Magnetic control coating control method, device and system and storage medium
By obtaining the substrate film thickness data of the sputtering coating equipment, building a deviation matrix and optimizing the magnetic field and exhaust control, the problem of uneven film thickness is solved, and higher film uniformity and target utilization are achieved.
Patent Information
- Application Number
- CN202510650641.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2025-05-20
- Publication Date
- 2025-08-29
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
When the existing magnetron sputtering technology generates films, there is a problem of uneven film thickness, especially in optical components or precision sensor manufacturing that require high uniformity films. The uniform rotation magnetic field technology leads to uneven utilization of the target material and large material loss.
By obtaining the substrate film thickness data of the sputtering coating equipment, a first uniform deviation matrix is constructed, and the matrix weight of the second uniform deviation matrix is optimized using a genetic algorithm, and combined with the preset magnetic field and exhaust control data, the coating process is optimized to improve the film uniformity.
Effectively identify and optimize the uneven situations during the coating process, improve the overall uniformity of the film, reduce material losses, and improve target utilization.
Smart Images

Figure CN120555981A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of magnetron sputtering coating, and in particular to a magnetron sputtering coating control method, device, system and storage medium. Background Art
[0002] Magnetron sputtering technology is an important process in the field of thin film preparation. It generally improves the film quality by regulating the movement of plasma within a certain range through magnetic fields. In actual industrial production, the requirements for thin film performance vary greatly in different situations. For example, in the manufacture of optical components or precision sensors that require ultra-uniform thin films, high atomic-level deposition accuracy is required. In scenarios where efficient use of target materials is pursued, uniform rotating magnetic field technology is better. Generally, the continuous rotation of the magnetic poles guides the plasma to spirally etch the target surface, so that each area of the target material can be used evenly, significantly reducing material loss. Thin films generated by magnetron sputtering in a rotating magnetic field can only produce relatively low-uniform films, resulting in uneven film thickness.
[0003] The above content is only used to assist in understanding the technical solution of the present invention and does not constitute an admission that the above content is prior art. Summary of the Invention
[0004] The main purpose of the present invention is to provide a magnetron coating control method, device, system and storage medium, aiming to improve the uniformity of film thickness.
[0005] To achieve the above object, the present invention provides a magnetron coating control method, which is applied to a sputtering coating device. The magnetron coating control method comprises the following steps:
[0006] Acquiring film thickness data of a substrate of a sputtering coating device, and determining a first uniformity deviation matrix based on the film thickness data, wherein each element of the first uniformity deviation matrix corresponds to a uniformity relative deviation value of a detection position on the substrate;
[0007] Determine a matrix weight corresponding to each second uniform deviation matrix according to the first uniform deviation matrix and the coating optimization target, wherein the second uniform deviation matrix is a uniform deviation matrix obtained by detecting after coating is performed under preset magnetic field control data and preset exhaust control data within a preset time;
[0008] Determining magnetic field control data and air extraction control data according to the second uniform deviation matrix, the corresponding matrix weight, and a preset corresponding relationship;
[0009] The operation of the sputtering coating equipment is controlled according to the magnetic field control data and the exhaust control data.
[0010] Optionally, the step of determining a second uniform deviation matrix and corresponding matrix weights according to the first uniform deviation matrix and the coating optimization target includes:
[0011] Determine an objective function according to the first uniform deviation matrix and the coating optimization target, and generate an initial weight vector;
[0012] Calculating a target weight vector corresponding to a Pareto optimal solution set according to the genetic algorithm, the objective function, and the initial weight vector, wherein elements of the target weight vector correspond one-to-one to matrix weights of the second uniform deviation matrix;
[0013] The matrix weight is determined according to the target weight vector.
[0014] Optionally, the step of determining an objective function according to the first uniform deviation matrix and the coating optimization target includes:
[0015] Subtracting the first uniform deviation matrix from the uniform matrix corresponding to the coating optimization target to obtain a target matrix;
[0016] The objective function is determined according to the target matrix, where the objective function is the root mean square error between the weighted matrix and the target matrix. Each of the second uniform deviation matrices is multiplied by the corresponding matrix weight as the corresponding third matrix to obtain multiple third matrices, and the weighted matrix is the sum of all third matrices.
[0017] Optionally, before the step of obtaining the film thickness data of the substrate of the sputtering coating device, the method further includes:
[0018] Controlling the coating time corresponding to different magnetic field directions, and collecting thickness change data of the film layer of the substrate during the coating time, wherein the coating time corresponding to each magnetic field direction is continuous;
[0019] The second uniform deviation matrix is updated according to the thickness variation data.
[0020] Optionally, the step of obtaining film thickness data of a substrate of a sputtering coating device includes:
[0021] controlling an infrared light source to illuminate the substrate and collecting a reflection spectrum of the substrate;
[0022] The thickness data is calculated based on the reflection spectrum.
[0023] Optionally, the preset correspondence includes a mapping table, which is a mapping relationship between the second uniform deviation matrix and the magnetic field information and the air extraction information. The step of determining the magnetic field control data and the air extraction control data according to the second uniform deviation matrix, the corresponding matrix weight, and the preset correspondence includes:
[0024] Determining corresponding magnetic field information and air extraction information in the mapping table according to the second uniform deviation matrix;
[0025] determining a coating compensation time corresponding to the magnetic field information and the exhaust information according to a matrix weight corresponding to each of the second uniform deviation matrices;
[0026] The magnetic field information and the exhaust gas information are used to determine the magnetic field control data and the exhaust gas control data by using the coating compensation time corresponding to the magnetic field information and the exhaust gas information.
[0027] Optionally, the film thickness data includes film thicknesses corresponding to various detection positions of the substrate, and the step of determining a first uniform deviation matrix based on the film thickness data includes:
[0028] Calculate the average thickness based on the film thicknesses corresponding to all the detection positions;
[0029] Determining a uniform deviation value at each detection position according to the average thickness and the film thickness corresponding to the detection position;
[0030] Each position of the substrate is mapped to the position of an element of a corresponding matrix, position mapping information, and the first uniform deviation matrix is determined according to the position mapping information and the uniform deviation value corresponding to each position.
[0031] In addition, to achieve the above-mentioned purpose, the present invention further provides a magnetron coating control device, the magnetron coating control device comprising:
[0032] an acquisition module, configured to acquire film thickness data of a substrate of a sputtering coating device, and determine a first uniformity deviation matrix based on the film thickness data, wherein each element of the first uniformity deviation matrix corresponds to a uniformity relative deviation value of a detection position on the substrate;
[0033] a matching module, configured to determine a matrix weight corresponding to each second uniform deviation matrix according to the first uniform deviation matrix and a coating optimization target, wherein the second uniform deviation matrix is a uniform deviation matrix obtained by detecting after coating is performed under preset magnetic field control data and preset exhaust control data within a preset time;
[0034] a generating module, configured to determine magnetic field control data and air extraction control data according to the second uniform deviation matrix, the corresponding matrix weights, and a preset corresponding relationship;
[0035] A control module is used to control the operation of the sputtering coating equipment according to the magnetic field control data and the exhaust control data.
[0036] In addition, to achieve the above-mentioned purpose, the present invention also provides a magnetron coating control system, which includes: a memory, a processor, and a magnetron coating control program stored in the memory and executable on the processor, wherein the magnetron coating control program is configured to implement the steps of the magnetron coating control method described in any one of the above-mentioned items.
[0037] In addition, to achieve the above-mentioned purpose, the present invention also provides a storage medium, on which a magnetron coating control program is stored. When the magnetron coating control program is executed by a processor, the steps of any of the above-mentioned magnetron coating control methods are implemented.
[0038] The present invention proposes a magnetron coating control method, which obtains the film thickness data of the substrate of the sputtering coating equipment and determines the first uniform deviation matrix based on the film thickness data, thereby effectively improving the identification of the uniformity of the film thickness, and determining the matrix weight corresponding to each second uniform deviation matrix based on the first uniform deviation matrix and the coating optimization target, that is, it is possible to determine the control data required to improve the uniformity subsequently, and execute the operation of the sputtering coating equipment according to the magnetic field control data and the exhaust control data. Compared with the method of controlling the magnetic field with uniform rotation, the present application can more effectively identify and optimize the unevenness in the coating process, thereby improving the uniformity of the thin film as a whole. BRIEF DESCRIPTION OF THE DRAWINGS
[0039] Figure 1 It is a structural diagram of a magnetron coating control device in a hardware operating environment according to an embodiment of the present invention;
[0040] Figure 2 Schematic diagram of the flow of the first embodiment of the magnetron coating control method of the present invention;
[0041] Figure 3 Schematic diagram of the flow chart of the second embodiment of the magnetron coating control method of the present invention;
[0042] Figure 4 1 is a flow chart of a third embodiment of a magnetron coating control method according to the present invention;
[0043] Figure 5 FIG. 4 is a flow chart of a fourth embodiment of a magnetron coating control method according to the present invention.
[0044] The purpose, features and advantages of the present invention will be further described with reference to the accompanying drawings and in conjunction with the embodiments. DETAILED DESCRIPTION
[0045] It should be understood that the specific embodiments described herein are only used to explain the present invention and are not intended to limit the present invention.
[0046] Reference Figure 1 , Figure 1 It is a structural diagram of the magnetron coating control system of the hardware operating environment involved in the embodiment of the present invention.
[0047] like Figure 1 As shown, the magnetron coating control system can be provided on a magnetron coating control device, which includes: a processor 1001, such as a central processing unit (CPU), a communication bus 1002, an interactive device 1003, a network interface 1004, and a memory 1005. The communication bus 1002 is used to enable communication between these components. The interactive device 1003 may include a display and an input unit, such as a keyboard. Optionally, the interactive device 1003 may also be connected to the communication bus via a standard wired interface or a wireless interface. The network interface 1004 may optionally include a standard wired interface or a wireless interface (such as a wireless fidelity (WI-FI) interface). The memory 1005 may be a high-speed random access memory (RAM) or a stable non-volatile memory (NVM), such as a disk storage device. The memory 1005 may also be a storage device independent of the processor 1001.
[0048] Those skilled in the art will understand that Figure 1 The structure shown in the figure does not constitute a limitation on the magnetron coating control device, and may include more or fewer components than shown in the figure, or combine certain components, or arrange the components differently.
[0049] like Figure 1 As shown, the memory 1005 as a storage medium may include an operating system, a data storage module, a network communication module, a user interface module and a magnetron coating control program.
[0050] exist Figure 1In the illustrated magnetron coating control device, the network interface 1004 is primarily used for data communication with other devices; the interactive device 1003 is primarily used for data interaction with a user; the processor 1001 and memory 1005 in the magnetron coating control device of the present invention can be provided within the magnetron coating control device. Furthermore, the magnetron coating control device further includes hardware controlled by a magnetron coating control program. The magnetron coating control program controls specific hardware to implement a specific control method within the magnetron coating control device. The magnetron coating control device invokes the magnetron coating control program stored in the memory 1005 via the processor 1001 and executes the magnetron coating control method provided by an embodiment of the present invention.
[0051] The embodiment of the present invention provides a magnetron coating control method, referring to Figure 2 , Figure 2 1 is a flow chart of a first embodiment of a magnetron coating control method according to the present invention. In this embodiment, the magnetron coating control method includes:
[0052] Step S1, obtaining film thickness data of a substrate of a sputtering coating device, and determining a first uniformity deviation matrix based on the film thickness data, wherein each element of the first uniformity deviation matrix corresponds to a uniformity relative deviation value of a detection position on the substrate;
[0053] In this embodiment, the sputtering coating apparatus generally includes: a substrate, a target, an anode on one side of the substrate, and a cathode on the other side of the target. Argon gas is typically injected between the substrate and target, ionizing the argon gas into argon ions and electrons. The argon ions bombard the target under the action of an electric field, causing the target's atoms or molecules to detach from the target surface and deposit on the substrate surface to form a thin film. In the art, a rotating magnetic field is typically created by rotating a ferromagnetic coil or coil using a mechanical rotating component, thereby increasing target utilization. It should be noted that the film thickness data here refers to the thickness of the film formed on the substrate, also generally referred to as coating thickness or film thickness, and does not refer to the thickness of the entire substrate. For established sputtering coating technology, the target-substrate distance often affects the degree of compactness formed during the coating process and is generally determined based on production experience. In this embodiment, the first uniformity deviation matrix reflects the film quality, namely, whether the thickness of each location in the film layer is uniform. Preferably, the film thickness data is measured every 3 cm, and the detection area is rectangular. This achieves a one-to-one correspondence between the first uniform deviation matrix and the thickness deviation of the film layer on the substrate. Furthermore, the size of the first uniform deviation matrix is generally not limited; rather, the first uniform deviation matrix and the second uniform deviation matrix are limited to the same size. In this embodiment, uniformity refers to the lateral uniformity of the film. Vertical uniformity is not included. Furthermore, this embodiment is not applicable to coating processes involving more than one film layer.
[0054] Step S2, determining a matrix weight corresponding to each second uniform deviation matrix according to the first uniform deviation matrix and the coating optimization target, wherein the second uniform deviation matrix is a uniform deviation matrix obtained by detecting after coating is performed under preset magnetic field control data and preset exhaust control data within a preset time;
[0055] The second uniformity deviation matrix is determined by monitoring changes in film thickness over a preset time period under a fixed preset magnetic field and fixed preset pumping control data. It should be noted that the gas supply method employed is binary to ensure uniform gas flow. Furthermore, multiple pumping channels are typically provided, and the pumping conditions are generally determined by controlling the operation of the molecular pump, i.e., the preset pumping control data. Generally speaking, when the pumping pump is operating normally, the pumping process is uniform, preventing uneven gas flow across different regions and reducing uniformity. However, when the molecular pump is partially activated, various film thickness variations can occur in response to magnetic fields of different directions, corresponding to the second uniformity deviation matrix. Although the preset magnetic field control data and preset pumping control data corresponding to the second uniformity deviation matrix do affect film uniformity, superimposing multiple second uniformity deviation matrices can actually optimize film thickness uniformity. The coating optimization goal here is to achieve a relative deviation of zero at each location. In practice, the matrix weights corresponding to each second uniformity deviation matrix must be determined jointly by the first uniformity deviation matrix and the coating optimization goal.
[0056] Step S3, determining magnetic field control data and air extraction control data according to the second uniform deviation matrix, the corresponding matrix weight and the preset corresponding relationship;
[0057] Specifically, since the second uniform deviation matrix corresponds to the preset magnetic field control data and the preset pumping control data, the matrix weights here actually determine the coating time. Preferably, the coating time under each magnetic field state and each pumping state is determined based on each matrix weight and the average thickness of the film thickness data. The magnetic field control data here includes: the direction of the magnetic field, the intensity of the magnetic field, and the coating time, etc. The pumping control data includes: the pumping channel used, the working status of the molecular pump, and the coating time under the corresponding state.
[0058] Step S4: controlling the operation of the sputtering coating equipment according to the magnetic field control data and the exhaust control data.
[0059] Based on the magnetic field control data and the exhaust control data, the operation of the sputtering coating equipment is controlled, thereby achieving uniform thin film production.
[0060] In this embodiment, by obtaining the film thickness data of the substrate of the sputtering coating equipment and determining the first uniform deviation matrix based on the film thickness data, the identification of the uniformity of the film thickness can be improved, and the matrix weight corresponding to each second uniform deviation matrix is determined according to the first uniform deviation matrix and the coating optimization target, and the magnetic field control data and the exhaust control data are determined according to the second uniform deviation matrix, the corresponding matrix weight and the preset correspondence. The operation of the sputtering coating equipment is controlled according to the magnetic field control data and the exhaust control data. Compared with the method of controlling the magnetic field with uniform rotation, the present application can more effectively identify and optimize the unevenness in the coating process, thereby improving the uniformity of the thin film as a whole.
[0061] Further, based on the first embodiment, a second embodiment of the magnetron coating control method of the present invention is proposed. In this embodiment, referring to Figure 3 The step of determining the second uniform deviation matrix and the corresponding matrix weight according to the first uniform deviation matrix and the coating optimization target includes:
[0062] Step S21, determining an objective function according to the first uniform deviation matrix and the coating optimization target, and generating an initial weight vector;
[0063] In this embodiment, an initial weight vector may be randomly generated. Each element of the weight vector corresponds to a second uniform deviation matrix, and the number of elements in the weight vector is the same as the number of the second uniform deviation matrices.
[0064] Step S22, calculating a target weight vector corresponding to the Pareto optimal solution set according to the genetic algorithm, the objective function, and the initial weight vector, wherein the elements of the target weight vector correspond one-to-one to the matrix weights of the second uniform deviation matrix;
[0065] The genetic algorithm herein is used to search for the optimal weight vector within the objective function as the target weight vector. Preferably, the parameters of the genetic algorithm include: population size, crossover probability, mutation probability, and maximum number of iterations. A larger number of second uniform deviation matrices corresponds to an increase in the corresponding population size and crossover probability. Of course, in other embodiments, the genetic algorithm may also be a simulated annealing algorithm. Through this algorithm, the target weight vector that most closely approximates the objective function can be determined, thereby obtaining specific control data for controlling the magnetic field and the air extraction.
[0066] Step S23: determining the matrix weight according to the target weight vector.
[0067] In this embodiment, the target weight vector corresponding to the Pareto optimal solution set is calculated through the genetic algorithm, the objective function and the initial weight vector, so that the uniformity of the film layer can be improved by combining the respective second uniform deviation matrices.
[0068] Furthermore, the step of determining the objective function according to the first uniform deviation matrix and the coating optimization target includes:
[0069] Subtracting the first uniform deviation matrix from the uniform matrix corresponding to the coating optimization target to obtain a target matrix;
[0070] The objective function is determined according to the target matrix, where the objective function is the root mean square error between the weighted matrix and the target matrix. Each of the second uniform deviation matrices is multiplied by the corresponding matrix weight as the corresponding third matrix to obtain multiple third matrices, and the weighted matrix is the sum of all third matrices.
[0071] Specifically, the uniform matrix here is a zero matrix having the same matrix size as the first uniform deviation matrix. A target matrix is obtained by performing matrix subtraction on the uniform matrix and the first uniform deviation matrix.
[0072] The weight vector here is: W=[w1,w2,w3,w4,...,w N ,], And w i ≥0;
[0073] The weighting matrix here is:
[0074] The target matrix here is T;
[0075] The second uniform deviation matrix here is: E i , i≥1;
[0076] The objective function here is:
[0077]
[0078] Among them, ||.|| F Represents the square root of the sum of the squares of the matrix elements.
[0079] In this embodiment, it is necessary to solve the minimum objective function. Here, when the minimum objective function can be obtained, it represents the most uniform film layer that can be obtained by superimposing the second uniform deviation matrix.
[0080] In this embodiment, the target weight vector is obtained through a genetic algorithm based on the objective function, and the matrix weight is determined according to the target weight vector, thereby improving the accuracy of subsequent magnetic field control data and further improving the uniformity of the film layer.
[0081] Further, based on the first embodiment or the second embodiment, a third embodiment of the magnetron coating control method of the present invention is proposed. In this embodiment, referring to Figure 4 , before the step of obtaining the film thickness data of the substrate of the sputtering coating equipment, it also includes:
[0082] Step S01, controlling the coating time corresponding to different magnetic field directions, and collecting thickness variation data of the film layer of the substrate during the coating time, wherein the coating time corresponding to each magnetic field direction is continuous;
[0083] To deposit a 300-500 nm thick molybdenum (Mo) film, it takes approximately 30-60 minutes for each 100 nm increase in film thickness under the conditions of 10-30 W sputtering power, argon working gas, and 100 V substrate bias. Furthermore, the coating time needs to be adjusted accordingly for different sputtering control data and process parameters. Optionally, 18 magnetic field directions are set, all perpendicular to the electric field direction, with one magnetic field direction typically spaced 20° apart. The coating time for each magnetic field direction is continuous, and the operator sets the specific coating time. The coating time can be set based on actual coating requirements. Generally, the coating time corresponding to the above-mentioned different magnetic field directions ensures that the film thickness reaches a certain percentage of the target thickness. For example, if the target thickness of the film is 500 nm, the coating time is set so that after coating in each magnetic field direction, the average film thickness reaches 400 nm, or 80% of the target thickness. In this process, the thickness change data of the film layer of the substrate during the coating time is collected, and the thickness change data is used to update or verify the second uniform deviation matrix at the same time as each magnetron sputtering coating. This method can easily adapt to various coating parameters. That is, it can adapt to different target-substrate distances, different voltages, and different argon concentrations while coating thin films with different index requirements. And it makes it easy to change the control scheme of the direction of the uniformly rotating magnetic field to the current magnetic field control method. Further reduce the test cost required for technical improvements. In this embodiment, it is necessary to set the weight w i The minimum step size, for example: the step size is 0.01, that is The minimum step size of 0.01 corresponds to the time required for a film thickness of 1 nm. In this embodiment, magnetron sputtering coating can be divided into two stages. The first stage is to rotate the magnetic field at a preset angle and coat the film over a period of time. Preferably, each coating time is the same. The second stage is to execute steps S1, S2, S3, and S4, thereby achieving high target material utilization while improving the uniformity of the film thickness.
[0084] Step S02: updating the second uniform deviation matrix according to the thickness variation data.
[0085] In this embodiment, in some embodiments, the second uniform deviation matrix can also be verified according to the thickness change data, for example, determining whether the corresponding second uniform deviation matrix is accurate when the magnetic field direction is 0° and the air is pumped normally.
[0086] Furthermore, the step of obtaining the film thickness data of the substrate of the sputtering coating equipment includes:
[0087] controlling an infrared light source to illuminate the substrate and collecting a reflection spectrum of the substrate;
[0088] In this embodiment, an infrared thickness measurement method is used, which can realize non-contact and efficient detection of the thickness of the film. In some implementation examples, multiple thickness measurement methods can also be used, such as: Quartz Crystal Microbalance Array (QCM).
[0089] The thickness data is calculated based on the reflection spectrum.
[0090] In this embodiment, the reflectance spectrum is used to monitor an opaque film. When both the substrate and the film are infrared transparent materials, the projected spectrum data can be measured and the thickness data can be calculated based on the spectrum data.
[0091] In this embodiment, the coating time corresponding to different magnetic field directions is controlled, and the thickness change data of the film layer of the substrate during the coating time is collected. The second uniform deviation matrix is updated according to the thickness change data, thereby improving the uniformity of the film layer thickness while reducing the testing cost.
[0092] Further, based on any of the above embodiments, a fourth embodiment of the magnetron coating control method of the present invention is proposed. In this embodiment, referring to Figure 5 The preset correspondence relationship includes a mapping table, which is a mapping relationship between the second uniform deviation matrix and the magnetic field information and the air extraction information. The step of determining the magnetic field control data and the air extraction control data according to the second uniform deviation matrix, the corresponding matrix weight and the preset correspondence relationship includes:
[0093] Step S31, determining corresponding magnetic field information and air extraction information in the mapping table according to the second uniform deviation matrix;
[0094] Optionally, the second uniform deviation matrix is numbered, with each number corresponding to a magnetic field information and an air extraction information. In the third embodiment, the magnetic field information preferably only includes the direction of the magnetic field, and does not need to include other magnetic field information. This is because the rotation control method in the third embodiment is different from the traditional continuous rotation method. In the first and second embodiments, the magnetic field information can also include the magnetic field strength in addition to the direction of the magnetic field.
[0095] Step S32, determining the coating compensation time corresponding to the magnetic field information and the exhaust information according to the matrix weight corresponding to each of the second uniform deviation matrices;
[0096] In the technical solution based on the third embodiment, the weight w i The minimum step size corresponds to the time required for the film to have a thickness of 1 nm, so the coating compensation time corresponding to the magnetic field information and the pumping information is determined according to the matrix weight.
[0097] Step S33 , determining magnetic field control data and exhaust control data based on the coating compensation time corresponding to the magnetic field information and the exhaust information.
[0098] In this embodiment, after determining the magnetic field information, the exhaust information and the corresponding coating compensation time, the sputtering coating equipment can actually be controlled based on the above data, and the other parameters do not need to be modified during the control process.
[0099] In this embodiment, by determining the corresponding magnetic field information and pumping information in the mapping table according to the second uniform deviation matrix and determining the coating compensation time corresponding to the magnetic field information and the pumping information according to the matrix weight corresponding to each second uniform deviation matrix, control data for accurately controlling the magnetic field and argon extraction can be obtained, and the subsequent execution of the above data can improve the uniformity of the film layer.
[0100] Furthermore, the film thickness data includes film thicknesses corresponding to various detection positions of the substrate, and the step of determining a first uniform deviation matrix based on the film thickness data includes:
[0101] Calculate the average thickness based on the film thicknesses corresponding to all the detection positions;
[0102] Determining a uniform deviation value at each detection position according to the average thickness and the film thickness corresponding to the detection position;
[0103] Each position of the substrate is mapped to the position of an element of a corresponding matrix, position mapping information, and the first uniform deviation matrix is determined based on the position mapping information and the uniform deviation value corresponding to each position. In addition, after the position mapping information is determined, the position mapping information is not changed by the rotation of the magnetic field.
[0104] In addition, an embodiment of the present invention further provides a magnetron coating control device, the magnetron coating control device comprising:
[0105] an acquisition module, configured to acquire film thickness data of a substrate of a sputtering coating device, and determine a first uniformity deviation matrix based on the film thickness data, wherein each element of the first uniformity deviation matrix corresponds to a uniformity relative deviation value of a detection position on the substrate;
[0106] a matching module, configured to determine a matrix weight corresponding to each second uniform deviation matrix according to the first uniform deviation matrix and a coating optimization target, wherein the second uniform deviation matrix is a uniform deviation matrix obtained by detecting after coating is performed under preset magnetic field control data and preset exhaust control data within a preset time;
[0107] a generating module, configured to determine magnetic field control data and air extraction control data according to the second uniform deviation matrix, the corresponding matrix weights, and a preset corresponding relationship;
[0108] The control module is used to control the operation of the sputtering coating device according to the magnetic field control data and the exhaust control data. The magnetron coating control device can perform the steps of any embodiment of the magnetron coating control method described above.
[0109] In addition, embodiments of the present invention further provide a magnetron coating control system, comprising: a memory, a processor, and a magnetron coating control program stored in the memory and executable on the processor. The magnetron coating control program is configured to implement the steps of any of the aforementioned embodiments of the magnetron coating control method. Furthermore, the magnetron coating control system can control the operation of a sputtering coating apparatus. The sputtering coating apparatus may include: a vacuum chamber, a target, a substrate, a magnetic field system, a gas supply system, a vacuum pump system, and a power supply system. The target is mounted within the vacuum chamber, with the substrate positioned opposite the target. The magnetic field system is positioned behind the target and generates a magnetic field orthogonal to the electric field. The gas supply system provides working gas, such as argon, into the vacuum chamber, while the vacuum pump system maintains the vacuum within the chamber. The power supply system provides a DC electric field between the target and substrate, ionizing the argon gas to generate plasma. The magnetic field and electric field are perpendicular to each other, causing electrons to spiral within the magnetic field, increasing the probability of collision with argon atoms and raising the plasma density, thereby enhancing sputtering efficiency.
[0110] In addition, an embodiment of the present invention further provides a storage medium storing a magnetron coating control program. When the magnetron coating control program is executed by a processor, the steps of any of the above-mentioned magnetron coating control method embodiments are implemented.
[0111] It should be noted that, in this document, the terms "comprises," "includes," or any other variations thereof are intended to encompass non-exclusive inclusion, such that a process, method, article, or system comprising a series of elements includes not only those elements but also other elements not explicitly listed, or elements inherent to such process, method, article, or system. In the absence of further limitations, an element defined by the phrase "comprising a ..." does not exclude the presence of other identical elements in the process, method, article, or system comprising the element.
[0112] The serial numbers of the above embodiments of the present invention are for description only and do not represent the advantages or disadvantages of the embodiments.
[0113] Through the description of the above embodiments, those skilled in the art can clearly understand that the above-mentioned embodiment methods can be implemented by means of software plus the necessary general hardware platform, and of course can also be implemented by hardware, but in many cases the former is a better embodiment. Based on this understanding, the technical solution of the present invention is essentially or the part that contributes to the prior art can be embodied in the form of a software product, which is stored in a storage medium (such as ROM / RAM, magnetic disk, optical disk) as described above, and includes a number of instructions for enabling a terminal device (which can be a mobile phone, computer, server, or network device, etc.) to execute the methods described in each embodiment of the present invention.
[0114] The above are only preferred embodiments of the present invention and are not intended to limit the patent scope of the present invention. Any equivalent structure or equivalent process transformation made using the contents of the present invention description and drawings, or directly or indirectly applied in other related technical fields, are also included in the patent protection scope of the present invention.
Claims
1. A magnetron coating control method, characterized in that: Applied to sputtering coating equipment, the magnetron coating control method includes the following steps: Acquiring film thickness data of a substrate of a sputtering coating device, and determining a first uniformity deviation matrix based on the film thickness data, wherein each element of the first uniformity deviation matrix corresponds to a uniformity relative deviation value of a detection position on the substrate; Determine a matrix weight corresponding to each second uniform deviation matrix according to the first uniform deviation matrix and the coating optimization target, wherein the second uniform deviation matrix is a uniform deviation matrix obtained by detecting after coating is performed under preset magnetic field control data and preset exhaust control data within a preset time; Determining magnetic field control data and air extraction control data according to the second uniform deviation matrix, the corresponding matrix weight, and a preset corresponding relationship; The operation of the sputtering coating equipment is controlled according to the magnetic field control data and the exhaust control data.
2. The magnetron coating control method according to claim 1, wherein: Before the step of obtaining the film thickness data of the substrate of the sputtering coating device, the method further includes: Controlling the coating time corresponding to different magnetic field directions, and collecting thickness change data of the film layer of the substrate during the coating time, wherein the coating time corresponding to each magnetic field direction is continuous; The second uniform deviation matrix is updated according to the thickness variation data.
3. The magnetron coating control method according to claim 1, wherein: The step of determining the second uniform deviation matrix and the corresponding matrix weight according to the first uniform deviation matrix and the coating optimization target includes: Determine an objective function according to the first uniform deviation matrix and the coating optimization target, and generate an initial weight vector; Calculating a target weight vector corresponding to a Pareto optimal solution set according to the genetic algorithm, the objective function, and the initial weight vector, wherein elements of the target weight vector correspond one-to-one to matrix weights of the second uniform deviation matrix; The matrix weight is determined according to the target weight vector.
4. The magnetron coating control method according to claim 3, wherein: The step of determining the objective function according to the first uniform deviation matrix and the coating optimization target includes: Subtracting the first uniform deviation matrix from the uniform matrix corresponding to the coating optimization target to obtain a target matrix; The objective function is determined according to the target matrix, where the objective function is the root mean square error between the weighted matrix and the target matrix. Each of the second uniform deviation matrices is multiplied by the corresponding matrix weight as the corresponding third matrix to obtain multiple third matrices, and the weighted matrix is the sum of all third matrices.
5. The magnetron coating control method according to claim 1, wherein: The step of obtaining the film thickness data of the substrate of the sputtering coating device includes: controlling an infrared light source to illuminate the substrate and collecting a reflection spectrum of the substrate; The thickness data is calculated based on the reflection spectrum.
6. The magnetron coating control method according to claim 1, wherein: The preset correspondence includes a mapping table, which is a mapping relationship between the second uniform deviation matrix and the magnetic field information and the air extraction information. The step of determining the magnetic field control data and the air extraction control data according to the second uniform deviation matrix, the corresponding matrix weight, and the preset correspondence includes: Determining corresponding magnetic field information and air extraction information in the mapping table according to the second uniform deviation matrix; determining a coating compensation time corresponding to the magnetic field information and the exhaust information according to a matrix weight corresponding to each of the second uniform deviation matrices; The magnetic field information and the exhaust gas information are used to determine the magnetic field control data and the exhaust gas control data by using the coating compensation time corresponding to the magnetic field information and the exhaust gas information.
7. The magnetron coating control method according to any one of claims 1 to 6, characterized in that: The film thickness data includes the film thickness corresponding to each detection position of the substrate, and the step of determining the first uniform deviation matrix based on the film thickness data includes: Calculate the average thickness based on the film thicknesses corresponding to all the detection positions; Determining a uniform deviation value at each detection position according to the average thickness and the film thickness corresponding to the detection position; Each position of the substrate is mapped to the position of an element of a corresponding matrix, position mapping information, and the first uniform deviation matrix is determined according to the position mapping information and the uniform deviation value corresponding to each position.
8. A magnetron coating control device, characterized in that: The magnetron coating control device comprises: an acquisition module, configured to acquire film thickness data of a substrate of a sputtering coating device, and determine a first uniformity deviation matrix based on the film thickness data, wherein each element of the first uniformity deviation matrix corresponds to a uniformity relative deviation value of a detection position on the substrate; a matching module, configured to determine a matrix weight corresponding to each second uniform deviation matrix according to the first uniform deviation matrix and a coating optimization target, wherein the second uniform deviation matrix is a uniform deviation matrix obtained by detecting after coating is performed under preset magnetic field control data and preset exhaust control data within a preset time; a generating module, configured to determine magnetic field control data and air extraction control data according to the second uniform deviation matrix, the corresponding matrix weights, and a preset corresponding relationship; A control module is used to control the operation of the sputtering coating equipment according to the magnetic field control data and the exhaust control data.
9. A magnetron coating control system, characterized in that: The magnetron coating control system includes: a memory, a processor, and a magnetron coating control program stored in the memory and executable on the processor. The magnetron coating control program is configured to implement the steps of the magnetron coating control method according to any one of claims 1 to 7.
10. A storage medium, characterized in that: The storage medium stores a magnetron coating control program, and when the magnetron coating control program is executed by the processor, the steps of the magnetron coating control method according to any one of claims 1 to 7 are implemented.