direction as the first barrier wall D2 disposed in the fourth color pixel opening SP4, the first barrier wall D2 disposed in the second color pixel opening SP2 connects to a vertex of its pixel opening, the first barrier wall D2 disposed in the fourth color pixel opening SP2 connects to a vertex of its pixel opening, and the extension direction of the first barrier wall D2 disposed in the second color pixel opening SP2 overlaps with the extension direction of the first barrier wall D2 disposed in the fourth color pixel opening SP4. The first barrier wall D2 disposed in the first color pixel opening SP1 is parallel to the extension direction of the first barrier wall D2 disposed in the second color pixel opening SP2.
[0175] exist Fig. 27 In the embodiment, the first barrier wall D2 disposed in the first color pixel opening SP1 has the same extension direction as the first barrier wall D2 disposed in the third color pixel opening SP3, the first barrier wall D2 disposed in the first color pixel opening SP1 is connected to a vertex corner of its pixel opening, the first barrier wall D2 disposed in the third color pixel opening SP3 is connected to a vertex corner of its pixel opening, and the extension direction of the first barrier wall D2 disposed in the first color pixel opening SP1 overlaps with the extension direction of the first barrier wall D2 disposed in the third color pixel opening SP3. The first barrier wall D2 disposed in the second color pixel opening SP2 has the same extension direction as the first barrier wall D2 disposed in the fourth color pixel opening SP4, the first barrier wall D2 disposed in the second color pixel opening SP2 is connected to a vertex corner of its pixel opening, the first barrier wall D2 disposed in the fourth color pixel opening SP2 is connected to a vertex corner of its pixel opening, and the extension direction of the first barrier wall D2 disposed in the second color pixel opening SP2 overlaps with the extension direction of the first barrier wall D2 disposed in the fourth color pixel opening SP4. The first blocking wall D2 disposed in the first color pixel opening SP1 and the first blocking wall D2 disposed in the second color pixel opening SP2 have their extension directions intersecting.
[0176] In some embodiments, Figures 19 to 24 As shown, in the case where a second barrier wall D3 is provided in at least one pixel opening SP, in at least one pixel opening SP, the second barrier wall D3 is attached to the pixel defining structure D1 to form a first opening SP-1, and the orthographic projection of the first opening SP-1 on the substrate 11 is located within the orthographic projection of the pixel opening SP on the substrate 11.
[0177] For example, in some implementations, the fluorine concentration at the first end D111 is too small, resulting in poor liquid repellency of the first end D111 (for example, the fluorine concentration at the first end D111 is not easy to control, resulting in poor liquid repellency of the first end D111). For example, when the thickness of the light-emitting layer is thicker and the volume of the ink droplets is larger, since the first thickness h1 of the pixel-defining structure D1 is larger, the ink droplets or the light-emitting layer are prone to excessive climbing on the pixel-defining structure D1. In some embodiments of the present application, by setting a second retaining wall D3, since the third thickness h3 of the second retaining wall D3 is smaller, the ink droplets or the light-emitting layer will not have a large climb on the second retaining wall D3 (the height of the side surface that can climb in the second retaining wall D3 is smaller), thereby improving the film formation uniformity of the light-emitting layer. Furthermore, when the second retaining wall D3 is made of a lyophobic material, since the side surface of the second retaining wall D3 and the surface away from the substrate 11 are also lyophobic surfaces, the fluidity of the ink droplets on the surface of the second retaining wall D3 away from the substrate 11 is reduced, thereby reducing or avoiding the climbing of the ink droplets on the pixel defining structure D1 and the second retaining wall D3.
[0178] For example, in some embodiments, the second retaining wall D3 is a closed annular structure to form the first opening SP-1.
[0179] In some embodiments, Fig.24 As shown, in the case where a second retaining wall D3 is provided in at least one pixel opening SP, the edge of the second retaining wall D3 on the side away from the nearest pixel defining structure D1 has a first climbing portion PA1, and the slope angle θ of the first climbing portion PA1 is 40 degrees to 50 degrees, and the slope angle θ is the angle between the tangent of the first climbing portion PA1 and the plane parallel to the substrate 11.
[0180] For example, the edge of the second barrier wall D3 away from the nearest pixel defining structure D1 has the first climbing portion PA1, which means that the edge of the second barrier wall D3 away from the pixel defining structure D1 it contacts has the first climbing portion PA1.
[0181] For example, the slope angle θ of the first climbing portion PA1 may be any value among 40 degrees, 42 degrees, 45 degrees, 48 degrees and 50 degrees.
[0182] For example, the slope angle θ of the first climbing portion PA1 is 40 to 50 degrees, which can make the ink droplets form a film layer of the light-emitting layer with uniform thickness at the edge of the first opening SP-1. After verification by the inventor, when the slope angle θ of the first climbing portion PA1 is too small (when the slope angle θ of the first climbing portion PA1 is less than 40 degrees), the ink droplets are prone to climb too much on the first climbing portion PA1, resulting in uneven film formation at the edge of the first opening SP-1. After verification by the inventor, when the slope angle θ of the first climbing portion PA1 is too large (when the slope angle θ of the first climbing portion PA1 is greater than 50 degrees), the ink droplets MO1 of the light-emitting layer are prone to poor wetting (De-Weeting) at the edge of the pixel defining structure D1, such as the shrinkage of some sub-film layers of the light-emitting layer. Too large a slope angle θ will also lead to a decrease in light extraction efficiency. After verification by the inventor, when the slope angle θ of the first climbing portion PA1 is 40 to 50 degrees, it is more conducive to the uniformity of the film formation of the light-emitting layer, while maintaining a high light extraction efficiency.
[0183] In some embodiments, Fig. 20 , Fig. 22 , Fig.23 and Fig.24 As shown, the pixel defining layer De includes multiple first retaining walls D2 and multiple second retaining walls D3, and the display substrate 1000 satisfies at least one of the following conditions: the pixel defining structure D1, the first retaining wall D2 and the second retaining wall D3 are connected to form a continuous structure; the third thickness h3 is less than or equal to the second thickness h2.
[0184] For example, the pixel defining layer De also includes a plurality of first retaining walls D2 and a plurality of second retaining walls D3. The pixel defining structure D1, the first retaining walls D2 and the second retaining walls D3 are connected to form a continuous structure, so that the ink droplets of the light-emitting layer can be evenly diffused in various parts of the first opening SP-1, which is conducive to uniform film formation. Fig. 22 As shown, the first retaining wall D2 and the second retaining wall D3 may both be in contact with the pixel defining structure D1, and the second retaining wall D3 is disposed on a side of the first retaining wall D2 away from the substrate 11. Fig.23 As shown, the second retaining wall D3 may be connected between the pixel defining structure D1 and the first retaining wall D2.
[0185] For example, the pixel defining layer De also includes a plurality of first retaining walls D2 and a plurality of second retaining walls D3, the second thickness h2 is less than the first thickness h1, and the third thickness h3 is less than or equal to the second thickness h2, so that the pixel defining structure D1 plays a role in defining the pixel opening SP, the first retaining wall D2 plays a role in dividing the second sub-opening SP01 and the second sub-opening SP02, and plays a role in making the light-emitting layer film-formed uniformly, and the second retaining wall D3 plays a role in making the light-emitting layer film-formed uniformly at various locations on the edge of the first opening SP-1. Through the joint action of the pixel defining structure D1, the first retaining wall D2 and the second retaining wall D3, the ink droplets of the light-emitting layer are uniformly filmed at various locations in the pixel opening SP, and the ink droplets of the light-emitting layer are uniformly filmed between different pixel openings SP.
[0186] It should be noted that, in some embodiments, Fig.24 As shown, in the extension direction perpendicular to the pixel defining structure D1, the width of the pixel defining structure D1 is a first width W1; in the extension direction perpendicular to the second retaining wall D3, the width of the second retaining wall D3 is a third width W3; the third width W3 is smaller than the first width W1, which can prevent the second retaining wall D3 from occupying too much area of the pixel opening PS and increase the area of the first opening SP-1.
[0187] In some embodiments, Fig. 20 , Fig. 22 , Fig.23 and Fig.24 As shown, the display substrate 1000 satisfies at least one of the following conditions: when a first barrier wall D2 is provided in at least one pixel opening SP, a ratio of the first thickness h1 to the second thickness h2 is greater than or equal to 3 and less than or equal to 6; when a second barrier wall D3 is provided in at least one pixel opening SP, a ratio of the second thickness h2 to the third thickness is greater than or equal to 1 and less than or equal to 1.5.
[0188] For example, the inventors have verified that the ratio of the first thickness h1 to the second thickness h2 is greater than or equal to 3 and less than or equal to 6. For example, the ratio of the first thickness h1 to the second thickness h2 can be any value of 3, 3.5, 4, 4.5, 5, 5.5 and 6. The first thickness h1 matches the thickness of the light-emitting layer, and the pixel defining structure D1 and the first retaining wall D2 can each play the corresponding effects mentioned above, so that the light-emitting layer is formed more uniformly.
[0189] For example, the inventors have verified that the ratio of the second thickness h2 to the third thickness is greater than or equal to 1 and less than or equal to 1.5. For example, the ratio of the second thickness h2 to the third thickness can be any value of 1, 1.1, 1.2, 1.3, 1.4 and 1.5. The first retaining wall D2 and the second retaining wall D3 can each play the corresponding effects mentioned above, so that the light-emitting layer is formed more uniformly.
[0190] For example, in some embodiments, the first thickness h1 is 1 micrometer to 1.2 micrometers. For example, the first thickness h1 may be any value among 1 micrometer, 1.05 micrometers, 1.1 micrometers, 1.15 micrometers, and 1.2 micrometers.
[0191] For example, in some embodiments, the second thickness h2 is 0.2 to 0.5 micrometers. For example, the second thickness h2 may be any value among 0.2 micrometers, 0.3 micrometers, and 0.4 micrometers.
[0192] For example, in some embodiments, the third thickness h3 is 0.1 to 0.3 micrometers. For example, the third thickness h3 may be any value of 0.1 micrometers, 0.15 micrometers, 0.2 micrometers, 0.25 micrometers, and 0.3 micrometers.
[0193] In some embodiments, the display substrate 1000 satisfies at least one of the following conditions: when a first retaining wall D2 is provided in at least one pixel opening SP, the pixel defining structure D1 is a liquid-repellent material, and the first retaining wall D2 is a liquid-philic material; when a second retaining wall D3 is provided in at least one pixel opening SP, the pixel defining structure D1 is a liquid-repellent material, and the second retaining wall D3 is a liquid-repellent material.
[0194] For example, in some embodiments, the pixel defining structure D1 is a lyophobic material, which can effectively limit the overflow of ink droplets, preventing the ink droplets from overflowing into adjacent pixels SP after exceeding the pixel opening SP, thereby increasing the floating amount of the ink droplets and improving the uniformity of film formation.
[0195] For example, in some embodiments, the first retaining wall D2 is made of a lyophilic material, which allows the ink droplets to flow on the side of the first retaining wall D2 away from the substrate 11, making it easier for the ink droplets to flow between the first sub-opening SP01 and the second sub-opening SP02, thereby improving film formation uniformity.
[0196] For example, in some embodiments, the second retaining wall D3 is made of a liquid-phobic material. Since the side surface of the second retaining wall D3 and the surface away from the substrate 11 are also liquid-phobic surfaces, the fluidity of the ink droplets on the surface of the second retaining wall D3 away from the substrate 11 is reduced, thereby reducing or avoiding the climbing of the ink droplets on the pixel defining structure D1 and the second retaining wall D3.
[0197] Illustratively, the lyophilic material may include polyimide, acrylic, or epoxy resin, but is not limited thereto.
[0198] Illustratively, the lyophobic material may include fluorine-containing polyimide, fluorine-containing acrylic, or fluorine-containing epoxy resin, but is not limited thereto.
[0199] Wherein, for example, in some embodiments, Fig. 22 As shown, a first retaining wall D2 and a second retaining wall D3 may be provided simultaneously in at least one pixel opening SP. At the connection between the first retaining wall D2 and the second retaining wall D3, when the second retaining wall D3 is made of a liquid-repellent material, the second retaining wall D3 is provided on the side of the first retaining wall D2 away from the substrate 11, so that the second retaining wall D3 at the connection serves to limit the overflow of ink droplets, thereby preventing the ink droplets from exceeding the first opening SP-1 and causing excessive climbing, thereby increasing the floating amount of the ink droplets and improving the uniformity of film formation.
[0200] It should be noted that in some of the above embodiments, the case where a first barrier wall D2 is provided in at least one pixel opening SP is used as an example for explanation; in some of the above embodiments, the case where a second barrier wall D3 is provided in at least one pixel opening SP is used as an example for explanation; in other implementations, the first barrier wall D2 and the second barrier wall D3 may be provided in at least one pixel opening SP at the same time.
[0201] It should be noted that, in some other embodiments, the second retaining wall D3 is made of a liquid-philic material. When the thickness of the light-emitting layer is small (for example, the number of sub-film layers in the light-emitting layer is small), the volume of the ink droplets is small, which can avoid poor wetting (De-Weeting) of the ink droplets MO1 of the light-emitting layer at the edge of the pixel defining structure D1. For example, it can avoid the shrinkage of some sub-film layers of the light-emitting layer, thereby improving the problem of uneven film formation of the light-emitting layer of the display panel.
[0202] It should be noted that in some other embodiments, Fig.23 As shown, a first barrier wall D2 and a second barrier wall D3 may be provided simultaneously in at least one pixel opening SP. At the connection between the first barrier wall D2 and the second barrier wall D3, when the second barrier wall D3 is made of a liquid-philic material, the second barrier wall D3 may be provided on the side of the first barrier wall D2 away from the substrate 11, or the first barrier wall D2 may be provided on the side of the second barrier wall D3 away from the substrate 11, or the second barrier wall D3 may be provided to be connected between the pixel defining structure D1 and the first barrier wall D2. At this time, when the thickness of the light-emitting layer is small (for example, when the number of sub-film layers in the light-emitting layer is small), the volume of the ink droplets is small, and poor wetting (De-Weeting) of the ink droplets MO1 of the light-emitting layer at the edge of the pixel defining structure D1 can be avoided, for example, the shrinkage of some sub-film layers of the light-emitting layer can be avoided, thereby improving the problem of uneven film formation of the light-emitting layer of the display panel.
[0203] It should be noted that in some other embodiments, Fig.23 As shown, when the second retaining wall D3 is made of a lyophilic material, the second retaining wall D3 and the first retaining wall D2 can be made of the same material and can be formed by the same process. In a pixel opening SP, the second retaining wall D3 and the first retaining wall D2 can be an integrally formed structure.
[0204] On the other hand, the present application provides a display substrate 1000, which includes a substrate 11 and a pixel defining layer De arranged on one side of the substrate 11, the pixel defining layer De includes a plurality of pixel defining structures D1, and a plurality of pixel openings SP defined by the pixel defining structures D1; wherein, the pixel defining layer De also includes a plurality of first retaining walls D2, at least one pixel opening SP is provided with a first retaining wall D2, the first retaining wall D2 divides the pixel opening SP into a first sub-opening SP01 and a second sub-opening SP02, in a direction perpendicular to the plane where the substrate 11 is located, the thickness of the pixel defining structure D1 is a first thickness h1, the thickness of the first retaining wall D2 is a second thickness h2, and the second thickness h2 is less than the first thickness h1; wherein, the areas of the first sub-opening SP01 and the second sub-opening SP02 are different.
[0205] For example, the areas of the first sub-opening SP01 and the second sub-opening SP02 are different, and the ink droplets of the light-emitting layer can be sprayed into the larger one of the first sub-opening SP01 and the second sub-opening SP02 to avoid the ink droplets of the light-emitting layer from being sprayed onto the first baffle wall D2 and splashing of the ink droplets of the light-emitting layer, thereby preventing the ink droplets of the light-emitting layer from splashing outside the corresponding pixel opening SP, thereby improving the film formation uniformity of the light-emitting layer.
[0206] For example, the first sub-opening SP01 and the second sub-opening SP02 have different areas. The display substrate 1000 may also have any other features of the above embodiments, which will not be described in detail herein.
[0207] The present application also provides a display panel, which includes the display substrate 1000 of any one of the above items, or the display panel includes the display substrate 1000 having any combination of the above features.
[0208] The present application also provides a display device, which includes the display panel described above, or includes the display substrate 1000 of any one of the above, or includes the display substrate 1000 combining any of the above features.
[0209] For example, the display device may be a mobile phone, a laptop computer, a television, etc., but is not limited thereto.
[0210] It should be noted that in the above embodiments, the description of each embodiment has its own emphasis, and for parts that are not described in detail in a certain embodiment, reference can be made to the relevant descriptions of other embodiments.
[0211] The above embodiments are only used to illustrate the technical solutions of the present application, rather than to limit them. Although the present application has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or make equivalent replacements for some of the technical features therein. However, these modifications or replacements do not deviate the essence of the corresponding technical solutions from the spirit and scope of the technical solutions of the embodiments of the present application.
[0212] Although the preferred embodiments of this specification have been described, those skilled in the art may make additional changes and modifications to these embodiments once they have learned the basic creative concept. Therefore, the appended claims are intended to be interpreted as including the preferred embodiments and all changes and modifications that fall within the scope of this specification.
[0213] Obviously, those skilled in the art can make various changes and modifications to this specification without departing from the spirit and scope of this specification. Thus, if these modifications and variations of this specification fall within the scope of the claims of this specification and their equivalents, this specification is also intended to include these modifications and variations.
Claims
1. A display substrate, It is characterized in that It comprises a substrate, and a pixel defining layer arranged on one side of the substrate, wherein the pixel defining layer comprises a plurality of pixel defining structures, and a plurality of pixel openings defined by the pixel defining structures; The material of the pixel defining structure includes fluorine element, and the side surface of the pixel defining structure facing the pixel opening has a gradual fluorine concentration along a direction perpendicular to the plane where the substrate is located, and in the side surface of the pixel defining structure, the fluorine concentration at one end close to the substrate is less than the fluorine concentration at one end away from the substrate.
2. The display substrate according to claim 1, It is characterized in that In the side surface of the pixel defining structure, a ratio of a fluorine concentration at an end close to the substrate to a fluorine concentration at an end far from the substrate is 0 to 0.
3.
3. The display substrate according to claim 1, It is characterized in that The pixel defining layer further includes a plurality of first retaining walls, at least one of the pixel openings is provided with the first retaining wall, the first retaining wall divides the pixel opening into a first sub-opening and a second sub-opening, in a direction perpendicular to the plane where the substrate is located, the thickness of the pixel defining structure is a first thickness, the thickness of the first retaining wall is a second thickness, and the second thickness is less than the first thickness; or / and The pixel defining layer also includes a plurality of second retaining walls, wherein the second retaining wall is disposed in at least one of the pixel openings, and the side of the second retaining wall away from the pixel opening is connected to the pixel defining structure, and the side of the second retaining wall close to the pixel opening faces the pixel opening, and in a direction perpendicular to the plane where the substrate is located, the thickness of the second retaining wall is a third thickness, and the third thickness is less than the first thickness.
4. The display substrate according to claim 3, It is characterized in that In the case where the first retaining wall is provided in at least one of the pixel openings, in the extension direction of the first retaining wall, the first retaining wall includes a first sub-retaining wall portion and a second sub-retaining wall portion located on at least one side of the first sub-retaining wall portion, the first sub-retaining wall portion is connected to the second sub-retaining wall portion, and in the direction perpendicular to the plane where the substrate is located, the thickness of the first sub-retaining wall portion is different from the thickness of the second sub-retaining wall portion.
5. The display substrate according to claim 4, It is characterized in that In the extension direction of the first retaining wall, the first retaining wall includes the first sub-retaining wall portion and two second sub-retaining wall portions located on both sides of the first sub-retaining wall portion, and the thickness of the first sub-retaining wall portion is greater than that of the second sub-retaining wall portion.
6. The display substrate according to claim 5, It is characterized in that With respect to the thickness in a direction perpendicular to the plane where the base is located, the thickness of the first sub-retaining wall portion gradually decreases toward the second sub-retaining wall portion.
7. The display substrate according to claim 4, It is characterized in that The thickness of the first sub-retaining wall portion is greater than the thickness of the second sub-retaining wall portion; The first retaining wall includes a first sub-membrane layer and a second sub-membrane layer arranged on a side of the first sub-membrane layer away from the substrate. The first sub-retaining wall portion is composed of the first sub-membrane layer and the second sub-membrane layer, and the second sub-retaining wall portion is composed of the first sub-membrane layer.
8. The display substrate according to claim 7, It is characterized in that The first sub-film layer is made of inorganic material, and the second sub-film layer is made of organic material.
9. The display substrate according to any one of claims 3 to 8, It is characterized in that In the case where the first barrier wall is disposed in at least one of the pixel openings, the first sub-opening and the second sub-opening have different areas.
10. The display substrate according to any one of claims 3 to 8, It is characterized in that In the case where the first barrier wall is disposed in at least one of the pixel openings, at least one of the following conditions is satisfied: The width of the pixel defining structure is greater than the width of the first retaining wall; The first retaining wall is arranged away from the center point of the pixel opening; A difference in area between the first sub-opening and the second sub-opening is greater than or equal to 10%.
11. The display substrate according to any one of claims 3 to 8, It is characterized in that In the case where the first barrier wall is disposed in at least one of the pixel openings, a width of an end of the at least one of the first barrier walls away from the substrate is greater than a width of an end of the first barrier wall close to the substrate; or / and The width of at least one end of the pixel definition structure away from the substrate is greater than the width of the end of the pixel definition structure close to the substrate.
12. The display substrate according to any one of claims 3 to 8, It is characterized in that In the case where the first barrier wall is disposed in at least one of the pixel openings, the display substrate further comprises a first electrode layer disposed between the base and the pixel defining layer, the first electrode layer comprising a plurality of first electrodes arranged in an array, and the pixel opening exposes the corresponding first electrode; The first electrode includes a first sub-electrode, a second sub-electrode and a spacer, the first sub-electrode and the second sub-electrode are arranged on both sides of the spacer to be spaced apart, and within the pixel opening, the orthographic projection of the first blocking wall on the substrate covers the orthographic projection of the spacer on the substrate.
13. The display substrate according to claim 3, It is characterized in that In the case where the second retaining wall is provided in at least one of the pixel openings, in the at least one of the pixel openings, the second retaining wall is attached to the pixel defining structure to form a first opening, and the orthographic projection of the first opening on the substrate is located within the orthographic projection of the pixel opening on the substrate.
14. The display substrate according to claim 3, It is characterized in that In the case where the second retaining wall is provided in at least one of the pixel openings, the edge of the second retaining wall away from the nearest pixel defining structure has a first climbing portion, and the slope angle of the first climbing portion is 40 to 50 degrees, and the slope angle is the angle between the tangent of the first climbing portion and the plane parallel to the substrate.
15. The display substrate according to claim 3, It is characterized in that The pixel defining layer includes a plurality of the first retaining walls and a plurality of the second retaining walls, and the display substrate satisfies at least one of the following conditions: The pixel defining structure, the first retaining wall and the second retaining wall are connected to form a continuous structure; The third thickness is less than or equal to the second thickness.
16. The display substrate according to claim 3, It is characterized in that At least one of the following conditions is met: In the case where the first barrier wall is disposed in at least one of the pixel openings, a ratio of the first thickness to the second thickness is greater than or equal to 3 and less than or equal to 6; In the case where the second barrier wall is disposed in at least one of the pixel openings, a ratio of the second thickness to the third thickness is greater than or equal to 1 and less than or equal to 1.
5.
17. The display substrate according to claim 3, It is characterized in that At least one of the following conditions is met: In the case where the first retaining wall is disposed in at least one of the pixel openings, the pixel defining structure is made of a liquid-repellent material, and the first retaining wall is made of a liquid-philic material; In the case where the second retaining wall is disposed in at least one of the pixel openings, the pixel defining structure is made of a liquid-repellent material, and the second retaining wall is made of a liquid-repellent material.
18. A display substrate, It is characterized in that It comprises a substrate, and a pixel defining layer arranged on one side of the substrate, wherein the pixel defining layer comprises a plurality of pixel defining structures, and a plurality of pixel openings defined by the pixel defining structures; The pixel defining layer further comprises a plurality of first retaining walls, at least one of the pixel openings is provided with the first retaining wall, the first retaining wall divides the pixel opening into a first sub-opening and a second sub-opening, in a direction perpendicular to the plane where the substrate is located, the thickness of the pixel defining structure is a first thickness, the thickness of the first retaining wall is a second thickness, and the second thickness is less than the first thickness; The first sub-opening and the second sub-opening have different areas.
19. A display panel, It is characterized in that A display substrate comprising any one of claims 1 to 17.
20. A display device, It is characterized in that Comprising a display panel as claimed in claim 19.