Purification solvent recovery method and system for preparing acetylene from natural gas

Through the full-phase evaporator heating and stirring technology, the problems of low recovery efficiency of purification solvents and polymer accumulation in the natural gas acetylene process are solved, and efficient recycling and environmental protection are achieved.

CN118993972APending Publication Date: 2024-11-22WANHUA CHEM (SICHUAN) CO LTD +1

Patent Information

Application Number
CN202411081972.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-08
Publication Date
2024-11-22

AI Technical Summary

Technical Problem

The purification solvent recovery efficiency in the existing natural gas acetylene process is low, and polymer accumulation leads to pipeline blockage and environmental pollution, and manual cleaning is dangerous.

Method used

The full-phase evaporator is used for heating and stirring, and the solvent is contacted with the solvent to be recovered by contacting the solvent. The polymer is adsorbed and dispersed by solid particles to achieve gas-liquid solid three-phase contact, and the solvent is collected and condensed to recover.

Benefits of technology

It improves the recycling efficiency of purified solvents, reduces manual cleaning, reduces environmental pollution and harmful gas emissions, and avoids polymer shaping.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118993972A_ABST
    Figure CN118993972A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of preparation of acetylene from natural gas, in particular to a purification solvent recovery method and system for preparation of acetylene from natural gas, and aims to solve the problems that in related technologies, the recovery efficiency of a to-be-recovered solvent in a purification solvent is low, effective deslagging cannot be realized due to polymer accumulation, and the recovery cost is low. And great harm is easily caused to the environment and the human body through manual deslagging. The invention relates to a method for recovering a purification solvent for preparing acetylene from natural gas. The recovery method comprises the following steps: heating and stirring a purification solvent by using a full-phase evaporator, so that a to-be-recovered solvent in the purification solvent is evaporated, and a polymer in the purification solvent is dispersed under stirring; and collecting and condensing the evaporated to-be-recovered solvent so as to recover the to-be-recovered solvent.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the technical field of producing acetylene from natural gas, and in particular to a method and system for recovering a purification solvent for producing acetylene from natural gas. Background Art

[0002] Acetylene is widely used in metal processing fields such as cutting and welding, as well as the synthesis of chemical products such as ethylene, vinyl chloride, vinyl acetate, acrylonitrile, polyacrylonitrile, 1,4-butanediol, etc. It is an important chemical raw material. There are many methods for producing acetylene, mainly including calcium carbide acetylene method, hydrocarbon cracking method, and direct production of acetylene from coal. Among them, calcium carbide acetylene is more polluting, and coal-to-acetylene represented by plasma cracking method is not yet mature. Non-catalytic partial oxidation cracking method in hydrocarbon cracking method is the main method for acetylene production.

[0003] The main equipment and process of the natural gas partial oxidation process for preparing acetylene currently used in industrial production equipment are as follows: natural gas and oxygen are preheated to 580℃~650℃ respectively in a preheating furnace, mixed in an acetylene cracking furnace and then burned in a reaction chamber. After a few milliseconds of reaction, spray water is used to cool down and end the reaction. The cracking gas products of the natural gas partial oxidation reaction mainly include acetylene, hydrogen, carbon monoxide, carbon dioxide, carbon black and high-grade acetylene gases such as diacetylene; after leaving the cracking furnace, the cracking gas enters the lower section of the water washing cooling tower, the electrostatic precipitator and the upper section of the cooling tower in sequence. This series of steps further cools the cracking gas and removes most of the carbon black; finally, the cracking gas is compressed and pressurized before entering the concentration and purification process, and the acetylene product gas is obtained after purification.

[0004] In the above-mentioned concentration and purification process, N-methylpyrrolidone (NMP for short) is generally used as a solvent. Acetylene and higher alkynes in the cracking gas are absorbed and analyzed by NMP solvent, acetylene gas is purified, and higher alkynes are separated. However, during the absorption and analysis process, some benzene, naphthalene and higher alkynes gather in the NMP solvent, which not only affects the absorption capacity of the solvent, but also these easily crystallized and easily polymerized substances will cause the absorption and analysis pipelines and fillers to be blocked. In view of the problem of polymer accumulation in the solvent, the efficiency of recovering the solvent to be recovered (such as NMP) in the purification solvent in the related technology is low, and the polymer is prone to accumulation and cannot be effectively discharged. For example, when the related technology recovers the solvent to be recovered by dry distillation of the contaminated solvent (i.e., the purification solvent), the polymer after dry distillation is in the form of a cake. If it is not handled in time, it is easy to cause problems such as polymer spontaneous combustion or smoldering. When cleaning manually, the manual operation volume is large, and a large amount of VOCs odorous gas will be discharged on site, causing harm to the environment and human body. Summary of the invention

[0005] Based on this, the present application provides a method and system for recovering a purified solvent for producing acetylene from natural gas, in order to solve the problems in the related art of low efficiency in recovering the solvent to be recovered in the purified solvent, and the inability to effectively discharge slag due to polymer accumulation, which easily causes great harm to the environment and human body through manual slag discharge.

[0006] In a first aspect, a method for recovering a purification solvent for producing acetylene from natural gas is provided, wherein the purification solvent comprises a polymer; and the recovery method comprises:

[0007] The purification solvent is heated and stirred by using a full-phase evaporator. The gas, liquid and solid three phases in the full-phase evaporator are in uniform contact for heat transfer, so that the solvent to be recovered in the purification solvent evaporates and the polymer in the purification solvent is dispersed under stirring;

[0008] The evaporated solvent to be recovered is collected and condensed to recover the solvent to be recovered.

[0009] Among them, the full-phase evaporator can be selected as a rake dryer or a paddle dryer.

[0010] Optionally, the purification solvent is heated and stirred by a full-phase evaporator to evaporate the solvent to be recovered in the purification solvent and to disperse the polymer in the purification solvent under stirring, comprising:

[0011] The purification solvent is sprayed into the full-phase evaporator under heating and stirring, and the purification solvent is contacted with the wall of the full-phase evaporator, thereby realizing gas-solid-liquid three-phase contact and heating the purification solvent.

[0012] Optionally, spraying the purification solvent into a full-phase evaporator under heating and stirring comprises:

[0013] Negative pressure is applied to the full-phase evaporator according to the heating temperature, and the purification solvent is sprayed into the full-phase evaporator by means of negative pressure suction, so as to adjust the spray amount of the purification solvent sprayed into the full-phase evaporator.

[0014] Optionally, the heating temperature and the absolute value of the negative pressure satisfy: T=106*P^(0.172), wherein T represents the heating temperature and P represents the absolute value of the negative pressure.

[0015] Optionally, the heating temperature T is 150° C. to 200° C., and the absolute value of the negative pressure P is 1 kPaA to 20 kPaA.

[0016] Optionally, the purification solvent is sprayed into a full-phase evaporator under heating and stirring, and the purification solvent is contacted with the wall of the full-phase evaporator. Before the purification solvent is heated, the recovery method further comprises:

[0017] Solid particles are loaded into the full-phase evaporator, and the solid particles are heated and stirred so as to utilize the solid particles to adsorb and conduct heat to the purified solvent sprayed into the full-phase evaporator.

[0018] Optionally, the solid particles satisfy at least one of the following conditions:

[0019] (1) The particle size of solid particles is 5mm~50mm;

[0020] (2) The filling volume of solid particles accounts for 10%~30% of the total volume of the full-phase evaporator;

[0021] (3) The solid particles include at least one of condensed aromatic hydrocarbon polymer particles and silicate particles.

[0022] Optionally, before the purification solvent is heated and stirred by a full-phase evaporator to evaporate the solvent to be recovered in the purification solvent and to disperse the polymer in the purification solvent under stirring, the recovery method further comprises:

[0023] The purification solvent is pretreated to control the polymer content to 2% to 20%; optionally, the pretreatment includes flash evaporation and / or centrifugal separation.

[0024] Optionally, a first slag discharge port is provided at the bottom of the full-phase evaporator; the step of collecting and condensing the evaporated solvent to be recovered to recover the solvent to be recovered comprises:

[0025] The gaseous product generated in the full-phase evaporator is captured, and the solid impurities entrained in the captured gaseous product are filtered out, and the gaseous product with the solid impurities filtered out is condensed to recover the solvent to be recovered; wherein the solid impurities can be polymer residues, such as polycyclic aromatic hydrocarbon polymers, or can be the above-mentioned added solid particles, such as polycyclic aromatic hydrocarbon polymer particles and / or silicate particles.

[0026] and / or,

[0027] The recovery method also includes: discharging the solid product produced in the full-phase evaporator through the first slag discharge port of the full-phase evaporator.

[0028] Optionally, an overflow weir is arranged above the first slag discharge port of the full-phase evaporator, and the upper end of the overflow weir is 0.01R~0.2R higher than the bottom surface of the full-phase evaporator, where R represents the inner diameter of the full-phase evaporator; discharging the solid product generated by the full-phase evaporator through the first slag discharge port of the full-phase evaporator, comprising:

[0029] When the material level of the solid product produced by the full-phase evaporator is higher than the upper end of the overflow weir, the solid product is discharged through the overflow through the first slag discharge port to the solid buffer tank for buffering.

[0030] Optionally, the recycling method further comprises:

[0031] At preset time intervals, the solid product in the solid buffer tank is discharged;

[0032] and / or,

[0033] When the material level of the solid product in the solid buffer tank reaches a preset height, the solid product in the solid buffer tank is discharged.

[0034] In a second aspect, a purification solvent recovery system for producing acetylene from natural gas is provided, comprising: a full-phase evaporator and a collection and condensation device for the solvent to be recovered;

[0035] Among them, a gas outlet is provided on the full-phase evaporator, and the full-phase evaporator is used to heat and stir the purification solvent, so that the solvent to be recovered in the purification solvent evaporates, and the polymer in the purification solvent is dispersed under stirring; the collection and condensation device of the solvent to be recovered is used to collect and condense the evaporated solvent to be recovered so as to recover the solvent to be recovered.

[0036] Optionally, the collection and condensation device for the solvent to be recovered includes: a cyclone separator and a gas condensation device;

[0037] The cyclone separator is used to capture the gaseous products generated in the full-phase evaporator and filter out the solid impurities entrained in the captured gaseous products;

[0038] The gas condensing device is used to condense the gas product from which solid impurities have been filtered out.

[0039] Optionally, the cyclone separator is an inverted cone structure, comprising an air inlet, an air outlet and a solid outlet;

[0040] The air inlet of the cyclone separator is arranged on the side wall of the inverted cone structure and is connected to the gas outlet of the full-phase evaporator. The air outlet of the cyclone separator is arranged on the top of the inverted cone structure and is connected to the gas condensing device. The solid outlet of the cyclone separator is arranged at the bottom of the inverted cone structure.

[0041] The recovery system also includes: a solid reflux pipe, a first end of which is communicated with the solid outlet of the cyclone separator, and a second end of which vertically extends into the full-phase evaporator.

[0042] Optionally, the distance between the second end of the solid reflux pipe and the bottom surface of the full-phase evaporator is 0.01R-0.2R, wherein R represents the inner diameter of the full-phase evaporator.

[0043] Optionally, the full-phase evaporator is further provided with a spraying device, which is used to spray the purification solvent into the full-phase evaporator.

[0044] Optionally, the full-phase evaporator is also provided with a feed port, which is used to load solid particles into the full-phase evaporator.

[0045] Optionally, the full-phase evaporator is a horizontal reactor, and a stirring device is also provided in the full-phase evaporator, the stirring device includes a stirring shaft and a plurality of stirring blades arranged on the stirring shaft, the stirring shaft extends along the axial direction of the horizontal reactor, each stirring blade is coplanar with the stirring shaft, and each stirring blade is further provided with side scrapers on opposite sides along the thickness direction and at one end away from the stirring shaft, and the angle α between the plane where each side scraper is located and the stirring shaft is greater than 0° and less than or equal to 36°.

[0046] Optionally, a first slag discharge port is provided at the bottom of the full-phase evaporator, an overflow weir is provided above the first slag discharge port of the full-phase evaporator, and an upper end surface of the overflow weir is 0.01R to 0.2R higher than the bottom surface of the full-phase evaporator, where R represents the inner diameter of the full-phase evaporator;

[0047] The recovery system also includes: a solid buffer tank connected below the first slag discharge port of the full-phase evaporator.

[0048] Optionally, the recovery system further comprises: a controller and a solid storage tank;

[0049] The solid storage tank is connected below the solid buffer tank. A second slag discharge port connected to the solid storage tank is provided at the bottom of the solid buffer tank. A solenoid valve is provided at the second slag discharge port of the solid buffer tank, and a controller is electrically connected to the solenoid valve. The controller is used to control the solenoid valve to open at preset time intervals to discharge the solid product in the solid buffer tank into the solid storage tank, and / or a material level detector is also provided in the solid buffer tank. The controller is used to control the solenoid valve to open when the material level detector detects that the material level in the solid buffer tank reaches a preset height, so as to discharge the solid product in the solid buffer tank into the solid storage tank.

[0050] Compared with the related art, this application has at least the following beneficial technical effects:

[0051] The purification solvent is heated and stirred by a full-phase evaporator, and the purification solvent is heated by contacting the wall of the full-phase evaporator at high temperature, so that the solvent to be recovered in the purification solvent evaporates. The evaporated solvent to be recovered can be condensed into a liquid for recovery by collecting and condensing the evaporated solvent to be recovered, and the polymer in the purification solvent is dispersed under stirring to obtain a granular slag material, which can avoid the slag material from being compacted. On the one hand, it can promote the separation of the polymer and the solvent to be recovered and improve the recovery efficiency of the solvent to be recovered. On the other hand, it can achieve effective slag discharge while reducing manual slag raking, and can reduce the emission of harmful gases during on-site manual slag discharge, thereby reducing environmental pollution and harm to the human body.

[0052] In summary, the present application solves the problems in the related art of low efficiency in recovering the solvent to be recovered in the purified solvent, inability to effectively discharge slag due to polymer accumulation, and the possibility of causing great harm to the environment and human body through artificial slag discharge. BRIEF DESCRIPTION OF THE DRAWINGS

[0053] FIG1 is a schematic structural diagram of a purification solvent recovery system for producing acetylene from natural gas provided in an embodiment of the present application;

[0054] FIG2 is a schematic diagram of a structure in which a lateral scraper is provided on a stirring blade according to an embodiment of the present application;

[0055] Figure 3 A schematic diagram of a structure in which an overflow weir is arranged above a slag discharge port of a full-phase evaporator provided in an embodiment of the present application;

[0056] Figure 4 This is a schematic diagram of the structure of the dry distillation recovery and purification solvent of Comparative Example 1 provided in the present application.

[0057] Reference numerals:

[0058] 1. Full-phase evaporator; 11. First slag discharge port; 12. Overflow weir; 2. Solid buffer tank; 10. Collection and condensation device for the solvent to be recovered; 13. Gas outlet; 14. Spraying device; 100. Vacuum system; 15. Feed port; 3. Cyclone separator; 4. Gas condensation device; 31. Air inlet; 32. Air outlet; 33. Solid outlet; 20. Solid reflux pipe; 16. Stirring device; 161. Stirring shaft; 162. Stirring blade; 163. Side scraper; 5. Controller; 6. Solid storage tank; 21. Second slag discharge port; a. Solenoid valve; 41. Condensation chamber; 42. Condensate spraying device; 43. Gas inlet; 44. Waste gas outlet; 421. Condensate sprayer; 101. Retort; 102. First condenser; 103. Vacuum pump; 104. Second condenser; 105. Solvent collection tank; 106. Slag discharge hole. DETAILED DESCRIPTION

[0059] In order to facilitate the understanding of the present application, the present application will be described more fully below with reference to the relevant drawings. The preferred embodiments of the present application are given in the drawings. However, the present application can be implemented in many different forms and is not limited to the embodiments described herein. On the contrary, the purpose of providing these embodiments is to make the understanding of the disclosure of the present application more thorough and comprehensive.

[0060] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as those commonly understood by those skilled in the art to which this application belongs. The terms used herein in the specification of this application are only for the purpose of describing specific embodiments and are not intended to limit this application. The term "and / or" used herein includes any and all combinations of one or more of the related listed items.

[0061] The present application will be further described in detail below in conjunction with specific embodiments. The present application can be implemented in many different forms and is not limited to the embodiments described herein. On the contrary, the purpose of providing these embodiments is to make the disclosure of the present application more thoroughly understood.

[0062] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as those commonly understood by those skilled in the art to which this application belongs. The terms used herein in the specification of this application are only for the purpose of describing specific embodiments and are not intended to limit this application.

[0063] In this application, "one or several" refers to any one, any two or more of the listed items. Among them, "several" refers to any two or more of the listed items.

[0064] In the present application, the terms "combination thereof", "any combination thereof", "any combination thereof" and the like include all suitable combinations of any two or more of the listed items.

[0065] In the present application, the technical features described in an open manner include closed technical solutions composed of the listed features, and also include open technical solutions containing the listed features.

[0066] In the present application, reference to a numerical range includes both endpoints of the numerical range unless otherwise specified.

[0067] In the present application, the percentage content, unless otherwise specified, refers to mass percentage for solid-liquid mixing and solid-solid mixing, and volume percentage for liquid-liquid mixing.

[0068] In this application, when it comes to percentage concentration, unless otherwise specified, it refers to the final concentration. The final concentration refers to the proportion of the added component in the system after the addition of the component.

[0069] In this application, when it comes to temperature parameters, unless otherwise specified, both constant temperature treatment and treatment within a certain temperature range are permitted. The constant temperature treatment allows the temperature to fluctuate within the precision range controlled by the instrument.

[0070] In view of the problem of polymer accumulation in the above-mentioned solvent, the related technology passes a part of the contaminated solvent (that is, the purification solvent in this application) through continuous flash evaporation to be initially concentrated, and the initially concentrated NMP solvent enters each retort for intermittent retort, and the retorted solvent is cooled and returned to the concentration and purification process, and the polymer is precipitated as retort slag. The retort operation is to pass the NMP solvent containing the polymer into the retort, and heat the polymer into a solid state by steam heating in the jacket. This step is an intermittent operation, the distillation time is long, the thermal efficiency is low, the retort slag is compacted in the shape of a cake, and manual raking of the slag is required, the manual operation amount is large, and a large amount of VOCs odorous gas will be discharged on site, causing harm to the environment and the human body. At the same time, since the retort slag is prone to spontaneous combustion, accidents of spontaneous combustion or smoldering of the retort slag are prone to occur, which is not conducive to the realization of safe production.

[0071] Based on the above, in a first aspect, some embodiments of the present application provide a method for recovering a purification solvent for producing acetylene from natural gas, wherein the purification solvent comprises a polymer; as shown in FIG1 , the recovery method comprises:

[0072] The purification solvent is heated and stirred by using a full-phase evaporator 1, so that the solvent to be recovered in the purification solvent evaporates and the polymer in the purification solvent is dispersed under stirring;

[0073] The evaporated solvent to be recovered is collected and condensed to recover the solvent to be recovered.

[0074] Among them, the full-phase evaporator 1 is a horizontal reactor, the stirring shaft is arranged along the axial direction of the reactor, and the stirring blades are arranged in sequence along the extension direction of the stirring shaft. By rotating the stirring blades in both directions, the material entering the full-phase evaporator 1 can be stirred. By setting a jacket shell, by passing steam or heat transfer oil into the jacket shell, the material entering therein can be heated. In addition, the stirring shaft and the stirring blades can also be provided with a heating medium flow channel, and by passing steam or heat transfer oil into the heating medium flow channel, the material entering the full-phase evaporator 1 can also be heated.

[0075] In the purification solvent recovery method for producing acetylene from natural gas provided in the embodiment of the present application, the purification solvent is heated and stirred by a full-phase evaporator 1, and the purification solvent is heated by contacting the purification solvent with the wall of the full-phase evaporator 1 at high temperature, so that the solvent to be recovered in the purification solvent evaporates, and the evaporated solvent to be recovered is collected and condensed, so that the solvent to be recovered can be condensed into a liquid for recovery, and the polymer in the purification solvent is dispersed under stirring to obtain a granular slag material, which can avoid the slag material from being compacted. On the one hand, it can promote the separation of the polymer and the solvent to be recovered, and improve the recovery efficiency of the solvent to be recovered. On the other hand, it can achieve effective slag discharge while reducing manual slag raking, and can reduce the emission of harmful gases during on-site manual slag discharge, thereby reducing environmental pollution and harm to the human body.

[0076] In summary, the present application solves the problems in the related art of low efficiency in recovering the solvent to be recovered in the purified solvent, inability to effectively discharge slag due to polymer accumulation, and the possibility of causing great harm to the environment and human body through artificial slag discharge.

[0077] In some embodiments, the purification solvent is heated and stirred by using the full-phase evaporator 1 to evaporate the solvent to be recovered in the purification solvent and disperse the polymer in the purification solvent under stirring, including:

[0078] The purification solvent is sprayed into the full-phase evaporator 1 under heating and stirring, and the purification solvent is heated by contacting the wall of the full-phase evaporator 1 with the purification solvent.

[0079] In these embodiments, by spraying the purification solvent into the full-phase evaporator 1, the purification solvent is dispersed in the full-phase evaporator 1, and the purification solvent sprayed into different positions is quickly heated by the wall of the full-phase evaporator 1, which can improve the heating uniformity of the purification solvent, facilitate the rapid evaporation of the solvent to be recovered and overflow from the polymer, and prevent the solvent to be recovered from being wrapped by the polymer and unable to be recovered, thereby improving the recovery efficiency of the solvent to be recovered. At the same time, by spraying the purification solvent into the full-phase evaporator 1, the polymer in the purification solvent is dispersed in different positions of the full-phase evaporator 1 for drying, which is more conducive to the dispersion of the polymer, can reduce polymer aggregation, thereby making it easier to disperse the polymer, reduce the particle size of the slag, and further improve the slag removal effect.

[0080] In some embodiments, the purification solvent is sprayed into the full-phase evaporator 1 under heating and stirring, comprising:

[0081] Negative pressure is applied to the full-phase evaporator 1 according to the heating temperature, and the purified solvent is sprayed into the full-phase evaporator 1 by means of negative pressure suction, so as to adjust the spray amount of the purified solvent sprayed into the full-phase evaporator 1.

[0082] In these embodiments, the negative pressure can be adjusted according to the heating temperature, so that the feed amount of the purification solvent can be adjusted, so as to match the feed amount and the heating temperature and improve the temperature uniformity of the evaporation recovery of the recovered solvent.

[0083] In some embodiments, the heating temperature and the absolute value of the negative pressure satisfy the relationship: T=106*P^(0.172), wherein T represents the heating temperature, and P represents the absolute value of the negative pressure.

[0084] In some embodiments, the heating temperature T is 150° C. to 200° C., and the absolute value of the negative pressure P is 1 kPaA to 20 kPaA.

[0085] In some embodiments, the purification solvent is sprayed into the full-phase evaporator 1 under heating and stirring, and the wall of the full-phase evaporator 1 is used to contact the purification solvent. Before the purification solvent is heated, the recovery method further includes:

[0086] Solid particles are loaded into the full-phase evaporator 1 , and the solid particles are heated and stirred so as to utilize the solid particles to adsorb and conduct heat to the purified solvent sprayed into the full-phase evaporator 1 .

[0087] In these embodiments, by pre-loading solid particles, heating and stirring the solid particles, when the purification solvent is sprayed into the full-phase evaporator 1, the solid particles can adsorb and conduct heat to the purification solvent, thereby heating the purification solvent. On the one hand, the solid particles can be polar molecules. The electrostatic attraction between the solid particles and the solvent to be recovered and the polymer can be used to adsorb the purification solvent, so that the solid particles are fully in contact with the solvent to be recovered and the polymer, which is convenient for the solid particles to evaporate the solvent to be recovered at high temperature and adsorb the polymer at the same time, which can effectively promote the rapid separation of the polymer and the solvent to be recovered, reduce the residual solvent to be recovered in the polymer, and thus improve the recovery efficiency of the solvent to be recovered; on the other hand, the good dispersibility of the solid particles themselves can further promote the dispersion of the polymer, reduce the accumulation and compaction of the polymer, and the stirring action of the stirring device in the full-phase evaporator 1 can further reduce the slag particle size of the polymer, thereby further improving the slag removal effect.

[0088] There is no specific limitation on the selection of the above-mentioned solid particles, and all polar solid materials with a smaller particle size and capable of stably existing in the above-mentioned process are within the protection scope of the present application.

[0089] In some embodiments, the solid particles satisfy at least one of the following conditions:

[0090] (1) The particle size of solid particles is 5mm~50mm;

[0091] (2) The filling volume of solid particles accounts for 10%~30% of the total volume of the full-phase evaporator;

[0092] (3) The solid particles include at least one of condensed aromatic hydrocarbon polymer particles and silicate particles.

[0093] In these embodiments, by controlling the particle size of the solid particles to be 5 mm to 50 mm, the adsorption and heat transfer effects can be effectively improved, thereby improving the recovery efficiency of the solvent to be recovered, and dispersing the polymer to reduce the particle size of the polymer slag, thereby achieving effective slag discharge; by controlling the filling volume of the solid particles to account for 10% to 30% of the total volume of the full-phase evaporator, the purified solvent can be effectively adsorbed and heat transferred, thereby improving the recovery efficiency of the solvent to be recovered; the use of polycyclic aromatic polymer particles and silicate particles can more effectively improve the adsorption and heat transfer effects. In addition, the polycyclic aromatic polymer can be the slag after the previous treatment, which is convenient for local material collection.

[0094] In some embodiments, the condensed aromatic polymer particles include: slag from dry distillation slag or solid slag produced in a full-phase evaporator.

[0095] In some embodiments, the silicate particles include at least one of molecular sieves, diatomaceous earth, and zeolites.

[0096] Furthermore, the condensed aromatic polymer particles can be selected from the residues of dry distillation slag, which is convenient for material collection and can realize the utilization of waste residues.

[0097] In some embodiments, before the purification solvent is heated and stirred by the full-phase evaporator 1 to evaporate the solvent to be recovered in the purification solvent and the polymer in the purification solvent is dispersed under stirring, the recovery method further comprises:

[0098] The purification solvent is pretreated to control the polymer content within 2%~20%.

[0099] In these embodiments, by controlling the polymer content to be within a range of 2% to 20%, the recovery efficiency of the solvent to be recovered can be effectively improved, and the slag removal effect can be improved.

[0100] Optionally, the pretreatment may include flash evaporation and / or centrifugation.

[0101] In some embodiments, as shown in FIG1 , a first slag discharge port 11 is provided at the bottom of the full-phase evaporator 1; the steps of collecting and condensing the evaporated solvent to be recovered to recover the solvent to be recovered include:

[0102] The gaseous product generated in the full-phase evaporator 1 is captured, and the solid impurities entrained in the captured gaseous product are filtered out, and the gaseous product from which the solid impurities are filtered out is condensed to recover the solvent to be recovered;

[0103] and / or,

[0104] The recovery method further comprises: discharging the solid product produced in the full-phase evaporator 1 through the first slag discharge port 11 of the full-phase evaporator 1 .

[0105] In these embodiments, by capturing the gaseous products generated in the full-phase evaporator 1 and filtering out the solid impurities entrained in the captured gaseous products, the gaseous products can be effectively purified and the solid impurities in the solvent after condensation can be reduced. When the solid products generated in the full-phase evaporator are discharged through the slag discharge port of the full-phase evaporator, timely slag discharge can be achieved through the full-phase evaporator.

[0106] In some embodiments, as shown in FIG1 , an overflow weir 12 is disposed above the first slag discharge port 11 of the full-phase evaporator 1, and the upper end of the overflow weir 12 is 0.01R to 0.2R higher than the bottom surface of the full-phase evaporator 1, where R represents the inner diameter of the full-phase evaporator 1; the solid product generated by the full-phase evaporator 1 is discharged through the first slag discharge port 11 of the full-phase evaporator 1, comprising:

[0107] When the material level of the solid product produced by the full-phase evaporator 1 is higher than the upper end of the overflow weir 12, the solid product is discharged through the first slag discharge port 11 to the solid buffer tank 2 for buffering.

[0108] In these embodiments, it is convenient to discharge slag in time under negative pressure, so as to realize automatic and continuous slag discharge of the system.

[0109] In some embodiments, the recycling method may further include:

[0110] At preset time intervals, the solid product in the solid buffer tank 2 is discharged;

[0111] and / or,

[0112] When the material level of the solid product in the solid buffer tank 2 reaches a preset height, the solid product in the solid buffer tank 2 is discharged.

[0113] In these embodiments, as the reaction proceeds, the solid product in the full-phase evaporator 1 increases continuously, and when the material level of the solid product is higher than the upper end of the overflow weir 12, it can be discharged through the overflow through the first slag discharge port 11 to the solid buffer tank 2 for temporary storage. By setting a preset time interval and / or a preset height in the solid buffer tank 2, the solid product in the solid buffer tank 2 is discharged at each preset time interval, and / or when the material level of the solid product in the solid buffer tank 2 reaches a preset height, the solid product in the solid buffer tank 2 is discharged, and automatic continuous operation and slag discharge can be further realized, which is convenient for automatic and continuous operation of the system.

[0114] In a second aspect, some embodiments of the present application provide a purification solvent recovery system for acetylene production from natural gas, as shown in FIG1 , the recovery system comprises: a full-phase evaporator 1 and a collection and condensation device 10 for the solvent to be recovered;

[0115] The full-phase evaporator 1 is provided with a gas outlet 13, and the full-phase evaporator 1 is used to heat and stir the purification solvent, so that the solvent to be recovered in the purification solvent evaporates, and the polymer in the purification solvent is dispersed under stirring. The collection and condensation device of the solvent to be recovered is used to collect and condense the evaporated solvent to be recovered, so as to recover the solvent to be recovered.

[0116] In the purification solvent recovery system provided in the embodiment of the present application, since the full-phase evaporator 1 is provided with a gas outlet 13, when the purification solvent is heated and stirred by the full-phase evaporator 1, the solvent to be recovered in the purification solvent can be evaporated and the polymer in the purification solvent can be dispersed under stirring. After evaporation, the solvent to be recovered can be discharged from the gas outlet 13, and the evaporated solvent to be recovered can be collected and condensed by the collection and condensation device of the solvent to be recovered, so that the solvent to be recovered can be recovered. In this process, a solid product with a smaller particle size can be obtained under the stirring of the full-phase evaporator 1, which is convenient for slag discharge and eliminates the need for manual slag raking, thereby reducing the environmental pollution and harm to the human body caused by manual slag raking in the related art; and by providing a gas outlet 13 on the full-phase evaporator 1 and connecting the gas outlet 13 with the collection and condensation device of the solvent to be recovered, the evaporated solvent to be recovered can be collected and condensed, thereby obtaining a liquid solvent, which can be directly reused.

[0117] In some embodiments, as shown in FIG. 1 , the full-phase evaporator 1 is further provided with a spray device 14 , and the spray device 14 is used to spray the purification solvent into the full-phase evaporator 1 .

[0118] In these embodiments, the spray device 14 can spray the purified solvent into the full-phase evaporator 1, which can improve the recovery efficiency of the solvent to be recovered and reduce the slag particle size of the polymer.

[0119] The spray device 14 may be any spray structure capable of spraying the purification solvent into the full-phase evaporator 1 , and is not specifically limited here.

[0120] In some embodiments, the spray device 14 is a spiral atomizing nozzle, which is a solid cone or hollow cone spray nozzle, and the angle range of the jet can be 60 to 120 degrees. The interior of the spiral atomizing nozzle has no structure and is a smooth passage. The purified solvent is sprayed in layers by impacting the layered interface of the spiral. Since the purified solvent is tangent to and collides with the continuously decreasing spiral surface, it becomes tiny liquid droplets and sprays out to form a mist. The streamlined design from the inlet to the outlet in the nozzle cavity reduces the resistance coefficient to a minimum. Therefore, the nozzle of this structure has a smooth flow channel that can minimize the blockage of the purified solvent and enable the purified solvent to reach the maximum flow rate on a pipeline of a given size.

[0121] In some embodiments, the feed amount of the spiral nozzle 14 can be controlled by controlling the pressure in the full-phase evaporator 1. Specifically, as described above, when controlling the feed amount of the purification solvent, the pressure (negative pressure) in the full-phase evaporator 1 can be controlled according to the heating temperature (such as the heating temperature T and the absolute value P of the negative pressure in the full-phase evaporator satisfy: T=106*P^(0.172)), and the suction amount of the purification solvent can be controlled by using the different negative pressures in the full-phase evaporator 1, thereby controlling the feed amount of the purification solvent, and keeping the heating temperature in the full-phase evaporator 1 stable.

[0122] The negative pressure can be obtained by applying the vacuum system 100 to the full-phase evaporator 1 .

[0123] In some embodiments, as shown in FIG. 1 , the full-phase evaporator 1 is further provided with a feed port 15 , and the feed port 15 is used to load solid particles into the full-phase evaporator 1 .

[0124] In these embodiments, a feed port 15 is provided on the full-phase evaporator 1 to facilitate loading of solid particles into the full-phase evaporator 1. The solid particles can adsorb and conduct heat to the purified solvent sprayed into the full-phase evaporator 1, so that the solid particles can be used to further improve the recovery efficiency of the solvent to be recovered and reduce the slagging particle size of the polymer. For a specific description, see the recovery method description.

[0125] In some embodiments, as shown in Figure 1, the collection and condensation device 10 for the solvent to be recovered includes: a cyclone separator 3 and a gas condensation device 4; wherein the cyclone separator 3 is used to capture the gas product generated in the full-phase evaporator 1, and filter out the solid impurities entrained in the captured gas product; the gas condensation device 4 is used to condense the gas product from which the solid impurities have been filtered out.

[0126] In these embodiments, the gaseous product generated in the full-phase evaporator 1 is captured by using a cyclone separator 3, and the solid impurities entrained in the captured gaseous product are filtered out, so that a purified gas can be obtained, and the gaseous product with the solid impurities filtered out is condensed by a gas condensation device 4, so that a liquid with less solid impurities can be obtained, thereby realizing the direct reuse of the solvent to be recovered.

[0127] In some embodiments, as shown in Figure 1, the cyclone separator 3 is an inverted conical structure, including an air inlet 31, an air outlet 32 ​​and a solid outlet 33; wherein, the air inlet 31 of the cyclone separator 3 is arranged on the side wall of the inverted conical structure, and is connected to the gas outlet 13 of the full-phase evaporator 1, the air outlet 32 ​​of the cyclone separator 3 is arranged at the top of the inverted conical structure, and is connected to the gas condensation device 4, and the solid outlet 33 of the cyclone separator 3 is arranged at the bottom of the inverted conical structure; the recovery system also includes: a solid reflux pipe 20, a first end of the solid reflux pipe 20 is connected to the solid outlet 33 of the cyclone separator 3, and a second end vertically extends into the full-phase evaporator 1.

[0128] In these embodiments, the cyclone separator can capture the gaseous products generated in the full-phase evaporator 1, and by configuring the cyclone separator into an inverted cone structure, with the solid outlet 33 disposed at the bottom of the inverted cone structure and the gas outlet 32 ​​disposed at the top of the inverted cone structure, the captured gaseous products and the solid impurities carried therewith can be separated by gravity, that is, the solid impurities can flow back into the full-phase evaporator 1 through the solid outlet 33 and the solid reflux pipe 20, and the purified gaseous products can enter the gas condensation device 4 through the gas outlet 32 ​​for further condensation and recovery, thereby reducing the solid impurity content in the recovered liquid.

[0129] In some embodiments, the distance between the second end of the solid reflux pipe 20 and the bottom surface of the full-phase evaporator 1 is 0.01R-0.2R, where R represents the inner diameter of the full-phase evaporator 1 .

[0130] In these embodiments, by inserting the second end of the solid reflux pipe 20 at a position 0.01R ~ 0.2R away from the bottom surface of the full-phase evaporator 1, the second end of the solid reflux pipe 20 can be inserted into the solid particles, which can prevent the solid particles from flowing back under negative pressure.

[0131] In some embodiments, as shown in Figures 1 and 2, the full-phase evaporator 1 is a horizontal reactor, and a stirring device 16 is also provided in the full-phase evaporator 1. The stirring device 16 includes a stirring shaft 161 and a plurality of stirring blades 162 arranged on the stirring shaft 161. The stirring shaft 161 extends along the axial direction of the horizontal reactor. Each stirring blade 162 is coplanar with the stirring shaft 161. Each stirring blade 162 is also provided with side scrapers 163 on opposite sides along the thickness direction and at one end away from the stirring shaft 161. The angle α between the plane where each side scraper 163 is located and the stirring shaft 161 is greater than 0° and less than or equal to 36°.

[0132] In these embodiments, as shown in FIG. 2 , lateral scrapers 163 are provided on both sides of each stirring blade 162 in the thickness direction and at one end away from the stirring shaft 161, and an angle α between the lateral scraper 163 and the stirring shaft 161 is set to be greater than 0° and less than or equal to 36°, which is equal to the angle of repose of the solid particles, which is beneficial to stirring the solid particles, thereby improving the mixing uniformity of the purification solvent and the solid particles.

[0133] In some embodiments, as shown in FIG. 1 and Figure 3 As shown, a first slag discharge port 11 is provided at the bottom of the full-phase evaporator 1, and an overflow weir 12 is provided above the first slag discharge port 11 of the full-phase evaporator 1. The upper end surface of the overflow weir 12 is higher than the bottom surface of the full-phase evaporator 1 by 0.01R~0.2R, where R represents the inner diameter of the full-phase evaporator 1;

[0134] The recovery system further includes: a solid buffer tank 2 connected below the first slag discharge port 11 of the full-phase evaporator 1 .

[0135] In these embodiments, by setting the overflow weir 12, the solid material in the full-phase evaporator 1 can be discharged into the solid buffer tank 2 through the first slag discharge port 11 when the height exceeds the upper end surface of the overflow weir 12, and continuous automatic slag discharge can be achieved under negative pressure.

[0136] Specifically, at the beginning of the reaction, the solid buffer tank 2 and the full-phase evaporator 1 are both in a negative pressure state. As the reaction proceeds, when the height of the solid product exceeds the upper end surface of the overflow weir 12, the solid product will be discharged into the solid buffer tank 2 through the first slag discharge port 11 through overflow.

[0137] In some embodiments, as shown in Figure 1, the recovery system may also include: a controller 5 and a solid storage tank 6, the solid storage tank 6 is connected to the bottom of the solid buffer tank 2, and the bottom of the solid buffer tank 2 is provided with a second slag discharge port 21 connected to the solid storage tank 6, and the second slag discharge port 21 of the solid buffer tank 2 is provided with an electromagnetic valve a, and the controller 5 is electrically connected to the electromagnetic valve a; the controller 5 is used to control the electromagnetic valve a to open at every preset time interval to discharge the solid product in the solid buffer tank 2 into the solid storage tank 6, and / or, a material level detector is also provided in the solid buffer tank 2, and the controller is used to control the electromagnetic valve a to open when the material level detector detects that the material level in the solid buffer tank 2 reaches a preset height, so as to discharge the solid product in the solid buffer tank 2 into the solid storage tank 6.

[0138] In these embodiments, as the reaction proceeds, when the solid product in the solid buffer tank 2 exceeds a certain amount or the operating time exceeds a certain period of time, the solid material in the solid buffer tank 2 can be discharged into the solid storage tank 6, further realizing automatic continuous operation and slag discharge of the system.

[0139] In some embodiments, the portion of the solid buffer tank 2 close to the second slag discharge port 21 is an inverted cone structure, and the cone apex angle of the inverted cone structure is 60° to 90°.

[0140] In these embodiments, it can be ensured that solid materials do not adhere to the wall during the slag discharge process, thereby improving the slag discharge effect.

[0141] In some embodiments, the specific structure of the gas condensing device 4 is not limited, as long as the gas condensing device 4 can condense the solvent to be recovered.

[0142] In some embodiments, as shown in Figure 1, the gas condensation device 4 includes a condensation chamber 41, and a condensate spraying device 42 arranged in the condensation chamber 41, a gas inlet 43 is arranged at the bottom of the condensation chamber 41, and a waste gas outlet 44 is arranged at the top of the condensation chamber 41. The condensate spraying device 42 is used to spray coolant so that the coolant contacts the gas product after gas-solid separation to condense the gas product after gas-solid separation, and the gas product that cannot be condensed can be discharged through the waste gas outlet 44.

[0143] The condensate spraying device 42 may include a multi-layer condensate sprayer 421, which may be arranged at different heights of the condensation chamber 41, and may perform multi-layer condensation on the gas product after gas-solid separation to improve the condensation effect. After the gas product that cannot be condensed is discharged through the exhaust gas outlet 44, for example, it may be transported to the incineration unit by a fan to incinerate the tail gas.

[0144] The above introduces the specific implementation methods of the present application. In order to objectively illustrate the technical effects produced by the present application, the following examples and comparative examples will be used for description.

[0145] In the following examples and comparative examples, all raw materials can be purchased in commercial form, and in order to maintain the reliability of the experiment, the raw materials used in the following examples and comparative examples have the same physical and chemical parameters or are processed in the same way.

[0146] Example 1

[0147] Example 1 provides a method for recovering a purified solvent from natural gas to acetylene, the specific steps of which are as follows:

[0148] As shown in Figures 1, 2 and Figure 3 As shown, 30% of the total volume of dry distillation slag with a particle size of 10 mm is filled in the rake dryer, and side scrapers 163 are provided on opposite sides of the stirring blade 162 along the thickness direction and at one end away from the stirring shaft 161. The angle between the plane where the side scraper 163 is located and the stirring shaft 161 is 10°. Steam is introduced into the jacket shell of the rake dryer to control the heating temperature to 150°C, and the pressure in the rake dryer is controlled to be -1 kPaA. The NMP contaminated solvent is sprayed into the rake dryer using a spiral nozzle, and the feed amount is 0.8m 3 / h, the gas product in the rake dryer is separated from the solid impurities by the cyclone separator 3 and then enters the gas condensation device 4 in the form of spraying, with a spray volume of 40m 3 / h, the temperature of the gas condensing device 4 near the exhaust gas outlet 44 is controlled to be 50°C, the exhaust gas is transported to the incineration unit through the fan, the cone vertex angle of the conical structure of the solid buffer tank 2 is 90°, and the automatic slag discharge process is performed every 60 minutes.

[0149] Example 2

[0150] The method for recovering the purification solvent from natural gas to acetylene provided in Example 2 is substantially the same as that in Example 1, except that:

[0151] The blade dryer was filled with diatomaceous earth with a particle size of 5 mm, accounting for 30% of the total volume. Side scrapers 163 were provided on opposite sides of the stirring blade 162 in the thickness direction and at one end away from the stirring shaft 161. The angle between the plane where the side scrapers 163 were located and the stirring shaft 161 was 36°. Steam was introduced into the jacket shell of the blade dryer to control the heating temperature to 200°C. The pressure in the blade dryer was controlled to be -20 kPaA. The NMP solvent was sprayed into the blade dryer using a spiral nozzle. The feed amount was 0.8 m 3 / h, the cone apex angle of the conical structure of the solid buffer tank 2 is 60°, and the automatic slag discharge process is performed every 60 minutes.

[0152] Example 3

[0153] The method for recovering the purification solvent from natural gas to acetylene provided in Example 3 is substantially the same as that in Example 1, except that:

[0154] Do not load the dry distillation slag into the rake dryer. Steam is introduced into the jacket shell of the rake dryer to control the heating temperature to 200°C. The pressure in the rake dryer is controlled to -20kPaA. The NMP solvent is sprayed into the rake dryer using a spiral nozzle. The feed amount is 0.8m 3 / h, the cone apex angle of the conical structure of the solid buffer tank 2 is 60°, and the automatic slag discharge process is performed every 60 minutes.

[0155] Example 4

[0156] The method for recovering the purification solvent for preparing acetylene from natural gas provided in Example 4 is substantially the same as that in Example 1, except that:

[0157] The rake dryer is filled with diatomaceous earth with a particle size of 5 mm, which accounts for 30% of the total volume. Side scrapers 163 are provided on opposite sides of the stirring blade along the thickness direction and at one end away from the stirring shaft 161. The angle between the plane where the side scrapers are located and the stirring shaft 161 is 5°. The cyclone separator 3 is bypassed, and the gas directly enters the condensation system without passing through the cyclone separator 3 for separation of solid impurities. The cone vertex angle of the conical structure of the solid buffer tank 2 is 60°, and an automatic slag discharge process is performed every 60 minutes.

[0158] Example 5

[0159] The method for recovering the purification solvent from natural gas to acetylene provided in Example 5 is substantially the same as that in Example 1, except that:

[0160] The rake dryer is filled with diatomaceous earth with a particle size of 5 mm, which accounts for 30% of the total volume. Side scrapers 163 are provided on opposite sides of the stirring blade 162 along the thickness direction and at one end away from the stirring shaft 161. The angle between the plane where the side scrapers 163 are located and the stirring shaft 161 is 40°.

[0161] Example 6

[0162] The method for recovering the purification solvent for preparing acetylene from natural gas provided in Example 6 is substantially the same as that in Example 1, except that:

[0163] The rake dryer was filled with diatomaceous earth with a particle size of 5 mm, accounting for 10% of the total volume. Side scrapers 163 were provided on opposite sides of the stirring blade 162 in the thickness direction and at one end away from the stirring shaft 161. The angle between the plane where the side scrapers 163 were located and the stirring shaft 161 was 36°. Steam was introduced into the jacket shell of the rake dryer to control the heating temperature to 200°C. The pressure in the rake dryer was controlled to be -20 kPaA. The NMP solvent was sprayed into the rake dryer using a spiral nozzle. The feed amount was 0.8 m 3 / h, the gas condensing device 4 is replaced by a heat exchanger for heat exchange, the temperature of the gas condensing device 4 near the exhaust gas outlet is controlled to be 60°C, the cone apex angle of the conical structure of the solid buffer tank 2 is 60°, and the automatic slag discharge process is performed every 60 minutes.

[0164] Example 7

[0165] The method for recovering the purification solvent for preparing acetylene from natural gas provided in Example 7 is substantially the same as that in Example 1, except that:

[0166] The rake dryer was filled with 20% of the total volume of dry distillation rake slag with a particle size of 10 mm. Steam was introduced into the jacket shell of the rake dryer to control the heating temperature to 200°C. The pressure in the rake dryer was controlled to -20 kPaA. The NMP solvent was sprayed into the rake dryer using a spiral nozzle. The feed amount was 0.8 m 3 / h, the cone apex angle of the conical structure of the solid buffer tank 2 is 120°, and the automatic slag discharge process is performed every 60 minutes.

[0167] Comparative Example 1

[0168] Use Figure 4 The intermittent distillation system shown in the figure processes NMP contaminated solvent (the composition is the same as that of Example 1), specifically: 5m 3 The NMP contaminated solvent is sent into the retort 101, the heating steam is turned on and the temperature is raised to 150° C. and passed into the jacket of the retort 101 to heat the NMP contaminated solvent, and the vacuum system is started. The pressure is controlled at -3 KpaA and the retort is distilled for 20 hours. During the retort, the steam is converted into cold liquid by heat exchange, and the gaseous product obtained by the retort passes through the first condenser 102, the vacuum pump 103 and the second condenser 104 in sequence, and the solvent to be recovered is condensed into the solvent collecting tank 105, and the uncondensed gaseous product is discharged as tail gas. The slag obtained by the retort is a coked block solid, and the slag is manually cleaned through the slag discharge hole 106.

[0169] Test Case

[0170] 1. The composition of the NMP contaminated solvent provided in Examples 1 to 7 and Comparative Example 1 was analyzed, and the analysis results were shown in Table 1 below:

[0171] Table 1 Analysis results of NMP contaminated solvent

[0172]

[0173] 2. The residual rate of NMP in the slag obtained by the methods provided in Examples 1 to 7 and Comparative Example 1 was detected, the NMP recovery rate and the volatile organic compound content (VOCs) were calculated, and the slag discharge was observed and counted. The specific test, calculation and statistical results are shown in Table 2 below:

[0174] Table 2 Test results

[0175]

[0176] Combining Table 1 and Table 2, it can be seen that the solvent recovery rates of Examples 1 and 2 are all above 99%, the NMP recovery liquid is clear and transparent, the fine slag particles are uniform, the D50 particle size is 1-2 mm, the slag discharge is smooth, and the gas temperature is stable, and the on-site VOCs content is less than 5 ppm, without obvious odor.

[0177] The solid product obtained by direct dry distillation in Comparative Example 1 is a coked block solid, which can only be cleaned manually and has a noticeable odor on site.

[0178] In Example 3, no solid particles were loaded, the gas-liquid-solid mixing effect was poor, the NMP recovery rate was slightly low, and the slag particle size was relatively large, but there was no obvious odor on site.

[0179] In Comparative Example 4 and Example 5, the inclination angle of the lateral scrapers on both sides of the end of the stirring blade away from the stirring shaft affects the gas-liquid-solid mixing, and it is necessary to ensure that the angle is smaller than the repose angle. When the angle deviates, the NMP recovery rate is low.

[0180] Comparing Example 4 and Example 6, the gas in Example 4 did not pass through the cyclone separator, resulting in a large amount of fine powder particles in the NMP recovery liquid, and the NMP recovery liquid looked like black water, and the quality was problematic; Example 6 used a heat exchanger for cooling, and the gas temperature near the exhaust gas outlet showed an upward trend, indicating that the heat exchanger was blocked and the NMP recovery rate decreased.

[0181] Comparing Example 1, Example 3 and Example 7, Example 7 adjusts the cone apex angle of the conical structure of the solid buffer tank 4, and after the adjustment, the material discharge is not smooth.

[0182] The technical features of the above-described embodiments may be arbitrarily combined. To make the description concise, not all possible combinations of the technical features in the above-described embodiments are described. However, as long as there is no contradiction in the combination of these technical features, they should be considered to be within the scope of this specification.

[0183] The above-described embodiments only express several implementation methods of the present application, and the descriptions thereof are relatively specific and detailed, but they cannot be construed as limiting the scope of the patent application. It should be pointed out that, for a person of ordinary skill in the art, several variations and improvements can be made without departing from the concept of the present application, and these all belong to the protection scope of the present application. Therefore, the protection scope of the patent application shall be subject to the attached claims.

Claims

1. A method for recovering a purification solvent for producing acetylene from natural gas, characterized in that: The purification solvent comprises a polymer; and the recovery method comprises: The purification solvent is heated and stirred by a full-phase evaporator (1) so that the solvent to be recovered in the purification solvent evaporates and the polymer in the purification solvent is dispersed under stirring; The evaporated solvent to be recovered is collected and condensed to recover the solvent to be recovered.

2. The recycling method according to claim 1, characterized in that: The method of using a full-phase evaporator (1) to heat and stir the purification solvent so that the solvent to be recovered in the purification solvent evaporates and the polymer in the purification solvent is dispersed under stirring comprises: The purification solvent is sprayed into the full-phase evaporator (1) under heating and stirring, and the purification solvent is heated by making use of the wall of the full-phase evaporator (1) to contact with the purification solvent.

3. The recycling method according to claim 2, characterized in that: Under heating and stirring, the purification solvent is sprayed into the full-phase evaporator (1), comprising: A negative pressure is applied to the full-phase evaporator (1) according to the heating temperature, and the purification solvent is sprayed into the full-phase evaporator (1) by means of negative pressure suction, so as to adjust the spray amount of the purification solvent sprayed into the full-phase evaporator (1).

4. The recycling method according to claim 3, characterized in that: The heating temperature and the absolute value of the negative pressure satisfy: T=106*P^(0.172), wherein T represents the heating temperature and P represents the absolute value of the negative pressure.

5. The recycling method according to claim 4, characterized in that: The heating temperature T is 150° C. to 200° C., and the absolute value P of the negative pressure is 1 kPaA to 20 kPaA.

6. The recovery method according to any one of claims 2 to 5, characterized in that: Under heating and stirring, the purification solvent is sprayed into the full-phase evaporator (1), and the purification solvent is contacted with the wall of the full-phase evaporator (1). Before the purification solvent is heated, the recovery method further comprises: Solid particles are loaded into the full-phase evaporator (1), and the solid particles are heated and stirred, so that the solid particles can be used to adsorb and conduct heat to the purified solvent sprayed into the full-phase evaporator (1).

7. The recycling method according to claim 6, characterized in that: The solid particles satisfy at least one of the following conditions: (1) The particle size of the solid particles is 5 mm to 50 mm; (2) The filling volume of the solid particles accounts for 10% to 30% of the total volume of the full-phase evaporator; (3) The solid particles include at least one of condensed aromatic hydrocarbon polymer particles and silicate particles.

8. The recycling method according to any one of claims 1 to 5, characterized in that: Before the purification solvent is heated and stirred by the full-phase evaporator (1) to evaporate the solvent to be recovered in the purification solvent and to disperse the polymer in the purification solvent under stirring, the recovery method further comprises: Pre-treating the purification solvent to control the content of the polymer to 2% to 20%; Optionally, the pretreatment comprises flash evaporation and / or centrifugal separation.

9. The recycling method according to any one of claims 1 to 5, characterized in that: The bottom of the full-phase evaporator (1) is provided with a first slag discharge port (11); the steps of collecting and condensing the evaporated solvent to be recovered to recover the solvent to be recovered include: Capturing the gaseous product generated in the full-phase evaporator (1), filtering out solid impurities entrained in the captured gaseous product, and condensing the gaseous product from which the solid impurities have been filtered out, so as to recover the solvent to be recovered; and / or, The recovery method further comprises: discharging the solid product produced in the full-phase evaporator (1) through a first slag discharge port (11) of the full-phase evaporator (1).

10. The recycling method according to claim 9, characterized in that: An overflow weir (12) is arranged above the first slag discharge port (11) of the full-phase evaporator (1), and the upper end of the overflow weir (12) is 0.01R~0.2R higher than the bottom surface of the full-phase evaporator (1), where R represents the inner diameter of the full-phase evaporator (1); Discharging the solid product produced by the full-phase evaporator (1) through the first slag discharge port (11) of the full-phase evaporator (1), comprising: When the material level of the solid product generated by the full-phase evaporator (1) is higher than the upper end of the overflow weir (12), the solid product is discharged through the first slag discharge port (11) to the solid buffer tank (2) for buffering by overflow.

11. The recycling method according to claim 10, characterized in that: The recycling method further comprises: Discharging the solid product in the solid buffer tank (2) at preset time intervals; and / or, When the material level of the solid product in the solid buffer tank (2) reaches a preset height, the solid product in the solid buffer tank (2) is discharged.

12. A purification solvent recovery system for producing acetylene from natural gas, characterized in that: include: A full-phase evaporator (1) and a collection and condensation device (10) for the solvent to be recovered; The full-phase evaporator (1) is provided with a gas outlet (13), and the full-phase evaporator (1) is used to heat and stir the purification solvent, so that the solvent to be recovered in the purification solvent evaporates, and the polymer in the purification solvent is dispersed under stirring; the collection and condensation device for the solvent to be recovered is used to collect and condense the evaporated solvent to be recovered, so as to recover the solvent to be recovered.

13. The recovery system according to claim 12, characterized in that: The device (10) for collecting and condensing the solvent to be recovered comprises: a cyclone separator (3) and a gas condensing device (4); The cyclone separator (3) is used to capture the gaseous product generated in the full-phase evaporator (1) and to filter out solid impurities entrained in the captured gaseous product; The gas condensation device (4) is used to condense the gas product from which solid impurities have been filtered out.

14. The recovery system according to claim 13, characterized in that: The cyclone separator (3) is an inverted cone-shaped structure, comprising an air inlet (31), an air outlet (32) and a solid outlet (33); The air inlet (31) of the cyclone separator (3) is arranged on the side wall of the inverted conical structure and is in communication with the gas outlet (13) of the full-phase evaporator (1); the air outlet (32) of the cyclone separator (3) is arranged at the top of the inverted conical structure and is in communication with the gas condensation device (4); and the solid outlet (33) of the cyclone separator (3) is arranged at the bottom of the inverted conical structure. The recovery system further comprises: a solid return pipe (20), wherein a first end of the solid return pipe (20) is in communication with a solid outlet (33) of the cyclone separator (3), and a second end of the solid return pipe (20) vertically extends into the full-phase evaporator (1).

15. The recovery system according to claim 14, characterized in that The distance between the second end of the solid reflux pipe (20) and the bottom surface of the full-phase evaporator (1) is 0.01R-0.2R, wherein R represents the inner diameter of the full-phase evaporator (1).

16. The recovery system according to any one of claims 12 to 15, characterized in that: The full-phase evaporator (1) is also provided with a spraying device (14), and the spraying device (14) is used to spray the purification solvent into the full-phase evaporator (1).

17. The recovery system according to any one of claims 12 to 15, characterized in that: The full-phase evaporator (1) is also provided with a feed port (15), and the feed port (15) is used to load solid particles into the full-phase evaporator (1).

18. The recovery system according to any one of claims 12 to 15, characterized in that: The full-phase evaporator (1) is a horizontal reactor. The full-phase evaporator (1) is further provided with a stirring device (16). The stirring device (16) comprises a stirring shaft (161) and a plurality of stirring blades (162) arranged on the stirring shaft (161). The stirring shaft (161) extends along the axial direction of the horizontal reactor. Each stirring blade (162) is coplanar with the stirring shaft (161). Each stirring blade (162) is further provided with side scrapers (163) on opposite sides along the thickness direction and at one end away from the stirring shaft (161). The angle α between the plane where each side scraper (163) is located and the stirring shaft (161) is greater than 0° and less than or equal to 36°.

19. The recovery system according to any one of claims 12 to 15, characterized in that: The bottom of the full-phase evaporator (1) is provided with a first slag discharge port (11), and an overflow weir (12) is provided above the first slag discharge port (11) of the full-phase evaporator (1), and the upper end surface of the overflow weir (12) is higher than the bottom surface of the full-phase evaporator (1) by 0.01R to 0.2R, where R represents the inner diameter of the full-phase evaporator (1); The recovery system further comprises: a solid buffer tank (2) connected below the first slag discharge port (11) of the full-phase evaporator (1).

20. The recovery system according to claim 19, characterized in that The recovery system further comprises: a controller (5) and a solid storage tank (6); The solid storage tank (6) is connected to the bottom of the solid buffer tank (2); a second slag discharge port (21) connected to the solid storage tank (6) is provided at the bottom of the solid buffer tank (2); a solenoid valve (a) is provided at the second slag discharge port (21) of the solid buffer tank (2); the controller (5) is electrically connected to the solenoid valve (a); the controller (5) is used to control the solenoid valve (a) to open at preset intervals to discharge the solid product in the solid buffer tank (2) into the solid storage tank (6); and / or, a material level detector is further provided in the solid buffer tank (2); the controller (5) is used to control the solenoid valve (a) to open when the material level detector detects that the material level in the solid buffer tank (2) reaches a preset height to discharge the solid product in the solid buffer tank (2) into the solid storage tank (6).

Citation Information

Patent Citations

  • Anti-blocking type vacuum harrow dryer

    CN104713335A

  • 2-benzothiazolethiol nitrogen circulation drying and solvent recovery method

    CN105004145A

  • A device for retrieving wrap up solvent among solid material

    CN207615355U

  • A TVR falling film evaporator

    CN220989687U

Cited By

  • Method for purifying and recovering NMP (N-Methyl Pyrrolidone) from NMP regenerated liquid

    CN120081774A