Flow-adjustable spraying disc device and film thickness control method
By introducing an adjustable through-hole structure and a double-layer diffuser into the spray disk device, the problem of film thickness is solved, and the gas flow adjustment is achieved in different areas is improved, and the film uniformity and processing adaptability are reduced. Cost and processing difficulty.
Patent Information
- Application Number
- CN202411527766.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-10-30
- Publication Date
- 2024-11-29
AI Technical Summary
The existing spray disk structure cannot achieve regional adjustment of gas flow, resulting in uneven film thickness, especially in the epitaxial process, the temperature uniformity of the heating disk is insufficient, affecting the film thickness uniformity.
A spray disk device with adjustable flow is designed, including a back plate, spray disk, lower diffuser, upper diffuser, adjustment block and set-up seat. The gas flow is controlled by adjusting the different pore rates of the block, using dual The positioning method of the layer diffuser and the mounting seat realizes local flow adjustment, thereby adjusting the film thickness.
By controlling the flow rate of process gas, the uniformity of film thickness is achieved, the machine's adaptability to different process formulations and gas flow rates is expanded, the film uniformity and processing efficiency are improved, and the processing difficulty and cost are reduced.
Smart Images

Figure CN119040858A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of semiconductor film growth, and in particular to a spray plate device with adjustable flow rate and a film thickness control method. Background Art
[0002] Chemical vapor deposition is to pass the reaction gas into the reaction chamber to grow a thin film on the surface of the wafer at a set pressure and temperature. Thin film equipment has multi-chip and single-chip structures. The single-chip vertical structure is to let the process gas flow down from the top of the wafer, distribute it through the spray plate, and then contact the wafer placed on the heating plate for thin film deposition. The thickness uniformity of the film depends largely on the structure of the spray plate. Therefore, by optimizing the design and configuration of the spray plate, the efficiency and film quality of the thin film deposition process can be significantly improved.
[0003] The existing spray plate structure is fixed to achieve uniform distribution of gas. However, there are many factors that affect the uniformity of film thickness, such as process gas temperature, flow rate, temperature uniformity of the heating plate, etc. In the epitaxial process, the uniformity of the heating temperature of the heating plate on the wafer is particularly important. The arrangement of the heating wires inside the heating plate cannot achieve absolute uniformity of temperature, and the process gas blowing on the wafer will take away heat. Therefore, in order to make the film thickness consistent, it is necessary to adjust the gas flow rate on specific areas of the wafer according to the process results. For example, in some areas with thicker film thickness, the process gas flowing down the spray plate must be reduced. There is no relevant background for regional flow adjustment of the spray plate in the prior art. Summary of the invention
[0004] The purpose of the present invention is to provide a spray plate device with adjustable flow rate and a film thickness control method to solve the problem.
[0005] The above technical objectives of the present invention are achieved through the following technical solutions: A spray plate device with adjustable flow rate, comprising a back plate, a spray plate, a lower diffuser, an upper diffuser, an adjustment block and a setting seat, characterized in that the spray plate is fixedly arranged on the back plate, a lower diffuser and an upper diffuser are installed between the back plate and the spray plate, the upper diffuser is installed above the lower diffuser, the lower diffuser is fixed on the back plate, the setting seat is located in the middle of the back plate and the spray plate, the setting seat is installed on the lower diffuser, a plurality of vacancies are opened on the setting seat, the vacancies are used to accommodate and position the adjustment block, the adjustment blocks are provided with multiple blocks, a plurality of through holes of different specifications are opened on the adjustment blocks, the outer contour of the adjustment block matches the inner contour of the vacancies on the setting seat, the height of the adjustment block and the setting seat are consistent, a reaction chamber is also installed on the spray plate, a closed reaction space is formed between the back plate, the spray plate and the reaction chamber, a heating plate that can be raised and lowered is arranged on the reaction chamber, and the heating plate is located directly below the spray plate.
[0006] Preferably, an air inlet is opened in the middle of the back plate, a process gas inlet pipeline is connected to the upper end of the back plate, a first diffusion chamber is formed between the upper diffuser and the back plate, a second diffusion chamber is formed between the upper diffuser and the lower diffuser, and a third diffusion chamber is formed between the lower diffuser and the spray plate.
[0007] Preferably, a flow channel is further provided on the back plate, the flow channel is connected to an external cooling device, a heat exchange fluid flows in the flow channel, and the temperature of the heat exchange fluid can be adjusted between 15-75°C.
[0008] Preferably, a recessed groove is provided in the middle of the upper end surface of the upper diffuser, the edge of the upper diffuser is a raised mounting portion, a first fine through hole is provided on the entire surface of the recessed groove, the upper end of the mounting portion is in contact with the back plate, screw through holes and countersunk holes are evenly distributed on the mounting portion, a number of bosses are provided on the recessed groove, the height of the bosses is consistent with the height of the mounting portion, a screw through hole is provided at the center of the boss, a second recessed groove is provided in the middle of the lower diffuser, the outer periphery of the lower diffuser is a flange, a threaded hole and a countersunk hole are provided on the flange, the threaded hole corresponds to the position of the countersunk hole one, the countersunk hole two corresponds to the screw through hole, a second fine through hole is opened on the disk surface of the second recessed groove, and a positioning column is also provided on the second recessed groove.
[0009] Preferably, the setting seat is a connecting rib-like structure, the width of the connecting rib is set to be narrow, a plurality of vacancies are set on the setting seat, and adjustment blocks can be placed inside the vacancies. The height of the setting seat is consistent with the height of the second diffusion chamber. The setting seat is set in the second diffusion chamber. A positioning hole is opened on the setting seat, and the positioning hole matches the positioning column of the lower diffuser. The shape of the setting seat can be matrix, radial, or regular hexagonal.
[0010] Preferably, a through hole is opened in the middle of the adjustment block, the area corresponding to the through hole is the opening area, the solid area on the edge of the adjustment block is the shielding area, the outer contour of the adjustment block matches the shape of the vacant space, and a through hole is arranged inside the adjustment block. The shape of the adjustment block can be rectangular, sector-shaped and hexagonal.
[0011] A method for controlling film thickness with adjustable flow rate, S1 benchmark formulation: remove all adjustment blocks 5 in the spray plate device, install the setting seat 6, at this time, the lower diffuser 3 and the upper diffuser 4 are completely connected without obstruction, and then the process gas is introduced into the operating formula under this working condition to obtain the film thickness data of the silicon wafer, at this time, the thinner or thicker film thickness area is marked, and the position of the thinner or thicker area is mapped to the position of the lower diffuser 3; S2 Adjustment block installation: open the spray plate 2 and the lower diffuser 3, and set the adjustment block 5 on the area of the lower diffuser 3 corresponding to the thinner or thicker film thickness area. The opening rate of the adjustment block 5 is 50% for the first time, and all the areas with thinner film thickness are placed on the adjustment block 5; S3: re-run the original recipe: re-run the original thin film process recipe to obtain the correlation data between the relevant film thickness and the opening rate of the adjustment block 5; S4: Accurately adjust the opening rate of the adjustment block: Based on the correlation data between the film thickness and the opening rate of the adjustment block 5 obtained in the previous round, adjust the opening rate of the adjustment block 5 corresponding to the area with thinner or thicker film thickness to an optimal value, and then run the process recipe to obtain the film thickness data. If the film thickness data meets the requirements, the adjustment method of the adjustment block ends. If the film thickness does not meet the standard, perform S3 and S4 again until it meets the standard.
[0012] Beneficial effects: The uniformity of film thickness is coordinated by controlling the flow rate of process gas. The adjustment block has multiple configurations. Different openings can be selected according to the opening rate, making the adjustment range wider and achieving better results. After adding adjustments to the hardware, the machine can be compatible with more working conditions, because the effects of a specific spray plate are different under different process formulas and different gas flow rates. Therefore, adding adjustable functions can make the machine better adapt to a variety of processes and help improve film uniformity. There are many adjustment blocks. If they are processed separately, the processing accuracy and assembly accuracy need to be controlled. The present invention embeds the adjustment block in the setting seat, and can be formed in one step by water jet cutting, laser cutting, wire cutting and other processing methods. There is no need to consider the direct tolerance of the mating parts, and the processing method has no waste, which is more efficient and low cost. A lower diffuser and an upper diffuser are arranged on the back plate and the spray plate. The double-layer diffuser is helpful for gas diffusion, so that the gas distribution is more uniform. At the same time, an adjustment block can be arranged between the two diffusers to selectively control the flow rate of a part of the area, and the heat taken away can be indirectly controlled by changing the flow rate of the process gas to adjust the uniformity of the film thickness. The present invention innovatively proposes a new idea of adjusting the local film thickness value by changing the local process gas flow rate, so that the global film thickness tends to be equal. The installation positioning method between the setting seat and the adjustment block utilizes the surrounding surfaces for positioning, which effectively reduces the size in the thickness direction. On the other hand, it is helpful for processing. The setting seat and the adjustment block can be processed as a whole at one time without setting a high matching accuracy, reducing the difficulty of processing. BRIEF DESCRIPTION OF THE DRAWINGS
[0013] Figure 1 The embodiment is a schematic cross-sectional view of the overall structure of the present application; Figure 2The embodiment is a schematic cross-sectional structure diagram for illustrating the local details of the present invention; Figure 3 This is a schematic diagram of the structure of the diffuser used to illustrate the embodiment; Figure 4 It is a partial structural schematic diagram of an embodiment for showing the setting seat and the adjusting block; Figure 5 The embodiment is a schematic diagram of the structure of the setting seat and the corresponding adjustment block for showing different shape schemes; Figure 6 This is a schematic diagram of an embodiment for showing that a vacant position adjustment seat shields a fine through hole; Figure 7 The embodiment is used to show the shapes of different schemes of the adjustment block and the schematic diagram of the pore structure of the corresponding shielding area; Figure 8 It is a schematic diagram of the method flow of the present invention.
[0014] Figure numerals: 1. back plate; 2. spray plate; 3. lower diffuser; 31. second groove; 32. flange; 33. threaded hole; 34. countersunk hole 2; 35. positioning column; 36. second fine through hole; 4. upper diffuser; 41. groove; 42. mounting portion; 43. screw hole; 44. countersunk hole 1; 45. boss; 46. first fine through hole; 5. adjustment block; 6. setting seat; 61. vacancy; 62. positioning hole; 611. shielding area; 612. opening area; 7. reaction chamber; 8. heating plate; 100. first diffusion chamber; 200. second diffusion chamber; 300. third diffusion chamber; 400. process reaction chamber. DETAILED DESCRIPTION
[0015] The following is only a preferred embodiment of the present invention, and the protection scope is not limited to this embodiment. All technical solutions under the concept of the present invention should belong to the protection scope of the present invention. At the same time, it should be pointed out that for ordinary technicians in this technical field, some improvements and modifications without departing from the principle of the present invention should also be regarded as the protection scope of the present invention.
[0016] like Figure 1As shown, a spray plate device with adjustable flow rate includes a back plate 1, a spray plate 2, a lower diffuser 3, an upper diffuser 4, an adjustment block 5 and a setting seat 6; the spray plate 2 is fixedly arranged on the back plate 1, and the lower diffuser 3 and the upper diffuser 4 are arranged between the back plate 1 and the spray plate 2, the upper diffuser 4 is installed above the lower diffuser 3, the lower diffuser 3 is fixed on the back plate 1, and the setting seat 6 is located in the middle of the back plate 1 and the spray plate 2, and the setting seat 6 is arranged on the lower diffuser 3 by positioning, and a plurality of vacancies are opened on the setting seat 6, and the vacancies are used to accommodate and position the adjustment block 5, and the adjustment block 5 is provided with multiple blocks, and the adjustment block 5 is opened with through holes of different specifications for controlling and adjusting the amount of gas flowing between the lower diffuser 3 and the upper diffuser 4, and the adjustment block 5 can be selectively placed on the setting seat 6, and the outer contour of the adjustment block 5 matches the inner contour of the vacancy on the setting seat 6; the height of the adjustment block 5 and the setting seat 6 are consistent.
[0017] like Figure 2 As shown, an air inlet is opened in the middle of the back plate 1, and the upper end of the back plate 1 is connected to the process gas inlet pipeline. The process gas flows down from the middle of the back plate 1 from top to bottom. A first diffusion chamber 100 is formed between the upper diffuser 4 and the back plate 1, a second diffusion chamber 200 is formed between the upper diffuser 4 and the lower diffuser 3, and a third diffusion chamber 300 is formed between the lower diffuser 3 and the spray plate 2. Along the transmission path of the process gas, the process gas enters the first diffusion chamber 100 in sequence, and then enters the second diffusion chamber 200 after passing through the upper diffuser 4. The gas volume is adjusted by setting an adjustment block 5 in the second diffusion chamber 200, and then enters the third diffusion chamber 300 through the lower diffuser 3, further diffuses, and finally enters the process reaction chamber 400 through the flow channel on the spray plate 2 to react with the wafer.
[0018] The back plate 1 is provided with a flow channel, which is connected to an external cooling device. A heat exchange fluid flows in the flow channel, and the temperature of the heat exchange fluid can be adjusted between 15-75°C, thereby regulating the temperature of the back plate 1, so that the process gas cannot perform unnecessary film deposition on the components on the spray plate device, thereby extending the maintenance cycle.
[0019] A closed reaction space is formed between the back plate 1, the spray plate 2 and the reaction chamber 7. A heating plate 8 that can be raised and lowered is provided on the reaction chamber 7. The heating plate 8 is located directly below the spray plate 2 and is used to carry and heat the wafer.
[0020] like Figure 3As shown, a sink 41 is provided in the middle of the upper end surface of the upper diffuser 4, and the edge is a raised mounting portion 42. The entire surface of the sink 41 is provided with a first fine through hole 46 for allowing the process gas to flow down. The upper end of the mounting portion 42 is in contact with the back plate 1, and screw through holes 43 and countersunk holes 44 are evenly distributed on the mounting portion 42. The countersunk holes of the countersunk holes 44 are on the upper end surface for placing the ends of the screws. Several bosses 45 are provided on the sink 41. The height of the bosses 45 is consistent with the height of the mounting portion 42, and a screw through hole is provided in the center of the bosses 45.
[0021] A second countersunk groove 31 is provided in the middle of the lower diffuser 3, and the outer periphery of the lower diffuser 3 is a flange 32. A threaded hole 33 and a second countersunk hole 34 are provided on the flange 32. The threaded hole 33 corresponds to the position of the first countersunk hole 44, the second countersunk hole 34 corresponds to the screw through hole 43, and the countersunk end of the second countersunk hole 34 is at the lower end surface. A second fine through hole 36 is opened on the disk surface of the second countersunk groove 31. A positioning column 35 is also provided on the second countersunk groove 31, and a countersunk hole is opened on the positioning column 35.
[0022] When the upper diffuser 4 and the lower diffuser 3 are installed, a first screw is arranged in the countersunk hole 1 44, and the threaded part of the first screw is connected with the threaded hole 33, so that the upper diffuser 4 and the lower diffuser 3 are fixedly connected. A second screw is arranged in the countersunk hole 2 34 of the lower diffuser 3, and the threaded part of the second screw is connected with the back plate 1 after passing through the screw through hole 43, and a second screw is arranged in the countersunk hole on the positioning column 35, and the second screw is connected with the back plate 1 after passing through the screw through hole of the boss 45. The lower diffuser 3 adopts the peripheral fixing and middle fixing methods. Since the thickness of the upper diffuser 4 and the lower diffuser 3 is relatively thin, it is easy to deform and the problem of uneven fitting occurs. This fixing method helps to make the upper diffuser 4 and the lower diffuser 3 firmly connected, so that the height of the second diffusion chamber 200 is consistent, and there is no gap between the upper and lower adjustment blocks, which is convenient for accurate control of the airflow. The first screw and the second screw are both central hole screws, which is conducive to evacuating the vacuum chamber.
[0023] like Figure 4 As shown, the setting seat 6 is in the shape of a connecting rib, the width of the connecting rib is set to be narrow, the position of the connecting rib is placed away from the position of the first fine through hole 46 and the second fine through hole 36 on the lower diffuser 3 and the upper diffuser 4, a plurality of vacancies 61 are provided on the setting seat 6, and the adjustment block 5 can be placed inside the vacancies 61, the height of the setting seat 6 is consistent with the height of the second diffusion chamber 200, the setting seat 6 is arranged in the second diffusion chamber 200, and a positioning hole 62 is opened on the setting seat 6, and the positioning hole matches the positioning column 35 of the lower diffuser 3, so that the setting seat 6 is placed in the lower diffuser 3 and is fixed in position and will not move.
[0024] like Figure 5 As shown, the shape of the seat 6 can be a matrix type a1, a radial type a2, or a regular hexagonal type a3.
[0025] like Figure 6 As shown, an adjustment block 5 is placed in each vacancy 61 on the seat 6, and a through hole is opened in the middle of the adjustment block 5. The area corresponding to the through hole is the opening area 612, and the solid area on the side of the adjustment block 5 is the shielding area 611. The ratio of the area of the opening area 612 to the outer contour area of the entire adjustment block 5 is the opening rate. From the top view, the shielding area 611 shields part of the first fine through hole 46 and the second fine through hole 36, and the process gas can only flow down from the opening area 612 in the middle. The process gas enters the opening area 612 from the first fine through hole 46 and then flows out from the second fine through hole 36. The positions of the first fine through hole 46 and the second fine through hole 36 are staggered, and the gas cannot flow down directly, which is conducive to gas diffusion and mixing.
[0026] The outer contour of the regulating block 5 matches the shape of the vacancy 61. A through hole is provided inside the regulating block 5. The area of the through hole can be processed and customized according to the requirements. The opening rate of the through hole can be selected between 0% and 100%. When 100%, the ventilation volume is the largest, and the regulating block 5 is not installed at this time. Using 0% of the regulating block 5 will block the vacancy 61 in the area and prevent the process gas from flowing down. Figure 7 As shown, the shape of the corresponding adjustment block 5 can be a rectangle b1, a sector b2 and a hexagon b3.
[0027] A film thickness control method with adjustable flow rate: S1 benchmark establishment: remove all the adjustment blocks 5 in the spray plate device, install the setting seat 6, and then the lower diffuser 3 and the upper diffuser 4 are completely connected without any obstruction. Then, the process gas is introduced under this working condition to run the recipe and obtain the film thickness data of the silicon wafer. At this time, the thinner or thicker film thickness areas are marked, and the positions of the thinner or thicker areas are mapped to the positions of the lower diffuser 3; S2 Adjustment block installation: open the spray plate 2 and the lower diffuser 3, and set the adjustment block 5 on the area of the lower diffuser 3 corresponding to the thinner or thicker film thickness area. The opening rate of the adjustment block 5 is 50% for the first time, and all the areas with thinner film thickness are placed on the adjustment block 5; S3: re-run the original recipe: re-run the original thin film process recipe to obtain the correlation data between the relevant film thickness and the opening rate of the adjustment block 5; S4: Accurately adjust the opening rate of the adjustment block: Based on the correlation data between the film thickness and the opening rate of the adjustment block 5 obtained in the previous round, adjust the opening rate of the adjustment block 5 corresponding to the area with thinner or thicker film thickness to an optimal value, and then run the process recipe to obtain the film thickness data. If the film thickness data meets the requirements, the adjustment method of the adjustment block ends. If the film thickness does not meet the standard, perform S3 and S4 again until it meets the standard.
Claims
1. A spray plate device with adjustable flow rate, comprising a back plate (1), a spray plate (2), a lower diffuser (3), an upper diffuser (4), an adjustment block (5) and a setting seat (6), characterized in that: The spray plate (2) is fixedly arranged on the back plate (1); a lower diffuser (3) and an upper diffuser (4) are installed between the back plate (1) and the spray plate (2); the upper diffuser (4) is installed above the lower diffuser (3); the lower diffuser (3) is fixed on the back plate (1); the setting seat (6) is located between the back plate (1) and the spray plate (2); the setting seat (6) is installed on the lower diffuser (3); a plurality of vacancies (61) are opened on the setting seat (6); the vacancies (61) are used to accommodate and position the adjustment block (5); the adjustment block (5) is arranged on the back plate (1) and the upper diffuser (4) is installed on the lower diffuser (3 ... A plurality of nodes (5) are provided, a plurality of through holes of different sizes are provided on the adjusting block (5), the outer contour of the adjusting block (5) matches the inner contour of the vacancy (61) on the setting seat (6), the adjusting block (5) and the setting seat (6) are of the same height, a reaction chamber (7) is also installed on the spray plate (2), a closed reaction space is formed between the back plate (1), the spray plate (2) and the reaction chamber (7), a heating plate (8) which can be raised and lowered is provided on the reaction chamber (7), and the heating plate (8) is located directly below the spray plate (2).
2. The flow-adjustable spray plate device according to claim 1, characterized in that: An air inlet is provided in the middle of the back plate (1); a process gas inlet pipeline is connected to the upper end of the back plate (1); a first diffusion chamber (100) is formed between the upper diffuser (4) and the back plate (1); a second diffusion chamber (200) is formed between the upper diffuser (4) and the lower diffuser (3); and a third diffusion chamber (300) is formed between the lower diffuser (3) and the spray plate (2).
3. The flow-adjustable spray plate device according to claim 2, characterized in that: The back plate (1) is also provided with a flow channel, the flow channel is connected to an external cooling device, a heat exchange fluid flows in the flow channel, and the temperature of the heat exchange fluid can be adjusted between 15-75°C.
4. The flow-adjustable spray plate device according to claim 1, characterized in that: A recessed groove (41) is provided in the middle of the upper end surface of the upper diffuser (4); the edge of the upper diffuser (4) is a raised mounting portion (42); a first fine through hole (46) is provided on the entire surface of the recessed groove (41); the upper end of the mounting portion (42) is in contact with the back plate (1); screw through holes (43) and countersunk holes (44) are evenly distributed on the mounting portion (42); a plurality of bosses (45) are provided on the recessed groove (41); the height of the bosses (45) is consistent with the height of the mounting portion (42); and the bosses (46) are provided on the entire surface of the recessed groove (41); and the first fine through hole (46) is ... 5) A screw through hole is arranged at the center. A second sink groove (31) is arranged in the middle of the lower diffuser (3). The outer periphery of the lower diffuser (3) is a flange (32). A threaded hole (33) and a second countersunk hole (34) are arranged on the flange (32). The threaded hole (33) corresponds to the position of the first countersunk hole (44). The second countersunk hole (34) corresponds to the screw through hole (43). A second fine through hole (36) is opened on the disk surface of the second sink groove (31). A positioning column (35) is also arranged on the second sink groove (31).
5. The flow-adjustable spray plate device according to claim 1, characterized in that: The setting seat (6) is a connecting rib-like structure, the width of the connecting rib is set to be narrow, a plurality of vacancies (61) are set on the setting seat (6), and the adjustment block (5) can be placed inside the vacancies (61). The height of the setting seat (6) is consistent with the height of the second diffusion chamber (200). The setting seat (6) is set in the second diffusion chamber (200). A positioning hole (62) is opened on the setting seat (6), and the positioning hole (62) matches the positioning column (35) of the lower diffuser (3). The shape of the setting seat (6) can be a matrix type, a radial type, or a regular hexagonal form.
6. The flow-adjustable spray plate device according to claim 5, characterized in that: A through hole is opened in the middle of the adjustment block (5), the area corresponding to the through hole is the opening area (612), the solid area on the edge of the adjustment block (5) is the shielding area (611), the outer contour of the adjustment block (5) matches the shape of the vacancy (61), a through hole is arranged inside the adjustment block (5), and the shape of the adjustment block (5) can be rectangular, sector-shaped or hexagonal.
7. A method for controlling film thickness with adjustable flow rate, which is used to control the spray disk device according to any one of claims 1 to 6, characterized in that: S1 benchmark establishment: remove all adjustment blocks (5) in the spray plate device, install the setting seat (6), at this time, the lower diffuser (3) and the upper diffuser (4) are completely connected without obstruction, and then the process gas is introduced under this working condition to run the recipe to obtain the film thickness data of the silicon wafer. At this time, the thinner or thicker film thickness area is marked, and the position of the thinner or thicker area is mapped to the position of the lower diffuser (3); S2. Installation of the adjustment block: Open the spray plate (2) and the lower diffuser (3), and set the adjustment block (5) on the area of the lower diffuser (3) corresponding to the thinner or thicker film thickness area. The opening rate of the adjustment block (5) is 50% for the first time, and all the areas with thinner film thickness are placed on the adjustment block (5); S3: re-run the original recipe: re-run the original thin film process recipe to obtain the correlation data between the relevant film thickness and the opening rate of the adjustment block (5); S4: Precisely readjust the opening rate of the adjustment block: Based on the correlation data between the film thickness and the opening rate of the adjustment block (5) obtained in the previous round, the opening rate of the adjustment block (5) corresponding to the area with thinner or thicker film thickness is adjusted to an optimal value, and then the process recipe is run to obtain the film thickness data. If the film thickness data meets the requirements, the adjustment method of the adjustment block is terminated. If the film thickness does not meet the requirements, S3 and S4 are performed again until the requirements are met.
Citation Information
Patent Citations
Substrate-processing apparatus and substrate-processing method for selectively inserting diffusion plates
CN102473610A
Two-gas isolate type central uniform gas dividing and spraying device
CN104178749A
Shower head of a wafer treatment apparatus having a gap controller
CN1781608A
Atomic layer deposition chamber capable of preventing parasitic plasma, and atomic layer deposition apparatus using of it
KR101724917B1
Cascade design showerhead for transient uniformity
US20140299681A1
Cited By
Back temperature control device and temperature control method of thin film equipment heating base
CN120210785A