Sulfonated emulsifier as well as preparation method and application thereof
The sulfonated emulsifier prepared through gas-liquid sulfonation reaction solves the problem of yellowing caused by sunlight irradiation of leather, provides a solution with high stability and good emulsification performance, and is suitable for improving the oxidation resistance of leather grease additives.
Patent Information
- Application Number
- CN202411222220.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-02
- Publication Date
- 2024-11-15
AI Technical Summary
Light-colored leather is prone to yellowing due to sunlight exposure during use, and the natural unsaturated oils in existing fat-adding agents are prone to oxidation, and the existing technology is difficult to effectively solve.
The gas-liquid sulfonation reaction is used to sulfonate cocoate and SO3-containing gas, and the SO3 volume content is controlled from 3% to 8%, so as to prepare a sulfonated emulsifier with good emulsification properties, and through aging and neutralization treatment. Improve product stability.
The prepared sulfonated emulsifier has a low iodine value, excellent yellowing resistance, good stability and strong emulsification ability, which can effectively improve the oxidation and yellowing problem of leather fat-adding agents.
Smart Images

Figure CN118956494A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of leather emulsifiers, and in particular to a sulfonated emulsifier and a preparation method and application thereof. Background Art
[0002] Light-colored leather is widely used in high-end sofas, car seat cushions and other fields. However, these leathers will inevitably be exposed to sunlight during use, resulting in yellowing. In fact, the leather itself does not produce yellowing phenomenon, these changes are related to the added chemical materials. Leather fatliquor is one of the important process sections in leather production. The use of fatliquor can make the leather soft and elastic, greatly enhancing its performance. However, the natural unsaturated oil in the fatliquor is easily oxidized and will bring the risk of yellowing to the leather.
[0003] In view of this, the present invention is proposed. Summary of the invention
[0004] The object of the present invention is to provide a sulfonated emulsifier and a preparation method and application thereof, so as to solve or improve the above technical problems.
[0005] The present invention can be implemented like this:
[0006] In a first aspect, the present invention provides a method for preparing a sulfonated emulsifier, comprising the following steps: subjecting coconut ester to a gas-liquid sulfonation reaction with a sulfonating agent to obtain sulfonated coconut ester;
[0007] The sulfonating agent is a mixed gas of SO3 and air, and the volume percentage of SO3 contained in the mixed gas is 3% to 8%.
[0008] In an optional embodiment, the gas-liquid sulfonation reaction has at least one of the following characteristics:
[0009] Feature 1: The molar ratio of coconut ester to SO3 in the sulfonating agent is 1:1 to 1.5:1;
[0010] Feature 2: The temperature of the gas-liquid sulfonation reaction is 50°C to 80°C;
[0011] Feature 3: The time of gas-liquid sulfonation reaction is 1min to 2min;
[0012] Feature 4: The iodine value of cocoate does not exceed 5.5g / 100g.
[0013] In an optional embodiment, the moisture content of the coco ester is 0.06% to 0.33%.
[0014] In an optional embodiment, the iodine value of the cocoate is 4.67 g / 100 g to 5.48 g / 100 g.
[0015] In an alternative embodiment, the acid value of the coco ester is 3.95 mg NaOH / g to 5.18 mg NaOH / g.
[0016] In an optional embodiment, the esterification rate of the coconut ester is not less than 95%.
[0017] In an optional embodiment, the method further comprises: subjecting the sulfonated coconut oil ester to an aging treatment;
[0018] The temperature of the aging treatment is 50°C to 80°C, and the time of the aging treatment is 3h to 6h.
[0019] In an optional embodiment, the method further comprises: neutralizing the sulfonated coconut oil ester after the aging treatment;
[0020] The temperature of the neutralization treatment is 40°C to 60°C, and the time of the neutralization treatment is 2h to 6h.
[0021] In an optional embodiment, the neutralizing agent used in the neutralization treatment is an alkaline solution.
[0022] In an alternative embodiment, the alkaline solution includes at least one of sodium hydroxide and potassium hydroxide.
[0023] In an optional embodiment, the mass concentration of the alkali in the alkali solution is 40% to 70%.
[0024] In an optional embodiment, the amount of the neutralizer used is 45 wt % to 50 wt % of the sulfonated coconut ester after aging treatment.
[0025] In an optional embodiment, the preparation of coconut ester comprises: conducting an esterification reaction between coconut oleic acid and fatty alcohol under the condition of p-toluenesulfonic acid as a catalyst;
[0026] The temperature of the esterification reaction is 80°C to 110°C, and the time of the esterification reaction is 4h to 8h.
[0027] In an optional embodiment, the fatty alcohol is a saturated alkyl alcohol having 10 to 16 carbon atoms.
[0028] In an alternative embodiment, the fatty alcohol comprises at least one of n-decanol, dodecanol, and hexadecanol.
[0029] In an optional embodiment, the molar ratio of coconut oleic acid to fatty alcohol is 1:1 to 1.3:1;
[0030] In an optional embodiment, the amount of the catalyst used is 0.1% to 0.5% of the total mass of coconut oleic acid and fatty alcohol.
[0031] In an optional embodiment, the method further comprises: subjecting the coconut oil ester obtained by the esterification reaction to a vacuum dehydration treatment.
[0032] In an optional embodiment, the vacuum dehydration treatment is carried out under the condition of 0.04MPa to 0.08MPa.
[0033] In a second aspect, the present invention provides a sulfonated emulsifier prepared by the preparation method of any one of the aforementioned embodiments.
[0034] In an optional embodiment, the sulfonated emulsifier has at least one of the following characteristics:
[0035] Feature 5: The combined SO3 content of the sulfonated emulsifier is 4% to 8%; preferably 4.6% to 7.9%;
[0036] Feature 6: The iodine value of the sulfonated emulsifier does not exceed 3 g / 100 g; preferably does not exceed 1.4 g / 100 g.
[0037] In a third aspect, the present invention provides a use of the sulfonated emulsifier according to the aforementioned embodiment, for example, using the sulfonated emulsifier in a leather processing process.
[0038] In a fourth aspect, the present invention provides a leather, wherein the raw materials for preparing the leather include the above-mentioned sulfonated emulsifier.
[0039] The beneficial effects of the present invention include:
[0040] The present invention uses gas containing SO3 as a sulfonating agent to carry out gas-liquid sulfonation reaction with coconut ester to obtain sulfonated coconut ester, wherein the sulfonating agent containing SO3 gas has the advantages of strong sulfonation ability, fast reaction, no generation of H2O and a large amount of waste acid, and the volume content of SO3 in the sulfonating agent is controlled to 3% to 8%, which can ensure that the sulfonation is more uniform, not only can avoid over-sulfonation and coking phenomena, improve the stability of the product, but also ensure that the product has good emulsification performance. The sulfonated emulsifier obtained by the above method has a lower iodine value, excellent yellowing resistance, better stability, and good emulsification ability, and can be used in the leather fatliquor process to improve the oxidation yellowing resistance of the fatliquor. BRIEF DESCRIPTION OF THE DRAWINGS
[0041] In order to more clearly illustrate the technical solutions of the embodiments of the present invention, the drawings required for use in the embodiments are briefly introduced below. It should be understood that the following drawings only show certain embodiments of the present invention and therefore should not be regarded as limiting the scope. For ordinary technicians in this field, other related drawings can be obtained based on these drawings without creative work.
[0042] Figure 1 This is a physical picture of the coconut oil ester prepared in Example 1;
[0043] Figure 2 This is a physical picture of the sulfonated emulsifier prepared in Example 1;
[0044] Figure 3 This is a physical picture of the sulfonated emulsifier prepared in Example 2;
[0045] Figure 4 This is a physical picture of the sulfonated emulsifier prepared in Example 3. DETAILED DESCRIPTION
[0046] In order to make the purpose, technical scheme and advantages of the embodiments of the present invention clearer, the technical scheme in the embodiments of the present invention will be described clearly and completely below. If the specific conditions are not specified in the embodiments, they are carried out according to conventional conditions or conditions recommended by the manufacturer. If the manufacturer of the reagents or instruments used is not specified, they are all conventional products that can be purchased commercially.
[0047] The sulfonated emulsifier provided by the present invention and its preparation method and application are specifically described below.
[0048] The invention provides a method for preparing a sulfonated emulsifier, which comprises the following steps: subjecting coconut oil ester and a sulfonating agent to a gas-liquid sulfonation reaction to obtain sulfonated coconut oil ester; wherein the sulfonating agent is a mixed gas of SO3 and air, and the volume percentage of SO3 contained in the mixed gas is 3% to 8%.
[0049] The present invention uses gas containing SO3 as a sulfonating agent to carry out gas-liquid sulfonation reaction with coconut ester to obtain sulfonated coconut ester, wherein the sulfonating agent containing SO3 gas has the advantages of strong sulfonation ability, fast reaction, and no generation of H2O and a large amount of waste acid. The volume content of SO3 in the sulfonating agent is controlled to be 3% to 8%, which can ensure more uniform sulfonation, avoid over-sulfonation and coking, improve product stability, and ensure that the product has good emulsification performance.
[0050] In an optional embodiment, the preparation of coconut ester may include: conducting an esterification reaction between coconut oleic acid and fatty alcohol in the presence of p-toluenesulfonic acid as a catalyst.
[0051] Among them, coconut oil acid has a lower iodine value, and coconut oil ester with a low iodine value can be prepared.
[0052] The fatty alcohol is a saturated alkyl alcohol having 10 to 16 carbon atoms (eg, 10, 11, 12, 13, 14, 15 or 16). In some typical embodiments, the fatty alcohol may include at least one of n-decanol, dodecanol and hexadecanol.
[0053] The use of the saturated alkyl alcohol having the above-mentioned number of carbon atoms is conducive to obtaining the sulfonated coconut oil ester with relatively balanced lipophilic and hydrophilic properties in the subsequent step, so that the sulfonated coconut oil ester has better emulsification properties.
[0054] The molar ratio of coconut oleic acid to fatty alcohol can be 1:1 to 1.3:1, such as 1:1, 1.1:1, 1.2:1 or 1.3:1, or other values within the range of 1:1 to 1.3:1.
[0055] The amount of the catalyst can be 0.1% to 0.5% of the total mass of coconut oil acid and fatty alcohol, such as 0.1%, 0.2%, 0.3%, 0.4% or 0.5%, etc., or other values within the range of 0.1% to 0.5%.
[0056] The temperature of the esterification reaction may be 80°C to 110°C, such as 80°C, 85°C, 90°C, 95°C, 100°C, 105°C or 110°C, etc., or other values within the range of 80°C to 110°C.
[0057] The esterification reaction time can be 4 h to 8 h, such as 4 h, 4.5 h, 5 h, 5.5 h, 6 h, 6.5 h, 7 h, 7.5 h or 8 h, or other values within the range of 4 h to 8 h.
[0058] Furthermore, the coconut oil ester obtained by the esterification reaction can also be subjected to vacuum dehydration treatment. For example, the vacuum dehydration treatment can be carried out under the conditions of 0.04MPa to 0.08MPa (such as 0.04MPa, 0.05MPa, 0.06MPa, 0.07MPa or 0.08MPa, etc.).
[0059] The esterification reaction between coconut oil acid and fatty alcohol will generate ester substances and water. The reaction is a reversible reaction with a relatively slow reaction rate. The reaction process can be accelerated by adding a catalyst, and the positive reaction can be promoted by dehydration.
[0060] In some optional embodiments, the iodine value of the cocoate is no more than 5.5 g / 100 g, such as 4.67 g / 100 g to 5.48 g / 100 g.
[0061] In some optional embodiments, the water content of coconut ester is 0.06% to 0.33%.
[0062] In some optional embodiments, the acid value of the coco ester is 3.95 mg NaOH / g to 5.18 mg NaOH / g.
[0063] In some optional embodiments, the esterification rate of coconut oil ester is not less than 95%.
[0064] In the present invention, the volume percentage of SO3 contained in the mixed gas can be 3%, 3.5%, 4%, 4.5%, 5%, 5.5%, 6%, 6.5%, 7%, 7.5% or 8%, etc., or other values within the range of 3% to 8%.
[0065] If the SO3 content in the mixed gas is too high, it will easily lead to over-sulfonation, which will cause the product to coke and have poor stability; on the other hand, it will easily lead to stronger hydrophilicity of the product and poor emulsification performance. If the SO3 content in the mixed gas is too low, it will be unfavorable for the sulfonation reaction, resulting in weakened hydrophilicity of the product and loss of emulsification performance.
[0066] The SO3 gas can be prepared, by way of example but not limitation, by a sulfur combustion method or a liquid SO3 evaporation method.
[0067] In some optional embodiments, the molar ratio of cocoate to SO3 in the sulfonating agent can be 1:1 to 1.5:1, such as 1:1, 1.1:1, 1.2:1, 1.3:1, 1.4:1 or 1.5:1, or other values within the range of 1:1 to 1.5:1.
[0068] If the molar ratio of cocoate to SO3 in the sulfonating agent is lower than 1:1 (such as 0.8:1), it is not conducive to product stability and the cocoate may break its chain; if the molar ratio of cocoate to SO3 in the sulfonating agent is higher than 1.5:1 (such as 1.8:1), it is not conducive to the sulfonation reaction.
[0069] In some optional embodiments, the temperature of the gas-liquid sulfonation reaction can be 50°C to 80°C, such as 50°C, 55°C, 60°C, 65°C, 70°C, 75°C or 80°C, etc., or other values within the range of 50°C to 80°C.
[0070] If the temperature of the gas-liquid sulfonation reaction is lower than 50°C, it is not conducive to the combination of sulfonate groups and the reaction rate drops sharply; if the temperature of the gas-liquid sulfonation reaction is higher than 80°C, over-sulfonation is likely to occur.
[0071] The time of the gas-liquid sulfonation reaction can be 1 to 2 minutes. For example, the stabilization of the SO3 gas after the reaction can be used as the reaction endpoint.
[0072] Furthermore, the sulfonated coconut ester is subjected to an aging treatment.
[0073] The temperature of the aging treatment can be 50°C to 80°C, such as 50°C, 55°C, 60°C, 65°C, 70°C, 75°C or 80°C, or other values within the range of 50°C to 80°C.
[0074] The aging treatment time can be 3 h to 6 h, such as 3 h, 3.5 h, 4 h, 4.5 h, 5 h, 5.5 h or 6 h, or other values within the range of 3 h to 6 h.
[0075] Through aging treatment, the sulfonation effect can be improved to obtain a sulfonated coconut ester product with a suitable SO3 content.
[0076] Furthermore, the sulfonated coconut ester after the aging treatment is subjected to a neutralization treatment.
[0077] The temperature of the neutralization treatment may be 40°C to 60°C, such as 40°C, 45°C, 50°C, 55°C or 60°C, etc., or other values within the range of 40°C to 60°C.
[0078] The time for the neutralization treatment can be 2 h to 6 h, such as 2 h, 2.5 h, 3 h, 3.5 h, 4 h, 4.5 h, 5 h, 5.5 h or 6 h, etc., or other values within the range of 2 h to 6 h.
[0079] The neutralizing agent used in the neutralization treatment is an alkaline solution. For example, the alkaline solution may include at least one of sodium hydroxide and potassium hydroxide. The mass concentration of the alkali in the alkaline solution may be 40% to 70%, such as 40%, 45%, 50%, 55%, 60%, 65% or 70%, or other values within the range of 40% to 70%.
[0080] The amount of the neutralizer can be 45wt% to 50wt% of the sulfonated coconut oil ester after aging treatment, such as 45wt%, 46wt%, 47wt%, 48wt%, 49wt% or 50wt%, etc., or other values within the range of 45wt% to 50wt%.
[0081] In some typical embodiments, the preparation of the sulfonated emulsifier can refer to the following process: coconut oil acid and fatty alcohol are subjected to esterification reaction under the condition of p-toluenesulfonic acid as a catalyst, after vacuum dehydration, the obtained coconut oil ester enters from the top of the membrane sulfonation reactor, and a thin liquid film is formed along the inner wall of the sulfonation tube. At the same time, the mixed gas containing SO3 is filtered through a filter according to a ratio and enters the top of the membrane sulfonator. The two flow downward in parallel, and SO3 quickly completes the gas-liquid sulfonation reaction on the liquid film to obtain sulfonated coconut oil ester. The sulfonator jacket is connected to circulating water to ensure a suitable reaction temperature. The sulfonated coconut oil ester flows out from the lower part of the sulfonation tube and enters an aging device to age the sulfonated coconut oil ester; subsequently, the sulfonated coconut oil ester obtained by the aging treatment is neutralized with an alkaline solution to obtain a sulfonated coconut oil ester product.
[0082] As described above, the present invention specifically selects low-iodine coconut oil acid and long-chain carbon alcohol as raw materials, obtains coconut oil ester by esterification reaction, and then sulfonates it by using mixed gas containing SO3 gas as sulfonating agent. The operation is simple, the reaction is fast, the efficiency is high, the environment is environmentally friendly, and the process can be industrialized.
[0083] Correspondingly, the present invention also provides a sulfonated emulsifier, which is prepared by the above preparation method.
[0084] The sulfonated emulsifier obtained by the method provided by the present invention has a lower iodine value, excellent yellowing resistance, good stability and good emulsification ability.
[0085] In some optional embodiments, the combined SO3 content of the sulfonated emulsifier is 4% to 8%. In some more typical embodiments, the combined SO3 content of the sulfonated emulsifier is 4.6% to 7.9%.
[0086] In some optional embodiments, the iodine value of the sulfonated emulsifier does not exceed 3 g / 100 g. In some more typical embodiments, the iodine value of the sulfonated emulsifier does not exceed 1.4 g / 100 g.
[0087] In some optional embodiments, the pH value (10%) of the sulfonated emulsifier is 7.5-10.5.
[0088] In addition, the present invention also provides an application of the above-mentioned sulfonated emulsifier, for example, using the sulfonated emulsifier in a leather processing process can solve or improve the problem of oxidative yellowing of leather products caused by using a fatliquor in the leather fatliquor process in the prior art.
[0089] In addition, the present invention also provides a leather, wherein the raw materials for preparing the leather include the above-mentioned sulfonated emulsifier, and the leather can have good softness, oiliness, and mercerization, and has good resistance to oxidation and yellowing.
[0090] The features and performance of the present invention are further described in detail below in conjunction with the embodiments.
[0091] Example 1
[0092] This embodiment provides a sulfonated emulsifier, and the preparation method thereof is as follows:
[0093] S1: preparing cocoate.
[0094] 21 kg of coconut oleic acid and 15.8 kg of n-decanol (i.e., the molar ratio of coconut oleic acid to fatty alcohol is 1:1) are put into a reactor, and after the temperature is raised to 60°C, 0.1 kg of p-toluenesulfonic acid (i.e., p-toluenesulfonic acid is about 0.27% of the total mass of coconut oleic acid and fatty alcohol) is added, and the temperature is maintained at 90°C for esterification. During the reaction, the vacuum pump is started, and the vacuum dehydration treatment is continuously performed. The esterification is terminated after 6 hours to obtain coconut ester (such as Figure 1 shown).
[0095] The results show that the water content of the coconut oil ester is 0.25%, the iodine value is 5.24 g / 100 g, the acid value is 5.11 mg NaOH / g, and the esterification rate is above 95%.
[0096] S2: Preparation of sulfonated emulsifier.
[0097] 36 kg of the above-mentioned coconut ester is pumped into the membrane sulfonation reactor (entering from the top) by a feed pump to form a thin liquid film on the inner wall of the sulfonation tube. At the same time, the mixed gas of SO3 and air (containing 5vt% SO3) is filtered through a filter and sent into the membrane sulfonation reactor (entering from the top), wherein the molar ratio of coconut ester to SO3 is 1.2:1. The two flow downward in parallel, and the temperature of the membrane sulfonation reactor is maintained at 60°C through the sulfonator jacket to externally connect circulating water until the SO3 gas is stable (the reaction time is about 1.2min) and the reaction is completed. The effluent is collected and sent to the aging kettle for aging. The aging temperature is maintained at 65°C and kept warm for 4h. After the aging is completed, a sodium hydroxide solution with a mass concentration of 50% is added in an amount of 50wt% of the sulfonated coconut ester. The temperature is maintained at 50°C for 3h. The pH (10%) is measured to be 9.7 to obtain the finished sulfonated coconut ester (such as Figure 2 shown).
[0098] The test showed that the sulfonated coconut ester had a combined SO3 content of 6.2%, an iodine value of 0.7 g / 100 g, was stable in acid and alkali resistance for 24 hours, and was stable in sodium salt resistance for 24 hours.
[0099] The above acid and alkali resistance and sodium salt resistance are tested in the following ways:
[0100] The specific test method for acid resistance stability is as follows: Measure 80ml of 55℃~60℃ distilled water into a 100ml stoppered measuring cylinder, add 10ml of the sample, cover the bottle stopper, and shake well. Add 10ml of 10% formic acid solution test liquid into the above stoppered measuring cylinder, cover the bottle stopper, turn it upside down for 1min (about 30 times), and shake well. Place it in an environment of 20℃~25℃, and observe after standing for 1h, 2h, 4h and 24h.
[0101] The specific test method for alkali resistance stability is as follows: measure 80ml of distilled water at 55℃~60℃ into a 100ml stoppered measuring cylinder, add 10ml of the sample, cover the bottle stopper, and shake well. Add 10ml of alkali test solution (1mol / L, 28% ammonia 68ml and distilled water to 1000ml) into the above stoppered measuring cylinder, cover the bottle stopper, turn it upside down for 1min (about 30 times), and shake well. Place it in an environment of 20℃~25℃, and observe it after standing for 1h, 2h, 4h and 24h.
[0102] The specific test method for sodium salt resistance stability is as follows: 80 ml of 55℃~60℃ distilled water is measured in a 100ml stoppered measuring cylinder, 10 ml of the sample is added, the stopper is tightly closed, and the mixture is shaken thoroughly. 10 ml of sodium salt test solution (10%, 50 g of sodium chloride and 50 g of sodium sulfate dissolved in 1000 ml of distilled water) is added to the above stoppered measuring cylinder, the stopper is tightly closed, and the mixture is turned upside down for 1 min (about 30 times), and the mixture is shaken thoroughly. The mixture is placed in an environment of 20℃~25℃, and the mixture is observed after standing for 1h, 2h, 4h and 24h.
[0103] Example 2
[0104] This embodiment provides a sulfonated emulsifier, and the preparation method thereof is as follows:
[0105] S1: preparing cocoate.
[0106] 46 kg of coconut oleic acid and 37 kg of dodecanol (i.e., the molar ratio of coconut oleic acid to dodecanol is 1.1:1) are put into a reactor, and after the temperature is raised to 60° C., 0.3 kg of p-toluenesulfonic acid (i.e., p-toluenesulfonic acid is about 0.36% of the total mass of coconut oleic acid and fatty alcohol) is added, and the temperature is maintained at 95° C. for esterification reaction. During the reaction, a vacuum pump is started, and vacuum dehydration treatment is continuously performed. The esterification is completed after 8 hours to obtain coconut ester.
[0107] The results show that the water content of the coconut oil ester is 0.11%, the iodine value is 5.05 g / 100 g, the acid value is 4.06 mg NaOH / g, and the esterification rate is above 95%.
[0108] S2: Preparation of sulfonated emulsifier.
[0109] 83 kg of the above-mentioned coconut ester is pumped into the membrane sulfonation reactor (entering from the top) by a feed pump to form a thin liquid film on the inner wall of the sulfonation tube. At the same time, the mixed gas of SO3 and air (containing 6vt% SO3) is filtered through a filter and sent into the membrane sulfonation reactor (entering from the top), wherein the molar ratio of coconut ester to SO3 is 1:1. The two flow downward in parallel, and the temperature of the membrane sulfonation reactor is maintained at 70°C through the sulfonator jacket with external circulating water until the SO3 gas is stable (the reaction time is about 1.5 min) and the reaction is completed. The effluent is collected and sent to the aging kettle for aging. The aging temperature is maintained at 80°C and kept warm for 3 hours. After the aging is completed, a sodium hydroxide solution with a mass concentration of 60% is added in an amount of 45wt% of the sulfonated coconut ester. The temperature is maintained at 60°C for 2 hours. The pH (10%) is measured to be 10.2 to obtain the finished sulfonated coconut ester (such as Figure 3 shown).
[0110] The test showed that the sulfonated coconut ester had a combined SO3 content of 7.5%, an iodine value of 0g / 100g, was stable in acid and alkali resistance for 24 hours, and was stable in sodium salt resistance for 24 hours.
[0111] Example 3
[0112] This embodiment provides a sulfonated emulsifier, and the preparation method thereof is as follows:
[0113] S1: preparing cocoate.
[0114] 42 kg of coconut oleic acid and 46 kg of hexadecanol (i.e., the molar ratio of coconut oleic acid to hexadecanol is 1.05:1) are put into a reactor, and after the temperature is raised to 100° C., 0.3 kg of p-toluenesulfonic acid (i.e., p-toluenesulfonic acid is about 0.34% of the total mass of coconut oleic acid and fatty alcohol) is added, and the temperature is maintained at 100° C. for esterification reaction. During the reaction, a vacuum pump is started, and vacuum dehydration treatment is continuously performed. The esterification is completed after 7 hours to obtain coconut ester.
[0115] The results show that the water content of the coconut oil ester is 0.16%, the iodine value is 4.99 g / 100 g, the acid value is 4.38 mg NaOH / g, and the esterification rate is above 95%.
[0116] S2: Preparation of sulfonated emulsifier.
[0117] 88 kg of the above-mentioned coconut ester is pumped into the membrane sulfonation reactor (entering from the top) by a feed pump to form a thin liquid film on the inner wall of the sulfonation tube. At the same time, the mixed gas of SO3 and air (containing 4.5vt% SO3) is filtered through a filter and sent into the membrane sulfonation reactor (entering from the top), wherein the molar ratio of coconut ester to SO3 is 1.1:1. The two flow downward in parallel, and the temperature of the membrane sulfonation reactor is maintained at 55°C through the sulfonator jacket and externally connected to circulating water until the SO3 gas is stable (reaction time is about 1min) and the reaction is completed. The effluent is collected and sent to the aging kettle for aging. The aging temperature is maintained at 70°C and kept warm for 5h. After the aging is completed, a sodium hydroxide solution with a mass concentration of 40% is added in an amount of 50wt% of the sulfonated coconut ester. The temperature is maintained at 55°C for 6h. The pH (10%) is measured to be 8.8 to obtain the finished sulfonated coconut ester (such as Figure 4 shown).
[0118] The test showed that the sulfonated coconut ester had a combined SO3 content of 5.5%, an iodine value of 1.1 g / 100 g, was stable in acid and alkali resistance for 24 hours, and was stable in sodium salt resistance for 24 hours.
[0119] Example 4
[0120] This embodiment provides a sulfonated emulsifier, and the preparation method thereof is as follows:
[0121] S1: preparing cocoate.
[0122] 42 kg of coconut oleic acid and 31 kg of dodecanol (i.e., the molar ratio of coconut oleic acid to dodecanol is 1.2:1) are put into a reactor, and after the temperature is raised to 60° C., 0.17 kg of p-toluenesulfonic acid (i.e., p-toluenesulfonic acid is about 0.23% of the total mass of coconut oleic acid and fatty alcohol) is added, and the temperature is maintained at 85° C. for esterification reaction. During the reaction, a vacuum pump is started, and vacuum dehydration treatment is continuously performed. The esterification is completed after 5 hours to obtain coconut ester.
[0123] The results show that the water content of the coconut oil ester is 0.28%, the iodine value is 5.37 g / 100 g, the acid value is 5.18 mg NaOH / g, and the esterification rate is above 95%.
[0124] S2: Preparation of sulfonated emulsifier.
[0125] 73kg of the above-mentioned coconut oil ester is pumped into the membrane sulfonation reactor (entering from the top) by a feed pump to form a thin liquid film on the inner wall of the sulfonation tube. At the same time, the mixed gas of SO3 and air (containing 7vt% SO3) is filtered through a filter and sent to the membrane sulfonation reactor (entering from the top), wherein the molar ratio of coconut oil ester to SO3 is 1.15:1. The two flow down in parallel, and the temperature of the membrane sulfonation reactor is maintained at 60°C through the sulfonator jacket and the circulating water is connected externally until the SO3 gas is stable (the reaction time is about 1.5min) to complete the reaction. The effluent is collected and aged in an aging kettle, and the aging temperature is maintained at 60°C for 5h. After the aging is completed, a sodium hydroxide solution with a mass concentration of 60% is added, and the amount is 45wt% of the sulfonated coconut oil ester, and the temperature is maintained at 60°C for 3h. The pH (10%) is measured to be 9.4 to obtain the sulfonated coconut oil ester finished product.
[0126] The test showed that the combined SO3 content of the sulfonated coconut ester was 4.8%, the iodine value was 0.9g / 100g, it was stable in acid and alkali resistance for 24 hours, and stable in sodium salt resistance for 24 hours.
[0127] Example 5
[0128] This embodiment provides a sulfonated emulsifier, and the preparation method thereof is as follows:
[0129] S1: preparing cocoate.
[0130] 42 kg of coconut oleic acid and 46 kg of hexadecanol (i.e., the molar ratio of coconut oleic acid to hexadecanol is 1.05:1) are put into a reactor, and after the temperature is raised to 60° C., 0.09 kg of p-toluenesulfonic acid (p-toluenesulfonic acid is about 0.1% of the total mass of coconut oleic acid and fatty alcohol) is added, and the temperature is maintained at 80° C. for esterification. During the reaction, a vacuum pump is started, and vacuum dehydration treatment is continuously performed. The esterification is completed after 8 hours to obtain coconut ester.
[0131] The results show that the water content of the coconut oil ester is 0.33%, the iodine value is 5.48 g / 100 g, the acid value is 5.11 mg NaOH / g, and the esterification rate is above 95%.
[0132] S2: Preparation of sulfonated emulsifier.
[0133] 88kg of the above-mentioned coconut oil ester is pumped into the membrane sulfonation reactor (entering from the top) by a feed pump to form a thin liquid film on the inner wall of the sulfonation tube. At the same time, the mixed gas of SO3 and air (containing 3vt% SO3) is filtered through a filter and sent into the membrane sulfonation reactor (entering from the top), wherein the molar ratio of coconut oil ester to SO3 is 1.3:1. The two flow down in parallel, and the temperature of the membrane sulfonation reactor is kept at 50°C by connecting the sulfonator jacket with external circulating water until the SO3 gas is stable (the reaction time is about 2min) to complete the reaction. The effluent is collected and aged in an aging kettle, and the aging temperature is maintained at 50°C for 6h. After the aging is completed, a potassium hydroxide solution with a mass concentration of 55% is added, and the amount is 45wt% of the sulfonated coconut oil ester, and the temperature is kept at 40°C for 6h. The pH (10%) is measured to be 10.0 to obtain the sulfonated coconut oil ester finished product.
[0134] The test showed that the combined SO3 content of the sulfonated coconut ester was 4.6%, the iodine value was 1.4g / 100g, it was stable in acid and alkali resistance for 24 hours, and stable in sodium salt resistance for 24 hours.
[0135] Example 6
[0136] This embodiment provides a sulfonated emulsifier, and the preparation method thereof is as follows:
[0137] S1: preparing cocoate.
[0138] 42 kg of coconut oleic acid and 46 kg of hexadecanol (i.e., the molar ratio of coconut oleic acid to hexadecanol is 1.05:1) are put into a reactor, and after the temperature is raised to 60° C., 0.44 kg of p-toluenesulfonic acid (p-toluenesulfonic acid is about 0.5% of the total mass of coconut oleic acid and fatty alcohol) is added, and the temperature is maintained at 110° C. for esterification. During the reaction, a vacuum pump is started, and vacuum dehydration treatment is continuously performed. The esterification is completed after 4 hours to obtain coconut ester.
[0139] The results show that the water content of the coconut oil ester is 0.06%, the iodine value is 4.67 g / 100 g, the acid value is 3.95 mg NaOH / g, and the esterification rate is above 95%.
[0140] S2: Preparation of sulfonated emulsifier.
[0141] 88kg of the above-mentioned coconut oil ester is pumped into the membrane sulfonation reactor (entering from the top) by a feed pump to form a thin liquid film on the inner wall of the sulfonation tube. At the same time, the mixed gas of SO3 and air (containing 8vt% SO3) is filtered through a filter and sent into the membrane sulfonation reactor (entering from the top), wherein the molar ratio of coconut oil ester to SO3 is 1.05:1. The two flow down in parallel, and the temperature of the membrane sulfonation reactor is kept at 80°C by connecting the sulfonator jacket with external circulating water until the SO3 gas is stable (the reaction time is about 1min) to complete the reaction. The effluent is collected and aged in an aging kettle, and the aging temperature is maintained at 80°C for 3h. After the aging is completed, a sodium hydroxide solution with a mass concentration of 70% is added, and the amount is 50wt% of the sulfonated coconut oil ester, and the temperature is maintained at 60°C for 2h. The pH (10%) is measured to be 10.5 to obtain the sulfonated coconut oil ester finished product.
[0142] The test showed that the sulfonated coconut ester had a combined SO3 content of 7.9%, an iodine value of 0g / 100g, was stable in acid and alkali resistance for 24 hours, and was stable in sodium salt resistance for 24 hours.
[0143] Comparative Example 1
[0144] The difference between this comparative example and Example 2 is that the volume percentage of SO3 contained in the mixed gas is 1%.
[0145] Comparative Example 2
[0146] The difference between this comparative example and Example 2 is that the volume percentage of SO3 contained in the mixed gas is 10%.
[0147] Comparative Example 3
[0148] The difference between this comparative example and Example 2 is that the molar ratio of coconut oil ester to SO3 in the sulfonating agent is 1:1.5.
[0149] Comparative Example 4
[0150] The difference between this comparative example and Example 2 is that the molar ratio of coconut oil ester to SO3 in the sulfonating agent is 2:1.
[0151] Comparative Example 5
[0152] The difference between this comparative example and Example 2 is that the temperature of the gas-liquid sulfonation reaction is 40°C.
[0153] Comparative Example 6
[0154] The difference between this comparative example and Example 2 is that the temperature of the gas-liquid sulfonation reaction is 90°C.
[0155] Comparative Example 7
[0156] The difference between this comparative example and Example 2 is that no aging treatment is performed during the preparation of the sulfonated emulsifier.
[0157] Comparative Example 8
[0158] The difference between this comparative example and Example 2 is that the aging temperature is 40°C.
[0159] Comparative Example 9
[0160] The difference between this comparative example and Example 2 is that the aging time is 2h.
[0161] Comparative Example 10
[0162] The difference between this comparative example and Example 2 is that no neutralization treatment is performed during the preparation of the sulfonated emulsifier.
[0163] Comparative Example 11
[0164] The difference between this comparative example and Example 2 is that the amount of the neutralizer used is 30wt% of the sulfonated coconut oil ester after aging treatment.
[0165] Comparative Example 12
[0166] The difference between this comparative example and Example 2 is that the neutralization time is 1 h.
[0167] The performance of the sulfonated emulsifiers obtained in Examples 1 to 6 and Comparative Examples 1 to 12 is summarized in Table 1. Among them, the samples of Comparative Examples 2, 3, 6, 7, 8, 9, 10, 11 and 12 have poor stability, delamination, dark color and opaqueness.
[0168] Table 1 Performance of sulfonated emulsifier
[0169]
[0170]
[0171] It can be seen from Table 1 that the sulfonated emulsifier prepared in the embodiment of the present invention can have a lower iodine value, good stability, and excellent yellowing resistance.
[0172] The yellowing resistance levels of Examples 1 to 6 are the same, namely: color fastness to artificial light level 4, heat resistance level 4, and resistance to hot and humid climate level 4.5. For comparison, the sulfonated oil product RS of Brother Technology Co., Ltd. has a yellowing resistance level of: color fastness to artificial light level 2, heat resistance level 1.5, and resistance to hot and humid climate level 3.5. The detection method of color fastness to artificial light refers to QB / T2727-2017, and the detection methods of heat resistance and resistance to hot and humid climate refer to QB / T 5250-2018.
[0173] In summary, the present invention uses gas containing SO3 as a sulfonating agent, has the advantages of strong sulfonating ability, fast reaction, no generation of H2O and a large amount of waste acid, and controls the volume content of SO3 in the mixed gas to 3% to 8%, which can ensure more uniform sulfonation, not only avoid over-sulfonation and coking, improve product stability, but also ensure that the product has good emulsification properties. The sulfonated emulsifier obtained by the above method has a lower iodine value, excellent yellowing resistance, good stability, and good emulsification ability, and can be used in the leather fatliquor process to improve the oxidative yellowing resistance of the fatliquor.
[0174] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. For those skilled in the art, the present invention may have various modifications and variations. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present invention shall be included in the protection scope of the present invention.
Claims
1. A method for preparing a sulfonated emulsifier, characterized in that: The following steps are involved: Carrying out gas-liquid sulfonation reaction between coconut ester and a sulfonating agent to obtain sulfonated coconut ester; Wherein, the sulfonating agent is a mixed gas of SO3 and air, and the volume percentage of SO3 contained in the mixed gas is 3% to 8%.
2. The preparation method according to claim 1, characterized in that: The gas-liquid sulfonation reaction has at least one of the following characteristics: Feature 1: The molar ratio of the coconut ester to the SO3 in the sulfonating agent is 1:1 to 1.5:1; Feature 2: The temperature of the gas-liquid sulfonation reaction is 50°C to 80°C; Feature 3: The time of gas-liquid sulfonation reaction is 1min to 2min; Feature 4: The iodine value of the cocoate is no more than 5.5 g / 100 g.
3. The preparation method according to claim 1 or 2, characterized in that: Also includes: Carrying out an aging treatment on the sulfonated coconut oil ester; The temperature of the aging treatment is 50°C to 80°C, and the time of the aging treatment is 3h to 6h.
4. The preparation method according to claim 3, characterized in that: Also includes: neutralizing the aged sulfonated coconut ester; The temperature of the neutralization treatment is 40°C to 60°C, and the time of the neutralization treatment is 2h to 6h; Preferably, the neutralizing agent used in the neutralization treatment is an alkaline solution; Preferably, the amount of the neutralizing agent used is 45 wt% to 50 wt% of the sulfonated coconut ester after aging treatment.
5. The preparation method according to claim 1, characterized in that: The preparation of the coconut ester comprises: carrying out an esterification reaction between coconut oleic acid and fatty alcohol under the condition of p-toluenesulfonic acid as a catalyst; The temperature of the esterification reaction is 80°C to 110°C, and the time of the esterification reaction is 4h to 8h; Preferably, the fatty alcohol is a saturated alkyl alcohol having 10 to 16 carbon atoms; more preferably, the fatty alcohol includes at least one of n-decanol, dodecanol and hexadecanol; Preferably, the molar ratio of the coconut oleic acid to the fatty alcohol is 1:1 to 1.3:1; Preferably, the amount of the catalyst used is 0.1% to 0.5% of the total mass of the coconut oleic acid and the fatty alcohol.
6. The preparation method according to claim 5, characterized in that: Also includes: The coconut ester obtained by the esterification reaction is subjected to vacuum dehydration treatment.
7. A sulfonated emulsifier, characterized in that: The invention is prepared by the preparation method according to any one of claims 1 to 6.
8. The sulfonated emulsifier according to claim 7, characterized in that The sulfonated emulsifier has at least one of the following characteristics: Feature 5: The combined SO3 content of the sulfonated emulsifier is 4% to 8%; Feature 6: The iodine value of the sulfonated emulsifier does not exceed 3g / 100g.
9. Use of a sulfonated emulsifier as claimed in claim 7 or 8, characterized in that: The sulfonated emulsifier is used in leather processing.
10. A leather, characterized in that: The raw materials for preparing the leather include the sulfonated emulsifier according to claim 6 or 7.