Surface treatment method of wear-resistant and corrosion-resistant wagon balance

Through the resistive material heating technology combined with the sintering tank and the sintering box, an wear-resistant and anti-corrosion coating is formed, which solves the corrosion and wear problems of the floor scale when transporting acidic, alkaline or salt materials, and improves the corrosion and wear resistance of the floor scale. Performance extends its service life.

CN118950434APending Publication Date: 2024-11-15QINGDAO SIMEI WEIGHING APP CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411006635.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-25
Publication Date
2024-11-15

AI Technical Summary

Technical Problem

Floor scales are prone to corrosion and wear when transporting acidic, alkaline or salty materials, resulting in structural damage and functional failure. The existing surface treatment methods cannot effectively protect their large-area working surfaces.

Method used

The method of combining the sintering tank and the sintering box is adopted to form a wear-resistant and anti-corrosion coating by DC heating of the resistive material. The slurry of the anti-corrosion material powder and the wear-resistant powder are dried and sintered in the sintering box, forming a thickness of up to 0.5. A wear-resistant and anti-corrosion coating of mm-3mm.

Benefits of technology

The corrosion resistance and wear resistance of the top steel plate on the floor scale are improved, which extends the service life and avoids the defects of multiple surfacing and splicing seams, providing a complete and effective surface treatment method.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The invention provides a surface treatment method of a wear-resistant and corrosion-resistant wagon balance, which comprises the following steps: loading a sintering box and a resistance material into a sintering tank, then brushing slurry, then putting a steel structure main body of the wagon balance into the sintering box, burying, surrounding and covering all the outer wall surfaces of the sintering box by the resistance material, then switching on a direct-current power supply, and carrying out surface treatment on the wagon balance. When direct current passes through the resistance material, the resistance material emits heat, heat generated by the resistance material outside the sintering box heats the wagon balance steel structure main body and the slurry layer in the sintering box, drying, sintering and natural cooling are carried out in sequence, and the wear-resistant and anti-corrosion coating is sintered; the effective surface treatment method and the surface treatment equipment large enough in volume are provided, a complete abrasion-resistant and corrosion-resistant coating can be formed on the working face of the wagon balance steel structure body at a time, multiple times of surfacing are not needed, no splicing seam exists, the corrosion resistance and the abrasion resistance of the working face of the wagon balance are improved, and the service life of the wagon balance is prolonged. Corrosion damage to materials containing acid, alkali or salt and the like is reduced, and the service life of the wagon balance is prolonged.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of floor scale equipment, and in particular relates to a surface treatment method for a wear-resistant and corrosion-resistant floor scale. Background Art

[0002] A weighbridge is a large scale installed on the ground. It is usually used to weigh the tonnage of a truck. It is the main weighing equipment used by factories, mines, and businesses to measure bulk goods. According to the structure of the scale, weighbridges can be divided into: I-beam weighbridges, T-beam weighbridges, L-beam steel weighbridges, U-beam weighbridges, channel steel weighbridges, reinforced concrete weighbridges, etc.; according to the type of sensor, they can be divided into digital weighbridges, analog weighbridges, etc. The weighbridge is mainly composed of three main parts: a load-bearing force transmission mechanism (scale body), a high-precision weighing sensor, and a weighing display instrument. The load-bearing force transmission mechanism is a mechanical platform that transmits the weight of an object to the weighing sensor. Common types include all-steel structures and steel-concrete structures.

[0003] The application scenarios of the scale are very wide. When the materials weighed by the scale are acidic liquids, alkaline liquids, acidic solid materials, alkaline solid materials, salt water, seafood and other materials containing acid, alkali or salt, due to automobile transportation, in the process of the car driving onto the scale, the car staying on the scale and the car driving off the scale, it is inevitable that more or less materials containing acid, alkali or salt will fall from the car onto the scale. The acid, alkali or salt-containing materials will corrode the scale. Moreover, the scale will be worn out by the car going up and down the scale. The corrosion and wear form a vicious circle. The strength and hardness of the corroded layer are significantly reduced, making it easier to be worn away. After being worn away, the fresh layer underneath is exposed and then corroded again. Such a vicious cycle will cause structural damage and functional failure of the scale over time.

[0004] Usually, the main structure of the scale is welded by steel plates, etc. The scale sizes commonly used by manufacturers are 3×12m, 3×14m, 3×16m, 3×18m, etc. For example, if the weighing vehicle is a model with four front and eight rear wheels, a 3×9m scale can be selected; if the weighing vehicle is a semi-trailer, a 3×16m scale can be selected, etc. It can be seen that the top working surface of the scale that contacts the vehicle is subjected to anti-corrosion and wear-resistant surface treatment. First, the volume of the scale is large, and second, the area of ​​this working surface is large, which limits the use of some commonly used surface treatment methods and surface treatment equipment.

[0005] Therefore, how to protect the top working surface of the scale that contacts the vehicle, improve the corrosion resistance and wear resistance of the top outer surface, reduce the corrosion damage of materials containing acid, alkali or salt, and increase the service life of the scale is a technical problem that technical personnel in this field urgently need to solve. Summary of the invention

[0006] The purpose of the invention is to provide a surface treatment method for a wear-resistant and corrosion-resistant floor scale.

[0007] In order to achieve the above object, the technical solution of the present invention is as follows:

[0008] A surface treatment method for a wear-resistant and corrosion-resistant floor scale comprises the following steps performed in sequence:

[0009] 1) Building the sintering tank: first, build a rectangular tank on the ground with refractory bricks, and then build at least one layer of insulation bricks on the refractory bricks at the bottom of the tank and on the refractory bricks at the inner side wall of the tank, and then obtain the sintering tank;

[0010] 2) Then, a layer of resistor material is laid on the inner bottom of the sintering tank, and then a sintering box with a top cover made of welded steel plates is lifted and placed on the resistor material on the inner bottom of the sintering tank;

[0011] Then, a resistor material is filled into the gap between the lateral inner wall surface of the sintering tank and the lateral outer wall surface of the sintering box, and during the filling process, a graphite rod anode is inserted into the resistor material pre-buried at one end of the length direction of the sintering tank, and a graphite rod cathode is inserted into the resistor material pre-buried at the other end of the length direction of the sintering tank to form a circuit;

[0012] 3) Apply slurry by brushing: Mix the anti-corrosion powder, wear-resistant powder, water and binder evenly to make slurry, then apply the slurry by brushing on the top length and width surface of the top steel plate of the main body of the scale steel structure, and then dry it;

[0013] 4) Laying a layer of refractory bricks on the inner bottom surface of the sintering box for electrical insulation, then hoisting the main body of the scale steel structure after the slurry is dried and placing it flat in the sintering box, controlling the main body of the scale steel structure to leave gaps between the lateral inner wall surface and the top wall surface of the sintering box to form electrical insulation, controlling the posture of the main body of the scale steel structure to arrange the top steel plate and the dried slurry layer in sequence from bottom to top, and then covering the top cover of the sintering box;

[0014] Then continue to fill the resistor material into the sintering tank until the resistor material completely buries, surrounds and covers the sintering box;

[0015] Then, a layer of heat-insulating material is laid on the top surface of the resistor material in the sintering tank for heat insulation;

[0016] 5) Drying: The graphite rod anode and the graphite rod cathode are electrically connected to the positive electrode and the negative electrode of the DC power supply respectively, and the DC power output by the graphite rod anode and the graphite rod cathode is transmitted to the resistor material. When the DC power passes through the resistor material, the resistor material generates heat, and the heat generated by the resistor material outside the sintering box heats and dries the steel structure body of the scale and the slurry layer in the sintering box;

[0017] 6) Sintering: Utilizing the heating of the resistor material, the temperature is continuously raised to the sintering temperature to sinter the scale steel structure body and the slurry layer in the sintering box, and after a period of heat preservation, a wear-resistant and anti-corrosion coating is sintered on the top long and wide surface of the top steel plate of the scale steel structure body;

[0018] After the sintering and heat preservation is completed, the power is turned off and the heating is stopped, and the sintering box is kept covered and buried by the resistor material to cool naturally until the temperature of the main body of the scale steel structure drops below 100°C;

[0019] 7) Remove the resistor material outside the sintering box, then open the top cover of the sintering box, and then lift the scale steel structure body out of the sintering box to obtain the scale steel structure body with wear-resistant and anti-corrosion coating on the top length and width surface.

[0020] Preferably, the anti-corrosion powder is aluminum-based brazing filler metal, nickel-based brazing filler metal, aluminum powder, nickel powder or ceramic binder;

[0021] The wear-resistant powder is silicon carbide;

[0022] The binder is a resin binder;

[0023] The particle sizes of the anti-corrosion powder and the wear-resistant powder are both 20 microns to 200 microns;

[0024] The mass of anti-corrosion powder: the mass of wear-resistant powder = (2-4): 1.

[0025] Preferably, the drying temperature is 110° C.-120° C., and the drying and heat preservation time is 2 h-4 h.

[0026] Preferably, the sintering holding temperature is 1000° C.-1500° C., and the holding time is 8 h-16 h.

[0027] Preferably, the thickness of the wear-resistant and anti-corrosion coating is 0.5 mm-3 mm.

[0028] This application has achieved the following beneficial technical effects:

[0029] In the present application, since the main structure of the scale is welded from steel plates, the wear-resistant and corrosion-resistant treatment is essentially performed on the top length and width surface of the top steel plate of the scale; firstly, the volume of the scale is large, and secondly, the area of ​​the top length and width surface is large, resulting in the lack of surface treatment equipment with a large enough volume in the prior art to form a complete wear-resistant and corrosion-resistant coating through one-time surface treatment, and the prior art usually adopts a small welding gun, multiple surfacing welding, and multiple long strip coatings spliced ​​together to obtain the coating;

[0030] To this end, the present application loads a sintering box and a resistor into a sintering tank, and brushes a slurry containing anti-corrosion powder and wear-resistant powder on the top length and width surface of the top steel plate of the main body of the steel structure of the scale, and then places the main body of the steel structure of the scale in the sintering box, controls the electrical insulation between the main body of the steel structure of the scale and the sintering box, and only loads the resistor outside the sintering box, and does not load the resistor in the sintering box, and continues to load the resistor until all the outer wall surfaces of the sintering box are buried, surrounded and covered, and then turns on a DC power supply, and the DC power is transmitted to the resistor through the graphite rod anode and the graphite rod cathode respectively. When the DC power passes through the resistor, the resistor generates heat, and the heat generated by the resistor outside the sintering box heats the main body of the steel structure of the scale and the slurry layer in the sintering box, and then performs drying and sintering treatments in sequence. After the drying and sintering treatments are completed, the main body of the steel structure of the scale is kept naturally cooled as it is, and a wear-resistant and anti-corrosion coating is fired on the top length and width surface of the top steel plate of the main body of the steel structure of the scale;

[0031] Thus, since the sintering box is made of welded steel plates with a top cover, the length, width, height and internal volume of the sintering box can be welded to be large enough, large enough to accommodate the steel structure body of the above-mentioned 3×18m scale;

[0032] In this way, since the sintering tank is built with refractory bricks and insulation bricks, the length, width, height and internal volume of the sintering tank can be built large enough to accommodate the sintering box with the steel structure of the scale inside.

[0033] Here, a sintering box is set in the sintering tank. First, the sintering box is used to separate the resistor material and the slurry to avoid the reduction reaction between the carbon resistor material and the slurry at the high sintering temperature, and to avoid the resistor material and the slurry from being sintered and connected together. Second, the sintering box is made of steel plate. Since the steel plate has good thermal conductivity, the resistor material indirectly heats the slurry. The sintering box and the main steel structure of the scale inside are electrically insulated. Therefore, the main steel structure of the scale is not electrified.

[0034] In this way, the present application provides an effective surface treatment method and a surface treatment device with a large enough volume, which can form a complete wear-resistant and anti-corrosion coating on the top long and wide surface of the top steel plate of the steel structure body of the scale through a one-time surface treatment. There is no need for multiple surfacing constructions, and there are no joints in the coating, thereby protecting the top working surface of the scale that contacts the vehicle, improving the corrosion resistance and wear resistance of the top outer surface, reducing the corrosion damage of materials containing acids, alkalis or salts, and increasing the service life of the scale. DETAILED DESCRIPTION

[0035] The following will be combined with the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. The described embodiments are only part of the embodiments of the present invention, not all of them. Therefore, based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0036] The present application provides a surface treatment method for a wear-resistant and corrosion-resistant floor scale, comprising the following steps performed in sequence:

[0037] 1) Building the sintering tank: first, build a rectangular tank on the ground with refractory bricks, and then build at least one layer of insulation bricks on the refractory bricks at the bottom of the tank and on the refractory bricks at the inner side wall of the tank, and then obtain the sintering tank;

[0038] 2) Then, a layer of resistor material is laid on the inner bottom of the sintering tank, and then a sintering box with a top cover made of welded steel plates is lifted and placed on the resistor material on the inner bottom of the sintering tank;

[0039] Then, a resistor material is filled into the gap between the lateral inner wall surface of the sintering tank and the lateral outer wall surface of the sintering box, and during the filling process, a graphite rod anode is inserted into the resistor material pre-buried at one end of the length direction of the sintering tank, and a graphite rod cathode is inserted into the resistor material pre-buried at the other end of the length direction of the sintering tank to form a circuit;

[0040] 3) Applying slurry by brushing: Anti-corrosion powder, wear-resistant powder, water and binder are stirred and mixed to form slurry, and then the slurry is brushed on the top long and wide surface of the top steel plate of the main body of the scale steel structure, and then dried;

[0041] 4) Laying a layer of refractory bricks on the inner bottom surface of the sintering box for electrical insulation, then hoisting the main body of the scale steel structure after the slurry is dried and placing it flat in the sintering box, controlling the main body of the scale steel structure to leave gaps between the lateral inner wall surface and the top wall surface of the sintering box to form electrical insulation, controlling the posture of the main body of the scale steel structure to arrange the top steel plate and the dried slurry layer in sequence from bottom to top, and then covering the top cover of the sintering box;

[0042] Then continue to fill the resistor material into the sintering tank until the resistor material completely buries, surrounds and covers the sintering box;

[0043] Then, a layer of heat-insulating material is laid on the top surface of the resistor material in the sintering tank for heat insulation;

[0044] 5) Drying: The graphite rod anode and the graphite rod cathode are electrically connected to the positive electrode and the negative electrode of the DC power supply respectively, and the DC power output by the graphite rod anode and the graphite rod cathode is transmitted to the resistor material. When the DC power passes through the resistor material, the resistor material generates heat, and the heat generated by the resistor material outside the sintering box heats and dries the steel structure body of the scale and the slurry layer in the sintering box;

[0045] 6) Sintering: Utilizing the heating of the resistor material, the temperature is continuously raised to the sintering temperature to sinter the scale steel structure body and the slurry layer in the sintering box, and after a period of heat preservation, a wear-resistant and anti-corrosion coating is sintered on the top long and wide surface of the top steel plate of the scale steel structure body;

[0046] After the sintering and heat preservation is completed, the power is turned off and the heating is stopped, and the sintering box is kept covered and buried by the resistor material to cool naturally until the temperature of the main body of the scale steel structure drops below 100°C;

[0047] 7) Remove the resistor material outside the sintering box, then open the top cover of the sintering box, and then lift the scale steel structure body out of the sintering box to obtain the scale steel structure body with wear-resistant and anti-corrosion coatings on the top long and wide surfaces;

[0048] Then the steel structure body of the weighbridge, the weighing sensor and the weighing display instrument are assembled into a weighbridge.

[0049] In one embodiment of the present application, the anti-corrosion powder is aluminum-based brazing filler metal, nickel-based brazing filler metal, aluminum powder, nickel powder or ceramic binder;

[0050] The wear-resistant powder is silicon carbide;

[0051] The binder is a resin binder, for example, a synthetic resin used as a binder for molding sand or core sand;

[0052] The particle sizes of the anti-corrosion powder and the wear-resistant powder are both 20 microns to 200 microns;

[0053] The mass of anti-corrosion powder: the mass of wear-resistant powder = (2-4): 1.

[0054] In one embodiment of the present application, the drying temperature is 110° C.-120° C., and the drying and heat preservation time is 1 h-2 h.

[0055] In one embodiment of the present application, the sintering holding temperature is 1000° C.-1500° C., and the holding time is 8 h-16 h.

[0056] In one embodiment of the present application, the thickness of the wear-resistant and anti-corrosion coating is 0.5 mm-3 mm.

[0057] In the present application, surface treatment includes hot-dip galvanizing, hot-dip aluminizing, and the like.

[0058] In the present application, there are many types of brazing filler metals for brazing, and filler metals based on aluminum, silver, copper, manganese and nickel are the most widely used; copper-based filler metals are commonly used for brazing of copper and iron parts; manganese-based and nickel-based filler metals are mostly used to weld parts such as stainless steel, heat-resistant steel and high-temperature alloys working at high temperatures; palladium-based, zirconium-based and titanium-based filler metals are commonly used for welding refractory metals such as beryllium, titanium, zirconium, graphite rods and ceramics; the melting point of the brazing filler metal is above 450°C, and commonly used brazing filler metals include copper-based filler metals, silver-based filler metals, aluminum-based filler metals, nickel-based filler metals and other alloys; the heating sources for brazing include torch flame, resistance electric heating, induction heating, salt bath heating and furnace heating; the brazing joint has high strength and is suitable for brazing workpieces with large forces or high working temperatures, such as carbide tools, bicycle frames, etc.

[0059] In this application, the abrasive is made of abrasives and binders. Abrasives are mainly divided into two categories: corundum abrasives and silicon carbide abrasives. Commonly used binders include ceramic binders, resin binders, rubber binders and metal binders. The sintering temperature of ceramic bond abrasives is generally around 1300°C. When a low melting point sintering binder is used, the sintering temperature is lower than 1000°C. The manufacturing process of metal bond abrasives includes powder metallurgy. The powder metallurgy method uses bronze as a binder, and after mixing, hot pressing or pressure molding at room temperature is used, and then sintering is performed.

[0060] In the present application, the structure and heating principle of the sintering tank are similar to those of the Acheson graphitization furnace. The cavity in the tank is filled with a resistor material for heating by electricity. The resistor material is granular metallurgical coke or graphitized metallurgical coke, preferably calcined petroleum coke, and the particle size of calcined petroleum coke is 3-20mm. The current passes through the resistor material to generate heat, and the steel structure body of the scale is heated to the temperature required for surface treatment. Graphitization furnaces are divided into two categories according to different methods: that is, they are divided into direct heating furnaces and indirect heating furnaces according to the heating method. The direct heating furnace uses the material to be heat-treated directly as the heating body, and the indirect heating furnace is that the material is only the heating body, and the heat comes from the resistor material outside the material; according to the operation design method, they are classified into: Acheson graphitization furnace, internal string graphitization furnace, vacuum graphitization furnace, continuous graphitization furnace and box-type graphitization furnace.

[0061] The methods and devices not described in detail in the present invention are all prior art and will not be described in detail.

[0062] In order to better understand the present invention, the present invention is further specifically described below through the following examples, but it should not be understood as a limitation of the present invention. Some non-essential improvements and adjustments made by technicians in this field based on the above invention content are also considered to fall within the protection scope of the present invention.

[0063] Example 1

[0064] A surface treatment method for a wear-resistant and corrosion-resistant floor scale comprises the following steps performed in sequence:

[0065] 1) Building the sintering tank: first, build a rectangular tank on the ground with refractory bricks, and then build at least one layer of insulation bricks on the refractory bricks at the bottom of the tank and on the refractory bricks at the inner side wall of the tank, and then obtain the sintering tank;

[0066] 2) Then, a layer of resistor material is laid on the inner bottom of the sintering tank, and then a sintering box with a top cover made of welded steel plates is lifted and placed on the resistor material on the inner bottom of the sintering tank;

[0067] Then, a resistor material is filled into the gap between the lateral inner wall surface of the sintering tank and the lateral outer wall surface of the sintering box, and during the filling process, a graphite rod anode is inserted into the resistor material pre-buried at one end of the length direction of the sintering tank, and a graphite rod cathode is inserted into the resistor material pre-buried at the other end of the length direction of the sintering tank to form a circuit;

[0068] 3) Applying slurry by brushing: Anti-corrosion powder, wear-resistant powder, water and binder are stirred and mixed to form slurry, and then the slurry is brushed on the top long and wide surface of the top steel plate of the main body of the scale steel structure, and then dried;

[0069] The anti-corrosion material powder is nickel-based solder;

[0070] The wear-resistant powder is silicon carbide;

[0071] The binder is a resin binder;

[0072] The particle sizes of the anti-corrosion powder and the wear-resistant powder are both 50 microns to 100 microns;

[0073] The mass of anti-corrosion powder: the mass of wear-resistant powder = 3:1;

[0074] 4) Laying a layer of refractory bricks on the inner bottom surface of the sintering box for electrical insulation, then hoisting the main body of the scale steel structure after the slurry is dried and placing it flat in the sintering box, controlling the main body of the scale steel structure to leave gaps between the lateral inner wall surface and the top wall surface of the sintering box to form electrical insulation, controlling the posture of the main body of the scale steel structure to arrange the top steel plate and the dried slurry layer in sequence from bottom to top, and then covering the top cover of the sintering box;

[0075] Then continue to fill the resistor material into the sintering tank until the resistor material completely buries, surrounds and covers the sintering box;

[0076] Then, a layer of heat-insulating material is laid on the top surface of the resistor material in the sintering tank for heat insulation;

[0077] 5) Drying: The graphite rod anode and the graphite rod cathode are electrically connected to the positive electrode and the negative electrode of the DC power supply respectively, and the DC power output by the graphite rod anode and the graphite rod cathode is transmitted to the resistor material. When the DC power passes through the resistor material, the resistor material generates heat, and the heat generated by the resistor material outside the sintering box heats and dries the steel structure body of the scale and the slurry layer in the sintering box;

[0078] The drying temperature is 110℃-115℃, and the drying and heat preservation time is 2h;

[0079] 6) Sintering: Utilizing the heating of the resistor material, the temperature is continuously raised to the sintering temperature to sinter the scale steel structure body and the slurry layer in the sintering box, and after a period of heat preservation, a wear-resistant and anti-corrosion coating is sintered on the top long and wide surface of the top steel plate of the scale steel structure body;

[0080] The sintering holding temperature is 1400℃-1450℃, and the holding time is 12h;

[0081] After the sintering and heat preservation is completed, the power is turned off and the heating is stopped, and the sintering box is kept covered and buried by the resistor material to cool naturally until the temperature of the main body of the scale steel structure drops below 100°C;

[0082] 7) Remove the resistor material outside the sintering box, then open the top cover of the sintering box, and then lift the scale steel structure body out of the sintering box to obtain the scale steel structure body with wear-resistant and anti-corrosion coatings on the top long and wide surfaces;

[0083] Then assemble the weighbridge steel structure body, weighing sensor and weighing display instrument into a weighbridge;

[0084] The thickness of the wear-resistant and anti-corrosion coating is 1mm-1.2mm.

[0085] Example 2

[0086] A surface treatment method for a wear-resistant and corrosion-resistant floor scale comprises the following steps performed in sequence:

[0087] 1) Building the sintering tank: first, build a rectangular tank on the ground with refractory bricks, and then build at least one layer of insulation bricks on the refractory bricks at the bottom of the tank and on the refractory bricks at the inner side wall of the tank, and then obtain the sintering tank;

[0088] 2) Then, a layer of resistor material is laid on the inner bottom of the sintering tank, and then a sintering box with a top cover made of welded steel plates is lifted and placed on the resistor material on the inner bottom of the sintering tank;

[0089] Then, a resistor material is filled into the gap between the lateral inner wall surface of the sintering tank and the lateral outer wall surface of the sintering box, and during the filling process, a graphite rod anode is inserted into the resistor material pre-buried at one end of the length direction of the sintering tank, and a graphite rod cathode is inserted into the resistor material pre-buried at the other end of the length direction of the sintering tank to form a circuit;

[0090] 3) Applying slurry by brushing: Anti-corrosion powder, wear-resistant powder, water and binder are stirred and mixed to form slurry, and then the slurry is brushed on the top long and wide surface of the top steel plate of the main body of the scale steel structure, and then dried;

[0091] The anti-corrosion material powder is nickel-based solder;

[0092] The wear-resistant powder is silicon carbide;

[0093] The binder is a resin binder;

[0094] The particle sizes of the anti-corrosion powder and the wear-resistant powder are both 30 microns to 60 microns;

[0095] The mass of anti-corrosion powder: the mass of wear-resistant powder = 4:1;

[0096] 4) Laying a layer of refractory bricks on the inner bottom surface of the sintering box for electrical insulation, then hoisting the main body of the scale steel structure after the slurry is dried and placing it flat in the sintering box, controlling the main body of the scale steel structure to leave gaps between the lateral inner wall surface and the top wall surface of the sintering box to form electrical insulation, controlling the posture of the main body of the scale steel structure to arrange the top steel plate and the dried slurry layer in sequence from bottom to top, and then covering the top cover of the sintering box;

[0097] Then continue to fill the resistor material into the sintering tank until the resistor material completely buries, surrounds and covers the sintering box;

[0098] Then, a layer of heat-insulating material is laid on the top surface of the resistor material in the sintering tank for heat insulation;

[0099] 5) Drying: The graphite rod anode and the graphite rod cathode are electrically connected to the positive electrode and the negative electrode of the DC power supply respectively, and the DC power output by the graphite rod anode and the graphite rod cathode is transmitted to the resistor material. When the DC power passes through the resistor material, the resistor material generates heat, and the heat generated by the resistor material outside the sintering box heats and dries the steel structure body of the scale and the slurry layer in the sintering box;

[0100] The drying temperature is 105℃-115℃, and the drying and heat preservation time is 3h;

[0101] 6) Sintering: Utilizing the heating of the resistor material, the temperature is continuously raised to the sintering temperature to sinter the scale steel structure body and the slurry layer in the sintering box, and after a period of heat preservation, a wear-resistant and anti-corrosion coating is sintered on the top long and wide surface of the top steel plate of the scale steel structure body;

[0102] The sintering holding temperature is 1400℃-1450℃, and the holding time is 14h;

[0103] After the sintering and heat preservation is completed, the power is turned off and the heating is stopped, and the sintering box is kept covered and buried by the resistor material to cool naturally until the temperature of the main body of the scale steel structure drops below 100°C;

[0104] 7) Remove the resistor material outside the sintering box, then open the top cover of the sintering box, and then lift the scale steel structure body out of the sintering box to obtain the scale steel structure body with wear-resistant and anti-corrosion coatings on the top long and wide surfaces;

[0105] Then assemble the weighbridge steel structure body, weighing sensor and weighing display instrument into a weighbridge;

[0106] The thickness of the wear-resistant and anti-corrosion coating is 1.5mm-1.8mm.

[0107] The above description of the disclosed embodiments enables one skilled in the art to implement or use the present invention. Various modifications to these embodiments will be apparent to one skilled in the art, and the general principles defined herein may be implemented in other embodiments without departing from the spirit or scope of the present invention. Therefore, the present invention will not be limited to the embodiments shown herein, but rather to the widest scope consistent with the principles and novel features disclosed herein.

Claims

1. A surface treatment method for a wear-resistant and corrosion-resistant weighbridge, characterized in that: The method includes the following steps: 1) Building the sintering tank: first, build a rectangular tank on the ground with refractory bricks, and then build at least one layer of insulation bricks on the refractory bricks at the bottom of the tank and on the refractory bricks at the inner side wall of the tank, and then obtain the sintering tank; 2) Then, a layer of resistor material is laid on the inner bottom of the sintering tank, and then a sintering box with a top cover made of welded steel plates is lifted and placed on the resistor material on the inner bottom of the sintering tank; Then, a resistor material is filled into the gap between the lateral inner wall surface of the sintering tank and the lateral outer wall surface of the sintering box, and during the filling process, a graphite rod anode is inserted into the resistor material pre-buried at one end of the length direction of the sintering tank, and a graphite rod cathode is inserted into the resistor material pre-buried at the other end of the length direction of the sintering tank to form a circuit; 3) Apply slurry by brushing: Mix the anti-corrosion powder, wear-resistant powder, water and binder evenly to make slurry, then apply the slurry by brushing on the top length and width surface of the top steel plate of the main body of the scale steel structure, and then dry it; 4) Laying a layer of refractory bricks on the inner bottom surface of the sintering box for electrical insulation, then hoisting the main body of the scale steel structure after the slurry is dried and placing it flat in the sintering box, controlling the main body of the scale steel structure to leave gaps between the lateral inner wall surface and the top wall surface of the sintering box to form electrical insulation, controlling the posture of the main body of the scale steel structure to arrange the top steel plate and the dried slurry layer in sequence from bottom to top, and then covering the top cover of the sintering box; Then continue to fill the resistor material into the sintering tank until the resistor material completely buries, surrounds and covers the sintering box; Then, a layer of heat-insulating material is laid on the top surface of the resistor material in the sintering tank for heat insulation; 5) Drying: The graphite rod anode and the graphite rod cathode are electrically connected to the positive electrode and the negative electrode of the DC power supply respectively, and the DC power output by the graphite rod anode and the graphite rod cathode is transmitted to the resistor material. When the DC power passes through the resistor material, the resistor material generates heat, and the heat generated by the resistor material outside the sintering box heats and dries the steel structure body of the scale and the slurry layer in the sintering box; 6) Sintering: Utilizing the heating of the resistor material, the temperature is continuously raised to the sintering temperature to sinter the scale steel structure body and the slurry layer in the sintering box, and after a period of heat preservation, a wear-resistant and anti-corrosion coating is sintered on the top long and wide surface of the top steel plate of the scale steel structure body; After the sintering and heat preservation is completed, the power is turned off and the heating is stopped, and the sintering box is kept covered and buried by the resistor material to cool naturally until the temperature of the main body of the scale steel structure drops below 100°C; 7) Remove the resistor material outside the sintering box, then open the top cover of the sintering box, and then lift the scale steel structure body out of the sintering box to obtain the scale steel structure body with wear-resistant and anti-corrosion coating on the top length and width surface.

2. The surface treatment method of a wear-resistant and corrosion-resistant floor scale according to claim 1 is characterized in that: The anti-corrosion powder is aluminum-based solder, nickel-based solder, aluminum powder, nickel powder or ceramic binder; The wear-resistant powder is silicon carbide; The binder is a resin binder; The particle sizes of the anti-corrosion powder and the wear-resistant powder are both 20 microns to 200 microns; The mass of anti-corrosion powder: the mass of wear-resistant powder = (2-4):

1.

3. The surface treatment method of a wear-resistant and corrosion-resistant floor scale according to claim 1, characterized in that: The drying temperature is 110℃-120℃, and the drying and heat preservation time is 2h-4h.

4. The surface treatment method of a wear-resistant and corrosion-resistant floor scale according to claim 1, characterized in that: The sintering holding temperature is 1000℃-1500℃, and the holding time is 8h-16h.

5. The surface treatment method of a wear-resistant and corrosion-resistant floor scale according to claim 1, characterized in that: The thickness of the wear-resistant and anti-corrosion coating is 0.5mm-3mm.