Method for preparing sodium carbonate by-products gypsum and calcium chloride from chemical high-salinity wastewater
By preparing saturated sodium chloride solution and calcium sulfate precipitate, sodium carbonate is produced by ammonia alkali method and calcined, gypsum is prepared by seed crystal method, and carbon dioxide and ammonia are recovered through ammonia distillation reaction, the high investment in chemical high-salt wastewater treatment is solved , the problem of high operating costs has achieved efficient and low-cost resource utilization and environmental protection properties.
Patent Information
- Application Number
- CN202411098935.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-12
- Publication Date
- 2024-11-22
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
During the treatment of high-salt wastewater in chemical industry, there are large investment, high operating costs, low value of crystalline salt produced by the salt separation system, and high cost of hazardous waste disposal. It is difficult for the existing technology to simplify the treatment process, reduce costs, and achieve high-value utilization. .
By preparing saturated sodium chloride solution and calcium sulfate precipitate, sodium carbonate is produced by ammonia alkali method and calcined to obtain sodium carbonate. Gypsum is prepared by seed crystal method, and carbon dioxide and ammonia are recovered through ammonia distillation reaction to achieve liquid conversion and resource utilization , reduce processing costs and improve preparation efficiency.
It has achieved simplification of process flow, improved preparation efficiency, reduced costs, enhanced resource utilization, reduced environmental pollution, and improved the economic benefits of products.
Smart Images

Figure CN118993109A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of comprehensive resource utilization, and specifically relates to a method for preparing soda ash by-product gypsum and calcium chloride from chemical high-salt wastewater. Background Art
[0002] The aforementioned chemical high-salt wastewater refers to wastewater containing high concentrations of soluble inorganic salts, more specifically, wastewater generated in the production process of industries such as coal chemical industry, petrochemical industry, fine chemical industry, printing and dyeing pharmaceutical industry, pesticide, metallurgy, coking, phosphorus chemical industry, etc., which is concentrated after zero-emission treatment. Usually, the mass fraction of total dissolved solids (TDS) is greater than 3.5‰ (i.e., TDS>35000mg / L), the content of sodium sulfate and sodium chloride is greater than 90%, and it also contains about 5% of other inorganic salts and organic matter. As can be seen from the above, the generation of chemical high-salt wastewater is quite extensive and has been increasing in recent years. Therefore, how to make high-value use of high-salt wastewater has become a practical problem that people pay attention to and hope to solve effectively.
[0003] If the sodium sulfate / sodium chloride after salt separation is directly used to prepare dilute acid and dilute alkali, it will not be valued by people due to the large investment and low efficiency; if sodium chloride is used for ion membrane caustic soda, that is, caustic soda (NaOH) is prepared by electrolyzing brine with ion exchange membrane method, although it has the advantages of high purity of the obtained caustic soda, low loss compared with the diaphragm method, low investment cost, pollution-free and relatively improved production efficiency, it has high requirements on the quality of brine, and the ion membrane is expensive and easy to damage. For example, even if the addition amount is controlled to 10-20%, it will still cause the electrolytic cell to be blocked, affecting the smooth progress of the preparation.
[0004] At present, the process flow commonly used for zero-discharge treatment of industrial wastewater is: advanced oxidation (degrading organic pollutants in water by producing hydroxyl free radicals (·OH) with strong oxidizing ability) → biochemical treatment system (using the life activities of microorganisms to remove organic pollutants in wastewater) → membrane treatment system (such as using microfiltration membranes, ultrafiltration membranes, nanofiltration membranes or reverse osmosis membranes) → salt separation system (separating and separating salt substances in wastewater) → evaporation crystallization system (changing the solution from unsaturated to saturated state and then crystallizing). This process flow has the following shortcomings: large investment and high operating costs. The crystallized salt produced by the salt separation system, that is, sodium salt, is mainly sodium sulfate and sodium chloride. The sodium salt has low added value and relatively narrow or even no use; if the crystallized mixed salt produced by the salt separation is not separated, it is hazardous waste. At present, the disposal cost of such hazardous waste is 2,000 to 3,000 yuan / ton, which brings a large economic burden to chemical companies.
[0005] Chemical high-salt wastewater has the characteristics of difficulty in disposal, high cost, and harm to the environment due to its wide sources, various types, and complex toxic and harmful components. However, it also has both environmental and resource attributes. Depending on the different chemical products, the composition of the wastewater is different, and even has significant differences, which increases the difficulty of treatment and utilization.
[0006] At present, there are many methods for resource utilization of chemical high-salt wastewater, typical examples include direct salt separation (including thermal salt separation, membrane salt separation, hot and cold + membrane and other process routes to separate sodium sulfate and sodium chloride); high-temperature pyrolysis of solid waste salt and dissolving it in water for salt separation, and the separated sodium sulfate and sodium chloride are used to make ammonium salt as a by-product of soda ash; solid sodium sulfate is obtained after liquid phase salt separation to make ammonium sulfate as a by-product of soda ash; the solid sodium chloride obtained after liquid phase salt separation is used for ion membrane caustic soda, etc.
[0007] CN111592161A discloses a novel integrated treatment method for zero discharge of high-salt wastewater in coal chemical industry, and its integrated treatment process includes five parts: hardness and silicon removal unit, advanced oxidation composite organic matter removal unit, turbidity removal and deep softening unit, membrane reduction and concentration unit, salt and nitrate separation unit and evaporation crystallization unit. The salt separation adopts membrane method + hot and cold method to separate and crystallize sodium sulfate and sodium chloride in water, but the final system impurity salt rate is 15-20%. Generally speaking, the cost of salt separation is 1,000 yuan per ton (based on the current treatment cost), while the price of sodium sulfate on the market is 100-300 yuan and the price of sodium chloride is 50-150 yuan, which leads to a loss; at the same time, with the gradual promotion of salt separation technology, most of the chemical clusters in China have gradually realized the separation of sodium sulfate and sodium chloride at this stage, and the output has increased year by year, resulting in a continuous decline in market digestion capacity and a phenomenon of sluggish sales of by-product salt in some areas.
[0008] CN116272743A provides a solid waste sodium salt regeneration soda ash device and method, including a solid waste refining system, a baking soda reaction system, an ammonia distillation system, an ammonium chloride system, an ammonium sulfate refining kettle, and a sulfuric acid evaporator; the solid waste refining system includes a high-temperature cracking furnace (for high-temperature cracking to remove organic matter), a dissolving tank, and an impurity dehydrator connected in sequence; the baking soda reaction system includes a single-pass reactor and a double-pass reactor connected to a soda tower, and the single-pass reactor is connected to the double-pass reactor; the ammonia distillation system includes an ammonia distillation tower and an absorption tower; the dissolving tank is connected to the absorption tower through a pipeline, the absorption tower is connected to the single-pass reactor, and the double-pass reactor is connected to the ammonia distillation tower; the ammonium chloride system is connected to the ammonia distillation tower and the absorption tower respectively, and the ammonia distillation tower is connected to the ammonium sulfate refining kettle and the ammonium sulfate evaporator in sequence. The present invention can refine and regenerate solid hazardous waste sodium sulfate / sodium chloride into soda ash as a chemical basic raw material, and simultaneously produce high-value-added agricultural grade ammonium sulfate / ammonium chloride as a by-product. However, high-temperature cracking to remove organic matter consumes a lot of energy and the effect is not obvious, and the by-product ammonium salt will lead to an inverted cost of ammonia. Moreover, the use of by-product ammonium sulfate / ammonium chloride in agriculture has always been controversial and the country has not explicitly permitted it.
[0009] CN111039304A introduces a method for preparing ammonium sulfate and sodium bicarbonate from sodium sulfate, which uses an ammonium source as a conversion medium for preparing ammonium sulfate and sodium bicarbonate from sodium sulfate, and the ammonium source includes any one of diammonium hydrogen phosphate, ammonium formate or ammonium nitrate, or a mixture of at least two of them. Although the method has the advantages of simple process, sodium sulfate utilization rate>85%, sodium bicarbonate purity≥90%, and the purity of ammonium sulfate product meets the requirements of GB535-1995. However, due to organic interference, the purity of soda ash needs to be further improved; the system requires solid sodium sulfate input, which needs to be evaporated and crystallized, and the double decomposition reaction needs to be dissolved in water, which is repeatedly dry and wet, and the cost is high; and the double decomposition reaction link needs to maintain the stability of the quaternary phase diagram, which is very difficult; in addition, the by-product ammonium salt will lead to an inverted cost of ammonia.
[0010] CN215250125U discloses a supercritical fluid extraction and electrochemical coupling treatment system for high-salt and high-organic wastewater, including a supercritical CO2 extraction and separation unit, an organic supercritical water treatment unit and a salt water electrocatalytic treatment unit; the supercritical CO2 extraction and separation unit is connected to the organic supercritical water treatment unit and the salt water electrocatalytic treatment unit through pipelines; wherein the supercritical CO2 extraction and separation unit is used to treat the wastewater to separate it into high salt water and extract, the salt water electrocatalytic treatment unit is used to electrocatalytically treat the high salt water, and the organic supercritical water treatment unit is used to perform supercritical water treatment on the extract. The organic content of the high-salt and high-concentration organic wastewater treated by this system directly meets the requirements of the refined dry salt for ion-exchange membrane caustic soda in "Salt for Ion-Exchange Membrane Caustic Soda" QB / T 5270-2018, where TOC <10mg / kg is required. However, supercritical water treatment requires high temperature and pressure, so the equipment investment is large and the operating costs are high. In addition, the ion membrane caustic soda system has strict requirements on the purity of sodium chloride. Existing cases show that the amount of waste salt added accounts for only 10-20%.
[0011] Therefore, how to make chemical high-salt wastewater meet the requirements of simplifying the treatment process, reducing treatment costs, reflecting clean production, liquid conversion without salt separation, and reflecting high-value utilization has become a technical problem that urgently needs to be solved in this field. Summary of the invention
[0012] The task of the present invention is to provide a method for preparing soda ash by-product gypsum and calcium chloride from chemical high-salt wastewater, which helps to simplify the process flow to reduce the processing cost, is conducive to using carbon dioxide discharged in chemical production as a raw material to reflect good resource utilization, is beneficial to abandoning salt separation and conducting liquid conversion to improve preparation efficiency and significantly save costs, and is convenient to reduce environmental pollution while ensuring good economic benefits to reflect high-value utilization.
[0013] The task of the present invention is accomplished by a method for preparing soda ash by-product gypsum and calcium chloride from chemical high-salt wastewater, comprising the following steps:
[0014] S1) preparing a saturated sodium chloride solution, first removing impurities from chemical high-salt wastewater, then deeply removing hardness and evaporating and concentrating to obtain a saturated sodium chloride solution and a calcium sulfate precipitate;
[0015] S2) preparing sodium carbonate, using an ammonia-soda process to react the saturated sodium chloride solution obtained in step S1 with ammonia and carbon dioxide to obtain sodium bicarbonate and a sodium bicarbonate mother liquor, and calcining the sodium bicarbonate to obtain sodium carbonate;
[0016] S3) preparing gypsum by using a seed crystal method to prepare gypsum from the calcium sulfate precipitate obtained in step S1), and controlling the process elements of the preparation to obtain gypsum;
[0017] S4) preparing ammonia evaporation waste liquid, subjecting the sodium bicarbonate mother liquor obtained in step S2) to an ammonia evaporation reaction with lime milk, recovering carbon dioxide and ammonia and recycling them to step S2), and obtaining ammonia evaporation waste liquid;
[0018] S5) Resource utilization of ammonia evaporation waste liquid, the ammonia evaporation waste liquid obtained in step S4) is subjected to solid-liquid separation, and the supernatant obtained after solid-liquid separation is divided into two streams, one of equal amount is used for the impurity removal treatment in step S1), and the other is used for preparing calcium chloride after evaporation and concentration, and sodium chloride therein is recovered and reused in step S1).
[0019] In a specific embodiment of the present invention, the impurity removal treatment of the chemical high-salt wastewater in step S1) includes the following steps in order: removal of inorganic impurities, removal of inert organic matter, removal of heavy metals, removal of potassium ions, removal of nitrates and removal of sulfates; the mass percentage of sodium chloride in the saturated sodium chloride solution is 23-26%; the calcium sulfate precipitate is precipitated calcium sulfate generated by reacting an equivalent amount of the supernatant in step S5) with sodium sulfate in the chemical high-salt wastewater.
[0020] In another specific embodiment of the present invention, the inorganic impurities are removed by using a high-density tank system to remove silicon, fluorine and phosphate in chemical high-salt wastewater, so that the silicon content is ≤5mg / L, the fluorine content is ≤1mg / L and the phosphate in terms of phosphorus is ≤1mg / L. The high-density tank system includes a coagulation tank, a reagent addition tank, a reaction tank, a flocculation tank and an inclined tube sedimentation tank; the inert organic matter is removed by using a functional nano-adsorption material to absorb and separate the inert COD in the chemical high-salt wastewater and make the removal rate reach more than 90%. The functional nano-adsorption material has a pore size of 0.1-5nm and a density of 1.3g / cm 3 , porosity is 75-80%, specific surface area is 1000-1500m2 / g of mesoporous carbon composite materials and microporous carbon composite materials; the removal of heavy metals is to use a polymer chelating agent to adsorb and separate lead, arsenic, mercury and chromium in chemical high-salt wastewater; the removal of potassium ions is to use modified clinoptilolite to adsorb and separate potassium ions; the removal of nitrate ions is to use a micro-electric field reduction method to make the nitrate ions in the chemical high-salt wastewater ≤20mg / L; the removal of sulfate ions is to use calcium chloride in ammonia waste liquid to react with sodium sulfate in high-salt wastewater to make the sodium sulfate in the chemical high-salt wastewater ≤1000mg / L.
[0021] In another specific embodiment of the present invention, the deep hardness removal treatment in step S1) is to remove the residual Mg in the solution by using a two-alkali method. 2+ and Ca 2+ , and by OH - The residual Mg in the solution 2+ Reaction to form magnesium hydroxide precipitate, making the Mg in the brine 2+ <20mg / L,CO3 2- It reacts with the residual calcium ions in the solution to form calcium carbonate precipitates, reducing the Ca in the brine. 2+ <30mg / L, the device used for evaporation and concentration is an MVR evaporator or a multiple-effect evaporator, the inlet temperature is 100°C, the saturation temperature rise is 16°C, the shell side material is 316L, and the tube side and impeller are made of titanium.
[0022] In another specific embodiment of the present invention, the ammonia-soda method described in step S2) includes the following steps: ammoniation, carbonation, filtration and calcination, and uses carbon dioxide (CO2) discharged in chemical production as a raw material, and the purity of the obtained sodium carbonate is 99%; the calcination temperature is 160-190° C., and the calcination time is 20-30 min;
[0023] In another specific embodiment of the present invention, the process elements for controlling the preparation in step S3) are: first, the calcium sulfate precipitate obtained in step S1) is introduced into a crystallization pool and the pH value of the feed solution is controlled to be 10-11, and then gypsum seeds are added to the crystallization pool to react with calcium and sulfate ions in the calcium sulfate precipitate and the reaction time is controlled, and then crystallization precipitation is carried out and the crystallization precipitation time is controlled, and then the gypsum is separated by filter pressing with a plate and frame filter device, and finally dried to obtain the by-product gypsum.
[0024] In a more specific embodiment of the present invention, the reaction time is controlled to be 25-35 minutes; the crystal precipitation time is controlled to be 110-130 minutes; the drying is carried out by rotary kiln drying equipment, the drying temperature and the drying time are 200-300°C and 30-60 minutes respectively, and the moisture content of the gypsum is less than 5%;
[0025] In a further specific embodiment of the present invention, the equipment used for the ammonia evaporation reaction in step S4) is an ammonia evaporation tower, the concentration of the lime milk is 160-200tt, the bottom temperature of the ammonia evaporation tower is 110-120°C, and the top temperature is 80-85°C.
[0026] In yet another specific embodiment of the present invention, the ammonia evaporation waste liquid in step S5) contains 12-13% by mass of calcium chloride (CaCl2) and 4-5% by mass of sodium chloride (NaCl), and the solid-liquid separation is to remove the coarse components by a cyclone separator, and then to obtain the supernatant by coagulation and precipitation, which is divided into two streams; the removal of the coarse components is to remove large solid particles including calcium carbonate (CaCO3) and calcium oxide (CaO) brought in by lime milk, so that the solid content is less than 0.5%, and the solid content of the supernatant is 10 mg / L.
[0027] In yet another specific embodiment of the present invention, the evaporation device used for the evaporation concentration in step S5) is an evaporation pond or an evaporator, and the concentration is to concentrate the supernatant to 3-4 times so that the NaCl therein tends to be saturated, and the sodium chloride slurry is obtained after centrifugal separation and is reused in step S1); the steam pressure used in the evaporation pond or evaporator is saturated steam with a temperature of 180-220° C. and a mass percentage of calcium chloride greater than 70%.
[0028] The technical solution provided by the present invention has the following advantages compared with the prior art:
[0029] 1. It adopts mature impurity removal and purification technology and liquid phase continuous treatment to shorten the processing cycle;
[0030] 2. Use ammonia wastewater to remove sulfate, achieve ion balance in the system, optimize salt circulation, and increase NaCl utilization to more than 95%;
[0031] 3. The ammonia-soda method is used to produce soda ash, which has high stability, strong adaptability and strong impact resistance;
[0032] 4. Use ammonia waste liquid to prepare calcium chloride byproduct to achieve chloride ion Cl - High value utilization;
[0033] 5. Using CO2 as raw material, each ton of Na2CO3 absorbs 0.415 tons of carbon dioxide, turning waste into treasure while taking into account carbon emission reduction;
[0034] 6. It not only highlights the environmental protection attribute, but also obtains the resource attribute, realizing the transformation of the environmental protection project from the "losing money to making money" model;
[0035] 7. Sodium carbonate products meet the requirements of Class II first-class products in GB / T 210-2022; sodium bicarbonate (baking soda) meets the requirements of Class II and above product specifications in GB / T1606-2008; calcium chloride products meet the requirements of industrial calcium chloride type II in GB / T26520-2011; gypsum products meet the GB / T 9776-2022 "Building Gypsum" standard. BRIEF DESCRIPTION OF THE DRAWINGS
[0036] Figure 1 Schematic diagram of the process flow of the method of the present invention;
[0037] Figure 2 The schematic diagram of the process flow of removing sulfate and by-product gypsum by the method of the present invention;
[0038] Figure 3 The schematic diagram of the process flow of preparing soda ash by the method of the present invention;
[0039] Figure 4 The present invention is a schematic diagram of the process flow of utilizing ammonia evaporation waste liquid. DETAILED DESCRIPTION
[0040] In order to make the purpose, technical solution and advantages of the present invention clearer, the present invention is further described in detail below. However, it should be understood that the description herein is only used to explain the present invention and is not intended to limit the scope of the present invention.
[0041] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as commonly understood by technicians in the technical field to which the present invention belongs. The terms used in the specification of the present invention are only for the purpose of describing specific embodiments and are not intended to limit the present invention.
[0042] In order to further understand the present invention, the present invention is further described in detail below in conjunction with the best embodiment.
[0043] Embodiment 1:
[0044] See also Figure 1 ,according to Figure 1 The method for preparing soda ash by-product gypsum and calcium chloride from coal chemical high salt of a coal chemical enterprise comprises the following steps:
[0045] S1) preparing a saturated sodium chloride solution, first removing impurities from the coal chemical high-salt wastewater produced in the production of the aforementioned coal chemical enterprise to obtain a saturated sodium chloride solution and a calcium sulfate precipitate, which can also be called a calcium sulfate precipitate suspension. In this step, the water quality of the coal chemical high-salt wastewater produced in the production of the aforementioned coal chemical enterprise is: inert organic matter COD is 1000 mg / L, TDS is 200000 mg / L, total hardness (calculated as CaCO3) is 100 mg / L, nitrate NO3 is 100 mg / L, and the content of ...- The concentration of sodium ions in the high-salt wastewater is 500mg / L, the concentration of sodium ions in the high-salt wastewater is 71000mg / L, the concentration of chloride ions in the high-salt wastewater is 28900mg / L, the concentration of sulfate ions in the high-salt wastewater is 95000mg / L, the pH value is 10, the concentration of potassium ions in the high-salt wastewater is 2000mg / L, the concentration of SiO2 in the high-salt wastewater is 800mg / L, and the concentration of heavy metals in the high-salt wastewater is 6mg / L. The order of removing impurities from the high-salt wastewater of the coal chemical industry is as follows: removing inorganic impurities, removing inert organic matter, removing heavy metals, removing potassium ions, removing nitrate and removing sulfate, and then performing deep hardness removal and evaporation concentration. The mass percentage of sodium chloride in the saturated sodium chloride solution described in this step is 23-26%; ① The removal of inorganic impurities is to use high-density pool technology (i.e., "high-density pool system") to remove silicon, fluorine, phosphate, etc. in the high-salt wastewater of the chemical industry, so that the silicon content (SiO2) is ≤5mg / l, and the fluorine (F - )≤1mg / l, phosphate (total phosphorus, in terms of P)≤1mg / l; the high-density tank system consists of a coagulation tank, a reagent dosing tank, a reaction tank, a flocculation tank and an inclined tube sedimentation tank, the pH value is controlled at 10-12, and hardness, alkalinity, SS, P, Si, F, etc. are removed simultaneously, and some heavy metals, organic matter, oil and other impurities can be removed at the same time; the high-density tank is equipped with a coagulant PAC dosing system, a coagulant aid PAM dosing system, a soda dosing system, a caustic soda dosing system and a stirring system; the surface load of the high-density tank is set to 10-25m 3 / (m 2 ·h); the sludge concentration of the high-density pool is set to 20-50g / l; ② the removal of inert organic matter is to use functional nano-adsorbent materials for adsorption and separation, so that the removal rate of inert COD in chemical high-salt wastewater reaches more than 90%; the functional nano-adsorbent materials are mesoporous carbon composite materials and microporous carbon composite materials with pore diameters of 0.1-5nm and density of 1.3g / cm 3 , porosity 75-80%, specific surface area 1000-1500m 2 / g, the adsorption material is loaded into the adsorption column, each group is 5 columns connected in series, the switching time of each column is preferably 4 to 8 hours, preferably 6 hours (6 hours is selected in this embodiment), the feed flow rate is preferably 1 to 2BV, preferably 1.5BV (1.5BV is selected in this embodiment), and the feed pH is 6 to 7; ③ the removal of heavy metals is carried out by adsorption separation using a polymer chelating agent, so that lead Pb≤0.05mg / l, arsenic As≤0.05mg / l, mercury Hg≤0.0001mg / l, and chromium Cr≤0.05mg / l; the heavy metal removal system includes a filtration unit and a chelating resin unit. According to the structural characteristics and selectivity of the chelating resin, the configured chelating agent reacts with certain metal ions. The formation of a stable complexing effect, the concentration and enrichment of a variety of metal ions, thereby achieving separation; the ratio of the pore diameter of the chelating resin to the diameter of the adsorbed metal ion is preferably 4 to 8:1, preferably 5:1 (5:1 is selected in this embodiment); the chelating agent is preferably one or a combination of phosphonic acid resin, mercapto resin, thiourea resin, and 4-aminotriazole resin; the adsorption selection order is preferably aminophosphonic acid type: Pb>Cu>Fe>Zn>Ca>Cd>Ni>Co>Sr>Ba; preferably mercapto type: Hg>Ag>Cu>Pb>Cd>Ni>Co>Fe>Ca>Na; ④ the removal of potassium ions is carried out by using modified clinoptilolite for adsorption separation, so that the potassium ions K + ≤5mg / l; The modified clinoptilolite adsorption separation system used for removing potassium ions includes a filtration unit and a zeolite adsorption column unit, and the feed pH value is controlled at 6-9. The filtration unit is composed of a multi-media filter and a security filter, one for backup and one for use, and the filter element accuracy of the security filter is 0.5-5μm; the zeolite adsorption column unit, each group is 5 columns in series, and the switching time of each column is preferably 4-8h, preferably 6h (6h is selected in this embodiment), and the feed flow rate is preferably 1-2BV, preferably 1.5BV (1.5BV is selected in this embodiment); ⑤ The removal of nitrate is to use a micro-electric field reduction method to reduce the nitrate (NO3 - )≤20mg / l; the removal of nitrate is carried out by micro-electric field reduction method, an aeration device is provided in the reaction tank, and the reaction is carried out under the action of micro-electric field and catalyst, and an immersed plate made of titanium, iridium and tantalum and an immersed plate made of iron are configured, and the effective area ratio of the titanium, iridium and tantalum plates to the iron plates is 3:1, or 2:1, or 1.5:1, or 1:1, and 2:1 is selected in this embodiment, the feed pH value is 3-5, the water temperature is preferably 20-30°C, preferably 25°C (25°C is selected in this embodiment), the hydraulic retention time is preferably 2-4h, preferably 3h (3h is selected in this embodiment), the air-water ratio of aeration is preferably 5-10:1, and 7:1 is selected in this embodiment, the micro-electric field is input with direct current or alternating current, the input voltage is 1-2.5V, and direct current input is selected in this embodiment, and the plate current density is 0.05mA / cm 2, the distance between the plates is 15cm; ⑥Please refer to Figure 2 And combined with Figure 1 The desulfurization is carried out by reacting calcium chloride (CaCl2) in the ammonia waste liquid with sodium sulfate (Na2SO4) in the high-salt waste water to make the sodium sulfate (Na2SO4) in the brine (i.e., chemical high-salt waste water) ≤1000mg / l; the feed pH value of the desulfurization process is controlled at 10-11, and the CaCl2 in the equivalent amount of the supernatant in step (5) is reacted with Na2SO4 in the chemical high-salt water to generate calcium sulfate (CaSO4) precipitation, and the reaction formula is: Na2SO4+CaCl2→CaSO4↓+2NaCl. The whole process can be obtained by Figure 2 Clearly reveal; ⑦ The deep hardness removal uses a two-base method to remove the residual Mg in the solution 2+ and Ca 2+ ; and by OH - The residual Mg in the solution 2+ Reaction, forming magnesium hydroxide [Mg(OH)2] precipitation, making the Mg in the brine 2+ <20mg / L, first add caustic soda and magnesium ions Mg in the solution 2+ Reaction, the reaction formula is: Mg 2+ +2OH - =Mg(OH)2↓; then add sodium carbonate (Na2CO3) and calcium ions Ca in the solution 2+ Reaction, forming calcium carbonate (CaCO3) precipitation, making the Ca in the brine 2+ <30mg / L, the reaction formula is: Na2CO3+Ca2 + →2Na + +CaCO3↓;⑧ The evaporation concentration adopts MVR evaporator or multi-effect evaporator, forced circulation, inlet temperature is 100℃, saturation temperature rise is 16℃, shell side material is 316L, tube side and impeller are titanium; the mass percentage of saturated sodium chloride solution obtained by ⑦ and ⑧ is 23% to 26%, the turbidity of refined brine is less than 50mg / L, and the refined brine (as Cl - (calculated) concentration (mol / L) ≥5.25.
[0046] S2) preparing sodium carbonate, i.e. preparing soda ash, using an ammonia-soda process to react the saturated sodium chloride solution obtained in step S1) with ammonia and carbon dioxide to obtain sodium bicarbonate and sodium bicarbonate mother liquor, calcining the sodium bicarbonate, the calcination temperature is preferably 160-190° C., preferably 175° C., 175° C. is selected in this embodiment, the calcination time is preferably 20-30 min, preferably 25 min, 25 min is selected in this embodiment, to obtain sodium carbonate, i.e. soda ash, with a purity of 99%. For details, see Figure 3The aforementioned ammonia-soda method includes the following steps: namely, ammoniation, carbonation, filtration and calcination. First, the refined saturated sodium chloride brine is input into the ammoniation unit, and fully absorbs ammonia in the ammonia absorption tower, so that the ammonia brine meets the requirements of the ammonia brine after ammonia absorption; secondly, the carbonation unit receives the ammonia brine that meets the standards, and the solid content of the ammonia brine is less than 100ppm. The carbon dioxide (CO2) discharged in the coal chemical production is used as a raw material to enter the compressor to compress the carbon dioxide (CO2) with a dust content of less than 10mg / m 3 In the carbonation reaction tower, CO2 reacts fully with ammonia water to obtain sodium bicarbonate and ammonium chloride. The amination reaction controls FNH3 and TCl - The ratio is 1.08-1.12, that is, FNH3 is 99-102tt, TCl - 89~94tt; Again, the obtained sodium bicarbonate is input into the filtering unit, and the filtering equipment adopts a rotary drum vacuum filter or a centrifuge to remove the mother liquor remaining between the heavy alkali crystals, so that the salt content of the soda ash is less than 0.3%, and the rotary drum vacuum filter and the centrifuge are preferably used in combination; Finally, the filtered sodium bicarbonate is input into the calcining unit, and the main equipment is a calcining furnace. The calcining temperature is preferably controlled at 160~190℃, and the present embodiment is controlled at 175℃, the calcining time is 25min, and the furnace gas contains CO2>90%, which is compressed and reused in the carbonation reaction tower;
[0047] The reaction formula of the ammonia-soda method is as follows:
[0048] 2NH3+CO2=NH2COO - +NH4 +
[0049] NH2COO - +H2O=HCO3 - +NH3
[0050] HCO3 - +Na + =NaHCO3
[0051] NaCl+NH3+CO2+H2O→NaHCO3↓+NH4Cl;
[0052] 2NaHCO3→Na2CO3+CO2↑+H2O↑
[0053] S3) preparing gypsum, using a seed crystal method to prepare gypsum from the calcium sulfate precipitate obtained in step S1), which can also be called a calcium sulfate precipitation suspension, and controlling the process elements of the preparation to obtain gypsum, wherein the aforementioned process elements of controlling the preparation are: firstly, the calcium sulfate precipitate obtained in step S1) (i.e., the calcium sulfate precipitation suspension) is introduced into a crystallization tank and the pH value of the calcium sulfate precipitation suspension is controlled to be 10-11, and then gypsum seeds are added to the crystallization tank to crystallize calcium and sulfate ions in the calcium sulfate precipitate (i.e., the calcium sulfate precipitation suspension) for reaction, and the reaction time is preferably 25-35 minutes, preferably 30 minutes (30 minutes is selected in this embodiment), and the crystallization precipitation and the crystallization precipitation time are preferably 110-130 minutes, preferably 120 minutes (120 minutes is selected in this embodiment), and then the gypsum is separated by filtration using a plate and frame filter device (also called "plate and frame filter press filtration"), and finally drying, and the drying temperature and time are controlled. Preferably, the drying temperature and drying time are 200-300°C and 30-60min, respectively, preferably 250°C and 45min, respectively (the drying temperature and drying time are selected as 250°C and 45min, respectively in this embodiment), to obtain byproduct gypsum, the dry basis mass ratio of the seed crystal added in this step to the calcium sulfate precipitation suspension is preferably 1:20-50, preferably 1:30-40, preferably 1:35 (the embodiment selects 1:35), the reaction in the aforementioned crystallization pool is at room temperature and under stirring, the time is preferably 25-35min, preferably 30min (the embodiment is 30min), the aforementioned stirring speed is preferably 40-80rpm, preferably 60rpm (the embodiment selects 60rpm), the aforementioned crystal precipitation time is preferably 110-130min, preferably 120min (the embodiment selects 120min), the aforementioned drying adopts a rotary kiln drying equipment, and the moisture content of the gypsum product obtained in this step is less than 5%;
[0054] S4) preparing ammonia evaporation waste liquid (also referred to as generating ammonia evaporation waste liquid), subjecting the sodium bicarbonate mother liquor obtained in step S2) to ammonia evaporation reaction with lime milk, recovering carbon dioxide and ammonia and recycling them to step S2), and obtaining ammonia evaporation waste liquid at the same time, the main equipment used for the ammonia evaporation reaction in this step is an ammonia evaporation tower, the lime milk concentration is preferably 160-200tt, preferably 170tt (170tt is selected in this embodiment), ammonia in the mother liquor after carbonation and filtration of heavy alkali and ammonia in the dilute liquid can be recovered by ammonia evaporation, the tower bottom temperature is controlled at 110-120°C, preferably 115°C (115°C is selected in this embodiment), the tower top temperature is preferably 80-85°C, preferably 82°C (82°C is selected in this embodiment), ammonia and CO2 are recovered by ammonia evaporation and recycled to prepare sodium bicarbonate in step S2), and ammonia evaporation waste liquid is obtained; the reaction formula is as follows: 2NH4Cl+Ca(OH)2→CaCl2+NH3↑+2H2O↑;
[0055] S5) Resource utilization of ammonia evaporation waste liquid, the ammonia evaporation waste liquid obtained in step S4) is subjected to solid-liquid separation, and the supernatant obtained after solid-liquid separation is divided into two streams, one of which is used for the impurity removal treatment (for removing sulfate) in step S1), and the other is used for preparing calcium chloride after evaporation and concentration, and the sodium chloride therein is recovered and reused in step S1), that is, used in the refining link of step S1). For more details, see Figure 4, the resource utilization of the above-mentioned ammonia evaporation waste liquid includes the following steps: solid-liquid separation, concentration, and calcium chloride preparation. The mass percentage of calcium chloride (CaCl2) in the ammonia evaporation waste liquid is 12-13%, and the mass percentage of sodium chloride (NaCl) is 4-5%. First, the solid-liquid separation uses a cyclone separator to remove coarse components, including large particles of solids brought in by lime milk, and a small amount of impurities such as calcium carbonate (CaCO3) and calcium oxide (CaO), so that the solid content is less than 0.5%. Then, after coagulation and precipitation, the solid content of the supernatant is less than 10 mg / L. The obtained supernatant is divided into two streams, and an equivalent amount of one supernatant is returned to the desulfurization in step S1); secondly, the concentration unit receives the other supernatant, and uses an evaporation pond or evaporator. After the supernatant is concentrated 3-4 times, the sodium chloride (NaCl) therein is close to saturation, and the NaCL (NaCl) obtained by thickening and centrifugation is obtained. The crystal slurry) resources are reused in the brine refining link of step S1), and the centrifugal mother liquor is returned to the feeding receiving pool of the concentration unit; the calcium chloride solution obtained after separating the sodium chloride continues to be concentrated to a calcium chloride (CaCl2) content of 50-60%, and the concentration is preferably combined with an evaporation pond and an evaporator; finally, a saturated solution with a calcium chloride mass percentage of 60% is input into the evaporator for reconcentration, and the saturated vapor pressure of the evaporation system is preferably input>1.5MPa, and the temperature is preferably controlled at 180-220°C, preferably controlled at 200°C (200°C is selected in this embodiment), and the calcium chloride (CaCl2) saturated solution is concentrated to a supersaturated state with a calcium chloride content of>70%, and the temperature is controlled at above 110°C, and then input into the finished product preparation link, and after rotary drum slicing and drying, it is made into a calcium chloride byproduct. As can be seen from the above: an equivalent amount of supernatant described in this step (the ammonia waste liquid is clarified in a clarification tank and divided into a supernatant and a bottom mud) reacts with sodium sulfate in chemical high-salt wastewater to generate precipitated calcium sulfate.
[0056] The above is only a preferred embodiment of the present invention. It should be pointed out that, for ordinary technicians in this field, several improvements in form but not in substance can be made without departing from the spirit of the present invention, but these improvements should be regarded as within the scope of the technical connotation disclosed by the present invention.
[0057] In summary, the technical solution provided by the present invention makes up for the shortcomings of the existing technology, successfully completes the invention task, and faithfully realizes the technical effects stated by the applicant in the technical effect column above.
Claims
1. A method for preparing soda ash as a by-product of gypsum and calcium chloride from chemical high-salt wastewater, characterized in that: The following steps are involved: S1) preparing a saturated sodium chloride solution, first removing impurities from chemical high-salt wastewater, then deeply removing hardness and evaporating and concentrating to obtain a saturated sodium chloride solution and a calcium sulfate precipitate; S2) preparing sodium carbonate, using an ammonia-soda process to react the saturated sodium chloride solution obtained in step S1 with ammonia and carbon dioxide to obtain sodium bicarbonate and a sodium bicarbonate mother liquor, and calcining the sodium bicarbonate to obtain sodium carbonate; S3) preparing gypsum by using a seed crystal method to prepare gypsum from the calcium sulfate precipitate obtained in step S1), and controlling the process elements of the preparation to obtain gypsum; S4) preparing ammonia evaporation waste liquid, subjecting the sodium bicarbonate mother liquor obtained in step S2) to an ammonia evaporation reaction with lime milk, recovering carbon dioxide and ammonia and recycling them to step S2), and obtaining ammonia evaporation waste liquid; S5) Resource utilization of ammonia evaporation waste liquid, the ammonia evaporation waste liquid obtained in step S4) is subjected to solid-liquid separation, and the supernatant obtained after solid-liquid separation is divided into two streams, one of equal amount is used for the impurity removal treatment in step S1), and the other is used for preparing calcium chloride after evaporation and concentration, and sodium chloride therein is recovered and reused in step S1).
2. The method for preparing soda ash by-product gypsum and calcium chloride from chemical high-salt wastewater according to claim 1, characterized in that: The impurity removal treatment of the chemical high-salt wastewater in step S1) includes the following steps in order: removal of inorganic impurities, removal of inert organic matter, removal of heavy metals, removal of potassium ions, removal of nitrates and removal of sulfates; the mass percentage of sodium chloride in the saturated sodium chloride solution is 23-26%; the calcium sulfate precipitate is precipitated calcium sulfate generated by reacting an equivalent amount of the supernatant in step S5) with sodium sulfate in the chemical high-salt wastewater.
3. The method for preparing soda ash by-product gypsum and calcium chloride from chemical high-salt wastewater according to claim 2, characterized in that: The inorganic impurities are removed by using a high-density tank system to remove silicon, fluorine and phosphate in chemical high-salt wastewater, so that the silicon content is ≤5mg / L, the fluorine content is ≤1mg / L and the phosphate in terms of phosphorus is ≤1mg / L. The high-density tank system includes a coagulation tank, a reagent addition tank, a reaction tank, a flocculation tank and an inclined tube sedimentation tank; the inert organic matter is removed by using a functional nano-adsorption material to absorb and separate the inert COD in the chemical high-salt wastewater and make the removal rate reach more than 90%. The functional nano-adsorption material has a pore size of 0.1-5nm and a density of 1.3g / cm 3 , porosity is 75-80%, specific surface area is 1000-1500m 2 / g of mesoporous carbon composites and microporous carbon composites; The removal of heavy metals is to use a polymer chelating agent to adsorb and separate lead, arsenic, mercury and chromium in chemical high-salt wastewater; the removal of potassium ions is to use modified clinoptilolite to adsorb and separate potassium ions; the removal of nitrates is to use a micro-electric field reduction method to make the nitrates in the chemical high-salt wastewater ≤20mg / L; the removal of sulfates is to use calcium chloride in ammonia waste liquid to react with sodium sulfate in the high-salt wastewater to make the sodium sulfate in the chemical high-salt wastewater ≤1000mg / L.
4. The method for preparing soda ash by-product gypsum and calcium chloride from chemical high-salt wastewater according to claim 1, characterized in that: The deep de-hardening treatment described in step S1) is to remove the residual Mg in the solution by using the two-alkali method. 2+ and Ca 2+ , and by OH - The residual Mg in the solution 2+ Reaction to form magnesium hydroxide precipitate, making the Mg in the brine 2+ <20mg / L,CO3 2- It reacts with the residual calcium ions in the solution to form calcium carbonate precipitates, reducing the Ca in the brine. 2+ <30mg / L, the device used for evaporation and concentration is an MVR evaporator or a multiple-effect evaporator, the inlet temperature is 100°C, the saturation temperature rise is 16°C, the shell side material is 316L, and the tube side and impeller are made of titanium.
5. The method for preparing soda ash as a by-product of gypsum and calcium chloride from chemical high-salt wastewater according to claim 1, characterized in that: The ammonia-soda method described in step S2) includes the following steps: ammoniation, carbonation, filtration and calcination, and uses carbon dioxide discharged in chemical production as a raw material, and the purity of the obtained sodium carbonate is 99%; the calcination temperature is 160-190° C., and the calcination time is 20-30 minutes.
6. The method for preparing soda ash as a by-product of gypsum and calcium chloride from chemical high-salt wastewater according to claim 1, characterized in that: The process elements for controlling the preparation described in step S3) are: first, the calcium sulfate precipitate obtained in step S1) is introduced into the crystallization pool and the pH value of the feed solution is controlled to 10-11, and then gypsum seeds are added to the crystallization pool to react with calcium and sulfate ions in the calcium sulfate precipitate and the reaction time is controlled, and then crystallization precipitation is carried out and the crystallization precipitation time is controlled, and then the gypsum is separated by filter pressing with a plate and frame filter device, and finally dried to obtain the by-product gypsum.
7. The method for preparing soda ash as a by-product of gypsum and calcium chloride from chemical high-salt wastewater according to claim 6, characterized in that: The controlling reaction time is to control the reaction time to 25-35 minutes; the controlling crystal precipitation time is to control the time to 110-130 minutes; the drying is carried out by rotary kiln drying equipment, the drying temperature and the drying time are 200-300°C and 30-60 minutes respectively, and the moisture content of the gypsum is <5%.
8. The method for preparing soda ash as a by-product of gypsum and calcium chloride from chemical high-salt wastewater according to claim 1, characterized in that: The equipment used for the ammonia evaporation reaction in step S4) is an ammonia evaporation tower, the concentration of the lime milk is 160-200tt, the bottom temperature of the ammonia evaporation tower is 110-120°C, and the top temperature is 80-85°C.
9. The method for preparing soda ash as a by-product of gypsum and calcium chloride from chemical high-salt wastewater according to claim 1, characterized in that: The ammonia evaporation waste liquid in step S5) contains 12-13% by mass of calcium chloride and 4-5% by mass of sodium chloride. The solid-liquid separation is to remove the coarse components by a cyclone separator, and then to obtain the supernatant by coagulation and precipitation, which is divided into two streams; the removal of the coarse components is to remove large solid particles of calcium carbonate and calcium oxide brought in by the lime milk, so that the solid content is less than 0.5%, and the solid content of the supernatant is 10 mg / L.
10. The method for preparing soda ash as by-product gypsum and calcium chloride from chemical high-salt wastewater according to claim 1, characterized in that: The evaporation device used for the evaporation concentration in step S5) is an evaporation pond or an evaporator. The concentration is to concentrate the supernatant to 3-4 times so that the NaCl therein tends to be saturated, and the sodium chloride slurry is obtained after centrifugal separation and is reused in step S1); the steam pressure used in the evaporation pond or evaporator is saturated steam with a temperature of 180-220° C. and the mass percentage of the calcium chloride is greater than 70% for cost preparation.
Citation Information
Cited By
High-salinity wastewater treatment system and method for producing alkali by adopting integrated carbon capture