Photovoltaic floor sealed by modified camellia oil adhesive film
By using modified camellia oil film and other structural components on photovoltaic floors, the problem of insufficient dependence and safety of existing photovoltaic floors on petroleum resources has been solved, carbon neutrality and safety has been improved, and the photovoltaic power generation area has been expanded. Application scope.
Patent Information
- Application Number
- CN202411138629.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-19
- Publication Date
- 2024-11-22
AI Technical Summary
Existing photovoltaic floors rely on petroleum derivatives in glue seals, making it difficult to achieve carbon neutrality, and lack waterproof and anti-slip structures, which cannot effectively increase the photovoltaic power generation area and safety.
Modified camellia oil adhesive film is used as the sealing material. By setting a modified camellia oil adhesive layer, sealing ring, fitting groove, fitting rod and anti-slip rod on the photovoltaic floor, a waterproof and anti-slip structure is formed to reduce the dependence of petroleum resources.
The carbon neutrality goal has been achieved, waterproof performance and anti-slip capabilities have been enhanced, the photovoltaic power generation area and application range have been expanded, and the artistic and interesting nature of the product has been improved.
Smart Images

Figure CN118997419A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of flooring, in particular to a photovoltaic flooring sealed by using a modified camellia oil film. Background Art
[0002] Photovoltaic flooring is a new type of flooring that combines flooring with photovoltaic power generation components. Installing photovoltaic power generation components on the floor can increase the area of photovoltaic power generation. Traditional floors use glue to seal photovoltaic cells. The glue is mostly petroleum derivatives. Excessive reliance on petroleum derivatives is not conducive to the realization of carbon neutrality.
[0003] The defects of the existing floor are: 1. The prior art KR1020140053994A discloses a photovoltaic module and a laminate. In this technology, the photovoltaic cells and glass panels are bonded using traditional petroleum derivative glue, which is not conducive to achieving carbon neutrality. Therefore, a photovoltaic floor sealed with a modified camellia oil film that does not use petroleum derivative glue for bonding and sealing is needed to solve this problem.
[0004] 2. The prior art KR100958396B1 discloses a floor, which does not have the technology to combine photovoltaic cells with the floor, and cannot use the floor to increase the power generation area of the photovoltaic cells. Therefore, a photovoltaic floor sealed with a modified camellia oil film that combines photovoltaic cells with the floor to increase the photovoltaic power generation area is needed to solve this problem.
[0005] 3. The prior art KR1020060030561A discloses a floor, which does not have a structure for splicing and sealing at the floor part. Water on the floor can easily seep downward through the splicing parts of the floor, which is not conducive to the drying of the battery cells. Therefore, a photovoltaic floor with a waterproof sealing structure and sealed with a modified camellia oil film is needed to solve this problem.
[0006] 4. Prior art CN107476534A discloses a multifunctional suspended assembled floor. This technical floor does not have an anti-slip structure. When photovoltaic cells are set on the floor, a glass surface is generally used as the floor surface. People are prone to slip when walking on the glass. Therefore, a photovoltaic floor with anti-slip ability and sealed with a modified camellia oil film is needed to solve this problem. Summary of the invention
[0007] One purpose of the present application is to provide a photovoltaic floor sealed with a modified camellia oil film, which can solve the technical problems raised in the prior art.
[0008] To achieve the above-mentioned purpose, the present invention provides the following technical scheme: a photovoltaic floor sealed with a modified camellia oil film, the photovoltaic floor comprising, from bottom to top, a glass plate 1, a modified camellia oil adhesive layer 1, a battery cell, a modified camellia oil adhesive layer 2, a glass plate 2, a sealing ring, an interlocking groove, an interlocking rod and an anti-slip rod, the modified camellia oil adhesive layer 1 is located above the glass plate 1, the battery cell is located above the modified camellia oil adhesive layer 1, the modified camellia oil adhesive layer 2 is located above the battery cell, the glass plate 2 is located above the modified camellia oil adhesive layer 2, the sealing ring is located on the outside of the glass plate 1, the modified camellia oil adhesive layer 1, the battery cell, the modified camellia oil adhesive layer 2 and the glass plate 2, the interlocking groove is opened on the front and right sides of the sealing ring, the interlocking rod is arranged on the left and back sides of the sealing ring, and the anti-slip rod is arranged at equal intervals above the glass plate 2.
[0009] Preferably, the preparation method of the modified camellia oil gum of the modified camellia oil gum layer 1 and the modified camellia oil gum layer 2 comprises the following steps: a: Add 200 g of camellia oil containing 0.224 mol into a flask, then add 37.1 g, 88 wt% of formic acid containing 0.710 mol and 149.9 g, 30 wt% of hydrogen peroxide containing 1.323 mol, and react in a water bath at 40°C for 20 hours. After the reaction is completed, extract the epoxidation product with ether, wash with distilled water and saturated sodium bicarbonate solution until neutral, then dry the ether phase over anhydrous magnesium sulfate, filter through diatomaceous earth, and remove the ether with a vacuum rotary evaporator; b: The synthesis of acrylate epoxy camellia oil AECO was carried out in a 500 ml three-necked flask equipped with a mechanical stirrer in a silicone oil bath. 1.1 mol of acrylic acid was used to 1 mol of epoxy camellia oil to obtain acrylate epoxy camellia oil containing 1 acrylic acid group per triglyceride. 100 g of 0.104 mol of epoxidized camellia oil was charged into the flask, and then 0.33 g of 0.003 mol of hydroquinone as an acrylate polymerization inhibitor and 0.435 g of AMC-2 as an acrylate catalyst were added. When the temperature of the reactants reached 80°C, 8.20 g of 7.81 ml of acrylic acid containing 0.114 mol was mixed into the flask. The reaction lasted for 4 hours. The product was purified by ether extraction, and the hydroquinone inhibitor and excess acrylic acid were washed off with water. The organic phase was dried over anhydrous magnesium sulfate, filtered and concentrated in vacuo to obtain AECO. c: Using AECO as raw material, water and acid as catalysts, the remaining epoxy groups were converted into dihydroxyl groups to synthesize acrylated camelina oil polyol DAECO; d: 50 g of AECO containing 0.048 mol was transferred to a 250 ml flask, 50 ml of tetrahydrofuran was added to dissolve AECO, 25 ml of distilled water and 1.073 ml of 70 wt% aqueous solution of 0.012 mol of perchloric acid were mixed in another flask, and then gradually dripped into the AECO flask under stirring within 2 minutes, and the reaction was continued at room temperature for 5 hours. The product was purified by extraction with ethyl acetate, washed with distilled water, neutralized with saturated sodium bicarbonate solution, and the organic phase was dried over anhydrous magnesium sulfate and evaporated with a rotary evaporator under vacuum to obtain 47.5 g of pure DAECO; e: DAECO was mixed with 2-EHA and rosin tackifying resin in a ratio of 2:2:1. In some formulations, 5% of the total mass fraction of photoinitiator 2-hydroxy-2-methylpropiophenone was added. The mixture was fully mixed with the help of a vortex mixer and a sonar to obtain a modified camellia oil glue solution.
[0010] Preferably, the sealing ring is made of soft rubber material.
[0011] Preferably, the anti-slip rod is made of plastic or rubber.
[0012] Preferably, the engaging rod is made of plastic or rubber.
[0013] Preferably, the glass plate 1 is ultra-white glass.
[0014] Preferably, the sealing ring is glued to the first glass plate, and the battery cell and the second glass plate by using modified camellia oil glue.
[0015] Preferably, the distance between the glass plate 1 and the glass plate 2 is 3 mm.
[0016] Preferably, the preparation method of the photovoltaic floor sealed with the modified camellia oil film is as follows: S1, placing a glass plate 1 on a substrate, then applying a modified camellia oil glue solution on the glass plate 1 to form a modified camellia oil glue layer 1, and then laying a cell flat on the modified camellia oil glue layer 1; S2, applying the modified camellia oil glue liquid on the battery cell to form a second modified camellia oil glue layer, and then laying the second glass plate flat on the second modified camellia oil glue layer; S3, coating the inner wall of the sealing ring with modified camellia oil glue, then sleeve the sealing ring on the outer sides of the glass plate 1, the battery cell and the glass plate 2, and then glue the anti-slip bars to the glass plate 2 at equal intervals using the modified camellia oil glue.
[0017] Preferably, it is characterized in that: said S3 also includes the following steps: S31. Before the sealing ring is sleeved on the outer sides of the glass plate 1, the battery cell and the glass plate 2, hot melt rubber is put into a mold to form a sealing ring with an engaging rod and an engaging groove.
[0018] Compared with the prior art, the present invention has the following beneficial effects: 1. The present invention is provided with a modified camellia oil glue layer 1 and a modified camellia oil glue layer 2. By using the modified camellia oil glue for sealing, it is helpful to reduce the dependence on petroleum resources and to achieve the goal of "carbon neutrality".
[0019] 2. The present invention combines photovoltaic tiles with buildings to construct photovoltaic floors, which increases the artistry and interest of the product and expands the application scope of photovoltaic tiles.
[0020] 3. The sealing ring, the interlocking rod and the interlocking groove provided in the present invention can effectively reduce the waterproof performance of the floor, so that the water above the glass plate is not easy to penetrate into the bottom of the spliced floor or onto the battery cells.
[0021] 4. The anti-slip rods provided in the present invention can effectively increase the anti-slip ability of the floor and reduce the probability of people slipping when walking on the glass plate. BRIEF DESCRIPTION OF THE DRAWINGS
[0022] Figure 1 It is a structural schematic diagram of the present invention; Figure 2 It is a schematic diagram of the battery cell structure of the present invention; Figure 3 It is a flow chart of the preparation method of the present invention.
[0023] In the figure: 1. Glass plate 1; 2. Modified camellia oil adhesive layer 1; 3. Battery cell; 4. Modified camellia oil adhesive layer 2; 5. Glass plate 2; 6. Sealing ring; 7. Fitting groove; 8. Fitting rod; 9. Anti-slip rod. DETAILED DESCRIPTION
[0024] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0025] In the description of the present invention, it should be noted that the terms "upper", "lower", "inner", "outer", "front end", "rear end", "two ends", "one end", "the other end" and the like indicate positions or positional relationships based on the positions or positional relationships shown in the drawings, and are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as limiting the present invention. In addition, the terms "first" and "second" are used for descriptive purposes only and cannot be understood as indicating or implying relative importance.
[0026] In the description of the present invention, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "provided with", "connected", etc. should be understood in a broad sense. For example, "connected" can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, or it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0027] See also Figure 1 , Figure 2 and Figure 3 A photovoltaic floor sealed with a modified camellia oil film, the photovoltaic floor comprising from bottom to top a glass plate 1, a modified camellia oil adhesive layer 2, a battery cell 3, a modified camellia oil adhesive layer 24, a glass plate 25, a sealing ring 6, an interlocking groove 7, an interlocking rod 8 and an anti-slip rod 9, the modified camellia oil adhesive layer 2 is located above the glass plate 1, the battery cell 3 is located above the modified camellia oil adhesive layer 2, the modified camellia oil adhesive layer 24 is located above the battery cell 3, the glass plate 25 is located above the modified camellia oil adhesive layer 24, the sealing ring 6 is located on the outer sides of the glass plate 1, the modified camellia oil adhesive layer 2, the battery cell 3, the modified camellia oil adhesive layer 24 and the glass plate 25, the interlocking groove 7 is opened on the front and right sides of the sealing ring 6, the interlocking rod 8 is arranged on the left and back sides of the sealing ring 6, and the anti-slip rods 9 are arranged above the glass plate 25 at equal intervals.
[0028] The preparation method of the modified camellia oil gum of the modified camellia oil gum layer 1 2 and the modified camellia oil gum layer 2 4 comprises the following steps: a: Add 200 g of camellia oil containing 0.224 mol into a flask, then add 37.1 g, 88 wt% of formic acid containing 0.710 mol and 149.9 g, 30 wt% of hydrogen peroxide containing 1.323 mol, and react in a water bath at 40°C for 20 hours. After the reaction is completed, extract the epoxidation product with ether, wash with distilled water and saturated sodium bicarbonate solution until neutral, then dry the ether phase over anhydrous magnesium sulfate, filter through diatomaceous earth, and remove the ether with a vacuum rotary evaporator; b: The synthesis of acrylate epoxy camellia oil AECO was carried out in a 500 ml three-necked flask equipped with a mechanical stirrer in a silicone oil bath. 1.1 mol of acrylic acid was used to 1 mol of epoxy camellia oil to obtain acrylate epoxy camellia oil containing 1 acrylic acid group per triglyceride. 100 g of 0.104 mol of epoxidized camellia oil was charged into the flask, and then 0.33 g of 0.003 mol of hydroquinone as an acrylate polymerization inhibitor and 0.435 g of AMC-2 as an acrylate catalyst were added. When the temperature of the reactants reached 80°C, 8.20 g of 7.81 ml of acrylic acid containing 0.114 mol was mixed into the flask. The reaction lasted for 4 hours. The product was purified by ether extraction, and the hydroquinone inhibitor and excess acrylic acid were washed off with water. The organic phase was dried over anhydrous magnesium sulfate, filtered and concentrated in vacuo to obtain AECO. c: Using AECO as raw material, water and acid as catalysts, the remaining epoxy groups were converted into dihydroxyl groups to synthesize acrylated camelina oil polyol DAECO; d: 50 g of AECO containing 0.048 mol was transferred to a 250 ml flask, 50 ml of tetrahydrofuran was added to dissolve AECO, 25 ml of distilled water and 1.073 ml of 70 wt% aqueous solution of 0.012 mol of perchloric acid were mixed in another flask, and then gradually dripped into the AECO flask under stirring within 2 minutes, and the reaction was continued at room temperature for 5 hours. The product was purified by extraction with ethyl acetate, washed with distilled water, neutralized with saturated sodium bicarbonate solution, and the organic phase was dried over anhydrous magnesium sulfate and evaporated with a rotary evaporator under vacuum to obtain 47.5 g of pure DAECO; e: DAECO was mixed with 2-EHA and rosin tackifying resin in a ratio of 2:2:1. In some formulations, 5% of the total mass fraction of photoinitiator 2-hydroxy-2-methylpropiophenone was added. The mixture was fully mixed with the help of a vortex mixer and a sonar to obtain a modified camellia oil glue solution.
[0029] The sealing ring 6 is made of soft rubber material.
[0030] The anti-slip bar 9 is made of plastic or rubber.
[0031] The engaging rod 8 is made of plastic or rubber.
[0032] Glass plate 1 is ultra-clear glass.
[0033] The sealing ring 6 is glued to the glass plate 1, the battery cell 3 and the glass plate 2 5 by using modified camellia oil glue.
[0034] The distance between glass plate 1 and glass plate 2 5 is 3 mm.
[0035] The preparation method of the photovoltaic floor sealed with modified camellia oil film is as follows: S1, placing a glass plate 1 on a substrate, then applying a modified camellia oil glue solution on the glass plate 1 to form a modified camellia oil glue layer 2, and then laying a battery cell 3 flat on the modified camellia oil glue layer 2; S2, applying the modified camellia oil glue liquid on the battery cell 3 to form a modified camellia oil glue layer 2 4, and then laying the glass plate 2 5 flat on the modified camellia oil glue layer 2 4; S3, apply modified camellia oil glue on the inner wall of the sealing ring 6, then put the sealing ring 6 on the outer side of the glass plate 1, the battery cell 3 and the glass plate 2 5, and then glue the anti-slip bars 9 to the glass plate 2 5 at equal intervals through the modified camellia oil glue.
[0036] S3 also includes the following steps: S31. Before the sealing ring 6 is sleeved on the outer sides of the glass plate 1 , the battery cell 3 and the glass plate 2 5 , hot melt rubber is put into a mold to form the sealing ring 6 with the engaging rod 8 and the engaging groove 7 .
[0037] Embodiment 1: 1. Place a glass plate 1 on the substrate, then apply the modified camellia oil glue solution on the glass plate 1 to form a modified camellia oil glue layer 2, and then lay the battery cell 3 flat on the modified camellia oil glue layer 2; 2. Apply the modified camellia oil glue liquid on the battery cell 3 to form a modified camellia oil glue layer 2 4, and then lay the glass plate 2 5 flat on the modified camellia oil glue layer 2 4; 3. Before the sealing ring 6 is sleeved on the outer sides of the glass plate 1, the battery cell 3 and the glass plate 2 5, hot melt rubber is put into the mold to form the sealing ring 6 with the interlocking rod 8 and the interlocking groove 7; Fourth, apply modified camellia oil glue on the inner wall of the sealing ring 6, then put the sealing ring 6 on the outside of the glass plate 1, the battery cell 3 and the glass plate 2 5, and then glue the anti-slip bars 9 to the glass plate 2 5 at equal intervals through the modified camellia oil glue.
[0038] Embodiment 2: 1. Place a glass plate 1 on the substrate, then apply the modified camellia oil glue solution on the glass plate 1 to form a modified camellia oil glue layer 2, and then lay the battery cell 3 flat on the modified camellia oil glue layer 2; 2. Apply the modified camellia oil glue liquid on the battery cell 3 to form a modified camellia oil glue layer 2 4, and then lay the glass plate 2 5 flat on the modified camellia oil glue layer 2 4; 3. Apply modified camellia oil glue on the inner wall of the sealing ring 6, then put the sealing ring 6 on the outside of the glass plate 1, the battery cell 3 and the glass plate 2 5, and then glue the anti-slip bars 9 to the glass plate 2 5 at equal intervals through the modified camellia oil glue.
[0039] Embodiment three: 1. Place a glass plate 1 on the substrate, then apply the modified camellia oil glue solution on the glass plate 1 to form a modified camellia oil glue layer 2, and then lay the battery cell 3 flat on the modified camellia oil glue layer 2; 2. Apply the modified camellia oil glue liquid on the battery cell 3 to form a modified camellia oil glue layer 2 4, and then lay the glass plate 2 5 flat on the modified camellia oil glue layer 2 4; 3. Before the sealing ring 6 is sleeved on the outer sides of the glass plate 1, the battery cell 3 and the glass plate 2 5, hot melt rubber is put into the mold to form the sealing ring 6 with the interlocking rod 8 and the interlocking groove 7; Fourth, the inner wall of the sealing ring 6 is coated with modified camellia oil glue, and then the sealing ring 6 is put on the outer sides of the glass plate 1, the battery cell 3 and the glass plate 2 5.
[0040] Embodiment 4: 1. Place a glass plate 1 on the substrate, then apply the modified camellia oil glue solution on the glass plate 1 to form a modified camellia oil glue layer 2, and then lay the battery cell 3 flat on the modified camellia oil glue layer 2; 2. Apply the modified camellia oil glue liquid on the battery cell 3 to form a modified camellia oil glue layer 2 4, and then lay the glass plate 2 5 flat on the modified camellia oil glue layer 2 4; 3. The anti-skid bars 9 are glued to the glass plate 2 5 at equal intervals by using modified camellia oil glue.
[0041] Embodiment five: 1. Place a glass plate 1 on the substrate, then apply the modified camellia oil glue solution on the glass plate 1 to form a modified camellia oil glue layer 2, and then lay the battery cell 3 flat on the modified camellia oil glue layer 2; 2. Apply the modified camellia oil glue liquid on the battery cell 3 to form a modified camellia oil glue layer 2 4 , and then lay the glass plate 2 5 flat on the modified camellia oil glue layer 2 4 .
[0042] Performance Test: 1. Waterproof performance of multiple floors after splicing: Splice the products of each embodiment separately, pour water on the spliced products, and observe whether there is water under the products after 10 minutes; 2. Anti-slip performance: A wooden board was placed on the product of each embodiment, and then an object of the same weight was placed on the wooden board, and then the thrust required to move the wooden board was measured.
[0043] Test data of each embodiment under the same test conditions Embodiment 1 Embodiment 2 Embodiment 3 Embodiment 4 Embodiment 5 Is there water? none none none have have Thrust size (N) 15.3 14.8 4.5 14.6 4.8 It can be seen from the experimental data that the setting of the sealing ring 6, the interlocking rod and the interlocking groove 7 can effectively reduce the waterproof performance of the floor, so that the water above the glass plate 1 is not easy to penetrate into the bottom of the spliced floor. The setting of the anti-slip rod 9 can effectively increase the anti-slip ability of the floor. The use of modified camellia oil glue for sealing is conducive to reducing dependence on petroleum resources and achieving the goal of "carbon neutrality". Combining photovoltaic tiles with buildings to construct photovoltaic floors increases the artistry and interest of the products and expands the application scope of photovoltaic tiles.
[0044] It is obvious to those skilled in the art that the present invention is not limited to the details of the exemplary embodiments described above, and that the present invention can be implemented in other specific forms without departing from the spirit or essential features of the present invention. Therefore, from all points of view, the embodiments should be regarded as exemplary and non-restrictive, and the scope of the present invention is defined by the appended claims rather than the above description, and it is intended that all changes falling within the meaning and scope of the equivalent elements of the claims are included in the present invention, and any reference signs in the claims should not be regarded as limiting the rights involved.
Claims
1. A photovoltaic floor sealed with a modified camellia oil film, characterized in that: The photovoltaic floor comprises, from bottom to top, a glass plate 1 (1), a modified camellia oil adhesive layer 1 (2), a battery cell (3), a modified camellia oil adhesive layer 2 (4), a glass plate 2 (5), a sealing ring (6), an interlocking groove (7), an interlocking rod (8) and an anti-slip rod (9), wherein the modified camellia oil adhesive layer 1 (2) is located above the glass plate 1 (1), the battery cell (3) is located above the modified camellia oil adhesive layer 1 (2), and the modified camellia oil adhesive layer 2 (4) is located above the battery cell (3). The second glass plate (5) is located above the second modified camellia oil adhesive layer (4), the sealing ring (6) is located outside the first glass plate (1), the first modified camellia oil adhesive layer (2), the battery cell (3), the second modified camellia oil adhesive layer (4) and the second glass plate (5), the engaging groove (7) is opened on the front and right sides of the sealing ring (6), the engaging rod (8) is arranged on the left and back sides of the sealing ring (6), and the anti-slip rods (9) are arranged above the second glass plate (5) at equal intervals.
2. The photovoltaic floor sealed with modified camellia oil film according to claim 1, characterized in that: The preparation method of the modified camellia oil gum of the modified camellia oil gum layer 1 (2) and the modified camellia oil gum layer 2 (4) comprises the following steps: a: Add 200 g of camellia oil containing 0.224 mol into a flask, then add 37.1 g, 88 wt% of formic acid containing 0.710 mol and 149.9 g, 30 wt% of hydrogen peroxide containing 1.323 mol, and react in a water bath at 40°C for 20 hours. After the reaction is completed, extract the epoxidation product with ether, wash with distilled water and saturated sodium bicarbonate solution until neutral, then dry the ether phase over anhydrous magnesium sulfate, filter through diatomaceous earth, and remove the ether with a vacuum rotary evaporator; b: The synthesis of acrylate epoxy camellia oil AECO was carried out in a 500 ml three-necked flask equipped with a mechanical stirrer in a silicone oil bath. 1.1 mol of acrylic acid was used to 1 mol of epoxy camellia oil to obtain acrylate epoxy camellia oil containing 1 acrylic acid group per triglyceride. 100 g of 0.104 mol of epoxidized camellia oil was charged into the flask, and then 0.33 g of 0.003 mol of hydroquinone as an acrylate polymerization inhibitor and 0.435 g of AMC-2 as an acrylate catalyst were added. When the temperature of the reactants reached 80°C, 8.20 g of 7.81 ml of acrylic acid containing 0.114 mol was mixed into the flask. The reaction lasted for 4 hours. The product was purified by ether extraction, and the hydroquinone inhibitor and excess acrylic acid were washed off with water. The organic phase was dried over anhydrous magnesium sulfate, filtered and concentrated in vacuo to obtain AECO. c: Using AECO as raw material, water and acid as catalysts, the remaining epoxy groups were converted into dihydroxyl groups to synthesize acrylated camelina oil polyol DAECO; d: 50 g of AECO containing 0.048 mol was transferred to a 250 ml flask, 50 ml of tetrahydrofuran was added to dissolve AECO, 25 ml of distilled water and 1.073 ml of 70 wt% aqueous solution of 0.012 mol of perchloric acid were mixed in another flask, and then gradually dripped into the AECO flask under stirring within 2 minutes, and the reaction was continued at room temperature for 5 hours. The product was purified by extraction with ethyl acetate, washed with distilled water, neutralized with saturated sodium bicarbonate solution, and the organic phase was dried over anhydrous magnesium sulfate and evaporated with a rotary evaporator under vacuum to obtain 47.5 g of pure DAECO; e: DAECO was mixed with 2-EHA and rosin tackifying resin in a ratio of 2:2:
1. In some formulations, 5% of the total mass fraction of photoinitiator 2-hydroxy-2-methylpropiophenone was added. The mixture was fully mixed with the help of a vortex mixer and a sonar to obtain a modified camellia oil glue solution.
3. The photovoltaic floor sealed with modified camellia oil film according to claim 1, characterized in that: The sealing ring (6) is made of soft rubber material.
4. The photovoltaic floor sealed with modified camellia oil film according to claim 1, characterized in that: The anti-slip rod (9) is made of plastic or rubber.
5. The photovoltaic floor sealed with modified camellia oil film according to claim 1, characterized in that: The engaging rod (8) is made of plastic or rubber.
6. A photovoltaic floor sealed with modified camellia oil film according to any one of claim 1, characterized in that: The glass plate 1 (1) is ultra-clear glass.
7. The photovoltaic floor sealed with modified camellia oil film according to claim 2, characterized in that: The sealing ring (6) is glued to the first glass plate (1), the battery cell (3) and the second glass plate (5) using modified camellia oil glue.
8. The photovoltaic floor sealed with modified camellia oil film according to claim 1, characterized in that: The distance between the glass plate 1 (1) and the glass plate 2 (5) is 3 mm.
9. The method for preparing a photovoltaic floor sealed with a modified camellia oil film according to claim 1, characterized in that: The preparation method of the photovoltaic floor sealed with the modified camellia oil film is as follows: S1, placing a glass plate (1) on a substrate, then applying a modified camellia oil adhesive liquid on the glass plate (1) to form a modified camellia oil adhesive layer (2), and then laying a battery cell (3) flat on the modified camellia oil adhesive layer (2); S2, applying the modified camellia oil glue liquid on the battery cell (3) to form a second modified camellia oil glue layer (4), and then laying a second glass plate (5) flat on the second modified camellia oil glue layer (4); S3, coating the inner wall of the sealing ring (6) with modified camellia oil glue, then putting the sealing ring (6) on the outer sides of the glass plate 1 (1), the battery cell (3) and the glass plate 2 (5), and then gluing the anti-slip bars (9) to the glass plate 2 (5) at equal intervals using the modified camellia oil glue.
10. The method for preparing a photovoltaic floor sealed with a modified camellia oil film according to claim 1, characterized in that: The S3 also includes the following steps: S31. Before the sealing ring (6) is sleeved on the outer sides of the glass plate 1 (1), the battery cell (3) and the glass plate 2 (5), hot melt rubber is put into a mold to form a sealing ring (6) with an engaging rod (8) and an engaging groove (7).
Citation Information
Patent Citations
Multifunctional suspension assembled floors
CN107476534A
Floorboard
KR100958396B1
Support for floor boards
KR1020060030561A
Photovoltaic module and laminate
KR1020140053994A