Laser welding process for small-pipe-diameter pipe fitting

Through the laser welding process, a high-stability laser light source is used to perform single-side laser irradiation and temperature control, which solves the problems of uneven heat and insufficient welding strength in welding small-diameter pipe fittings, and achieves high-quality welding and airtightness improvement. It is suitable for Welding requirements for complex structures.

CN119237926AInactive Publication Date: 2025-01-03SUZHOU LANMU JINGRONG TECHNOLOGY CO LTD
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN202411669208.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-11-21
Publication Date
2025-01-03
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

In the welding of small-pipe-diameter pipe fittings, there are problems such as uneven heat, difficult welding, large heat-affected zones and insufficient welding strength. Especially when the heat-affected zones are limited, the difficulty of flame welding increases, resulting in uneven welding and insufficient strength.

Method used

Using laser welding technology, a laser light source with high stability and high controllability is used for single-sided laser irradiation. Through spot homogenization and temperature control, we ensure uniform temperature heating in the welding area, fully flowing and filling the weld, and improving welding strength and airtightness.

Benefits of technology

It realizes high-quality welding under the restricted heated area, improves welding strength and enhances airtightness. It is suitable for welding needs of various pipe diameters and complex structures, and is stable and efficient, suitable for large-scale production.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119237926A_ABST
    Figure CN119237926A_ABST
Patent Text Reader

Abstract

The invention belongs to the technical field of welding, and particularly relates to a laser welding process for a small-pipe-diameter pipe fitting. In the laser welding process, a high-stability and high-precision controllable laser light source serves as a heat source to conduct single-face laser irradiation, the temperature of the irradiation position is precisely controlled within a set range, 360-degree overall heating is achieved in a heat conduction mode, it is guaranteed that the temperatures of all positions of welding flux exceed the melting point of the welding flux, and the welding flux flows sufficiently; uniform filling is achieved, and the effect of overall welding of the pipe fitting is finally achieved; overall laser welding of the small-diameter pipe fitting on the premise that the small-diameter pipe fitting does not rotate can be achieved. And laser welding with high degree of freedom, large fusion depth and high uniformity can be realized in application scenes of small-pipe-diameter radiators, shunt pipes, complex small-pipe-diameter welding and the like.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of welding, and in particular relates to a laser welding process for small-diameter pipe fittings. Background Art

[0002] At present, flame welding is usually used in the field of welding small-diameter pipe fittings. For small-diameter pipe fittings, the problem of too thin pipe wall makes flame welding more difficult. Generally speaking, the smaller the pipe diameter, the more difficult the flame welding is, and it is easy to be welded through due to uneven heating. In welding scenarios such as small-diameter radiators, shunt pipes, and complex small-diameter pipelines, when the heating area is limited, there are problems such as difficulty in flame welding, uneven welding, large heat-affected zone, and insufficient welding strength. Summary of the invention

[0003] In order to solve the above technical problems, the purpose of the present invention is to provide a laser welding process for small diameter pipe fittings, which utilizes the high stability and high controllability of laser to achieve high-quality welding of small diameter pipe fittings under the premise of limited heating area.

[0004] In order to achieve the above object, the technical solution adopted by the present invention is as follows:

[0005] A laser welding process for small-diameter pipe fittings comprises the following steps:

[0006] Step 1: Install two small-diameter metal pipes to be welded on the fixture of the welding platform and clamp the pipes to ensure the stability and precise positioning of the pipes during welding;

[0007] Step 2: Select solder;

[0008] Among them, the melting point of the solder is required to be lower than that of the pipe material to ensure that the solder can melt first during the welding process, fill the weld, and improve the welding strength and air tightness;

[0009] Step 3: Start the laser, set the laser power and defocus amount according to the target requirements, and after the spot homogenization process, evenly irradiate the laser beam emitted by the laser on the welding position of the small-diameter pipe fittings, and ensure that the spot can completely cover the irradiation surface of the pipe fittings;

[0010] Step 4: Start the laser welding machine, irradiate the welding position of the pipe with a single-side laser, and perform welding using the set defocus amount and the homogenized spot;

[0011] When the overall temperature of the welding area exceeds the melting point of the solder, the solder begins to melt and flows into the weld for welding;

[0012] Step 5: After welding is completed, gradually reduce the temperature to allow the weld to cool naturally to ensure the structural integrity and mechanical properties of the weld.

[0013] Preferably, the present invention discloses a laser welding system, the laser welding system comprising:

[0014] Lasers, welding platforms, fixtures, and temperature control devices;

[0015] Among them, the laser can choose a variety of laser light sources such as infrared, green light, blue light, etc. according to the characteristics of the pipe material;

[0016] The welding platform is used to mount two small-diameter metal pipes to be welded, to install the fixture, and to enable it to move horizontally or vertically to align the pipes;

[0017] The clamp is used to clamp two small-diameter metal pipes to be welded so that they do not deviate during the welding process;

[0018] The temperature control device is used to control the temperature of the welding area so that it remains above the melting point of the solder and does not exceed the melting point of the welded pipe to ensure sufficient flow of the solder.

[0019] Preferably, the present invention discloses a method for mounting two small-diameter metal pipes to be welded on a fixture of a welding platform, comprising the following steps:

[0020] Step (1) cleaning two small-diameter metal pipes to be welded to remove oxides and grease to ensure a good welding contact surface;

[0021] Step (2) Select a suitable clamp and clamp the two small-diameter metal pipes to be welded with the clamps to ensure that they can be firmly fixed and will not move or deviate during the welding process and will not damage the pipes;

[0022] Step (3) adjusts the position of the clamp on the welding platform to ensure that the two small-diameter metal pipes to be welded are aligned and in a stable position, and to provide operating space for laser welding.

[0023] Preferably, the present invention discloses a specific method for filling a weld, comprising the following steps:

[0024] Step (1) selecting a suitable solder according to the material of the pipe fitting, the melting point of the solder is lower than the melting point of the pipe fitting material to ensure that the solder can be melted preferentially during the welding process, and the composition of the solder should be compatible with the pipe fitting material to ensure the mechanical properties and corrosion resistance of the joint after welding;

[0025] Step (2) cleaning the solder surface to remove oxides and other impurities to ensure that it can fully flow and fill the weld during the melting process;

[0026] Step (3) processing the solder into a shape and size matching the welded pipe fitting so as to facilitate filling into the weld;

[0027] Step (4) placing solder at the joint of the pipe to be welded, and reasonably arranging the position of the solder according to the shape of the pipe and the width of the weld to ensure that the solder is evenly distributed over the entire length of the weld to avoid uneven welding or weld defects;

[0028] Step (5) Check the accuracy of solder placement and use tools to fine-tune the position and amount of solder to ensure that it can fully melt and fill the entire weld during the welding process to ensure welding quality.

[0029] Compared with the prior art, the present invention has the following beneficial effects:

[0030] In the present invention, a laser light source with high stability and high precision controllability is used as a heat source for single-sided laser irradiation, so that the temperature of the irradiated position can be accurately controlled within a set range, and 360-degree overall heating is achieved by heat conduction, ensuring that the temperature of all positions of the solder exceeds its melting point and fully flows to achieve uniform filling; and because the heat conduction direction is omnidirectional, not only the solder temperature will increase, but also the temperature of the metal pipe at the weld will increase, and the sufficient temperature of the metal at the weld ensures that the molten liquid solder will not solidify when it encounters cold during the flow of the weld, thereby ensuring the full flow of the liquid solder, and the full flow of the solder further ensures the penetration depth and air tightness; this method is suitable for welding needs of various pipe diameters and complex structures, is stable and efficient, has high repeatability, and can be mass-produced. BRIEF DESCRIPTION OF THE DRAWINGS

[0031] Figure 1 It is a schematic diagram of the structure of the laser welding process in the present invention;

[0032] Figure 2 It is a schematic diagram of the specific process of the laser welding process in the present invention;

[0033] Figure 3 It is a schematic diagram of two small-diameter metal pipes to be welded installed on a fixture of a welding platform in Example 2 of the present invention;

[0034] Figure 4 is a schematic diagram of the welding position of the laser beam irradiated on the small-diameter metal pipe to be welded in Example 2 of the present invention;

[0035] Figure 5 is a schematic structural diagram of the solder molten flow filling the weld in Example 2 of the present invention;

[0036] Figure 6 It is a schematic diagram of the solder melting and flowing into the weld for welding in Example 2 of the present invention.

[0037] In the figure: 1. Small-diameter metal pipe fittings to be welded 1; 2. Small-diameter metal pipe fittings to be welded 2; 3. Solder; 4. Laser beam; 5. Laser head; 6. Heat conduction direction; 7. Fixture 1; 8. Fixture 2; 9. Welding gun; 10. Welding platform; 11. Laser spot; 12. Welded pipe fittings. DETAILED DESCRIPTION

[0038] The technical solutions in the embodiments of the present invention will be clearly and completely described below in conjunction with the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, rather than all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of the present invention.

[0039] Compared with flame welding, laser can be focused to a very small spot size and provide very high energy density, which enables laser welding to accurately concentrate heat in the welding area without causing excessive thermal impact on the surrounding area, thereby reducing thermal deformation and internal stress of the material; select laser welding equipment with high stability and high-precision controllability, equipped with a precise power control system, which can adjust the laser output power according to material properties and welding requirements, and can quickly respond to changes in power and spot size to ensure that the temperature of the welding area is maintained within the required range; control the laser power according to the material and diameter of the pipe, and set a certain defocus amount and spot homogenization treatment method for the laser spot to ensure uniform spot energy distribution, avoid local overheating, and improve welding quality and consistency.

[0040] Example 1

[0041] This embodiment discloses a laser welding system, which includes:

[0042] Lasers, welding platforms, fixtures, and temperature control devices;

[0043] Among them, the laser can choose a variety of laser light sources such as infrared, green light, blue light, etc. according to the characteristics of the pipe material;

[0044] The welding platform is used to mount two small-diameter metal pipes to be welded, to install the fixture, and to enable it to move horizontally or vertically to align the pipes;

[0045] The clamp is used to clamp two small-diameter metal pipes to be welded so that they do not deviate during the welding process;

[0046] The temperature control device is used to control the temperature of the welding area so that it remains above the melting point of the solder and does not exceed the melting point of the welded pipe to ensure sufficient flow of the solder.

[0047] Example 2

[0048] This embodiment discloses a laser welding process for small-diameter pipe fittings, comprising the following steps:

[0049] Step 1: Install two small-diameter metal pipe fittings to be welded (small-diameter metal pipe fitting 1 to be welded and small-diameter metal pipe fitting 2 to be welded) on two clamps (clamp 1 and clamp 2) on the welding platform respectively, and clamp the pipe fittings to ensure the stability and precise positioning of the pipe fittings during the welding process;

[0050] The fixture on the welding platform can be moved horizontally or vertically, and the position of the fixture on the welding platform can be controlled manually or electrically. Before welding, the weld is set according to the material and diameter of the pipe fittings, and the pipe center is aligned;

[0051] Before welding, preheat the pipe to reduce thermal deformation during welding and improve welding quality;

[0052] Step 2: Select a fixture suitable for small-diameter pipe fittings and a solder suitable for the material of the pipe fittings, ensuring that its melting point is lower than that of the pipe fitting material;

[0053] Step 3: Start the laser, set the laser power and defocus amount according to the target requirements, and after the spot homogenization process, evenly irradiate the laser beam emitted by the laser on the welding position of the small-diameter pipe fittings, and ensure that the spot can completely cover the irradiation surface of the pipe fittings;

[0054] Depending on the material of the pipe, you can choose a variety of laser light sources such as infrared, green light, and blue light. Equipped with a precise control system, the laser output power can be adjusted according to the material characteristics and welding requirements, and it can quickly respond to changes in power, spot size, and defocus to ensure that the temperature of the welding area is maintained within the required range;

[0055] According to the material and diameter of the pipe, set the appropriate laser defocus and laser power, and use optical lenses or other optical elements to homogenize the laser spot so that the laser spot can be evenly irradiated on the welding position. The diameter of the irradiated area is larger than the diameter of the weld and the pipe, ensuring that the spot can completely cover the irradiated surface of the pipe and ensure full and sufficient heat conduction. The spot can be round or square;

[0056] Step 4: Start the laser welding machine, irradiate the welding position of the pipe with a single-side laser, and perform welding using the set defocus amount and the homogenized spot; when the overall temperature of the welding area exceeds the melting point of the solder, the solder begins to melt and flows into the weld for welding;

[0057] Process the solder into a shape and size that matches the welded pipe fittings;

[0058] In this embodiment, the selected metal small-diameter pipe fittings are copper, copper alloy, aluminum and other pipe fittings, and the materials of the two pipe fittings to be welded can be the same or different;

[0059] The welding gun is located on one side of the weld of the pipe to be welded. It can be irradiated from any side, but there are requirements on the distance between the welding gun and the weld.

[0060] During the laser irradiation process, the thermal conductivity of the pipe material is used to control the temperature of the laser irradiation area so that it does not exceed the melting point of the metal pipe, avoiding melting deformation or burning through the pipe. The heat is transferred from the irradiation area to the entire welding area through the thermal conductivity of the pipe material.

[0061] When the temperature of the welding area exceeds the melting point of the solder, the solder begins to melt and flow into the weld. At the same time, the temperature of the welding area is controlled to keep it above the melting point of the solder and below the melting point of the pipe to ensure sufficient flow of the solder. Through all-round heat conduction, the temperature of the metal pipe at the weld is high enough to ensure that the liquid solder will not solidify when it encounters cold during the flow process, thereby ensuring the penetration depth and air tightness of the weld;

[0062] Control the laser irradiation time and irradiation energy, adjust the laser power according to the material and thickness of the pipe and solder, and ensure that the solder flows fully to evenly fill the entire weld without welding through the pipe;

[0063] Install a temperature monitoring device in the laser welding system to monitor the temperature of the welding area during the welding process, and judge the temperature by combining manual observation of the color and melting condition of the welding area;

[0064] Step 5: After welding is completed, gradually reduce the temperature to allow the weld to cool naturally to ensure the structural integrity and mechanical properties of the weld;

[0065] Clean the welding area to remove slag and residual solder and ensure that the welding area remains clean.

[0066] Example 3

[0067] This embodiment discloses a method for mounting two small-diameter metal pipes to be welded on a fixture of a welding platform, comprising the following steps:

[0068] Step (1) cleaning two small-diameter metal pipes to be welded to remove oxides and grease to ensure a good welding contact surface;

[0069] Step (2) Select a suitable clamp and clamp the two small-diameter metal pipes to be welded with the clamps to ensure that the pipes can be firmly fixed and will not move or deviate during the welding process and will not damage the pipes;

[0070] Step (3) adjusts the position of the clamp on the welding platform to ensure that the two small-diameter metal pipes to be welded are aligned and in a stable position, and to provide operating space for laser welding.

[0071] Example 4

[0072] This embodiment discloses a specific method for filling a weld, including the following steps:

[0073] Step (1) selecting a suitable solder according to the material of the pipe fitting, the melting point of the solder is lower than the melting point of the pipe fitting material to ensure that the solder can be melted preferentially during the welding process, and the composition of the solder should be compatible with the pipe fitting material to ensure the mechanical properties and corrosion resistance of the joint after welding;

[0074] Step (2) cleaning the solder surface to remove oxides and other impurities to ensure that it can fully flow and fill the weld during the melting process;

[0075] Step (3) processing the solder into a shape and size matching the welded pipe fitting so as to facilitate filling into the weld;

[0076] Step (4) placing solder at the joint of the pipe to be welded, and reasonably arranging the position of the solder according to the shape of the pipe and the width of the weld to ensure that the solder is evenly distributed over the entire length of the weld to avoid uneven welding or weld defects;

[0077] Step (5) Check the accuracy of solder placement and use tools to fine-tune the position and amount of solder to ensure that it can fully melt and fill the entire weld during the welding process to ensure welding quality.

[0078] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.

Claims

1. A laser welding process for small diameter pipe fittings, characterized in that: The following steps are involved: Step 1: Install two small-diameter metal pipes to be welded on the clamps of the welding platform and clamp the pipes; Step 2: Select solder; Step 3: Start the laser and set the laser power and defocus amount; Step 4: Start the laser welding machine and perform single-sided laser irradiation on the welding position of the pipe fitting; When the overall temperature of the welding area exceeds the melting point of the solder, the solder begins to melt and flows into the weld for welding; Step 5: After welding is completed, lower the temperature and allow the weld to cool naturally.

2. A laser welding process for small diameter pipe fittings according to claim 1, characterized in that: Step 1 specifically includes the following steps: Step (1) cleaning two small-diameter metal pipes to be welded to remove oxides and grease to ensure a good welding contact surface; Step (2) Select a suitable clamp and clamp the two small-diameter metal pipes to be welded with the clamps to ensure that they can be firmly fixed and will not move or deviate during the welding process and will not damage the pipes; Step (3) adjusts the position of the clamp on the welding platform to ensure that the two small-diameter metal pipes to be welded are aligned and in a stable position, and to provide operating space for laser welding.

3. A laser welding process for small diameter pipe fittings according to claim 1, characterized in that: In the step 1, the two small-diameter metal pipes to be welded are made of any one of copper, copper alloy and aluminum.

4. A laser welding process for small diameter pipe fittings according to claim 1, characterized in that: In the step 2, the melting point of the solder is lower than the melting point of the pipe material.

5. The laser welding process for small diameter pipe fittings according to claim 1 is characterized in that: The step three also includes a light spot homogenization process, so that the laser beam is evenly irradiated on the welding position of the two small-diameter metal pipes to be welded, and ensures that the light spot can completely cover the irradiation surface of the pipe.

6. A laser welding process for small diameter pipe fittings according to claim 1, characterized in that: In the step 4, the light source of the laser includes any one of infrared, green light and blue light.

Citation Information

Patent Citations

  • Cup joint hollow copper pipe manufacturing method and device based on laser cutting and welding

    CN106624362A

  • Petroleum pipeline laser arc hybrid welding device and method

    CN111347162A

  • Process for welding elbow and metal pipe of heat exchanger through laser cladding

    CN117161562A

  • Production of bent tube joint ring for endoscope

    JP1995241689A