Method and device for representing corrosion state of alloy material

Through LIBS technology, the elemental component analysis of the alloy material corrosion layer was solved, and the problem of surface element detection of alloy material corrosion layer was achieved, in-situ rapid and non-destructive characterization was achieved, damage and cost were reduced, and real-time full-element analysis capabilities were provided.

CN119044152APending Publication Date: 2024-11-29ADVANCED ENERGY SCIENCE & TECHNOLOGY GUANGDONG LABORATORY +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411144981.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-20
Publication Date
2024-11-29

AI Technical Summary

Technical Problem

The prior art cannot effectively detect the types and content of elements on the surface of the corrosive layer of alloy materials. Especially in high-risk, high radiation or high temperature environments, traditional offline characterization methods have stability and safety challenges and are economically cost-effective.

Method used

Using laser induced breakdown spectroscopy (LIBS), the corrosion layer of alloy material is ablated by a single pulse, the LIBS spectrum is recorded, the intensity information of the characteristic spectrum line is selected, and the LIBS signal characteristics are constructed to achieve in-situ, rapid and corrosion state of the alloy material. Nearly non-destructive characterization.

Benefits of technology

It realizes in-situ, rapid and near-destructive characterization of the corrosion state of alloy materials, reduces the degree of damage, avoids the sample preparation process, has real-time full-element analysis capabilities, and has huge application potential.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119044152A_ABST
    Figure CN119044152A_ABST
Patent Text Reader

Abstract

The embodiment of the invention relates to the technical field of analysis and detection, in particular to an alloy material corrosion state characterization method and device, the laser-induced breakdown spectroscopy technology, namely the LIBS technology, is adopted, element composition analysis is conducted on the surface of a corroded alloy material through the LIBS technology, and particularly, element composition analysis is conducted on the surface of the corroded alloy material through the laser-induced breakdown spectroscopy technology. The method comprises the following steps: ablating a to-be-measured area on the surface of a corrosion layer of an alloy material by using a single laser pulse, measuring an LIBS spectrum generated in the to-be-measured area, quickly obtaining element types and content information of the surface of the corrosion layer in situ in a near-lossless manner through spectral analysis, and finally realizing in-situ, quick and near-lossless characterization of the corrosion state of the alloy material. Compared with the traditional corrosion characterization technology, the method has the advantages of low damage degree, in-situ measurement, no need of sample preparation, real-time all-element analysis, pure optical element linkage and the like, so that the method has huge application potential in the aspect of near-lossless characterization of the surface corrosion state of the corrosion layer of the alloy material.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The embodiments of the present invention relate to the technical field of analysis and detection, and specifically to a method and device for characterizing the corrosion state of an alloy material. Background Art

[0002] Alloy material corrosion refers to the process in which alloy materials react physically, chemically or electrochemically with the surrounding medium in a natural environment or a specific working medium, causing the material performance to decay. The corrosion of alloy materials is one of the key factors affecting the life and performance of industrial equipment, building structures and transportation systems. A typical example of alloy material corrosion: during the operation of a lead-cooled fast reactor, lead-based liquid metal (such as pure lead, lead-bismuth alloy, lead-magnesium alloy, etc.) is in a high temperature state and has a strong corrosiveness to the alloy component materials in contact with it, which is bound to affect the service life of the component materials. The corrosion of lead-based liquid metal mainly has the following two processes: 1. When the oxygen content in the lead-based liquid metal is low, dissolution corrosion is the main corrosion process, which is achieved through the mutual diffusion and mass transfer of elements between the liquid metal and the material; 2. When the oxygen content in the lead-based liquid metal is high, in addition to the dissolution corrosion caused by the mutual diffusion and mass transfer of elements between the liquid metal and the material, the surface of the alloy material will also undergo an oxidation corrosion process, which is manifested as the formation of a complex oxidation corrosion layer on the surface of the original alloy material. In both basic research and application fields involving alloy material corrosion, such as lead-based liquid metal corrosion, the problem of characterizing the surface corrosion state of the alloy material corrosion layer needs to be solved.

[0003] It is well known that the element composition on the surface of the corrosion layer and the content characteristics of the constituent elements are one of the important data for characterizing the corrosion state of the material. For example, during the operation of a lead-cooled fast reactor, the elements in the original alloy material will diffuse from the inside to the outside along the corrosion channel during the corrosion process. When there is oxidative corrosion but the corrosion state is more serious, the content of the elements that diffuse outward will usually be enriched at the solid-liquid interface. In this case, the degree of enrichment of the elements of the original alloy material on the surface of the oxidative corrosion layer can be used as an important indicator for characterizing the corrosion state. Therefore, it is very important to detect the type and content of elements on the surface of the material corrosion layer. In addition, the characterization of the corrosion state often needs to be carried out in harsh environments such as high risk, high radiation or high temperature, and the offline characterization method in the laboratory after sampling not only brings challenges to the stability and safety of industrial operations, but also adds an additional economic burden. Summary of the invention

[0004] In view of the above problems, an example of the present invention provides a method and device for characterizing the corrosion state of an alloy material, which is used to solve the problem in the prior art that the type and content of elements on the surface of the corrosion layer of the material cannot be detected.

[0005] According to one aspect of an example of the present invention, a method for characterizing the corrosion state of an alloy material is provided, the method comprising: Performing single pulse ablation on a certain area to be tested of the corrosion layer of the alloy material by using a LIBS device, and recording the LIBS spectrum of the area to be tested; According to the LIBS spectrum, the characteristic spectral line of the element to be measured is selected, and the intensity information of the characteristic spectral line is extracted; A LIBS signal feature characterizing the corrosion state of the material is constructed according to the intensity information of the element to be measured, and the corrosion state of the alloy material is characterized according to the LIBS signal feature.

[0006] In some optional embodiments, performing single pulse ablation on a certain area to be tested of the corrosion layer of the alloy material by using a LIBS device and recording the LIBS spectrum of the area to be tested specifically includes: The pulsed laser of the LIBS device generates plasma on the surface of the material corrosion layer after the laser passes through the focusing lens; The light signal emitted by the plasma enters the collection lens, is introduced into the spectrometer through the optical fiber, and is converted into a digital signal after passing through the spectrometer and collected by the computer to obtain the LIBS spectrum.

[0007] In some optional embodiments, the number of the regions to be tested is n, the positions of the n regions to be tested in the corrosion layer of the alloy material are all different, and the LIBS spectrum of each region to be tested is recorded as S1, S2, S3, ..., S n .

[0008] In some optional embodiments, selecting characteristic spectral lines of the element to be measured according to the LIBS spectrum and extracting intensity information of the characteristic spectral lines specifically includes: The characteristic spectral line of the element to be measured is selected as the analysis line, the integral area of ​​the characteristic spectral line is calculated as the integral intensity of the analysis line, and the integral intensities obtained from n spectral data are averaged, and the average integral intensity is used as the intensity information of the characteristic spectral line.

[0009] In some optional embodiments, constructing the LIBS signal feature characterizing the corrosion state of the material according to the intensity information of the element to be measured specifically includes: Obtain the intensity information of the elements to be tested at different corrosion times; According to the positive correlation between the intensity information and the concentration of the element to be measured under the local thermal equilibrium condition of plasma, the LIBS signal characteristics of the corrosion layer of the alloy material are constructed with the intensity information.

[0010] In some optional embodiments, the enrichment degree of the element to be measured on the surface of the corrosion layer of the alloy material shows a monotonically increasing trend with the extension of corrosion time, indicating that the corrosion degree of the alloy material shows a gradually increasing trend with the extension of corrosion time.

[0011] In some optional embodiments, the element to be detected is chromium.

[0012] In some optional embodiments, the alloy material is SIMP steel material.

[0013] In some optional embodiments, the alloy material corrosion layer includes an inner corrosion layer and an outer corrosion layer, the inner corrosion layer includes a spinel layer, and the outer corrosion layer includes magnetite.

[0014] According to another aspect of an embodiment of the present invention, there is provided a device for characterizing the corrosion state of an alloy material, the device comprising: A LIBS spectrum acquisition module is used to perform single-pulse ablation on a certain area to be tested of the corrosion layer of the alloy material through a LIBS device, and record the LIBS spectrum of the area to be tested; The intensity calculation module of the element to be measured is used to select the characteristic spectral line of the element to be measured according to the LIBS spectrum and extract the intensity information of the characteristic spectral line; And a characterization module is used to construct a LIBS signal feature characterizing the corrosion state of the material according to the intensity information of the element to be measured, and characterize the corrosion layer state of the alloy material according to the LIBS signal feature.

[0015] The present invention provides a method and device for characterizing the corrosion state of alloy materials, and its beneficial effects are as follows: the present invention adopts laser induced breakdown spectroscopy technology, namely LIBS technology, and performs elemental composition analysis on the surface of the alloy material that is subject to corrosion through LIBS technology. Specifically, a single laser pulse is used to ablate the area to be tested on the surface of the corrosion layer of the alloy material, and the LIBS spectrum generated by the area to be tested is measured. Through spectral analysis, the type of elements and their content information on the surface of the corrosion layer can be obtained in situ, quickly, and nearly non-destructively, and finally the in situ, rapid, and nearly non-destructive characterization of the corrosion state of the alloy material is achieved. Compared with traditional corrosion characterization technology, the present invention has the advantages of low damage, in-situ measurement, no sample preparation, real-time full element analysis, and pure optical element connection. Therefore, it has great application potential in the nearly non-destructive characterization of the corrosion state of the corrosion layer surface of alloy materials.

[0016] The above description is only an overview of the technical solution of the example of the present invention. In order to more clearly understand the technical means of the embodiment of the present invention, it can be implemented in accordance with the contents of the specification. In order to make the above and other purposes, features and advantages of the example of the present invention more obvious and easy to understand, the specific implementation methods of the present invention are specifically listed below. BRIEF DESCRIPTION OF THE DRAWINGS

[0017] The accompanying drawings are only used to illustrate the embodiments and are not to be considered as limiting the present invention. In addition, the same reference symbols are used to represent the same components throughout the accompanying drawings. In the accompanying drawings: Figure 1 A schematic flow chart of a first embodiment of a method for characterizing the corrosion state of an alloy material according to Embodiment 1 of the present invention is shown; Figure 2 A schematic diagram showing the results of the spectral line intensity of the Cr I 425.4 nm analysis line obtained by LIBS measurement and analysis of the SIMP steel corrosion layer corroded for 700, 1000, 4000 and 6000 hours respectively in a static LBE environment provided by the present invention; Figure 3 The schematic diagram of the structure of the device for characterizing the corrosion state of alloy materials provided in Example 3 of the present invention is shown. DETAILED DESCRIPTION

[0018] Exemplary embodiments of the present invention will be described in more detail below with reference to the accompanying drawings. Although exemplary embodiments of the present invention are shown in the drawings, it should be understood that the present invention can be implemented in various forms and should not be limited to the embodiments set forth herein.

[0019] Embodiment 1: Figure 1 The first embodiment of the method for characterizing the corrosion state of alloy materials of the present invention is shown, and the method comprises: 110, ablating the area to be tested of the corrosion layer of the alloy material by a LIBS device, and recording the LIBS spectrum of the area to be tested; in step 110, a single pulse ablation is performed on the area to be tested of the corrosion layer of the alloy material by a LIBS device, and the LIBS spectrum of the area to be tested is recorded, specifically including: using the pulsed laser of the LIBS device, the laser after passing through the focusing lens and the surface of the material corrosion layer to generate plasma; the light signal emitted by the plasma enters the collection lens, is introduced into the spectrometer through the optical fiber, and is converted into a digital signal after passing through the spectrometer and collected by the computer to obtain the LIBS spectrum. The area to be tested can be any area on the surface of the corrosion layer of the alloy material, and its shape and size are not limited. The scheme of selecting the area to be tested in the corrosion layer of the alloy material falls within the protection scope of this application.

[0020] 120. According to the LIBS spectrum, the characteristic spectral line of the element to be measured is selected, and the intensity information of the characteristic spectral line is extracted. In step 120, according to the LIBS spectrum, the characteristic spectral line of the element to be measured is selected, and the intensity information of the characteristic spectral line is extracted, which specifically includes: selecting the characteristic spectral line of the element to be measured as the analysis line, calculating the integral area of ​​the characteristic spectral line as the integral intensity of the analysis line, and averaging the integral intensities obtained from n spectral data, and taking the average integral intensity as the intensity information of the characteristic spectral line.

[0021] 130, constructing a LIBS signal feature characterizing the corrosion state of the material according to the intensity information of the element to be measured, and characterizing the corrosion state of the alloy material according to the LIBS signal feature. In step 130, constructing a LIBS signal feature characterizing the corrosion state of the material according to the intensity information of the element to be measured, specifically includes: obtaining the intensity information of the element to be measured at different corrosion times; according to the positive correlation between the intensity information and the concentration of the element to be measured under the local thermal equilibrium condition of the plasma, constructing the LIBS signal feature of the corrosion layer of the alloy material according to the intensity information.

[0022] The present invention adopts laser induced breakdown spectroscopy technology, namely LIBS technology, and uses LIBS technology to perform elemental composition analysis on the surface of the alloy material that has been corroded. Specifically, a single laser pulse is used to ablate the area to be tested on the surface of the corrosion layer of the alloy material, and the LIBS spectrum generated by the area to be tested is measured. Through spectral analysis, the type of elements and their content information on the surface of the corrosion layer can be obtained in situ, quickly, and nearly non-destructively, and finally the in situ, rapid, and nearly non-destructive characterization of the corrosion state of the alloy material is achieved. Compared with traditional corrosion characterization technology, the present invention has the advantages of low damage, in-situ measurement, no sample preparation, real-time full element analysis, and pure optical element connection. Therefore, it has great application potential in the nearly non-destructive characterization of the corrosion state of the corrosion layer surface of the alloy material.

[0023] Embodiment 2: This embodiment provides a second embodiment of the method for characterizing the corrosion state of an alloy material of the present invention. This embodiment is based on and further defines the first embodiment, and specifically includes: In some optional embodiments, the area to be tested of the corrosion layer of the alloy material is ablated by a LIBS device, and the LIBS spectrum of the area to be tested is recorded, including: the pulsed laser of the LIBS device generates plasma with the surface of the corrosion layer of the material after passing through a focusing lens; the light signal emitted by the plasma enters the collection lens, is introduced into the spectrometer through an optical fiber, and is converted into a digital signal after passing through the spectrometer and is collected by a computer to obtain a LIBS spectrum. With a pulsed laser as the excitation source, the laser after passing through a focusing lens interacts with the surface of the corrosion layer of the material to generate plasma; the light signal emitted by the plasma enters the collection lens, is introduced into the spectrometer through an optical fiber, and is converted into a digital signal after passing through the spectrometer and is collected by a computer to obtain a corresponding LIBS spectrum.

[0024] The number of the tested regions is n, the positions of the n tested regions in the corrosion layer of the alloy material are all different, and the LIBS spectra of each tested region are recorded as S1, S2, S3, ..., S nIn a specific embodiment, the LIBS device is adjusted to make the ablation depth of each laser pulse uniform, and the outgoing laser is focused on the surface of the SIMP steel corrosion material after being expanded by a beam expander. Any one of the four sample samples is selected for LIBS measurement, and a single laser pulse is ablated at 90 different positions on the surface of the corrosion layer, and the LIBS spectrum data corresponding to each position is measured, which is recorded as S1, S2, S3...S 90 .

[0025] In some optional embodiments, according to the LIBS spectrum, the characteristic spectrum line of the element to be measured is selected, and the intensity information of the characteristic spectrum line is extracted, which specifically includes: selecting the characteristic spectrum line of the element to be measured as the analysis line, calculating the integral area of ​​the characteristic spectrum line as the integral intensity of the analysis line, and averaging the integral intensity obtained from n spectral data, and using the average integral intensity as the intensity information of the characteristic spectrum line. In a specific embodiment, for the spectral data of step 110, the characteristic spectrum line of Cr I 429.0 nm can be selected as the analysis line, the integral area of ​​the characteristic spectrum line is calculated as the integral intensity of the analysis line, and the integral intensity of the Cr I 429.0 nm spectrum line obtained from 90 spectral data is averaged, and the average integral intensity is used as the spectrum line intensity of the Cr I 429.0 nm analysis line.

[0026] In some optional embodiments, the LIBS signal characteristics characterizing the corrosion state of the material are constructed based on the intensity information of the element to be measured, specifically including: obtaining the intensity information of the element to be measured at different corrosion times; based on the positive correlation between the intensity information and the concentration of the element to be measured under local thermal equilibrium conditions of the plasma, the LIBS signal characteristics of the corrosion layer of the alloy material are constructed with the intensity information. The enrichment degree of the element to be measured on the surface of the corrosion layer of the alloy material shows a monotonically increasing trend with the extension of corrosion time, which indicates that the corrosion degree of the alloy material tends to gradually increase with the extension of corrosion time. In a specific example, steps 110 and 120 are repeated to obtain the spectral line intensity of the Cr element on the surface of the corrosion layer at different corrosion times, and the results are as follows. Figure 2 As shown. According to the positive correlation between the intensity of the analytical line and the element concentration under the local thermal equilibrium condition of the plasma, the intensity value of the Cr I 425.4 nm analytical line represents the enrichment of the Cr element on the surface of the corrosion layer to a certain extent. Therefore, the intensity of the Cr element spectrum can be constructed as a LIBS signal feature representing the enrichment degree of the raw material element on the surface of the corrosion layer. Figure 2 It can be seen that under the corrosion conditions of this case, the enrichment degree of Cr element on the surface of the corrosion layer shows a monotonically increasing trend with the extension of corrosion time, which can indicate that the corrosion degree of the material tends to gradually increase with the extension of corrosion time.

[0027] Embodiment 3: Figure 3 The first embodiment of the alloy material corrosion state characterization device of the present invention is shown. This embodiment is based on embodiments 1 and 2. The alloy material corrosion state characterization device 300 of this embodiment specifically includes: LIBS spectrum acquisition module 310, used in step 110 of embodiment 1; The measured element intensity calculation module 320 is used in step 120 of embodiment 1; And a characterization module 330, used in step 130 of Example 1.

[0028] In a specific embodiment, four SIMP steel corrosion samples corroded for 700, 1000, 4000 and 6000 hours respectively in a static liquid lead-bismuth eutectic (LBE) environment at 450°C and a dissolved oxygen concentration of about 3.0×10^(-4)wt% are selected as example samples for constructing the present method.

[0029] After the SIMP steel undergoes dissolution and oxidation corrosion under the above conditions, an oxidation corrosion layer with a double-layer structure will be formed on the surface of the material: the outer corrosion layer is mainly composed of magnetite (Fe3O4) produced by the diffusion and oxidation of Fe atoms on the original surface, and the inner corrosion layer is a spinel layer [(Fe, Cr)3O4] formed by the reaction of oxygen invading the original surface with Cr and Fe. The following is a LIBS signal feature that can be used to characterize the corrosion state of the material corrosion layer surface in the form of an embodiment.

[0030] The steps to construct a LIBS signal feature that can represent the enrichment of elements in the raw material on the surface of the corrosion layer are as follows: Step 1: Adjust the LIBS equipment. To make the ablation depth of each laser pulse uniform, the outgoing laser is expanded by a beam expander and focused on the surface of SIMP steel corrosion material. Select any one of the four sample samples for LIBS measurement, perform single laser pulse ablation on 90 different positions on the corrosion layer surface, and measure the LIBS spectrum data corresponding to each position, recorded as S1, S2, S3...S 90 .

[0031] Step 2: For the spectral data in step 1, select the characteristic spectral line Cr I 429.0 nm as the analysis line, calculate the integral area of ​​the characteristic spectral line as the integral intensity of the analysis line, and average the integral intensities of the Cr I 429.0 nm spectral line obtained from 90 spectral data, and use the average integral intensity as the spectral line intensity of the Cr I 429.0 nm analysis line.

[0032] Step 3: Repeat steps 1 and 2 for the other 3 sample samples to obtain the spectral line intensity of Cr element on the corrosion layer surface at different corrosion times. The results are as follows: Figure 2As shown. According to the positive correlation between the intensity of the analytical line and the element concentration under the local thermal equilibrium condition of the plasma, the intensity value of the Cr I 425.4 nm analytical line represents the enrichment of the Cr element on the surface of the corrosion layer to a certain extent. Therefore, the intensity of the Cr element spectrum can be constructed as a LIBS signal feature representing the enrichment degree of the raw material element on the surface of the corrosion layer. Figure 2 It can be seen that under the corrosion conditions of this case, the enrichment degree of Cr element on the surface of the corrosion layer shows a monotonically increasing trend with the extension of corrosion time, which can indicate that the corrosion degree of the material tends to gradually increase with the extension of corrosion time.

[0033] Combining the above steps, the surface of the corrosion layer of the alloy material was measured based on the LIBS technology to obtain the spectral line intensity of the Cr element to be measured. By constructing the LIBS signal characteristics of the Cr element enrichment degree that can characterize the corrosion state of the alloy material, the corrosion state of SIMP steel at different corrosion times in a static LBE environment was finally characterized.

[0034] The above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit them; it should be emphasized that any indicator characterizing the corrosion state of the corrosion layer surface derived from the LIBS spectrum data of the corrosion layer surface should be included in the protection scope of the patent. Although the present invention has been described in detail with reference to the above embodiments, a person of ordinary skill in the art should understand that the technical solutions described in the above embodiments can still be modified, or some of the technical features can be replaced by equivalents; and these modifications or replacements do not make the essence of the corresponding technical solutions deviate from the spirit and scope of the technical solutions of the embodiments of the present invention.

[0035] The algorithms or displays provided herein are not inherently related to any particular computer, virtual system or other device. In addition, the embodiments of the present invention are not directed to any particular programming language.

[0036] In the description provided herein, a large number of specific details are described. However, it is understood that embodiments of the present invention can be practiced without these specific details. Similarly, in order to simplify the present invention and help understand one or more of the various inventive aspects, in the above description of exemplary embodiments of the present invention, the various features of the embodiments of the present invention are sometimes grouped together into a single embodiment, figure, or description thereof. Wherein, the claims that follow the specific embodiment are hereby expressly incorporated into the specific embodiment, wherein each claim itself is a separate embodiment of the present invention.

[0037] Those skilled in the art will appreciate that the modules in the devices in the embodiments may be adaptively changed and arranged in one or more devices different from the embodiments. The modules or units or components in the embodiments may be combined into one module or unit or component, and further may be divided into a plurality of submodules or subunits or subcomponents. Except that at least some of such features and / or processes or units are mutually exclusive.

[0038] It should be noted that the above embodiments illustrate the present invention rather than limit it, and that those skilled in the art may devise alternative embodiments without departing from the scope of the appended claims. In the claims, any reference symbol between brackets shall not be construed as a limitation on the claims. The word "comprising" does not exclude the presence of elements or steps not listed in the claims. The word "one" or "an" preceding an element does not exclude the presence of a plurality of such elements. The present invention may be implemented by means of hardware comprising a number of different elements and by means of a suitably programmed computer. In a unit claim enumerating a number of devices, several of these devices may be embodied by the same hardware item. The use of the words first, second, and third, etc. does not indicate any order. These words may be interpreted as names. The steps in the above embodiments, unless otherwise specified, should not be understood as limitations on the order of execution.

Claims

1. A method for characterizing the corrosion state of an alloy material, characterized in that: The method comprises: Performing single pulse ablation on a test area of ​​the corrosion layer of the alloy material by using a LIBS device, and recording a LIBS spectrum of the test area; According to the LIBS spectrum, the characteristic spectral line of the element to be measured is selected, and the intensity information of the characteristic spectral line is extracted; A LIBS signal feature characterizing the corrosion state of the material is constructed according to the intensity information of the element to be measured, and the corrosion state of the alloy material is characterized according to the LIBS signal feature.

2. A method for characterizing the corrosion state of an alloy material according to claim 1, characterized in that: The method of performing single pulse ablation on the area to be tested of the corrosion layer of the alloy material by using a LIBS device and recording the LIBS spectrum of the area to be tested specifically includes: The pulsed laser of the LIBS device generates plasma on the surface of the material corrosion layer after the laser passes through the focusing lens; The light signal emitted by the plasma enters the collection lens, is introduced into the spectrometer through the optical fiber, and is converted into a digital signal after passing through the spectrometer and collected by the computer to obtain the LIBS spectrum.

3. The method for characterizing the corrosion state of an alloy material according to claim 1, characterized in that: The number of the regions to be tested is n, and the positions of the n regions to be tested in the corrosion layer of the alloy material are all different, and the LIBS spectra of each region to be tested are recorded as S1, S2, S3, ..., S n .

4. A method for characterizing the corrosion state of an alloy material according to claim 3, characterized in that: The step of selecting characteristic spectral lines of the element to be measured according to the LIBS spectrum and extracting the intensity information of the characteristic spectral lines specifically includes: The characteristic spectral line of the element to be measured is selected as the analysis line, the integral area of ​​the characteristic spectral line is calculated as the integral intensity of the analysis line, and the integral intensities obtained from n spectral data are averaged, and the average integral intensity is used as the intensity information of the characteristic spectral line.

5. A method for characterizing the corrosion state of an alloy material according to claim 4, characterized in that: The step of constructing the LIBS signal feature characterizing the corrosion state of the material according to the intensity information of the element to be measured specifically includes: Obtain the intensity information of the elements to be tested at different corrosion times; According to the positive correlation between the intensity information and the concentration of the element to be measured under the local thermal equilibrium condition of plasma, the LIBS signal characteristics of the corrosion layer of the alloy material are constructed with the intensity information.

6. A method for characterizing the corrosion state of an alloy material according to claim 5, characterized in that: The enrichment degree of the element to be measured on the surface of the corrosion layer of the alloy material shows a monotonically increasing trend as the corrosion time prolongs, indicating that the corrosion degree of the alloy material shows a gradually increasing trend as the corrosion time prolongs.

7. A method for characterizing the corrosion state of an alloy material according to claim 6, characterized in that: The element to be detected is chromium.

8. The method for characterizing the corrosion state of an alloy material according to claim 1, characterized in that: The alloy material is SIMP steel material.

9. The method for characterizing the corrosion state of an alloy material according to claim 1, characterized in that: The alloy material corrosion layer includes an inner corrosion layer and an outer corrosion layer, the inner corrosion layer includes a spinel layer, and the outer corrosion layer includes magnetite.

10. A device for characterizing the corrosion state of an alloy material, characterized in that: The device comprises: A LIBS spectrum acquisition module is used to perform single-pulse ablation on a test area of ​​the corrosion layer of the alloy material through a LIBS device, and record the LIBS spectrum of the test area; The intensity calculation module of the element to be measured is used to select the characteristic spectral line of the element to be measured according to the LIBS spectrum and extract the intensity information of the characteristic spectral line; And a characterization module is used to construct a LIBS signal feature characterizing the corrosion state of the material according to the intensity information of the element to be measured, and characterize the state of the corrosion layer of the alloy material according to the LIBS signal feature.